Shaft gear part with large length-diameter ratio and machining method thereof
Through de-surplus processing, heat treatment and annealing and stress removal treatment, combined with the design of the intermediate bracket and clamping mechanism, the problems of low pass rate and high production costs of large-length diameter-biased shaft teeth-type parts are solved, and the processing accuracy and part rigidity are improved. A more stable processing process is achieved.
Patent Information
- Application Number
- CN202410892364.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-04
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2044-07-04
AI Technical Summary
The existing processing methods for large-length-diameter shaft teeth have problems such as low pass rate, high production cost, and inability to meet the requirements. The parts are prone to tempering cracks and bending deformation after forging, which affects subsequent processing and use.
The deflection and processing of heat treatment, tempering, straightening, annealing and stress removal, coarse grinding and precision forming are adopted, and the deflection and processing deformation of the parts are reduced by setting up an intermediate bracket and a specific clamping mechanism.
It effectively improves the machining accuracy and qualification rate of large-length-diameter shaft teeth parts, reduces production costs, stabilizes the size and shape of the parts, reduces deflection, and improves the rigidity and machining stability of the parts.
Smart Images

Figure CN118893430A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of mechanical processing tools, and in particular relates to a shaft gear part with a large aspect ratio and a processing method thereof. Background Art
[0002] The power take-off connecting shaft is one of the important parts of the tractor transmission. It is mainly used to transmit torque between the transmission and the power take-off. It is a typical large aspect ratio shaft and gear part. Its preparation accuracy has an important impact on the performance of the tractor transmission. However, the existing large aspect ratio shaft and gear part processing methods have the following main defects: large aspect ratio shaft and gear parts need to be tempered after forging, and tempering cracks will appear on the surface of the tempered parts, and the bending deformation of the parts is large, which affects the subsequent processing and use of the forging blank; the structural characteristics of the parts determine that the rigidity of such parts is extremely poor. During the processing, they are affected by the cutting force and their own gravity, and are prone to cutting chatter and processing deformation.
[0003] Due to the existence of the above two bottleneck problems, the qualified rate of large aspect ratio shaft gear parts is relatively low, the production cost remains high, and large-scale production is impossible. Therefore, it is urgent to develop a suitable and complete processing method for such parts. Summary of the invention
[0004] The purpose of the present invention is to provide a method for processing large aspect ratio shaft gear parts to solve the technical problems existing in the prior art of low qualified rate of large aspect ratio shaft gear parts, high production cost and machining accuracy that cannot meet the requirements.
[0005] The technical solution adopted by the present invention is:
[0006] A method for processing shaft gear parts with a large aspect ratio comprises the following steps:
[0007] Step 1, performing excess removal processing on the forging blank to obtain a blank to be processed;
[0008] Step 2, heat treating and tempering the blank to be processed to obtain a tempered blank;
[0009] Step 3, respectively opening center holes for straightening at both ends of the quenched and tempered blank; positioning the quenched and tempered blank with the center holes for straightening and completing straightening to obtain a straightened blank;
[0010] Step 4, annealing the straightened blank to relieve stress, to obtain an annealed blank;
[0011] Step 5, flatten the end faces of both ends of the annealed blank; re-drill the center hole at the position of the center hole for straightening; and perform rough outer grinding of the annealed blank on an outer cylindrical grinding machine with the center hole as the positioning hole to obtain a rounded blank;
[0012] Step 6, clamping and fixing the rounded blank on a clamping mechanism for rough turning to obtain a rough blank;
[0013] Step 7: Pre-grind the rough blank to the target size and then grind the outer circle;
[0014] Step 8: Finish turning.
[0015] The present invention also has the following technical features:
[0016] Specifically, the clamping mechanism includes a base, a three-jaw chuck arranged on the base, and a tail end tip arranged relative to the three-jaw chuck, and an intermediate bracket is also arranged between the three-jaw chuck and the tail end tip.
[0017] Furthermore, the center hole for straightening includes a first center hole and a second center hole, and the first center hole is coaxially arranged with the second center hole.
[0018] Furthermore, in step 6 and step 8, the clamping position of the intermediate bracket satisfies the following conditions:
[0019]
[0020] Where:
[0021] L is the length of the shaft and gear parts with large aspect ratio, in mm;
[0022] a is the distance between the center point of the top surface of the center bracket and the front end surface of the three-jaw chuck, in mm.
[0023] Furthermore, in the fine turning process described in step 8, the tool is moved from the three-jaw chuck toward the tail center.
[0024] Furthermore, in step 3, the warping amount of the blank after straightening is ≤0.3 mm.
[0025] Furthermore, the annealing stress relief treatment described in step 4 specifically includes placing the straightened blank into a pit furnace, hanging it, heating it to 450±10°C, and keeping it warm for 2.5 hours; cooling it to 200°C with the furnace, and cooling it to room temperature after it is taken out of the furnace.
[0026] Compared with the prior art, the present invention has the following beneficial effects:
[0027] The processing method provided by the present invention effectively solves the problems of low qualified rate of large length-diameter ratio shaft gear parts, high production cost and processing accuracy unable to meet product requirements; the method of the present invention performs excess removal processing on the forging blank and then performs tempering, which can eliminate forging cracks; the residual stress of the parts is eliminated by performing stress relief annealing heat treatment on the straightened parts, the size and shape of the parts are stabilized, and deformation and cracks in subsequent processing and use are reduced; the deflection of large length-diameter ratio shaft gear parts is effectively reduced by arranging an intermediate bracket; the clamping mechanism provided by the present invention has a simple structure, is easy to use, and is worth promoting. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] Figure 1 This is a schematic diagram of the finishing clamping of the part to be processed in Example 1;
[0029] Figure 2 The deflection calculation simulation results of the large aspect ratio shaft gear parts prepared in Example 1;
[0030] Figure 3 The deflection calculation simulation results of the large aspect ratio shaft gear parts prepared in comparative example 1;
[0031] Figure 4 The deflection calculation simulation results of the large aspect ratio shaft gear parts prepared in comparative example 2;
[0032] Figure 5 A simplified mechanical calculation model for shaft and gear parts with a large aspect ratio constructed in Example 1;
[0033] Figure 6 A schematic diagram of the tool direction for machining existing parts;
[0034] Figure 7 Schematic diagram of the tool direction for part machining in Example 1.
[0035] The numbers in the figure indicate:
[0036] 1- three-jaw chuck, 2- tail center, 3- middle bracket, 4- parts to be processed. DETAILED DESCRIPTION
[0037] In accordance with the above technical scheme, specific embodiments of the present invention are given below. It should be noted that the present invention is not limited to the following specific embodiments, and all equivalent changes made on the basis of the technical scheme of this application fall within the protection scope of the present invention.
[0038] The technical terms involved in the present invention are explained as follows:
[0039] Large aspect ratio parts: parts with a ratio of workpiece length to diameter ≥ 25.
[0040] Allowance: The thickness of the material to be processed
[0041] Remove the remaining material: remove the remaining material to be processed
[0042] The present invention is further described in detail below with reference to the embodiments.
[0043] Example 1
[0044] This embodiment provides a method for processing shaft gear parts with a large aspect ratio to obtain qualified shaft gear parts with a large aspect ratio, which specifically includes the following steps:
[0045] Step 1: Remove the excess material from the forging blank to obtain the blank to be processed; there are forging cracks on the surface of the forging blank, and direct quenching and tempering will cause the cracks on the surface of the forging blank to further expand, which will have a serious impact on the quality of the processed parts. Therefore, it is necessary to remove the excess material from the forging blank.
[0046] Step 2: heat treat and temper the blank to obtain a tempered blank; the surface hardness of the tempered blank is 31-35HRC. Due to the existence of tempering thermal stress, the tempered blank will have a certain amount of warping. Since the warping amount is large, the tempered blank cannot be directly fine-turned, so the tempered blank needs to be straightened and annealed to relieve stress.
[0047] Step 3, respectively opening center holes for straightening at both ends of the quenched and tempered blank, the center holes for straightening comprising a first center hole and a second center hole, the first center hole and the second center hole being coaxially arranged; positioning the quenched and tempered blank with the center holes for straightening and completing straightening to obtain a straightened blank; the warping amount of the straightened blank is ≤0.3mm.
[0048] Step 4: In order to prevent the straightened blank from rebounding due to the release of its own residual stress, the straightened blank needs to be annealed to relieve stress, thereby obtaining an annealed blank;
[0049] The annealing stress relief treatment specifically includes: placing the straightened blank into a pit furnace, hanging it, heating it to 450±10℃, and keeping it warm for 2.5 hours; cooling it to 200℃ with the furnace, and cooling it to room temperature after it is taken out of the furnace.
[0050] Step 5: mill the end faces of both ends of the annealed blank flat, ensuring that the milled length is greater than or equal to the total length of the part; re-drill the center hole at the location of the center hole for straightening; and perform rough grinding of the annealed blank on a cylindrical grinding machine with the center hole as the positioning hole to obtain a rounded blank;
[0051] In this embodiment, the width of the center bracket selected for use is 40mm. Therefore, a reference with a width greater than or equal to 44mm is ground in the middle of the length of the blank after annealing, and the runout of the processed outer cylindrical surface is ensured to be less than or equal to 0.02mm to ensure that the center bracket used for support does not interfere during rough turning.
[0052] Step 6, clamping and fixing the rounded blank on a clamping mechanism for rough turning to obtain a rough blank;
[0053] Among them, the clamping mechanism includes a base, a three-jaw chuck 1 arranged on the base and a tail end tip 2 arranged relative to the three-jaw chuck 1, and an intermediate bracket 3 is also arranged between the three-jaw chuck 1 and the tail end tip 2; with the help of the three-jaw chuck 1 and the tail end tip 2 arranged relative to the three-jaw chuck 1, they are fixed at both ends of the part 4 (blank) to be processed, and the part 4 (blank) to be processed is supported by the intermediate bracket 3, which can effectively reduce the deflection of the workpiece. If the part is bent and deformed, it will inevitably cause vibration, and in severe cases, tool hitting will occur, causing damage to the machine tool accuracy. The provision of the intermediate bracket 3 can effectively solve the above problems.
[0054] First, a rectangular coordinate system is established with the center of the front end face of the three-jaw chuck 1 as the origin, the axial direction of the part 4 (blank) to be processed as the X-axis direction, and the direction in the same horizontal plane as the X-axis direction and perpendicular to the X-axis direction as the Y-axis direction. The distance between the center point of the top surface of the center bracket 4 and the front end face of the three-jaw chuck 1 is defined as a.
[0055] With the center bracket as the fulcrum, the large aspect ratio shaft gear parts are divided into two sections, that is, the section from the three-jaw chuck 1 to the center point of the top surface of the intermediate bracket 4 is one section, and the section from the center point of the top surface of the intermediate bracket 4 to the right end surface of the part to be processed 4 (blank) is one section. These two sections correspond to two different flexural states and correspond to different models.
[0056] For any point on a large aspect ratio shaft gear part, when 0≤x≤a, the mechanical model of this section is a beam model with two ends fixed. When a≤x≤L (the length of the large aspect ratio shaft gear part), the mechanical model of this section is a beam model with one end fixed and the other end simply supported.
[0057] The deflection equation corresponding to any point on the large aspect ratio shaft gear parts is as follows:
[0058]
[0059] Where:
[0060] q is the self-distributed load of the large aspect ratio shaft and gear parts, and q = mg / L, in N / mm;
[0061] L is the length of the shaft and gear parts with large aspect ratio, in mm;
[0062] a is the distance between the center point of the top surface of the center bracket and the front end surface of the three-jaw chuck, in mm;
[0063] E is Young's modulus, in MPa;
[0064] x is the distance between any point on the large aspect ratio shaft gear parts and the three-jaw chuck, in mm;
[0065] y is the deflection of any point on the shaft gear parts with large aspect ratio, in mm;
[0066] I is the section inertia moment of the shaft gear parts with large aspect ratio, Unit: mm 4 ;
[0067] D is the diameter of the shaft and gear parts with aspect ratio to be processed, in mm.
[0068] Derivative the above two deflection equations and set the derivative equations to zero to obtain the X coordinates of the maximum values of the two deflection functions. Substitute the two X coordinates into the corresponding deflection equations to obtain the maximum values y1 and y2 of the two deflection equations. Let y1 = y2 to obtain the clamping position of the middle bracket, that is, the relationship equation between the center bracket position a and L:
[0069]
[0070] Solving the equation shows that when a=0.545L, the deflection of shaft gear parts with large aspect ratio is the smallest.
[0071] Step 7: Pre-grind the rough blank to the target size and then grind the outer circle;
[0072] To ensure the quality of fine turning, the rough blank can be pre-ground before fine turning, and the center bracket support and the three-jaw chuck clamping point can be ground externally to ensure that the runout of these two positions is less than 0.02mm, and ultimately ensure that the runout of all external circles of the parts after processing is less than 0.03mm.
[0073] Step 8, clamp and fix the rough blank processed in step 7 on the clamping mechanism, and perform fine turning to obtain the rough blank. During fine turning, the tool is moved from the three-jaw chuck to the tail center. Such a tool movement direction setting can significantly reduce the axial force of the part.
[0074] In this step, the clamping position of the center bracket is also determined by the following formula:
[0075]
[0076] Finally, it was determined that a=0.545L.
[0077] Specific as Figure 6As shown, according to the existing tool feeding direction, that is, tool feeding from the tail center to the three-jaw chuck, the relationship between the axial pressure FB applied to the part by the tail center, the axial cutting force FC borne by the part, and the axial supporting force FA applied to the part by the three-jaw chuck is: FA=FB+FC, and the axial forces on the parts at both ends of the intermediate bracket are: FB+2FC, FB-FC respectively.
[0078] from Figure 7 It can be seen that, using the cutting direction provided in this embodiment, the axial cutting force FC and the axial pressure FB applied to the part by the tail tip are in opposite directions, and the axial forces on the parts at both ends of the intermediate bracket are: FB-2FC, FB+FC, respectively, and the axial force on the parts is significantly reduced.
[0079] In this embodiment, the deflection test of the final prepared part was carried out, including: placing the center bracket at a = 0.4L, a = 0.7L and a = 0.545L respectively, and then obtaining the deflection at different positions on the part to obtain the deflection curve. The results are as follows: Figure 2 As shown in the figure, it can be seen that:
[0080] When a=0.4L, the maximum deflection occurs in the section a≤x≤L, and the maximum deflection is 0.003mm
[0081] When a=0.7L, the maximum deflection occurs in the segment 0≤x≤a, and the maximum deflection is 0.0027mm
[0082] When a=0.545L, the maximum deflection of the two sections is equal, and the maximum deflection is 0.001mm
[0083] From the above results, it can be determined that when the center support is located at 0.545L from the three claws, the part deflection is the smallest, which is more conducive to processing.
[0084] Comparative Example 1
[0085] This comparative example provides a processing method for shaft gear parts with a large aspect ratio. The operating steps of this comparative example are the same as those of Example 1, except that in step 6 and step 8, when clamping, the clamping method is to clamp one end with three jaws and leave the other end suspended.
[0086] The deflection test of the final parts prepared in this comparative example was carried out, and the results are as follows: Figure 4 As shown, the maximum deflection occurs at the suspended end, and the maximum deflection is -0.546mm.
[0087] Comparative Example 2
[0088] This comparative example provides a method for processing shaft gear parts with a large aspect ratio. The operation steps of this comparative example are the same as those of Example 1, except that in step 6 and step 8, when clamping, the clamping method is to clamp with three jaws at one end and to tighten with the tail center at the other end.
[0089] The deflection test of the final parts prepared in this comparative example was carried out, and the results are as follows: Figure 5 As shown in the figure, the maximum deflection occurs at the suspended end. The maximum deflection occurs in the middle of the workpiece, and the maximum deflection is -0.023mm.
[0090] It can be seen from Example 1, Comparative Example 1 and Comparative Example 2 that:
[0091] The deflection of the shaft gear parts with a large aspect ratio prepared by the method of the present invention is greatly reduced, thereby effectively enhancing the rigidity of the parts.
[0092] The preferred embodiments of the present disclosure are described in detail above in conjunction with the accompanying drawings; however, the present disclosure is not limited to the specific details in the above embodiments. Within the technical concept of the present disclosure, a variety of simple modifications can be made to the technical solution of the present disclosure, and these simple modifications all fall within the protection scope of the present disclosure.
[0093] It should also be noted that the various specific technical features described in the above specific embodiments can be combined in any suitable manner without contradiction. In order to avoid unnecessary repetition, the present disclosure will not further describe various possible combinations.
[0094] In addition, various embodiments of the present disclosure may be arbitrarily combined, and as long as they do not violate the concept of the present disclosure, they should also be regarded as the contents disclosed by the present disclosure.
Claims
1. A processing method for shaft gear parts with large aspect ratio, It is characterized in that The following steps are involved: Step 1, performing excess removal processing on the forging blank to obtain a blank to be processed; Step 2, heat treating and tempering the blank to be processed to obtain a tempered blank; Step 3, respectively opening center holes for straightening at both ends of the quenched and tempered blank; positioning the quenched and tempered blank with the center holes for straightening and completing straightening to obtain a straightened blank; Step 4, annealing the straightened blank to relieve stress, to obtain an annealed blank; Step 5, flatten the end faces of both ends of the annealed blank; re-drill the center hole at the position of the center hole for straightening; and perform rough outer grinding of the annealed blank on an outer cylindrical grinding machine with the center hole as the positioning hole to obtain a rounded blank; Step 6, clamping and fixing the rounded blank on a clamping mechanism for rough turning to obtain a rough blank; Step 7: Pre-grind the rough blank to the target size and then grind the outer circle; Step 8: Finish turning.
2. The method for processing shaft gear parts with large aspect ratio according to claim 1, It is characterized in that The clamping mechanism comprises a base, a three-jaw chuck arranged on the base and a tail end tip arranged relative to the three-jaw chuck, and an intermediate bracket is also arranged between the three-jaw chuck and the tail end tip.
3. The method for processing shaft gear parts with large aspect ratio as claimed in claim 1, It is characterized in that The center hole for straightening includes a first center hole and a second center hole, and the first center hole is coaxially arranged with the second center hole.
4. The method for processing shaft gear parts with large aspect ratio as claimed in claim 2, It is characterized in that In step 6 and step 8, the clamping position of the intermediate bracket is determined by the following formula: Where: L is the length of the shaft gear parts with large aspect ratio, in mm. a is the distance between the center point of the top surface of the center bracket and the front end surface of the three-jaw chuck, in mm.
5. The method for processing shaft gear parts with large aspect ratio according to claim 1, It is characterized in that In the fine turning process described in step 8, the tool is moved from the three-jaw chuck toward the tail center.
6. The method for processing shaft gear parts with large aspect ratio according to claim 1, It is characterized in that In the step 3, the warping amount of the blank after straightening is ≤0.3 mm.
7. The method for processing shaft gear parts with large aspect ratio according to claim 1, It is characterized in that The annealing stress relief treatment described in step 4 specifically includes placing the straightened blank into a pit furnace, hanging and hoisting it, heating it to 450±10°C, and keeping it warm for 2.5 hours; cooling it to 200°C with the furnace, and cooling it to room temperature after it is taken out of the furnace.
8. The method for processing shaft gear parts with large aspect ratio as claimed in claim 1, It is characterized in that In step 7, when the outer circle is ground, the outer circle runout of the machined end surface at the three-jaw chuck and the intermediate bracket is less than 0.02 mm.
Citation Information
Patent Citations
Method for machining long and thin rod part on ordinary lathe
CN103611948A
Improvement method of shaft part machining technology
CN104959629A
Arrangement method for temporary supports for intermediate shaft
CN105234209A
Processing technology of engine crankshaft
CN109746649A
Method for machining zirconium alloy shaft of mother liquor circulating pump
CN116160206A