Preparation method of pressure-resistant annular air-blowing optical cable

By using silicone oil grooves, barrier plates, side slide plates and side slide plate grooves in the air-blow optical cable, the problem of insufficient side pressure resistance is solved, the air blowing performance and material stability are improved, and the High speed operation during air blowing.

CN118897362AActive Publication Date: 2024-11-05FAR EAST COMMUNICATIONS CO LTD
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
CN202410979948.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-22
Publication Date
2024-11-05
Estimated Expiration
2044-07-22

AI Technical Summary

Technical Problem

The existing air-blowing optical cables are insufficient in the laid process, which is prone to bursting and fiber damage, affecting the air-blowing performance.

Method used

A pressure-resistant annular air-blown optical cable is designed, using a silicone oil groove, a grid baffle, a side slide and a side slide groove. Silicone oil flows to push the grid baffle and a side slide when under pressure to form an annular support and disperse the pressure. Aramid reinforcement is added to the inner sheath to improve the resistance to side pressure.

Benefits of technology

It effectively improves the side pressure resistance and air blowing performance of the air blowing optical cable, avoids deformation of the optical fiber during bending and flattening, improves the stability and rigidity of the material, and realizes high-speed operation during air blowing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118897362A_ABST
    Figure CN118897362A_ABST
Patent Text Reader

Abstract

The invention discloses a pressure-resistant annular air-blowing optical cable and a preparation method thereof, the optical cable comprises a cable core, an inner sheath, a silicone oil groove, a grid baffle plate, an outer sheath, side sliding plates and side sliding pressure-resistant annular air-blowing optical cable plate grooves, the inner sheath is arranged in the cable oil groove, a flow channel is arranged between the side sliding plate grooves, and the grid baffle plate is in a sector; a first side sliding plate groove; the silicon oil groove is formed between the inner sheath and the outer sheath, the grid baffle is arranged on the outer layer of the outer sheath in a sliding mode, the side sliding plate is arranged in the side sliding plate groove, and a side sliding plate sliding outlet is formed in the side sliding plate, the outer sheath, the flow channel, the side sliding plate and the side sliding plate groove in the same side formed by the side sliding plate groove and the center of the cable core. One side of the inner grid baffle plate of the inner sheath is provided with a one-way limiting convex plate groove connected position provided with a convex groove, and the inner side of the inner sheath is provided with a corresponding concave groove close to the corresponding position of the flow channel. According to the invention, the displacement of the grid baffle plate and the side sliding plate under the pushing of silicone oil realizes the bidirectional improvement of the side pressure resistance and the air blowing performance of the air-blowing optical cable.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for preparing a pressure-resistant annular air-blown optical cable, belonging to the technical field of optical cables. Background Art

[0002] With the development of network communication technology, the demand for information and communication has exploded. The existing pipeline resources can no longer meet the needs of network expansion, and the construction of new communication pipelines has problems such as high cost, difficult construction, and serious damage to public facilities. Air-blown optical cable technology can effectively solve the above problems. The optical cable designed in this scheme has a small diameter, high fiber density, high laying efficiency and easy recovery. It has become the preferred optical cable type for domestic and foreign trunk lines. In this technical scheme, the optical cable is installed in the pre-installed pipeline through viscous tension. In the actual laying process, air-blowing heads and high-pressure gas are generally used to push the optical cable. The most critical factor in the process of pushing the optical cable is the stiffness of the optical cable. Its lateral pressure resistance energy will directly affect the air-blowing performance of the optical cable. When the optical cable's lateral pressure resistance is insufficient, problems such as bursting and optical fiber damage often occur. How to improve the optical fiber's lateral pressure resistance and air-blowing performance is the key to improving the performance of air-blown optical cables. Summary of the invention

[0003] The object of the present invention is to provide a method for preparing a pressure-resistant annular air-blown optical cable to solve the problems in the above-mentioned background technology.

[0004] The technical scheme for achieving the purpose of the present invention is: a pressure-resistant annular air-blown optical cable, comprising a cable core, an inner sheath, a silicone oil groove, a baffle, an outer sheath, a side slide and a side slide groove, wherein the inner sheath is arranged on the periphery of the cable core, the silicone oil groove is arranged between the inner sheath and the outer sheath, the baffle is slidably arranged in the silicone oil groove, the side slide groove is arranged at intervals on the outer layer of the outer sheath, the side slide is arranged in the side slide groove, a flow channel is arranged between the side slide and the outer sheath, the baffle, the flow channel, the side slide and the side slide groove are located in the same fan-shaped formed by the side slide groove and the center of the cable core; the silicone oil groove is filled with silicone oil; the space between the cable core and the inner sheath is filled with cable paste; a side slide sliding outlet is arranged on one side of the side slide groove; a one-way limiting protrusion is arranged on one side of the inner baffle of the inner sheath; a convex groove is arranged at a position on the outer side of the outer sheath that is not connected to the side slide groove, and a corresponding groove is arranged on its inner side near the corresponding position of the flow channel.

[0005] During use, when the outer sheath is squeezed, the convex groove is squeezed first, the silicone oil in the silicone oil groove flows, the baffle plate is displaced under the push of the silicone oil, the silicone oil in the flow channel flows to the side slide groove, and the side slide is pushed out from the side slide sliding outlet under the push of the silicone oil, the baffle plate is pushed to the bottom of the convex groove, and the side slide is pushed to the top of the convex groove. The baffle plate and the side slide form an annular support, and the extrusion force on the convex groove is dispersed to the silicone oil groove. The silicone oil acts as a partition layer and reduces the stress on the inner sheath at the same time, reducing the stress on the internal optical fiber and the inner sheath.

[0006] In the above structure, the convex groove and the concave groove cooperate to increase the silicone oil capacity in the silicone oil tank, thereby reducing the required force.

[0007] In the above structure, the good fluidity of silicone oil can effectively reduce the stress time, but too good fluidity will cause dripping problems. It is necessary to control the dynamic viscosity of silicone oil at 20°C (68°F) to 1200-1800mPa.s.

[0008] Further or optionally, aramid reinforcements are evenly arranged around the cable core inside the inner sheath, and the aramid reinforcements are used to support the inner sheath. The aramid reinforcements are evenly distributed in a 360° circle and placed at the center of the inner sheath, and are formed into one body with the inner sheath by extrusion. The bonding strength between the aramid reinforcements and the inner sheath is above 60N, which can effectively avoid displacement between the aramid reinforcements and the inner sheath during bending and flattening.

[0009] Further or optionally, in order to improve the flexibility of the blocking plate and the side sliding plate, the elastic modulus is limited to 520-640 GPa and the density is: 1.3-1.6 g / cm 3 The compressive parameters and density of the baffle and side slide affect the progress and stability of the annular support. The lighter they are, the faster they can move, thereby reducing the stress time and reducing the bending and jamming problems during the air blowing process. During preparation, it is necessary to strictly select the materials. During preparation, carbon fiber composite materials are first mixed with graphite and glue to prepare a carbon fiber composite material in an effective ratio, so that the elastic modulus is controlled at 520-640GPa and the density is controlled at 1.8-2.0g / cm 3 Then, TPU is extruded and foamed on the outer layer of the carbon fiber composite to reduce its density to 1.3-1.6 g / cm 3 .

[0010] Further or optionally, the hardness of the loose tube is ≥110Shore D, and the elastic modulus is ≥2400Mpa. Its specific components are bisphenol S (50-60 parts), epichlorohydrin (10-20 parts), polyimide PI slurry (5-10 parts), ABS resin (5-15 parts), chopped glass fiber (0.5-3 parts), antioxidant (2-4 parts), calcium carbonate (4-8 parts), silica (0.5-3 parts), polyphenylene sulfide PPS resin (5-15 parts). In this scheme, the benzene ring is further expanded by upgrading bisphenol A to bisphenol S, and the strength and modulus are simultaneously improved by introducing glass fiber and silica. The mixed extrusion of polyphenylene sulfide, ABS resin and PC resin further improves the hardness properties of the material, and the epoxide ring-opening polymerization method, blending modification and directional stretching process are continuously used in the production process to further improve the stability and rigidity of the material.

[0011] Further or optionally, in order to enhance the strength of the cable core, the cable core includes a central reinforcement member and an optical fiber unit arranged from the inside to the outside, the optical fiber unit is arranged around the central reinforcement member, includes a loose tube and an optical fiber, and fiber paste is filled between the optical fiber and the loose tube; the loose tube is made of polycarbonate.

[0012] In order to avoid the bending of the optical cable under the push of air flow and the friction and extrusion with the inner wall of the pipe during the air blowing process, the anti-lateral pressure is insufficient, the loose tube will be flattened, and the space of the optical fiber in the loose tube will be further compressed, resulting in increased bending loss and even fiber breakage. In the process of preparing the cable core, the performance of polycarbonate needs to be strictly selected so that its anti-lateral pressure can reach 1400N at 0.15mm. In order to achieve this parameter, it is generally recommended that its hardness be controlled at 110Shore D and the elastic modulus be kept above 2400Mpa.

[0013] Further or optionally, in order to make the force on each part more uniform, the baffle plate, the side slide plate and the side slide plate groove are three groups evenly distributed at 120°, and the flow channel, the convex groove and the concave groove are multiple.

[0014] The present invention also provides a method for preparing a pressure-resistant annular air-blown optical cable, comprising the following steps:

[0015] Prepare the guardrail and side skid plates;

[0016] preparing an aramid reinforcement;

[0017] preparing an inner sheath;

[0018] Prepare the outer sheath and side slide grooves.

[0019] The preparation method has simple steps and smooth connections between the steps, which can effectively improve production efficiency.

[0020] Further or optionally, the steps of preparing the baffle plate and the side slide plate are:

[0021] Immersing the carbon fiber composite yarn in a graphene dispersion to obtain a mixture;

[0022] The mixture is molded to obtain the guard plate and the side skid plate parts;

[0023] The baffle plate and side slide plate parts are placed into the mold core in the form of extruded tubes and initially fixed.

[0024] In the above steps, pay attention to adjusting the tension according to the size of the silk thread during the pay-off process, pay attention to the preheating temperature when the carbon fiber is immersed in the graphene dispersion, perform multi-stage preheating and pay attention to controlling the production speed to maintain the fusion rate; in the process of curing the glue, pay attention to graded treatment to maintain uniform curing of the inner and outer ends, and at the same time use the increase in hardness during the curing process to prevent scratches and damage during the flow process.

[0025] Further or optionally, the steps of preparing the outer sheath and the side slide plate groove are:

[0026] The inner jacket and the baffle plate are put into the mold core through the oil-filled pipe and extruded together with the silicone oil;

[0027] Cooling the extruded product;

[0028] In the above extrusion process, the mold core and the mold sleeve are respectively provided with symmetrical convex grooves, and the flow channels and side slide plate slots are provided at the intermediate positions thereof, so as to enter the mold sleeve in the form of an extruded tube.

[0029] During the above extrusion process, it is necessary to pay attention to maintaining the pressure so that the silicone oil can be evenly filled in the silicone oil groove and the flow channel; the side slide is released by active wire release, and passes through the side slide fixing device before entering the machine head, and enters the mold sleeve in the form of an extruded tube through the side slide slot hole in the mold core. The mold sleeve is also provided with corresponding side slide slots, so that the overall shape is extruded and formed. After forming, it directly enters the cooling water tank at 10°C for cooling. The temperature of the second water tank is set to 0°C. Rapid cooling is used to avoid the leakage of silicone oil.

[0030] By adopting the above technical solution, the present invention has the following beneficial effects:

[0031] (1) The present application provides an air-blown optical cable that can effectively improve the ability to resist lateral pressure, thereby achieving a two-way improvement in the ability to resist lateral pressure and the air-blowing performance of the air-blown optical cable.

[0032] (2) The structure of the present invention also provides an inner sheath with an aramid reinforcement support, which can effectively prevent the inner sheath from being deformed during the bending process of the optical cable.

[0033] (3) The present invention also selects the loose tube material so that its lateral pressure resistance can reach 1400N at 0.15mm, and the material hardness reaches 110Shore D, thereby improving the air blowing performance of the optical cable.

[0034] (4) The present invention also limits the number of baffles, side slides and side slide grooves to make the force more uniform and the performance better.

[0035] (5) The present invention also provides a method for preparing a pressure-resistant annular air-blown optical cable, which has excellent process connectivity and a simple preparation process, and is conducive to large-scale production. BRIEF DESCRIPTION OF THE DRAWINGS

[0036] In order to make the content of the present invention more clearly understood, the present invention is further described in detail below according to specific embodiments and in conjunction with the accompanying drawings, wherein

[0037] Figure 1 It is a structural schematic diagram of the present invention.

[0038] Figure 2 It is a schematic diagram of the structure of the present invention under extrusion.

[0039] Figure 3 and Figure 4 It is a schematic diagram of the process of the preparation method of the present invention.

[0040] The reference numerals in the accompanying drawings are:

[0041] Cable core 1, central reinforcement member 11, optical fiber unit 12, loose tube 121, optical fiber 122, inner sheath 2, aramid reinforcement member 21, silicone oil groove 3, baffle plate 4, outer sheath 5, convex groove 51, concave groove 52, side slide plate 6, side slide plate groove 7, flow channel 8. DETAILED DESCRIPTION

[0042] In order to better understand the above technical solution, the above technical solution will be described in detail below in conjunction with the accompanying drawings and specific implementation methods.

[0043] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Generally, the components of the embodiments of the present invention described and shown in the drawings here can be arranged and designed in various different configurations.

[0044] Therefore, the following detailed description of the embodiments of the present invention provided in the accompanying drawings is not intended to limit the scope of the invention claimed for protection, but merely represents selected embodiments of the present invention. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0045] It should be noted that similar reference numerals and letters denote similar items in the following drawings, and therefore, once an item is defined in one drawing, further definition and explanation thereof is not required in subsequent drawings.

[0046] In the description of the embodiments of the present invention, it should be understood that the terms "center", "up", "down", "left", "right", "vertical", "horizontal", "inside", "outside", etc. indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, or are the orientations or positional relationships in which the inventive product is conventionally placed when used, or are the orientations or positional relationships conventionally understood by those skilled in the art. They are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present invention.

[0047] In the description of the embodiments of the present invention, it is also necessary to explain that, unless otherwise clearly specified and limited, the terms "set", "installed", "connected" and "connected" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral connection; it can be directly connected, or indirectly connected through an intermediate medium, or it can be the internal connection of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances. The present invention is further described below in conjunction with the accompanying drawings. The following embodiments are only used to more clearly illustrate the technical solution of the present invention, and cannot be used to limit the scope of protection of the present invention.

[0048] (Example 1)

[0049] See Figure 1 A pressure-resistant annular air-blown optical cable, comprising a cable core 1, an inner sheath 2, a silicone oil groove 3, a baffle plate 4, an outer sheath 5, a side slide plate 6 and a side slide plate groove 7, wherein the inner sheath 2 is arranged on the outer periphery of the cable core 1, the silicone oil groove 3 is arranged between the inner sheath 2 and the outer sheath 5, the baffle plate 4 is slidably arranged in the silicone oil groove 3, the side slide plate groove 7 is arranged at intervals on the outer layer of the outer sheath 5, the side slide plate 6 is arranged in the side slide plate groove 7, a flow channel 8 is arranged between the side slide plate 6 and the outer sheath 5, the baffle plate 4 is arranged on the outer periphery of the cable core 1, the silicone oil groove 3 is arranged between the inner sheath 2 and the outer sheath 5, the baffle plate 4 is slidably arranged in the silicone oil groove 3, the side slide plate groove 7 is arranged on the outer layer of the outer sheath 5, the side slide plate 6 is arranged in the side slide plate groove 7, a flow channel 8 is arranged between the side slide plate 6 and the outer sheath 5, the baffle plate The plate 4, the flow channel 8, the side slide plate 6 and the side slide plate groove 8 are located in the same sector formed by the side slide plate groove 7 and the center of the cable core 1; the silicone oil groove 3 is filled with silicone oil; the space between the cable core 1 and the inner sheath 2 is filled with cable paste; a side slide plate sliding outlet is provided on one side of the side slide plate groove 7; a one-way limiting protrusion is provided on one side of the inner baffle plate of the inner sheath; a convex groove 51 is provided at a position on the outside of the outer sheath 5 that is not connected to the side slide plate groove 7, and a corresponding groove 52 is provided on its inner side near the corresponding position of the flow channel 8.

[0050] The baffle plate 4, the side slide plate 6 and the side slide plate groove 7 are three groups evenly distributed at 120 degrees, and the flow channel 8, the convex groove 51 and the concave groove 52 are multiple.

[0051] After adopting this structure, pressure is applied to the outer wall of the pressure-resistant annular air-blown optical cable, and its structure after being stressed is as follows: Figure 2As shown, the silicone oil in the silicone oil groove 3 flows, and the baffle plate 4 moves in a fixed direction under the action of the limit device. The silicone oil enters the side slide groove 7 through the flow channel 8, and the side slide 6 is pushed by the silicone oil to move through the side slide sliding outlet, thereby finally achieving 360° rigid protection for the outer layer of the optical cable.

[0052] Aramid reinforcement members 21 are evenly arranged inside the inner sheath 2 and around the cable core 1 .

[0053] It should be emphasized that the aramid reinforcement member 21 is extruded inside the inner sheath 2 to prevent the occurrence of misalignment that causes the rigidity of the inner sheath to decrease. When the aramid reinforcement member 21 is extruded outside the inner sheath 2, the inner sheath 2 is deformed before and after being squeezed. Figure 3 As shown, only one side thereof is deformed, and the overall strength is reduced, which is not conducive to protecting the internal cable core structure. When the aramid reinforcement 21 is extruded inside the inner sheath 2, the inner sheath 2 is deformed as a whole. During the compression process of the inner sheath 2, all the aramid reinforcements 21 will be used for support, so that the optical cable will be elliptical after being subjected to force.

[0054] The cable core 1 includes a central reinforcement member 11 and an optical fiber unit 12 arranged from the inside to the outside. The optical fiber unit 12 is arranged around the central reinforcement member 11 and includes a loose tube 121 and an optical fiber 122. The space between the optical fiber 122 and the loose tube 121 is filled with fiber paste; the loose tube 121 is made of polycarbonate.

[0055] According to the test, when the wall thickness of the loose tube 121 is 0.15 mm, the lateral pressure resistance can reach 1400 N. There is a great margin in the process of air blowing laying, which is conducive to high-speed air blowing operation.

[0056] The present invention also provides a method for preparing a pressure-resistant annular air-blown optical cable, comprising the following steps:

[0057] Prepare the baffle plate 4 and the side slide plate 6;

[0058] Preparing an aramid reinforcement member 21;

[0059] preparing an inner sheath 2;

[0060] The outer sheath 5 and the side slide plate groove 7 are prepared.

[0061] The steps for preparing the baffle plate 4 and the side slide plate 6 are as follows:

[0062] Immersing the carbon fiber composite yarn in a graphene dispersion to obtain a mixture;

[0063] The mixture is molded to obtain the baffle plate 4 and the side slide plate 6 parts;

[0064] The baffle plate 4 and the side slide plate 6 parts are placed into the mold core in the form of extruded tubes and preliminarily fixed.

[0065] The specific process is as follows Figure 3 and Figure 4 As shown,

[0066] The carbon fiber composite yarn is released in an active pay-off form, and the tension is adjusted according to the yarn size, and is controlled in the range of 100g to 350g. A two-stage roller positioning device is configured, and a box immersed in graphene dispersion is configured in front of the roller positioning device, and a preheating device is configured behind the box immersed in graphene dispersion. The preheating temperature is 65±5°C, and the production speed is 0.5m / min. The box of graphene dispersion consists of a positioning mold, an injection port, a reflux injection port and an overflow collection box. The carbon fiber composite yarn passes through the positioning mold into the box and through the graphene dispersion. The overflowed graphene dispersion flows into the overflow collection box and is injected into the box through the reflux pipeline. Continuous injection ensures that the carbon fiber composite yarn is completely immersed in the graphene dispersion. Low-speed production and complete immersion ensure that the graphene is uniformly adsorbed on the carbon fiber surface or penetrates into the fiber. The four-stage positioning mold ensures the center position of the carbon fiber composite yarn to avoid the reduction of the fusion rate caused by the scratching of the graphene adsorbed on the carbon fiber surface due to the angle difference. The mixture is formed by an extrusion die, and a box for graphene dispersion and a glue injection box are arranged in front of the extrusion die, a preheating device is arranged behind the glue injection box, and a baking device is arranged behind the extrusion die. Through multi-stage preheating, the liquid graphene dispersion is combined with the carbon fiber composite yarn in a solid form and effectively bonded by glue, and then baked for shaping (multi-stage segmented heating ensures uniform curing of the inner and outer ends, while improving the fusion of each section of graphene. After curing, it is converted from liquid to solid, reducing the scratching and loss caused by the roller positioning device, and further improving the fusion of the graphene dispersion and the carbon fiber composite yarn). A plurality of composite materials after baking are actively released, and the above operations are continued to form baffles and side slides of different shapes. The baffles and side slides of different shapes pass through the mold core in the form of extruded tubes and are vacuumed to achieve the adhesion of TPU to the baffles and side slides, and are cooled through a cooling water tank and then collected on a tray.

[0067] Specifically, the central reinforcement and the loose tube 121 are produced by SZ twisting and fixed by aramid yarn. The absolute value of the linear expansion coefficient of the aramid yarn at 80°C is less than 5.3×10-6°C-1. The extremely low shrinkage reduces the problem of tightening the bundle tube due to thermal expansion and contraction during the temperature cycle, thereby reducing the optical fiber duty cycle and increasing the loss. The yarn pitch and the twisting pitch are adjusted according to the product structure. The cable core is filled with water-blocking cable paste for water blocking, while preventing the inner sheath 1 from directly contacting the loose tube 121. If the inner sheath 2 directly contacts the loose tube 121 during the extrusion process, the loose tube 121 will expand due to heat, causing the excess length to change. At the same time, it is easy to adhere to the inner sheath 2 and change with the inner sheath 2, thereby further inducing the excess length change, so the cable paste is fully filled. The cable core 1 is molded from the center hole of the mold core, and the aramid strength member 21 enters from the evenly distributed holes on the mold core and is molded at the same time as the cable core 1. The sheath material is squeezed in from between the mold core and the mold sleeve. The mold core is a tubular structure. During extrusion, the cable core 1 and the aramid strength member 21 can be effectively separated, so that the aramid strength member 21 is extruded between the inner sheaths 2, and the cable core 1 is extruded inside the inner sheath 2. The extrusion temperature is from 155 to 185°C. Low-temperature extrusion is also to reduce the influence of heat on the excess length of the loose tube.

[0068] The steps for preparing the outer sheath 5 and the side slide plate groove 7 are as follows:

[0069] The inner sheath 5 and the baffle plate 4 are introduced into the mold core through the oil filling pipe and extruded together with the silicone oil;

[0070] Cooling the extruded product;

[0071] In the above extrusion process, the mold core and the mold sleeve are respectively provided with symmetrical convex grooves, and the flow channel 8 and the side slide plate groove 7 holes are provided at the intermediate positions thereof, so as to enter the mold sleeve in the form of an extruded tube.

[0072] Specifically, the inner sheath 2 and the baffle plate 3 are molded together through the oil filling pipe, and are extruded together with the silicone oil during the production process. The oil filling device automatically maintains the pressure, so that the silicone oil can be evenly filled in the flow channel. The mold core and the mold sleeve are respectively provided with symmetrical convex grooves, and the flow channel 8 and the side slide plate groove 7 are set in the neutral position. The side slide plate 6 is released by active wire release, and passes through the side slide plate 6 fixing device before entering the head. The side slide plate groove 7 in the mold core is extruded into the mold sleeve in the form of a tube. The mold sleeve is also provided with a corresponding side slide plate groove 7, so that the overall shape is extruded and molded. After molding, it directly enters the cooling water tank at 10°C for cooling. The temperature of the second water tank is set to 0°C. Through rapid cooling, the leakage of silicone oil is avoided. After cooling, the optical cable is collected on the reel.

[0073] The specific embodiments described above further illustrate the objectives, technical solutions and beneficial effects of the present invention in detail. It should be understood that the above description is only a specific embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A pressure-resistant annular air-blown optical cable, characterized in that: The invention comprises a cable core (1), an inner sheath (2), a silicone oil groove (3), a baffle plate (4), an outer sheath (5), a side slide plate (6) and a side slide plate groove (7), wherein the inner sheath (2) is arranged on the outer periphery of the cable core (1), the silicone oil groove (3) is arranged between the inner sheath (2) and the outer sheath (5), the baffle plate (4) is slidably arranged in the silicone oil groove (3), the side slide plate groove (7) is arranged at intervals on the outer layer of the outer sheath (5), the side slide plate (6) is arranged in the side slide plate groove (7), and the side slide plate (6) and the outer sheath are connected to each other. (5), a flow channel (8) is provided between the baffle plate (4), the flow channel (8), the side slide plate (6) and the side slide plate groove (8) are located in the same sector formed by the side slide plate groove (7) and the center of the cable core (1); a side slide plate sliding outlet is provided on one side of the side slide plate groove (7); a one-way limiting protrusion is provided on one side of the baffle plate inside the inner sheath; a convex groove (51) is provided at a position on the outside of the outer sheath (5) not connected to the side slide plate groove (7), and a corresponding concave groove (52) is provided on the inside thereof near a corresponding position of the flow channel (8).

2. A pressure-resistant annular air-blown optical cable according to claim 1, characterized in that: Aramid reinforcement members (21) are evenly arranged around the cable core (1) inside the inner sheath (2).

3. A pressure-resistant annular air-blown optical cable according to claim 1, characterized in that: The cable core (1) comprises a central reinforcement member (11) and an optical fiber unit (12) arranged from the inside to the outside. The optical fiber unit (12) is arranged around the central reinforcement member (11) and comprises a loose tube (121) and an optical fiber (122). The optical fiber (122) and the loose tube (121) are filled with fiber paste. The loose tube (121) is made of polycarbonate, and its hardness is ≥110 Shore D, and its elastic modulus is ≥2400Mpa.

4. A pressure-resistant annular air-blown optical cable according to claim 3, characterized in that: The specific components of the loose tube are bisphenol S (50-60 parts), epichlorohydrin (10-20 parts), polyimide PI slurry (5-10 parts), ABS resin (5-15 parts), chopped glass fiber (0.5-3 parts), antioxidant (2-4 parts), calcium carbonate (4-8 parts), silicon dioxide (0.5-3 parts), and polyphenylene sulfide PPS resin (5-15 parts).

5. The pressure-resistant annular air-blown optical cable according to claim 1, characterized in that: The elastic modulus of the blocking plate (6) and the side sliding plate (7) is 520-640 GPa, and the density is 1.3-1.6 g / cm3.

6. A pressure-resistant annular air-blown optical cable according to any one of claims 1 to 5, characterized in that: The baffle plate (4), the side slide plate (6) and the side slide plate groove (7) are three groups evenly distributed at 120 degrees, and the flow channel (8), the convex groove (51) and the concave groove (52) are multiple.

7. A method for preparing a pressure-resistant annular air-blown optical cable, characterized in that The following steps are involved: Prepare a baffle plate (4) and a side slide plate (6); preparing an aramid reinforcement member (21); preparing an inner sheath (2); Prepare the outer sheath (5) and the side slide plate groove (7).

8. The method for preparing a pressure-resistant annular air-blown optical cable according to claim 7, characterized in that: The steps for preparing the baffle plate (4) and the side slide plate (6) are as follows: Immersing the carbon fiber composite yarn in a graphene dispersion to obtain a mixture; The mixture is molded to obtain the baffle plate (4) and the side slide plate (6) parts; The baffle plate (4) and the side slide plate (6) parts are placed into the mold core in the form of extruded tubes and are preliminarily fixed.

9. The method for preparing a pressure-resistant annular air-blown optical cable according to claim 7, characterized in that: The steps for preparing the outer sheath (5) and the side slide plate groove (7) are as follows: The inner sheath (5) and the baffle plate (4) are introduced into the mold core through the oil filling pipe and extruded together with the silicone oil; Cooling the extruded product; In the above extrusion process, the mold core and the mold sleeve are respectively provided with symmetrical convex grooves, and the flow channel (8) and the side slide plate groove (7) holes are provided at the intermediate positions thereof, so as to enter the mold sleeve in the form of an extruded tube.

Citation Information

Patent Citations

  • Miniature half-tight-sleeving gas-blast optical fiber unit

    CN102122049A

  • Superfine and anti-fermite air-blowing optical cable and fabrication method thereof

    CN109061822A

  • Optical fiber cable with long service life

    CN112433321A

  • Novel electric power composite optical cable

    CN208580236U

  • Anti-extrusion optical cable