Semiconductor structure and manufacturing method thereof
By forming character line trenches in isolation and active areas during semiconductor manufacturing, and depositing dielectric layers, the leakage problem in semiconductor structures caused by too close spacing is solved, and process yield and performance are improved.
Patent Information
- Application Number
- CN202310661639.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-05-02
- Filing Date
- 2023-06-06
- Publication Date
- 2024-11-05
AI Technical Summary
During semiconductor manufacturing, due to the reduction of the semiconductor structure size, components are prone to leakage due to too close spacing, resulting in a decrease in process yield and it is difficult to effectively reduce leakage problems.
By forming an isolation region and an active region in the substrate, and forming the first and second character line trenches in the active region and the isolation region, dielectric layers are deposited and etched to form a character line structure, ensuring etching of the dielectric material Depth consistency to reduce leakage.
It achieves better control of the depth and consistency of the character line structure, reduces leakage problems, and improves the performance of the semiconductor structure.
Smart Images

Figure CN118900559A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a semiconductor structure and a manufacturing method thereof, and more particularly, the present invention relates to a semiconductor structure with a word line structure and a manufacturing method thereof. Background Art
[0002] As electronic devices become lighter and thinner, semiconductor devices such as dynamic random access memory (DRAM) are becoming more highly integrated. In addition, the performance of DRAM is improved by shortening the pitch between semiconductor structures in DRAM. As the size of semiconductor structures decreases, in addition to increasing the difficulty of the process, the components in the semiconductor structure are also prone to leakage due to the close pitch.
[0003] Therefore, in the semiconductor manufacturing process, how to reduce leakage to improve the process yield of the semiconductor structure becomes an important issue. Summary of the invention
[0004] Some embodiments of the present invention provide a method for manufacturing a semiconductor structure, comprising the following steps. An isolation region and an active region are formed in a substrate, and the active region and the isolation region are adjacent. A first word line trench is formed in the active region. A first dielectric layer is deposited in the first word line trench and on the active region and the isolation region. A second word line trench is formed in the active region and the isolation region by etching the first dielectric layer, and the second word line trench is linear and extends through the active region and the isolation region, and a portion of the first dielectric layer is retained at the bottom of the second word line trench. In addition, a word line structure is formed in the second word line trench.
[0005] In some embodiments, the first word line trench has a first depth, and the second word line trench has a second depth; and the first depth is greater than the second depth.
[0006] In some embodiments, the first dielectric layer is deposited such that the first dielectric layer is higher than the active region and has a height equal to the second depth of the second word line trench.
[0007] In some embodiments, forming a first word line trench in the active region includes: forming a first mask layer on the isolation region and a first portion of the active region, wherein the first mask layer has a first opening to expose a second portion of the active region; and etching the second portion of the active region through the first opening so that the first word line trench is formed in the active region.
[0008] In some embodiments, forming a second word line trench in the substrate includes: forming a second mask layer over a first portion of the isolation region and a third portion of the active region, the second mask layer having a second opening to expose a fourth portion of the active region, and the second mask layer having a third opening to expose a second portion of the isolation region; and etching the fourth portion of the active region through the second opening, and etching the second portion of the isolation region through the third opening, so that a second word line trench is formed in the active region and the isolation region.
[0009] In some embodiments, the first width of the second opening is equal to the second width of the third opening.
[0010] In some embodiments, forming an active region in the substrate includes forming a source / drain region in the active region, and the source / drain region has a third depth.
[0011] In some embodiments, the first depth is greater than the third depth.
[0012] In some embodiments, the second depth is greater than the third depth.
[0013] In some embodiments, forming a word line structure in the second word line groove includes: forming a liner dielectric layer on an inner surface of the second word line groove, and the liner dielectric layer includes a bottom portion and a side portion; forming a conductive layer in the second word line groove, and the conductive layer contacts the bottom portion and the side portion; and forming a covering layer in the second word line groove, and the covering layer is stacked on the conductive layer.
[0014] In some embodiments, the pad dielectric layer includes a bottom pad dielectric layer and a side pad dielectric layer; and the bottom of the word line structure includes a portion of the first dielectric layer and the bottom pad dielectric layer.
[0015] In some embodiments, the dielectric material of the pad dielectric layer is an oxide or a high-k dielectric constant material.
[0016] In some embodiments, the dielectric material of the first dielectric layer is an oxide.
[0017] In some embodiments, depositing the first dielectric layer is by an atomic layer deposition process.
[0018] Some embodiments of the present invention provide a semiconductor structure including a substrate and a word line structure. The substrate includes an isolation region and an active region. The word line structure is linear and extends through the isolation region and the active region, and the word line structure includes a conductive layer and a dielectric layer. The dielectric layer includes a bottom portion and a side portion, and the bottom portion contacts the bottom of the conductive layer, and the side portion contacts the side of the conductive layer, and the bottom portion of the dielectric layer has a thickness greater than the thickness of the side portion of the dielectric layer.
[0019] In some embodiments, the word line structure further includes a cover layer disposed on the conductive layer.
[0020] In some embodiments, the bottom portion of the dielectric layer includes a bottom dielectric layer and a bottom liner dielectric layer, and has an interface between the bottom dielectric layer and the bottom liner dielectric layer.
[0021] In some embodiments, the active region includes a source / drain region, and the source / drain region is disposed on two sides of the conductive layer.
[0022] In some embodiments, the depth of the word line structure is a first depth, the depth of the bottom pad dielectric layer of the word line structure is a second depth, and the depth of the source / drain region is a third depth.
[0023] In some embodiments, the first depth is greater than the second depth, and the second depth is greater than the third depth.
[0024] According to the method for manufacturing a semiconductor structure provided by an embodiment of the present invention, before forming a word line structure, a first word line groove is formed in the active region, and the depth of the first word line groove is greater than the depth of the word line structure. Therefore, in the etching process of forming the word line structure, only the etching rate of the dielectric material needs to be considered. In addition, the etching depth of the word line structure can be better controlled and consistent. Therefore, the semiconductor structure provided by an embodiment of the present invention can reduce leakage problems and has better performance.
[0025] It is to be understood that both the foregoing general description and the following detailed description are examples, and are intended to provide further explanation of the disclosure as claimed. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] The following embodiments are read in conjunction with the accompanying drawings to clearly understand the concept of the present invention. It should be noted that, in accordance with standard practice in the industry, various features are not drawn to scale. In fact, the size of various features may be arbitrarily enlarged or reduced for the sake of clarity of discussion.
[0027] Figures 1 to 3 is a diagram of a method of manufacturing a semiconductor structure during formation of isolation regions and active regions according to some embodiments of the present invention;
[0028] Figures 4 to 7 is a diagram of a method of manufacturing a semiconductor structure during formation of a first word line trench according to some embodiments of the present invention;
[0029] Figures 8 to 10 is a diagram of a method of manufacturing a semiconductor structure during formation of a second word line trench according to some embodiments of the present invention;
[0030] Figures 11 to 14is a diagram of a method of manufacturing a semiconductor structure during formation of a word line structure according to some embodiments of the present invention; and
[0031] Fig.15 is a cross-sectional view of a semiconductor structure according to some embodiments of the present invention. DETAILED DESCRIPTION
[0032] Reference will now be made in detail to embodiments of the present invention, examples of which are illustrated in the accompanying drawings. Wherever possible, the same reference numerals are used in the drawings and the description to refer to the same or like parts.
[0033] In addition, for ease of description, spatially relative terms such as "on", "above", "below", "between", etc. may be used in the present invention to describe the relationship of one element or feature to another element as shown in the drawings) or function. In addition to the orientation depicted in the drawings, spatially relative terms are intended to encompass different orientations of the device in use or operation. The device may be otherwise oriented (rotated 90 degrees or in other orientations), and the spatially relative descriptors used in the present invention should be interpreted accordingly.
[0034] The terms "including", "having", "comprising" and the like used in the present invention are open terms, meaning including but not limited to.
[0035] In the related art of the process of etching word line trenches, the word line usually extends through two materials of the substrate, such as silicon in the active region and a dielectric material (e.g., oxide) in the isolation region, and the two materials have different etching rates in the substrate. Therefore, after the process of etching the word line trenches, the depth of the word line trench in the isolation region is different from the depth of the word line trench in the active region, thereby causing electrical problems.
[0036] According to various embodiments of the present invention, after the active region and the isolation region are formed in the substrate, a portion of the active region can be etched through a mask layer having an opening. Then, the dielectric material is refilled above the substrate. Therefore, in the process of the word line structure of the semiconductor structure, only the dielectric material needs to be etched. In this way, in the process of the semiconductor structure, it is easier to control the depth of the word line structure. In addition, a semiconductor structure with better performance can also be obtained in the process of the semiconductor structure.
[0037] It should be noted that when the following drawings (such as Figures 1 to 14) is described and illustrated as a series of operations or steps, the order in which these operations or steps are described should not be limited. For example, some operations or steps may be performed in a different order than in the present invention, or some operations or steps may occur simultaneously, or some operations may not be performed, and / or some operations or steps may be repeated. In addition, the actual operations or steps of the process stage may need to be performed before the semiconductor structure (e.g., Fig.14 Additional operations or steps are performed before, during, or after the semiconductor structure 100 in the embodiment to complete the semiconductor structure 100. Therefore, the present invention may briefly describe some of these additional operations or steps. In addition, unless otherwise specified, for the following figures (e.g. Figures 1 to 14 )The same explanations discussed above can be directly applied to the other figures.
[0038] See also Figures 1 to 3 , Figures 1 to 3 is a diagram of a method of manufacturing a semiconductor structure 100 during formation of an isolation region 104 and an active region 106 according to some embodiments of the present invention, wherein Figure 1 is a top view of a semiconductor structure 100 having an isolation region 104 and an active region 106 according to some embodiments of the present invention, Figure 2 , Figure 3 According to some embodiments of the present invention, Figure 1 FIG. 1 is a cross-sectional view taken along line NN′ of FIG. 1 , which is a cross-sectional view of one of the process stages of forming the isolation region 104 and the active region 106 .
[0039] like Figure 1 and Figure 2 As shown, an isolation region 104 and an active region 106 are formed in a substrate 102. The substrate 102 is a semiconductor material and may include silicon, such as silicon crystal, polycrystalline silicon, or amorphous silicon. In some embodiments, the substrate 102 may include an elemental semiconductor, such as germanium (Ge). In some embodiments, the substrate 102 may include an alloy semiconductor, such as silicon germanium (SiGe), silicon carbide phosphide (SiPC), gallium arsenide phosphide (GaAsP), aluminum indium arsenide (AlInAs), aluminum gallium arsenide (AlGaAs), gallium indium arsenide (GaInAs), gallium indium phosphide (GaInP), gallium indium phosphide (GaInAsP), or other suitable materials. In some embodiments, the substrate 102 may include a compound semiconductor, such as silicon carbide (SiC), silicon phosphide (SiP), gallium arsenide (GaAs), gallium phosphide (GaP), indium phosphide (InP), indium arsenide (InAs), indium antimonide (InSb), zinc oxide (ZnO), zinc selenide (ZnSe), zinc sulfide (ZnS), zinc telluride (ZnTe), cadmium selenide (CdSe), cadmium sulfide (CdS), cadmium telluride (CdTe), or other suitable materials.
[0040] The isolation regions 104 are formed in the substrate 102. The material of the isolation regions 104 includes an oxide, such as silicon oxide. In some embodiments, each isolation region 104 can be formed by a shallow trench isolation (STI) process. After the isolation regions 104 are formed, the semiconductor material located around each isolation region 104 and extending from the substrate 102 can be used as active regions 106 respectively. In addition, each active region 106 is adjacent to each isolation region 104, and each isolation region 104 separates adjacent active regions 106.
[0041] Then, if Figure 3 As shown, a source / drain (S / D) region 108 is formed in an active region 106 of a substrate 102. An ion implantation process may be performed on the substrate 102 to dope N-type or P-type dopants into the active region 106 of the substrate 102. In some embodiments, the N-type dopant may include phosphorus or arsenic, and the P-type dopant may include boron or boron fluoride.
[0042] Next, see Figures 4 to 7 , Figures 4 to 7 is a diagram of a method of manufacturing a semiconductor structure 100 before forming a first word line trench 120 according to some embodiments of the present invention, wherein Figure 4 is a top view of a semiconductor structure 100 for forming a first word line trench 120 according to some embodiments of the present invention. Figures 5 to 7 According to some embodiments of the present invention, Figure 4 The cross-sectional view taken along section line NN′ of FIG. 1 is a cross-sectional view of one of the process stages for forming the first word line trench 120 of the semiconductor structure 100 .
[0043] like Figure 4 As shown in FIG. 1 , a first mask layer 110 is formed on the surface of the isolation region 104 and the first portion 106a of the active region 106. In the top view, a layout is formed on the surface of the isolation region 104 and the active region 106 through the first mask layer 110, and a word line pattern 112 (as shown by the dotted line) extending through the isolation region 104 and the active region 106 can be obtained through the layout. Figure 5 As shown, the first mask layer 110 is formed on the surface of the isolation region 104 and the first portion 106a of the active region 106, and the first mask layer 110 has a first opening OP1 exposing the second portion 106b of the active region 106, that is, the second portion 106b of the active region 106 is not covered by the first mask layer 110. It should be noted that Figure 5Four first openings OP1 are shown, but the number of the first openings OP1 is not limited thereto. In addition, only the first openings OP1 of the first mask layer 110 expose the active region 106, while the first openings OP1 of the first mask layer 110 do not expose the isolation region 104. In some embodiments, the first mask layer 110 is a hard mask layer.
[0044] Then, if Figure 6 As shown, a first word line trench 120 is formed in the active region 106 corresponding to the first opening OP1. The first word line trench 120 is linear and extends through the active region 106 based on the word line pattern 112. Further, the first word line trench 120 is formed by etching the active region 106 corresponding to the first opening OP1 using a suitable etching process, such as a dry etching process or a wet etching process. In addition, although Figure 6 Four first word line trenches 120 are shown, but the number of first word line trenches 120 is not limited thereto. In addition, each first word line trench 120 has a first depth D1, and the first depth D1 of the first word line trench 120 is greater than the third depth D3 of each S / D region 108. In some embodiments, the first depth D1 is 270 nanometers (nm).
[0045] Then, if Figure 7 As shown, a first dielectric layer 122 is deposited in the first word line trench 120 and on the active region 106 and the isolation region 104. Similarly, the first dielectric layer 122 is deposited on the active region 106 so that the first dielectric layer 122 has a height H from the active region 106, and the height H is equal to the second depth D2 (at Fig.10 ), which will be described later. In some embodiments, the first dielectric layer 122 is formed of any suitable dielectric material. In some embodiments, the dielectric material may include an oxide, such as silicon oxide. In some embodiments, the first dielectric layer 122 is formed by an atomic layer deposition (ALD) process, other suitable techniques, or a combination thereof.
[0046] For further information, see Figures 8 to 10 , Figures 8 to 10 is a diagram of a method of manufacturing a semiconductor structure 100 during formation of a second word line trench 130 according to some embodiments of the present invention, wherein Figure 8 is a top view of the semiconductor structure 100 in which the second word line trench 130 is formed according to some embodiments of the present invention. Figures 9 and 10 According to some embodiments of the present invention, Figure 8FIG. 1 is a cross-sectional view taken along line NN′ of FIG. 1 during one of the process stages of forming the second word line trench 130 during manufacturing the semiconductor structure 100 .
[0047] like Figure 8 As shown, according to the word line pattern 112, a second mask layer 124 is formed on a portion of the surface of the first dielectric layer 122. Fig. 9 As shown, the second mask layer 124 is formed above the first portion 104a of the isolation region 104 and the third portion 106c of the active region 106. The second mask layer 124 has a second opening OP2 exposing the fourth portion 106d of the active region 106, and the second mask layer 124 has a third opening OP3 exposing the second portion 104b of the isolation region 104. In addition, the position of each second opening OP2 is set above each first word line trench 120. It is worth mentioning that the width W1 of each second opening OP2 is equal to the width W1 of each third opening OP3. In addition, although Fig. 9 Four second openings OP2 and one third opening OP3 are shown, but the number of the second openings OP2 and the third openings OP3 is not limited thereto.
[0048] Then, if Fig.10 As shown, second word line trenches 130 are formed in the substrate 102 corresponding to the second opening OP2 and the third opening OP3. In addition, each second word line trench 130 is linear and extends through the isolation region 104 and the active region 106. Further, the second word line trenches 130 are formed by etching the active region 106 using a suitable etching process, such as a dry etching process or a wet etching process.
[0049] In addition, when etching the first dielectric layer 122 (eg Fig. 9After etching, a portion of the first dielectric layer 122 will be retained at the bottom of the second word line trench 130, namely the bottom dielectric layer 122r. After etching, each second word line trench 130 has a second depth D2. In some embodiments, the second depth D2 is 145nm. The second depth D2 is greater than the third depth D3 of each S / D region 108. Adjacent S / D regions 108 are disposed on opposite sides of each second word line trench 130. In some embodiments, the first depth D1 of each first word line trench 120 is greater than the second depth D2 of each second word line trench 130. In some embodiments, the second depth D2 of each second word line trench 130 is related to the height H of the aforementioned deposition, and in some embodiments, the second depth D2 of each second word line trench 130 is equal to the height H of the aforementioned deposition. In addition, in this step, since the same dielectric material (e.g., oxide) is etched in the active region 106 and the isolation region 104, the etching depth of each second word line trench 130 in the isolation region 104 and the active region 106 is easier to control. In addition, the etching depth of each second word line trench 130 in the isolation region 104 and the active region 106 is the same.
[0050] For further information, see Fig.11 , Fig.11 FIG. 1 is a top view of a semiconductor structure 100 having word line structures 138 according to some embodiments of the present invention. The word line structures 138 are formed in the isolation region 104 and the active region 106. Each word line structure 138 is linear and extends through the isolation region 104 and the active region 106. Details of forming the word line structures 138 are described as follows.
[0051] Please refer to Figure 12 to Figure 14 , Figure 12 to Figure 14 According to some embodiments of the present invention, Fig.111 is a cross-sectional view of one of the process stages of forming a word line structure 138 during the manufacture of the semiconductor structure 100 along the NN' section line. A liner dielectric layer 132 is formed on the inner surface 130S of each second word line trench 130, and the liner dielectric layer 132 includes a bottom portion and a side portion. In some embodiments, the liner dielectric layer 132 can conformally cover the inner surface 130S of each second word line trench 130. The liner dielectric layer 132 is formed of any suitable dielectric material, and the dielectric material may include silicon oxide or a high dielectric constant material. In some embodiments, the high dielectric constant material is hafnium oxide (HfO2), zirconium oxide (ZrO2), tantalum pentoxide (Ta2O5) or a combination thereof. The method of forming the liner dielectric layer 132 on the inner surface 130S of each second word line trench 130 may include using a chemical vapor deposition (CVD) process, an ALD process, an oxygen plasma oxidation process, a thermal oxidation process, other suitable techniques or a combination thereof. The liner dielectric layer 132 includes a bottom liner dielectric layer 132a and a side liner dielectric layer 132b. It is worth mentioning that the bottom of the word line structure 138 has a bottom dielectric layer 122r and a bottom liner dielectric layer 132a, while the side of the word line structure 138 only has a side liner dielectric layer 132b. Therefore, the thickness of the dielectric material at the bottom of the word line structure 138 is greater than the thickness of the dielectric material on the side of the word line structure 138.
[0052] Then, if Fig.13 As shown, a conductive layer 134 is formed in each second word line trench 130, and the conductive layer 134 contacts the bottom portion of the pad dielectric layer 132 and the side portion of the pad dielectric layer 132. The conductive layer 134 is located at least partially overlapping each S / D region 108, that is, the S / D region 108 is disposed on opposite sides of the conductive layer 134. In some embodiments, the conductive layer 134 is formed of any suitable conductive material, such as a semiconductor, a metal, a metal nitride, a metal silicide, other suitable conductive materials or combinations thereof. For example, the conductive layer 134 may include doped polysilicon, titanium (Ti), tungsten (W), tantalum (Ta), titanium nitride (TiN), tungsten nitride (WN), tantalum nitride (TaN), titanium silicon nitride (TiSiN), tantalum silicon nitride (TaSiN), tungsten silicon nitride (WSiN), other suitable conductive materials or combinations thereof.
[0053] In addition, if Fig.14As shown, a capping layer 136 is formed in each second word line trench 130, and the capping layer 136 is stacked on the conductive layer 134. In some embodiments, the material of the capping layer 136 may include silicon oxide, silicon nitride, silicon oxynitride, or a combination thereof. Fig.14 After the steps of , the semiconductor structure 100 having the word line structure 138 is completed. In addition, each word line structure 138 in the isolation region 104 and each word line structure 138 in the active region 106 are the same. For example, the depth of each word line structure 138 in the isolation region 104 is equal to the depth of each word line structure 138 in the active region 106, that is, the depth of each word line structure 138 in the isolation region 104 and the active region 106 is the first depth D1 of the first word line trench 120.
[0054] According to the method for manufacturing the semiconductor structure 100 provided by the embodiment of the present invention, since the first opening OP1 of the first mask layer 110 is formed only above the active region 106, the first word line trench 120 is also formed only in the active region 106. Then, the dielectric material is refilled in each first word line trench 120 and above the substrate 102. Then, through the second opening OP2 and the third opening OP3 of the second mask layer 124, the second word line trench 130 is formed in the active region 106 and the isolation region 104 respectively, and the position of the active region 106 exposed by the first opening OP1 and the second opening OP2 is the same. In addition, since the first depth D1 of each first word line trench 120 is greater than the second depth D2 of each second word line trench 130, when forming the second word line trench 130, only the dielectric material needs to be etched. Therefore, without considering the different etching rates of the silicon (active region 106) and the dielectric material (isolation region 104) in the substrate 102, the depth of the word line structure 138 in the active region 106 and the depth of the word line structure 138 in the isolation region 104 are easier to control, thereby obtaining a semiconductor structure 100 with better performance.
[0055] In addition, the semiconductor structure 100 having the word line structure 138 has some technical features as described below. Fig.15 , Fig.15 is a schematic diagram of a semiconductor structure 100 according to some embodiments of the present invention.
[0056] like Fig.15 As shown, an embodiment of the present invention provides a semiconductor structure 100. The semiconductor structure 100 includes a substrate 102 and a word line structure 138. The substrate 102 includes an isolation region 104 and an active region 106. The word line structure 138 is linear and extends the isolation region 104 and the active region 106. In addition, each active region 106 includes adjacent S / D regions 108, and the S / D regions 108 are disposed on opposite sides of the word line structure 138.
[0057] The word line structure 138 includes a dielectric layer 133, a conductive layer 134, and a cover layer 136. The dielectric layer 133 includes a bottom portion and a side portion. The bottom portion of the dielectric layer 133 contacts the bottom of the conductive layer 134, and the side portion of the dielectric layer 133 contacts the side wall of the conductive layer 134. In addition, the dielectric layer 133 includes a bottom dielectric layer 122r and a pad dielectric layer 132, and the pad dielectric layer 132 includes a bottom pad dielectric layer 132a and a side pad dielectric layer 132b. The bottom of the dielectric layer 133 includes a bottom dielectric layer 122r and a bottom pad dielectric layer 132a, and an interface IF is provided between the bottom dielectric layer 122r and the bottom pad dielectric layer 132a. The cover layer 136 is disposed on the conductive layer 134.
[0058] Furthermore, if Fig.15 As shown, the depth of the word line structure 138 is a first depth D1, the depth of the bottom liner dielectric layer 132a is a second depth D2, and the depth of the S / D region is a third depth D3. The first depth D1 is greater than the second depth D2, and the second depth D2 is greater than the third depth D3. In addition, the position of the conductive layer 134 of the word line structure 138 at least partially overlaps with the S / D region 108, that is, the adjacent S / D regions 108 are arranged on opposite sides of the conductive layer 134.
[0059] like Fig.15 As shown, the bottom thickness T of the word line structure 138 is the first thickness T1 of the bottom dielectric layer 122r plus the second thickness T2 of the bottom pad dielectric layer 132a. Therefore, compared with the side of the dielectric layer 133, the bottom of the dielectric layer 133 is thicker, that is, the bottom thickness T of the word line structure 138 is greater than the third thickness T3 of the word line structure 138. In addition, the width W2 of the word line structure 138 in each active region 106 is equal to the width W2 of the word line structure 138 in each isolation region 104.
[0060] According to the embodiment of the present invention, the word line structure 138 disposed in the active region 106 and the word line structure 138 disposed in the isolation region 104 are the same. For example, the depth of each word line structure 138 in the active region 106 is the same as the depth of each word line structure 138 in the isolation region 104. Therefore, the semiconductor structure 100 provided by the embodiment of the present invention can solve the problem of power loss caused by the different depths of the word line structures in the active region and the isolation region. In addition, the semiconductor structure 100 provided by the embodiment of the present invention can also reduce the problem of leakage.
[0061] Although some embodiments of the present invention have been described in considerable detail, other embodiments are possible. Therefore, the spirit and scope of the claims should not be limited to the embodiments described herein.
[0062] The above briefly describes the features of multiple embodiments of the present invention, so that those skilled in the art can more easily understand the present invention. Any person skilled in the art should understand that the present invention can easily serve as a basis for the change or design of other structures or processes to achieve the same purpose and / or obtain the same advantages as the embodiments of the present invention. Any person skilled in the art can also understand that the structures equivalent to the above do not depart from the spirit and scope of protection of the present invention, and can be changed, replaced and modified without departing from the spirit and scope of the present invention.
[0063]
Explanation of symbols
[0064] 100:Semiconductor structure
[0065] 102:Substrate
[0066] 104: Quarantine
[0067] 104a,106a:Part I
[0068] 104b,106b:Part 2
[0069] 106: Active Zone
[0070] 106c: Part 3
[0071] 106d: Part 4
[0072] 108: Source / Drain Region / S / D Region
[0073] 110: First mask layer
[0074] 112: Character line pattern
[0075] 120: first word line groove
[0076] 122: first dielectric layer
[0077] 122r: bottom dielectric layer
[0078] 124: Second mask layer
[0079] 130: Second word line groove
[0080] 130S: Inner surface
[0081] 132: liner dielectric layer
[0082] 132a: bottom liner dielectric layer
[0083] 132b: Side liner dielectric layer
[0084] 133: Dielectric layer
[0085] 134: Conductive layer
[0086] 136: Covering layer
[0087] 138: Character Line Structure
[0088] D1: First Depth
[0089] D2: Second Depth
[0090] D3: Third Depth
[0091] H: Height
[0092] NN': hatch line
[0093] T: Bottom thickness
[0094] T1: First thickness
[0095] T2: Second thickness
[0096] T3: The third thickness
[0097] OP1: First opening
[0098] OP2: Second opening
[0099] OP3: The third opening
[0100] IF: Interface
[0101] W1,W2: width.
Claims
1. A method for manufacturing a semiconductor structure, characterized in that: include: forming an isolation region and an active region in a substrate, wherein the active region is adjacent to the isolation region; forming a first word line trench in the active region; forming a first dielectric layer in the first word line trench and on the isolation region and the active region; Etching the first dielectric layer to form a second word line trench in the active region and the isolation region, wherein the second word line trench is linear and extends through the isolation region and the active region, and a portion of the first dielectric layer remains at a bottom of the second word line trench; and A word line structure is formed in the second word line trench.
2. The method according to claim 1, characterized in that The first word line trench has a first depth, and the second word line trench has a second depth; and The first depth is greater than the second depth.
3. The method according to claim 2, characterized in that The first dielectric layer is deposited so that the first dielectric layer is higher than the active region, and the height is equal to the second depth of the second word line trench.
4. The method according to claim 1, characterized in that: Forming the first word line trench in the active region includes: forming a first mask layer on the isolation region and the first portion of the active region, wherein the first mask layer has a first opening to expose the second portion of the active region; and The second portion of the active region is etched through the first opening so that the first word line trench is formed in the active region.
5. The method according to claim 1, characterized in that Forming the second word line trench in the substrate includes: forming a second mask layer over the first portion of the isolation region and the third portion of the active region, wherein the second mask layer has a second opening to expose the fourth portion of the active region, and the second mask layer has a third opening to expose the second portion of the isolation region; and The fourth portion of the active region is etched through the second opening, and the second portion of the isolation region is etched through the third opening, so that the second word line trench is formed in the active region and the isolation region.
6. The method according to claim 5, characterized in that The first width of the second opening is equal to the second width of the third opening.
7. The method according to claim 2, characterized in that Forming the active region in the substrate includes: A source / drain region is formed in the active region, wherein the source / drain region has a third depth.
8. The method according to claim 7, characterized in that The first depth is greater than the third depth.
9. The method according to claim 7, characterized in that: The second depth is greater than the third depth.
10. The method according to claim 1, characterized in that Forming the word line structure in the second word line trench comprises: forming a liner dielectric layer on the inner surface of the second word line trench, wherein the liner dielectric layer comprises a bottom portion and a side portion; forming a conductive layer in the second word line trench, wherein the conductive layer contacts the bottom portion and the side portion; and A covering layer is formed in the second word line trench, and the covering layer is stacked on the conductive layer.
11. The method according to claim 10, characterized in that The liner dielectric layer includes a bottom liner dielectric layer and a side liner dielectric layer; and The bottom of the word line structure includes the portion of the first dielectric layer and the bottom liner dielectric layer.
12. The method according to claim 10, characterized in that The dielectric material of the liner dielectric layer is oxide or a high dielectric constant material.
13. The method according to claim 1, characterized in that The dielectric material of the first dielectric layer is oxide.
14. The method according to claim 1, characterized in that The first dielectric layer is deposited by an atomic layer deposition process.
15. A semiconductor structure, characterized in that: include: a substrate, including an isolation region and an active region; as well as A word line structure is linear and extends through the isolation region and the active region, wherein the word line structure comprises: Conductive layer; as well as The dielectric layer comprises a bottom portion and a side portion, wherein the bottom portion contacts the bottom of the conductive layer, and the side portion contacts the side of the conductive layer, wherein the thickness of the bottom portion of the dielectric layer is greater than the thickness of the side portion of the dielectric layer.
16. The semiconductor structure according to claim 15, characterized in that The word line structure further comprises: The covering layer is arranged on the conductive layer.
17. The semiconductor structure according to claim 15, characterized in that The bottom portion of the dielectric layer includes a bottom dielectric layer and a bottom liner dielectric layer, and has an interface between the bottom dielectric layer and the bottom liner dielectric layer.
18. The semiconductor structure according to claim 17, characterized in that: The active region includes a source / drain region, and the source / drain region is disposed on two sides of the conductive layer.
19. The semiconductor structure according to claim 18, characterized in that The depth of the word line structure is a first depth, the depth of the bottom pad dielectric layer of the word line structure is a second depth, and the depth of the source / drain region is a third depth.
20. The semiconductor structure according to claim 19, characterized in that The first depth is greater than the second depth, and the second depth is greater than the third depth.