Display module and preparation method and application thereof

By setting a touch function layer on the back of the polarizer and combining it with the organic light emitting diode display module, the problems of complex preparation process and poor anti-interference ability in the prior art are solved, and higher preparation yield and anti-interference ability are achieved. Reduced production costs.

CN118900599AInactive Publication Date: 2024-11-05SUZHOU QUINGYUE OPTOELECTRONICS TECH CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410984414.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-22
Publication Date
2024-11-05
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The existing PMOLED on-cell solution has complex preparation process, poor anti-interference ability, low production yield, high production cost, and close touch layer to interference source, resulting in poor screen touch effect.

Method used

It is provided on the back of the polarizer, including a first insulating layer, a nano-silver wire layer and a second insulating layer stacked in turn. It is combined with the organic light emitting diode display module through simple process steps to enhance anti-interference ability .

Benefits of technology

The preparation process is simplified, production costs are reduced, preparation yield is improved, and the anti-interference ability and touch effect of the display module are significantly enhanced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118900599A_ABST
    Figure CN118900599A_ABST
Patent Text Reader

Abstract

According to the display module and the preparation method and application thereof, by means of the preparation method of the display module, preparation of the touch control integrated display module can be achieved, a touch control function layer is manufactured on a conventional polaroid through a simple process, and therefore the touch control function layer can be manufactured on the conventional polaroid. Due to the fact that the polaroid is cheaper than an organic light-emitting diode display module, even if unqualified products are produced, the loss is small, the production cost of the products is reduced, the preparation technology is simplified, and in addition, the anti-interference capacity of the prepared display module is higher.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the field of display technology, and in particular relates to a display module and a preparation method and application thereof. Background Art

[0002] With the continuous development of science and technology, touch display devices are moving towards the direction of being thinner and lighter. Traditional touch display solutions are relatively thick. In order to reduce the thickness of touch display devices, touch display devices use an integrated design of touch panel and liquid crystal panel, that is, display touch integration. However, the existing PMOLED on-cell solution has a complex preparation process, poor anti-interference ability, and low preparation yield. If a defect occurs, the entire screen will be scrapped, the material loss is large, and the production cost is too high.

[0003] CN108666357A discloses a display panel, a manufacturing method thereof and a display device, wherein the display panel comprises: a substrate, an organic light emitting diode device formed on the substrate, a touch electrode layer formed on the organic light emitting diode device, a circular polarizing layer formed on the touch electrode layer, and a protective layer formed on the circular polarizing layer; CN107870697A discloses an OLED touch display panel, comprising: an array substrate; an organic light emitting layer disposed on the array substrate; a cathode metal layer disposed on the organic light emitting layer; wherein the cathode metal layer is patterned to form first touch signal lines disposed in parallel and spaced apart; an encapsulation layer disposed on the cathode metal layer; and a circular polarizer disposed on the encapsulation layer.

[0004] In the preparation method disclosed in the above patent, the touch electrode layer in the display panel is directly formed on the organic light-emitting diode device, which reduces the product preparation yield, complicates the preparation process, causes large interference to the display's own signal, and the touch layer is close to the interference source, resulting in poor anti-interference ability, poor screen touch effect, and high production cost. Therefore, it is urgent to design a better method to prepare a display module with touch function. Summary of the invention

[0005] In view of the deficiencies in the prior art, the purpose of the present invention is to provide a display module and a preparation method and application thereof. Through the design of raw materials and process steps, the process steps can be simplified, the preparation yield of the product can be improved, the production cost is low, and the obtained display module has a touch function and strong anti-interference ability.

[0006] To achieve this object, the present invention adopts the following technical solutions:

[0007] In a first aspect, the present invention provides a method for preparing a display module, the method comprising:

[0008] A touch function layer is arranged on the back of the polarizer, and the touch function layer includes a first insulating layer, a nano silver wire layer and a second insulating layer which are sequentially stacked; the first insulating layer is bonded to the back of the polarizer; a silver paste layer is arranged on the pins of the nano silver wires at the binding position of the nano silver wire layer; functional patterns and wiring are etched on the nano silver wire layer through the second insulating layer; one side of the optical glue is bonded to the surface of the second insulating layer away from the nano silver wire layer; a flexible circuit board of the touch function layer is bonded to the silver paste layer; the other side of the optical glue is bonded to an organic light emitting diode display module; the flexible circuit board of the touch function layer is welded to the flexible circuit board of the organic light emitting diode display module to obtain the display module.

[0009] The preparation method provided by the present invention uses a relatively simple process to produce a touch function layer on a conventional polarizer. Since the polarizer is cheaper than the organic light emitting diode display module, even if unqualified products are produced, the loss is small, thereby reducing the production cost of the product. In addition, the prepared display module has a stronger anti-interference ability.

[0010] More specifically, the preparation method provided by the present invention can be used to prepare a touch-integrated PMOLED (passive matrix organic light-emitting diode) display module.

[0011] The organic light emitting diode display module (OLED module) can be purchased, for example, from Suzhou Qingyue Optoelectronics Technology Co., Ltd.

[0012] In the present invention, the back side of the polarizer refers to the surface of the lower layer TAC (triacetate film) of the polarizer original plate.

[0013] The following are preferred technical solutions of the present invention, but are not intended to limit the technical solutions provided by the present invention. Through the following preferred technical solutions, the objectives and beneficial effects of the present invention can be better achieved and realized.

[0014] As a preferred technical solution, the thickness of the first insulating layer is 1-3μm, for example, it can be 1μm, 1.2μm, 1.4μm, 1.6μm, 1.8μm, 2μm, 2.2μm, 2.4μm, 2.6μm, 2.8μm or 3μm, as well as specific point values ​​between the above point values. Due to limited space and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values ​​included in the said range.

[0015] Preferably, the uniformity of the first insulating layer is ≤5%, for example, it may be 0.5%, 1%, 1.5%, 2%, 2.5%, 3%, 3.5%, 4% or 4.5%.

[0016] The uniformity refers to the uniformity of the film thickness, which is measured using an ellipsometer (manufacturer: HORIBA; model SMART SE). The larger the value, the worse the uniformity of the film thickness, and the smaller the value, the better the uniformity of the film thickness.

[0017] Preferably, the first insulating layer is provided by the following method, the method comprising: coating a first insulating oil on the back surface of the polarizer, and then sequentially performing a first baking and a first curing to form the first insulating layer.

[0018] Preferably, the first baking time is 100-500s, for example, it can be 100s, 120s, 150s, 180s, 200s, 220s, 250s, 300s, 350s, 400s, 450s or 500s, as well as specific point values ​​between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values ​​included in the range.

[0019] Preferably, the temperature of the first baking is 60-80°C, for example, it can be 60°C, 62°C, 64°C, 66°C, 68°C, 70°C, 72°C, 74°C, 76°C, 78°C or 80°C, as well as specific point values ​​between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values ​​included in the range.

[0020] Preferably, the first curing time is 15-45s, for example, it can be 15s, 18s, 20s, 25s, 28s, 30s, 32s, 35s, 38s, 40s, 42s or 45s, as well as specific point values ​​between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values ​​included in the range.

[0021] Preferably, the first curing temperature is 30-50°C, for example, it can be 30°C, 32°C, 34°C, 36°C, 38°C, 40°C, 42°C, 44°C, 46°C, 48°C or 50°C, as well as specific point values ​​between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values ​​included in the range.

[0022] Preferably, the nano silver wire layer is provided by the following method, the method comprising: coating the nano silver wires on the surface of the first insulating layer away from the back surface of the polarizer, and then performing a second baking to form the nano silver wire layer.

[0023] Preferably, the method of coating the silver nanowires comprises slit coating.

[0024] Preferably, the second baking time is 100-500s, for example, it can be 100s, 120s, 150s, 180s, 200s, 220s, 250s, 300s, 350s, 400s, 450s or 500s, as well as specific point values ​​between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values ​​included in the range.

[0025] Preferably, the temperature of the second baking is 60-80°C, for example, it can be 60°C, 62°C, 64°C, 66°C, 68°C, 70°C, 72°C, 74°C, 76°C, 78°C or 80°C, as well as specific point values ​​between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values ​​included in the range.

[0026] Preferably, the square resistance of the nano silver wire is 20-40Ω, for example, it can be 20Ω, 22Ω, 24Ω, 26Ω, 28Ω, 30Ω, 32Ω, 34Ω, 36Ω, 38Ω or 40Ω, as well as specific point values ​​between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values ​​included in the range; using nano silver wires with lower square resistance can increase anti-interference ability.

[0027] Preferably, the thickness of the nano silver wire layer is 50-4000 nm, for example, it can be 50 nm, 100 nm, 200 nm, 500 nm, 800 nm, 1000 nm, 1500 nm, 2000 nm, 2500 nm, 3000 nm, 3500 nm or 4000 nm, as well as specific values ​​between the above points. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific points included in the range.

[0028] Preferably, the thickness of the second insulating layer is ≤1 μm, for example, may be 0.1 μm, 0.2 μm, 0.3 μm, 0.4 μm, 0.5 μm, 0.6 μm, 0.7 μm, 0.8 μm or 0.9 μm.

[0029] Preferably, the uniformity of the second insulating layer is ≤5%, for example, it may be 0.5%, 1%, 1.5%, 2%, 2.5%, 3%, 3.5%, 4% or 4.5%.

[0030] Preferably, the second insulating layer is provided by the following method, the method comprising: coating a second insulating oil on a surface of the nano silver wire layer away from the first insulating layer, and then sequentially performing a third baking and a second curing to form the second insulating layer.

[0031] Preferably, the materials of the first insulating oil and the second insulating oil each independently include acrylic resin.

[0032] Preferably, the third baking time is 100-300s, for example, it can be 100s, 120s, 140s, 160s, 180s, 200s, 220s, 240s, 250s, 260s, 280s or 300s, as well as specific point values ​​between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values ​​included in the range.

[0033] Preferably, the temperature of the third baking is 60-80°C, for example, it can be 60°C, 62°C, 64°C, 66°C, 68°C, 70°C, 72°C, 74°C, 76°C, 78°C or 80°C, as well as specific point values ​​between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values ​​included in the range.

[0034] Preferably, the second curing time is 10-35s, for example, it can be 10s, 15s, 18s, 20s, 22s, 25s, 28s, 30s, 32s or 35s, as well as specific point values ​​between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values ​​included in the range.

[0035] Preferably, the temperature of the second curing is 30-50°C, for example, it can be 30°C, 32°C, 34°C, 36°C, 38°C, 40°C, 42°C, 44°C, 46°C, 48°C or 50°C, as well as specific point values ​​between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values ​​included in the range.

[0036] Preferably, the first curing and the second curing methods include curing using ultraviolet light.

[0037] Preferably, the thickness of the silver paste layer is 5-15 μm, for example, it can be 5 μm, 6 μm, 7 μm, 8 μm, 9 μm, 10 μm, 11 μm, 12 μm, 13 μm, 14 μm or 15 μm, as well as specific point values ​​between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values ​​included in the range.

[0038] Preferably, the silver paste layer is provided by the following method, the method comprising: printing silver paste on the pins of the nano-silver wires at the binding positions of the nano-silver wire layer, and performing a third curing to form the silver paste layer.

[0039] Preferably, the temperature of the third curing is 60-80°C, for example, it can be 60°C, 62°C, 64°C, 66°C, 68°C, 70°C, 72°C, 74°C, 76°C, 78°C or 80°C, as well as specific point values ​​between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values ​​included in the range.

[0040] Preferably, the third curing time is 2-4h, for example, it can be 2h, 2.2h, 2.4h, 2.6h, 2.8h, 3h, 3.2h, 3.4h, 3.6h, 3.8h or 4h, as well as specific point values ​​between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values ​​included in the range.

[0041] Preferably, the printing method comprises screen printing.

[0042] Preferably, the etching method includes laser engraving.

[0043] Preferably, the light energy of the laser engraving is 1-3W, for example, it can be 1W, 1.2W, 1.4W, 1.6W, 1.8W, 2W, 2.2W, 2.4W, 2.6W, 2.8W or 3W, as well as specific point values ​​between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values ​​included in the said range; the light energy of the laser engraving is adjusted according to the thickness of the first insulating layer, the second insulating layer and the nano silver wire layer, and is required to penetrate the second insulating layer and the nano silver wire layer without causing damage to the first insulating layer.

[0044] Preferably, the thickness of the optical adhesive is 50-125 μm, for example, it can be 50 μm, 60 μm, 70 μm, 80 μm, 90 μm, 100 μm, 110 μm, 120 μm or 125 μm, as well as specific point values ​​between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values ​​included in the range.

[0045] Preferably, before the optical adhesive is bonded to the second insulating layer, a hole is firstly opened in the optical adhesive at a position corresponding to the binding position.

[0046] Preferably, the hole-making method includes die-cutting hole-making or laser-cutting hole-making.

[0047] Preferably, after the optical adhesive is bonded to the second insulating layer, the polarizer bonded to the optical adhesive is cut according to the shape of the organic light emitting diode display module.

[0048] Preferably, the cutting method includes die cutting or laser cutting.

[0049] The preparation method provided by the present invention uses a relatively simple coating and printing process on a large polarizer to make a touch function layer, and then bonds it with a large optical adhesive (OCA). Then, the large polarizer is cut according to the shape of the organic light-emitting diode display module and then bonds it with the organic light-emitting diode display module through OCA. The preparation process is simpler.

[0050] Preferably, after the cutting is completed, the method further includes a step of performing a functional test on the polarizer after the cutting.

[0051] Preferably, the binding is performed by the following method, which includes: using an anisotropic conductive adhesive film for the binding.

[0052] Preferably, the binding temperature is 140-160°C, for example, it can be 140°C, 142°C, 144°C, 146°C, 148°C, 150°C, 152°C, 158°C or 160°C, as well as specific point values ​​between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values ​​included in the range.

[0053] Preferably, the binding pressure is 1-3MPa, for example, it can be 1MPa, 1.2MPa, 1.4MPa, 1.6MPa, 1.8MPa, 2MPa, 2.2MPa, 2.4MPa, 2.6MPa, 2.8MPa or 3MPa, as well as specific point values ​​between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values ​​included in the range.

[0054] Preferably, the binding time is 10-15s, for example, it can be 10s, 11s, 12s, 13s, 14s or 15s, as well as specific point values ​​between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values ​​included in the range.

[0055] Preferably, the preparation method specifically comprises the following steps:

[0056] (1) a touch function layer is arranged on the back of the polarizer, wherein the touch function layer comprises a first insulating layer, a nano silver wire layer, and a second insulating layer which are stacked in sequence; and the method for setting the touch function layer comprises the following steps:

[0057] (S1) After applying the first insulating oil to the back side of the polarizer, first baking and first curing are sequentially performed to form the first insulating layer; the thickness of the first insulating layer is 1-3 μm; the uniformity of the first insulating layer is ≤5%; the first baking time is 100-500 s; the first baking temperature is 60-80° C.; the first curing time is 15-45 s; the first curing temperature is 30-50° C.;

[0058] (S2) coating the silver nanowires on the surface of the first insulating layer away from the back of the polarizer by a slit coating method, and then performing a second baking to form the silver nanowire layer; the second baking time is 100-500s; the second baking temperature is 60-80°C; the square resistance of the silver nanowires is 20-40Ω; the thickness of the silver nanowire layer is 50-4000nm;

[0059] (S3) after applying the second insulating oil to the surface of the nano silver wire layer away from the first insulating layer, performing a third baking and a second curing in sequence to form the second insulating layer; the thickness of the second insulating layer is ≤1 μm; the uniformity of the second insulating layer is ≤5%; the time of the third baking is 100-300 seconds; the temperature of the third baking is 60-80° C.; the time of the second curing is 10-35 seconds; the temperature of the second curing is 30-50° C.; the first curing and the second curing methods include curing by irradiation with ultraviolet light;

[0060] (2) printing silver paste on the pins of the nanosilver wires at the binding positions of the nanosilver wire layer by screen printing, and then performing a third curing to form a silver paste layer; the temperature of the third curing is 60-80° C.; the time of the third curing is 2-4 hours; the thickness of the silver paste layer is 5-15 μm;

[0061] (3) using laser engraving to etch functional patterns and wiring on the nano silver wire layer through the second insulating layer; the light energy of the laser engraving is 1-3W;

[0062] (4) opening a hole in the optical glue at a position corresponding to the binding position, and then laminating one side of the optical glue to the surface of the second insulating layer away from the nano silver wire layer, and then cutting the polarizer laminating the optical glue according to the shape of the organic light emitting diode display module, and then performing a functional test on the cut polarizer; the thickness of the optical glue is 50-125 μm;

[0063] (5) using anisotropic conductive adhesive film to bind the flexible circuit board of the touch function layer on the silver paste layer; the binding temperature is 140-160° C.; the binding pressure is 1-3 MPa; and the binding time is 10-15 s;

[0064] (6) bonding the other side of the optical adhesive to the organic light emitting diode display module;

[0065] (7) Welding the flexible circuit board of the touch function layer to the flexible circuit board of the organic light emitting diode display module to obtain the display module.

[0066] In a second aspect, the present invention provides a display module, wherein the display module is prepared by the preparation method described in the first aspect.

[0067] In a third aspect, the present invention provides an application of the display module as described in the second aspect, wherein the display module is used in a mask plate or a mobile phone.

[0068] Compared with the prior art, the present invention has the following beneficial effects:

[0069] The preparation method provided by the present invention realizes the preparation of an integrated touch display module, and uses a relatively simple process to produce a touch function layer on a conventional polarizer. Since the polarizer is relatively cheap compared to the organic light-emitting diode display module, even if unqualified products are produced, the loss is small, which reduces the production cost of the product and simplifies the preparation process. In addition, the prepared display module has a stronger anti-interference ability. BRIEF DESCRIPTION OF THE DRAWINGS

[0070] Figure 1 is a schematic cross-sectional structural diagram of a display module provided in Example 1;

[0071] Among them, 1-polarizer, 2-first insulating layer, 3-nano silver wire layer, 4-second insulating layer, 5-optical glue, 6-organic light emitting diode display module, 7-flexible circuit board of touch function layer, 8-flexible circuit board of organic light emitting diode display module, 9-silver paste layer. DETAILED DESCRIPTION

[0072] The technical solution of the present invention is further described below in conjunction with the accompanying drawings and through specific implementation methods. It should be understood by those skilled in the art that the embodiments are only to help understand the present invention and should not be regarded as specific limitations of the present invention.

[0073] The sources of some components in the embodiments and comparative examples are as follows:

[0074] (1) Polarizer: purchased from Suzhou Qingyue Optoelectronics Technology Co., Ltd., specification 370×470 mm;

[0075] (2) Acrylic resin: purchased from Suzhou Qingyue Optoelectronics Technology Co., Ltd.

[0076] (3) Nanosilver wire: purchased from Jiangsu Nameida Optoelectronics Technology Co., Ltd., with a square resistance of 30Ω;

[0077] (4) Optical adhesive: purchased from Feiou Technology (Suzhou) Co., Ltd., thickness 50 μm;

[0078] (5) Organic light emitting diode display module: purchased from Suzhou Qingyue Optoelectronics Technology Co., Ltd., model: 0108N module. VGM256064A4W11.HSF;

[0079] (6) Anisotropic conductive film: purchased from Suzhou Qingyue Optoelectronics Technology Co., Ltd.

[0080] Example 1

[0081] A display module and a method for manufacturing the same, wherein the cross-sectional structure diagram of the display module is as follows Figure 1 As shown, it includes a polarizer 1, a first insulating layer 2, a nano silver wire layer 3, a second insulating layer 4, an optical glue 5, an organic light emitting diode display module 6, a flexible circuit board 7 of a touch function layer, a flexible circuit board 8 of an organic light emitting diode display module, and a silver paste layer 9;

[0082] The preparation method comprises the following steps:

[0083] (1) a touch function layer is provided on the back side of the polarizer, wherein the touch function layer comprises a first insulating layer, a nano silver wire layer, and a second insulating layer which are stacked in sequence;

[0084] The method for setting the touch function layer comprises the following steps:

[0085] (S1) coating an acrylic resin on the back of the polarizer, baking the resin at 60° C. for 500 seconds, and curing the resin at 30° C. for 45 seconds under ultraviolet light to form the first insulating layer; the thickness of the first insulating layer is 1 μm; and the uniformity of the first insulating layer is 5%;

[0086] (S2) coating the silver nanowires on the surface of the first insulating layer away from the back of the polarizer by a slit coating method, and baking at 60° C. for 500 seconds to form the silver nanowire layer; the silver nanowire layer has a thickness of 50 nm;

[0087] (S3) coating acrylic resin on the surface of the silver nanowire layer away from the first insulating layer, baking at 60° C. for 300 seconds, and curing at 30° C. for 35 seconds under ultraviolet light to form the second insulating layer; the thickness of the second insulating layer is 0.4 μm; and the uniformity of the second insulating layer is 5%;

[0088] (2) printing silver paste on the pins of the nano-silver wires at the binding position of the nano-silver wire layer by screen printing, and then curing at 60° C. for 4 hours to form a silver paste layer; the thickness of the silver paste layer is 5 μm;

[0089] (3) using laser engraving to etch functional patterns and wiring on the nano silver wire layer through the second insulating layer; the light energy of the laser engraving is 1 W;

[0090] (4) opening a hole in the optical glue at a position corresponding to the binding position, and then laminating one side of the optical glue to the surface of the second insulating layer away from the nano silver wire layer, and then cutting the polarizer laminating the optical glue according to the shape of the organic light emitting diode display module, and then performing a functional test on the cut polarizer using ChipSemi_Developkit software;

[0091] (5) using an anisotropic conductive adhesive film on the silver paste layer to bond the flexible circuit board with the touch function layer at 140° C. and 3 MPa for 10 seconds;

[0092] (6) bonding the other side of the optical adhesive to the organic light emitting diode display module;

[0093] (7) Welding the flexible circuit board of the touch function layer to the flexible circuit board of the organic light emitting diode display module to obtain the display module.

[0094] Example 2

[0095] A display module and a preparation method thereof, the preparation method comprising the following steps:

[0096] (1) a touch function layer is provided on the back side of the polarizer, wherein the touch function layer comprises a first insulating layer, a nano silver wire layer, and a second insulating layer which are stacked in sequence;

[0097] The method for setting the touch function layer comprises the following steps:

[0098] (S1) coating an acrylic resin on the back of the polarizer, baking the resin at 80° C. for 100 seconds, and curing the resin at 50° C. for 15 seconds under ultraviolet light to form the first insulating layer; the thickness of the first insulating layer is 3 μm; and the uniformity of the first insulating layer is 1%;

[0099] (S2) coating the silver nanowires on the surface of the first insulating layer away from the back of the polarizer by a slit coating method, and baking at 80° C. for 100 seconds to form the silver nanowire layer; the silver nanowire layer has a thickness of 4 μm;

[0100] (S3) coating acrylic resin on the surface of the silver nanowire layer away from the first insulating layer, baking at 80° C. for 100 seconds, and curing at 50° C. for 10 seconds under ultraviolet light to form the second insulating layer; the thickness of the second insulating layer is 1 μm; and the uniformity of the second insulating layer is 5%;

[0101] (2) printing silver paste on the pins of the nano-silver wires at the binding position of the nano-silver wire layer by screen printing, and then curing at 80° C. for 2 hours to form a silver paste layer; the thickness of the silver paste layer is 15 μm;

[0102] (3) using laser engraving to etch functional patterns and wiring on the silver nanowire layer through the second insulating layer; the light energy of the laser engraving is 3W;

[0103] (4) opening a hole in the optical glue at a position corresponding to the binding position, and then laminating one side of the optical glue to the surface of the second insulating layer away from the nano silver wire layer, and then cutting the polarizer laminating the optical glue according to the shape of the organic light emitting diode display module, and then performing a functional test on the cut polarizer using ChipSemi_Developkit software;

[0104] (5) using an anisotropic conductive adhesive film on the silver paste layer to bond the flexible circuit board of the touch function layer at 160° C. and 1 MPa for 15 seconds;

[0105] (6) bonding the other side of the optical adhesive to the organic light emitting diode display module;

[0106] (7) Welding the flexible circuit board of the touch function layer to the flexible circuit board of the organic light emitting diode display module to obtain the display module.

[0107] Example 3

[0108] A display module and a preparation method thereof, the preparation method comprising the following steps:

[0109] (1) a touch function layer is provided on the back side of the polarizer, wherein the touch function layer comprises a first insulating layer, a nano silver wire layer, and a second insulating layer which are stacked in sequence;

[0110] The method for setting the touch function layer comprises the following steps:

[0111] (S1) coating an acrylic resin on the back of the polarizer, baking the resin at 70° C. for 300 seconds, and curing the resin at 40° C. for 30 seconds under ultraviolet light to form the first insulating layer; the thickness of the first insulating layer is 2 μm; and the uniformity of the first insulating layer is 2.5%;

[0112] (S2) coating the silver nanowires on the surface of the first insulating layer away from the back of the polarizer by a slit coating method, and baking at 70° C. for 300 seconds to form the silver nanowire layer; the silver nanowire layer has a thickness of 2 μm;

[0113] (S3) coating acrylic resin on the surface of the silver nanowire layer away from the first insulating layer, baking at 70° C. for 200 seconds, and curing at 40° C. for 25 seconds under ultraviolet light to form the second insulating layer; the thickness of the second insulating layer is 0.7 μm; and the uniformity of the second insulating layer is 5%;

[0114] (2) printing silver paste on the pins of the nano-silver wires at the binding position of the nano-silver wire layer by screen printing, and then curing at 70° C. for 3 hours to form a silver paste layer; the thickness of the silver paste layer is 10 μm;

[0115] (3) using laser engraving to penetrate the second insulating layer and etch functional patterns and wiring on the nano silver wire layer; the light energy of the laser engraving is 2W;

[0116] (4) opening a hole in the optical glue at a position corresponding to the binding position, and then laminating one side of the optical glue to the surface of the second insulating layer away from the nano silver wire layer, and then cutting the polarizer laminating the optical glue according to the shape of the organic light emitting diode display module, and then performing a functional test on the cut polarizer using ChipSemi_Developkit software;

[0117] (5) using an anisotropic conductive adhesive film on the silver paste layer to bond the flexible circuit board of the touch function layer at 150° C. and 2 MPa for 12.5 seconds;

[0118] (6) bonding the other side of the optical adhesive to the organic light emitting diode display module;

[0119] (7) Welding the flexible circuit board of the touch function layer to the flexible circuit board of the organic light emitting diode display module to obtain the display module.

[0120] Comparative Example 1

[0121] A display module and a preparation method thereof, the preparation method comprising the following steps:

[0122] (1) using anisotropic conductive adhesive film on the upper ITO surface of the organic light emitting diode display module, and bonding the flexible circuit board on the upper ITO surface at 150° C. and 2 MPa for 12.5 seconds;

[0123] (2) welding the flexible circuit board with the upper ITO surface to the flexible circuit board of the organic light emitting diode display module to obtain the display module;

[0124] (3) Use ChipSemi_Developkit software to perform functional testing.

[0125] Performance Test:

[0126] (1) Anti-interference ability test: At 20°C, a 2.1-inch display module was tested for its anti-interference ability using the software ChipSemi_Developkit with the same test fixture board and OTP firmware configuration, while the display module was lit and stationary; the closer the data of each test node is to 0, the stronger the anti-interference ability is; the display modules provided in Examples 1-3 and Comparative Example 1 were tested according to the above method, and the test results are shown in Tables 1-4:

[0127] Table 1

[0128]

[0129] Table 2

[0130]

[0131]

[0132] Table 3

[0133]

[0134] Table 4

[0135]

[0136]

[0137] It can be seen from Tables 1-4 that the display module provided in Comparative Example 1 is subject to relatively serious electromagnetic interference, while the test data of each node of the display module provided in Examples 1-3 are relatively small, and have stronger anti-interference ability. This is because the display module prepared by the preparation method provided in Comparative Example 1 has the situation of automatic touch reporting after the display module is lit, while the display module prepared by the preparation method provided by the present invention has no automatic touch reporting in the long-term display module lighting verification, and the relative touch performance is relatively stable, so the anti-interference ability is strong;

[0138] (2) Preparation yield test: Display modules were prepared according to the preparation methods provided in Examples 1-3 and Comparative Example 1, and 100 pcs of OLED modules were respectively used. The product was determined to be qualified according to the general standard for appearance inspection (as shown in Table 5) and the function inspection software program, and the preparation yield was tested. The test results are shown in Table 6.

[0139] Table 5

[0140]

[0141] Note: In Table 5, “ψ” represents the dot diameter; the AA area represents the effective display area, and the non-AA area represents the non-effective display area.

[0142] Table 6

[0143]

[0144]

[0145] It can be seen from the test data in Table 6 that the preparation yield of the display module prepared by the preparation method provided by the present invention is higher than that of the comparative example, and the preparation method provided by the present invention can better save costs.

[0146] The applicant declares that the present invention illustrates the detailed process flow of the present invention through the above-mentioned embodiments, but the present invention is not limited to the above-mentioned detailed process flow, that is, it does not mean that the present invention must rely on the above-mentioned detailed process flow to be implemented. Those skilled in the art should understand that any improvement of the present invention, equivalent replacement of various raw materials of the product of the present invention, addition of auxiliary components, selection of specific methods, etc., all fall within the protection scope and disclosure scope of the present invention.

Claims

1. A method for preparing a display module, characterized in that: The preparation method comprises: A touch function layer is arranged on the back of the polarizer, wherein the touch function layer comprises a first insulating layer, a nano silver wire layer and a second insulating layer which are stacked in sequence; the first insulating layer is bonded to the back of the polarizer; Disposing a silver paste layer on the pins of the nano-silver wires at the binding positions of the nano-silver wire layer; Etching functional patterns and routing on the silver nanowire layer through the second insulating layer; Laminating one side of the optical adhesive to the surface of the second insulating layer away from the silver nanowire layer; A flexible circuit board with the touch function layer bonded to the silver paste layer; Laminating the other side of the optical adhesive to the organic light emitting diode display module; The flexible circuit board of the touch function layer is welded to the flexible circuit board of the organic light emitting diode display module to obtain the display module.

2. The preparation method according to claim 1, characterized in that: The thickness of the first insulating layer is 1-3 μm; Preferably, the uniformity of the first insulating layer is ≤5%; Preferably, the first insulating layer is provided by the following method, the method comprising: applying a first insulating oil to the back surface of the polarizer, and then sequentially performing a first baking and a first curing to form the first insulating layer; Preferably, the first baking time is 100-500s; Preferably, the temperature of the first baking is 60-80°C; Preferably, the first curing time is 15-45s; Preferably, the temperature of the first curing is 30-50°C.

3. The preparation method according to claim 1 or 2, characterized in that: The nano silver wire layer is provided by the following method, the method comprising: coating the nano silver wire on the surface of the first insulating layer away from the back surface of the polarizer, and performing a second baking to form the nano silver wire layer; Preferably, the method of coating the nano silver wires comprises slit coating; Preferably, the second baking time is 100-500s; Preferably, the temperature of the second baking is 60-80°C; Preferably, the square resistance of the silver nanowire is 20-40Ω; Preferably, the thickness of the nano silver wire layer is 50-4000 nm.

4. The preparation method according to claim 2 or 3, characterized in that: The thickness of the second insulating layer is ≤1 μm; Preferably, the uniformity of the second insulating layer is ≤5%; Preferably, the second insulating layer is provided by the following method, the method comprising: coating a second insulating oil on a surface of the nano silver wire layer away from the first insulating layer, and then sequentially performing a third baking and a second curing to form the second insulating layer; Preferably, the materials of the first insulating oil and the second insulating oil each independently include acrylic resin; Preferably, the third baking time is 100-300s; Preferably, the temperature of the third baking is 60-80°C; Preferably, the second curing time is 10-35s; Preferably, the temperature of the second curing is 30-50°C; Preferably, the first curing and the second curing methods include curing using ultraviolet light.

5. The preparation method according to any one of claims 1 to 4, characterized in that: The thickness of the silver paste layer is 5-15 μm; Preferably, the silver paste layer is provided by the following method, the method comprising: printing silver paste on the pins of the nano silver wires at the binding positions of the nano silver wire layer, performing a third curing to form the silver paste layer; Preferably, the temperature of the third curing is 60-80°C; Preferably, the third curing time is 2-4h; Preferably, the printing method comprises screen printing.

6. The preparation method according to any one of claims 1 to 5, characterized in that: The etching method includes laser engraving; Preferably, the light energy of the laser engraving is 1-3W.

7. The preparation method according to any one of claims 1 to 6, characterized in that: The thickness of the optical adhesive is 50-125 μm; Preferably, before the optical adhesive is bonded to the second insulating layer, a hole is firstly opened at a position of the optical adhesive corresponding to the binding position; Preferably, the hole-making method includes die-cutting hole-making or laser-cutting hole-making; Preferably, after the optical adhesive is bonded to the second insulating layer, the polarizer bonded to the optical adhesive is cut according to the shape of the organic light emitting diode display module; Preferably, the cutting method includes die cutting or laser cutting; Preferably, after the cutting is completed, the method further comprises the step of performing a functional test on the polarizer after the cutting; Preferably, the binding adopts the following method, which includes: using anisotropic conductive adhesive film to perform the binding; Preferably, the binding temperature is 140-160°C; Preferably, the binding pressure is 1-3MPa; Preferably, the binding time is 10-15s.

8. The preparation method according to any one of claims 1 to 7, characterized in that: The preparation method specifically comprises the following steps: (1) a touch function layer is provided on the back side of the polarizer, wherein the touch function layer comprises a first insulating layer, a nano silver wire layer, and a second insulating layer which are stacked in sequence; The method for setting the touch function layer comprises the following steps: (S1) applying a first insulating oil to the back side of the polarizer, and then sequentially performing a first baking and a first curing to form the first insulating layer; The thickness of the first insulating layer is 1-3 μm; the uniformity of the first insulating layer is ≤5%; the first baking time is 100-500 s; the first baking temperature is 60-80° C.; the first curing time is 15-45 s; the first curing temperature is 30-50° C.; (S2) coating the silver nanowires on the surface of the first insulating layer away from the back surface of the polarizer by a slit coating method, and then performing a second baking to form the silver nanowire layer; The second baking time is 100-500s; the second baking temperature is 60-80°C; the square resistance of the silver nanowire is 20-40Ω; the thickness of the silver nanowire layer is 50-4000nm; (S3) coating a second insulating oil on a surface of the silver nanowire layer away from the first insulating layer, and then sequentially performing a third baking and a second curing to form the second insulating layer; The thickness of the second insulating layer is ≤1 μm; the uniformity of the second insulating layer is ≤5%; the time of the third baking is 100-300 seconds; the temperature of the third baking is 60-80°C; the time of the second curing is 10-35 seconds; the temperature of the second curing is 30-50°C; The first curing and the second curing methods include curing by irradiation with ultraviolet light; (2) printing silver paste on the pins of the silver nanowires at the binding positions of the silver nanowire layer by screen printing, and then performing a third curing to form a silver paste layer; The temperature of the third curing is 60-80° C.; the time of the third curing is 2-4 hours; the thickness of the silver paste layer is 5-15 μm; (3) using laser engraving to etch functional patterns and wiring on the silver nanowire layer through the second insulating layer; The light energy of the laser engraving is 1-3W; (4) opening a hole in the optical glue at a position corresponding to the binding position, and then laminating one side of the optical glue to the surface of the second insulating layer away from the nano silver wire layer, and then cutting the polarizer laminating the optical glue according to the shape of the organic light emitting diode display module, and then performing a functional test on the cut polarizer; The thickness of the optical adhesive is 50-125 μm; (5) using an anisotropic conductive adhesive film to bind the flexible circuit board with the touch function layer on the silver paste layer; The binding temperature is 140-160°C; the binding pressure is 1-3MPa; the binding time is 10-15s; (6) bonding the other side of the optical adhesive to the organic light emitting diode display module; (7) Welding the flexible circuit board of the touch function layer to the flexible circuit board of the organic light emitting diode display module to obtain the display module.

9. A display module, characterized in that: The display module is prepared by the preparation method according to any one of claims 1 to 8.

10. An application of the display module according to claim 9, characterized in that: Application of the display module in a mask plate or a mobile phone.