Homogenized tobacco high-temperature extract, preparation method thereof and heating cigarette

By heat treatment, crushing and oxidizing the tobacco raw materials, it forms modified microparticles, combined with ultrasonic and mechanical stirring homogenization, the phase separation problem of tobacco high-temperature extracts during placement is solved, and the taste and quality of the heated cigarette is stable. sex.

CN118902162AActive Publication Date: 2024-11-08HUBEI CHINA TOBACCO INDUSTRY CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411308004.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-19
Publication Date
2024-11-08
Estimated Expiration
2044-09-19

AI Technical Summary

Technical Problem

When placed, the tobacco high-temperature extract is prone to separation of the aqueous phase and the oil phase, resulting in the delamination of light and heavy components and hydrophilic and hydrophobic components. When added to the flake, the feeding is uneven, which affects the suction of the heated cigarette. Consistent taste.

Method used

High-temperature extract and semi-coke residue were obtained by heat treatment of tobacco raw materials. After pulverization, the modified microparticles were formed, and mixed with the high-temperature extract. Through mechanical stirring and ultrasonic homogenization, homogenized tobacco without phase separation was formed. High temperature extract.

Benefits of technology

The stable homogeneous state of tobacco high-temperature extract is achieved, phase separation is avoided, the taste consistency and quality of the heating cigarette is ensured, and the generation of impurities gases from non-tobacco sources is avoided.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
  • Figure SMS_2
    Figure SMS_2
Patent Text Reader

Abstract

The invention provides a tobacco high-temperature extract homogenizing method. The tobacco high-temperature extract homogenizing method comprises the following steps that tobacco raw materials are subjected to heat treatment and condensation, and a high-temperature extract and semi-coke residues are obtained; crushing the semi-coke residues to obtain microparticles; carrying out oxidation treatment on the microparticles to obtain modified microparticles; and mixing the high-temperature extract with the modified microparticles to obtain the homogenized tobacco high-temperature extract. The surface of the by-product semicoke obtained through a tobacco high-temperature extraction process contains a large number of hydrophilic groups mainly containing hydroxyl and a part of hydrophobic groups containing nitrogen. After the semicoke is subjected to high-temperature partial oxidation, hydrophobic groups on the surface of the semicoke can be remarkably increased, so that the semicoke microparticles subjected to high-temperature oxidation modification have amphipathy in a solution. Moreover, after the amphiphilic semi-coke microparticles are ground into nanoscale size, the amphiphilic semi-coke microparticles can be well and stably dispersed in the extract, so that the non-uniform tobacco high-temperature extract forms a stable homogeneous liquid, and phase separation does not occur in the long-time storage process.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of tobacco, in particular to a homogenized high-temperature tobacco extract and a preparation method thereof and a cigarette. Background Art

[0002] The smoking temperature of heated cigarettes is low, and the harmful components in the smoke released are significantly reduced, which has significant advantages in reducing tar and reducing harm. However, the lower smoking temperature also leads to insufficient thermal cracking of the slices, insufficient release of nicotine and flavor components, etc., resulting in insufficient aroma and satisfaction when smoking. Adding high-temperature tobacco extract to the slices is an effective way to enhance the aroma and satisfaction of heated cigarettes.

[0003] The composition of high-temperature tobacco extract is complex, including hydrophilic compounds such as water, small molecule acids, aldehydes, alcohols, ketones, and hydrophobic compounds such as long-chain fats, aromatics, large heterocycles, and oligomers. It is difficult for each component to fully dissolve, and the water phase and oil phase are easily separated when left standing, resulting in direct stratification of light and heavy components and hydrophilic and hydrophobic components. After the extract is separated, when it is added to the slice, it is easy to cause the quality of the slice to fluctuate due to uneven feeding, which ultimately affects the consistency of the taste of the heated cigarette.

[0004] Therefore, it is very necessary to provide a homogenized high-temperature tobacco extract without phase separation. Summary of the invention

[0005] In view of this, the technical problem to be solved by the present invention is to provide a homogenized high-temperature tobacco extract. The high-temperature tobacco extract provided by the present invention does not undergo phase separation, and when added to the slices, no impurity gas from non-tobacco sources is generated, and has no effect on the taste of the smoke.

[0006] The present invention provides a method for homogenizing a high-temperature tobacco extract, comprising the following steps:

[0007] A) The tobacco raw material is heat treated and condensed to obtain a high temperature extract and a semi-coke residue;

[0008] B) crushing the semi-coke residue to obtain micro particles;

[0009] C) oxidizing the microparticles to obtain modified microparticles;

[0010] D) The high temperature extract and the modified microparticles are mixed to obtain a homogenized tobacco high temperature extract.

[0011] Preferably, in step A), the heat treatment temperature is 300-950° C., the treatment time is 20-40 min, and the heat treatment atmosphere is an inert atmosphere.

[0012] Preferably, the particle size of the microparticles in step B) is below 800 nm, preferably below 500 nm.

[0013] Preferably, the oxidation treatment parameters in step C) include:

[0014] The oxygen content in the reaction atmosphere is 1~4%, the temperature is 400~800°C, and the time is 10~30 min.

[0015] Preferably, the N content of the semi-coke residue is not less than 2%; when the N content is less than 2%, 1-3% of an external nitrogen source is added to the oxidation treatment atmosphere so that the N content of the treated semi-coke residue is not less than 2%, and the external nitrogen source is NH3.

[0016] Preferably, in step D), the mixing is mechanical stirring combined with ultrasonic homogenization, and the mixing time is 5 to 20 minutes;

[0017] The homogenization parameters are: the speed of the mechanical stirrer is 800-2000 r / min; the power of the ultrasonic treatment is 20-40 W / L, and the ultrasonic time is 20-40 min;

[0018] Preferably, the content of microparticle semi-coke in the homogenized high-temperature tobacco extract in step D) is 0.1-3 wt%.

[0019] The present invention provides a homogenized high-temperature tobacco extract, which is prepared by the method disclosed in any one of the above technical solutions.

[0020] The present invention provides a tobacco material, comprising the homogenized high-temperature tobacco extract described in the above technical solution.

[0021] The present invention provides a cigarette, comprising the tobacco material described in the above technical solution.

[0022] Compared with the prior art, the present invention provides a method for homogenizing tobacco high-temperature extract, comprising the following steps: A) heat-treating tobacco raw materials and condensing to obtain high-temperature extracts and semi-coke residues; B) crushing the semi-coke residues to obtain microparticles; C) oxidizing the microparticles to obtain modified microparticles; D) mixing the high-temperature extracts and modified microparticles to obtain homogenized tobacco high-temperature extracts. The surface of the semi-coke, a byproduct obtained by the tobacco high-temperature extraction process of the present invention, contains a large number of hydrophilic groups mainly composed of hydroxyl groups and some nitrogen-containing hydrophobic groups. After the semi-coke is partially oxidized at high temperature, the hydrophobic groups on the surface of the semi-coke can be significantly increased, so that the semi-coke microparticles modified by high-temperature oxidation have amphiphilicity in the tobacco high-temperature extract solution. In addition, after the amphiphilic semi-coke particles are ground into nano-scale size, they can be well and stably dispersed in the extract, thereby forming a stable homogeneous liquid of the non-uniform tobacco high-temperature extract, and no phase separation occurs during the long-term storage process. DETAILED DESCRIPTION

[0023] The present invention provides a homogenized high-temperature tobacco extract and a preparation method thereof and a heated cigarette. Those skilled in the art can refer to the content of this article and appropriately improve the process parameters to achieve the same. It should be particularly noted that all similar substitutions and modifications are obvious to those skilled in the art, and they all fall within the scope of protection of the present invention. The methods and applications of the present invention have been described through preferred embodiments, and relevant personnel can obviously modify or appropriately change and combine the methods and applications of this article without departing from the content, spirit and scope of the present invention to implement and apply the technology of the present invention.

[0024] In this application, the term "and / or" describes the association relationship of associated objects, indicating that there may be three relationships. For example, A and / or B can represent: A exists alone, A and B exist at the same time, and B exists alone. A and B can be singular or plural.

[0025] In this application, "at least one" means one or more, "more than one" means two or more. "At least one of the following" or similar expressions refers to any combination of these items, including any combination of single or plural items.

[0026] Unless otherwise defined herein, scientific and technical terms related to the present invention shall have the meanings understood by those of ordinary skill in the art.

[0027] Furthermore, unless otherwise indicated herein, singular terms shall include pluralities and plural terms shall include the singular. More specifically, as used in this specification and the appended claims, the singular forms "a," "an," and "the" include plural referents unless expressly indicated otherwise.

[0028] The terms "include", "comprising" and "having" are used interchangeably herein and are intended to indicate the inclusiveness of the solution, meaning that the solution may have other elements in addition to the listed elements. At the same time, it should be understood that the use of "include", "comprising" and "having" descriptions herein also provides a "consisting of..." solution.

[0029] The term "and / or" as used herein includes the meanings of "and", "or" and "all or any other combination of elements linked by the associated term".

[0030] The term "smoking article" refers to any product that can be smoked, whether based on tobacco, tobacco derivatives, expanded tobacco, reconstituted tobacco or tobacco substitutes, or any product that can provide a smoking experience. For example, smoking articles may include smokable articles such as cigarettes, cigars and cigarillos. As another example, smoking articles may include combustion smoking articles and heat smoking articles.

[0031] In the following embodiments, "tobacco material" can refer to the material that produces smoke and / or aerosol or is used for smoking.For example, smoking material can include tobacco material.Tobacco material can include for example tobacco leaf sheet, tobacco stem or the material processed by it etc.As a more specific example, tobacco material can include crushed tobacco leaf, crushed reconstituted tobacco, expanded shredded filler, expanded stem and lobule etc.But the present invention is not limited to this.In addition, tobacco material can have but not limited to the form of tobacco shredded filler, tobacco particles, tobacco sheet, tobacco pearl, tobacco particles or tobacco high temperature extract.

[0032] In certain embodiments, smoking material can also include additives, such as wetting agent (wetting agent), flavoring agent and / or organic acid.For example, wetting agent can include at least one of glycerol, propylene glycol, ethylene glycol, dipropylene glycol, diethylene glycol, triethylene glycol, tetraethylene glycol and oleyl alcohol.Wetting agent can keep the moisture in tobacco raw material at appropriate level, soften its inherent taste, enrich atomization amount.In addition, flavoring agent includes, for example, liquorice, sucrose, fructose syrup, isosweet, cocoa, lavender, cinnamon, cardamom, celery, fenugreek, black currant, sandalwood, bergamot, geranium, honey essence, rose oil, vanilla, lemon oil, orange oil, peppermint oil, cinnamon, coriander, brandy, jasmine, chamomile, menthol, cinnamon, ylang-ylang, sage, spearmint, ginger, coriander, clove extract (or clove material) or coffee.

[0033] According to some embodiments of the present disclosure, a tobacco high-temperature extract sheet can be provided. The tobacco high-temperature extract sheet can be prepared from a sheet liquid containing at least one tobacco high-temperature extract solution and a sheet-forming agent, and can be applied to smoking articles in various ways to enhance the stability of the smoking articles. Phase separation can be avoided during long-term storage.

[0034] The present invention provides a method for homogenizing a high-temperature tobacco extract, comprising the following steps:

[0035] A) The tobacco raw material is heat treated and condensed to obtain a high temperature extract and a semi-coke residue;

[0036] B) crushing the semi-coke residue to obtain micro particles;

[0037] C) oxidizing the microparticles to obtain modified microparticles;

[0038] D) The high temperature extract and the modified microparticles are mixed to obtain a homogenized tobacco high temperature extract.

[0039] The method for homogenizing high-temperature tobacco extract provided by the invention firstly heat-treats tobacco raw materials and condenses them to obtain high-temperature extracts and semi-coke residues.

[0040] The present invention does not limit the tobacco raw materials, and any materials known to those skilled in the art may be tobacco leaves, tobacco stems, tobacco dust, tobacco waste, etc. known to those skilled in the art.

[0041] The temperature of the heat treatment of the present invention is preferably 300-950° C., more preferably 350-800° C., most preferably 400-650° C., and particularly preferably 450-500° C. The time of the heat treatment of the present invention is preferably 20-40 min, more preferably 25-35 min, and particularly preferably 30 min.

[0042] The atmosphere of the heat treatment is an inert gas, which may include N2, Ar, etc.

[0043] The present invention does not limit the specific conditions for the above condensation, which are well known to those skilled in the art.

[0044] The semi-coke residue is crushed to obtain fine particles.

[0045] The invention takes the solid residue semi-coke after high-temperature treatment of tobacco and crushes it into micro particles.

[0046] The present invention does not limit the pulverization method, which is well known to those skilled in the art. Preferably, ball milling is used; the particle size of the pulverized particles after ball milling is less than 800 nm.

[0047] The particle size of the microparticles of the present invention is below 800 nm, preferably below 500 nm.

[0048] In a specific embodiment, the particle size of the microparticles is 200 nm to 400 nm.

[0049] The microparticles are oxidized to obtain modified microparticles.

[0050] According to the present invention, the oxidation treatment parameters include:

[0051] Oxygen content 1~4%, temperature 400~800°C, time 10~30 min.

[0052] In some specific embodiments, the oxidation treatment parameters include:

[0053] 500~700°C, 2%~3% oxygen content for 15~25 min;

[0054] In a specific embodiment, the oxidation treatment parameters include:

[0055] Treated at 600°C and 2% oxygen content for 20 min.

[0056] The N content of the semi-coke residue of the present invention is not less than 2%;

[0057] When the N content is lower than 2%, 1-3% of an external nitrogen source is added to the oxidation atmosphere, and the external nitrogen source is NH3.

[0058] The high-temperature extract and the modified microparticles are mixed to obtain a homogenized tobacco high-temperature extract.

[0059] The mixing of the present invention is mechanical stirring combined with ultrasonic homogenization, and the mixing time is 5 to 20 min, more preferably 10 to 20 min.

[0060] The homogenization parameters are: the speed of the mechanical stirrer is 800-2000 r / min; the power of the ultrasonic treatment is 20-40 W / L, and the ultrasonic time is 20-40 min;

[0061] The content of microparticle semi-coke in the homogenized high-temperature tobacco extract is preferably 0.1-3 wt %.

[0062] The present invention provides a homogenized high-temperature tobacco extract, which is prepared by the method disclosed in any one of the above technical solutions.

[0063] The present invention provides a tobacco material, comprising the homogenized high-temperature tobacco extract described in the above technical solution.

[0064] The tobacco material of the present invention includes tobacco flakes and the like, which are well known to those skilled in the art.

[0065] The present invention provides a tobacco product, comprising the tobacco material described in the above technical solution.

[0066] The present invention provides a cigarette, comprising the tobacco material described in the above technical solution.

[0067] The cigarette of the present invention also includes conventional auxiliary materials used by those skilled in the art, which are not limited in the present invention.

[0068] The invention provides a method for homogenizing a tobacco high-temperature extract, comprising the following steps: A) heat-treating tobacco raw materials and condensing to obtain a high-temperature extract and a semi-coke residue; B) crushing the semi-coke residue to obtain microparticles; C) oxidizing the microparticles to obtain modified microparticles; and D) mixing the high-temperature extract and the modified microparticles to obtain a homogenized tobacco high-temperature extract. The surface of the semi-coke, a byproduct obtained by the tobacco high-temperature extraction process, contains a large number of hydrophilic groups mainly composed of hydroxyl groups and some nitrogen-containing hydrophobic groups. After the semi-coke is partially oxidized at high temperature or the nitrogen-containing groups are increased, the hydrophobic groups on the surface of the semi-coke can be significantly increased, so that the semi-coke microparticles after high-temperature oxidation modification or nitrogen content regulation have amphiphilicity in the solution. Moreover, after the amphiphilic semi-coke particles are ground into nanometer-sized sizes, they can be well and stably dispersed in the extract, thereby forming a stable homogeneous liquid from the non-uniform tobacco high-temperature extract, and no phase separation occurs during the long-term storage process.

[0069] The materials used in the method of the present invention are all from tobacco. Tobacco semi-coke is a by-product of high-temperature extraction. After it is added to the slice, no impurity gas from non-tobacco sources will be generated.

[0070] It should be understood that in the various embodiments of the present application, the size of the serial numbers of the above-mentioned processes does not mean the order of execution, some or all of the steps can be executed in parallel or sequentially, and the execution order of each process should be determined by its function and internal logic, and should not constitute any limitation on the implementation process of the embodiments of the present application.

[0071] The numerical ranges and parameters involved in the present invention have presented the relevant numerical values ​​in the specific embodiments as accurately as possible. However, any numerical value essentially inevitably contains standard deviations due to individual testing methods. Therefore, unless otherwise explicitly stated, it should be understood that all numerical ranges or specific data used in this disclosure may have certain reasonable deviations within a certain range, for example: within 1% or 0.5%.

[0072] Some cases are recorded in the embodiments and comparative examples of the present invention, wherein the embodiments show certain implementation modes of the present invention. However, this does not mean that the effects of the present invention can only be achieved in these cases.

[0073] In order to further illustrate the present invention, a homogenized high-temperature tobacco extract, a preparation method thereof and a cigarette provided by the present invention are described in detail below in conjunction with examples.

[0074] Example 1

[0075] Take a kind of tobacco dust, and after high temperature reaction at 550℃ and nitrogen atmosphere for 20 minutes, obtain 10kg of tobacco high temperature extract, and take 1kg of residual semi-coke. The residual semi-coke is ball-milled for 4 hours, and sieved to obtain 0.3kg of semi-coke nanoparticles with a particle size of 200~400nm. The semi-coke nanoparticles are subjected to elemental analysis, and the N content is measured to be 3.8 wt% (received basis). The semi-coke nanoparticles are treated at 600°C and 2% oxygen content for 20 minutes to obtain modified micro-particle semi-coke. 10kg of tobacco high temperature extract and 0.2kg of modified micro-particle semi-coke are fully mixed, and ultrasonic and mechanical stirring are carried out for 20 minutes to obtain a homogenized tobacco high temperature extract.

[0076] The tobacco high-temperature extract obtained in Example 1 was placed in a sealed bottle and allowed to stand at 4° C. for 72 h, and no phase separation was observed.

[0077] Example 2

[0078] Take a kind of tobacco dust, and after high temperature reaction at 550℃ and nitrogen atmosphere for 20 min, obtain 10kg of tobacco high temperature extract, and take 1kg of residual semi-coke. The residual semi-coke is ball-milled for 4 h, and sieved to obtain 0.3kg of semi-coke nanoparticles with a particle size of 200~400 nm. The semi-coke nanoparticles are subjected to elemental analysis, and the N content is measured to be 1.6 wt% (received basis). The semi-coke nanoparticles are treated at 600°C, 2% oxygen content, and 2% NH3 content for 20 min to obtain modified micro-particle semi-coke. 10 kg of tobacco high temperature extract and 0.2 kg of modified micro-particle semi-coke are fully mixed, and ultrasonic and mechanical stirring are carried out for 20 min to obtain a homogenized tobacco high temperature extract.

[0079] The tobacco high-temperature extract obtained in Example 2 was placed in a sealed bottle and allowed to stand at 4° C. for 72 h, and no phase separation was observed.

[0080] Comparative Example 1

[0081] Take a kind of tobacco dust, and after high temperature reaction at 550℃ and nitrogen atmosphere for 20 minutes, obtain 10kg of tobacco high temperature extract, and take 1kg of residual semi-coke. The residual semi-coke is ball-milled for 1 hour, and sieved to obtain 0.3kg of semi-coke nanoparticles with a particle size of 800~1500 nm. The semi-coke nanoparticles are subjected to elemental analysis, and the N content is measured to be 3.8 wt% (received basis). The semi-coke nanoparticles are treated at 600°C and 2% oxygen content for 20 minutes to obtain modified micro-particle semi-coke. 10kg of tobacco high temperature extract and 0.2kg of modified micro-particle semi-coke are fully mixed, and ultrasonic and mechanical stirring are carried out for 20 minutes to obtain the mixed tobacco high temperature extract.

[0082] The tobacco high-temperature extract obtained in this comparative example 1 was placed in a sealed bottle and allowed to stand at 4°C. Phase separation was observed at the 4th hour, obvious phase separation began to appear at the 8th hour, and a stable separation state was maintained at the 11th hour.

[0083] Comparative Example 2

[0084] Take a kind of tobacco dust, and after high temperature reaction at 550℃ and nitrogen atmosphere for 20 minutes, obtain 10kg of tobacco high temperature extract, and take 1kg of residual semi-coke. The residual semi-coke is ball-milled for 4 hours, and sieved to obtain 0.3kg of semi-coke nanoparticles with a particle size of 200~400nm. The semi-coke nanoparticles are subjected to elemental analysis, and the N content is measured to be 1.6 wt% (received basis). The semi-coke nanoparticles are treated at 600°C and 2% oxygen content for 20 minutes to obtain modified micro-particle semi-coke. 10kg of tobacco high temperature extract and 0.2kg of modified micro-particle semi-coke are fully mixed, and ultrasonic and mechanical stirring are carried out for 20 minutes to obtain a homogenized tobacco high temperature extract.

[0085] The tobacco high-temperature extract obtained in Comparative Example 2 was placed in a sealed bottle and allowed to stand at 4°C. Phase separation was observed at the 16th hour, obvious phase separation began to appear at the 31st hour, and a stable separation state was maintained at the 43rd hour.

[0086] Comparative Example 3

[0087] Take a kind of tobacco dust, and after high temperature reaction at 550℃ and nitrogen atmosphere for 20 minutes, obtain 10kg of tobacco high temperature extract, and take 1kg of residual semi-coke. The residual semi-coke is ball-milled for 4 hours, and sieved to obtain 0.3kg of semi-coke nanoparticles with a particle size of 200~400 nm. The semi-coke nanoparticles are subjected to elemental analysis, and the N content is measured to be 3.8 wt% (received basis). The semi-coke nanoparticles are treated at 600°C and nitrogen atmosphere for 20 minutes to obtain modified micro-particle semi-coke. 10kg of tobacco high temperature extract and 0.2kg of modified micro-particle semi-coke are fully mixed, and ultrasonic and mechanical stirring are carried out for 20 minutes to obtain a homogenized tobacco high temperature extract.

[0088] The tobacco high-temperature extract obtained in this comparative example 3 was placed in a sealed bottle and allowed to stand at 4°C. Phase separation was observed at the 18th hour, obvious phase separation began to appear at the 27th hour, and a stable separation state was maintained at the 33rd hour.

[0089] The high-temperature tobacco extract obtained in the embodiment and the comparative example was stirred evenly and then added to the thick pulp flakes at a ratio of 0.1 wt% by a method well known to those skilled in the art, and heated cigarettes were produced; and the high-temperature tobacco extract obtained in the comparative example was left to stand for 72 hours, and the upper and lower extracts after phase separation were taken, and thick pulp flakes were prepared according to the above method, and heated cigarettes were produced. Professional smoking testers conducted sensory quality scoring according to the national standard (sensory technical requirements) GB5606.4-2005, and the results are shown in the following table.

[0090] Table 1 Sensory quality rating of the examples

[0091]

[0092] Table 2 Sensory quality scores of comparative examples

[0093]

[0094] According to the standing experiment of tobacco high-temperature extract and the sensory quality scoring results in the above table, the heated cigarettes produced by the thin slices prepared by the tobacco high-temperature extract of the present invention have significantly improved stability during storage, compared with Comparative Example 1 with different ball-milled particle sizes, Comparative Example 2 with insufficient N element, and Comparative Example 3 with different atmosphere conditions. No phase separation was observed after standing for 72 hours. The comparative example results show that when the tobacco high-temperature extract is not mixed with semi-coke nanoparticles, or the mixed semi-coke particles are not processed to the nanometer level, or are not oxidatively modified or N content is not regulated, there are different degrees of insufficient stability. The essential reason is that the liquid phase system of the tobacco high-temperature extract lacks a uniform dispersion medium (i.e., the modified semi-coke nanoparticles of the present invention) that allows the water phase and oil phase components to dissolve.

[0095] When the high-temperature tobacco extract is in a homogeneous state, or is artificially mixed before use, the scores of the heated cigarettes produced increase consistently; when the high-temperature tobacco extract is phase separated, the scores of the heated cigarettes produced by different phase extracts increase, but there are obvious differences in the sub-item scores and the total score, indicating that the phase separation of the high-temperature tobacco extract will obviously cause the quality fluctuation of the heated cigarette products. The homogenization method of the present invention can effectively solve the above problems.

[0096] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.

Claims

1. A method for homogenizing a high-temperature tobacco extract, It is characterized in that The steps include: A) The tobacco raw material is heat treated and condensed to obtain a high temperature extract and a semi-coke residue; B) crushing the semi-coke residue to obtain micro particles; C) oxidizing the microparticles to obtain modified microparticles; D) The high temperature extract and the modified microparticles are mixed to obtain a homogenized tobacco high temperature extract.

2. The method according to claim 1, It is characterized in that Step A) The heat treatment temperature is 300-950°C, and the treatment time is 20-40 min; the heat treatment atmosphere is an inert atmosphere.

3. The method according to claim 1, It is characterized in that Step B) The particle size of the microparticles is below 800 nm, preferably below 500 nm.

4. The method according to claim 1, It is characterized in that Step C) The oxidation treatment parameters include: The oxygen content in the reaction atmosphere is 1~4%, the temperature is 400~800°C, and the time is 10~30 min.

5. The method according to claim 4, It is characterized in that The N content of the semi-coke residue is not less than 2%; when the N content is less than 2%, 1-3% of an external nitrogen source is added to the oxidation treatment atmosphere so that the N content of the semi-coke residue after treatment is not less than 2%, and the external nitrogen source is NH 3 .

6. The method according to claim 1, It is characterized in that Step D) The mixing is mechanical stirring combined with ultrasonic homogenization, and the mixing time is 5-20 min; the homogenization parameters are: the speed of the mechanical stirrer is 800-2000 r / min; the power of the ultrasonic treatment is 20-40 W / L, and the ultrasonic time is 20-40 min.

7. The method according to claim 1, It is characterized in that Step D) The content of microparticle semi-coke in the homogenized high-temperature tobacco extract is 0.1-3 wt%.

8. A homogenized high-temperature tobacco extract, It is characterized in that Prepared by the method according to any one of claims 2 to 7.

9. A tobacco material, It is characterized in that The invention comprises the homogenized high-temperature tobacco extract as described in claim 8.

10. A smoking article, It is characterized in that Comprising the tobacco material of claim 9.

Citation Information

Patent Citations

  • Method of extracting essential oil from biomass wastes and a device thereof

    CA2681816A1

  • Improved tobacco flavor dry powder formulations

    CN114554876A

  • Method for preparing tobacco extract

    CN118266625A

  • Smokable material containing thermally degraded tobacco by-products and its method of preparation

    US4256123A

  • Tobacco flavoring components of enhanced aromatic content and method of providing same