Continuous extrusion die for aluminum wires

Through the design of the aluminum wire continuous extrusion mold, the continuous extrusion channel and flow improve the structure, the problems of cumbersome processes and long cycles in aluminum welding wire production are solved, and efficient and stable aluminum wire forming and quality improvement are achieved.

CN118904954APending Publication Date: 2024-11-08SOLOMON (CHANGZHOU) ALLOY NEW MATERIAL CO LTD +1
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202411322758.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-23
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The existing problems are that the process of producing aluminum wires with a diameter of less than 2mm is complicated and the production cycle is long. It is necessary to obtain the welding wire of the required diameter through multiple drawing and annealing treatments.

Method used

Using a continuous extrusion die of aluminum wire, a continuous extrusion channel is formed by a coaxial feed base and an aluminum wire die seat using the first feeding hole and a plurality of second feeding holes, combining with hemispherical resistance. The flow block, flow-promoting part, inclined stop block and electrostatic removal fan realizes continuous extrusion molding of aluminum and reduces drawing and annealing treatment.

Benefits of technology

One-step molding of aluminum wire is achieved, which significantly improves production efficiency, reduces production costs, and improves product quality and stability, avoids turbulence and static problems.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118904954A_ABST
    Figure CN118904954A_ABST
Patent Text Reader

Abstract

The invention relates to a continuous extrusion die for aluminum wires, and belongs to the technical field of metal material machining, the continuous extrusion die comprises a feeding base and an aluminum wire die holder which are coaxially arranged and connected, a first material channel hole is formed in the feeding base in the axial direction, a mounting cavity is formed in the side, facing the aluminum wire die holder, of the feeding base, and the mounting cavity and the first material channel hole are communicated and coaxial; the aluminum wire die holder is mounted in the mounting cavity; a plurality of second material channel holes communicating with the mounting cavity are formed in the aluminum wire die holder, and the hole diameter of the second material channel holes is 1.2 mm-2mm. According to the aluminum wire die, the feeding base and the aluminum wire die holder are coaxially arranged and connected, and the first material channel holes are formed in the feeding base and used for guiding aluminum materials to enter the die; the second material channel hole is formed in the aluminum wire die holder, the diameter of the final aluminum welding wire is directly determined by the hole diameter of the second material channel hole, a continuous extrusion channel is formed by the first material channel hole and the second material channel hole, and accurate control over the diameter is achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of metal material processing, and in particular relates to a continuous extrusion die for aluminum wire. Background Art

[0002] In the field of metal processing, aluminum welding wire, as an important welding material, is widely used in aerospace, automobile manufacturing, electronic communications and other industries.

[0003] For example, the invention patent with patent authorization announcement number: CN103143858B discloses a method for producing aluminum welding wire. After being extruded by an extruder to form an aluminum wire with a diameter of 16.5 mm, it undergoes multiple drawing processes to obtain an aluminum wire with a diameter of 2.4 mm.

[0004] Based on the search of the above patent authorization announcement number and the shortcomings found therein:

[0005] When producing aluminum welding wire with a diameter of less than 2mm, we usually first try to use an extruder to extrude aluminum wire with a larger diameter, and then use a multi-pass drawing process. After a complex process of multiple drawing, annealing, and re-drawing, we finally get the welding wire of the required diameter. Although this can produce high-quality aluminum welding wire, the process is cumbersome and the production cycle is long. Summary of the invention

[0006] In order to solve the problem that when producing aluminum welding wire with a diameter within 2 mm, an extruder is generally used to extrude an aluminum wire with a larger diameter, and then a multi-pass drawing process is adopted. After a complex process of multiple drawing, annealing, and re-drawing, the welding wire of the required diameter is finally obtained. Although high-quality aluminum welding wire can be produced in this way, the process is cumbersome and the production cycle is long. The present invention provides a continuous extrusion die for aluminum wire.

[0007] The purpose of the present invention can be achieved through the following technical solutions:

[0008] A continuous extrusion die for aluminum wire, comprising a feed base and an aluminum wire die base that are coaxially arranged and connected, the feed base being provided with a first material channel hole along the axial direction, the feed base being provided with an installation cavity on the side facing the aluminum wire die base, the installation cavity being connected to the first material channel hole and being coaxial, the aluminum wire die base being installed in the installation cavity; the aluminum wire die base being provided with a plurality of second material channel holes connected to the installation cavity, the aperture of the second material channel holes being 1.2 mm-2 mm.

[0009] As a preferred technical solution of the present invention, a hemispherical baffle is provided on the side of the aluminum wire die seat facing the feed base, the hemispherical baffle is coaxially arranged with the aluminum wire die seat, and a plurality of the second material channel holes are evenly arranged around the hemispherical baffle.

[0010] As a preferred technical solution of the present invention, a flow-promoting portion is provided at one end of the second material channel hole connected to the installation cavity, and the flow-promoting portion is a smooth curved surface whose diameter gradually decreases from the surface of the aluminum wire die seat toward the second material channel hole.

[0011] As a preferred technical solution of the present invention, it also includes a sloped stop block, a first mounting groove is provided on the side of the feed base away from the mounting cavity, the first mounting groove is located next to the first material channel hole, and the sloped stop block is installed in the first mounting groove; the first material channel hole includes a turning feed channel close to the sloped stop block and a straight feed channel close to the mounting cavity, the side wall of the turning feed channel away from the sloped stop block gradually turns and extends in the direction away from the sloped stop block, the extended stop portion provided on the sloped stop block and the turning feed channel together form a feeding channel, and the angle between the feeding channel and the straight feed channel is greater than 90°.

[0012] As a preferred technical solution of the present invention, it also includes a pad, which is connected to the side of the feed base facing the aluminum wire mold seat, the aluminum wire mold seat is clamped between the pad and the feed base, and the pad is provided with a first air avoidance hole corresponding to the second material channel hole.

[0013] As a preferred technical solution of the present invention, it also includes a fixed mold base, which is connected to the side of the feed base facing the aluminum wire mold base, and a second mounting groove is provided on the side of the fixed mold base facing the feed base, and the pad is clamped between the second mounting groove and the feed base. A second air avoidance hole is opened on the fixed mold base, and the second air avoidance hole is connected to the first air avoidance hole.

[0014] As a preferred technical solution of the present invention, the fixed mold base is connected to the feed base by bolts.

[0015] As a preferred technical solution of the present invention, the fixed mold base is provided with two lifting ring holes for connecting external lifting rings.

[0016] As a preferred technical solution of the present invention, a static-eliminating fan is provided on the side of the fixed mold base away from the aluminum wire mold base, and the static-eliminating fan is used to deliver anti-static cold air, and its air outlet direction is toward the second air-avoiding hole.

[0017] As a preferred technical solution of the present invention, the inclined surface stop block is connected to the feed base by bolts.

[0018] The beneficial effects of the present invention are:

[0019] The present invention arranges a feed base coaxially and connects with an aluminum wire die base, and opens a first feed channel hole in the feed base to guide the aluminum material into the die; opens a second feed channel hole on the aluminum wire die base, and the hole diameter of the second feed channel hole directly determines the diameter of the final aluminum welding wire. The first feed channel hole and the second feed channel hole form a continuous extrusion channel, thereby realizing precise control of the diameter. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] In order to facilitate understanding by those skilled in the art, the present invention is further described below with reference to the accompanying drawings.

[0021] Figure 1 This is a schematic diagram of a first three-dimensional structure of a continuous extrusion die for aluminum wire according to the present invention;

[0022] Figure 2 It is a second three-dimensional structural schematic diagram of a continuous extrusion die for aluminum wire of the present invention;

[0023] Figure 3 A first exploded view of a continuous extrusion die for aluminum wire according to the present invention;

[0024] Figure 4 A second exploded view of a continuous extrusion die for aluminum wire according to the present invention;

[0025] Figure 5 A cross-sectional view of a continuous extrusion die for aluminum wire according to the present invention;

[0026] Figure 6 This is a schematic diagram of the three-dimensional structure of a feed base of a continuous extrusion die for aluminum wire according to the present invention;

[0027] Figure 7 It is a schematic diagram of the three-dimensional structure of an aluminum wire die base of a continuous extrusion die for aluminum wire according to the present invention;

[0028] Figure 8 This is a schematic diagram of the three-dimensional structure of an inclined surface stopper block of a continuous extrusion die for aluminum wire according to the present invention;

[0029] Fig. 9 This is a schematic diagram of the three-dimensional structure of a backing plate of a continuous extrusion die for aluminum wire according to the present invention;

[0030] Fig.10 It is a schematic diagram of the three-dimensional structure of a fixed die base of a continuous extrusion die for aluminum wire of the present invention;

[0031] Description of main symbols

[0032] In the figure: 1. Feed base; 11. First material channel hole; 111. Turning feed channel; 112. Straight feed channel; 113. Feed channel; 12. Mounting cavity; 13. First mounting groove; 2. Aluminum wire mold base; 21. Second material channel hole; 211. Flow promotion part; 22. Hemispherical flow blocking block; 3. Inclined material blocking block; 31. Extended material blocking part; 4. Pad; 41. First air avoidance hole; 5. Fixed mold base; 51. Second mounting groove; 52. Second air avoidance hole; 53. Lifting ring hole. DETAILED DESCRIPTION

[0033] In order to further explain the technical means and effects adopted by the present invention to achieve the predetermined invention purpose, the specific implementation methods, structures, features and effects of the present invention are described in detail below in conjunction with the accompanying drawings and preferred embodiments.

[0034] See also Figure 1-10 The present embodiment provides a continuous extrusion die for aluminum wire, comprising a feed base 1 and an aluminum wire die base 2 which are coaxially arranged and connected. The feed base 1 is provided with a first material channel hole 11 along the axial direction, and a mounting cavity 12 is provided on the side of the feed base 1 facing the aluminum wire die base 2. The mounting cavity 12 is connected to the first material channel hole 11 and is coaxial. The aluminum wire die base 2 is installed in the mounting cavity 12; a plurality of second material channel holes 21 which are connected to the mounting cavity 12 are provided on the aluminum wire die base 2, and the aperture of the second material channel hole 21 is 1.2 mm-2 mm.

[0035] In order to solve the problems of complicated procedures and long production cycles in the traditional production process of aluminum welding wire, the present invention realizes one-step forming of aluminum wire by adopting continuous extrusion technology, reduces the need for multiple drawing and annealing treatments, thereby improving production efficiency and reducing production costs. Specifically, when using the continuous extrusion die of the present invention, the aluminum material enters the feed base 1 through the first material channel hole 11 under pressure, and is then continuously extruded and differentiated through multiple second material channel holes 21 on the aluminum wire die base 2 to form aluminum wire with a diameter of 1.2mm-2mm, reducing the multiple drawing and annealing processes in the traditional small-diameter aluminum wire manufacturing process, and significantly improving the production efficiency of aluminum welding wire. It should be noted that the diameter of the second material channel hole 21 in this embodiment can be 1.2mm, 2mm, 1.5mm or 1.7mm. Preferably, six second material channel holes 21 are provided in this embodiment.

[0036] Furthermore, in the continuous extrusion process of the aluminum wire, in order to ensure that the aluminum material can flow into each second material channel hole 21 evenly and stably, and avoid the formation of turbulence or eddy current inside the mold, thereby causing inconsistent extrusion quality of the aluminum wire, a hemispherical baffle block 22 is provided on the side of the aluminum wire die base 2 facing the feed base 1. The hemispherical baffle block 22 is coaxially arranged with the aluminum wire die base 2, and a plurality of second material channel holes 21 are evenly arranged around the hemispherical baffle block 22. During the operation of the mold, the aluminum material first enters the installation cavity 12 through the first material channel hole 11 of the feed base 1, and then, under the guidance and distribution of the hemispherical baffle block 22, the aluminum material is evenly dispersed to the entrance of each second material channel hole 21. Under the action of pressure, the aluminum material is continuously extruded through the second material channel hole 21 to form an aluminum wire of the required diameter. During the whole process, the hemispherical baffle block 22 ensures the smooth and uniform flow of the aluminum material, avoids the formation of turbulence and eddy current, thereby improving the stability of the extrusion process and the product quality of the aluminum welding wire. In addition, the hemispherical flow-block 22 also has a certain flow-blocking effect and can adjust the flow rate and flow velocity of the aluminum material.

[0037] Specifically, during the continuous extrusion of the aluminum wire, in order to further improve the flow performance of the aluminum material in the mold, reduce the flow resistance, and ensure that the aluminum material can more smoothly enter the second material channel hole 21 and be extruded, in this embodiment, the second material channel hole 21 is connected to one end of the mounting cavity 12 and is provided with a flow-promoting portion 211. The flow-promoting portion 211 is a smooth curved surface whose diameter gradually decreases from the surface of the aluminum wire die base 2 toward the second material channel hole 21. The smooth curved surface can effectively guide the aluminum material to flow toward the second material channel hole 21, reduce the resistance and eddy current phenomenon during the flow process, and enable the aluminum material to enter the second material channel hole 21 more smoothly. In addition, since the diameter of the flow-promoting portion 211 gradually decreases, the contact area between the aluminum material and the inner wall of the mold during the flow process is also gradually reduced, thereby reducing the friction resistance and facilitating the rapid flow of the aluminum material.

[0038] Furthermore, the present invention also includes a bevel stop block 3, and a first mounting groove 13 is provided on the side of the feed base 1 away from the mounting cavity 12. The first mounting groove 13 is located next to the first material channel hole 11, and the bevel stop block 3 is installed in the first mounting groove 13; the first material channel hole 11 includes a turning feed channel 111 close to the bevel stop block 3 and a straight feed channel 112 close to the mounting cavity 12, and the side wall of the turning feed channel 111 away from the bevel stop block 3 gradually turns and extends in the direction away from the bevel stop block 3, and the extended stop part 31 provided on the bevel stop block 3 and the turning feed channel 111 together form a feed channel 113, and the angle between the feed channel 113 and the straight feed channel 112 is greater than 90°. It can be understood that before entering the straight feed channel 112, the aluminum material first goes through a gradual turning process, which helps to slow down the flow rate of the aluminum material and reduce its impact force, thereby avoiding blockage and turbulence in the feed channel. The angle between the feed channel 113 and the straight feed channel 112 is greater than 90°, which can further disperse the flow direction of the aluminum material, making the aluminum material more uniform and stable when entering the straight feed channel 112. The large angle also helps to reduce the energy loss of the aluminum material during the turning process and improve the feeding efficiency.

[0039] Furthermore, the present invention further comprises a backing plate 4, which is connected to the side of the feed base 1 facing the aluminum wire die base 2, and the aluminum wire die base 2 is sandwiched between the backing plate 4 and the feed base 1, and the backing plate 4 is provided with a first avoidance hole 41 corresponding to the second material channel hole 21. In this embodiment, the first avoidance hole 41 corresponds to the second material channel hole 21 one by one.

[0040] Furthermore, the present invention also includes a fixed die base 5, which is connected to the side of the feed base 1 facing the aluminum wire die base 2, and a second mounting groove 51 is provided on the side of the fixed die base 5 facing the feed base 1, and the pad 4 is clamped between the second mounting groove 51 and the feed base 1, and a second air avoidance hole 52 is provided on the fixed die base 5, and the second air avoidance hole 52 is connected to the first air avoidance hole 41. Optionally, the second air avoidance hole 52 can be provided in a one-to-one correspondence with the first air avoidance hole 41. In this embodiment, one second air avoidance hole 52 is provided, and the second air avoidance hole 52 covers all the first air avoidance holes 41, so that the discharge of the first air avoidance holes 41 will not be blocked.

[0041] Specifically, the fixed die base 5 is connected to the feed base 1 by bolts. It is understandable that bolt connection is a reliable and strong connection method, which can effectively fix the fixed die base 5 and the feed base 1 tightly together, ensuring that the mold will not loosen or shift during the extrusion process, thereby ensuring the overall stability and operational reliability of the mold. When the mold parts need to be replaced or repaired, it can be easily disassembled and assembled by simply loosening the bolts. In addition, since the pad 4 is installed between the fixed die base 5 and the feed base 1, the tightening force of the bolt connection can be controlled by adjusting the tightening degree of the bolts to apply different degrees of extrusion force to the pad 4. This flexibility enables the continuous extrusion die of this embodiment to better adapt to the extrusion requirements of aluminum materials of different specifications and materials.

[0042] Specifically, the inclined surface blocking block 3 is connected to the feed base 1 by bolts.

[0043] Furthermore, in order to facilitate the overall lifting of the mold and reduce the difficulty and risk of manual handling, the present embodiment provides two lifting ring holes 53 on the fixed mold base 5 for connecting external lifting rings, so that the mold can be hoisted as a whole after installation, which is convenient for movement. When the lifting ring is lifted by an external lifting device (such as a crane or a crane), the force is transmitted to the lifting ring hole 53 through the lifting ring, and then dispersed to the entire structure of the fixed mold base 5, thereby realizing the overall lifting of the mold.

[0044] Furthermore, during the continuous extrusion of aluminum wire, the surface temperature of the newly extruded aluminum wire is relatively high due to the plastic deformation under high temperature and high pressure. At the same time, due to the friction and contact between metals, static electricity accumulation may also occur, and both high temperature and static electricity may have an adverse effect on the quality of the aluminum wire, subsequent processing and production environment. Therefore, in this embodiment, a static electricity removal fan is provided on the side of the fixed mold base 5 away from the aluminum wire mold base 2. The static electricity removal fan is used to transport anti-static cold air, and its air outlet direction is toward the second air-avoiding hole 52. During operation, the static electricity removal fan will continue to work and transport cold air to the aluminum wire outlet, that is, the orifice of the second air-avoiding hole 52. When the cold air contacts the high-temperature aluminum wire that has just been extruded, it will quickly take away the heat on its surface and reduce its temperature. At the same time, it will also react with the static charge on the surface of the aluminum wire, thereby reducing the accumulation of static electricity. The entire cooling and static electricity removal process is carried out simultaneously with the extrusion process of the aluminum wire, without the need for additional shutdown operations, thereby improving production efficiency.

[0045] It is understandable that the present invention realizes the continuous extrusion and differentiation molding of aluminum materials under pressure by designing the coaxially arranged feed base 1 and aluminum wire die base 2, as well as the reasonably arranged second material channel hole 21 and hemispherical flow block 22, and realizes the one-step molding of 1.2mm-2mm aluminum wire, reducing the dependence on multiple drawing and annealing treatments. At the same time, the design of the inclined surface stop block 3 and the flow promotion part 211 is used to improve the flow performance of the aluminum material in the mold, reduce the flow resistance and eddy current phenomenon. In addition, the introduction of the anti-static fan effectively solves the high temperature and static electricity problems in the aluminum wire extrusion process, further improving the product quality.

[0046] The above description is only a preferred embodiment of the present invention and does not limit the present invention in any form. Although the present invention has been disclosed as a preferred embodiment as above, it is not used to limit the present invention. Any technical personnel in this field can make some changes or modify the technical contents disclosed above into equivalent embodiments without departing from the scope of the technical solution of the present invention. However, any brief modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention without departing from the content of the technical solution of the present invention are still within the scope of the technical solution of the present invention.

Claims

1. A continuous extrusion die for aluminum wire, characterized in that: It includes a feed base and an aluminum wire die base that are coaxially arranged and connected, the feed base is provided with a first material channel hole along the axial direction, the feed base is provided with an installation cavity on the side facing the aluminum wire die base, the installation cavity is connected to the first material channel hole and is coaxial, and the aluminum wire die base is installed in the installation cavity; the aluminum wire die base is provided with a plurality of second material channel holes that are connected to the installation cavity, and the aperture of the second material channel hole is 1.2mm-2mm.

2. The continuous extrusion die for aluminum wire according to claim 1, characterized in that: A hemispherical baffle is arranged on one side of the aluminum wire die seat facing the feed base, the hemispherical baffle is coaxially arranged with the aluminum wire die seat, and a plurality of the second material channel holes are evenly arranged around the hemispherical baffle.

3. The continuous extrusion die for aluminum wire according to claim 2, characterized in that: One end of the second material channel hole connected to the installation cavity is provided with a flow-promoting portion, and the flow-promoting portion is a smooth curved surface whose diameter gradually decreases from the surface of the aluminum wire die seat toward the second material channel hole.

4. The continuous extrusion die for aluminum wire according to claim 1, characterized in that: It also includes a sloped material stopper block, a first mounting groove is provided on the side of the feed base away from the mounting cavity, the first mounting groove is located next to the first material channel hole, and the sloped material stopper block is installed in the first mounting groove; the first material channel hole includes a turning feed channel close to the sloped material stopper block and a straight feed channel close to the mounting cavity, the turning feed channel gradually turns and extends away from the sloped material stopper block from the side wall thereof, the extended material stopper portion provided on the sloped material stopper block and the turning feed channel together form a feeding channel, and the angle between the feeding channel and the straight feeding channel is greater than 90°.

5. The continuous extrusion die for aluminum wire according to claim 1, characterized in that: It also includes a pad, which is connected to the side of the feed base facing the aluminum wire mold base, the aluminum wire mold base is clamped between the pad and the feed base, and the pad is provided with a first avoidance hole corresponding to the second material channel hole.

6. The continuous extrusion die for aluminum wire according to claim 5, characterized in that: It also includes a fixed mold base, which is connected to the side of the feed base facing the aluminum wire mold base, and a second installation groove is provided on the side of the fixed mold base facing the feed base. The pad is clamped between the second installation groove and the feed base, and a second air avoidance hole is opened on the fixed mold base, and the second air avoidance hole is connected to the first air avoidance hole.

7. The continuous extrusion die for aluminum wire according to claim 6, characterized in that: The fixed mold base is connected to the feed base through bolts.

8. The continuous extrusion die for aluminum wire according to claim 6, characterized in that: The fixed die base is provided with two lifting ring holes for connecting external lifting rings.

9. The continuous extrusion die for aluminum wire according to claim 6, characterized in that: A static-eliminating fan is arranged on one side of the fixed mold base away from the aluminum wire mold base. The static-eliminating fan is used to deliver anti-static cold air, and its air outlet direction is toward the second air-avoiding hole.

10. The continuous extrusion die for aluminum wire according to claim 4, characterized in that: The inclined surface blocking block is connected to the feeding base through bolts.

Citation Information

Patent Citations

  • Continuously extruding method and extruding device of non-radial feeding

    CN103111481A

  • Continuous cladding method and device of obtuse angle flowing channel

    CN103121043A

  • Large thin-wall square tube extrusion mold

    CN104942033A

  • Multi-channel rotary extrusion grain refining device and magnesium alloy superfine-diameter wire extrusion method

    CN118237422A

  • Alloy filament preparation facilities

    CN204747096U