Manufacturing process of ultra-large wall thickness ring forge piece

By installing an integrated core rolling mold on the ring rolling machine for overall rolling of super-large wall-thick ring forgings, the problems of low structural strength and material utilization in traditional processes are solved, and an efficient and low-cost production process is achieved, and processing is simplified. Steps and improve productivity.

CN118905120APending Publication Date: 2024-11-08SHANDONG IRAETA HEAVY IND
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411072204.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-06
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

In the traditional manufacturing process of ultra-large wall thickness ring forgings, due to the large edge width, the connection between the inner ring and the outer ring is weak, which reduces the structural strength, and the processing process is complex, the material utilization rate is low, the cost is high, and the production cycle is long.

Method used

The integrated core roll mold is installed on the rolling ring mill for forging. The grooves and connecting keys of the core roll mold are used to realize the overall rolling of the forging blank, breaking through the maximum rolling capacity of the equipment, ensuring structural strength, reducing material waste and subsequent mechanical processing Steps to shorten the production cycle.

Benefits of technology

High-strength molding of ultra-large wall-thick ring forgings is achieved, reducing material waste and processing time, reducing production costs, improving production efficiency and simplifying the processing process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118905120A_ABST
    Figure CN118905120A_ABST
Patent Text Reader

Abstract

The invention provides a manufacturing process for an ultra-large-wall-thickness ring forged piece, and relates to the technical field of large forged piece processes. According to the technology, the characteristics of existing equipment and ultra-large wall thickness ring forgings are combined, an original core roller is sleeved with an integrated core roller mold, the maximum rolling capacity of the original equipment is broken through, integrated forming is achieved, the structural strength is guaranteed, material waste is reduced, the material utilization rate is increased, and the production cost is reduced. The subsequent machining steps and workload are reduced, and the machining time and cost are saved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of large forging technology, in particular to a manufacturing process of a super-large wall thickness ring forging. Background Art

[0002] With the progress of the times and the development of society, tunnels and underground projects have received more and more attention from people and are widely used in transportation and logistics, municipal facilities, water conservancy and hydropower, resource storage, mineral development, national defense construction and other fields. A large number of new technologies, new processes, new equipment, new materials and even new engineering theories and concepts have emerged in an endless stream, and mechanical equipment in related fields has gradually developed towards large-scale and heavy-duty. As a key component in the equipment, the application of ultra-thick ring forgings that withstand alternating loads is becoming more and more extensive.

[0003] The so-called super-thickness ring forgings refer to ring forgings with a large difference between the inner diameter and the outer diameter (i.e., a large side width) (such as Figure 1 As shown in the figure, it is usually used as the cutter head flange and drive box flange of the shield machine. As a key supporting component in the shield machine, its manufacturing and testing require high precision and strict quality control to ensure the efficient and safe operation of the shield machine.

[0004] Forgings are ideal for flange manufacturing due to their uniform internal structure and no welding defects. However, due to the large side width of the super thick ring forgings, it has exceeded the limit size of the ring rolling machine. To address this problem, the traditional approach is as follows Figure 2 As shown in the figure, the super thick ring forging is divided into two parts, the inner ring and the outer ring, which are both forgings, and then the inner ring and the outer ring are connected by welding to form the super thick ring forging. In this method, although the inner ring and the outer ring are forgings with good internal uniformity and mechanical properties, the connection between the two is relatively weak, which reduces the structural strength of the entire super thick ring forging. Summary of the invention

[0005] In view of the above problems, the present application provides a manufacturing process for ultra-large wall thickness ring forgings, which can complete the processing of ultra-large wall thickness ring forgings on the basis of existing ring rolling machines to form ultra-large wall thickness ring forgings.

[0006] The technical solution adopted by the present invention to solve the technical problem is:

[0007] A manufacturing process for a super thick wall ring forging comprises the following steps:

[0008] First, the steel ingot forging process;

[0009] Second, the steel ingot after forging is roughened, stretched and punched to obtain a forging blank with a hole in the center;

[0010] Third, the forging blank obtained in the second step is expanded;

[0011] Fourth, rolling the forging blank obtained in the third step;

[0012] 4.1 Install the core roller mold on the core roller of the ring rolling machine;

[0013] The core roller mold is coaxially sleeved on the outside of the core roller of the ring rolling machine, and a groove is provided on the outer side of the core roller mold;

[0014] 4.2 The forging blank obtained in the third step is placed on a ring rolling machine, a core roller equipped with a core roller mold is inserted into the inner hole of the forging blank, the inner ring end of the forging blank is inserted into the groove of the core roller mold, the outer ring end of the forging blank is against the driving roller of the ring rolling machine, and the end of the outer ring end of the forging blank facing away from the driving roller is extended between two end face rollers for rolling, and finally a forging blank is obtained;

[0015] Fifth, the forging blank obtained in the fourth step is subjected to post-forging heat treatment.

[0016] Furthermore, the forging blank obtained in the fifth step is machined in sequence to obtain a ring forging with dimensions that meet the requirements.

[0017] Furthermore, a shoulder is provided on the core roller of the ring rolling machine, the lower end surface of the core roller mold abuts against the shoulder of the core roller, a connecting key is provided on the core roller, and a keyway matching the connecting key is provided on the inner cylindrical surface of the core roller mold.

[0018] Furthermore, a hoisting hole is arranged on the upper end surface of the core roller mold.

[0019] Furthermore, the plurality of hoisting holes are evenly arranged in a circumferential direction around the inner hole of the core roller mold.

[0020] Furthermore, when the steel ingot is forged, the steel ingot is first heated, chamfered and rounded, and then returned to the furnace for heat preservation after the water riser is removed.

[0021] Furthermore, the temperature of the furnace is 1250±20°C, and the insulation time is 8 to 12 hours.

[0022] Furthermore, in the second step, after roughening, the steel is returned to the furnace for insulation at 1250±20°C for 3 to 7 hours and then stretched.

[0023] Furthermore, during the hole expansion process, both ends of the forging blank are leveled so that the height of the forging blank is less than or equal to the width of the groove on the core roller mold.

[0024] The beneficial effects of the present invention are:

[0025] The manufacturing process of a super-thick ring forging provided in the embodiment of the present application combines the characteristics of existing equipment and super-thick ring forgings. By setting an integrated core roller mold on the original core roller, it not only breaks through the maximum rolling capacity of the original equipment, realizes one-piece molding, ensures structural strength, but also reduces material waste, improves material utilization, reduces the steps and workload of subsequent mechanical processing, and saves processing time and cost. Compared with the method of forging super-thick ring forgings through traditional free forging technology, the present invention uses a specific integrated mold forging and rolling based on the traditional forging process, breaking through the maximum processing limit of the equipment, and the mold matching is high. While saving production costs, it shortens the production cycle of forgings and improves production efficiency. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 It is a schematic diagram of the structure of a super thick wall ring forging;

[0027] Figure 2 This is a schematic diagram of the structure of the traditional production of extra-large wall thickness ring forgings;

[0028] Figure 3 A schematic diagram of a manufacturing process for a super thick wall ring forging provided in an embodiment of the present application;

[0029] Figure 4 is a top view of the core roller mold;

[0030] Figure 5 is a cross-sectional view of a core roller mold;

[0031] Figure 6 This is a schematic diagram of the installation structure of the core roller mold;

[0032] Figure 7 for Figure 6 A schematic diagram of the enlarged structure of part A;

[0033] Figure 8 A processing diagram of a manufacturing process of an ultra-thick wall ring forging provided in an embodiment of the present application;

[0034] Fig. 9 A cross-sectional view of a ring forging obtained by using a manufacturing process for a super-thick ring forging provided in an embodiment of the present application;

[0035] Fig.10 This is a cross-sectional view of a conventional ring forging.

[0036] In the figure: 1. Extra-thick wall ring forging; 11. Inner ring; 12. Outer ring; 21. Driving roller; 22. Core roller; 221. Connecting key; 222. Shoulder; 23. End roller; 3. Core roller mold; 31. First shaft section; 32. Second shaft section; 33. Third shaft section; 34. Groove; 35. Keyway; 36. Lifting hole. DETAILED DESCRIPTION

[0037] In order to enable those skilled in the art to better understand the technical solutions in the present application, the technical solutions in the embodiments of the present application will be described in detail below in conjunction with the drawings in the embodiments of the present application, and the described embodiments are only part of the embodiments of the present application, not all of the embodiments. All other embodiments obtained by those skilled in the art without creative work on the basis of the embodiments of the present application shall belong to the protection scope of the present application.

[0038] A manufacturing process of an ultra-thickness ring forging 1 comprises the following steps:

[0039] First, the steel ingot is forged. The steel ingot is heated by a hydraulic press, then chamfered and rounded, and then returned to the furnace for heat preservation after the water riser is removed.

[0040] The temperature of the furnace is 1250±20℃, and the insulation time is 8 to 12 hours.

[0041] Secondly, the steel ingot after forging is roughened, stretched and punched to obtain a forging blank with a hole in the center.

[0042] After roughening, it needs to be returned to the furnace and kept warm at 1250±20℃ for 3 to 7 hours before stretching.

[0043] Third, the forging blank obtained in the second step is expanded by a horse frame.

[0044] During the expansion process, the two ends are properly leveled according to the actual forging height growth. During leveling, the height of the forging blank should be strictly controlled within the required range to avoid mutual influence between the core roller mold 3 and the forging blank, thereby avoiding damage to the core roller mold 3 and the forging blank itself. Figure 5 As shown, the height of the forging blank is smaller than the width M of the groove 34 of the core roller mold 3.

[0045] Fourth, the forging billet obtained in the third step is rolled.

[0046] 4.1 Install the core roller mold 3 on the core roller 22 of the ring rolling machine.

[0047] like Figure 4 and Figure 5As shown, the core roller mold 3 is coaxially sleeved on the outside of the core roller 22 of the ring rolling machine, and the outer side surface of the core roller mold 3 includes a first shaft section 31, a second shaft section 32 and a third shaft section 33 from top to bottom, the diameter of the second shaft section 32 is smaller than the diameters of the first shaft section 31 and the third shaft section 33, and the first shaft section 31, the second shaft section 32 and the third shaft section 33 together form an annular groove 34. That is, the outer side surface of the core roller mold 3 is a dumbbell-shaped structure with a thin center and thick ends, and the rotary cross section of the core roller mold 3 is a U-shaped structure with an opening facing outward (the side away from the axis is the outer side). Preferably, the diameter of the first shaft section 31 is equal to the diameter of the third shaft section 33.

[0048] As a specific implementation method, Figure 6 and Figure 7 As shown, in this embodiment, the core roller 22 of the ring rolling machine is provided with a shoulder 222, the core roller mold 3 is sleeved on the core roller 22 of the ring rolling machine, and the lower end surface of the core roller mold 3 abuts against the shoulder 222 of the core roller 22. The core roller 22 is provided with a connecting key 221, and the inner cylindrical surface of the core roller mold 3 is provided with a keyway 35 that axially penetrates the core roller mold 3, and the connecting key 221 cooperates with the keyway 35 to limit the freedom of rotation of the core roller mold 3 relative to the core roller 22.

[0049] Furthermore, in order to facilitate installation, Figure 4 and Figure 5 As shown, a hoisting hole 36 is provided on the upper end surface of the core roller mold 3. As a specific implementation, in this embodiment, a plurality of hoisting holes 36 are provided on the upper end surface of the core roller mold 3, and the plurality of hoisting holes 36 are evenly arranged along the circumferential direction around the inner hole of the core roller mold 3. Exemplarily, the hoisting hole 36 is a screw hole, and three hoisting holes 36 are provided on the upper end surface of the core roller mold 3.

[0050] 4.2 The forging blank obtained in the third step is placed on the ring rolling machine, and the core roller 22 equipped with the core roller mold 3 is inserted into the inner hole of the forging blank. The inner ring end (i.e., the end close to the inner hole) of the forging blank is inserted into the groove 34 of the core roller mold 3, and the outer ring end (the end radially away from the inner hole) of the forging blank is pressed against the driving roller 21 of the ring rolling machine under the extrusion of the core roller 22, and the forging blank rotates under the driving action of the driving roller 21. The end of the outer ring end of the forging blank facing away from the driving roller 21 extends between the two end rollers 23, and the two end rollers 23 squeeze each other to roll the forging blank to obtain a forging blank.

[0051] Fifth, the forging blank obtained in the fourth step is subjected to post-forging heat treatment.

[0052] Sixth, the forging blank obtained in the fifth step is subjected to semi-finishing, ultrasonic testing, physical and chemical testing and finishing in sequence, and finally an extra-large wall thickness ring forging 1 with dimensions meeting the requirements is obtained.

[0053] like Figure 8 As shown, the core roller mold 3 itself can control the longitudinal deformation of the inner ring end of the forging billet during the rolling process, and finally obtain the following Fig. 9 The ultra-thick ring forging 1 with a small step is shown. The traditional method of splicing is used to produce the ultra-thick ring forging 1. After obtaining the forging blank, it needs to be machined once. After splicing, in order to remove the weld, the welding surface needs to be machined twice. Therefore, during forging, it is necessary to reserve two machining allowances on the welding surface, such as Fig.10 The thickness shown is B. The present application provides a manufacturing process for a super thick ring forging 1 that can complete the integrated processing of the super thick ring forging 1 without splicing, so only one machining margin needs to be reserved at the outer end of the original welding surface position, such as Fig. 9 The thickness shown is A, and the inner end of the original welding surface position will not grow too much under the restriction of the core roller mold 3. Fig. 9 and Fig.10 It can be seen that, compared with the traditional method, the forging blank obtained by the manufacturing process of the ultra-thick ring forging 1 provided by the present application is closer to the finished product, and the removed part is less ( Fig. 9 The dotted line frame part is the saving part), which can not only save materials and reduce costs, but also reduce machining time and improve machining efficiency.

[0054] Other embodiments obtained by those skilled in the art by combining, splitting, reorganizing, etc. the embodiments of the present application on the basis of the embodiments provided in the present application do not exceed the protection scope of the present application.

[0055] The above specific implementation methods have detailed the purpose, technical solutions and beneficial effects of the embodiments of the present application. The above are only specific implementation methods of the embodiments of the present application and are not used to limit the protection scope of the embodiments of the present application. That is, any modifications, equivalent substitutions, improvements, etc. made on the basis of the embodiments of the present application should be included in the protection scope of the embodiments of the present application.

Claims

1. A manufacturing process for a super thick ring forging, characterized in that: The following steps are included: First, the steel ingot forging process; Second, the steel ingot after forging is roughened, stretched and punched to obtain a forging blank with a hole in the center; Third, the forging blank obtained in the second step is expanded; Fourth, rolling the forging blank obtained in the third step; 4.1 Installing a core roller mold (3) on a core roller (22) of a ring rolling machine; The core roller mold (3) is coaxially sleeved on the outside of the core roller (22) of the ring rolling machine, and a groove (34) is provided on the outer side surface of the core roller mold (3); 4.2 The forging blank obtained in the third step is placed on a ring rolling machine, a core roller (22) equipped with a core roller mold (3) is inserted into the inner hole of the forging blank, the inner ring end of the forging blank is inserted into the groove (34) of the core roller mold (3), the outer ring end of the forging blank is abutted against the driving roller (21) of the ring rolling machine, and the end of the outer ring end of the forging blank facing away from the driving roller (21) is extended between two end face rollers (23) for rolling, and finally a forging blank is obtained; Fifth, the forging blank obtained in the fourth step is subjected to post-forging heat treatment.

2. The manufacturing process of the super thick wall ring forging according to claim 1 is characterized in that: The forging blank obtained in the fifth step is machined in sequence to obtain a ring forging with dimensions that meet the requirements.

3. The manufacturing process of the super thick wall ring forging according to claim 1 is characterized in that: The core roller (22) of the ring rolling machine is provided with a shoulder (222), the lower end surface of the core roller mold (3) abuts against the shoulder (222) of the core roller (22), the core roller (22) is provided with a connecting key (221), and the inner cylindrical surface of the core roller mold (3) is provided with a keyway (35) matching with the connecting key (221).

4. The manufacturing process of the super thick wall ring forging according to claim 1 is characterized in that: A hoisting hole (36) is provided on the upper end surface of the core roller mold (3).

5. The manufacturing process of the super thick wall ring forging according to claim 4 is characterized in that: The plurality of lifting holes (36) are evenly arranged in a circumferential direction around the inner hole of the core roller mold (3).

6. The manufacturing process of the super thick wall ring forging according to claim 1 is characterized in that: When forging the steel ingot, the ingot is first heated, chamfered and rounded, and then returned to the furnace for heat preservation after the water riser is removed.

7. A process for manufacturing a super thick wall ring forging according to claim 6, characterized in that: The temperature of the furnace is 1250±20℃, and the insulation time is 8 to 12 hours.

8. The manufacturing process of the super thick wall ring forging according to claim 1 is characterized in that: In the second step, after roughening, the steel is returned to the furnace for insulation at 1250±20℃ for 3 to 7 hours and then stretched.

9. The manufacturing process of the super thick wall ring forging according to claim 1 is characterized in that: During the hole expansion process, both ends of the forging blank are leveled so that the height of the forging blank is less than or equal to the width of the groove (34) on the core roller mold (3).

Citation Information

Patent Citations

  • Near-net forming manufacturing process for hundred-ton special-shaped section ring forge piece

    CN113182470A

  • Radial-axial multi-roller collaborative near-net rolling forming method for large outer contour sharp variable ring piece

    CN114535472A

  • Split type ring rolling machine core roller and forming process for rolling concave ring piece

    CN115780705A

  • Rolling forming process for cylinder with ultra-large specification and ultra-large wall thickness

    CN116786739A