Method and system for preparing communication mold based on magnesium alloy semi-solid state
Through the composition optimization and process processing of semi-solid materials of magnesium alloy, the shortcomings in strength, corrosion resistance and precision control of traditional mold preparation methods are solved, and communication mold preparation is achieved with high strength, high toughness and precision.
Patent Information
- Application Number
- CN202411186719.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-28
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2044-08-28
AI Technical Summary
Traditional communication mold preparation methods have the inability to meet the needs of complex equipment in terms of strength, corrosion resistance and weight, and conventional manufacturing processes have shortcomings in precision control, complex structure forming and production cycle.
Using magnesium alloy semi-solid material, communication molds with high strength, high toughness and precision are prepared through composition ratio analysis, liquid phase distribution state and solid phase particle distribution state, combined with furnace, stirring, cooling and die-casting processes. And carry out defect detection and repair.
The performance improvement of communication molds is achieved, ensuring that the mold has consistent performance in different parts, improving the strength and toughness of the molds, and avoiding the generation of bad products.
Smart Images

Figure CN118905178A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of mold preparation, and in particular to a method for preparing a communication mold based on a semi-solid magnesium alloy. Background Art
[0002] Magnesium alloy semi-solid communication mold is a mold used to manufacture magnesium alloy semi-solid parts. Magnesium alloy semi-solid forming technology is a new type of metal forming technology that combines the advantages of casting and forging to produce high-precision, high-strength and high-toughness parts. Communication molds are molds used to manufacture communication equipment parts, such as mobile phone housings, antennas, etc. Using magnesium alloy semi-solid communication molds can produce lighter, higher-strength communication equipment parts, improving the performance and quality of communication equipment.
[0003] At present, the traditional communication mold preparation method mainly relies on a single metal material and conventional manufacturing processes. Although these methods can produce communication molds to a certain extent, they have obvious limitations. Among them, a single metal material may not be able to meet the increasingly complex communication equipment requirements in terms of strength, corrosion resistance and weight; conventional manufacturing processes may have deficiencies in precision control, complex structure molding and production cycle. Therefore, a communication mold preparation method based on semi-solid magnesium alloy is needed to improve the performance of the mold. Summary of the invention
[0004] In order to solve the above problems, the present invention provides a method for preparing a communication mold based on a semi-solid magnesium alloy, and the present invention can improve the performance of the communication mold.
[0005] In a first aspect, the present invention provides a method for preparing a communication mold based on a semi-solid magnesium alloy, comprising: Acquire the prepared material of the communication mold, analyze the composition ratio of the prepared material, and obtain the target material when the composition ratio meets the preset ratio, wherein the prepared material refers to a magnesium alloy semi-solid material; Dissolving the target material in a preconfigured furnace to obtain a liquid material, analyzing a liquid phase distribution state of the liquid material, and obtaining a first processed material when the liquid phase distribution state meets a preset state; Using a pre-configured stirring device to stir the first processed material to obtain a stirred material, analyzing the solid phase particle distribution state of the stirred material, and obtaining a second processed material when the solid phase particle distribution state meets a preset state; The second processed material is cooled by a pre-configured cooling device, and when the second processed material is in a semi-solid state, the cooling is completed to obtain a third processed material, the third processed material is die-casted by a pre-configured die-casting device to obtain an initial mold, the initial mold is subjected to a toughness test, and when the toughness test result is excellent, a target mold is obtained, and the target mold is rough-processed to obtain a first processed mold; The first processing mold is subjected to defect detection. When the first processing mold has defects, the defects are repaired to obtain a repair mold. The repair mold is finely processed to obtain a target communication mold.
[0006] In a possible implementation of the first aspect, after analyzing the composition ratio of the prepared material, the method further includes: Query the measured proportion of each element in the prepared material; Based on the measured ratio, the variance test statistic of the magnesium alloy composition in the prepared material is calculated in combination with the following formula: in, represents the test statistic of magnesium alloy composition variance, A represents the A element in the magnesium alloy semi-solid material, represents the ideal ratio of A element, represents the measured proportion of element A, and B represents element B in the semi-solid material of magnesium alloy. represents the ideal ratio of B element, represents the measured proportion of element B, C represents the C element in the semi-solid material of magnesium alloy, represents the ideal ratio of C elements, represents the measured proportion of C element, N represents the N element in the semi-solid material of magnesium alloy, represents the ideal ratio of N elements, Indicates the measured proportion of N element.
[0007] In a possible implementation of the first aspect, dissolving the target material in a preconfigured furnace to obtain a liquid material includes: After adding the preconfigured inert gas into the preconfigured furnace, the preconfigured furnace is started to dissolve the target material; During the material dissolution process, the preconfigured furnace temperature is controlled within a preset range, and when the target material becomes liquid, a liquid material is obtained.
[0008] In a possible implementation of the first aspect, analyzing the liquid phase distribution state of the liquid material includes: collecting a surface image of the liquid material; Performing image enhancement processing on the surface image to obtain an enhanced image; Extracting the image texture and image shape of the enhanced image, and calculating the average diameter of particles in the liquid phase of the liquid material; The liquid phase distribution state of the liquid material is analyzed based on the image texture, the image shape and the average diameter.
[0009] In a possible implementation manner of the first aspect, analyzing the liquid phase distribution state of the liquid material based on the image texture, the image shape, and the average diameter includes: Calculating the distribution density and uniformity of particles in the liquid material based on the image texture and the image shape; Based on the distribution density, the uniformity and the average diameter, the distribution difference of the liquid material is calculated using the following formula: in, represents the distribution difference, represents the average diameter, represents the ideal mean diameter corresponding to the mean diameter, represents the distribution density, represents the ideal distribution density corresponding to the distribution density, Indicates uniformity, The uniformity corresponds to the ideal uniformity; Based on the distribution difference, the liquid phase distribution state of the liquid material is determined.
[0010] In a possible implementation of the first aspect, the using a preconfigured stirring device to stir the first processed material to obtain the stirred material includes: Obtaining a mixing process for mixing the material; Using the stirring process, setting the stirring speed and stirring time of the preconfigured stirring device; Based on the stirring speed and the stirring time, the first processed material is stirred using the preconfigured stirring device to obtain a stirred material.
[0011] In a possible implementation of the first aspect, analyzing the distribution state of solid phase particles of the stirred material includes: Acquiring a microscopic image of the stirred material; Identifying solid phase particles in the microscopic image, and marking the solid phase particles to obtain marked particles; Identifying the particle position, particle size and particle shape of the marked particles; The solid phase particle distribution state of the stirred material is determined based on the particle position, the particle size and the particle shape.
[0012] In a possible implementation of the first aspect, cooling the second processed material using a preconfigured cooling device, and completing cooling when the second processed material is in a semi-solid state to obtain a third processed material, comprises: Design cooling channels and layout water channels for the preconfigured cooling device to obtain a target cooling device; Setting parameters of the cooling medium corresponding to the target cooling device to obtain a set cooling medium; Cooling the second processed material using the target cooling device and the set cooling medium; When the second processed material is in a semi-solid state, cooling is completed to obtain a third processed material.
[0013] In a possible implementation manner of the first aspect, performing a toughness test on the initial mold includes: Querying the material properties of the initial mold; Analyzing the tensile strength of the initial mold according to the material properties; impact testing the initial mold based on the tensile strength; Based on the results of the impact test, the fracture toughness of the target metal plate and the weld is determined.
[0014] In a second aspect, the present invention provides a communication mold preparation system based on a semi-solid magnesium alloy, the system comprising: A component ratio analysis module, used to obtain the prepared material of the communication mold, analyze the component ratio of the prepared material, and obtain the target material when the component ratio meets the preset ratio, wherein the prepared material refers to a magnesium alloy semi-solid material; A liquid phase distribution analysis module, used for dissolving the target material using a pre-configured furnace to obtain a liquid material, analyzing the liquid phase distribution state of the liquid material, and obtaining a first processed material when the liquid phase distribution state meets a preset state; a solid phase particle distribution analysis module, configured to stir the first processed material using a pre-configured stirring device to obtain a stirred material, analyze the solid phase particle distribution state of the stirred material, and obtain a second processed material when the solid phase particle distribution state meets a preset state; A mold rough processing module is used to cool the second processing material using a pre-configured cooling device, and complete cooling when the second processing material is in a semi-solid state to obtain a third processing material, and to die-cast the third processing material using a pre-configured die-casting device to obtain an initial mold, and to perform a toughness test on the initial mold. When the test result of the toughness test is excellent, a target mold is obtained, and the target mold is rough-processed to obtain a first processing mold; The mold finishing module is used to perform defect detection on the first processing mold, and when the first processing mold has defects, perform defect repair on the first processing mold to obtain a repaired mold, and perform fine processing on the repaired mold to obtain a target communication mold.
[0015] Compared with the prior art, the technical principle and beneficial effects of this solution are: The embodiment of the present invention can obtain the basic material for preparing the mold by obtaining the preparation material of the communication mold, wherein the preparation material refers to a semi-solid material of a magnesium alloy, and the target material is dissolved by a pre-configured furnace to obtain a liquid material, so that the elements in the target material can be more fully mixed, so that the composition is more uniform, and the mold has consistent performance in different parts. Further, the embodiment of the present invention stirs the first processing material by using a pre-configured stirring device to obtain a stirred material, which can use the shear force generated by stirring to break the growing grains in the material, inhibit the growth of grains, thereby obtaining a finer grain structure, and improving the strength and toughness of the mold. Further, the embodiment of the present invention cools the second processing material by using a pre-configured cooling device, and completes cooling when the second processing material is semi-solid, and obtains a third processing material to obtain a solid material, so as to facilitate the processing of the communication mold, and the first processing mold is defect-detected to understand whether there are defects inside the first processing mold, such as cracks, uneven concave and convex conditions, to avoid the subsequent production of defective products. A method and system for preparing a communication mold based on a semi-solid magnesium alloy is proposed in the embodiment of the present invention, which can improve the performance of the communication mold. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] The accompanying drawings, which are incorporated in and constitute a part of this specification, illustrate embodiments consistent with the invention and, together with the description, serve to explain the principles of the invention.
[0017] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, for ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative labor.
[0018] Figure 1 A schematic flow chart of a method for preparing a communication mold based on a semi-solid magnesium alloy according to an embodiment of the present invention; Figure 2 A schematic diagram of a module of a communication mold preparation system based on a semi-solid magnesium alloy provided by an embodiment of the present invention. DETAILED DESCRIPTION
[0019] It should be understood that the specific embodiments described herein are only used to explain the present invention, and are not used to limit the present invention.
[0020] The embodiment of the present invention provides a method for preparing a communication mold based on a semi-solid state of a magnesium alloy, and the execution subject of the method for preparing a communication mold based on a semi-solid state of a magnesium alloy includes but is not limited to at least one of the electronic devices such as a server and a terminal that can be configured to execute the method provided by the embodiment of the present invention. In other words, the method for preparing a communication mold based on a semi-solid state of a magnesium alloy can be executed by software or hardware installed on a terminal device or a server device, and the software can be a blockchain platform. The server includes but is not limited to: a single server, a server cluster, a cloud server or a cloud server cluster, etc. The server can be an independent server, or it can be a cloud server that provides basic cloud computing services such as cloud services, cloud databases, cloud computing, cloud functions, cloud storage, network services, cloud communications, middleware services, domain name services, security services, content distribution networks (Content Delivery Network, CDN), and big data and artificial intelligence platforms.
[0021] See also Figure 1 FIG. 1 is a flow chart of a method for preparing a communication mold based on a semi-solid magnesium alloy according to an embodiment of the present invention. Figure 1 A method for preparing a communication mold based on a semi-solid magnesium alloy is described in the invention, comprising: S1. Obtaining materials for preparing a communication mold, analyzing the composition ratio of the materials for preparing, and obtaining target materials when the composition ratio meets a preset ratio, wherein the materials for preparing are semi-solid magnesium alloy materials.
[0022] In the embodiment of the present invention, the basic material for preparing the mold can be obtained by obtaining the preparation material of the communication mold, wherein the preparation material refers to a magnesium alloy semi-solid material.
[0023] Furthermore, in the embodiment of the present invention, by analyzing the composition ratio of the prepared material, it is possible to understand whether the prepared material meets the preset ratio, and the composition ratio can be obtained through actual detection.
[0024] Furthermore, after analyzing the composition ratio of the prepared material, the embodiment of the present invention further includes: querying the measured ratio of each element in the prepared material, and calculating the variance test statistic of the magnesium alloy composition in the prepared material based on the measured ratio in combination with the following formula: in, represents the test statistic of magnesium alloy composition variance, A represents the A element in the magnesium alloy semi-solid material, represents the ideal ratio of A element, represents the measured proportion of element A, and B represents element B in the semi-solid material of magnesium alloy. represents the ideal ratio of B element, represents the measured proportion of element B, C represents the C element in the semi-solid material of magnesium alloy, represents the ideal ratio of C elements, represents the measured proportion of C element, N represents the N element in the semi-solid material of magnesium alloy, represents the ideal ratio of N elements, Indicates the measured proportion of N element.
[0025] The test statistic refers to a hypothesis testing method for statistical analysis, which is usually used to compare whether the variances of two or more groups of data are equal, or to test the significance of certain parameters in a statistical model, etc. When the composition ratio meets the preset ratio, the target material is obtained. The value of satisfies the preset ratio, which is usually determined based on specific material requirements, process standards and experience. It is a judgment limit used to determine whether the composition ratio is within an acceptable range.
[0026] S2. Dissolving the target material in a pre-configured furnace to obtain a liquid material, analyzing a liquid phase distribution state of the liquid material, and obtaining a first processed material when the liquid phase distribution state meets a preset state.
[0027] The embodiment of the present invention utilizes the preconfigured melting furnace to dissolve the target material to obtain a liquid material, which can enable the elements in the target material to be more fully mixed, thereby making the composition more uniform and ensuring that the mold has consistent performance in different parts.
[0028] As an embodiment of the present invention, the method of dissolving the target material using a preconfigured furnace to obtain a liquid material includes: adding a preconfigured inert gas into the preconfigured furnace, starting the preconfigured furnace to dissolve the target material, and during the material dissolution process, controlling the temperature of the preconfigured furnace within a preset range, and obtaining a liquid material when the target material becomes liquid.
[0029] Among them, the preconfigured furnace can be a resistance furnace or a gas furnace, the inert gas refers to argon, and during the material dissolution process, controlling the temperature of the preconfigured furnace within a preset range means controlling the change in the temperature of the configured furnace within a range, such as within ±5°C. The temperature can be detected in real time by using a high-precision temperature sensor, and the temperature control equipment can be used to provide real-time feedback to adjust the heating work of the preconfigured furnace.
[0030] Furthermore, the embodiment of the present invention can evaluate the quality uniformity of the liquid material and whether there is local component segregation or temperature difference by analyzing the liquid phase distribution state of the liquid material.
[0031] As an embodiment of the present invention, the analyzing the liquid phase distribution state of the liquid material includes: A surface image of the liquid material is collected, image enhancement processing is performed on the surface image to obtain an enhanced image, image texture and image shape of the enhanced image are extracted, an average diameter of particles in a liquid phase in the liquid material is calculated, and a liquid phase distribution state of the liquid material is analyzed based on the image texture, the image shape and the average diameter.
[0032] Optionally, the surface image can be collected by a thermal imaging device, and the surface image can be enhanced by image enhancement processing. The enhanced image refers to enhanced image details. The surface image can be filtered by a filter and then sharpened. The average diameter of particles in the liquid phase of the liquid material can be measured by a particle size analyzer.
[0033] As an optional embodiment of the present invention, the analyzing the liquid phase distribution state of the liquid material based on the image texture, the image shape and the average diameter includes: calculating the distribution density and uniformity of particles in the liquid material based on the image texture and the image shape, and calculating the distribution difference of the liquid material based on the distribution density, the uniformity and the average diameter using the following formula: in, represents the distribution difference, represents the average diameter, represents the ideal mean diameter corresponding to the mean diameter, represents the distribution density, represents the ideal distribution density corresponding to the distribution density, Indicates uniformity, The uniformity corresponds to the ideal uniformity; Based on the distribution difference, the liquid phase distribution state of the liquid material is determined.
[0034] The process of calculating the distribution density and uniformity of particles in the liquid material based on the image texture and the image shape is as follows: using the image texture and the image shape to identify the texture features and shape features of the particles in the liquid phase, and using machine learning or other data analysis methods based on the texture features and the shape features to analyze and model the extracted features to calculate the distribution density and uniformity of the particles.
[0035] It should be noted that when the liquid phase distribution state meets the preset state, obtaining the first processed material means that the calculated result of the distribution difference is not greater than the preset value, and the material that meets the subsequent operation requirements is obtained. The preset value may be set to 0.1, or may be set according to actual application scenarios.
[0036] S3. Using a preconfigured stirring device to stir the first processed material to obtain a stirred material, analyzing the solid phase particle distribution state of the stirred material, and when the solid phase particle distribution state meets a preset state, obtaining a second processed material.
[0037] In the embodiment of the present invention, the first processing material is stirred by using the pre-configured stirring device to obtain the stirred material, which can use the shear force generated by the stirring to break the growing grains in the material, inhibit the growth of the grains, thereby obtaining a finer grain structure and improving the strength and toughness of the mold. The pre-configured stirring device can be a mechanical stirring device.
[0038] As an embodiment of the present invention, the method of using a preconfigured stirring device to stir the first processed material to obtain a stirred material includes: obtaining a stirring process for stirring the material, using the stirring process to set a stirring speed and a stirring time of the preconfigured stirring device, and based on the stirring speed and the stirring time, using the preconfigured stirring device to stir the first processed material to obtain a stirred material. The stirring process refers to the parameters of the stirring device during stirring, such as a stirring speed of 100-200 rpm and a stirring time of 10-20 minutes, which can be adjusted according to specific application scenarios.
[0039] Furthermore, in the embodiment of the present invention, the stirring effect of the stirring material can be understood by analyzing the distribution state of the solid phase particles of the stirring material.
[0040] As an embodiment of the present invention, the analysis of the solid phase particle distribution state of the stirred material includes: obtaining a microscopic image of the stirred material, identifying solid phase particles in the microscopic image, marking the solid phase particles to obtain marked particles, identifying the particle position, particle size and particle shape of the marked particles, and determining the solid phase particle distribution state of the stirred material based on the particle position, the particle size and the particle shape.
[0041] Among them, the microscopic image of the stirred material can be obtained through a scanning electron microscope, the solid-phase particles in the microscopic image can be identified by a deep learning model through the image features of the microscopic image, and based on the image feature identification, the solid-phase particles are labeled, and the labeled particles can be labeled through a U-Net network. The process of determining the distribution state of the solid-phase particles of the stirred material based on the particle position, the particle size and the particle shape is: using the particle position to determine whether the solid-phase particles are evenly distributed in the liquid phase of the stirred material, and determining whether the solid-phase particles are small and smooth based on the particle size and the particle shape.
[0042] It should be noted that when the distribution state of the solid phase particles meets the preset state, obtaining the second processed material means that the distribution state of the solid phase particles is small, uniform and nearly spherical solid phase particles are uniformly distributed in the liquid phase, and the spacing between the solid phase particles is relatively consistent. If the distribution state of the solid phase particles does not meet the preset state, the stirring parameters of the preconfigured stirring device are adjusted until the distribution state of the solid phase particles meets the preset state.
[0043] S4. Use a preconfigured cooling device to cool the second processing material, and complete cooling when the second processing material is in a semi-solid state to obtain a third processing material, use a preconfigured die-casting device to die-cast the third processing material to obtain an initial mold, perform a toughness test on the initial mold, and when the test result of the toughness test is excellent, obtain a target mold, perform rough processing on the target mold to obtain a first processing mold.
[0044] In the embodiment of the present invention, the second processing material is cooled by the preconfigured cooling device, and when the second processing material is semi-solid, the cooling is completed to obtain the third processing material, so that a solid material can be obtained to facilitate the processing of the communication mold.
[0045] As an embodiment of the present invention, the method of cooling the second processed material using a preconfigured cooling device and completing cooling when the second processed material is in a semi-solid state to obtain a third processed material includes: designing cooling channels and waterway layouts for the preconfigured cooling device to obtain a target cooling device, setting parameters for the cooling medium corresponding to the target cooling device to obtain a set cooling medium, cooling the second processed material using the target cooling device and the set cooling medium, and completing cooling when the second processed material is in a semi-solid state to obtain a third processed material. The preconfigured cooling device is a water-cooled cooling device. The semi-solid state refers to an intermediate state in which the material is neither completely liquid nor completely solid.
[0046] Optionally, the cooling channel design and water channel layout of the preconfigured cooling device are performed to obtain a target cooling device. The density of cooling water channels can be increased at key parts of the mold, or conformal cooling water channels can be set. The parameters of the cooling medium corresponding to the target cooling device are set to obtain the set cooling medium. The temperature, flow rate and pressure of the cooling medium, such as water, oil or air, can be set. The cooling rate of the cooling device can be controlled within a certain range by setting the temperature, flow rate and pressure. 5 - 10 ° C / sec, specifically set in combination with the actual application scenario, when the second processed material is semi-solid, cooling is completed to obtain the third processed material by analyzing the solid phase ratio (volume fraction of the solid phase) of the second processed material, and the solid phase ratio is generally between 20% - 80%.
[0047] Furthermore, the embodiment of the present invention uses the preconfigured die-casting device to die-cast the third processed material to obtain an initial mold, which can quickly fill the semi-solid magnesium alloy slurry into the mold cavity of the die-casting machine under high pressure, thereby achieving high-precision molding of complex-shaped mold blanks, ensuring the accuracy of size and shape, and meeting the design requirements of communication molds.
[0048] Optionally, the process of die-casting the third processed material using a preconfigured die-casting device to obtain an initial mold is as follows: inputting the third processed material into the barrel of the preconfigured die-casting device, and setting the die-casting pressure within the range of 50 - 100 MPa, and setting the die-casting speed to 3 - 5 m / s to obtain a preliminarily formed mold blank, and in the microstructure morphology of the mold blank, the solid phase particles should maintain a good shape and distribution.
[0049] Furthermore, the embodiment of the present invention can determine whether the mold meets the expected toughness standard by performing a toughness test on the initial mold, judge its ability to withstand impact, vibration and alternating loads during use, and thus evaluate the quality and reliability of the mold.
[0050] As an embodiment of the present invention, the toughness test on the initial mold includes: querying the material properties of the initial mold, analyzing the tensile strength of the initial mold according to the material properties, performing an impact test on the initial mold based on the tensile strength, and determining the fracture toughness of the target metal plate and the weld based on the result of the impact test.
[0051] The material properties refer to the properties, characteristics or features of the material under specific conditions, such as hardness, melting point, thermal conductivity and expansion coefficient, which can be obtained by accessing the matwab database to query the raw materials of the processed materials.
[0052] It should be noted that when the test result of the toughness test is excellent, obtaining the target mold means that the target mold has no cracks and obvious deformation in the test.
[0053] In the embodiment of the present invention, by rough machining the target mold to obtain the first processed mold, an initial mold with relatively good quality can be obtained. The rough machining refers to the preliminary engraving of the mold.
[0054] Optionally, the rough processing of the target mold to obtain the first processing mold can be performed by performing heat processing on the target mold to obtain a heat-processed mold, and the heat-processed mold is cut by a CNC machine tool according to a preset mold shape and size.
[0055] S5. Perform defect detection on the first processing mold. When the first processing mold has defects, perform defect repair on the first processing mold to obtain a repair mold. Perform fine processing on the repair mold to obtain a target communication mold.
[0056] In the embodiment of the present invention, by performing defect detection on the first processing mold, it is possible to understand whether there are defects inside the first processing mold, such as cracks, unevenness, and avoid the subsequent production of defective products.
[0057] As an embodiment of the present invention, the defect detection on the first processing mold includes: acquiring a finished product image of the first processing mold, performing image edge detection on the finished product image, performing image segmentation on the finished product image based on a result of the image edge detection to obtain a segmented image, identifying image features of the segmented image, and performing defect detection on the first processing mold based on the image features to obtain a defect detection result.
[0058] Optionally, performing image edge detection on the finished image refers to the process of identifying and locating the boundaries of objects in the image in digital image processing, which is achieved through Canny edge detection; performing image segmentation on the finished image based on the result of the image edge detection to obtain the segmented image is achieved through a target segmentation algorithm; identifying image features of the segmented image is achieved through a convolutional neural network algorithm; performing defect detection on the first processing mold based on the image features to obtain the defect detection result is performed through image matching analysis of a large number of finished product images related to the first processing mold collected by a deep learning model.
[0059] Furthermore, in the embodiment of the present invention, when the first processing mold has defects, the defects of the first processing mold are repaired to obtain a repaired mold that can compensate for the defects of the mold during processing to ensure the quality of the finished mold in the production process. The defects of the first processing mold can be repaired by welding or filling.
[0060] Furthermore, the embodiment of the present invention can improve the service life and performance of the mold by fine-machining the repair mold to obtain the target communication mold, wherein the fine machining refers to using a high-precision CNC machine tool to perform processing with a cutting depth of 0.1-0.2 mm until the accuracy and surface roughness requirements required for the communication mold are achieved, and the mold after fine machining is surface treated by chemical plating or electroplating to coat the mold surface with a wear-resistant and corrosion-resistant coating, such as nickel, chromium, etc.
[0061] As an embodiment of the present invention, after fine processing the repair mold to obtain the target communication mold, the method further includes: calculating the comprehensive production score of the target communication mold using the following formula: and, 1 in, Indicates the comprehensive production score, represents the average deviation of the elemental composition, It represents the total deviation of the liquid material particle characteristics from the ideal value. It represents the total deviation of the solid phase particle characteristics from the ideal value. represents the total deviation of cooling and die casting parameters from the ideal values, It represents the total deviation of defects and repair effects from the ideal value. express The weight of express , , express The weight of express The weight of .
[0062] It should be noted that the comprehensive production score can be used to understand the level of comprehensive and comprehensive evaluation of the target communication mold, avoiding focusing on a single link and ignoring other factors that may have a significant impact on the mold quality.
[0063] like Figure 2 Shown is a functional module diagram of a communication mold preparation system based on semi-solid magnesium alloy according to the present invention.
[0064] The communication mold preparation system 200 based on the semi-solid state of magnesium alloy described in the present invention can be installed in an electronic device. According to the functions to be implemented, the communication mold preparation system based on the semi-solid state of magnesium alloy can include a component ratio analysis module 201, a liquid phase distribution analysis module 202, a solid phase particle distribution analysis 203, a mold rough processing module 204 and a mold finishing module 205. The module described in the present invention can also be called a unit, which refers to a series of computer program segments that can be executed by an electronic device processor and can complete fixed functions, which are stored in the memory of the electronic device.
[0065] In the embodiment of the present invention, the functions of each module / unit are as follows: The component ratio analysis module 201 is used to obtain the prepared material of the communication mold, analyze the component ratio of the prepared material, and obtain the target material when the component ratio meets the preset ratio, wherein the prepared material refers to a magnesium alloy semi-solid material; The liquid phase distribution analysis module 202 is used to dissolve the target material using a pre-configured furnace to obtain a liquid material, analyze the liquid phase distribution state of the liquid material, and obtain a first processed material when the liquid phase distribution state meets a preset state; The solid phase particle distribution analysis 203 is used to stir the first processed material using a pre-configured stirring device to obtain a stirred material, analyze the solid phase particle distribution state of the stirred material, and obtain a second processed material when the solid phase particle distribution state meets a preset state; The mold rough processing module 204 is used to cool the second processing material using a pre-configured cooling device, and complete cooling when the second processing material is semi-solid to obtain a third processing material, and use a pre-configured die-casting device to die-cast the third processing material to obtain an initial mold, perform a toughness test on the initial mold, and when the test result of the toughness test is excellent, obtain a target mold, and perform rough processing on the target mold to obtain a first processing mold; The mold finishing module 205 is used to perform defect detection on the first processing mold, and when the first processing mold has defects, repair the defects of the first processing mold to obtain a repaired mold, and perform fine processing on the repaired mold to obtain a target communication mold.
[0066] In detail, each module in the scene modeling system 200 for realizing intelligent transportation based on digital twins described in the embodiment of the present invention is used in the same manner as described above. Figure 1 The technical means described in the text is the same as the scene modeling method for smart transportation based on digital twins, and can produce the same technical effects, so I will not go into details here.
[0067] In the several embodiments provided by the present invention, it should be understood that the disclosed systems and methods can be implemented in other ways. For example, the system embodiments described above are only illustrative, for example, the division of the modules is only a logical function division, and there may be other division methods in actual implementation.
[0068] The modules described as separate components may or may not be physically separated, and the components shown as modules may or may not be physical units, that is, they may be located in one place or distributed on multiple network units. Some or all of the modules may be selected according to actual needs to achieve the purpose of the solution of this embodiment.
[0069] In addition, each functional module in each embodiment of the present invention may be integrated into one processing unit, each unit may exist physically separately, or two or more units may be integrated into one unit. The above-mentioned integrated unit may be implemented in the form of hardware or in the form of hardware plus software functional modules.
[0070] It is obvious to those skilled in the art that the present invention is not limited to the details of the above exemplary embodiments, and that the present invention can be implemented in other specific forms without departing from the spirit or essential characteristics of the present invention.
[0071] Therefore, no matter from which point of view, the embodiments should be regarded as illustrative and non-restrictive, and the scope of the present invention is limited by the appended claims rather than the above description, so it is intended that all changes falling within the meaning and scope of the equivalent elements of the claims are included in the present invention. Any attached figure mark in the claims should not be regarded as limiting the claims involved.
[0072] It should be noted that, in this article, relational terms such as "first" and "second" are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the sentence "comprise a ..." do not exclude the existence of other identical elements in the process, method, article or device including the elements.
[0073] The above description is only a specific embodiment of the present invention, so that those skilled in the art can understand or implement the present invention. Various modifications to these embodiments will be apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but should conform to the widest scope consistent with the principles and novel features invented herein.
Claims
1. A method for preparing a communication mold based on a semi-solid magnesium alloy, characterized in that: The method comprises: Acquire the prepared material of the communication mold, analyze the composition ratio of the prepared material, and obtain the target material when the composition ratio meets the preset ratio, wherein the prepared material refers to a magnesium alloy semi-solid material; Dissolving the target material in a preconfigured furnace to obtain a liquid material, analyzing a liquid phase distribution state of the liquid material, and obtaining a first processed material when the liquid phase distribution state meets a preset state; Using a pre-configured stirring device to stir the first processed material to obtain a stirred material, analyzing the solid phase particle distribution state of the stirred material, and obtaining a second processed material when the solid phase particle distribution state meets a preset state; The second processed material is cooled by a pre-configured cooling device, and when the second processed material is in a semi-solid state, the cooling is completed to obtain a third processed material, the third processed material is die-casted by a pre-configured die-casting device to obtain an initial mold, the initial mold is subjected to a toughness test, and when the toughness test result is excellent, a target mold is obtained, and the target mold is rough-processed to obtain a first processed mold; The first processing mold is subjected to defect detection. When the first processing mold has defects, the defects are repaired to obtain a repair mold. The repair mold is finely processed to obtain a target communication mold.
2. The method according to claim 1, characterized in that After analyzing the composition ratio of the prepared material, the method further comprises: Query the measured proportion of each element in the prepared material; Based on the measured ratio, the variance test statistic of the magnesium alloy composition in the prepared material is calculated in combination with the following formula: in, represents the test statistic of magnesium alloy composition variance, A represents the A element in the magnesium alloy semi-solid material, represents the ideal ratio of A element, represents the measured proportion of element A, and B represents element B in the semi-solid material of magnesium alloy. represents the ideal ratio of B element, represents the measured proportion of element B, C represents the C element in the semi-solid material of magnesium alloy, represents the ideal ratio of C elements, represents the measured proportion of C element, N represents the N element in the semi-solid material of magnesium alloy, represents the ideal ratio of N elements, Indicates the measured proportion of N element.
3. The method according to claim 1, characterized in that: The method of dissolving the target material by using a pre-configured furnace to obtain a liquid material includes: After adding the preconfigured inert gas into the preconfigured furnace, the preconfigured furnace is started to dissolve the target material; During the material dissolution process, the preconfigured furnace temperature is controlled within a preset range, and when the target material becomes liquid, a liquid material is obtained.
4. The method according to claim 1, characterized in that: The analyzing the liquid phase distribution state of the liquid material comprises: collecting a surface image of the liquid material; Performing image enhancement processing on the surface image to obtain an enhanced image; Extracting the image texture and image shape of the enhanced image, and calculating the average diameter of particles in the liquid phase of the liquid material; The liquid phase distribution state of the liquid material is analyzed based on the image texture, the image shape and the average diameter.
5. The method according to claim 4, characterized in that The analyzing the liquid phase distribution state of the liquid material based on the image texture, the image shape and the average diameter includes: Calculating the distribution density and uniformity of particles in the liquid material based on the image texture and the image shape; Based on the distribution density, the uniformity and the average diameter, the distribution difference of the liquid material is calculated using the following formula: in, represents the distribution difference, represents the average diameter, represents the ideal mean diameter corresponding to the mean diameter, represents the distribution density, represents the ideal distribution density corresponding to the distribution density, Indicates uniformity, The uniformity corresponds to the ideal uniformity; Based on the distribution difference, the liquid phase distribution state of the liquid material is determined.
6. The method according to claim 1, characterized in that The method of using a pre-configured stirring device to stir the first processed material to obtain a stirred material includes: Obtaining a mixing process for mixing the material; Using the stirring process, setting the stirring speed and stirring time of the preconfigured stirring device; Based on the stirring speed and the stirring time, the first processed material is stirred using the preconfigured stirring device to obtain a stirred material.
7. The method according to claim 1, characterized in that The analyzing the distribution state of solid phase particles of the stirred material comprises: Acquiring a microscopic image of the stirred material; Identifying solid phase particles in the microscopic image, and marking the solid phase particles to obtain marked particles; Identifying the particle position, particle size and particle shape of the marked particles; The solid phase particle distribution state of the stirred material is determined based on the particle position, the particle size and the particle shape.
8. The method according to claim 1, characterized in that The method of cooling the second processed material by using a pre-configured cooling device and completing the cooling when the second processed material is in a semi-solid state to obtain a third processed material comprises: Design cooling channels and layout water channels for the preconfigured cooling device to obtain a target cooling device; Setting parameters of the cooling medium corresponding to the target cooling device to obtain a set cooling medium; Cooling the second processed material using the target cooling device and the set cooling medium; When the second processed material is in a semi-solid state, cooling is completed to obtain a third processed material.
9. The method according to claim 1, characterized in that: The toughness test of the initial mold comprises: Querying the material properties of the initial mold; Analyzing the tensile strength of the initial mold according to the material properties; impact testing the initial mold based on the tensile strength; Based on the results of the impact test, the fracture toughness of the target metal plate and the weld is determined.
10. A communication mold preparation system based on semi-solid magnesium alloy, characterized in that: The system comprises: A component ratio analysis module, used to obtain the prepared material of the communication mold, analyze the component ratio of the prepared material, and obtain the target material when the component ratio meets the preset ratio, wherein the prepared material refers to a magnesium alloy semi-solid material; A liquid phase distribution analysis module, used to dissolve the target material using a pre-configured furnace to obtain a liquid material, analyze the liquid phase distribution state of the liquid material, and obtain a first processed material when the liquid phase distribution state meets a preset state; a solid phase particle distribution analysis module, configured to stir the first processed material using a pre-configured stirring device to obtain a stirred material, analyze the solid phase particle distribution state of the stirred material, and obtain a second processed material when the solid phase particle distribution state meets a preset state; A mold rough processing module is used to cool the second processing material using a pre-configured cooling device, and complete cooling when the second processing material is in a semi-solid state to obtain a third processing material, and to die-cast the third processing material using a pre-configured die-casting device to obtain an initial mold, and to perform a toughness test on the initial mold. When the test result of the toughness test is excellent, a target mold is obtained, and the target mold is rough-processed to obtain a first processing mold; The mold finishing module is used to perform defect detection on the first processing mold, and when the first processing mold has defects, perform defect repair on the first processing mold to obtain a repaired mold, and perform fine processing on the repaired mold to obtain a target communication mold.
Citation Information
Patent Citations
Method and device for preparing semi-solid slurry
CN105328143A
Semisolid metal slurry preparation device and method
CN105855498A
Magnesium alloy automobile part semi-solid die casting forming process
CN106424631A
Novel magnesium alloy semi-solid state forming process
CN111922313A
Method for monitoring solid fraction of semi-solid die-casting slurry on line
CN115533062A