Multi-doubly-fed wind generator aluminum rotor and aluminum row end-to-end welding structure and method
By adopting H-shaped clamping structure and special aluminum alloy material in the aluminum rotor of the double-feed wind turbine, combined with infrared temperature measurement and pressurized clamping device, the mechanical strength and temperature control problems in aluminum rotor clamping head welding are solved, and the mechanical strength and temperature control problems in aluminum rotor clamping head welding is improved. Welding quality and efficiency.
Patent Information
- Application Number
- CN202411207705.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-30
- Publication Date
- 2024-11-08
AI Technical Summary
The existing double-feed wind turbine aluminum rotor welding structure has insufficient mechanical strength and electrical performance, resulting in poor welding quality and difficulty in meeting technical standards. It also has serious problems in temperature control and solder loss, which affects production efficiency.
Adopt H-shaped clamping structure and special aluminum alloy material, combined with infrared temperature measurement and pressurized clamping device, optimize welding methods, increase welding area and fill amount, and solve temperature control and solder loss through medium frequency induction welding machines and horizontal induction welding methods. question.
It improves the mechanical strength and welding quality of the clamp welding structure, effectively controls the welding temperature, reduces solder loss and sag, and improves production efficiency and welding efficiency.
Smart Images

Figure CN118905405A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of aluminum rotors for doubly-fed wind generators, and in particular to a plurality of aluminum rotors for doubly-fed wind generators and aluminum row parallel head welding structures and methods. Background Art
[0002] Due to the current cost pressure on the main components and main raw materials of wind turbines, various main engine manufacturers and motor manufacturers have gradually adopted a cost-reduction method of replacing high-cost traditional materials with low-cost new materials. Based on the successful development of aluminum stators, the development of aluminum rotors has become a cutting-edge topic of technical research for various main engine manufacturers and motor manufacturers.
[0003] Since the aluminum rotors of doubly-fed wind turbines are currently in the initial development stage in China, the core of developing aluminum rotors lies in the successful application of aluminum wire as the conductor material of the rotor coil. How to apply aluminum wire conductor materials to the aluminum rotors of doubly-fed wind turbines is the main focus of current technical research in wind turbine structural design, process technology, etc.
[0004] In addition, due to the large gap between aluminum wire and traditional copper wire in mechanical strength, electrical properties, melting point and other properties, there are great difficulties in the rotor head welding process. The quality of the rotor head welding is the key to ensuring the electrical performance of the motor and the key to ensuring the power output of the motor. How to ensure the corresponding production efficiency while meeting various technical standards and quality requirements is the key problem in the current aluminum rotor research.
[0005] At present, the existing copper rotor parallel head structure is a "straight" structure, such as Figure 1 As shown. The commonly used copper rotor joint welding method is induction welding, which usually uses a medium-frequency induction welding machine and an induction welding gun that matches the joint head size. After the joint head is heated by electromagnetic induction, the solder is filled. If the copper rotor joint head structure and its welding method are directly used for aluminum rotor joint welding, it will not meet the relevant technical standards and the welding quality will be poor.
[0006] The rotor needs to rotate at high speed during actual operation. If the joint head has low structural strength and poor joint head welding quality, high-speed rotation can easily cause the joint head to crack or break.
[0007] Among them, when the aluminum wire is at a high temperature close to its melting point, there is no obvious reaction (no color reaction), and the temperature of the base material cannot be judged by naked eye observation. The melting point of aluminum wire is usually around 600°C, and the melting point of the corresponding solder is usually around 500°C. There is only a difference of about 100°C between the melting points of the two. It is easy for the solder to melt and overheat during welding, causing the base material to melt, making it difficult to control the temperature during welding.
[0008] In addition, the commonly used aluminum solder has poor solid phase properties and good liquid phase properties, which leads to its strong fluidity when melted, making it difficult to solder during welding. When welding, the solder cannot fully fill the gaps in the joint structure, and the solder loses and sags seriously. Summary of the invention
[0009] To solve the above problems, the present invention discloses a variety of doubly-fed wind turbine aluminum rotor and aluminum row joint welding structures and methods, which can optimize and improve the strength of the joint welding structure, effectively control the welding temperature and welding gap, improve the welding efficiency, and ensure the quality of the doubly-fed wind turbine aluminum rotor and aluminum row joint welding.
[0010] The specific plan is as follows: The invention discloses a plurality of aluminum rotor and aluminum row parallel welding structures of a doubly-fed wind turbine generator, comprising a rotor aluminum row, an H-shaped parallel wedge, a parallel foil and a welding piece assembly. The rotor aluminum row has four aluminum rows, two of which form a group. The two groups of aluminum rows are symmetrically arranged in the upper and lower grooves of the H-shaped parallel wedge, and each group of aluminum rows is symmetrically arranged. A parallel foil is arranged between the two aluminum rows of each group, and the left and right sides of the parallel foil are respectively welded to the left and right aluminum rows through welding piece one, the left and right side surfaces of the groove of the H-shaped parallel head are respectively welded to the aluminum row through welding piece two, and the bottom surface of the groove is welded to the aluminum row through welding piece three.
[0011] As a further improvement of the present invention, the height of the welding sheet 1 is the same as that of the header foil.
[0012] As a further improvement of the present invention, the second welding piece has the same height as the groove of the parallel wedge.
[0013] As a further improvement of the present invention, the third welding piece has the same width as the aluminum bar and is common to the second welding piece.
[0014] As a further improvement of the present invention, the rotor aluminum bar adopts a special aluminum alloy material. Compared with the traditional pure aluminum material with a melting point of 600°C, the melting point of the special aluminum alloy material is 650-680°C, the tensile strength is 180-200 MPa, the yield strength is 120 MPa, the conductivity is 86% relative to pure copper, the hardness is 50-60 HDB (special heat treatment), and the elongation is 15-18%. This welding method is suitable for the welding of rotor aluminum bar coils made of this special aluminum material, and the other materials are for reference only.
[0015] A variety of double-fed wind turbine aluminum rotor aluminum row joint welding methods, comprehensive special treatment of medium-frequency induction welding machines, induction welding gun head and related equipment, including temperature control solutions and solutions for severe solder loss and sagging.
[0016] As a further improvement of the present invention, the temperature control scheme is: during welding, the temperature of the workpiece is measured in real time by an infrared temperature measuring probe, and the corresponding data is transmitted to the welding machine temperature control system program. When in the protective welding temperature range, the welding machine automatically outputs stable power and induced current.
[0017] As a further improvement of the present invention, the infrared temperature measuring probe is installed on the welding gun head to form an infrared sensing gun head, wherein the protective welding temperature range is 550-650°C, the over-temperature welder automatically stops heating, the stable power and induced current are 25kw and 30%A for the medium frequency induction welder, and the welding time is 30-45s.
[0018] As a further improvement of the present invention, the solution to the serious solder loss and sagging is: using horizontal induction welding, the H-shaped wedge can effectively hold a certain amount of lost solder at the bottom during horizontal induction welding, ensuring the filling of solder in the most critical middle part of the welding.
[0019] As a further improvement of the present invention, a pressure clamping device is directly installed on the infrared sensing gun head, and the workpiece is pressurized and clamped when the solder melts during parallel welding. After the corresponding solder is fully filled, the corresponding clamping device is released, so as to control the welding gap, reduce solder loss, and avoid solder sagging.
[0020] The beneficial effects of the present invention are: the structure is ingenious, the handle and the valve stem are in a circular floating fit, and the fixation can be completed after the installation orientation is confirmed. The installation operation is simple, the work efficiency is improved, and the installation errors are reduced. At the same time, the handle adopts a dual fixing method of threaded fit and interference fit, which can effectively reduce the risk of inability to open and close caused by the loosening and failure of the handle. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 It is a traditional "single-line" parallel head structure diagram.
[0022] Figure 2 It is a structural schematic diagram of the present invention.
[0023] Figure 3 This is a schematic diagram of the infrared sensing gun head.
[0024] Figure 4 This is a schematic diagram of the infrared sensing gun head combined with the pressure clamping device.
[0025] List of reference numerals: 1-rotor aluminum row, 2-H-type parallel wedge, 3-parallel foil, 4-welding piece one, 5-welding piece two, 6-welding piece three, 7-I-shaped parallel wedge. DETAILED DESCRIPTION
[0026] The present invention will be further explained below in conjunction with the accompanying drawings and specific embodiments. It should be understood that the following specific embodiments are only used to illustrate the present invention and are not used to limit the scope of the present invention.
[0027] like Figure 1 As shown, it is a traditional "straight" joint structure. The welding surface between the aluminum bars is mainly one surface above and below the middle part of the straight joint wedge 7 (expanded to double-sided welding through the joint foil, because the joint foil is thin, one surface is actually considered), a total of 2 surfaces, and the direct welding surface between the aluminum bar and the joint wedge is one surface above and below the middle part of the "straight" joint wedge, a total of 2 surfaces. The total effective welding surface is 4. The number of welding pieces of different sizes that can be filled in this structure is 6 pieces.
[0028] like Figure 2 As shown, the present application provides a variety of aluminum rotor and aluminum row parallel head welding structures of doubly fed wind turbine generators, including rotor aluminum rows 1, H-shaped parallel head wedges 2, parallel head foils 3 and welding piece assemblies. There are four rotor aluminum rows, two of which are in a group. The two groups of aluminum rows are symmetrically arranged in the upper and lower grooves of the H-shaped parallel head wedge, and each group of aluminum rows is symmetrically arranged on the left and right. A parallel head foil is arranged between the two aluminum rows of each group, and the left and right sides of the parallel head foil are respectively welded to the left and right aluminum rows through welding piece one 4, the left and right side surfaces of the groove of the H-shaped parallel head are respectively welded to the aluminum row through welding piece two 5, and the bottom surface of the groove is welded to the aluminum row through welding piece three 6.
[0029] In this embodiment, the first welding piece has the same height as the header foil, the second welding piece has the same height as the groove of the header wedge, and the third welding piece has the same width as the aluminum row and is common to the second welding piece.
[0030] The "H-type" parallel structure, the welding surface between the aluminum bars is mainly 1 vertical surface above and below the middle part of the H-type parallel wedge (expanded to double-sided welding through the parallel foil, because the parallel foil is thin, actually consider 1 surface), a total of 2 surfaces, the aluminum bar and the "H-type" parallel wedge directly contact welding surface has 6 surfaces. A total of 8 effective welding surfaces. The number of welding pieces of different sizes that can be filled with this structure is 10 pieces.
[0031] In summary, the "H-type" parallel head structure can increase the welding area of the parallel head welding within the limited rotor parallel head structure space, and at the same time increase the solder filling amount, thereby improving the mechanical strength of the parallel head welding structure.
[0032] In this embodiment, the rotor aluminum bar adopts a special aluminum alloy material. Compared with the traditional pure aluminum material with a melting point of 600°C, the special aluminum alloy material has a melting point of 650-680°C, a tensile strength of 180-200 MPa, a yield strength of 120 MPa, a conductivity of 86% relative to pure copper, a hardness of 50-60 HDB (special heat treatment), and an elongation of 15-18%. This welding method is suitable for the welding of rotor aluminum bar coils made of this special aluminum material, and the other materials are for reference only.
[0033] In order to solve the technical problems of aluminum rotor joint welding, such as temperature control difficulties, solder loss, and severe sagging during induction welding, the present application proposes a variety of double-fed wind turbine aluminum rotor aluminum row joint welding methods, and conducts comprehensive and specialized treatment of medium-frequency induction welding machines and induction welding gun head related equipment, including temperature control solutions and solutions to severe solder loss and sagging.
[0034] In this embodiment, the temperature control scheme is: during welding, the temperature of the workpiece is measured in real time by an infrared temperature measuring probe, and the corresponding data is transmitted to the welding machine temperature control system program. When in the protective welding temperature range, the welding machine automatically outputs stable power and induced current.
[0035] Among them, Figure 3 As shown, the infrared temperature probe is installed on the welding gun head to form an infrared sensing gun head. The protective welding temperature range is 550-650℃, and the over-temperature welder automatically stops heating. The stable power and induction current are 25kw and 30%A for the medium frequency induction welder, and the welding time is 30-45s.
[0036] In this embodiment, the solution to serious solder loss and sagging is to use horizontal induction soldering, that is, Figure 2 The workpiece is vertically inductively welded in the direction shown in the figure. Rotate 90° clockwise. When the H-shaped joint wedge is used for horizontal induction welding, it can effectively hold a certain amount of lost solder at the bottom to ensure the solder filling in the middle part of the joint welding, which is the most critical part. Install a pressure clamping device directly on the infrared induction gun head, such as Figure 4 As shown, when the solder for parallel welding is melted, the workpiece is clamped under pressure, and after the corresponding solder is fully filled, the corresponding clamping device is released, so as to control the welding gap, reduce solder loss, and avoid solder sagging.
[0037] The technical means disclosed in the scheme of the present invention are not limited to the technical means disclosed in the above-mentioned implementation mode, but also include technical schemes composed of any combination of the above-mentioned technical features. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention, and these improvements and modifications are also regarded as the protection scope of the present invention.
Claims
1. Multiple double-fed wind turbine aluminum rotor aluminum row parallel welding structure, characterized in that: It includes a rotor aluminum row, an H-shaped parallel head wedge, a parallel head foil and a welding piece assembly. There are four rotor aluminum rows, two of which form a group. The two groups of rotor aluminum rows are symmetrically arranged in the upper and lower grooves of the H-shaped parallel head wedge, and each group of rotor aluminum rows is symmetrically arranged. A parallel head foil is arranged between the two rotor aluminum rows of each group, and the left and right sides of the parallel head foil are respectively welded to the left and right rotor aluminum rows through welding piece 1, the left and right side surfaces of the groove of the H-shaped parallel head are respectively welded to the rotor aluminum row through welding piece 2, and the bottom surface of the groove is welded to the rotor aluminum row through welding piece 3.
2. The multiple aluminum rotor and aluminum row parallel welding structure of double-fed wind turbine generator according to claim 1 is characterized in that: The welding piece 1 has the same height as the header foil.
3. The multiple aluminum rotor and aluminum row parallel welding structure of double-fed wind turbine generator according to claim 1 is characterized in that: The second welding piece has the same height as the groove of the wedge.
4. The multiple aluminum rotor and aluminum row parallel welding structure of double-fed wind turbine generator according to claim 1 is characterized in that: The welding piece 3 has the same width as the rotor aluminum row and is common to the welding piece 2.
5. The multiple aluminum rotor and aluminum row parallel welding structure of double-fed wind turbine generator according to claim 1 is characterized in that: The rotor aluminum bar is made of a special aluminum alloy material with a melting point of 650-680°C, a tensile strength of 180-200 MPa, a yield strength of 120 MPa, a conductivity of 86% relative to pure copper, a hardness of 50-60 HDB, and an elongation of 15-18%.
6. Multiple methods for welding aluminum rotors and aluminum rows of double-fed wind turbine generators, characterized in that: Based on the parallel welding structure as described in any one of claims 1 to 5, comprehensive special treatment is performed on the medium frequency induction welding machine and the induction welding gun head related equipment, including temperature control solutions and solutions for serious solder loss and sagging.
7. The method for welding multiple aluminum rotors and aluminum rows of double-fed wind turbine generators in parallel according to claim 6, characterized in that: The temperature control scheme is: during welding, the temperature of the workpiece is measured in real time by an infrared temperature measuring probe, and the corresponding data is transmitted to the temperature control system program of the welding machine. When it is in the protective welding temperature range, the welding machine automatically outputs stable power and induced current.
8. The method for welding multiple aluminum rotors and aluminum rows of double-fed wind turbine generators in parallel according to claim 7, characterized in that: The infrared temperature measuring probe is installed on the welding gun head to form an infrared sensing gun head, wherein the protective welding temperature range is 550-650°C, the over-temperature welder automatically stops heating, the stable power and induced current are 25kw and 30%A for the medium frequency induction welder, and the welding time is 30-45s.
9. The method for welding multiple aluminum rotors and aluminum rows of double-fed wind turbine generators in parallel according to claim 8, characterized in that: The solution to the serious problem of solder loss and sagging is to adopt horizontal induction welding. During horizontal induction welding, the H-shaped joint wedge can effectively hold a certain amount of lost solder at the bottom to ensure the filling of solder in the middle part which is the most critical part of joint welding.
10. The method for welding multiple aluminum rotors and aluminum rows of double-fed wind turbine generators in parallel according to claim 9, characterized in that: A pressure clamping device is directly installed on the infrared induction gun head. The workpiece is pressurized and clamped when the solder melts during parallel welding. After the corresponding solder is fully filled, the corresponding clamping device is released to control the welding gap, reduce solder loss, and avoid solder sagging.