Hollow glass and manufacturing method thereof

By installing an air pressure balance device and adding adjustment and inspection processes during the manufacturing process of hollow glass, the problem of air pressure in the intermediate layer is solved, and the ultra-flat surface of the hollow glass is realized, the inspection and debugging process is simplified, and the production efficiency is improved.

CN118908596APending Publication Date: 2024-11-08信义节能玻璃(江门)有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410950172.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-16
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

During the manufacturing process of hollow glass, the air pressure of the intermediate layer is unstable, resulting in the thickness that does not meet the requirements, causing image distortion and deformation. The traditional inspection and debugging methods are cumbersome and the processing efficiency is low.

Method used

During the production of hollow glass, an air pressure balance device is installed and the adjustment and inspection process is added. The air pressure adjustment is performed by measuring the thickness of the intermediate layer to ensure the stability of the air pressure of the hollow layer, and seal the air pressure balance device when appropriate to optimize the air inlet and outlet of the intermediate frame. Air holes are designed to achieve sealing.

Benefits of technology

It solves the problem of image distortion and deformation in hollow glass processing, reduces manufacturing cost and quality losses, simplifies the inspection and debugging process, and improves the processing efficiency of large-scale production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118908596A_ABST
    Figure CN118908596A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of glass manufacturing, in particular to hollow glass and a manufacturing method thereof, and the manufacturing method comprises the following working procedures: a middle frame treatment working procedure, a glass semi-finished product processing working procedure, a compounding working procedure and an adjusting and inspecting working procedure. A preparation method of the hollow glass is improved, an air pressure balancing device is installed before glue sealing treatment of the center control glass, an adjusting and checking procedure is added, the thickness of a middle layer of the glass is measured after the hollow glass is obtained through the adjusting and checking procedure, and inflation or exhaust treatment is conducted through the installed air pressure balancing device according to the deviation value of the thickness of the middle layer. The thickness of the layer after the air pressure of the hollow layer is stabilized meets the requirement of the current production batch, and then the air pressure balancing device is sequentially sealed with the air inlet hole connecting position and the air outlet hole connecting position of the middle frame, so that the problem of image distortion caused by the hollow glass processing technology is solved, and the process manufacturing cost and the external quality loss are reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of glass manufacturing, in particular to a hollow glass and a manufacturing method thereof. Background Art

[0002] When manufacturing insulating glass, the appearance image effect of insulating glass is usually achieved by controlling the flatness of tempered glass. However, since the hollow production process assembly process cannot control the air pressure between the hollow spacer and the glass layer, the air pressure of the intermediate layer structure after assembly is unstable, which easily causes the thickness of the intermediate layer to be concave or convex due to the air intake of the hollow layer of the insulating glass, resulting in the thickness of the intermediate layer failing to meet the processing requirements and poor overall flatness, causing the image distortion and deformation after the insulating glass is installed. The traditional method of handling the inspection and debugging of the intermediate layer of insulating glass is to seal the insulating glass as a whole in the insulating glass production process to prevent gas leakage after molding, and then conduct thickness inspection. At this time, the outer periphery of the gas adjustment hole used for filling and discharging gas needs to be sealed with sealant independently. At the same time, when the layer thickness of the current intermediate layer in the sealed state is found to not meet the requirements after the sealing is completed, it is necessary to remove the glue and fill it again. The operation process is too cumbersome, and the processing efficiency in mass production is not ideal. Summary of the invention

[0003] In view of the problems in the prior art, the present invention provides a hollow glass and a manufacturing method thereof.

[0004] The technical solution adopted by the present invention to solve the technical problem is: a hollow glass and a manufacturing method thereof, comprising the following processes: an intermediate frame processing process, a glass semi-finished product processing process, a compounding process and an adjustment and inspection process;

[0005] The intermediate frame processing step is used to bend the frame into shape, and then install the air pressure balance device along the air inlet and outlet of the frame. After the installation is completed, the inner side of the frame is filled with molecular sieves by a filling machine, and butyl glue is applied along the cover position of the frame surface to obtain a complete intermediate frame;

[0006] The glass semi-finished product processing step is used to put the tempered glass on the sheet and remove the film of the tempered glass structural adhesive. After the film removal is completed, the tempered glass is transported to an automatic film washing machine, deionized water is used to wash the tempered glass, and then the tempered glass is dried to obtain the outer glass;

[0007] The composite process receives the intermediate frame obtained in the intermediate frame processing process and the outer glass obtained in the semi-finished glass processing process, and conveys them to the frame-mounting machine, and the butyl adhesive-coated side of the intermediate frame is bonded to the surface of the outer glass by the frame-mounting machine. After the bonding is completed, the outer glass with the intermediate frame is conveyed to the automatic flat press, and another piece of outer glass is closed by the automatic flat press and flat-pressed to obtain the hollow glass, and then the hollow glass is conveyed to the adjustment and inspection process;

[0008] After the insulating glass is obtained in the adjustment and inspection process, the thickness measuring instrument is connected to the middle layer of the central control glass to measure the thickness of the middle layer of the glass. The air pressure balance device is used to inflate or exhaust the air according to the thickness deviation of the middle layer, so that the layer thickness after the air pressure of the hollow layer is stabilized meets the requirements of the current production batch. Then, the air pressure balance device is sealed at the connection between the air inlet and the air outlet of the middle frame in turn to obtain ultra-flat insulating glass.

[0009] Preferably, the production process also includes a packaging process. After receiving the ultra-flat insulating glass, the packaging process injects sealant along the outer channel of the insulating glass through an automatic glue injection machine. After the injection is completed, the ultra-flat insulating glass is lowered to the placement rack by an automatic unloader and sent into a curing room to complete the curing process. After curing, the finished product can be packaged.

[0010] Preferably, the air pressure balancing device used in the intermediate frame processing step includes an air inlet plug, an air outlet plug and a hole plugging member for sealing the air inlet and air outlet pores of the intermediate frame, and the hole plugging member is detachably connected to the air pore plug and the air outlet plug.

[0011] Preferably, the air inlet plug-in and the air outlet plug-in both include a filling plug and an I-shaped compression bellows, wherein a threaded groove is provided on the inner side of the filling plug, and an intermediate layer sealing folding groove and a gas introduction folding groove are provided on the upper and lower sides of the I-shaped compression bellows respectively, the I-shaped compression bellows receives external gas supply through the gas introduction folding groove, and the I-shaped compression bellows inputs filling gas into the air inlet of the intermediate frame through the intermediate layer sealing folding groove, the hole plugging component includes a closing plug, a pressing plug, a filling plug and a threaded joint, and after the threaded joint is threadedly connected to the filling plug, the sealing of the air inlet or air outlet of the intermediate frame is achieved.

[0012] Preferably, the intermediate frame processing procedure is also used to open the air inlet and air outlet holes of the intermediate frame, so that the air inlet plug-in and the air outlet plug-in can be connected to the intermediate frame, and the air inlet and air outlet holes of the intermediate frame are respectively opened on both sides of the outer wall of the intermediate frame, wherein the air inlet is located on the lower side of the intermediate frame and is 68-70mm away from the bottom edge of the intermediate frame, and the air outlet is located on the upper side of the intermediate frame and is 78-80mm away from the top edge of the intermediate frame.

[0013] Compared with the prior art, the beneficial effects of the present invention are as follows: the present invention improves the preparation method of insulating glass, installs an air pressure balancing device before the sealing process of the central control glass, and adds an adjustment and inspection process. The thickness of the middle layer of the glass is measured after the insulating glass is obtained through the adjustment and inspection process. According to the deviation of the thickness of the middle layer, the air pressure balancing device is installed to perform inflation or exhaust treatment, so that the layer thickness after the air pressure of the hollow layer is stabilized meets the requirements of the current production batch, and then the air pressure balancing device is sealed at the connection between the air inlet and the air outlet of the middle frame in turn, thereby solving the image distortion caused by the processing technology of the insulating glass and reducing the process manufacturing cost and external quality loss. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] The present invention is further described below in conjunction with the accompanying drawings and embodiments.

[0015] Figure 1 is a flow chart of the present invention;

[0016] Figure 2 A schematic diagram of the state of installing an air pressure balancing device in the air inlet hole of the insulating glass in the present invention;

[0017] Figure 3 A schematic diagram of a state in which an air pressure balancing device is installed in the air outlet of the insulating glass in the present invention;

[0018] Figure 4 It is a schematic structural diagram of the air pressure balancing device for insulating glass in the present invention. DETAILED DESCRIPTION

[0019] In order to make the technical means, creative features, objectives and effects achieved by the present invention easy to understand, the present invention is further explained below in conjunction with specific implementation methods.

[0020] like Figure 1-Figure 4 As shown, the hollow glass and its manufacturing method described in the present invention include the following steps: an intermediate frame processing step, a glass semi-finished product processing step, a compounding step and an adjustment and inspection step.

[0021] The intermediate frame processing step is used to bend the frame into shape, and then install the air pressure balance device along the air inlet and outlet of the frame. After the installation is completed, the molecular sieve is filled on the inside of the frame through a filling machine, and butyl glue is applied along the cover position of the frame surface to obtain a complete intermediate frame.

[0022] The glass semi-finished product processing procedure is used to put the tempered glass on the sheet and remove the film on the tempered glass structural adhesive. After the film removal is completed, the tempered glass is transported to the automatic film washing machine, deionized water is used to clean the tempered glass, and then the tempered glass is dried to obtain the outer layer of glass.

[0023] The composite process receives the intermediate frame obtained from the intermediate frame processing process and the outer glass obtained from the semi-finished glass processing process, and conveys them to the upper frame machine. The butyl adhesive-coated side of the intermediate frame is bonded to the surface of the outer glass by the upper frame machine. After the bonding is completed, the outer glass with the intermediate frame is conveyed to the automatic flat press. The automatic flat press closes another piece of outer glass and performs flat pressing to obtain insulating glass. The insulating glass is then conveyed to the adjustment and inspection process.

[0024] After obtaining the insulating glass through the adjustment and inspection process, the thickness measuring instrument is connected to the middle layer of the central control glass to measure the thickness of the middle layer of the glass. According to the thickness deviation of the middle layer, the air pressure balance device is used to inflate or exhaust the air so that the thickness of the hollow layer after the air pressure is stabilized meets the requirements of the current production batch. Then, the air pressure balance device and the air inlet connection and the air outlet connection of the middle frame are sealed in turn to obtain ultra-flat insulating glass.

[0025] In this embodiment, the present invention aims to solve the problem that the traditional processing method of insulating glass for inspection and debugging of the middle layer is usually to conduct thickness inspection after the insulating glass is sealed as a whole in the insulating glass manufacturing process, and the sealant filled around the gas adjustment hole for filling and discharging gas needs to be independently sealed, and when the layer thickness of the current middle layer in the sealed state is detected to be unsatisfactory after the sealing is completed, the glue needs to be removed and filled again, the operation process is too cumbersome, and the processing efficiency in mass production is not ideal. The existing processing procedures of insulating glass are sheeting-film removal-cleaning and drying, followed by frame making-filling molecular sieve-coating butyl glue, and after completion, frame putting-sheeting-sheet pressing-sealing-sheet unloading-curing-inspection-packaging. Compared with the prior art, the processing sequence of the preparation method proposed in the present invention is divided into an intermediate frame processing step, a glass semi-finished product processing step, a compounding step, an adjustment and inspection step, and a packaging step, that is, the process of the present invention is frame bending - installing an air pressure balance device - filling molecular sieves - coating butyl glue, and then putting the glass on - removing the film - cleaning and drying - putting on the frame - closing the sheets - pressing the sheets - checking the inner and outer concavities of the middle control layer - adjusting the internal and external pressure balance of the middle control layer - sealing - unloading - curing - packaging. By comparing the preparation method of the present invention with the preparation method of the prior art, it can be learned that the improvement of the present invention lies in the installation of the air pressure balance device and the processing of the adjustment and inspection steps.

[0026] In this embodiment, the specific implementation steps of the present invention include:

[0027] S1. Prepare the glass to the upper part of the insulating line, so that it reaches the glass semi-finished product processing process, and then the glass is put on the insulating line by the loading machine, and the structural adhesive on the surface of the glass is removed by the film removal equipment, and after the treatment, it is sent to the automatic film washing machine for cleaning.

[0028] S2. The glass is sent to the automatic film washer, which completes the cleaning and drying process and then sends it to the frame loading process.

[0029] S3. Then the glass is transferred to the middle frame processing process. The automatic frame bending machine bends the appropriate size of the spacer frame according to the order requirements, and the inflatable plug-in of the insulating glass is used to install it on the insulating glass spacer frame.

[0030] S3. Use a butyl adhesive coating machine to evenly coat the glass spacer frame with butyl adhesive.

[0031] S4, the frame-mounting process installs the spacer frame coated with butyl rubber on one of the layers of glass as required, and after completion, it is transferred to the laminating process.

[0032] S5. In the laminating process, the two layers of glass are pressed together by an automatic press and then transferred to the next process.

[0033] S6. After the insulating glass is pressed, the air pressure balance device is used to inflate and exhaust the hollow layer. The thickness of the middle layer of the glass is measured by a thickness measuring instrument at the middle measuring point of the glass. After the thickness of the hollow layer meets the requirement, the sealing end of the air pressure balance device is wrapped with butyl rubber, and the air inlet is sealed first, and then the air outlet is sealed. The sealing process after the thickness is adjusted is carried out to ensure that the surface of the insulating glass has no inner concave or outer convexity, thereby obtaining an ultra-flat insulating glass surface.

[0034] S7. In the packaging process, the automatic glue injection machine is used to inject the sealant glue on the outer channel of the insulating glass. After the injection is completed, the glass is put on the placement rack by the automatic unloading machine, or it can be manually operated to send the central control glass to the curing room for curing treatment to complete the production of the insulating glass.

[0035] In an optional implementation of this embodiment, the production process also includes a packaging process. After the packaging process receives the ultra-flat insulating glass, sealant is injected along the outer channel of the insulating glass through an automatic glue injection machine. After the injection is completed, the ultra-flat insulating glass is lowered to the placement rack by an automatic unloader and sent into the curing room to complete the curing process. After curing, the finished product can be packaged.

[0036] In an optional implementation of this embodiment, the air pressure balancing device used in the intermediate frame processing process includes an air inlet plug, an air outlet plug and a hole plugging member for sealing the air inlet and air outlet pores of the intermediate frame, and the hole plugging member is detachably connected to the air pore plug and the air outlet plug.

[0037] The air inlet plug and the air outlet plug both include a hole-filling plug and an I-shaped compression leather cavity. Among them, a threaded groove is provided inside the hole-filling plug. Intermediate layer sealing folding grooves and gas inlet folding grooves are respectively provided on the upper and lower sides of the I-shaped compression leather cavity. The I-shaped compression leather cavity receives externally supplied gas through the gas inlet folding groove, and the I-shaped compression leather cavity inputs filling gas into the air inlet of the intermediate frame through the intermediate layer sealing folding groove. The hole-blocking plug member includes a sealing plug, a pressing plug, a filling plug, and a threaded joint. After the threaded joint is threadedly docked with the hole-filling plug, the air inlet or air outlet of the intermediate frame is sealed.

[0038] In this embodiment, in order to avoid the need to re-dissolve the glue and fill it when it is detected that the layer thickness under the current intermediate layer sealing state does not meet the requirements after the sealing has been completed, the present invention installs a pneumatic balance device at the positions of the air inlets and air outlets of the intermediate frame of the central control glass in the preparation process. The I-shaped compression leather cavity is fixed inside the hole-filling plug. After the hole-filling plug is placed inside the air inlet and air outlet, a sealing structural adhesive is injected along the gap between the air inlet and the hole-filling plug to achieve sealing. When the I-shaped compression leather cavity is in an uncompressed state, the intermediate layer sealing folding groove and the gas inlet folding groove remain in a state of air communication. The operator can insert a nozzle into the stuffing hole to inflate. After the sealing plug is inserted into the inside of the hole-filling plug, it is rotated by the threaded fit between the threaded joint and the threaded groove inside the hole-filling plug, so that the sealing plug part presses the hole-filling plug under the action of the thread. The I-shaped compression leather cavity is in a folded state under the action of pressure. At this time, the outer peripheral surface of the I-shaped compression leather cavity seals the gas inlet folding groove and the intermediate layer sealing folding groove after folding, so that the filling plug, the hole-filling plug, and the I-shaped compression leather cavity form a three-layer sealing structure for detecting the sealing of the front air inlet and air outlet. The gas inlet folding groove and the intermediate layer sealing groove are U-shaped grooves. After the I-shaped compression leather cavity is squeezed, both the gas inlet folding groove and the intermediate layer sealing groove are U-shaped grooves and are folded into a V shape under the compression action. At the same time, the gas inlet folding groove and the intermediate layer sealing groove are arranged in a staggered manner and will not communicate in the compressed state of the I-shaped compression leather cavity. Among them, the filling plug and the pressing plug are used to fill the gap between the threaded joint and the threaded groove of the hole-filling plug. During the debugging and inspection process, due to the setting of the pneumatic balance device, the internal air pressure of the intermediate layer can be adjusted at any time.

[0039] The intermediate frame processing procedure is also used for the opening of the air inlets and air outlets of the intermediate frame, so that the air inlet plug and the air outlet plug can be connected to the intermediate frame. The air inlets and air outlets of the intermediate frame are respectively opened on both sides of the outer wall of the intermediate frame. Among them, the air inlet is located on the lower side of the intermediate frame and is 68 - 70 mm away from the bottom edge of the intermediate frame, and the air outlet is located on the upper side of the intermediate frame and is 78 - 80 mm away from the top edge of the intermediate frame.

[0040] In this embodiment, a one-time bending frame is used, and after the sheets are combined and pressed, an air hole is punched at the 68-70mm㎜ position on the lower side of the insulating glass spacer frame for inflation, and an air hole is punched at the 78-80mm㎜ position on the upper side of the spacer frame to exhaust and vent the insulating glass. Then, the middle of the glass is used as a thickness measurement point, and a thickness measuring instrument is used to measure the thickness of the middle layer of the glass. After the thickness of the hollow layer meets the requirement, butyl rubber is wrapped around the windward end of the air pressure balance device to first seal the air inlet hole and then seal the air outlet hole to ensure that there is no concave or convex on the surface of the insulating glass, thereby obtaining an ultra-flat insulating glass surface.

[0041] The above shows and describes the basic principles, main features and advantages of the present invention. Those skilled in the art should understand that the present invention is not limited to the above embodiments. The above embodiments and descriptions are only for explaining the principles of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention. The scope of the present invention is defined by the attached claims and their equivalents.

Claims

1. A method for manufacturing insulating glass, characterized in that: It includes the following processes: intermediate frame processing process, glass semi-finished product processing process, compounding process and adjustment and inspection process; The intermediate frame processing step is used to bend the frame into shape, and then install the air pressure balance device along the air inlet and outlet of the frame. After the installation is completed, the inner side of the frame is filled with molecular sieves by a filling machine, and butyl glue is applied along the cover position of the frame surface to obtain a complete intermediate frame; The glass semi-finished product processing step is used to put the tempered glass on the sheet and remove the film of the tempered glass structural adhesive. After the film removal is completed, the tempered glass is transported to an automatic film washing machine, deionized water is used to wash the tempered glass, and then the tempered glass is dried to obtain the outer glass; The composite process receives the intermediate frame obtained in the intermediate frame processing process and the outer glass obtained in the semi-finished glass processing process, and conveys them to the frame-mounting machine, and the butyl adhesive-coated side of the intermediate frame is bonded to the surface of the outer glass by the frame-mounting machine. After the bonding is completed, the outer glass with the intermediate frame is conveyed to the automatic flat press, and another piece of outer glass is closed by the automatic flat press and flat-pressed to obtain the hollow glass, and then the hollow glass is conveyed to the adjustment and inspection process; After the insulating glass is obtained in the adjustment and inspection process, the thickness measuring instrument is connected to the middle layer of the central control glass to measure the thickness of the middle layer of the glass. The air pressure balance device is used to inflate or exhaust the air according to the thickness deviation of the middle layer, so that the layer thickness after the air pressure of the hollow layer is stabilized meets the requirements of the current production batch. Then, the air pressure balance device is sealed at the connection between the air inlet and the air outlet of the middle frame in turn to obtain ultra-flat insulating glass.

2. The method for manufacturing insulating glass according to claim 1, characterized in that: The production process also includes a packaging process. After receiving the ultra-flat insulating glass, the packaging process injects sealant along the outer channel of the insulating glass through an automatic glue injection machine. After the injection is completed, the ultra-flat insulating glass is lowered to the placement rack by an automatic unloader and sent into the curing room to complete the curing process. After curing, the finished product can be packaged.

3. The method for manufacturing insulating glass according to claim 1, characterized in that: The air pressure balancing device used in the intermediate frame processing step includes an air inlet plug, an air outlet plug and a hole plug for sealing the air inlet and air outlet pores of the intermediate frame. The hole plug is detachably connected to the air hole plug and the air outlet plug.

4. The method for manufacturing insulating glass according to claim 3, characterized in that: The air inlet plug-in and the air outlet plug-in both include a filling plug and an I-shaped compression bellows, wherein a threaded groove is provided on the inner side of the filling plug, and an intermediate layer sealing folding groove and a gas introduction folding groove are provided on the upper and lower sides of the I-shaped compression bellows respectively, the I-shaped compression bellows receives external gas supply through the gas introduction folding groove, and the I-shaped compression bellows inputs filling gas into the air inlet of the intermediate frame through the intermediate layer sealing folding groove, the hole plugging component includes a closing plug, a pressing plug, a filling plug and a threaded joint, and after the threaded joint is threadedly connected with the filling plug, the sealing of the air inlet or air outlet of the intermediate frame is achieved.

5. The method for manufacturing insulating glass according to claim 1, characterized in that: The intermediate frame processing procedure is also used to open the air inlet and air outlet of the intermediate frame, so that the air inlet plug-in and the air outlet plug-in can be connected to the intermediate frame, and the air inlet and air outlet of the intermediate frame are respectively opened on both sides of the outer wall of the intermediate frame, wherein the air inlet is located on the lower side of the intermediate frame and is 68-70mm away from the bottom edge of the intermediate frame, and the air outlet is located on the upper side of the intermediate frame and is 78-80mm away from the top edge of the intermediate frame.

6. A hollow glass, characterized in that: The insulating glass is obtained by the method for preparing the insulating glass according to any one of claims 1 to 5.