Anti-freezing wellhead thermal insulation material and use method thereof

By using anti-freeze wellhead insulation materials made of cement and other materials, and providing electric heating with photovoltaic effect, the problems of aging of insulation materials, gap seepage, freezing blockage and other problems in the existing technology have been solved, and more efficient and environmentally friendly insulation effects have been achieved. Security.

CN118908635AInactive Publication Date: 2024-11-08TIANJIN QIANHAI PETROLEUM EQUIPMENT MANUFACTURING CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410981969.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-22
Publication Date
2024-11-08
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The existing anti-freeze wellhead insulation materials aged in high temperature environments, resulting in increased replacement frequency, gaps lead to rainwater seepage, causing pipeline corrosion, poor insulation effect in winter, prone to freezing, cracking, and polluting the environment. The materials are harmful to the human body, and the dismantling cost is high. .

Method used

Antifreeze wellhead insulation material made of cement, fly ash, slag powder, fiber materials, silicate gelling, antifreeze and biomass ash. By stirring and pre-wetting the fiber material, the addition of antifreeze reduces the freezing point, combined with the photovoltaic effect Provide electric heating belts to ensure thermal insulation and environmental protection.

Benefits of technology

It extends the service life of insulation materials, reduces the frequency of replacement, avoids freezing cracks and corrosion, reduces environmental pollution and human injuries, improves the stability of winter production, and reduces employee labor intensity and safety risks.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118908635A_ABST
    Figure CN118908635A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of anti-freezing well mouth thermal insulation materials, and discloses an anti-freezing well mouth thermal insulation material and a using method thereof.The anti-freezing well mouth thermal insulation material is prepared from, by weight, 10-30 parts of cement, 10-30 parts of fly ash, 10-30 parts of slag powder, 0.5-2 parts of fiber materials, 5-20 parts of silicate gel, 0.5-5 parts of anti-freezing agent and 5-20 parts of biomass ash; the preparation method of the anti-freezing wellhead thermal insulation material comprises the following steps: S1, preparing quantitative cement, fly ash, slag powder, fiber material, silicate gel, anti-freezing agent and biomass ash. Light energy is converted into electric energy through the detachable heat preservation sleeve and the photovoltaic effect, the electric energy provides energy for the ribbon heater, the ribbon heater generates heat energy to provide heat for the water well, normal production of the water injection well in winter is guaranteed, the workload generated by pipeline replacement and field cleaning due to pipeline frost crack is reduced, and the labor intensity of workers is relieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of antifreeze wellhead thermal insulation materials, in particular to an antifreeze wellhead thermal insulation material and a use method thereof. Background Art

[0002] Antifreeze wellhead insulation materials are usually used to protect wellhead equipment from freezing in cold environments. However, in conventional insulation methods for water injection wells, the insulation layer is exposed to high temperatures in summer, causing serious aging of the material. The replacement frequency of the insulation cover for water injection wells increases, resulting in increased material consumption. At the same time, in conventional insulation methods for water injection wells, due to the wide gap between the insulation layer and the wellhead, rainwater flows along the gap to the insulation layer and is absorbed by the felt inside, causing the wrapped pipeline to be in a humid environment for a long time and be easily corroded.

[0003] Moreover, when the temperature is low in winter, the insulation layer has poor insulation effect, and pipelines and valves are prone to freezing, cracking, and leakage, causing pollution to the environment. At the same time, insulation materials such as fiberglass cloth and paint can cause harm to the human body, and the removed old insulation materials need to be specially disposed of, resulting in increased costs.

[0004] Therefore, those skilled in the art provide an antifreeze wellhead insulation material and a method of using the same to solve the problems raised in the above background technology. Summary of the invention

[0005] In view of the deficiencies in the prior art, the present invention provides an antifreeze wellhead insulation material and a method of using the same, which solves the problem that a wide gap between the insulation layer and the wellhead causes rainwater to flow along the gap to the insulation layer and be absorbed by the felt inside, resulting in the wrapped pipeline being in a humid environment for a long time, which is easy to be corroded; and when the seasonal temperature is low, the insulation effect of the insulation layer is poor, and the pipeline and valves are prone to freezing, cracking, and puncture leakage, causing pollution to the environment.

[0006] To achieve the above purpose, the present invention is implemented by the following technical scheme: the antifreeze wellhead insulation material comprises the following raw materials in parts by weight: 10 to 30 parts of cement, 10 to 30 parts of fly ash, 10 to 30 parts of slag powder, 0.5 to 2 parts of fiber material, 5 to 20 parts of silicate gelling agent, 0.5 to 5 parts of antifreeze agent, and 5 to 20 parts of biomass ash;

[0007] The method for preparing the antifreeze wellhead insulation material comprises the following steps:

[0008] S1. Prepare a certain amount of cement, fly ash, slag powder, fiber material, silicate gelling agent, antifreeze agent and biomass ash;

[0009] S2, placing cement, fly ash and slag powder in a container in turn, and mixing and stirring them with a stirrer to obtain a uniform dry mix, and at the same time, placing fiber material and water in a container for premixing to fully wet the fiber;

[0010] S3, adding the fiber material to the dry blend and stirring and mixing again to ensure that the fiber is evenly dispersed in the mixture;

[0011] S4, adding silicate gel to the mixture, stirring and mixing to obtain a uniform wet mix;

[0012] S5. Gradually add an appropriate amount of water to the wet mixture while stirring and mixing until a paste-like consistency is achieved;

[0013] S6. Add antifreeze to the mixture and stir thoroughly to ensure that the antifreeze is evenly dispersed in the mixture;

[0014] S7, gradually adding biomass ash to the mixture, and stirring and mixing to obtain a uniform mixture;

[0015] S8. After the mixture is prepared, it is inverted into a pre-prepared mold or construction site according to the needs, and compacted and shaped;

[0016] S9. Carry out maintenance according to the characteristics of the mixture and environmental conditions.

[0017] Fly ash and slag powder are used to improve the performance of cement, increase the material's cold resistance and thermal insulation properties; fiber materials can increase the toughness and crack resistance of concrete, and pre-wetting the fiber materials helps the fiber to fully combine with concrete; silicate gelling agents can improve the strength and durability of concrete and ensure that the mixture has sufficient bearing capacity and stability; gradually adding water and stirring can turn the dry mix into a slurry, ensuring that the mixture has appropriate fluidity and viscosity; adding antifreeze can lower the freezing point of the mixture, prevent freezing in cold environments, and ensure smooth construction; adding biomass ash can improve the working performance and impermeability of concrete, while being environmentally friendly; the mixture is inverted into a mold and compacted and shaped to ensure that the mixture has the desired shape and density after solidification; curing: curing is carried out according to the characteristics of the mixture and environmental conditions to ensure that the mixture can fully harden and reach the designed strength.

[0018] Preferably, the stirring time interval of the agitator for stirring and mixing in step S2 is 5min to 10min, and the stirring speed range of the agitator is 60r / min to 120r / min. The stirring time interval of the fiber material for stirring and mixing in step S3 is 5min to 10min, and the stirring speed range is 60r / min to 120r / min.

[0019] Preferably, the time interval for stirring and mixing after adding silicate gelation in step S4 is 5min to 15min, and the stirring speed interval is 80r / min to 100r / min. The stirring time interval of the stirrer in step S5 is 2min to 10min, and the stirring speed interval is 60r / min to 80r / min.

[0020] Preferably, the stirring speed range after adding the antifreeze agent in step S6 is 100 r / min to 120 r / min, and the stirring time range is 10 min to 20 min. The stirring speed range after adding the biomass ash in step S7 is 120 r / min to 140 r / min, and the stirring time range is 20 min to 30 min.

[0021] Preferably, the curing temperature range in step S8 is 5° C. to 25° C., and the humidity range is 50% to 80%.

[0022] The method for using the antifreeze wellhead insulation material comprises the following steps:

[0023] S1. Select the pre-buried location of the solar panel foundation according to the sunshine conditions and line direction;

[0024] S2. Tailor the wellhead and customize the corresponding insulation cover according to the wellhead size;

[0025] S3. Install solar panels and batteries according to the pre-buried solar panel foundation;

[0026] S4. After the installation is completed, conduct a test on photovoltaic power generation energy;

[0027] S5. Install a pre-customized detachable insulation cover according to the size and shape of the wellhead.

[0028] According to the sunshine conditions and the line direction, choose a suitable location for pre-embedding to ensure that the solar panels can obtain sufficient sunshine energy; tailor and customize the insulation cover to ensure that the insulation cover can completely cover the wellhead and provide effective insulation effect; use the photovoltaic effect to convert light energy into electrical energy to provide energy for the subsequent electric belts; photovoltaic power generation energy test to ensure the normal operation of the solar panels and battery system, and to provide stable energy for the subsequent electric belts.

[0029] Preferably, in step S3, the photovoltaic effect is used to directly convert light energy into electrical energy to provide energy to the electric heating belt in the thermal insulation material. The electric heating belt generates heat energy to provide heat for the water well, thereby ensuring normal production of the water injection well in winter.

[0030] Preferably, when installing the detachable insulation cover in the S5 step, the electric heating belt is first put on the bandage fixed inside the insulation cover, evenly distributed on the inner side of the insulation cover, and then wrapped on the corresponding position of the wellhead. The detachable insulation cover is connected by Velcro, tied with a drawstring, and fixed with an I-shaped buckle.

[0031] The present invention provides an antifreeze wellhead insulation material and a method of using the same. It has the following beneficial effects:

[0032] 1. The present invention installs a detachable insulation sleeve and utilizes the photovoltaic effect to directly convert light energy into electrical energy, providing energy to the electric belt in the insulation material. The electric belt generates heat energy to provide heat for the water well, ensuring the normal production of the injection well in winter, solving the workload caused by pipeline replacement and on-site cleaning due to pipeline freezing and cracking, reducing the labor intensity of employees, and improving employee job satisfaction.

[0033] 2. The present invention wears the electric heating belt into a bandage fixed inside the insulation sleeve, evenly distributes it inside the insulation sleeve, and then wraps it at the corresponding position of the wellhead. It also directly converts light energy into electrical energy by utilizing the photovoltaic effect to provide energy to the electric heating belt in the insulation material, thereby solving the safety risks of ground icing and employee slips and falls caused by pipeline freezing and cracking. At the same time, it solves the harm to employees caused by the spraying of high-pressure water columns due to pipeline leakage, thereby ensuring the personal safety of employees.

[0034] 3. The present invention prevents produced water from flowing into farmland and causing damage to crops, reduces problems between workers and farmers, and maintains unity and stability in the oil field. In addition, the preparation of the thermal insulation material adopts environmentally friendly materials to reduce environmental pollution. BRIEF DESCRIPTION OF THE DRAWINGS

[0035] Figure 1 It is a schematic diagram of a method for preparing the antifreeze wellhead insulation material of the present invention;

[0036] Figure 2 This is a schematic diagram of a method for using the antifreeze wellhead insulation material of the present invention;

[0037] Figure 3 It is a temperature comparison schematic diagram of wellhead temperature monitoring of the present invention. DETAILED DESCRIPTION

[0038] The following will be combined with the drawings in the specification of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0039] Embodiment 1:

[0040] Preparation method of antifreeze wellhead insulation material:

[0041] S1. Prepare a certain amount of cement 20 parts, fly ash 20 parts, slag powder 20 parts, fiber material 1 part, silicate gelling agent 10 parts, antifreeze agent 2 parts, and biomass ash 10 parts;

[0042] S2. Invert cement, fly ash and slag powder in a container in sequence and mix them with a stirrer for 8 minutes at a stirring speed of 100 r / min. At the same time, place fiber material and water in a container for premixing to fully wet the fiber. The premixing time is 5 minutes.

[0043] S3, adding the fiber material to the dry blend and stirring again, the stirring time is 8 minutes, the stirring speed is 100r / min, and the fiber is evenly dispersed in the mixture;

[0044] S4, adding silicate gel to the mixture, stirring and mixing for 10 minutes at a stirring speed of 90 r / min to obtain a uniform wet mixture;

[0045] S5. Gradually add an appropriate amount of water to the wet mixture and stir to achieve a paste-like viscosity. The stirring time is 5 minutes and the stirring speed is 70 r / min.

[0046] S6. Add antifreeze to the mixture and stir thoroughly for 15 min at a stirring speed of 110 r / min to ensure that the antifreeze is evenly dispersed in the mixture;

[0047] S7, gradually adding biomass ash to the mixture and stirring to mix, the stirring time is 30 minutes, the stirring speed is 130r / min, and a uniform mixture is obtained;

[0048] S8. After the mixture is prepared, it is inverted into a pre-prepared mold or construction site according to the needs, and compacted and shaped;

[0049] S9. Carry out maintenance according to the characteristics of the mixture and environmental conditions.

[0050] Directions:

[0051] S1. Select the pre-buried location of the solar panel foundation according to the sunshine conditions and line direction;

[0052] S2. Tailor the wellhead and customize the corresponding insulation cover according to the wellhead size;

[0053] S3. Install solar panels and batteries according to the pre-buried solar panel foundation;

[0054] S4. After the installation is completed, conduct a test on photovoltaic power generation energy;

[0055] S5. Install the pre-customized detachable insulation cover according to the size and shape of the wellhead. During installation, first put the electric heating belt into the bandage fixed inside the insulation cover, evenly distribute it on the inside of the insulation cover, and then wrap it around the corresponding position of the wellhead. The detachable insulation cover is connected with Velcro, tied with drawstring, and fixed with I-shaped buckle.

[0056] Summary: In this embodiment, the solar panel converts light energy directly into electrical energy through the photovoltaic effect, provides energy for the electric heating tape in the insulation material, and then generates heat energy to provide heat for the water well, ensuring the normal production of the injection well in winter. The installation of the detachable insulation cover adopts Velcro connection, drawstring bundling and I-shaped buckle fixing, which is convenient for disassembly and maintenance.

[0057] Embodiment 2:

[0058] Preparation method of antifreeze wellhead insulation material:

[0059] S1. Prepare a certain amount of cement 30 parts, fly ash 30 parts, slag powder 30 parts, fiber material 2 parts, silicate gelling agent 20 parts, antifreeze agent 5 parts, and biomass ash 20 parts;

[0060] S2. Invert cement, fly ash and slag powder in a container in sequence and mix them with a stirrer for 10 minutes at a stirring speed of 120 r / min. Meanwhile, place fiber material and water in a container for premixing to fully wet the fiber. The premixing time is 10 minutes.

[0061] S3, adding the fiber material to the dry blend and stirring again, the stirring time is 10 minutes, the stirring speed is 120r / min, and the fiber is evenly dispersed in the mixture;

[0062] S4, adding silicate gel to the mixture, stirring and mixing for 15 minutes at a stirring speed of 100 r / min to obtain a uniform wet mixture;

[0063] S5. Gradually add an appropriate amount of water to the wet mixture and stir to achieve a paste-like viscosity. The stirring time is 2 minutes and the stirring speed is 60 r / min.

[0064] S6. Add antifreeze to the mixture and stir thoroughly for 20 min at a stirring speed of 120 r / min to ensure that the antifreeze is evenly dispersed in the mixture;

[0065] S7, gradually adding biomass ash to the mixture and stirring to mix, the stirring time is 30 minutes, the stirring speed is 140r / min, to obtain a uniform mixture;

[0066] S8. After the mixture is prepared, it is inverted into a pre-prepared mold or construction site according to the needs, and compacted and shaped;

[0067] S9. Carry out maintenance according to the characteristics of the mixture and environmental conditions.

[0068] Directions:

[0069] S1. Select the pre-buried location of the solar panel foundation according to the sunshine conditions and line direction;

[0070] S2. Tailor the wellhead and customize the corresponding insulation cover according to the wellhead size;

[0071] S3. Install solar panels and batteries according to the pre-buried solar panel foundation;

[0072] S4. After the installation is completed, conduct a test on photovoltaic power generation energy;

[0073] S5. Install the pre-customized detachable insulation cover according to the size and shape of the wellhead. During installation, first put the electric heating belt into the bandage fixed inside the insulation cover, evenly distribute it on the inside of the insulation cover, and then wrap it around the corresponding position of the wellhead. The detachable insulation cover is connected with Velcro, tied with drawstring, and fixed with I-shaped buckle.

[0074] Summary: In this embodiment, the solar panel converts light energy directly into electrical energy through the photovoltaic effect, provides energy for the electric heating belt in the insulation material, and then generates heat energy to provide heat for the water well, ensuring the normal production of the water injection well in winter. The installation of the detachable insulation cover adopts Velcro connection, drawstring bundling and I-shaped buckle fixing, which is convenient for disassembly and maintenance. Compared with the first embodiment, the proportion of raw materials used in the second embodiment is higher, and the stirring time and stirring speed are different.

[0075] Embodiment three:

[0076] Preparation method of antifreeze wellhead insulation material:

[0077] S1. Prepare a certain amount of cement 25 parts, fly ash 25 parts, slag powder 25 parts, fiber material 1.5 parts, silicate gelling agent 15 parts, antifreeze agent 3 parts, and biomass ash 15 parts;

[0078] S2. Invert cement, fly ash and slag powder in a container in sequence and mix them with a stirrer for 9 minutes at a stirring speed of 110 r / min. Meanwhile, place fiber material and water in a container for premixing to fully wet the fiber. The premixing time is 7 minutes.

[0079] S3, adding the fiber material to the dry blend and stirring again, the stirring time is 9 minutes, the stirring speed is 110r / min, and the fiber is evenly dispersed in the mixture;

[0080] S4, adding silicate gel to the mixture, stirring and mixing for 12 minutes at a stirring speed of 100 r / min to obtain a uniform wet mixture;

[0081] S5. Gradually add an appropriate amount of water to the wet mixture and stir to achieve a paste-like viscosity. The stirring time is 4 minutes and the stirring speed is 80 r / min.

[0082] S6. Add antifreeze to the mixture and stir thoroughly for 18 min at a stirring speed of 120 r / min to ensure that the antifreeze is evenly dispersed in the mixture;

[0083] S7, gradually adding biomass ash to the mixture and stirring to mix, the stirring time is 35 minutes, the stirring speed is 150r / min, to obtain a uniform mixture;

[0084] S8. After the mixture is prepared, it is inverted into a pre-prepared mold or construction site according to the needs, and compacted and shaped;

[0085] S9. Carry out maintenance according to the characteristics of the mixture and environmental conditions.

[0086] Directions:

[0087] S1. Select the pre-buried location of the solar panel foundation according to the sunshine conditions and line direction;

[0088] S2. Tailor the wellhead and customize the corresponding insulation cover according to the wellhead size;

[0089] S3. Install solar panels and batteries according to the pre-buried solar panel foundation;

[0090] S4. After the installation is completed, conduct a test on photovoltaic power generation energy;

[0091] S5. Install the pre-customized detachable insulation cover according to the size and shape of the wellhead. During installation, first put the electric heating belt into the bandage fixed inside the insulation cover, evenly distribute it on the inside of the insulation cover, and then wrap it around the corresponding position of the wellhead. The detachable insulation cover is connected with Velcro, tied with drawstring, and fixed with I-shaped buckle.

[0092] Summary: In this embodiment, the solar panel converts light energy directly into electrical energy through the photovoltaic effect, provides energy for the electric heating belt in the insulation material, and then generates heat energy to provide heat for the water well, ensuring the normal production of the water injection well in winter. The installation of the detachable insulation cover adopts Velcro connection, drawstring bundling and I-shaped buckle fixing, which is convenient for disassembly and maintenance. Compared with Embodiment 1 and Embodiment 2, the raw material ratio, stirring time and stirring speed used in Embodiment 3 are adjusted to adapt to different needs and scenarios.

[0093] Embodiment 4:

[0094] Preparation method of antifreeze wellhead insulation material:

[0095] S1. Prepare a certain amount of cement 15 parts, fly ash 15 parts, slag powder 15 parts, fiber material 0.5 parts, silicate gelling agent 5 parts, antifreeze agent 1 part, biomass ash 5 parts;

[0096] S2. Invert cement, fly ash and slag powder in a container in sequence and mix them with a stirrer for 6 minutes at a stirring speed of 90 r / min. At the same time, place fiber material and water in a container for premixing to fully wet the fiber. The premixing time is 3 minutes.

[0097] S3, adding the fiber material to the dry blend and stirring again, the stirring time is 6 minutes, the stirring speed is 90r / min, and the fiber is evenly dispersed in the mixture;

[0098] S4, adding silicate gel to the mixture, stirring and mixing for 8 minutes at a stirring speed of 80 r / min to obtain a uniform wet mixture;

[0099] S5. Gradually add an appropriate amount of water to the wet mixture and stir to achieve a paste-like viscosity. The stirring time is 3 minutes and the stirring speed is 50 r / min.

[0100] S6. Add antifreeze to the mixture and stir thoroughly for 10 min at a stirring speed of 100 r / min to ensure that the antifreeze is evenly dispersed in the mixture;

[0101] S7, gradually adding biomass ash to the mixture and stirring to mix, the stirring time is 20 minutes, the stirring speed is 120r / min, to obtain a uniform mixture;

[0102] S8. After the mixture is prepared, it is inverted into a pre-prepared mold or construction site according to the needs, and compacted and shaped;

[0103] S9. Carry out maintenance according to the characteristics of the mixture and environmental conditions.

[0104] Directions:

[0105] S1. Select the pre-buried location of the solar panel foundation according to the sunshine conditions and line direction;

[0106] S2. Tailor the wellhead and customize the corresponding insulation cover according to the wellhead size;

[0107] S3. Install solar panels and batteries according to the pre-buried solar panel foundation;

[0108] S4. After the installation is completed, conduct a test on photovoltaic power generation energy;

[0109] S5. Install the pre-customized detachable insulation cover according to the size and shape of the wellhead. During installation, first put the electric heating belt into the bandage fixed inside the insulation cover, evenly distribute it on the inside of the insulation cover, and then wrap it around the corresponding position of the wellhead. The detachable insulation cover is connected with Velcro, tied with drawstring, and fixed with I-shaped buckle.

[0110] Summary: In this embodiment, the solar panel converts light energy directly into electrical energy through the photovoltaic effect, provides energy for the electric heating belt in the insulation material, and then generates heat energy to provide heat for the water well, ensuring the normal production of the water injection well in winter. The installation of the detachable insulation cover adopts Velcro connection, drawstring binding and I-shaped buckle fixing, which is convenient for disassembly and maintenance. Compared with Embodiment 1, Embodiment 2 and Embodiment 3, the proportion of raw materials used in Embodiment 4 is lower, and the stirring time and stirring speed are adjusted to adapt to different needs and scenarios.

[0111] Embodiment five:

[0112] Preparation method of antifreeze wellhead insulation material:

[0113] S1. Prepare a certain amount of cement 18 parts, fly ash 18 parts, slag powder 18 parts, fiber material 1 part, silicate gelling agent 12 parts, antifreeze agent 2.5 parts, and biomass ash 12 parts;

[0114] S2. Invert cement, fly ash and slag powder in a container in sequence and mix them with a stirrer for 7 minutes at a stirring speed of 95 r / min. Meanwhile, place fiber material and water in a container for premixing to fully wet the fiber. The premixing time is 4 minutes.

[0115] S3, adding the fiber material to the dry blend and stirring again, the stirring time is 7 minutes, the stirring speed is 95r / min, and the fiber is evenly dispersed in the mixture;

[0116] S4, adding silicate gel to the mixture, stirring and mixing for 9 minutes at a stirring speed of 85 r / min to obtain a uniform wet mixture;

[0117] S5. Gradually add an appropriate amount of water to the wet mixture and stir to achieve a slurry viscosity. The stirring time is 4 minutes and the stirring speed is 65 r / min.

[0118] S6. Add antifreeze to the mixture and stir thoroughly for 15 min at a stirring speed of 105 r / min to ensure that the antifreeze is evenly dispersed in the mixture;

[0119] S7, gradually adding biomass ash to the mixture and stirring to mix, the stirring time is 25 minutes, the stirring speed is 135r / min, to obtain a uniform mixture;

[0120] S8. After the mixture is prepared, it is inverted into a pre-prepared mold or construction site according to the needs, and compacted and shaped;

[0121] S9. Carry out maintenance according to the characteristics of the mixture and environmental conditions.

[0122] Directions:

[0123] S1. Select the pre-buried location of the solar panel foundation according to the sunshine conditions and line direction;

[0124] S2. Tailor the wellhead and customize the corresponding insulation cover according to the wellhead size;

[0125] S3. Install solar panels and batteries according to the pre-buried solar panel foundation;

[0126] S4. After the installation is completed, conduct a test on photovoltaic power generation energy;

[0127] S5. Install the pre-customized detachable insulation cover according to the size and shape of the wellhead. During installation, first put the electric heating belt into the bandage fixed inside the insulation cover, evenly distribute it on the inside of the insulation cover, and then wrap it around the corresponding position of the wellhead. The detachable insulation cover is connected with Velcro, tied with drawstring, and fixed with I-shaped buckle.

[0128] Summary: In this embodiment, the solar panel converts light energy directly into electrical energy through the photovoltaic effect, provides energy for the electric heating tape in the insulation material, and then generates heat energy to provide heat for the water well, ensuring the normal production of the water injection well in winter. The installation of the detachable insulation cover adopts Velcro connection, drawstring binding and I-shaped buckle fixing, which is convenient for disassembly and maintenance. Compared with Example 1, Example 2, Example 3 and Example 4, the raw material ratio, stirring time and stirring speed used in Example 5 are adjusted to adapt to different needs and scenarios.

[0129] Summary: Example 1 uses cement, fly ash, slag powder, fiber material, silicate gelling agent, antifreeze and biomass ash to prepare thermal insulation materials, and the stirring time, stirring speed and additive ratio are moderate; Example 2 uses a higher raw material ratio, and the stirring time and stirring speed are longer; Example 3 uses a moderate raw material ratio, and the stirring time and stirring speed are longer; Example 4 uses a lower raw material ratio, and the stirring time and stirring speed are shorter; Example 5 uses a moderate raw material ratio, and the stirring time and stirring speed are moderate. In general, each embodiment uses a solar panel to provide energy for the electric belt, converts light energy into electrical energy through the photovoltaic effect, and after the thermal insulation material is prepared, a detachable insulation cover is installed to ensure the thermal insulation performance of the wellhead, and it is convenient for disassembly and maintenance.

[0130] Comparative experiment 1: Comparative experiment on thermal insulation effect of thermal insulation materials

[0131] Experimental group 1: using the antifreeze wellhead insulation material prepared in Example 1

[0132] Experimental Group 2: Using the antifreeze wellhead insulation material prepared in Example 3

[0133] Control group: no insulation material was used

[0134] Experimental parameters:

[0135] Measurement time: Continuous measurement for 48 hours

[0136] Measurement indicators: wellhead temperature

[0137] Experimental data table:

[0138] Time (h) Experimental group 1 Temperature (℃) Experimental group 2 Temperature (℃) Temperature of control group (℃) 0 5 5 5 6 10 8 5 12 12 10 5 18 13 11 5 24 14 12 5 30 15 13 5 36 16 14 5 42 17 15 5 48 18 16 5

[0139] Analysis of experimental results: The experimental data show that the thermal insulation effect of experimental group 1 and experimental group 2 using antifreeze wellhead insulation materials is significantly better than that of the control group. Over time, the wellhead temperatures of experimental group 1 and experimental group 2 are higher than that of the control group, indicating that the antifreeze wellhead insulation material can effectively improve the thermal insulation performance of the wellhead and reduce heat loss.

[0140] Experiment 2: Comparative experiment of detachable insulation cover by installation method

[0141] Experimental group 1: using the detachable insulation cover installation method in Example 1

[0142] Experimental Group 2: Using the detachable insulation cover installation method in Example 5

[0143] Experimental parameters:

[0144] Measuring time: continuous measurement for 24 hours

[0145] Measurement indicators: wellhead temperature, fixation of insulation sleeve (velcro connection, drawstring binding, I-shaped buckle fixation)

[0146] Experimental data table:

[0147] time Experimental group 1 temperature Fixation method of experimental group 1 Experimental Group 2 Temperature Fixation method of experimental group 2 0h 5℃ Velcro connection 5℃ Velcro connection 6h 10℃ Drawstring tying 8℃ I-shaped buckle fixed 12h 12℃ Velcro connection 10℃ Drawstring tying 18h 13℃ I-shaped buckle fixed 11℃ Drawstring tying 24h 14℃ Velcro connection 12℃ I-shaped buckle fixed

[0148] Analysis of experimental results: It can be seen from the experimental data that the installation method of the detachable insulation cover has an impact on the thermal insulation effect. Experimental group 1 uses Velcro to fix the insulation cover, and the thermal insulation effect is relatively good and the temperature is relatively stable; Experimental group 2 uses drawstring bundling and I-shaped buckle fixing methods, and the thermal insulation effect is relatively poor, and the temperature fluctuates greatly, indicating that the Velcro connection method is more suitable for fixing the insulation cover and can effectively prevent heat loss.

[0149] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. Antifreeze wellhead insulation material, characterized in that: The raw material composition includes the following parts by weight: 10 to 30 parts of cement, 10 to 30 parts of fly ash, 10 to 30 parts of slag powder, 0.5 to 2 parts of fiber material, 5 to 20 parts of silicate gelling agent, 0.5 to 5 parts of antifreeze agent, and 5 to 20 parts of biomass ash; The method for preparing the antifreeze wellhead insulation material comprises the following steps: S1. Prepare a certain amount of cement, fly ash, slag powder, fiber material, silicate gelling agent, antifreeze agent and biomass ash; S2, placing cement, fly ash and slag powder in a container in turn, and mixing and stirring them with a stirrer to obtain a uniform dry mix, and at the same time, placing fiber material and water in a container for premixing to fully wet the fiber; S3, adding the fiber material to the dry blend and stirring and mixing again to ensure that the fiber is evenly dispersed in the mixture; S4, adding silicate gel to the mixture, stirring and mixing to obtain a uniform wet mix; S5. Gradually add an appropriate amount of water to the wet mixture while stirring and mixing until a paste-like consistency is achieved; S6. Add antifreeze to the mixture and stir thoroughly to ensure that the antifreeze is evenly dispersed in the mixture; S7, gradually adding biomass ash to the mixture, and stirring and mixing to obtain a uniform mixture; S8. After the mixture is prepared, it is inverted into a pre-prepared mold or construction site according to the needs, and compacted and shaped; S9. Carry out maintenance according to the characteristics of the mixture and environmental conditions.

2. The antifreeze wellhead insulation material according to claim 1, characterized in that: In step S2, the stirring time interval for stirring and mixing by the agitator is 5min to 10min, and the stirring speed interval of the agitator is 60r / min to 120r / min. In step S3, the stirring time interval for stirring and mixing the fiber material is 5min to 10min, and the stirring speed interval is 60r / min to 120r / min.

3. The antifreeze wellhead insulation material according to claim 1, characterized in that: In the step S4, the time interval for stirring and mixing after adding silicate gelation is 5 minutes to 15 minutes, and the stirring speed interval is 80 r / min to 100 r / min. In the step S5, the stirring time interval of the stirrer is 2 minutes to 10 minutes, and the stirring speed interval is 60 r / min to 80 r / min.

4. The antifreeze wellhead insulation material according to claim 1, characterized in that: The stirring speed range after adding the antifreeze agent in step S6 is 100 r / min to 120 r / min, and the stirring time range is 10 min to 20 min. The stirring speed range after adding the biomass ash in step S7 is 120 r / min to 140 r / min, and the stirring time range is 20 min to 30 min.

5. The antifreeze wellhead insulation material according to claim 1, characterized in that: The curing temperature range in the step S8 is 5° C. to 25° C., and the humidity range is 50% to 80%.

6. A method for using an antifreeze wellhead thermal insulation material, according to the antifreeze wellhead thermal insulation material according to any one of claims 1 to 5, characterized in that: The following steps are involved: S1. Select the pre-buried location of the solar panel foundation according to the sunshine conditions and line direction; S2. Tailor the wellhead and customize the corresponding insulation cover according to the wellhead size; S3. Install solar panels and batteries according to the pre-buried solar panel foundation; S4. After the installation is completed, conduct a test on photovoltaic power generation energy; S5. Install a pre-customized detachable insulation cover according to the size and shape of the wellhead.

7. The method for using the antifreeze wellhead insulation material according to claim 6, characterized in that: In the step S3, the photovoltaic effect is used to directly convert light energy into electrical energy to provide energy to the electric heating belt in the thermal insulation material. The electric heating belt generates heat energy to provide heat for the water well, thereby ensuring the normal production of the water injection well in winter.

8. The method for using the antifreeze wellhead insulation material according to claim 6, characterized in that: When installing the detachable insulation cover in the step S5, the electric heating belt is first put into the bandage fixed inside the insulation cover, evenly distributed inside the insulation cover, and then wrapped around the corresponding position of the wellhead. The detachable insulation cover is connected by Velcro, tied with a drawstring, and fixed with an I-shaped buckle.