Production equipment and method for separating ferrophosphorus from yellow phosphorus slag

Through multi-step processing in the equipment system, including crushing, screening, magnetic separation and high-temperature reduction reaction, the separation efficiency of yellow phosphorus furnace slag is successfully improved, iron metal impurities are reduced, and efficient and environmentally friendly resource recycling and product purity improvement are achieved.

CN118910348AInactive Publication Date: 2024-11-08YUNNAN COSDA NEW MATERIALS CO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202411406606.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-10
Publication Date
2024-11-08
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

In the prior art, when the yellow phosphorus furnace slag is separated, it is easy to cause more impurities to be recovered by iron metal, and the separation efficiency is low, making it difficult to effectively reduce iron metal impurities.

Method used

The equipment system including jaw crusher, vibrating screen, magnetic separator, stirring reactor, ball mill grinder and high-temperature reduction furnace is adopted. The equipment system includes jaw crusher, screening, magnetic separation, water washing, drying, reduction reaction and distillation separation are separated. Phosphorus elements and molten iron are further removed from impurities in the refining furnace and the purity of molten iron is improved.

Benefits of technology

It improves the separation efficiency of yellow phosphorus furnace slag, reduces the composition of iron metal impurities, achieves efficient and environmentally friendly resource recycling, and ensures the stability and purity of product quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118910348A_ABST
    Figure CN118910348A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of metal production and refining, in particular to production equipment and method for separating ferrophosphorus from yellow phosphorus slag, and the production equipment system for separating ferrophosphorus comprises a jaw crusher for crushing the yellow phosphorus slag; the vibrating screen is used for screening crushed powder of the jaw crusher; the magnetic separator is used for performing magnetic separation screening on the materials screened by the vibrating screen; the classifying conveyor is used for conveying the yellow phosphorus slag separated by the magnetic separator into the metal and nonmetal; according to the yellow phosphorus slag screening device, crushed yellow phosphorus slag enters the vertical conveying cylinder through the inclined pipe and the flexible butt joint pipe and then is conveyed back to the feeding hopper through the vertical conveying screw driven by the third servo motor, and reciprocating machining treatment is conducted till the needed screening effect is achieved. Due to the design of reciprocating circulation, not only is the treatment efficiency of the yellow phosphorus slag improved, but also the accuracy and the stability of a screening result are ensured, the processing time of the yellow phosphorus slag is effectively shortened, and impurity components in iron metal are reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of metal production and refining, and in particular to a production device and a method for separating ferrophosphorus from yellow phosphorus slag. Background Art

[0002] Yellow phosphorus is an important basic industrial raw material. With the expansion of the application fields and variety of some important phosphides (important intermediates in phosphorus chemical industry), especially high-quality phosphorus chemicals, the market has put forward new requirements for the quality of yellow phosphorus products. Therefore, a lot of research has been conducted on the purification methods of yellow phosphorus at home and abroad. However, due to the special properties of yellow phosphorus itself, the industrial yellow phosphorus purification technology is difficult to obtain from the aspects of safety, economy, reaction conditions and process, and many purification methods have not yet been industrialized. Due to the influence of factors such as raw materials, motors and electric furnace thermal conditions, yellow phosphorus products are inevitably mixed with impurities such as arsenic, organic matter (commonly known as oil), silicon, sulfur, iron and metal. The ordinary hot water rinsing method is used to purify yellow phosphorus, and the purification depth is prioritized. In particular, the removal of arsenic, organic matter and iron is more difficult. Arsenic mainly exists in phosphate rock in the form of arsenate. Since phosphorus and arsenic belong to two adjacent elements in the same main group and have many similar physical and chemical properties, arsenic is also reduced while reducing phosphorus during the production process. Most of the arsenic (41.5% by mass) is concentrated in the product yellow phosphorus, mainly in the form of arsenic phosphide, and eutectics are easily formed between phosphorus and arsenic, making it difficult to separate them. In the electric furnace, the volatile matter in the coke enters the condensation system with the phosphorus furnace gas, and most of it is condensed into liquid together with the phosphorus vapor to form organic matter in the yellow phosphorus. The organic matter (mainly hydrocarbons, phenols and polyaromatic hydrocarbons) has a strong affinity with yellow phosphorus and is difficult to separate. In the high temperature area, a small amount of fluorine and silicon dioxide generate silicon fluoride gas, and during condensation, a part of it is hydrolyzed into colloidal silicon dioxide and mixed into the yellow phosphorus. The invention of application number 201510957512.1 relates to a method for purifying yellow phosphorus, and specifically to the following method, which comprises: adding an oxidant to yellow phosphorus and stirring to remove impurities from the yellow phosphorus; and adding a solution containing an additive having a specific functional group in a chemical formula structure to the yellow phosphorus from which the impurities have been removed and stirring to remove impurities, thereby effectively removing impurities from the yellow phosphorus used as a raw material of phosphoric acid to improve the purity of the phosphoric acid. A Chinese patent discloses a purification process for yellow phosphorus (Announcement No. CN109607501B), which discloses a purification process for yellow phosphorus, comprising the following steps: I. heating and stirring yellow phosphorus and hydrogen peroxide, separating the yellow phosphorus, and washing with water; II. heating and stirring the yellow phosphorus washed in step I and a dearsenicizing adsorbent, separating the yellow phosphorus, and washing with water; III. adding the yellow phosphorus washed in step II to an oxidizing enhancer and nitric acid, heating and stirring, separating the yellow phosphorus, and washing with water; IV. heating and stirring the yellow phosphorus washed in step III and a deironizing adsorbent, separating the yellow phosphorus, and washing with water. The yellow phosphorus purification process of the present invention is simple, safe to operate, has high arsenic removal rate and iron removal rate, excellent phosphorus recovery rate, and is easy to achieve industrial scale-up. The patented technology solves the problem of low phosphorus recovery rate and limited purification effect faced by chemical and physical methods for removing impurities in yellow phosphorus.

[0003] However, in the prior art, yellow phosphorus slag is usually separated into metallic slag and non-metallic slag at the same time when separating ferrophosphorus, which easily leads to a large amount of impurities in the recovered iron metal. It is necessary to solve the problem of increasing the separation efficiency and reducing the iron metal impurities when separating yellow phosphorus slag in the prior art.

[0004] Therefore, those skilled in the art provide a production device and method for separating ferrophosphorus from yellow phosphorus slag to solve the problems raised in the above background technology. Summary of the invention

[0005] In order to solve the above technical problems, the present invention provides: A production equipment for separating ferrophosphorus from yellow phosphorus slag, the ferrophosphorus separation production equipment system comprises: Jaw crusher for crushing yellow phosphorus slag; A vibrating screen for screening the crushed powder of the jaw crusher; A magnetic separator for magnetically separating and screening the materials screened by the vibrating screen; A classification conveyor for conveying the yellow phosphorus slag separated into metallic and non-metallic types by the magnetic separator; a stirred reactor for mixing the classification conveyor with an external additive; A dryer for drying the material after being treated in the stirred reactor; A mixing and stirring machine for mixing the dried product after drying in the dryer; A ball mill for grinding the materials mixed by the mixer into powder; A high-temperature reduction furnace for high-temperature reduction of the material ground into powder by the ball mill; The magnetic separator comprises a magnetic separation closed cylinder, and three magnetic separation conveying cylinders are installed inside the magnetic separation closed cylinder, and the inner edges of the bottoms of the three magnetic separation conveying cylinders are equipped with graded screening nets with different mesh sizes; the magnetic separator can grade and screen out metal powders of different mesh sizes from the yellow phosphorus slag through the three graded screening nets.

[0006] Preferably: the drainage end of the stirred reactor is connected to a filtering device for filtering yellow phosphorus slag, and the drainage end of the filtering device is connected to a wastewater treatment device.

[0007] Preferably, the additives added to the stirred reactor are specifically reducing agents and slagging agents.

[0008] Preferably: the magnetic separator discharges the non-metallic slag magnetically filtered out from the yellow phosphorus slag for centralized treatment.

[0009] Preferably: when the high-temperature reduction furnace is heated at high temperature, the air in the internal space needs to be evacuated to a vacuum state, and an inert gas can be added.

[0010] Preferably: the high-temperature gas inside the high-temperature reduction furnace can be discharged and connected to a condenser, and the condensed water source condensed by the condenser is discharged and connected to a distillation separation device.

[0011] Preferably: the high-temperature reduction furnace can discharge molten iron and slag separated from metal.

[0012] Preferably: an electromagnetic magnetic screener capable of controlling the magnitude of the magnetic force is provided below the grading screening net, a discharge chute opened inside the magnetic separation closed cylinder is provided below the electromagnetic magnetic screener, a discharge hopper is sealed at the bottom of one inclined end of the discharge chute, a solenoid valve is installed between the discharge hopper and the discharge chute, a discharge hose for discharging the screened metal powder is connected to one end of the discharge hopper, the bottom of one inclined end of the discharge chute is connected to the magnetic separation conveying cylinder below, and a solenoid valve is installed at the connection.

[0013] Preferably: one end of the magnetic separation conveying cylinder is connected to a flexible connecting pipe, and one end of the flexible connecting pipe away from the magnetic separation conveying cylinder is connected to a vertical hopper for discharging non-metallic yellow phosphorus coal slag powder.

[0014] The present invention also provides: a production method for separating ferrophosphorus from yellow phosphorus slag, comprising the following steps: Step 1: slag pretreatment; The yellow phosphorus slag is crushed by a jaw crusher, and the crushed yellow phosphorus slag falls into the vibrating screen, and the yellow phosphorus slag is screened through a 100-mesh screen; The yellow phosphorus slag that does not pass through the vibrating screen is re-transmitted to the jaw crusher for crushing; The yellow phosphorus slag that has passed through the vibrating screen is discharged into the magnetic separator for magnetic separation of metal slag and non-metallic powder. The non-metallic powder slag in the magnetic separator can be discharged for centralized treatment. The metal powder slag magnetically separated in the magnetic separator is divided into three levels, which can be transported to the stirred reactor for separate treatment through the classification conveyor; The metal powder slag is first washed and stirred in the stirred reactor, and then the washing liquid is discharged through the filtering equipment, and the washed yellow phosphorus slag is dried by the dryer; Step 2: Selection of reducing agent and slagging agent; The reducing agent in the additive is selected to be a carbonaceous material such as coke, coal powder or carbon monoxide as the reducing agent; The slag-forming agent in the additive is selected to be limestone and quartz sand to adjust the melting point and fluidity of the slag and promote the effective separation of phosphorus and iron; Step 3: material mixing and grinding; The pretreated slag, reducing agent and slag-forming agent are mixed evenly according to the proportion, and equal amounts of reducing agent, slag-forming agent and yellow phosphorus slag are placed in a mixing and stirring machine for thorough mixing; The yellow phosphorus slag mixed with the reducing agent and the slag-forming agent is placed in a ball mill for grinding to increase the contact area between the reactants and accelerate the reduction reaction. Step 4: high temperature vacuum reduction reaction; The yellow phosphorus slag processed by the ball mill in step 3 is transferred to a high-temperature reduction furnace and heated to 1200-1500° C., while maintaining a vacuum state in the furnace to reduce phosphorus oxidation. After maintaining for 2-3 hours, the yellow phosphorus slag can be fully reduced; Step 5: Condensation and separation of phosphorus; The evaporated hot air in the high-temperature reduction furnace in step 4 is transferred to a condenser, and the phosphorus vapor is rapidly cooled after the reduction reaction is completed by utilizing the low boiling point of phosphorus to condense into a liquid or solid state; When the cooled phosphorus liquid or solid is separated and collected by physical methods, the phosphorus element after condensation of the liquid or solid is separated from the iron and other impurities in the slag by a distillation separation device, thereby completing the separation and collection of the phosphorus element in the yellow phosphorus slag; Step 6: Molten iron collection and slag treatment; After collecting the phosphorus element in the yellow phosphorus slag inside the high-temperature reduction furnace in step 4, the molten iron can be collected, and the solid slag remaining inside the high-temperature reduction furnace is treated harmlessly; Step 7: refining and purification of molten iron; The collected molten iron contains trace impurities, including the residue of the reducing agent that has not been completely reacted, trace elements in the slag, etc. In order to obtain high-purity iron products, the molten iron needs to be sent to a refining furnace for further processing. In the refining furnace, an appropriate amount of desulfurizer (such as lime) and deoxidizer (such as ferrosilicon) can be added to remove impurities such as sulfur and oxygen in the molten iron through chemical reactions. During the refining process, the appropriate temperature and air pressure in the furnace need to be maintained to ensure the effective removal of impurities and the stability of the quality of the molten iron. After refining, the purity and quality of the molten iron will be significantly improved to meet the needs of subsequent processing or use; Step 8: Exhaust gas treatment and environmental protection measures; During the entire production process, whether it is the pretreatment of yellow phosphorus slag, high-temperature reduction reaction or the refining process of molten iron, tail gas emissions may be generated. These tail gases may contain harmful gases, dust and other pollutants, which pose a threat to the environment and human health. Therefore, effective tail gas treatment measures must be taken. Dust removal equipment and tail gas purification devices can be installed at each emission point to remove harmful substances in the tail gas through filtration, adsorption, chemical reaction and other methods. At the same time, ventilation and air exchange at the production site should be strengthened to ensure the air quality of the working environment. In addition, production equipment and environmental protection facilities should be regularly maintained and inspected to ensure their normal operation and effective environmental protection role; Step 9: Product testing and quality control; In order to ensure that the quality and performance of the final product meet the standard requirements, strict quality control is required for each link in the production process. In the production process of separating ferrophosphorus from yellow phosphorus slag, raw materials, intermediate products and final products should be tested regularly. The test content includes but is not limited to the composition analysis of slag, purity and impurity content of molten iron, separation efficiency of phosphorus element, etc. Through the feedback of test results, the production process parameters and equipment operation status are adjusted in time to ensure the stability and reliability of product quality. At the same time, a complete quality management system and traceability mechanism are established to record and monitor each link in the production process so that the cause can be quickly located and corresponding corrective measures can be taken when problems arise.

[0015] Technical effects and advantages of the present invention: In the present invention, the entire process of slag treatment is aimed at achieving efficient and environmentally friendly resource recovery. First, the slag is initially crushed by a jaw crusher to ensure that the particles are fine and uniform, and then further screened by a vibrating screen. The slag that does not pass the screening will be recycled back to the crusher for treatment. The screened slag enters the magnetic separator, and the metal and non-metal components are effectively separated by an electromagnetic magnetic suction screen. The metal powder slag is classified by grade, washed, stirred, filtered and dried. The magnetic separator is uniquely designed, and can achieve graded screening and cyclic crushing of slag through a servo motor, worm gear drive and cylinder control, thereby ensuring the treatment effect.

[0016] In the present invention, the slag is mixed with a reducing agent and a slag-forming agent in an appropriate proportion, stirred and ground to improve the reaction efficiency. Subsequently, in a high-temperature reduction furnace, the slag undergoes a reduction reaction under a vacuum state, and the phosphorus is separated from iron and other impurities by a physical method by utilizing the low boiling point of phosphorus. The collected molten iron needs to be further refined to improve the quality, while the solid slag is subjected to harmless treatment.

[0017] The present invention uses a magnetic separator to efficiently crush the yellow phosphorus slag. The crushed yellow phosphorus slag enters a vertical transmission cylinder through an inclined inclined tube and a flexible butt tube, and is then transmitted back to a feed hopper by a vertical transmission screw driven by a servo motor for reciprocating processing until the desired screening effect is achieved. This reciprocating cycle design not only improves the processing efficiency of the yellow phosphorus slag, but also ensures the accuracy and stability of the screening results, effectively shortens the processing time of the yellow phosphorus slag, and reduces the impurity components in the iron metal. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 This is a schematic structural diagram of a production device and method for separating ferrophosphorus from yellow phosphorus slag provided by the present application; Figure 2 This is a schematic diagram of the structure of a magnetic separator in a production device for separating ferrophosphorus from yellow phosphorus slag provided by the present application; Figure 3 This is a schematic diagram of the structure of a side view of a production device for separating ferrophosphorus from yellow phosphorus slag provided by the present application; Figure 4 It is a structural schematic diagram of a lower hopper in a production device for separating ferrophosphorus from yellow phosphorus slag provided by the present application; Figure 5 This is a schematic structural diagram of a vertical transmission cylinder in a production device for separating ferrophosphorus from yellow phosphorus slag provided by the present application; Figure 6 This is a schematic structural diagram of a closed arc plate in a production device for separating ferrophosphorus from yellow phosphorus slag provided by the present application; Figure 7 It is a schematic structural diagram of a transverse transmission spiral in a production device for separating ferrophosphorus from yellow phosphorus slag provided in the present application.

[0019] In the figure: 1. Jaw crusher; 2. Vibrating screen; 3. Magnetic separator; 301. Magnetic separation closed cylinder; 302. Magnetic separation conveying cylinder; 303. Grading screening net; 304. Discharging chute; 305. Discharging hopper; 306. Discharging hose; 307. Closed arc plate; 308. External gear ring; 309. Gear rack; 310. Cylinder 1; 311. Transmission rod; 312. Horizontal transmission screw; 313. Worm gear; 314. Worm; 315. Servo motor 1; 316, flexible connecting pipe; 317, vertical hopper; 318, cylinder 2; 319, support frame; 320, crushing box; 321, crushing roller; 322, toothed disc; 323, servo motor 2; 324, inclined inclined pipe; 325, flexible butt pipe; 326, vertical transmission cylinder; 327, feed hopper; 328, vertical transmission screw; 329, servo motor 3; 330, electromagnetic magnetic screener; 4. Classification conveyor; 5. Stirring reactor; 6. Filtration equipment; 7. Wastewater treatment equipment; 8. Dryer; 9. Mixer; 10. Ball mill; 11. High-temperature reduction furnace; 12. Condenser; 13. Distillation separation device. DETAILED DESCRIPTION

[0020] The present invention is further described in detail below in conjunction with the accompanying drawings and specific embodiments. The embodiments of the present invention are provided for the purpose of illustration and description, and are not intended to be exhaustive or to limit the present invention to the disclosed forms. Many modifications and variations will be apparent to those of ordinary skill in the art. The embodiments are selected and described in order to better illustrate the principles and practical applications of the present invention, and to enable those of ordinary skill in the art to understand the present invention and thereby design various embodiments with various modifications suitable for specific uses.

[0021] For example, see Figure 1In this embodiment, a production equipment for separating ferrophosphorus from yellow phosphorus slag is provided. The ferrophosphorus separation production equipment system includes: Jaw crusher 1 for crushing yellow phosphorus slag; A vibrating screen 2 for screening the crushed powder of the jaw crusher 1; A magnetic separator 3 for magnetically separating and screening the materials screened by the vibrating screen 2; A classification conveyor 4 for conveying the yellow phosphorus slag separated into metallic and non-metallic types by the magnetic separator 3; a stirred reactor 5 for mixing the classification conveyor 4 with the external additive; A dryer 8 for drying the material after being treated in the stirred reactor 5; A mixing and stirring machine 9 for mixing the dried product in the dryer 8; A ball mill 10 for grinding the materials mixed by the mixer 9 into powder; A high-temperature reduction furnace 11 for performing high-temperature reduction on the powdered material ground by the ball mill 10; The drainage end of the stirred reactor 5 is connected to a filtering device 6 for filtering yellow phosphorus slag, and the drainage end of the filtering device 6 is connected to a wastewater treatment device 7 .

[0022] The filtering device 6 is used to separate the solid and liquid in the stirred reactor 5 after the additives react.

[0023] The additives added to the stirred reactor 5 are specifically a reducing agent and a slag-forming agent.

[0024] The magnetic separator 3 discharges the non-metallic slag magnetically filtered out from the yellow phosphorus slag for centralized treatment.

[0025] When the high-temperature reduction furnace 11 is heated at high temperature, the air in the internal space needs to be evacuated to a vacuum state, and inert gas can be added. The high-temperature gas inside the high-temperature reduction furnace 11 can be discharged and connected to a condenser 12, and the condensed water source condensed by the condenser 12 is discharged and connected to a distillation separation device 13.

[0026] The high-temperature reduction furnace 11 may discharge molten iron and slag separated from metal.

[0027] For example 2, please refer to Figures 2 to 7 In this embodiment, a magnetic separator 3 is provided in a production device for separating ferrophosphorus from yellow phosphorus slag; The magnetic separator 3 includes a magnetic separation closed cylinder 301, and three magnetic separation conveying cylinders 302 are installed inside the magnetic separation closed cylinder 301. The inner edges of the bottoms of the three magnetic separation conveying cylinders 302 are equipped with graded screening nets 303 with different mesh sizes; the magnetic separator 3 can grade and screen out metal powders of different mesh sizes from the yellow phosphorus slag through the three graded screening nets 303.

[0028] An electromagnetic magnetic screener 330 capable of controlling the magnitude of the magnetic attraction force is provided below the grading screening net 303, and a feed chute 304 opened inside the magnetic separation closed cylinder 301 is provided below the electromagnetic magnetic screener 330, and a feed hopper 305 is sealedly connected to the bottom of one inclined end of the feed chute 304, and a solenoid valve is installed between the feed hopper 305 and the feed chute 304, and a feed hose 306 for discharging the screened metal powder is connected to one end of the feed hopper 305, and the bottom of one inclined end of the feed chute 304 is connected to the magnetic separation conveying cylinder 302 below, and a solenoid valve is installed at the connection.

[0029] One end of the magnetic separation conveying cylinder 302 is connected to a flexible connecting pipe 316 , and the other end of the flexible connecting pipe 316 away from the magnetic separation conveying cylinder 302 is connected to a vertical hopper 317 for discharging non-metallic yellow phosphorus coal slag powder.

[0030] A closed arc plate 307 is provided below the grading screening net 303, and the closed arc plate 307 is tightly attached to the bottom of the magnetic separation closed cylinder 301. The outer wall of one end of the closed arc plate 307 is rotatably installed on the outside of the magnetic separation closed cylinder 301, and is fixedly equipped with an outer gear ring 308. The outer gear ring 308 is meshed with a gear rack 309, and a cylinder 310 is fixedly installed in the middle of the gear rack 309. The end of the cylinder 310 away from the gear rack 309 is installed on the outer wall of the magnetic separation closed cylinder 301.

[0031] A transmission rod 311 is rotatably installed on the inner side of the magnetic separation conveying cylinder 302, and a horizontal transmission screw 312 is fixedly installed on the outer wall of the transmission rod 311, which is close to the surface of the grading screening net 303. One end of the transmission rod 311 is sealed and rotatably penetrates the outside of the magnetic separation sealing cylinder 301, and a worm gear 313 is fixedly installed on the outer wall, and the worm gear 313 is meshed with a worm 314, and a servo motor 315 is connected to the top of the worm 314.

[0032] The upper and lower walls of the middle part of the vertical hopper 317 are both installed with a cylinder 2 318 , and the cylinder 2 318 is installed on the outer wall of the magnetic separation sealing cylinder 301 . The vertical hopper 317 can be vertically adjusted in height along the magnetic separation sealing cylinder 301 through the cylinder 2 318 .

[0033] The bottom end of the vertical hopper 317 is connected to a crushing box 320, and two crushing rollers 321 for crushing larger particles of powder are rotatably installed inside the crushing box 320. One end of the two crushing rollers 321 rotates through the outside of the crushing box 320 and is fixedly equipped with a toothed disc 322. The two crushing rollers 321 are meshed with each other through the toothed disc 322. The other end of the single crushing roller 321 passes through the outside of the crushing box 320 and is connected to a servo motor 323. The bottom of the crushing box 320 is connected to an inclined tube 324. The end of the inclined tube 324 away from the crushing box 320 is sealed and connected to a flexible butt tube 325. The end of the flexible butt tube 325 away from the inclined tube 324 is connected to a vertical transmission cylinder 326. A vertical transmission screw 328 is rotatably installed inside the vertical transmission cylinder 326. The bottom end of the vertical transmission screw 328 rotates and passes through the bottom end of the vertical transmission cylinder 326, and is connected to a servo motor 329. A feed hopper 327 is connected to the top of the vertical transmission cylinder 326, and the feed hopper 327 is sealed and docked with the magnetic separation conveying cylinder 302.

[0034] A support frame 319 is integrally fixed to the outer wall of the magnetic separation sealing cylinder 301 .

[0035] For example 3, please refer to Figure 1 In this embodiment, a production method for separating ferrophosphorus from yellow phosphorus slag is provided, comprising the following steps: Step 1: slag pretreatment; The yellow phosphorus slag is crushed by a jaw crusher 1, and the crushed yellow phosphorus slag falls into a vibrating screen 2, and the yellow phosphorus slag is sieved through a 100-mesh screen; The yellow phosphorus slag that does not pass through the vibrating screen 2 is re-transmitted to the jaw crusher 1 for crushing; The yellow phosphorus slag that has passed through the vibrating screen 2 is discharged into the magnetic separator 3, and the metal slag and non-metal powder are separated by magnetic separation. The non-metal powder slag in the magnetic separator 3 can be discharged for centralized treatment; The metal powder slag magnetically separated in the magnetic separator 3 is divided into three levels, which can be transported to the stirring reactor 5 through the classification conveyor 4 for separate treatment; The metal powder slag is firstly washed and stirred in the stirred reactor 5, and then the washing liquid is discharged through the filter 6, and the washed yellow phosphorus slag is dried by the dryer 8; Step 2: Selection of reducing agent and slagging agent; The reducing agent in the additive is selected to be a carbonaceous material such as coke, coal powder or carbon monoxide as the reducing agent; The slag-forming agent in the additive is selected to be limestone and quartz sand to adjust the melting point and fluidity of the slag and promote the effective separation of phosphorus and iron; Step 3: material mixing and grinding; The pretreated slag, reducing agent and slag-forming agent are mixed uniformly according to the proportion, and equal amounts of reducing agent, slag-forming agent and yellow phosphorus slag are placed in a mixing and stirring machine 9 for thorough mixing; The yellow phosphorus slag mixed with the reducing agent and the slag-forming agent is placed in the ball mill 10 for grinding to increase the contact area between the reactants and accelerate the reduction reaction; Step 4: high temperature vacuum reduction reaction; The yellow phosphorus slag processed by the ball mill 10 in step 3 is transferred to the high-temperature reduction furnace 11 and heated to 1200-1500° C., while maintaining a vacuum state in the furnace to reduce phosphorus oxidation. After maintaining for 2-3 hours, the yellow phosphorus slag can be fully reduced; Step 5: Condensation and separation of phosphorus; The evaporated hot air in the high-temperature reduction furnace 11 in step 4 is transmitted to the condenser 12, and the phosphorus vapor is condensed into liquid or solid by rapidly cooling after the reduction reaction by taking advantage of the low boiling point of phosphorus. When the cooled phosphorus liquid or solid is separated and collected by physical methods, the phosphorus element after condensation of the liquid or solid is separated from the iron and other impurities in the slag by the distillation method of the distillation separation device 13, so as to complete the separation and collection of the phosphorus element in the yellow phosphorus slag; Step 6: Molten iron collection and slag treatment; After collecting the phosphorus element in the yellow phosphorus slag inside the high-temperature reduction furnace 11 in step 4, the molten iron can be collected, and the solid slag remaining inside the high-temperature reduction furnace 11 can be harmlessly treated; Step 7: refining and purification of molten iron; The collected molten iron contains trace impurities, including the residue of the reducing agent that has not been completely reacted, trace elements in the slag, etc. In order to obtain high-purity iron products, the molten iron needs to be sent to a refining furnace for further processing. In the refining furnace, an appropriate amount of desulfurizer (such as lime) and deoxidizer (such as ferrosilicon) can be added to remove impurities such as sulfur and oxygen in the molten iron through chemical reactions. During the refining process, the appropriate temperature and air pressure in the furnace need to be maintained to ensure the effective removal of impurities and the stability of the quality of the molten iron. After refining, the purity and quality of the molten iron will be significantly improved to meet the needs of subsequent processing or use; Step 8: Exhaust gas treatment and environmental protection measures; During the entire production process, whether it is the pretreatment of yellow phosphorus slag, high-temperature reduction reaction or the refining process of molten iron, tail gas emissions may be generated. These tail gases may contain harmful gases, dust and other pollutants, which pose a threat to the environment and human health. Therefore, effective tail gas treatment measures must be taken. Dust removal equipment and tail gas purification devices can be installed at each emission point to remove harmful substances in the tail gas through filtration, adsorption, chemical reaction and other methods. At the same time, ventilation and air exchange at the production site should be strengthened to ensure the air quality of the working environment. In addition, production equipment and environmental protection facilities should be regularly maintained and inspected to ensure their normal operation and effective environmental protection role; Step 9: Product testing and quality control; In order to ensure that the quality and performance of the final product meet the standard requirements, strict quality control is required for each link in the production process. In the production process of separating ferrophosphorus from yellow phosphorus slag, raw materials, intermediate products and final products should be tested regularly. The test content includes but is not limited to the composition analysis of slag, purity and impurity content of molten iron, separation efficiency of phosphorus element, etc. Through the feedback of test results, the production process parameters and equipment operation status are adjusted in time to ensure the stability and reliability of product quality. At the same time, a complete quality management system and traceability mechanism are established to record and monitor each link in the production process so that the cause can be quickly located and corresponding corrective measures can be taken when problems arise.

[0036] According to the above embodiments, the working principle of the present invention is: The slag is first crushed by a jaw crusher 1, and then screened by a vibrating screen. The slag that fails to pass the screening will be re-entered into the jaw crusher 1 for processing to ensure that the slag particles are fine and uniform. The slag that passes the screening will enter the magnetic separator 3 for magnetic separation to separate the metal slag and non-metallic powder. The metal powder slag is classified by grade and transferred to the stirred reactor 5 for water washing, stirring and filtering, and then processed by the dryer 8.

[0037] When the magnetic separator 3 classifies the yellow phosphorus slag, the yellow phosphorus slag processed by the vibrating screen 2 is transferred to the inside of a magnetic separation conveying cylinder 302 through a feed hopper 327, and the servo motor 315 is started, and the servo motor 315 is started to drive the worm 314 to rotate, and the worm 314 rotates to engage the worm wheel 313 to rotate, so that the worm wheel 313 drives the transmission rod 311 to rotate, and the transmission rod 311 drives the horizontal transmission screw 312 to move close to the grading screening net 303; The yellow phosphorus slag of different mesh sizes can be screened along the graded screening net 303 to the inner side of the unloading chute 304. When the unloading chute 304 is screening the non-metallic powder of the yellow phosphorus slag, the solenoid valve installed on the unloading hopper 305 is in a closed state. The yellow phosphorus slag is sequentially dropped into the inner side of the magnetic separation conveying cylinder 302, and the yellow phosphorus slag is passed through the electromagnetic magnetic suction screener 330 to magnetically absorb the metal powder of the yellow phosphorus slag; The three magnetic separation conveying cylinders 302 can be opened or closed respectively and used separately; Start the cylinder 1 310, and the extension and contraction of the cylinder 1 310 can drive the gear rack 309 to move, and the gear rack 309 engages with the outer gear ring 308 to rotate, and the rotation of the outer gear ring 308 drives the closed arc plate 307 to rotate 180 degrees, so as to open or close the closure of the graded screening net 303; When the yellow phosphorus slag is reciprocated, the yellow phosphorus slag that has not passed through the grading screening net 303 falls into the vertical hopper 317 through the flexible connecting pipe 316, and enters the crushing box 320 through the vertical hopper 317, and after starting the servo motor 2 323, the servo motor 2 323 drives the single crushing roller 321 to rotate, so that the two crushing rollers 321 are meshed with each other through the toothed disc 322 to bite and crush the yellow phosphorus slag, and then discharged into the inclined inclined pipe 324, and discharged into the vertical transmission tube 326 through the flexible connecting pipe 325 connected to the inclined inclined pipe 324, and after starting the servo motor 329, the servo motor 329 starts to drive the vertical transmission screw 328 to rotate, and the yellow phosphorus slag that has been crushed again is transmitted to the feed hopper 327 in the vertical transmission tube 326 through the vertical transmission screw 328 for reciprocating processing; When the magnetic separator 3 classifies the yellow phosphorus slag, the entire process is designed to be both efficient and flexible. First, the yellow phosphorus slag that has been preliminarily treated by the vibrating screen 2 is fed into the magnetic separation conveying cylinder 302. By starting the servo motor 315, the worm 314 and the worm wheel 313 are driven to rotate, and then the horizontal transmission screw 312 is driven to move on the graded screening net 303, so as to achieve effective screening of yellow phosphorus slag of different mesh sizes. The non-metallic powder after screening is collected by the unloading chute 304, while the metal powder is adsorbed by the electromagnetic magnetic suction screener 330.

[0038] It is worth mentioning that the magnetic separation conveying cylinder 302 is flexible, and they can be opened or closed separately to meet different processing requirements. In addition, through the extension and contraction of the cylinder 1 310, the meshing rotation of the tooth rack 309 and the outer tooth ring 308, the closed arc plate 307 can rotate 180 degrees, so as to conveniently open or close the grading screening net 303, further enhancing the convenience of operation of the equipment.

[0039] For the yellow phosphorus slag that does not pass the graded screening net 303, they will be poured into the crushing box 320 for further crushing. The start of the servo motor 2 323 drives the two crushing rollers 321 to mesh with each other through the toothed disc 322, and the yellow phosphorus slag is efficiently bitten and crushed. The crushed yellow phosphorus slag enters the vertical transmission cylinder 326 through the inclined inclined pipe 324 and the flexible butt pipe 325, and then is transmitted back to the feed hopper 327 by the vertical transmission screw 328 driven by the servo motor 3 329, and is reciprocated until the desired screening effect is achieved. This reciprocating cycle design not only improves the processing efficiency of the yellow phosphorus slag, but also ensures the accuracy and stability of the screening results.

[0040] When the non-metallic yellow phosphorus slag is discharged, the electromagnetic valve at the bottom of the three lower hoppers 305 is opened to allow the non-metallic yellow phosphorus slag to be discharged directly; When the metallic yellow phosphorus slag is discharged, after closing the solenoid valve of the discharge chute 304 and opening the solenoid valve of the discharge hopper 305, and closing the electromagnetic magnetic screener 330, the metallic yellow phosphorus slag falls into the discharge chute 304, and the classification and grading of the yellow phosphorus slag can be completed.

[0041] Next, appropriate reducing agents (such as coke, coal powder or carbon monoxide) and slag-forming agents (such as limestone, quartz sand) are selected to adjust the melting point and fluidity of the slag and promote the effective separation of phosphorus and iron. These additives are mixed evenly with the pretreated slag in proportion, and are fully stirred in a mixer 9, and then sent to a ball mill 10 for grinding to increase the contact area between the reactants and accelerate the reduction reaction.

[0042] The ground slag is transferred to the high temperature reduction furnace 11, where the reduction reaction is carried out at a high temperature of 1200-1500°C and under vacuum for 2-3 hours to ensure sufficient reaction. After the reaction is completed, the phosphorus vapor is rapidly cooled to condense into liquid or solid state by taking advantage of the low boiling point of phosphorus, and the phosphorus element is separated from the iron and other impurities in the slag by physical methods such as distillation.

[0043] After the phosphorus element is separated, the molten iron is collected, and the solid slag in the high-temperature reduction furnace 11 is harmlessly treated. The collected molten iron needs to be further processed in a refining furnace, and desulfurizers and deoxidizers are added to remove impurities to improve the purity and quality of the molten iron.

[0044] During the entire production process, it is necessary to pay attention to exhaust gas treatment and environmental protection measures, install dust removal equipment and exhaust gas purification devices to ensure that the exhaust gas meets environmental protection standards. At the same time, strengthen ventilation at the production site to ensure the air quality of the working environment.

[0045] Finally, the products are regularly tested, including slag composition analysis, molten iron purity and impurity content, phosphorus separation efficiency, etc., and process parameters and equipment status are adjusted according to the test results to ensure stable and reliable product quality. At the same time, a quality management system and traceability mechanism are established to comprehensively monitor and record the production process.

[0046] In the present invention, unless otherwise clearly stipulated and limited, for example, it can be a fixed connection, a detachable connection, or an integrated one; it can be a mechanical connection or an electrical connection; it can be directly connected or indirectly connected through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. Unless otherwise clearly defined, for ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to the specific circumstances.

[0047] Obviously, the described embodiments are only some embodiments of the present invention, not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field and related fields without creative work should fall within the scope of protection of the present invention. The structures, devices and operating methods not specifically described and explained in the present invention are implemented according to the conventional means in the field unless otherwise specified and limited.

Claims

1. A production equipment for separating ferrophosphorus from yellow phosphorus slag, characterized in that: The separation ferrophosphorus production equipment system includes: A jaw crusher (1) for crushing yellow phosphorus slag; A vibrating screen (2) for screening the crushed powder of the jaw crusher (1); A magnetic separator (3) for magnetically separating and screening the material screened by the vibrating screen (2); A classification conveyor (4) for conveying the yellow phosphorus slag separated into metallic and non-metallic types by the magnetic separator (3); A stirred reactor (5) for mixing the classification conveyor (4) with an external additive; A dryer (8) for drying the material after being treated in the stirred reactor (5); A mixing and stirring machine (9) for mixing the dried product in the dryer (8); A ball mill (10) for grinding the materials mixed in the mixer (9) into powder; A high-temperature reduction furnace (11) for reducing the material ground into powder by the ball mill (10); The magnetic separator (3) comprises a magnetic separation closed cylinder (301), and three magnetic separation conveying cylinders (302) are installed inside the magnetic separation closed cylinder (301), and the inner edges of the bottoms of the three magnetic separation conveying cylinders (302) are equipped with grading screening nets (303) of different mesh sizes; the magnetic separator (3) grades and screens the yellow phosphorus slag through the three grading screening nets (303) to obtain metal powders of different mesh sizes.

2. The production equipment for separating ferrophosphorus from yellow phosphorus slag according to claim 1, characterized in that: The drainage end of the stirred reactor (5) is connected to a filtering device (6) for filtering yellow phosphorus slag, and the drainage end of the filtering device (6) is connected to a wastewater treatment device (7).

3. A production equipment for separating ferrophosphorus from yellow phosphorus slag according to claim 2, characterized in that: The additives added to the stirred reactor (5) are specifically a reducing agent and a slag-forming agent.

4. The production equipment for separating ferrophosphorus from yellow phosphorus slag according to claim 1, characterized in that: The magnetic separator (3) discharges the non-metallic slag magnetically filtered out from the yellow phosphorus slag for centralized treatment.

5. The production equipment for separating ferrophosphorus from yellow phosphorus slag according to claim 1, characterized in that: When heating is performed in the high-temperature reduction furnace (11), air needs to be evacuated from the internal space to a vacuum state, and inert gas is added.

6. A production equipment for separating ferrophosphorus from yellow phosphorus slag according to claim 5, characterized in that: The gas discharge from the high-temperature reduction furnace (11) is connected to a condenser (12), and the condensed water source condensed by the condenser (12) is discharged from a distillation separation device (13).

7. The production equipment for separating ferrophosphorus from yellow phosphorus slag according to claim 5, characterized in that: The high-temperature reduction furnace (11) discharges molten iron and slag separated from metal.

8. The production equipment for separating ferrophosphorus from yellow phosphorus slag according to claim 1, characterized in that: An electromagnetic magnetic screener (330) for controlling the magnitude of the magnetic attraction force is provided below the grading screening net (303). A material discharge chute (304) opened inside the magnetic separation closed cylinder (301) is provided below the electromagnetic magnetic screener (330). A material discharge hopper (305) is sealedly connected to the bottom of one inclined end of the material discharge chute (304). A solenoid valve is installed between the material discharge hopper (305) and the material discharge chute (304). A material discharge hose (306) for discharging screened metal powder is connected to one end of the material discharge chute (305). The bottom of one inclined end of the material discharge chute (304) is connected to the magnetic separation conveying cylinder (302) below, and a solenoid valve is installed at the connection.

9. The production equipment for separating ferrophosphorus from yellow phosphorus slag according to claim 8, characterized in that: One end of the magnetic separation conveying cylinder (302) is connected to a flexible connecting pipe (316), and one end of the flexible connecting pipe (316) away from the magnetic separation conveying cylinder (302) is connected to a vertical hopper (317) for discharging non-metallic yellow phosphorus coal slag powder.

10. A production method for separating ferrophosphorus from yellow phosphorus slag, characterized in that: The following steps are involved: Step 1: slag pretreatment; The yellow phosphorus slag is crushed by a jaw crusher (1), and the crushed yellow phosphorus slag falls into a vibrating screen (2) to perform screening on the yellow phosphorus slag; The yellow phosphorus slag that has not passed through the vibrating screen (2) is re-transmitted to the jaw crusher (1) for crushing; The yellow phosphorus slag that has passed through the vibrating screen (2) is discharged into a magnetic separator (3) to separate the metal slag and the non-metallic powder by magnetic separation, and the non-metallic powder slag in the magnetic separator (3) is discharged for centralized treatment; The metal powder slag magnetically separated in the magnetic separator (3) is divided into three levels and transported to the stirring reactor (5) for classification treatment via the classification conveyor (4); The metal powder slag is first washed and stirred in the stirred reactor (5), and then the washing liquid is discharged through the filtering device (6), and the washed yellow phosphorus slag is dried through the dryer (8); Step 2: Selection of reducing agent and slagging agent; Selecting the reducing agent in the additive as a carbonaceous material such as coke as the reducing agent; Select limestone as the slagging agent in the additive; Step 3: material mixing and grinding; The pretreated slag, reducing agent and slag-forming agent are mixed evenly, and the reducing agent, slag-forming agent and yellow phosphorus slag are placed in a mixing and stirring machine (9) for thorough mixing; The yellow phosphorus slag after mixing the reducing agent and the slag-forming agent is placed in a ball mill (10) for grinding to accelerate the reduction reaction; Step 4: vacuum reduction reaction; The yellow phosphorus slag processed by the ball mill (10) in step 3 is transferred to a high-temperature reduction furnace (11) and heated to 1200-1500° C., while maintaining a vacuum state in the furnace for 2-3 hours to allow the yellow phosphorus slag to fully undergo a reduction reaction; Step 5: Condensation and separation of phosphorus; The evaporated hot air in the high temperature reduction furnace (11) in step 4 is transmitted to the condenser (12) to condense the phosphorus vapor into liquid; When the cooled phosphorus liquid is separated and collected by physical methods, the phosphorus element after condensation of the liquid is separated from the iron impurities in the slag by a distillation method of the distillation separation device (13), thereby completing the separation and collection of the phosphorus element in the yellow phosphorus slag.

Citation Information

Patent Citations

  • Method for producing copper-powder-containing iron by reducing copper-containing furnace cinders directly

    CN102363218A

  • Equipment and method for producing yellow phosphorus from middle-low-grade phosphate ore

    CN107686099A

  • Method of extracting elements phosphorus and ferrum from yellow phosphorus byproduct ferrophosphorus slag

    CN108300826A

  • Production process and production equipment for preparing iron phosphate by taking yellow phosphorus byproduct ferrophosphorus slag as raw material

    CN114620697A

  • High-carbon ferrochrome electric furnace slag metal recovery system

    CN115466849A