Production method of desilting mechanical arm

By applying polyurethane wear-resistant and anti-corrosion coating on the bottom silt robot arm, the problem of corrosion and damage of the robot arm is solved, and its toughness and service life are improved, and underwater silt work is conveniently carried out.

CN118911220AInactive Publication Date: 2024-11-08XIAMEN XINLANG CONSTRUCTION ENGINEERING CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411223167.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-03
Publication Date
2024-11-08
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The robotic arms in existing bottom silting equipment are susceptible to corrosion and damage, have poor toughness, and are difficult to maintain an effective state during underwater work.

Method used

Polyurethane wear-resistant and anti-corrosion coating is used to mix isocyanate and resin through high-pressure mixing equipment and spray it on the surface of the robotic arm to form a 2mm-3mm thick coating, which increases corrosion and friction resistance and after the coating wears Repeatable to extend service life.

Benefits of technology

It effectively improves the toughness and strength of the robotic arm, extends the service life, and conveniently performs underwater dredging, improving the handling and durability of the equipment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118911220A_ABST
    Figure CN118911220A_ABST
Patent Text Reader

Abstract

The production method comprises the steps that a first machine arm and a second machine arm are provided, and the surface of the first machine arm and the surface of the second machine arm are coated with coatings; the end of the first arm is connected to the middle of the second arm through a rotating shaft; a first hydraulic driving rod is provided, the first end of the first hydraulic driving rod is connected to the middle of the first machine arm, and the second end of the first hydraulic driving rod is connected to the first end of the second machine arm; a second hydraulic driving rod is provided, the first end of the second hydraulic driving rod is connected to the first end of the second machine arm, and the second end of the second hydraulic driving rod is connected to the first end of a first connecting rod in the middle of the second machine arm. Through the arrangement of the structure, the surfaces of the first vehicle arm and the second vehicle arm are coated with the paint to form the coatings, the coatings can protect the first vehicle arm and the second vehicle arm, the anti-corrosion and anti-friction effects are achieved, meanwhile, the toughness and strength of the first vehicle arm and the second vehicle arm can be improved, and the service life of the product is prolonged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of dredging equipment, and in particular to a production method of a dredging mechanical arm. Background Art

[0002] Underwater dredging can effectively reduce the sediment deposited in the water, lower the height of the riverbed and lake bottom, improve the navigation capacity of rivers and lakes, and at the same time reduce the threat of floods, protect the ecological environment, and prevent the accumulation of sediment from damaging the ecological environment in the water. It has obvious significance in protecting people's livelihood and protecting the natural environment.

[0003] At present, the existing underwater dredging work mostly uses equipment such as excavators, dredging ships, suction dredging ships and sludge solidification devices; these devices all require the use of robotic arms to move dredging work heads such as reamer heads and buckets to the underwater working area. Therefore, the robotic arms are also underwater for a long time. Most of the robotic arms are made of metal or engineering plastics, which have poor toughness and are easily scratched during movement. The robotic arms are easily corroded and damaged.

[0004] To this end, the present invention provides a production method of a dredging robot arm, which can effectively solve the above problems. Summary of the invention

[0005] In order to overcome the deficiencies of the prior art, the present invention provides a production method of a dredging robot arm, which can effectively solve the above problems.

[0006] The technical solution adopted by the present invention to solve its technical problem is:

[0007] A production method of a dredging robot arm, comprising:

[0008] Providing a first machine arm and a second machine arm, and applying a coating on a surface of the first machine arm and a surface of the second machine arm;

[0009] Connecting the end of the first arm to the middle of the second arm via a rotating shaft;

[0010] Providing a first hydraulic drive rod, connecting a first end of the first hydraulic drive rod to the middle of the first machine arm, and connecting a second end of the first hydraulic drive rod to the first end of the second machine arm;

[0011] A second hydraulic drive rod is provided, a first end of the second hydraulic drive rod is connected to the first end of the second machine arm, and a second end of the second hydraulic drive rod is connected to the first end of the first connecting rod in the middle of the second machine arm.

[0012] Furthermore, the coating is a polyurethane wear-resistant and anti-corrosion coating.

[0013] Furthermore, the thickness of the coating is 2mm-3mm.

[0014] Furthermore, the step of applying a coating on the surface of the first arm and the surface of the second arm includes: heating the isocyanate and the resin to 60-71° C. respectively; using high-pressure mixing equipment to mix the isocyanate and the resin in a 1:1 ratio, and atomizing and spraying them on the surface of the first arm and the surface of the second arm.

[0015] Furthermore, the equipment hydraulic pressure of the high-pressure mixing equipment is 3.8-17.2 MPa.

[0016] Furthermore, before the step of coating the first arm surface and the second arm surface, the first arm surface and the second arm surface are also pre-treated to cut off protruding parts, fill structural gaps, clean and dry.

[0017] Furthermore, after the step of coating the first arm surface and the second arm surface, the method further includes checking the coating thickness. When the coating thickness is less than 2 mm, repeating the step of coating the first arm surface and the second arm surface.

[0018] Furthermore, after the step of pretreating the first arm surface and the second arm surface and before the step of coating the first arm surface and the second arm surface, the method further includes: treating the first arm surface and the second arm surface with a surface treatment liquid.

[0019] Furthermore, a second connecting rod is provided, and the second end of the first connecting rod is connected to the middle of the second machine arm, and the first end of the second connecting rod is connected to the first end of the first connecting rod and / or the second end of the second hydraulic drive rod.

[0020] Furthermore, the surfaces of the first arm and the second arm are both provided with reinforcing ribs, the reinforcing ribs are arranged obliquely, and two adjacent reinforcing ribs are connected end to end in sequence.

[0021] The beneficial effects of the present invention are as follows: through the arrangement of the above-mentioned structure, paint is applied on the surface of the first arm and the surface of the second arm to form a coating, which can protect the first arm and the second arm, achieve anti-corrosion and anti-friction effects, and at the same time improve the toughness and strength of the first arm and the second arm, thereby improving the service life of the product; and after the coating is worn and thinned, the paint can be applied again to strengthen the coating, thereby further improving the service life of the product; the first hydraulic drive rod is extended and retracted to drive the first arm and the second arm to rotate relative to each other; the second hydraulic drive rod is extended and retracted to drive the output end connected to the second arm to rotate relative to the second arm, thereby facilitating the user to control the robotic arm and conveniently perform underwater dredging work. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for use in the description of the embodiments. The drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.

[0023] The present invention is further described below in conjunction with the accompanying drawings and embodiments.

[0024] Figure 1 It is a schematic diagram of the overall structure of the dredging mechanical arm of the present invention;

[0025] Figure 2 is a flow chart of a first embodiment of the present invention;

[0026] Figure 3 is a flow chart of a second embodiment of the present invention;

[0027] Figure 4 is a flow chart of a third embodiment of the present invention;

[0028] Figure 5 is a flow chart of a fourth embodiment of the present invention;

[0029] Figure 6 is a flow chart of the fifth embodiment of the present invention. DETAILED DESCRIPTION

[0030] Embodiment 1

[0031] Reference Figure 1 and Figure 2 , a production method of a dredging robot arm, comprising:

[0032] Step S101, providing a first arm 10 and a second arm 20, and applying a coating on the surface of the first arm 10 and the surface of the second arm 20;

[0033] Step S102, connecting the end of the first arm 10 to the middle of the second arm 20 via a rotating shaft;

[0034] Step S103, providing a first hydraulic driving rod 30, connecting a first end of the first hydraulic driving rod 30 to the middle of the first machine arm 10, and connecting a second end of the first hydraulic driving rod 30 to a first end of the second machine arm 20;

[0035] Step S104 , providing a second hydraulic driving rod 40 , connecting a first end of the second hydraulic driving rod 40 to a first end of the second arm 20 , and connecting a second end of the second hydraulic driving rod 40 to a first end of a first connecting rod 50 in the middle of the second arm 20 .

[0036] Through the arrangement of the above structure, paint is applied on the surface of the first arm 10 and the surface of the second arm 20 to form a coating, which can protect the first arm 10 and the second arm 20 to achieve anti-corrosion and anti-friction effects, while improving the toughness and strength of the first arm 10 and the second arm 20, thereby increasing the service life of the product; and after the coating is worn and thinned, the paint can be applied again to strengthen the coating, thereby further increasing the service life of the product; the first hydraulic drive rod 30 is extended and retracted to drive the first arm 10 and the second arm 20 to rotate relative to each other; the second hydraulic drive rod 40 is extended and retracted to drive the output end connected to the second arm 20 to rotate relative to the second arm 20, thereby facilitating the user to control the robotic arm and conveniently perform underwater dredging work.

[0037] Preferably, the coating is a coating formed of a polyurethane wear-resistant and anti-corrosion material, which has stronger corrosion resistance and wear resistance and is easy to apply.

[0038] Preferably, the thickness of the coating is 2-3 mm. A coating of this thickness is easy to shape, and the anti-corrosion and anti-friction effects can also achieve the expected results. It also does not affect the appearance and structure of the first arm 10 and the second arm 20, thereby ensuring the flexibility of the first arm 10 and the second arm 20 and facilitating users to operate the arms.

[0039] Preferably, a second connecting rod 60 is provided, and the second end of the first connecting rod 50 is connected to the middle of the second machine arm 20, and the first end of the second connecting rod 60 is connected to the first end of the first connecting rod 50 and / or the second end of the second hydraulic drive rod 40. Through the arrangement of the above structure, the second hydraulic drive rod 40 is extended and retracted, driving the first end of the first connecting rod 50 and the first end of the second connecting rod 60 to move, and then driving the bucket, reamer head and other dredging devices connected to the second end of the second machine arm 20 to rotate relative to the second machine arm 20, so that the user can control the movement of the mechanical arm and the bucket, reamer head and other dredging devices connected to the mechanical arm, and the operation is convenient.

[0040] Among them, the surfaces of the first machine arm 10 and the second machine arm 20 are both provided with reinforcing ribs 12, the reinforcing ribs 12 are arranged obliquely, and two adjacent reinforcing ribs 12 are sequentially connected end to end. Through the arrangement of the above structure, the surfaces of the first machine arm 10 and the second machine arm 20 are both provided with reinforcing ribs 12, which can effectively strengthen the strength of the first machine arm 10 and the second machine arm 20, and improve the stability and service life of the product; and the adjacent reinforcing ribs 12 are sequentially connected end to end, and the two adjacent reinforcing ribs 12 and the edge of the first machine arm 10 or the second machine arm 20 form a triangular stable structure, which further improves the strength and stability of the product, and can reduce the weight of the mechanical arm, reduce the energy consumed by operating the mechanical arm, save energy, and reduce the cost of the product.

[0041] Embodiment 2

[0042] Reference Figure 1 and Figure 3 , a production method of a dredging robot arm, comprising:

[0043] Step S2011, heating the isocyanate and the resin to 60-71° C. respectively;

[0044] Step S2012, using a high-pressure mixing device to mix the isocyanate and the resin in a ratio of 1:1, and spraying the mixture onto the surface of the first arm 10 and the surface of the second arm 20 in an atomized manner;

[0045] Step S202, connecting the end of the first arm 10 to the middle of the second arm 20 via a rotating shaft;

[0046] Step S203, providing a first hydraulic driving rod 30, connecting a first end of the first hydraulic driving rod 30 to the middle of the first machine arm 10, and connecting a second end of the first hydraulic driving rod 30 to a first end of the second machine arm 20;

[0047] Step S204 , providing a second hydraulic drive rod 40 , connecting a first end of the second hydraulic drive rod 40 to a first end of the second arm 20 , and connecting a second end of the second hydraulic drive rod 40 to a first end of a first connecting rod 50 in the middle of the second arm 20 .

[0048] Through the arrangement of the above structure, the coating is applied on the surface of the first arm 10 and the surface of the second arm 20 to form a coating, which can protect the first arm 10 and the second arm 20, achieve the effect of anti-corrosion and anti-friction, and at the same time improve the toughness and strength of the first arm 10 and the second arm 20, and improve the service life of the product; and after the coating is worn and thinned, the coating can be applied again to strengthen the coating, further improving the service life of the product; the first hydraulic drive rod 30 is extended and retracted to drive the first arm 10 and the second arm 20 to rotate relative to each other; the second hydraulic drive rod 40 is extended and retracted to drive the output end connected to the second arm 20 to rotate relative to the second arm 20, which is convenient for users to control the mechanical arm and conveniently perform underwater dredging. The isocyanate and the resin are heated to the reaction temperature, generally 60-71°C, respectively, and the two are mixed and sprayed on the surface of the first arm 10 and the surface of the second arm 20. The isocyanate and the resin react on the surface of the first arm 10 and the surface of the second arm 20 to form a coating, which can quickly achieve the laminating work with high production efficiency.

[0049] Embodiment 3

[0050] Reference Figure 1 and Figure 4 , a production method of a dredging robot arm, comprising:

[0051] Step S301, pre-treating the surface of the first arm 10 and the surface of the second arm 20, cutting off protruding parts, filling structural gaps, cleaning and drying;

[0052] Step S3021, heating the isocyanate and the resin to 60-71° C. respectively;

[0053] Step S3022, using a high-pressure mixing device to mix the isocyanate and the resin in a ratio of 1:1, and spraying the mixture onto the surface of the first arm 10 and the surface of the second arm 20 in an atomized manner;

[0054] Step S303, connecting the end of the first arm 10 to the middle of the second arm 20 via a rotating shaft;

[0055] Step S304, providing a first hydraulic driving rod 30, connecting a first end of the first hydraulic driving rod 30 to the middle of the first machine arm 10, and connecting a second end of the first hydraulic driving rod 30 to a first end of the second machine arm 20;

[0056] Step S305 , providing a second hydraulic driving rod 40 , connecting the first end of the second hydraulic driving rod 40 to the first end of the second arm 20 , and connecting the second end of the second hydraulic driving rod 40 to the first end of the first connecting rod 50 in the middle of the second arm 20 .

[0057] By setting the above structure, paint is applied on the surface of the first arm 10 and the surface of the second arm 20 to form a coating, which can protect the first arm 10 and the second arm 20, achieve anti-corrosion and anti-friction effects, and at the same time improve the toughness and strength of the first arm 10 and the second arm 20, thereby improving the service life of the product; pre-treating the surface of the first arm 10 and the second arm 20, cutting off protruding parts, filling structural gaps, cleaning and drying, can make the coating more closely combined with the surface of the first arm 10 and the second arm 20, and the product is more solid; the first hydraulic drive rod 30 is extended and retracted to drive the first arm 10 and the second arm 20 to rotate relative to each other; the second hydraulic drive rod 40 is extended and retracted to drive the output end connected to the second arm 20 to rotate relative to the second arm 20, so that the user can operate the robot arm conveniently and carry out underwater dredging work. The isocyanate and the resin are heated to the reaction temperature, generally 60-71°C, respectively, and the two are mixed and sprayed on the surface of the first arm 10 and the surface of the second arm 20. The isocyanate and the resin react on the surface of the first arm 10 and the surface of the second arm 20 to form a coating, which can quickly achieve lamination work with high production efficiency.

[0058] Embodiment 4

[0059] Reference Figure 1 and Figure 5 , a production method of a dredging robot arm, comprising:

[0060] Step S401, pre-treating the surface of the first arm 10 and the surface of the second arm 20, cutting off protruding parts, filling structural gaps, cleaning and drying;

[0061] Step S4021, heating the isocyanate and the resin to 60-71° C. respectively;

[0062] Step S4022, using a high-pressure mixing device to mix the isocyanate and the resin in a ratio of 1:1, and spraying the mixture onto the surface of the first arm 10 and the surface of the second arm 20 in an atomized manner;

[0063] Step S403, check the coating thickness, when the coating thickness is less than 2 mm, repeat steps S4021 and S4022;

[0064] Step S404, connecting the end of the first arm 10 to the middle of the second arm 20 via a rotating shaft;

[0065] Step S405, providing a first hydraulic driving rod 30, connecting a first end of the first hydraulic driving rod 30 to the middle of the first machine arm 10, and connecting a second end of the first hydraulic driving rod 30 to a first end of the second machine arm 20;

[0066] Step S406 , providing a second hydraulic drive rod 40 , connecting the first end of the second hydraulic drive rod 40 to the first end of the second arm 20 , and connecting the second end of the second hydraulic drive rod 40 to the first end of the first connecting rod 50 in the middle of the second arm 20 .

[0067] Through the arrangement of the above structure, the coating is applied on the surface of the first arm 10 and the surface of the second arm 20 to form a coating, which can protect the first arm 10 and the second arm 20, achieve the effect of anti-corrosion and anti-friction, and at the same time improve the toughness and strength of the first arm 10 and the second arm 20, and improve the service life of the product; after spraying the coating, checking the coating thickness can ensure the product yield and improve the service life of the first arm 10 and the second arm 20. The first hydraulic drive rod 30 is telescopic to drive the first arm 10 and the second arm 20 to rotate relative to each other; the second hydraulic drive rod 40 is telescopic to drive the output end connected to the second arm 20 to rotate relative to the second arm 20, which is convenient for users to control the mechanical arm and conveniently perform underwater dredging. The isocyanate and the resin are heated to the reaction temperature, generally 60-71°C, respectively, and the two are mixed and sprayed on the surface of the first arm 10 and the second arm 20. The isocyanate and the resin react on the surface of the first arm 10 and the second arm 20 to form a coating, which can quickly achieve the laminating work with high production efficiency.

[0068] Embodiment 5

[0069] Reference Figure 1 and Figure 6 , a production method of a dredging robot arm, comprising:

[0070] Step S501, pre-treating the surface of the first arm 10 and the surface of the second arm 20, cutting off protruding parts, filling structural gaps, cleaning and drying;

[0071] Step S502, using a surface treatment liquid to treat the surface of the first arm 10 and the surface of the second arm 20;

[0072] Step S5031, heating the isocyanate and the resin to 60-71° C. respectively;

[0073] Step S5032, using a high-pressure mixing device to mix the isocyanate and the resin in a ratio of 1:1, and spraying the mixture onto the surface of the first arm 10 and the surface of the second arm 20 in an atomized manner;

[0074] Step S504, check the coating thickness, when the coating thickness is less than 2 mm, repeat steps S5031 and S5032;

[0075] Step S505, connecting the end of the first arm 10 to the middle of the second arm 20 via a rotating shaft;

[0076] Step S506, providing a first hydraulic driving rod 30, connecting a first end of the first hydraulic driving rod 30 to the middle of the first machine arm 10, and connecting a second end of the first hydraulic driving rod 30 to a first end of the second machine arm 20;

[0077] Step S507 , providing a second hydraulic drive rod 40 , connecting the first end of the second hydraulic drive rod 40 to the first end of the second arm 20 , and connecting the second end of the second hydraulic drive rod 40 to the first end of the first connecting rod 50 in the middle of the second arm 20 .

[0078] Through the arrangement of the above structure, the coating is applied on the surface of the first arm 10 and the surface of the second arm 20 to form a coating, which can protect the first arm 10 and the second arm 20, achieve the effect of anti-corrosion and anti-friction, and at the same time improve the toughness and strength of the first arm 10 and the second arm 20, and improve the service life of the product; and before applying the coating, the surface of the first arm 10 and the second arm 20 can be treated with a surface treatment liquid to make the coating more tightly connected to the surface of the first arm 10 and the second arm 20. After spraying the coating, checking the coating thickness can ensure the product yield and improve the service life of the first arm 10 and the second arm 20. The first hydraulic drive rod 30 is telescopic to drive the first arm 10 and the second arm 20 to rotate relative to each other; the second hydraulic drive rod 40 is telescopic to drive the output end connected to the second arm 20 to rotate relative to the second arm 20, which is convenient for users to control the mechanical arm and conveniently perform underwater dredging work. The isocyanate and the resin are heated to the reaction temperature, generally 60-71°C, respectively, and the two are mixed and sprayed on the surface of the first arm 10 and the surface of the second arm 20. The isocyanate and the resin react on the surface of the first arm 10 and the surface of the second arm 20 to form a coating, which can quickly achieve lamination work with high production efficiency.

[0079] As described above, one or more implementation methods are provided in combination with specific contents, and the specific implementation of the present invention is not limited to these descriptions. Any similarity or similarity with the method, structure, etc. of the present invention, or any technical deduction or replacement based on the concept of the present invention, shall be regarded as the protection scope of the present invention.

Claims

1. A method for producing a dredging robot arm, characterized in that: include: Providing a first machine arm (10) and a second machine arm (20), and applying a coating on the surface of the first machine arm (10) and the surface of the second machine arm (20); Connecting the end of the first arm (10) to the middle of the second arm (20) via a rotating shaft; Providing a first hydraulic drive rod (30), connecting a first end of the first hydraulic drive rod (30) to the middle of the first machine arm (10), and connecting a second end of the first hydraulic drive rod (30) to the first end of the second machine arm (20); A second hydraulic drive rod (40) is provided, a first end of the second hydraulic drive rod (40) is connected to a first end of the second machine arm (20), and a second end of the second hydraulic drive rod (40) is connected to a first end of a first connecting rod (50) in the middle of the second machine arm (20).

2. The method for producing a dredging robot arm according to claim 1, characterized in that: The coating is a polyurethane wear-resistant and anti-corrosion coating.

3. The method for producing a dredging robot arm according to claim 1, characterized in that: The thickness of the coating is 2mm-3mm.

4. The method for producing a dredging robot arm according to claim 1, characterized in that: The step of coating the surface of the first arm (10) and the surface of the second arm (20) comprises: heating the isocyanate and the resin to 60-71° C. respectively; using a high-pressure mixing device to mix the isocyanate and the resin in a ratio of 1:1, and spraying them onto the surface of the first arm (10) and the surface of the second arm (20).

5. The method for producing a dredging robot arm according to claim 4, characterized in that: The equipment hydraulic pressure of the high-pressure mixing equipment is 3.8-17.2MPa.

6. The method for producing a dredging robot arm according to claim 1, characterized in that: Before the step of coating the surface of the first arm (10) and the surface of the second arm (20), the method further includes pre-treating the surface of the first arm (10) and the surface of the second arm (20), cutting off protruding parts, filling structural gaps, cleaning and drying.

7. The method for producing a dredging robot arm according to claim 1, characterized in that: After the step of coating the first arm (10) and the second arm (20), the method further includes checking the coating thickness. When the coating thickness is less than 2 mm, the step of coating the first arm (10) and the second arm (20) is repeated.

8. The method for producing a dredging robot arm according to claim 6, characterized in that: After the step of pretreating the surface of the first arm (10) and the surface of the second arm (20), and before the step of coating the surface of the first arm (10) and the surface of the second arm (20), the method further includes: treating the surface of the first arm (10) and the surface of the second arm (20) using a surface treatment liquid.

9. The method for producing a dredging robot arm according to claim 1, characterized in that: A second connecting rod (60) is provided, the second end of the first connecting rod (50) is connected to the middle of the second machine arm (20), and the first end of the second connecting rod (60) is connected to the first end of the first connecting rod (50) and / or the second end of the second hydraulic drive rod (40).

10. The method for producing a dredging robot arm according to claim 1, characterized in that: in, The surfaces of the first machine arm (10) and the second machine arm (20) are both provided with reinforcing ribs (12), the reinforcing ribs (12) are arranged obliquely, and two adjacent reinforcing ribs (12) are sequentially connected end to end.