Method for building CO2 sealed storage layer by utilizing temperature to control coal conversion
Through water vapor temperature regulation, the coal seam is subjected to in-situ pyrolysis to form a high porosity reservoir. Combined with CO2 geological storage, the problems of in-situ pyrolysis and CO2 storage in the existing technology are solved, and efficient and stable CO2 can be achieved Seal effect.
Patent Information
- Application Number
- CN202411343752.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-25
- Publication Date
- 2024-11-08
AI Technical Summary
The existing coal in-situ pyrolysis and CO2 storage technology are difficult to take into account at the same time, which can easily lead to uncontrollable goaf and surface subsidence, affecting the efficiency and stability of CO2 storage.
The coal seam is subjected to in-situ pyrolysis by water vapor temperature regulation to form a high porosity reservoir. The reservoir is used to adsorb CO2, combined with the CO2 geological sealing method, the degree of pyrolysis and pore structure of the coal seam are controlled to ensure the effective sealing of CO2 .
It realizes efficient CO2 storage, avoids goaf and surface subsidence, improves the permeability and CO2 adsorption capacity of coal seams, and reduces storage pressure and energy consumption.
Smart Images

Figure CN118911659A_ABST
Abstract
Description
Technical Field
[0001] The invention provides a method for constructing a CO2 sealing storage layer by controlling coal conversion through temperature, belonging to the technical field of coal development. Background Art
[0002] Storing CO2 in unmineable coal seams is the main method and hot research direction for CO2 geological storage. The low permeability of coal makes it difficult to inject CO2 into coal seams, which becomes a technical difficulty in storing CO2 in coal seams. Coal is an organic rock that can be pyrolyzed or oxidized at high temperatures to produce combustible gases and form porous rocks. Underground coal gasification is a method of using coal oxidation reactions to convert solid coal into combustible gases and achieve fluidized mining. However, since the scope of underground coal oxidation (combustion) is difficult to control, it will form goafs (combustion channels) with uncontrollable shapes, cause surface subsidence, and then cause groundwater to invade the combustion zone, making it difficult for the reaction to continue.
[0003] The patent "A method for integrating in-situ pyrolysis of oil-rich coal and geological storage of CO2" (patent application number: 202110943836.5) utilizes the pyrolysis characteristics of oil-rich coal to convert coal into oil and gas resources, and uses its residual carbon to store CO2. High-temperature pyrolysis of coal is the main method for producing coke. The above patent (patent application number: 202110943836.5) only proposes in principle to produce oil and gas through pyrolysis and to use pyrolysis residual carbon to store CO2, ignoring the control effect of temperature on coal pyrolysis. It is very easy to produce similar disadvantages as underground coal gasification, such as uncontrollable goafs and surface subsidence, and ultimately CO2 storage cannot be achieved. Therefore, in-situ pyrolysis of coal and CO2 storage cannot be taken into account at the same time. Pyrolysis of solid coal fluidized mining will lead to excessive pyrolysis of residual carbon, reduce its adsorption of CO2, and thus affect the storage capacity. Even after excessive pyrolysis, goafs will be formed, destroying the storage space. The patent "A method for in-situ coal sorting and mining based on pyrolysis" (CN113803048A) also has the above-mentioned shortcomings.
[0004] Therefore, in view of the bottlenecks and challenges of the current domestic CO2 geological storage technology based on in-situ coal pyrolysis, it is urgent to propose an effective technology for coal seam modification to form a coal reservoir space with high porosity, high stability, and almost negligible or stable formation deformation, so as to achieve large-scale CO2 geological storage. Summary of the invention
[0005] In view of the problems existing in the above-mentioned prior art, the present invention provides a method for constructing a CO2 storage layer by controlling coal conversion by temperature, which combines water vapor temperature control, coal in-situ pyrolysis and CO2 geological storage methods. The key point of this method is to select a suitable water vapor temperature, use the heat carried by water vapor to pyrolyze the coal in-situ, pyrolyze a certain amount of volatile matter in the coal and collect it to form a reservoir with the required porosity, and then stop pyrolysis. Inject CO2 into the high-porosity and high-permeability coal seam formed after pyrolysis to carry out CO2 geological storage.
[0006] In order to solve the above technical problems, the technical solution adopted by the present invention is: a method for constructing a CO2 storage layer by controlling coal conversion by temperature, comprising the following steps: Step 1: Take samples from the target coal seam and measure its physical and chemical parameters; Step 2: construct two or more directional wells in parallel in the target coal seam and perform heat insulation treatment on the wellbore, wherein the directional well used for injecting heat source is the heat injection well, and the directional well used for collecting volatile products is the production well; Step 3: Using a known method, the coal body between the coal seam sections of the directional well is fractured to increase permeability and construct a gas seepage channel; Step 4: inject a constant temperature heat source into the coal seam through a heat injection well to heat the coal seam to pyrolysis, and the gas products produced by pyrolysis are discharged from the production well under the drive of the injected gas flow; Step 5: Calculate the new porosity of the coal seam based on the amount of pyrolysis products to prevent over-pyrolysis of the coal body, and then readjust the temperature of the heat source based on the porosity of the coal seam after pyrolysis to controllably pyrolyze the coal body to form a reservoir with the required porosity; Step 6: Exchange the heat injection well and the production well, and repeat steps 4 and 5 to make the pores formed by coal pyrolysis between the heat injection well and the production well more uniform; Step 7: After obtaining the reservoir with the required porosity through pyrolysis, high-pressure CO2 is injected into the production well and injection well. CO2 enters the well and adsorbs on the pyrolyzed coal body. After the adsorption is saturated, the injection is stopped, the heat injection well and production well are closed, and the geological storage of CO2 is completed.
[0007] The physical and chemical parameters of the target coal seam measured in step one are used to determine the heat source temperature required for initial pyrolysis of the coal seam.
[0008] The heat source is water vapor.
[0009] In step five, the heat injection well is used as a constant temperature heat source, and a numerical calculation method is used to simulate the temperature field in the coal seam. The newly added porosity of the coal body is determined based on the corresponding relationship between temperature and pyrolysis. When the porosity reaches the design value, the heat injection well and the production well are replaced, and water vapor at the same temperature is injected to fully pyrolyze the coal, eventually forming a reservoir with the required porosity as a CO2 storage layer.
[0010] During the coal pyrolysis process, the water vapor temperature is regulated by the calculated new porosity, and a heating method from low to high is adopted. The pyrolysis degree of the coal and the amount of newly added porosity are controlled by controlling the temperature of the injected water vapor, so that the reservoir after pyrolysis has sufficient stability.
[0011] The porosity increment is calculated based on the amount of pyrolysis products, and the time of pyrolysis termination is determined. The calculation formula of the porosity increment is as follows: ; in Δn is the porosity increment, m g is the mass of pyrolysis products, m c is the mass of coal in the pyrolysis zone.
[0012] The collected pyrolysis products are used as fuel to heat water vapor.
[0013] In step 2, the well arrangement method and number are determined according to the area and thickness of the target coal seam, wherein the well arrangement method includes two methods: vertical parallel arrangement of directional wells and horizontal parallel arrangement of directional wells.
[0014] The beneficial effects of the present invention compared with the prior art are as follows: (1) By controlling the temperature of the coal, the coal is pyrolyzed moderately to avoid high-temperature pyrolysis that turns the coal into coke, thereby reducing the coal seam's ability to adsorb CO2; (2) By controlling the temperature of the coal body, the coal body is pyrolyzed moderately to avoid uncontrolled pyrolysis to form goaf areas, causing the overlying rock strata to collapse and destroy the stratum structure; (3) Increased coal porosity, thereby increasing coal permeability, making it easier to inject CO2 into coal seams; (4) Taking advantage of the strong adsorption of CO2 by coal, the reservoir after pyrolysis has a developed pore structure and its storage capacity is greater than that of the original coal reservoir; (5) Compared with sandstone reservoirs, when the CO2 storage capacity is the same, the CO2 stored in the pyrolysis reservoir has a lower storage pressure and lower energy consumption in the storage process because CO2 exists in the reservoir in an adsorbed and free state. (6) The oil and gas produced by pyrolysis are oil-based fuels and chemical raw materials; (7) This method is applicable to coal reservoirs of different coal ranks. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] The present invention will be further described below in conjunction with the accompanying drawings: Figure 1 is a flow chart of the method of the present invention; Figure 2It is a structural schematic diagram of vertically parallel arrangement of directional wells; Figure 3 It is a structural schematic diagram of directional wells arranged horizontally and in parallel; Figure 4 The figure is a curve diagram of the porosity and permeability of bituminous coal as a function of temperature, which is determined by experiments in the present invention. DETAILED DESCRIPTION
[0016] like Figure 1-4 As shown, the present invention provides a method for constructing a CO2 sealing storage layer by controlling coal conversion by temperature, wherein the coal seam is fractured and permeated by a known method to form a seepage channel for high-temperature steam; water vapor of a certain temperature is injected to perform in-situ pyrolysis on the coal seam, and a developed pore structure is formed after the pyrolysis of the coal; based on the output of pyrolysis products, the number of newly added pores in the coal seam is calculated, the appropriate water vapor temperature is adjusted, and the coal is pyrolyzed in a controlled manner to form a reservoir with the required porosity.
[0017] The method of the present invention is divided into three stages: water vapor temperature control, in-situ coal pyrolysis and CO2 geological storage. First, injection wells and production wells are constructed in the coal seam respectively, and the well layout and number are determined according to the area of the coal seam and the thickness of the coal seam, wherein the well layout includes vertical parallel arrangement of directional wells and horizontal parallel arrangement of directional wells. The coal body between the coal seam sections of the directional well is fractured to increase permeability, and a gas seepage channel is constructed, and then this channel is used as a storage place for CO2. By regulating the water vapor temperature, the coal is in-situ pyrolyzed using constant temperature water vapor to extract a certain amount of volatile substances and form a reservoir with the required porosity. In addition, the extracted volatile products can be used as fuel for heating water vapor. In-situ pyrolysis is carried out using constant temperature water vapor, and the injection well is used as a constant temperature heat source. A numerical calculation method is used to simulate the temperature field in the coal seam. According to the corresponding relationship between temperature and pyrolysis ( Figure 4 ), determine the newly added porosity of the coal body, and when the porosity reaches the design value, it is considered that the in-situ pyrolysis of the coal is completed. At this point, the CO2 storage stage begins. In the CO2 storage stage, a high-pressure pump is used to simultaneously inject high-pressure CO2 into the production well and the heat injection well to complete the geological storage of CO2. On the one hand, after pyrolysis of coal, a developed pore structure is formed, which improves the permeability of coal and makes it easier to inject CO2 into the coal seam; on the other hand, coal has a strong adsorption effect on CO2; therefore, CO2 in the reservoir can quickly achieve adsorption saturation, and eventually CO2 exists in the reservoir in an adsorbed state and a free state. Compared with sandstone reservoirs, due to the adsorption of CO2 by coal, when the CO2 storage amount is the same, the CO2 stored in the reservoir after pyrolysis has a lower storage pressure and lower energy consumption in the storage process.
[0018] The specific implementation steps of this method are as follows: Step 1: Take samples from the target coal seam and measure its physical and chemical parameters such as porosity, permeability, and volatile content; Step 2: construct two or more directional wells in parallel in the target coal seam, and perform heat insulation treatment on the wellbore. The well used for injecting constant temperature water vapor is the heat injection well, and the well used for collecting volatile products is the production well; Step 3: Fracturing and permeability enhancement of the coal bodies between the coal seam sections of the directional well to construct gas seepage channels; Step 4: Inject constant temperature steam into the coal seam through the heat injection well to heat the coal seam to pyrolysis, and the gas products produced by pyrolysis are discharged from the production well under the drive of the injected gas flow; Step 5: Calculate the newly added porosity of the coal seam based on the output of pyrolysis products to prevent excessive pyrolysis of the coal body; then readjust the temperature of the water vapor based on the newly added porosity, pyrolyze the coal body in a controlled manner, and form a reservoir with the required porosity; Step 6: Exchange the heat injection well and the production well. Exchange the heat injection well and the production well in steps 3 and 4 to make the pores formed by pyrolysis between them more uniform; inject constant temperature steam again in the manner described in steps 4 and 5; Step 7: After pyrolysis is completed, high-pressure CO2 is injected into the production well and the injection well at the same time. CO2 enters the well and adsorbs on the pyrolyzed coal body. After adsorption saturation, injection is stopped. The heat injection well and production well are closed to complete the geological storage of CO2.
[0019] The coal seam is heated to pyrolysis by injecting constant temperature steam into the coal seam through the hot injection well. The hot injection well is used as a constant temperature heat source, and the temperature field in the coal seam is simulated by a numerical calculation method. According to the corresponding relationship between temperature and pyrolysis ( Figure 4 ), determine the newly added porosity of the coal body. When the porosity reaches the design value, replace the heat injection well and the production well, inject water vapor at the same temperature, and fully pyrolyze the coal. Finally, a reservoir with the required porosity is formed as a CO2 sealing storage layer. In this process, the water vapor temperature can be adjusted according to the new porosity during the pyrolysis process, so that the reservoir after pyrolysis has sufficient stability, which can effectively prevent the roof from sinking seriously, deforming and rupturing due to excessive pyrolysis, and prevent CO2 leakage.
[0020] When pyrolyzing a coal seam, the pyrolysis degree of the coal and the amount of newly added porosity are controlled by controlling the temperature of the injected water vapor. The porosity increment is calculated based on the amount of pyrolysis products to determine the time when pyrolysis is terminated.
[0021] When pyrolyzing coal seams, the nonlinear relationship between the amount of pyrolysis products of different types of coal and temperature obtained from scientific experiments is as follows: Figure 4 The figure shows the curve of the measured porosity and permeability of bituminous coal as a function of temperature. By heating from low to high, the temperature of the injected water vapor is controlled to control the degree of pyrolysis of the coal and the amount of newly added porosity. The newly added porosity is calculated based on the amount of pyrolysis products (Formula 1), and the time when pyrolysis ends is determined.
[0022] (1); in Δn is the porosity increment, m g is the mass of pyrolysis products, m c is the mass of coal in the pyrolysis zone.
[0023] The heat injection well and the production well are connected through the gas seepage channel after coal pyrolysis. At the same time, high-pressure CO2 is injected into the production well and the heat injection well to fully utilize the CO2 storage space.
[0024] The heat carrier used in the present invention is water vapor (300℃-800℃). This type of high-temperature medium is relatively easy to obtain, and has good heat transfer performance, high heat carrying efficiency, and strong diffusion capacity. It helps to heat the coal seam evenly and increase the heating surface of the coal seam. The high-temperature medium after pyrolysis is easy to recover and recycle, further reducing the project cost.
[0025] The collected pyrolysis products can be used as fuel to heat water vapor, and the heat injection well and the production well are connected through a gas seepage channel.
[0026] The reservoir required for porosity formed after pyrolysis has the following characteristics: the reservoir has sufficient stability to effectively prevent CO2 leakage caused by severe roof subsidence, deformation and rupture due to excessive pyrolysis, and achieve protection of the reservoir.
[0027] The present invention will be further described below with reference to the embodiments.
[0028] Example 1 like Figure 2 As shown, the method of the present invention is used to store CO2 in a nearly horizontal single medium and thick coal seam 1 with a thickness of more than 10m and a burial depth of more than 100m. Figure 2 The well arrangement shown in the figure is a vertical parallel arrangement. Figure 2 In (a), 1-2 are heat injection wells, and 1-3 are production wells. Figure 2 In (b), 2-2 is a heat injection well and 2-3 is a production well. The difference between the two is Figure 2 (a) The horizontal section of the middle heat injection well is close to the roof of coal seam 1. Figure 2 (b) The horizontal section of the middle heat injection well is close to the bottom plate of the coal seam 1; the method of the present invention is used to Figure 1 The steps for storing CO2 in coal seam 1 are as follows: 1) Directional wells for heat injection and volatile product recovery are constructed to coal seam 1, one directional well is located in the upper part of the coal seam, close to the coal seam roof, and the other directional well is located in the lower part of the coal seam, close to the coal seam floor, and the wellbores of the two positioning wells are insulated.
[0029] 2) Use directional perforating to implement coal seam hydraulic fracturing, inject proppant into the cracks in the coal layer to be mined through the injection well, and wash the well and drain the water to achieve permeability enhancement of the coal body between adjacent directional wells.
[0030] 3) Regulate the water vapor temperature and inject constant temperature water vapor through the heat injection well to heat the coal seam to pyrolysis. The gas products produced by pyrolysis are discharged from the production well under the drive of the injected air flow.
[0031] 4) Exchange the heat injection well and the production well, use the heat injection well in step 3) as a new production well for volatile product recovery, and use the production well in step 3) as a new heat injection well. Inject water vapor at the same temperature again in the manner described in step 3) to fully pyrolyze the coal seam.
[0032] 5) Calculate the increase in porosity based on the amount of pyrolysis products, and stop pyrolysis when the required porosity is reached.
[0033] 6) Inject high-pressure CO2 into the production well and injection well at the same time. CO2 is adsorbed on the pyrolyzed coal body. Stop injection after adsorption is saturated. Close the heat injection well and production well to complete the geological storage of CO2.
[0034] Example 2 like Figure 3 As shown, in a nearly horizontal single thin coal seam 1 with a thickness of less than 10 m and a burial depth of more than 100 m, the method of the present invention is used to carry out in-situ heating of the coal seam. Figure 3 The well arrangement shown in the figure is a horizontal parallel arrangement. Figure 3 In (a), 1-2 is a heat injection well, 1-3 and 1-4 are production wells. Figure 3 In (b), 2-2 is a production well, 2-3 and 2-4 are heat injection wells. The difference between this example and Example 1 is that the well arrangement method in step 1) is different according to the different characteristics of the coal seam. The coal seam in Example 1 is a single medium and thick coal seam, and the coal seam in Example 2 is a single thin coal seam. Figure 3 (a) The hot injection well is located between two production wells. Figure 3 In (b), the production well is located between two heat injection wells.
[0035] The present invention utilizes the temperature-sensitive property of volatiles in coal and utilizes different temperatures to pyrolyze volatiles of different chemical components in the coal body, thereby controllably pyrolyzing the volatiles in the coal body, increasing the porosity of the coal body, increasing the specific surface area of the coal body for adsorbing CO2, increasing the permeability of the coal body, and minimizing the strength of the coal body, thereby constructing a structurally stable CO2 storage space in the coal seam. In addition, water vapor can be recycled, and the pyrolyzed volatile matter can be used as fuel for heating water vapor.
[0036] According to the coal rank of the coal reservoir, the present invention selects a suitable water vapor temperature to pyrolyze a certain amount of coal to form the required porosity. It can not only realize the construction of a coal reservoir with the required porosity according to the design, but also effectively prevent CO2 leakage caused by severe roof subsidence, deformation and cracking due to excessive pyrolysis, thereby protecting the cap layer (the dense rock layer overlying the reservoir) and providing a safe and reliable storage place for CO2 geological storage. The method uses water vapor to perform in-situ pyrolysis on the coal seam, and stops pyrolysis after forming a reservoir with the required porosity. The storage amount of CO2 can be determined based on the measured porosity of the reservoir. The degree of coal pyrolysis is controlled by regulating the water vapor temperature, and then the deformation and subsidence of the roof are indirectly controlled, thereby ensuring the sealing of the reservoir cap layer.
[0037] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. A method for constructing a CO2 storage layer by temperature-controlled coal conversion, characterized in that: The following steps are involved: Step 1: Take samples from the target coal seam and measure its physical and chemical parameters; Step 2: construct two or more directional wells in parallel in the target coal seam and perform heat insulation treatment on the wellbore, wherein the directional well used for injecting heat source is the heat injection well, and the directional well used for collecting volatile products is the production well; Step 3: Using a known method, the coal body between the coal seam sections of the directional well is fractured to increase permeability and construct a gas seepage channel; Step 4: inject a constant temperature heat source into the coal seam through a heat injection well to heat the coal seam to pyrolysis, and the gas products produced by pyrolysis are discharged from the production well under the drive of the injected gas flow; Step 5: Calculate the new porosity of the coal seam based on the amount of pyrolysis products to prevent over-pyrolysis of the coal body, and then readjust the temperature of the heat source based on the porosity of the coal seam after pyrolysis to controllably pyrolyze the coal body to form a reservoir with the required porosity; Step 6: Exchange the heat injection well and the production well, and repeat steps 4 and 5 to make the pores formed by coal pyrolysis between the heat injection well and the production well more uniform; Step 7: After obtaining the reservoir with the required porosity through pyrolysis, high-pressure CO2 is injected into the production well and injection well. CO2 enters the well and adsorbs on the pyrolyzed coal body. After the adsorption is saturated, the injection is stopped, the heat injection well and production well are closed, and the geological storage of CO2 is completed.
2. A method for constructing a CO2 storage layer by temperature-controlled coal conversion according to claim 1, characterized in that: The physical and chemical parameters of the target coal seam measured in step one are used to determine the heat source temperature required for initial pyrolysis of the coal seam.
3. The method for constructing a CO2 storage layer by temperature-controlled coal conversion according to claim 1, characterized in that: The heat source is water vapor.
4. The method of constructing a CO2 storage layer by temperature-controlled coal conversion according to claim 3, characterized in that: In step five, the heat injection well is used as a constant temperature heat source, and a numerical calculation method is used to simulate the temperature field in the coal seam. The newly added porosity of the coal body is determined based on the corresponding relationship between temperature and pyrolysis. When the porosity reaches the design value, the heat injection well and the production well are replaced, and water vapor at the same temperature is injected to fully pyrolyze the coal, eventually forming a reservoir with the required porosity as a CO2 storage layer.
5. A method for constructing a CO2 storage layer by temperature-controlled coal conversion according to claim 4, characterized in that: During the coal pyrolysis process, the water vapor temperature is regulated by the calculated new porosity, and a heating method from low to high is adopted. The pyrolysis degree of the coal and the amount of newly added porosity are controlled by controlling the temperature of the injected water vapor, so that the reservoir after pyrolysis has sufficient stability.
6. The method of constructing a CO2 storage layer by temperature-controlled coal conversion according to claim 5, characterized in that: The porosity increment is calculated based on the amount of pyrolysis products, and the time of pyrolysis termination is determined. The calculation formula of the porosity increment is as follows: ; in Δn is the porosity increment, m g is the mass of pyrolysis products, m c is the mass of coal in the pyrolysis zone.
7. The method of constructing a CO2 storage layer by temperature-controlled coal conversion according to claim 3, characterized in that: The collected pyrolysis products are used as fuel to heat water vapor.
8. The method of constructing a CO2 storage layer by temperature-controlled coal conversion according to claim 1, characterized in that: In step 2, the well arrangement method and number are determined according to the area and thickness of the target coal seam, wherein the well arrangement method includes two methods: vertical parallel arrangement of directional wells and horizontal parallel arrangement of directional wells.