Plane shadowless light source and light guide plate

By using foam to isolate the increase lens and light guide plate in a flat shadowless light source, and improving the structure of the scattering dots into round holes, the problems of water ripple and light guide plate are solved, the imaging quality and thermal conductivity are improved, and more efficient is achieved light conversion rate.

CN118912420APending Publication Date: 2024-11-08东莞康视达自动化科技有限公司 +1
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202410949700.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2024-04-11
Filing Date
2024-07-15
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The existing flat shadowless light source is caused by direct contact between the lens and the light guide plate, which is susceptible to damage and contamination, and the materials and processes of the thermal pads have problems such as insufficient resilience and precipitation of silicone oil, which affects the imaging quality.

Method used

In the flat shadowless light source, foam isolation lens and light guide plate are used, silicon-free thermal gaskets are used, and the scattering dot structure is improved to form a circular hole to improve the light conversion rate.

Benefits of technology

The water ripple phenomenon and moiré phenomenon are eliminated, the imaging clarity of the light source and the light conversion rate of the light guide plate are improved, and silicone oil precipitation and thermal conductivity are improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118912420A_ABST
    Figure CN118912420A_ABST
Patent Text Reader

Abstract

The present invention provides a planar shadowless light source, comprising: a housing having a mounting space inside, a first opening at the bottom, and a third opening at the top; the PCBA board, the LED lamp beads, the light guide board, the first lens increasing lens and the second lens increasing lens are installed in the installation space, the first lens increasing lens, the light guide board and the second lens increasing lens are sequentially arranged from bottom to top, the PCBA board is arranged on the side face of the light guide board, the LED lamp beads are evenly arranged on the side, facing the light guide board, of the PCBA board, and the LED lamp beads irradiate towards the light guide board; in the vertical direction, a circle of foam is arranged between the lower surface of the first lens increasing lens and the shell, between the lower surface of the light guide plate and the upper surface of the first lens increasing lens, between the upper surface of the light guide plate and the lower surface of the second lens increasing lens and between the upper surface of the second lens increasing lens and the shell respectively.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of light sources, and in particular to a planar shadowless light source and a light guide plate. Background Art

[0002] Currently, the flat shadowless light sources on the market are assembled by stacking cover plate + lens enhancement + light guide plate + bottom shell. In this assembly process, the bottom of the lens enhancement is directly attached to the top of the light guide plate. Due to the difference in surface flatness, water ripples appear on the contact surface, which reduces the clarity of the final image of the light source and causes ghosting. At the same time, one side of the light guide plate is in direct contact with the air. When the light source is actually used, the surface of the light guide plate is easily damaged and contaminated by sharp objects, chemical gases, daily illegal maintenance, etc., further causing a decline in the quality of the image.

[0003] The illuminant of the flat shadowless light source generally adopts chip LED, which is welded on the PCBA through the SMT process. The PCBA is then assembled on the shell through thermal double-sided adhesive or thermal silicone pad. The heat generated by the LED is conducted to the thermal pad through the PCBA, and then to the bottom shell. If the thermal double-sided adhesive is used, because the thickness is between 0.1-0.25mm, the material does not have resilience, there will be a situation where the manufacturing tolerance requirements of the relevant materials are high, and the material processing cost will also increase relatively. In addition, the adhesive uses oily acrylic ester, and the oily substance will evaporate at high temperature, and then be adsorbed to the surface of the light guide plate or the lens through the gap of the contact surface, forming a frosted effect, which affects the quality of the light source. At the same time, the double-sided adhesive makes it more difficult to repair and disassemble the light source, and the thermal conductivity is also low, with a value below 1.0W / m·K, and the light source power cannot be increased. If it is replaced with a thermal silicone pad, because the thermal silicone pad has good resilience and surface wettability, it can solve the problems of excessive processing precision and high maintenance difficulty, and the thermal conductivity can also be above 2W / m·K. However, the manufacturing process of the thermal conductive silicone pad contains organic silicone oil, and the finished product contains silicone oil. After a long time, the silicone oil will precipitate or the siloxane will volatilize, and then be adsorbed to the surface of the light guide plate or the lens along the gap of the contact surface, forming a frosted and foggy effect, thereby rendering the light source function ineffective.

[0004] The manufacturing process of the light guide plate of the flat shadowless light source can be roughly divided into the following three categories:

[0005] Screen printing: The screen printing equipment is used to print dots with certain shapes and regular arrangements on the surface of the light guide plate using inks prepared in a certain proportion and dot distribution rules. The light guide plate substrate is made of PMMA, and two layers of ink are printed on the surface of one side of the substrate. The inner layer is white reflective ink, and the outer layer is black light-absorbing ink (such as Figure 1 , Figure 2 The optical principle is that when light hits the diffusion point, the reflected light will diffuse to all angles, thus destroying the total reflection condition (such as Figure 3). In actual production, if the ink is not mixed properly, the light guide plate will turn yellow after printing, and some dots will be darker and the dots will stick together. When used for flat shadowless light sources, the more fatal problem is that the viscosity of the ink is difficult to control, and the repeated printing alignment accuracy is not high, resulting in eccentricity of the white reflective dots. In addition, because it is a 2D plane graphic, there must be a production limit for the dot size. The current limit is 0.18mm for white dots and 0.32mm for black dots, which reduces the clarity of the image.

[0006] Hot Press Forming: The processing of dots is completed by using the physical principle of plastic deformation of the light guide plate (LGP) substrate when heated (see Figure 4 ). Specifically, during product processing, two rollers rotating in opposite directions are pre-heated and the gap is adjusted (pressurized). The rollers are wrapped with a stainless steel template with a processed microstructure (PATTERN). The LGP is sent between the two rollers by a conveyor. The temperature of the two rollers and the template is transmitted to the contact surface with the LGP (theoretically, it is a line contact). At this time, the LGP undergoes surface plastic deformation due to heat and pressure, and the microstructure (PATTERN) on the template is completely transferred to the LGP surface, completing the processing of the LGP microstructure (PATTERN dots). However, it is difficult to overcome that if the processing is not carried out in a vacuum environment, tiny bubbles will be generated in the light guide plate. The bubble size is between 5μm and 65μm. The bubbles will scatter the reflected light of the imaging object, and the background of the imaging picture will be white, resulting in a very blurred visual experience and a significant decrease in the contrast of the picture. In addition, due to the large temperature change during the cooling process of the LGP, thermal residual stress will be generated, and the heat dissipation points will easily deform, forming a crater phenomenon (see Figure 5 ), affecting the function of the light source.

[0007] Photolithography: Through the action of energy beam, the graphic structure on the design data is transferred to the photoresist on the surface of the light guide plate substrate (LGP), and then the scattering dots are processed through etching (see Figure 6). Specifically: 1. Surface preparation, clean and dry the LGP surface; 2. Glue coating, apply a thin layer of photoresist on the LGP surface by spin coating; 3. Soft baking, partially evaporate the photoresist solvent by heating; 4. Alignment and exposure, precise alignment of the mask and LGP, and exposure of the photoresist, the negative photoresist is a polymer; 5. Development, remove the non-polymerized photoresist; 6. Hard baking, continue to evaporate the solvent; 7. Development inspection, check the alignment and defects of the surface; 8. Etching, remove the top layer of LGP through the opening of the photoresist; 9. Remove the photoresist (peeling), remove the photoresist on the LGP; 10. Final inspection, surface inspection for etching irregularities or other problems. At present, the better scattering dots on the market are regularly arranged. When using the light field camera imaging solution, the dots will directly participate in the imaging. This is because the 3D graphic structure of the dots is similar to a semicircle. When the reflected light from the imaging object passes through the dots, it will be first focused to a focal point and then diverged. It will then be refocused after passing through the microlens of the light field camera to participate in the final imaging. Due to the optical path difference, the optical path difference between the reflected light that has not passed through the dots and the reflected light that has passed through the dots is inconsistent, resulting in aberrations, which directly causes this light source to not be used in the light field camera imaging solution. Summary of the invention

[0008] The main purpose of the present invention is to provide a planar shadowless light source and a light guide plate, which can eliminate the water ripple phenomenon of the light source and the moiré phenomenon of the light guide plate.

[0009] In order to achieve the above purpose, the technical solution adopted by the present invention is: a planar shadowless light source, comprising:

[0010] The housing has an installation space inside, a first opening at the bottom, and a third opening at the top;

[0011] A PCBA board, LED lamp beads, a light guide plate, a first amplification lens, and a second amplification lens are installed in the installation space. The first amplification lens, the light guide plate, and the second amplification lens are arranged in sequence from bottom to top. The PCBA board is arranged on the side of the light guide plate. A plurality of LED lamp beads are evenly arranged on one side of the PCBA board facing the light guide plate. The LED lamp beads irradiate toward the light guide plate. It is characterized in that:

[0012] In the up and down directions, a circle of foam is respectively arranged between the lower surface of the first amplifying lens and the outer shell, between the lower surface of the light guide plate and the upper surface of the first amplifying lens, between the upper surface of the light guide plate and the lower surface of the second amplifying lens, and between the upper surface of the second amplifying lens and the outer shell.

[0013] Preferably, a thermal pad is provided on a side of the PCBA board facing away from the light guide plate, and the thermal pad is a silicon-free thermal pad.

[0014] Preferably, the shell includes a bottom shell and a cover plate, the first opening is arranged at the bottom of the bottom shell, and the second opening is arranged at the top, the first opening and the second opening are both square, and the size of the second opening is larger than that of the first opening, the cover plate is detachably arranged at the second opening to block or open the second opening, and the third opening is formed on the cover plate, the third opening is also square, and its size is the same as that of the first opening.

[0015] Preferably, the beam angle θ of the LED lamp bead satisfies the following conditions:

[0016] θ≤2θ i ,

[0017] Among them, θ i is the critical value of the incident angle of the light emitted by the LED lamp bead entering the light guide plate, θ i Satisfies the refraction theorem:

[0018] n i sinθ i =n t sinθ t ,

[0019] n i is the refractive index of air, n t is the refractive index of the light guide plate, θ t is the refraction angle, when θ t When is the critical angle of total reflection,

[0020] θ t =arcsin(1 / n t ).

[0021] Preferably, the light guide plate comprises a body and a plurality of scattering dot structures arranged at the bottom of the body, the scattering dot structures are truncated cone holes, and the diameter of the inner bottom surface of the truncated cone hole is smaller than the diameter of the outer bottom surface.

[0022] Preferably, the diameters of the inner and outer bottom surfaces of the scattering dot structure meet the following requirements: the scattering dot structure is not displayed in the image captured by the camera, and the diameters of the inner and outer bottom surfaces are larger than the minimum size that can be achieved by the etching process.

[0023] Preferably, the distribution of the plurality of scattering point structures on the body meets the following requirements:

[0024] 1) When viewed from above, the distance between the centers of adjacent scattering dot structures is not greater than a first predetermined value and not less than a second predetermined value, and the second predetermined value is less than the first predetermined value;

[0025] 2) A circle with each of the centers as the center and a radius R does not include other scattering point structures, and the value of the radius R is determined based on experience.

[0026] Preferably, the heights of the plurality of frustum holes are randomly arranged within a certain range.

[0027] Preferably, the height of the dot scattering structure satisfies that reflected light irradiating the inner bottom edge of the dot scattering structure and reflected light irradiating the outer bottom edge of the dot scattering structure will not be totally reflected when irradiated onto the light emitting surface of the light guide plate.

[0028] Preferably, the light guide plate is manufactured by the following method, which specifically comprises the following steps:

[0029] Step 1: Surface preparation: clean and dry the surface of the light guide plate substrate, which is optical glass;

[0030] Step 2: Glue coating: coating a layer of negative photoresist on the surface of the light guide plate substrate;

[0031] Step 3: Soft baking: partially evaporate the photoresist solvent by heating;

[0032] Step 4: Alignment and exposure: precisely align the mask with the light guide plate substrate and expose the negative photoresist. After exposure, the negative photoresist produces a polymer that is insoluble in the developer. Holes corresponding to the scattering dot structure are pre-formed on the mask.

[0033] Step 5, development: applying a developer on the upper surface of the photoresist to remove the non-polymerized photoresist and form a hollow structure on the photoresist;

[0034] Step 6: hard baking to continue evaporating the photoresist solvent;

[0035] Step 7. Development inspection: Check the alignment and defects of the surface;

[0036] Step 8, etching: removing the upper surface of the light guide plate substrate through the hollow structure of the photoresist;

[0037] Step 9, removing the photoresist: removing the photoresist on the light guide plate substrate;

[0038] Step 10: Final inspection: perform surface inspection for etching irregularities or other problems.

[0039] Compared with the prior art, the present invention has the following beneficial effects:

[0040] 1) Foam is arranged between the upper and lower sides of the light guide plate of the present invention and the corresponding amplification lenses, so as to avoid direct contact between the amplification lenses and the light guide plate, thereby eliminating the water ripple phenomenon;

[0041] 2) The present invention improves the scattering dot structure of the light guide plate, and adopts a truncated cone form to improve the light conversion efficiency of the light guide plate. BRIEF DESCRIPTION OF THE DRAWINGS

[0042] Figure 1 and Figure 2 It is a scattered dot pattern of screen printing in the prior art;

[0043] Figure 3 It is a schematic diagram of the light transmission in the light guide plate;

[0044] Figure 4 It is a schematic diagram of the hot pressing forming of the light guide plate in the prior art;

[0045] Figure 5 It is a cross-sectional view of the crater phenomenon;

[0046] Figure 6 It is a schematic diagram of the light guide plate produced by photolithography;

[0047] Figure 7 is an exploded view of the planar shadowless light source of the present invention;

[0048] Figure 8 It is the optical path diagram of the light that is totally reflected in the light guide plate;

[0049] Fig. 9 These are three different cross-section scattering dot structure diagrams;

[0050] Fig.10 A light diagram of light irradiated onto the scattering dot structure of the present invention is made by a drawing method;

[0051] Fig.11 It is the truncated cone shape of the scattering mesh mechanism of the present invention;

[0052] Figure 12-14 is a structural diagram of a light guide plate of the present invention;

[0053] Fig.15 It is the distribution principle diagram of the scattering dot structure on the light guide plate;

[0054] Fig.16 It is a production principle diagram of light guide plate. DETAILED DESCRIPTION

[0055] The following description is used to disclose the present invention so that those skilled in the art can implement the present invention. The preferred embodiments described below are only examples, and those skilled in the art may think of other obvious variations.

[0056] like Figure 7As shown, a planar shadowless light source includes a shell with an installation space inside and a PCBA board 3 arranged in the installation space, LED lamp beads 4 arranged on the PCBA board 3, a light guide plate 6, a first amplification lens 5, and a second amplification lens 7. When viewed from above, the shell and the installation space are both square, the PCBA board 3 has four, which correspond to the four sides of the shell respectively, each PCBA board 3 is attached to the inner side of the shell through a thermal pad 2, and a plurality of LED lamp beads 4 are arranged on one side of each PCBA board 3 facing the center of the bottom shell 1. The light guide plate 6 is square and is arranged in a space surrounded by a plurality of LED lamp beads 4. The plurality of LED lamp beads 4 are irradiated toward the light guide plate 6, and the light emitted by the LED lamp beads 4 enters the light guide plate 6. The first amplifying lens 5 is arranged below the light guide plate 6, and the second amplifying lens 7 is arranged above the light guide plate 6. Foam 9 is respectively arranged on the edges of the upper and lower surfaces of the first amplifying lens 5, and foam 9 is also arranged on the edges of the upper and lower surfaces of the second amplifying lens 7. That is, foam isolation is used between two adjacent structures, which acts as a buffer, avoids contact between adjacent structures, and eliminates water ripples.

[0057] The housing includes a bottom shell 1 and a cover plate 8. A first opening is provided at the bottom of the bottom shell 1, and a second opening is provided at the top. The first opening and the second opening are both square, and the size of the second opening is larger than the size of the first opening. The cover plate 8 is detachably provided at the position of the second opening to block the second opening. A third opening is formed on the cover plate 8. The third opening is also square, and its size is the same as that of the first opening. Light emitted from the light guide plate 6 is emitted from the first opening and the third opening for illumination.

[0058] The light guide plate 6 is made of optical quartz glass.

[0059] The thermal pad 2 is a silicon-free thermal pad, and no silicone oil seeps out during use, thereby ensuring that there is no silicone oil or silicone molecule contamination when used in specific occasions.

[0060] The beam angle θ of the LED lamp bead meets the following conditions:

[0061] θ≤2θ i ,

[0062] Among them, θ i is the critical value of the incident angle of the light emitted by the LED lamp bead entering the light guide plate 6, θ i Satisfies the refraction theorem:

[0063] n i sinθ i =n t sinθ t ,

[0064] n iis the refractive index of air, n t is the refractive index of the light guide plate, θ t is the refraction angle, see Figure 8 , when θ t When is the critical angle of total reflection,

[0065] θ t =arcsin(1 / n t ).

[0066] The light guide plate 6 includes a body 601 and a plurality of scattering dot structures 602 disposed at the bottom of the body 601. The scattering dot structures 602 are actually holes, and the holes are in a truncated cone structure. Fig.11 , the diameter of the upper end is smaller than the diameter of the lower end, Fig. 9 There are three scattering dot structures with different cross sections, which are rectangular, semicircular and trapezoidal. Table 1 shows the light conversion rates of the three scattering dot structures obtained by optical simulation. It can be seen from Table 1 that the light conversion rate of the micro-trapezoidal groove array is the highest. Therefore, the present invention adopts micro-trapezoidal grooves as the dot scattering structure.

[0067] Table 1 Light conversion efficiency of three scattering dot structures

[0068] According to the requirements of field camera shooting and etching process, determine the approximate diameter of the inner and outer bottom surfaces of the dot scattering structure. The camera shooting requirement must meet the requirement that the dot scattering structure cannot be displayed in the image taken during shooting, that is, the size of the dot scattering structure should be as small as possible. For the etching process, when the required dot scattering structure is too small, the etching process is difficult to achieve, that is, the requirements of both must be met at the same time. Generally, the diameter of the inner bottom surface ranges from 12-18um, and the diameter of the outer bottom surface ranges from 25-30um.

[0069] After determining the diameters of the inner and outer bottom surfaces, according to the calculated θ t , the light path refraction theorem, and the reversibility of the light path determine the height of the dot scattering structure. The height of the dot scattering structure satisfies: the reflected light of the light irradiated to the upper edge of the dot scattering structure and the reflected light of the light irradiated to the lower edge of the dot scattering structure will not be totally reflected when irradiated to the light exiting surface of the light guide plate. In practice, the height of the dot scattering structure is randomly selected and randomly arranged within 5μm-9μm to eliminate the stray light interference of the scattering dots on the imaging of the light field camera.

[0070] The distribution of the plurality of scattering point structures 602 on the main body 601 meets the following requirements:

[0071] 1) When viewed from above, the distance between the centers of adjacent scattering dot structures is not greater than a first predetermined value and not less than a second predetermined value. For example, the first predetermined value is 120 um and the second predetermined value is 30 um. The first predetermined value and the second predetermined value are determined according to the requirements of the processing technology. Fig.12 ;

[0072] 2) The circle with each center as the center and a radius R does not include other scattering network point structures. The value of the radius R is determined based on experience, see Fig.15 ;

[0073] When the above two conditions are met, the plurality of scattering dot structures 602 are randomly distributed.

[0074] The light guide plate 6 is manufactured by the following method, which specifically includes the following steps:

[0075] Step 1: Surface preparation: clean and dry the surface of the light guide plate substrate, which is optical glass;

[0076] Step 2: Glue coating: Spin coating a thin layer of negative photoresist on the surface of the light guide plate substrate;

[0077] Step 3: Soft baking: partially evaporate the photoresist solvent by heating;

[0078] Step 4: Alignment and exposure: precisely align the mask with the light guide plate substrate and expose the photoresist. After exposure, the negative photoresist produces a polymer that is insoluble in the developer. Holes corresponding to the scattering dot structure are pre-formed on the mask.

[0079] Step 5, development: applying a developer on the upper surface of the photoresist to remove the non-polymerized photoresist and form a hollow structure on the photoresist;

[0080] Step 6: hard baking to continue evaporating the photoresist solvent;

[0081] Step 7. Development inspection: Check the alignment and defects of the surface;

[0082] Step 8, etching: removing the upper surface of the light guide plate substrate through the hollow structure of the photoresist;

[0083] Step 9: Remove the photoresist (stripping): remove the photoresist on the LGP;

[0084] Step 10: Final inspection: perform surface inspection for etching irregularities or other problems.

[0085] Another method can also be used to manufacture the light guide plate 6, and the specific steps are as follows:

[0086] Step 1: making a quartz template according to the arrangement of the scattering dot structure on the light guide plate 6;

[0087] Step 2: Move the quartz template to the top of the light guide plate substrate and press it down. The light guide plate substrate is made of PMMA. The structure on the PMMA is a polymer structure layer processed by nanoimprint technology.

[0088] Step 3: Move the quartz template upwards to demold it, and transfer the pattern on the quartz template to the light guide plate substrate.

[0089] The above shows and describes the basic principles, main features and advantages of the present invention. Those skilled in the art should understand that the present invention is not limited to the above embodiments. The above embodiments and descriptions only describe the principles of the present invention. The present invention may be subject to various changes and improvements without departing from the spirit and scope of the present invention. These changes and improvements fall within the scope of the present invention. The scope of protection claimed by the present invention is defined by the attached claims and their equivalents.

Claims

1. A planar shadowless light source, comprising: The housing has an installation space inside, a first opening at the bottom, and a third opening at the top; A PCBA board, LED lamp beads, a light guide plate, a first amplification lens, and a second amplification lens are installed in the installation space. The first amplification lens, the light guide plate, and the second amplification lens are arranged in sequence from bottom to top. The PCBA board is arranged on the side of the light guide plate. A plurality of LED lamp beads are evenly arranged on one side of the PCBA board facing the light guide plate. The LED lamp beads irradiate toward the light guide plate. It is characterized in that: In the up and down directions, a circle of foam is respectively arranged between the lower surface of the first amplifying lens and the outer shell, between the lower surface of the light guide plate and the upper surface of the first amplifying lens, between the upper surface of the light guide plate and the lower surface of the second amplifying lens, and between the upper surface of the second amplifying lens and the outer shell.

2. A planar shadowless light source according to claim 1, characterized in that: The shell includes a bottom shell and a cover plate, the first opening is arranged at the bottom of the bottom shell, and the second opening is arranged at the top, the first opening and the second opening are both square, and the size of the second opening is larger than that of the first opening, the cover plate is detachably arranged at the second opening to block or open the second opening, and the third opening is formed on the cover plate, the third opening is also square, and its size is the same as that of the first opening.

3. A planar shadowless light source according to claim 2, characterized in that: The beam angle θ of the LED lamp bead meets the following conditions: θ≤2θ i , Among them, θ i is the critical value of the incident angle of the light emitted by the LED lamp bead entering the light guide plate, θ i Satisfies the refraction theorem: n i sinθ i =n t sinθ t , n i is the refractive index of air, n t is the refractive index of the light guide plate, θ t is the refraction angle, when θ t When is the critical angle of total reflection, θ t =arcsin(1 / n t )。 4. The planar shadowless light source according to claim 3, characterized in that: The light guide plate comprises a body and a plurality of scattering dot structures arranged at the bottom of the body. The scattering dot structures are truncated cone holes, and the diameter of the inner bottom surface of the truncated cone hole is smaller than the diameter of the outer bottom surface.

5. The planar shadowless light source according to claim 4, characterized in that: The diameters of the inner bottom surface and the outer bottom surface of the scattering dot structure meet the following requirements: the scattering dot structure is not displayed in the image captured by the camera, and the diameters of the inner bottom surface and the outer bottom surface are larger than the minimum size that can be achieved by the etching process.

6. The planar shadowless light source according to claim 5, characterized in that: The distribution of the multiple scattering point structures on the body meets the following requirements: 1) When viewed from above, the distance between the centers of adjacent scattering dot structures is not greater than a first predetermined value and not less than a second predetermined value, and the second predetermined value is less than the first predetermined value; 2) A circle with each of the centers as the center and a radius R does not include other scattering point structures, and the value of the radius R is determined based on experience.

7. The planar shadowless light source according to claim 6, characterized in that: The heights of the multiple frustum holes are randomly set within a certain range.

8. The planar shadowless light source according to claim 7, characterized in that: The height of the dot scattering structure satisfies that the reflected light irradiated on the inner bottom edge of the dot scattering structure and the reflected light irradiated on the outer bottom edge of the dot scattering structure will not be totally reflected when irradiated on the light emitting surface of the light guide plate.

9. The planar shadowless light source according to claim 8, characterized in that: The light guide plate is manufactured by the following method, which specifically includes the following steps: Step 1: Surface preparation: clean and dry the surface of the light guide plate substrate, which is optical glass; Step 2: Glue coating: coating a layer of negative photoresist on the surface of the light guide plate substrate; Step 3: Soft baking: partially evaporate the photoresist solvent by heating; Step 4: Alignment and exposure: precisely align the mask with the light guide plate substrate and expose the negative photoresist. After exposure, the negative photoresist produces a polymer that is insoluble in the developer. Holes corresponding to the scattering dot structure are pre-formed on the mask. Step 5, development: applying a developer on the upper surface of the photoresist to remove the non-polymerized photoresist and form a hollow structure on the photoresist; Step 6: hard baking to continue evaporating the photoresist solvent; Step 7. Development inspection: Check the alignment and defects of the surface; Step 8, etching: removing the upper surface of the light guide plate substrate through the hollow structure of the photoresist; Step 9, removing the photoresist: removing the photoresist on the light guide plate substrate; Step 10: Final inspection: perform surface inspection for etching irregularities or other problems.

10. A light guide plate, comprising: ontology; A plurality of scattering point structures are arranged at the bottom of the body, characterized in that: The scattering point structure is a frustum-shaped hole.

Citation Information

Patent Citations

  • Backlight structure of liquid crystal display television

    CN103676318A

  • Display backlight unit

    CN205139529U

  • Backlight module with lattice point structure for preventing light guide plate and reflector plate from being adsorbed

    CN211402808U

  • Shadowless coaxial surface light source capable of eliminating lattice point influence

    CN220688866U

  • Optical waveguide, method for manufacturing the same surface light source device, liquid crystal display, and light source panel therefor