Whole-course testing device for reheating main throttle valve and welding method

By designing a full-process test device and welding method on the reheating main valve, the problem of the valve being unable to open under high load is solved. The material performance is enhanced through spot welding and heat treatment, ensuring that the valve can be opened smoothly and extended under high load conditions and used successfully under high load conditions. life.

CN118913671APending Publication Date: 2024-11-08DATANG GUIZHOU FAER POWER GENERATION
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410975057.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-19
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

Due to the large pressure difference between the front and rear of the valve disc under high load due to the flip-shaped structure and the valve under high load, the valve cannot be opened during high load operation, which may cause the steam turbine overspeed accident.

Method used

Design a full-process test device for reheating main valve, including reheating main valve main valve body and cylinder. By installing cylinders on the valve stem, balancing holes are opened on both sides of the valve disc to weld the pipe seat, and spot welding and heat treatment methods are adopted. , first polish and clean the area to be welded, preheat and weld layer by layer, and then perform electric heating and heat treatment to enhance the mechanical properties and corrosion resistance of the material.

Benefits of technology

It effectively solves the problem that the valve cannot be opened, enhances the mechanical properties and corrosion resistance of the material, extends the service life of the welded parts, and ensures that the valve can be opened smoothly under high load conditions and meets the active test conditions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118913671A_ABST
    Figure CN118913671A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of reheating main valves, and particularly relates to a reheating main valve whole-course test device and a welding method. The reheating main valve whole-course test device comprises a reheating main valve main body and an air cylinder; an air cylinder is installed at one end of the reheating main valve body valve rod, and a valve clack is installed on the inner side of the reheating main valve body valve rod. According to the whole-course test device for the reheated main valve and the welding method, the reheated main valve body, the pipe seat, the pressure-bearing pipe and the balance pipe are subjected to spot welding, in the re-welding process, a to-be-welded area and a surrounding area within 25 mm are firstly polished, the to-be-welded area and the surrounding area within 50 mm are cleaned, the to-be-welded area is preheated, heat treatment is conducted after welding, the mechanical property and corrosion resistance of materials are enhanced, and the reheated main valve body, the pipe seat, the pressure-bearing pipe and the balance pipe are welded together. After the components of the reheating main throttle valve whole-course test device are welded, the mechanical property and corrosion resistance of the material are enhanced, so that the service life and the reliability of the welding piece are prolonged, the valve activity test condition is met, and the valve is smoothly opened.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of a reheat main steam valve, in particular to a full-range test device and a welding method for a reheat main steam valve. Background Art

[0002] The reheat main steam valve is a flap-type reheat main steam valve that controls the flow and temperature of the reheat steam. The reheat main steam valve can adjust the amount of reheat steam to ensure that the heat in the reheater is fully utilized and that the temperature of the reheat steam meets the design requirements, thereby improving the thermal efficiency of the steam turbine and ensuring the stability and safety of the system operation.

[0003] The reheat main steam valve is installed on the reheat steam inlet pipe between the reheater and the reheat regulating steam valve to control the flow and temperature of the reheat steam. In order to prevent power production accidents and turbine overspeed accidents, the reheat main steam valve needs to be tested regularly. Since the reheat main steam valve is a flap-type structure and the pressure difference before and after the high-load valve disc is too large, it is easy to cause the valve to be unable to open after closing during high-load operation of the unit. In order to solve the problem of the reheat main steam valve closing and unable to open, and prevent turbine overspeed accidents, we proposed a full-range test device for the reheat main steam valve. Summary of the invention

[0004] The purpose of the present invention is to provide a full-range test device and welding method for a reheat main steam valve, so as to solve the problem that the reheat main steam valve proposed in the above background technology is a flap-type structural feature, and the pressure difference before and after the high-load valve disc is too large, which easily leads to the problem that the valve cannot be opened after being closed during high-load operation of the unit.

[0005] To achieve the above-mentioned object, the present invention provides the following technical solutions: a reheat main steam valve full-range test device, comprising a reheat main steam valve valve body and a cylinder;

[0006] A cylinder is installed at one end of the valve stem of the reheat main steam valve body, and a valve disc is installed on the inner side of the valve stem of the reheat main steam valve body. Balance holes are separately opened on both sides of the reheat main steam valve body close to the valve disc, and the balance holes are welded to the pipe seat, and the pipe seat is welded to the pressure-bearing pipe, and a weld is arranged between the balance hole and the pipe seat.

[0007] A welding method comprises the following steps:

[0008] S1. Welding pretreatment;

[0009] S1.1, Welding cleaning: Grind the balance hole and the area to be welded on the pipe seat and the surrounding area within 25mm;

[0010] S1.2, Welding cleaning: Use alcohol or acetone to clean the area to be welded and the surrounding area 50mm;

[0011] S1.3. Welding burn prevention: Use appropriate materials to protect the surrounding parent material before welding;

[0012] S2. Welding heating: preheat the area to be welded before welding;

[0013] S2.1. Welding requirements: electrode drying;

[0014] S2.2, welding layer by layer; self-inspection of welds;

[0015] S3. Post-welding treatment: Post-welding heat treatment uses electric heating;

[0016] S3.1、Welding flaw detection: grinding welds;

[0017] Preferably, in S1.1, a grinder is used to grind the area to be welded and the surrounding area within 25 mm to remove scale, burrs, sharp corners, etc. In S1.2, alcohol or acetone is used to clean the area to be welded and the surrounding area within 50 mm to remove impurities such as oil and grease.

[0018] Preferably, in S2, the preheating temperature is 150-200°C, the preheating width starts from the center of the joint, each side is not less than 3 times the thickness of the weldment, and not less than 100 mm. During welding, the temperature of the welding area is ensured to be between 200 and 250°C, and the temperature measuring position should be at least 75 mm away from the welding area. During preheating before welding and welding, a spot temperature gun can be used to measure the temperature and track the interlayer temperature to ensure that the process requirements are met.

[0019] Preferably, in S2.1, the welding rod is dried before use according to the requirements of the welding rod manufacturer, and the welding rod is stored in a heat preservation cylinder during welding and can be taken out when needed.

[0020] Preferably, in S2.2, when welding is performed, the welding is performed layer by layer, the slag needs to be carefully cleaned between layers, and the quality of each weld is self-checked. Welding defects such as pores, slag inclusions, cracks, and lack of fusion are not allowed. Once found, welding should be stopped and welding can only be continued after grinding and removal.

[0021] Preferably, in S3, the heating plate covers an area of ​​400 mm around the tube holder, and the temperature is heated to 720° C. After heating, it is covered with heat-insulating cotton to cool down slowly.

[0022] Preferably, in S3.1, the weld surface is polished to meet the requirements of flaw detection, and nondestructive testing is performed 24 hours after welding and heat treatment are completed.

[0023] Compared with the prior art, the beneficial effects of the present invention are as follows: the reheat main steam valve full-range test device and welding method spot weld the reheat main steam valve valve body, pipe seat, pressure-bearing pipe and balance pipe, and then during the welding process, first grind the area to be welded and the surrounding area within 25mm, clean the area to be welded and the surrounding area 50mm, preheat the area to be welded, and then perform heat treatment after welding to enhance the mechanical properties and corrosion resistance of the material. After the components of the reheat main steam valve full-range test device are welded, the mechanical properties and corrosion resistance of the material are enhanced, thereby extending the service life and reliability of the welded parts, meeting the valve activity test conditions and opening smoothly.

[0024] 1. The reheat main steam valve full-range test device and welding method spot weld the reheat main steam valve body, pipe seat, pressure pipe and balance pipe. During the welding process, the area to be welded and the surrounding area within 25mm are first polished and the area to be welded and the surrounding area within 50mm are cleaned. The area to be welded is preheated, and then heat treatment is performed after welding to eliminate or reduce welding residual stress and avoid deformation or cracking of parts caused by stress concentration. Post-weld heat treatment can improve the metal structure of the welding joint area and refine the grains, thereby improving the tensile strength and toughness of the welding joint, thereby extending the service life and reliability of the welded parts. After the components of the reheat main steam valve full-range test device are welded, the mechanical properties and corrosion resistance of the materials are enhanced, thereby extending the service life and reliability of the welded parts, meeting the valve activity test conditions and opening smoothly. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 It is a schematic diagram of the three-dimensional structure of the balance hole and the tube seat of the present invention;

[0026] Figure 2 It is a schematic diagram of the three-dimensional structure of the pipe seat and the weld of the present invention;

[0027] Figure 3 The figure is a schematic flow chart of the welding method of the full-process test device for the reheat main steam valve of the present invention.

[0028] In the figure: 1. reheat main steam valve body; 101. cylinder; 102. valve disc; 2. balance hole; 201. pipe seat; 2011. welding seam; 202. pressure pipe. DETAILED DESCRIPTION

[0029] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0030] See also Figure 1 and Figure 2, the present invention provides a technical solution: a reheat main steam valve full-range test device, comprising a reheat main steam valve valve body 1 and a cylinder 101;

[0031] A cylinder 101 is installed at one end of the valve stem of the reheat main steam valve body 1, and a valve disc 102 is installed on the inner side of the valve stem of the reheat main steam valve body 1. Balance holes 2 are separately opened on both sides of the reheat main steam valve body 1 close to the valve disc 102, and the balance hole 2 is welded to the pipe seat 201. The pipe seat 201 is welded to the pressure-bearing pipe 202. A welding seam 2011 is arranged between the balance hole 2 and the pipe seat 201. The pipe seat 201 is 100 mm long, 12 mm thick, and φ124×12 mm.

[0032] In specific implementation, according to Figure 1 and Figure 2 , the pipe seat 201 and the pressure-bearing pipe 202 are spot-welded and fixed, and then the balancing hole 2 is opened on the reheat main steam valve body 1. After the balancing hole 2 is expanded, the groove is made, and the groove is made by the inserted pipe seat 201 welding method, the groove angle is 50°~60°, the balancing hole 2 is expanded to φ100mm, the balancing hole 2 and the pipe seat 201 are spot-welded and fixed, the reheat main steam valve body 1 and the pipe seat 201 are welded together, and then the pressure-bearing pipe 202 and the balancing pipe are spot-welded and fixed. The diameter of the balancing pipe is φ100mm, the wall thickness is 8mm, and a manual stop valve is installed on the balancing pipe. By opening a valve before and after the valve disc 102 of the reheat main steam valve body 1 Balance hole 2: a balance hole 2 is opened before and after the bottom disc 102 of the reheat main steam valve, which is controlled by a manual stop valve. Its flow rate is lower than the no-load flow rate at the rated speed. The pressure before and after the disc 102 can be balanced through the pipe seat 201, the pressure pipe 202 and the balance pipe to ensure that the reheat main steam valve body 1 can be opened smoothly. During the use of the reheat main steam valve body 1, there are difficulties in opening the valve and the valve cannot be tested for activity. At the same time, since the working medium of the valve is high temperature and high pressure, the hole expansion, heat treatment and welding process requirements are extremely high. The inner hole of the balance pipe is expanded to φ100mm and heat treated to meet the valve activity test conditions and open smoothly.

[0033] See also Figure 3 The present invention provides a technical solution: a welding method, comprising the following steps:

[0034] S1. Welding pretreatment;

[0035] S1.1, Welding cleaning: Grind the balance hole 2 and the pipe seat 201 to be welded area and the surrounding area within 25mm;

[0036] S1.2, Welding cleaning: Use alcohol or acetone to clean the area to be welded and the surrounding area 50mm;

[0037] S1.3. Welding burn prevention: Use appropriate materials to protect the surrounding parent material before welding;

[0038] S2. Welding heating: preheat the area to be welded before welding;

[0039] S2.1. Welding requirements: electrode drying;

[0040] S2.2, welding layer by layer; self-inspection of welds;

[0041] S3. Post-welding treatment: Post-welding heat treatment uses electric heating;

[0042] S3.1、Welding flaw detection: grinding welds;

[0043] In S1.1, use a grinder to grind the area to be welded and the surrounding area within 25mm to remove scale, burrs, sharp corners, etc. In S1.2, use alcohol or acetone to clean the area to be welded and the surrounding area 50mm to remove impurities such as oil and grease. In S2, the preheating temperature is 150-200℃, and the preheating width starts from the center of the joint, each side is not less than 3 times the thickness of the weldment, and not less than 100mm. During welding, ensure that the temperature of the welding area is 200-250℃, and the temperature measurement position should be at least 75mm away from the welding area. During the preheating and welding process before welding, a spot temperature gun can be used to measure the temperature and track the interlayer temperature to ensure that it meets the process requirements. In S2.1, Before use, the welding rod shall be dried according to the requirements of the welding rod manufacturer. During welding, the welding rod shall be stored in the insulation tube and taken out as needed. In S2.2, welding shall be performed layer by layer, and the slag shall be carefully cleaned between layers. The quality of each weld shall be self-checked. Welding defects such as pores, slag inclusions, cracks, and unfused welds are not allowed. Once found, welding shall be stopped and welding can only be continued after grinding and removal. In S3, the heating plate covers an area of ​​400mm around the pipe seat 201, and the temperature is heated to 720℃. After heating, it is covered with insulation cotton and cooled slowly. In S3.1, the weld surface is ground to meet the requirements of flaw detection. Nondestructive testing is performed 24 hours after welding and heat treatment.

[0044] In specific implementation, when the reheat main steam valve body 1, the pipe seat 201, the pressure pipe 202 and the balance pipe are spot welded, it is necessary to first grind the area to be welded and the surrounding area within 25mm to ensure the quality and strength of the weld. After removing the oxide scale, burrs, sharp corners, etc., the weld can be more uniform and firm. Use alcohol or acetone to clean the area to be welded and the surrounding area 50mm. After removing impurities such as oil and grease, the possibility of defects such as pores and slag inclusions during welding can be effectively reduced. By preheating the temperature to 150-200°C, the material can achieve a more uniform temperature distribution, reduce the residual stress caused by welding, and thus reduce the risk of deformation. It can also improve the metal organization and grain structure of the welding area, making the weld more uniform and dense, and improving the quality and strength of the welding. During the welding process, preheating can make the welding parameters easier to control, the welding speed more efficient, and preheating can improve the welding speed. The high impact toughness and fatigue resistance of the welded joint make the welded connection more reliable and durable. Welding layer by layer and removing the welding slag between layers can prevent it from being mixed in the weld, thereby avoiding the formation of welding defects such as pores and slag inclusions. The post-weld heat treatment uses electric heating to effectively eliminate or reduce welding residual stress and avoid deformation or cracking of parts caused by stress concentration. Post-weld heat treatment can improve the metal structure in the welded joint area and refine the grains, thereby improving the tensile strength and toughness of the welded joint. In particular, heat preservation at high temperature helps to dissolve the carbides in the weld evenly, further improve the welding quality, and improve the corrosion resistance of the welded joint, making it more stable and durable in use. After the components of the reheat main steam valve full-process test device are welded, the mechanical properties and corrosion resistance of the material are enhanced, thereby extending the service life and reliability of the welded parts.

[0045] In summary, the reheat main steam valve body 1, the pipe seat 201, the pressure pipe 202 and the balance pipe are spot welded. During the welding process, the area to be welded and the surrounding area within 25mm are first polished and the area to be welded and the surrounding area 50mm are cleaned to reduce the possibility of defects such as pores and slag inclusions during welding. The area to be welded is preheated to improve the metal organization and grain structure of the welding area, so that the weld is more uniform and dense, and the quality and strength of the welding are improved. After welding, heat treatment is performed to eliminate or reduce welding residual stress and avoid deformation or cracking of parts caused by stress concentration, thereby improving the tensile strength and toughness of the welded joint, enhancing the mechanical properties and corrosion resistance of the material, thereby extending the service life and reliability of the welded parts, and after the components of the reheat main steam valve full-range test device are welded, the mechanical properties and corrosion resistance of the material are enhanced, thereby extending the service life and reliability of the welded parts, meeting the valve activity test conditions and opening smoothly. The contents not described in detail in this description belong to the prior art known to professional and technical personnel in this field.

[0046] Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments, or to make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A full-range test device for a reheat main steam valve, characterized in that: It comprises a reheat main steam valve body (1) and a cylinder (101); A cylinder (101) is installed at one end of the valve stem of the reheat main steam valve body (1), and a valve flap (102) is installed on the inner side of the valve stem of the reheat main steam valve body (1). The reheat main steam valve body (1) is provided with balancing holes (2) on both sides close to the valve flap (102), and the balancing holes (2) are welded to a pipe seat (201), and the pipe seat (201) is welded to a pressure-bearing pipe (202), and a welding seam (2011) is provided between the balancing hole (2) and the pipe seat (201).

2. A welding method for a full-range test device for a reheat main steam valve, characterized in that: The following steps are involved: S1. Welding pretreatment; S1.

1. Welding cleaning: Grind the area to be welded of the balancing hole (2) and the pipe seat (201) and the surrounding area within 25 mm; S1.2, Welding cleaning: Use alcohol or acetone to clean the area to be welded and the surrounding area 50mm; S1.

3. Welding burn prevention: Use appropriate materials to protect the surrounding parent materials before welding; S2. Welding heating: preheat the area to be welded before welding; S2.

1. Welding requirements: electrode drying; S2.2, welding layer by layer; self-inspection of welds; S3. Post-welding treatment: Post-welding heat treatment uses electric heating; S3.

1. Welding flaw detection: Grinding welds.

3. The welding method of the reheat main steam valve full-range test device according to claim 2 is characterized in that: In S1.1, use a grinder to grind the area to be welded and the surrounding area within 25 mm to remove scale, burrs, sharp corners, etc. In S1.2, use alcohol or acetone to clean the area to be welded and the surrounding area within 50 mm to remove impurities such as oil and grease.

4. The welding method of the reheat main steam valve full-range test device according to claim 2 is characterized in that: In S2, the preheating temperature is 150-200℃, the preheating width starts from the center of the joint, each side is not less than 3 times the thickness of the weldment, and not less than 100mm. During welding, the temperature of the welding area is guaranteed to be between 200 and 250℃, and the temperature measurement position should be at least 75mm away from the welding area. During the preheating before welding and the welding process, a spot temperature gun can be used to measure the temperature and track the interlayer temperature to ensure that it meets the process requirements.

5. The welding method of the reheat main steam valve full-range test device according to claim 2 is characterized in that: In S2.1, the welding rod is dried according to the requirements of the welding rod manufacturer before use. During welding, the welding rod is stored in a heat preservation tube and can be taken out when needed.

6. The welding method of the reheat main steam valve full-range test device according to claim 2 is characterized in that: In S2.2, welding is performed layer by layer, and slag needs to be carefully cleaned between layers. The quality of each weld should be self-checked. Welding defects such as pores, slag inclusions, cracks, and lack of fusion are not allowed. Once found, welding should be stopped and welding can only be continued after grinding and removal.

7. The welding method of the reheat main steam valve full-range test device according to claim 2 is characterized in that: In S3, the heating plate covers an area of ​​400 mm around the tube holder, and the temperature is heated to 720°C. After heating, it is covered with thermal insulation cotton to slowly cool down.

8. The welding method of the reheat main steam valve full-range test device according to claim 2 is characterized in that: In S3.1, the weld surface is ground to meet the requirements of flaw detection, and nondestructive testing is performed 24 hours after welding and heat treatment are completed.