Method for rapidly and repeatedly verifying lithium ion battery material system and process performance

By adopting threaded connection and vacuum valve technology, the problems of long development cycle and waste of materials in the lithium-ion battery material system and process are solved, and fast, stable and repeatable battery performance verification is achieved, equipment and labor costs are reduced, and the cost of equipment is increased. Battery consistency and safety.

CN118914871APending Publication Date: 2024-11-08SHENYANG GUOKE NEW ENERGY MATERIALS & DEVICES IND TECH RES INST CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410941016.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-15
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

At this stage, the development cycle of lithium-ion battery material system and process is long, the performance is difficult to repeat, the equipment requirements are high, the manpower and material cost is large, and the experimental battery packaging materials are seriously wasted, which cannot meet the needs of fast, stable and repeatable verification.

Method used

The packaging body consisting of a battery test base, sealing ring, upper cover plate, battery cell under test and fastening bolts is used to achieve a closed space through threaded connection and sealing ring. The vacuum check valve and vacuum pressure relief valve are used for battery assembly and disassembly. Replace traditional ultrasonic welding and laser welding to achieve rapid, lossless disassembly and reuse.

Benefits of technology

It realizes rapid and repeated verification of the material system and process performance of lithium-ion batteries, reduces equipment costs and manpower and material investment, reduces waste of packaging materials, improves the consistency and repeatability of experimental batteries, and ensures stability in a wide temperature range. Sex and safety.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118914871A_ABST
    Figure CN118914871A_ABST
Patent Text Reader

Abstract

The invention relates to the field of new energy lithium ion battery research, manufacturing and testing, in particular to a method for rapidly and repeatedly verifying a lithium ion battery material system and process performance. A packaging main body of the experimental lithium ion battery is composed of a battery testing base, a sealing ring, an upper cover plate, a tested battery cell and a fastening bolt, the battery testing base, the sealing ring and the upper cover plate are injection-molded by using an electrolyte-resistant material, and all the components are in threaded connection or elastically attached by virtue of tight connection among the battery testing base, the sealing ring and the upper cover plate. A closed space isolated from the outside is formed, and a good electrochemical reaction environment is provided; according to the invention, by designing the packaging shell structure of the tested battery cell, on the premise of not influencing the electrochemical reaction and performance of the lithium ion battery, the preparation and test of the experimental lithium ion battery are quicker and more convenient, the battery can be quickly disassembled after the test is completed, and the assembly can be repeatedly used after being cleaned and dried, and is green, environment-friendly, firm and durable.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the research, manufacture and testing fields of new energy lithium-ion batteries, and specifically to a method for rapidly and repeatedly verifying lithium-ion battery material systems and process performance. Background Art

[0002] Since the advent of lithium-ion secondary battery technology, it has been widely used due to its excellent performance, such as in digital products, transportation, power tools, aerospace exploration and other fields. With the development of society, the use of power sources has become more complex and the environment has become more harsh, such as requiring a wider operating temperature, higher power density or energy density, and higher safety performance. There is an urgent need to develop more advanced battery technology.

[0003] In the previous research on lithium-ion battery-related materials and systems, scholars need to conduct systematic analysis and characterization of the research objects, such as infrared, Raman, scanning electron microscopy, and X-ray diffraction, to deduce the physical and chemical properties of the materials, and try to reveal the influence of material structure on electrochemical reactions from the perspective of materials science. The results are further verified by preparing half-cell tests to guide the development direction of the new generation of lithium battery materials. The research on traditional battery material systems usually uses half-cells as carriers to analyze the performance advantages of new material systems under specific conditions. However, due to their own high impedance, low current density, and easy short circuits during the packaging process, half-cells can only meet performance tests under certain conditions, and the performance under a wider temperature range and higher power density, as well as the stability and safety performance of the system, cannot be accurately evaluated.

[0004] Some scholars choose to prepare new materials or processes into full batteries, and prove their research results through the test data of full batteries. Compared with half-batteries, full batteries can illustrate the performance of materials and systems on a larger scale, and full batteries meet the needs of high and low temperature adaptability, power type verification, safety assessment and other work, and can more comprehensively and specifically discuss the advanced nature of the research content. Similar to commercial batteries, full batteries used in laboratory research usually adopt soft packs, cylindrical aluminum shells or square aluminum shells, but due to structural limitations, specific instruments and equipment are required to assist in battery assembly, such as aluminum-plastic film punching machines, heat sealing machines, ultrasonic welding machines, laser welding machines, etc. The processing is complex and the precision requirements are high. It is easy to have problems such as poor packaging and electrolyte leakage, which affect the performance of the battery. After the test is completed, because the components cannot be disassembled without loss and cannot be reused many times, they are scrapped, which is a serious waste of resources and is not conducive to environmental protection.

[0005] With the increasing research on new material systems and processes for lithium-ion batteries, there is an urgent need for a method that can quickly, stably and repeatably verify the performance of new materials and processes for lithium-ion batteries. Summary of the invention

[0006] In the process of studying new lithium-ion battery material systems and process performance, there are difficulties such as long experimental lithium-ion battery preparation cycle, poor consistency and difficulty in repeated verification, and serious waste of packaging materials. The purpose of the present invention is to provide a method for quickly and repeatedly verifying the performance of lithium-ion battery material systems and processes, so as to solve the problems of long development cycle, difficult performance duplication, high equipment requirements, and large investment in manpower and material costs in the current research of lithium-ion battery material systems and processes.

[0007] The technical solution of the present invention is as follows:

[0008] A method for quickly and repeatedly verifying the material system and process performance of a lithium-ion battery. The packaging body of the experimental lithium-ion battery is composed of a battery test base, a sealing ring, an upper cover, a tested battery cell and fastening bolts. The battery test base, the sealing ring and the upper cover are injection molded using electrolyte-resistant materials. The three are tightly connected, and each component is threaded or elastically fitted to form a closed space isolated from the outside world, providing a good electrochemical reaction environment.

[0009] The upper cover plate and the battery test base are arranged opposite to each other in upper and lower parts. A groove one is opened on the left side of the battery test base for placing the battery cell under test. A groove two is opened close to the right side of the groove one for storage during battery formation and transition buffering during exhaust operation. A groove three is opened on the top of the battery test base and on the outer sides of the groove one and the groove two. A sealing groove corresponding to the groove three is opened on the bottom of the upper cover plate. The sealing ring is embedded in the groove three and the sealing groove and fits well.

[0010] The method for quickly and repeatedly verifying the material system and process performance of a lithium-ion battery is to open two internal threaded through holes in the middle of the upper cover plate and the corresponding position of the groove 2, and install a pure copper vacuum check valve and a vacuum pressure relief valve respectively, which are used for vacuum exhaust of the battery after battery assembly is completed and vacuum relief operation when the battery is disassembled after testing is completed.

[0011] The method for quickly and repeatedly verifying the material system and process performance of a lithium-ion battery is characterized in that the outer sides of a battery test base and an upper cover are square, the length and width of the outer sides of the battery test base and the upper cover are the same, through holes are made at the edges of the battery test base and the upper cover, and are evenly distributed along a circle of the battery test base and the upper cover, bolts are inserted into the through holes and tightened with nuts to achieve connection between the base and the upper cover; a regular hexagonal groove is opened at the hole opening position on the bottom surface of the battery test base, the nuts used are embedded in the groove and fixed with glue, the bolts are inserted into the through holes and tightened, so that the battery test base and the upper cover are fitted together, and the bolts cooperate with the sealing ring to achieve isolation between the tested battery cell and the external environment.

[0012] The method for quickly and repeatedly verifying the material system and process performance of a lithium-ion battery is characterized in that the battery test base is provided with an aluminum positive electrode test terminal and a copper negative electrode test terminal, the positive electrode test terminal and the negative electrode test terminal are provided with a vertical bolt structure on the inner side of a groove in which the tested battery cell is placed in the battery test base, and the positive electrode test terminal and the negative electrode test terminal are placed on the outer side of the groove in which the tested battery cell is placed in the battery test base. One of sheet, line, stud, and metal table is selected according to the test channel; the positive electrode ear and the negative electrode ear of the tested battery cell are punched in advance, and the bolts on the positive electrode test terminal and the negative electrode test terminal are respectively inserted during assembly, and are pressed with a metal pressing block of a corresponding material, and then tightened with a nut, and the battery test base and the upper cover are tightened with bolts and nuts.

[0013] The method for quickly and repeatedly verifying the material system and process performance of a lithium-ion battery, the battery test base includes a positive electrode test terminal, a positive electrode test end rivet bolt, a negative electrode test terminal, a negative electrode test end rivet bolt, and a base, and the specific structure is as follows:

[0014] A groove is provided in the middle of the rectangular base, and base through holes are evenly provided around the top edge of the rectangular base. The grooves include groove one, groove two, and groove three. The rectangular groove one is connected to the rectangular groove two to form a stepped base total groove. The length of the groove one is equal to the length of the groove two, and the width and depth of the groove one are respectively greater than the width and depth of the groove two. A rectangular groove three is provided on the periphery of the base total groove; the ends of the positive test terminal and the negative test terminal extending into the groove one are the internal connection ends of the pole ears, and the positive test terminal A positive test terminal rivet bolt is provided on the internal connection end of the tab of the sub-electrode, and a negative test terminal rivet bolt is provided on the internal connection end of the tab of the negative test terminal. The positive test terminal and the negative test terminal correspond to the positive tab and the negative tab of the tested battery cell respectively through the internal connection end of the tab. The positive test end rivet bolt and the negative test end rivet bolt are respectively connected to the central openings of the positive tab and the negative tab. The positive test terminal and the negative test terminal are extended to the ends outside the groove to respectively open a positive test terminal through hole and a negative test terminal through hole.

[0015] The method for quickly and repeatedly verifying the material system and process performance of a lithium-ion battery comprises installing the positive electrode test terminal and the negative electrode test terminal in parallel on the same side of the base perpendicular to the width direction of the groove, or installing the positive electrode test terminal and the negative electrode test terminal in parallel on the opposite side of the base perpendicular to the width direction of the groove.

[0016] The method for quickly and repeatedly verifying the material system and process performance of a lithium-ion battery is as follows: groove three is a sealing groove with a semicircular rectangular cross section opened at the outermost side of the total groove of the base, and a sealing groove with a semicircular rectangular cross section corresponding to groove three is opened at the bottom of the upper cover plate, so that the sealing ring is embedded in groove three and the sealing groove and fits tightly.

[0017] The method for quickly and repeatedly verifying the material system and process performance of a lithium-ion battery is characterized in that the tested battery cell is of square design, and the tested battery cell is composed of a positive electrode sheet, a negative electrode sheet and a diaphragm, and the composition is stacked or wound; the positive electrode system is one or more of lithium iron phosphate, lithium iron manganese phosphate, lithium nickel cobalt manganese oxide, lithium manganate, and metallic lithium; the negative electrode system is one or more of graphite, modified coated graphite, hard carbon, soft carbon, mesophase carbon microspheres, and lithium metal; and the diaphragm material is one or more of polyethylene and polypropylene or a composite of the two.

[0018] The method for quickly and repeatedly verifying the material system and process performance of a lithium-ion battery, the battery test base, upper cover plate and sealing ring required for the packaging body of the experimental lithium-ion battery are all made of electrolyte-resistant materials, the battery test base and upper cover plate are made of resin polymer materials that are resistant to electrolytes and do not participate in electrochemical reactions, including one or more of polyvinyl chloride, polytetrafluoroethylene, polypropylene and polyethylene; an annular sealing ring is used between the battery test base and the upper cover plate, and the material of the sealing ring includes one or more of ethylene propylene diene monomer rubber, perfluoroether rubber and silicone.

[0019] The method for quickly and repeatedly verifying the material system and process performance of lithium-ion batteries comprises the following steps: in a low-humidity environment with an ambient dew point temperature of less than -45°C, circular holes are opened on the top of the positive and negative ears of the tested battery cell, and the tested battery cell is placed in a rectangular slotted space of a battery test base; the positive ear of the tested battery cell is inserted into the positive test end rivet bolt on the positive test terminal, and then a nut made of aluminum or aluminum alloy is used to lock and connect it to the positive test terminal on the battery test base; in the same way, the negative ear of the tested battery cell is inserted into the negative test end rivet bolt on the negative test terminal, and then a nut made of copper or copper-plated nickel is used to connect it to the negative test terminal on the battery test base; the required electrolyte is injected into the groove of the battery test base where the tested battery cell is located, and then the battery is sealed on the top of the base. Put the sealing ring on the sealing groove, cover the upper cover, and align the upper cover with the edge of the battery test base; use bolts and nuts to penetrate the through holes of the upper cover and the base, and tighten the bolts to ensure that the upper cover and the battery test base are well sealed; close the vacuum pressure relief valve on the upper cover, and let it stand for 6 to 24 hours to ensure that the electrolyte fully infiltrates the tested battery cell; transfer the package body of the experimental lithium-ion battery to a normal atmosphere, connect the vacuum check valve on the upper cover and the vacuum pump, turn on the vacuum pump to evacuate the battery until the relative vacuum degree is below -95KPa, and disconnect the pipeline; at this point, the preparation of the experimental lithium-ion battery package body is completed, and the battery test and test data are sorted. After the battery test is completed, the tested battery cell and the battery test base are disassembled non-destructively, and the battery test base is reused after cleaning and drying.

[0020] The technical design ideas of the present invention are as follows:

[0021] Traditional lithium-ion battery structures, such as soft packs, cylindrical and square aluminum shells, require ultrasonic welding to complete the connection between the tested battery cell tabs and the shell during the assembly process; cylindrical and aluminum shell batteries also require laser welding equipment to complete the shell packaging when the cover plate and the shell are connected, and soft packs require a heat sealer to complete the packaging. However, the equipment cost of the laser welding machine is relatively high, and special tooling and fixtures are required during welding processing. The tooling debugging is cumbersome when switching battery models, or when using soft pack aluminum plastic film packaging, poor packaging, gas leakage and electrolyte leakage problems occur, and the stable testing of the battery over a long period of time cannot be guaranteed; during the battery assembly process, the battery components have become one, and non-destructive disassembly cannot be achieved after the test is completed. The battery can only be scrapped, resulting in a large amount of packaging material waste.

[0022] Here, we propose a method for quickly and repeatedly verifying the material system and process performance of lithium-ion batteries. Specifically, the battery packaging body is made of materials with certain physical strength and no swelling and deformation under long-term immersion in organic solvents within a wide temperature range; materials with good sealing performance and no swelling and deformation under long-term immersion in organic solvents are selected as the sealing medium of the experimental lithium-ion battery; the positive and negative ears of the tested battery cell and the positive and negative test terminals on the battery test base are connected by bolts instead of traditional ultrasonic welding. After the battery test is completed, the tested battery cell and the battery test base can be disassembled without loss by unscrewing the bolts, and the battery test base can be reused after cleaning and drying; a vacuum check valve and a vacuum pressure relief valve are set on the cover plate of the experimental lithium-ion battery, which can be connected to an external vacuum device to provide a negative pressure or vacuum internal environment for the battery. The battery test base, the tested battery cell, the sealing ring, the upper cover plate and the fastening bolts are connected and assembled in sequence. There is no need to use ultrasonic welding, laser welding, aluminum-plastic film punching machine, heat sealing machine and other equipment. Only the bolts at the corresponding positions need to be tightened to complete the assembly of the experimental lithium-ion battery, thereby achieving the purpose of rapid and repeated verification of the lithium-ion battery material system and process performance.

[0023] The advantages and beneficial effects of the present invention are:

[0024] 1. Compared with the traditional lithium-ion battery assembly process, the present invention adopts bolt connection instead of ultrasonic welding, and the shell packaging uses bolts and sealing rings to replace aluminum-plastic film heat sealing and laser welding. The battery assembly, packaging and disassembly process can be realized by manually tightening the bolts, which is convenient and fast.

[0025] 2. The components used in the present invention are only fastened and connected mechanically, and the electrolyte will not damage the components. After the battery is disassembled, the components can be repeatedly used after cleaning and drying, reducing the loss of packaging materials, such as aluminum-plastic film, tabs, aluminum shell and aluminum cover, which is green and environmentally friendly.

[0026] 3. The present invention arranges a vacuum check valve and a vacuum pressure relief valve on the upper cover plate of the battery. After the battery is assembled, the vacuum is evacuated and the air is sealed to provide a good internal environment for the electrochemical reaction of the tested battery cell. After the test is completed, the vacuum in the battery can be released to facilitate the rapid disassembly and anatomical research of the battery. Moreover, once a large amount of gas is produced during the battery test, the gas can be discharged automatically through the vacuum check valve to avoid battery explosion and injury due to excessive accumulation of gas pressure, which is safer and more reliable.

[0027] 4. The material used for the battery shell of the present invention is colorless and translucent, and the color and state changes of the tested battery cell and electrolyte during the test process can be observed visually, which can assist in evaluating the battery status.

[0028] 5. The experimental lithium-ion battery prepared by the present invention has good consistency and high repeatability. At the same time, it can meet the research and testing needs of different battery systems, different ambient temperatures, different processing technologies, etc., and has high compatibility. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] Figure 1 It is a flow chart of the implementation process of the present invention.

[0030] Figure 2 This is a schematic diagram of the battery test base structure used for wide-temperature lithium iron phosphate material system research. In the figure, 1-positive electrode test terminal, 2-positive electrode test terminal rivet bolt, 3-positive electrode test terminal through hole, 4-negative electrode test terminal, 5-negative electrode test terminal rivet bolt, 6-negative electrode test terminal through hole, 7-base, 8-groove 1, 9-groove 2, 10-groove 3, 11-base through hole, 12-ear internal connection terminal.

[0031] Figure 3 The 1C discharge curve of the wide-temperature design lithium iron phosphate experimental lithium-ion battery at different temperatures. In the figure, the horizontal axis Capacity Percent represents the discharge capacity percentage (%), and the vertical axis voltage represents the voltage (V).

[0032] Figure 4 This is a schematic diagram of the battery test base structure used for the research of power-type lithium iron phosphate material system. In the figure, 1-positive electrode test terminal, 2-positive electrode test terminal rivet bolt, 3-positive electrode test terminal through hole, 4-negative electrode test terminal, 5-negative electrode test terminal rivet bolt, 6-negative electrode test terminal through hole, 7-base, 8-groove 1, 9-groove 2, 10-groove 3, 11-base through hole, 12-ear internal connection terminal.

[0033] Figure 5The discharge curve of the experimental lithium iron phosphate lithium-ion battery designed for power type at room temperature from 1C to 9C. In the figure, the horizontal axis Capacity Percent represents the discharge capacity percentage (%), and the vertical axis voltage represents the voltage (V). DETAILED DESCRIPTION

[0034] In the specific implementation process, the present invention proposes a method for quickly and repeatedly verifying the material system and process performance of lithium-ion batteries. The battery packaging body is composed of five components: a battery test base, a sealing ring, an upper cover plate, a tested battery cell and a fastening bolt. The battery test base, the sealing ring and the upper cover plate are injection molded using electrolyte-resistant materials. Relying on the close connection between the three, a closed space isolated from the outside world is formed to provide a good electrochemical reaction environment. All components are threaded or elastically fitted, which is convenient and fast to disassemble and assemble. Except for the tested battery cell, the components can be reused after cleaning and drying.

[0035] The battery test base is provided with an aluminum positive test terminal and a copper negative test terminal. The positive test terminal and the negative test terminal are provided with a vertical bolt structure on the inner side of the groove where the tested battery cell is placed in the battery test base. The positive test terminal and the negative test terminal can be selected from one of sheet, line, stud, and metal table according to the test channel on the outside of the groove where the tested battery cell is placed in the battery test base; the positive and negative ears of the tested battery cell are punched in advance, and the bolts on the positive and negative test terminals are respectively inserted during assembly, and are pressed with metal blocks of corresponding materials, and then tightened with nuts. The battery test base and the upper cover are tightened with bolts and nuts.

[0036] The outer sides of the battery test base and the upper cover are square, and the length and width of the outer sides of the battery test base and the upper cover are the same. Through holes are made at the edges of the battery test base and the upper cover, and multiple holes are distributed along the battery test base and the upper cover. Bolts are inserted into the through holes and tightened with nuts to achieve the connection between the base and the upper cover. Preferably, a regular hexagonal groove can be opened at the hole opening position on the bottom surface of the battery test base, and the nuts used are embedded in the grooves and fixed with AB glue. The bolts are inserted into the through holes and tightened to make the battery test base fit with the upper cover. The bolts cooperate with the sealing ring to achieve the isolation of the tested battery cell from the external environment.

[0037] A groove one is opened on the left side of the battery test base for placing the battery cell under test, and a groove two is opened on the right side near the groove one for storage when the battery is formed and gas is produced and for transition buffering during exhaust operations; two internal threaded through holes are opened in the middle of the upper cover plate corresponding to the groove two, and a pure copper vacuum check valve and a vacuum pressure relief valve are respectively installed, which are used for vacuum exhaust of the battery after battery assembly is completed and for vacuum relief operations when the battery is disassembled after testing is completed.

[0038] The internal tested cell of the experimental lithium-ion battery is of square design. The tested cell is composed of a positive electrode sheet, a negative electrode sheet and a separator. The composition includes but is not limited to a stacked type or a wound type. The positive electrode system can be one or more of lithium iron phosphate, lithium iron manganese phosphate, lithium nickel cobalt manganese oxide, lithium manganese oxide, and metallic lithium. The negative electrode system can be one or more of graphite, modified coated graphite, hard carbon, soft carbon, mesophase carbon microspheres, and lithium metal. The separator material can be one of polyethylene and polypropylene or a composite of both.

[0039] The battery test base, upper cover and sealing ring required for the battery packaging body are all made of electrolyte-resistant materials. They will not dissolve, swell or deform when in contact with the electrolyte and can be used multiple times. The battery test base and upper cover are made of resin polymer materials that are resistant to electrolytes and do not participate in electrochemical reactions, including but not limited to one or more of polyvinyl chloride (PVC), polytetrafluoroethylene (PVDF), polypropylene (PP) and polyethylene (PE); an annular sealing ring is used between the battery test base and the upper cover, and the material of the sealing ring includes but is not limited to one or more of ethylene propylene diene monomer rubber (EPDM), perfluoroether rubber (FFKM), and silicone. The materials used for the battery packaging body components can maintain good physical properties in a wide temperature range of -70°C to 85°C, meet the battery performance research under different temperature environments and different charge and discharge rates, and have a safe structure.

[0040] The method requires that in a clean room or glove box (hereinafter referred to as a low-humidity environment) with an ambient dew point temperature of less than -45°C, circular holes are opened on the top of the positive and negative ears of the tested battery cell, and the tested battery cell is placed in the rectangular slotted space of the battery test base; the positive ear of the tested battery cell is inserted into the positive test end rivet bolt on the positive test terminal, and then locked and connected to the positive test terminal on the battery test base using a nut made of aluminum or aluminum alloy; in the same way, the negative ear of the tested battery cell is inserted into the negative test end rivet bolt on the negative test terminal, and then connected to the negative test terminal on the battery test base using a nut made of copper or copper-plated nickel; the required electrolyte is injected into the groove of the battery test base where the tested battery cell is located Then put the sealing ring in the sealing groove at the top of the base, cover the upper cover, and align the upper cover with the edge of the battery test base; use bolts and nuts to penetrate the through holes of the upper cover and the base, and tighten the bolts to ensure that the upper cover and the battery test base are well sealed; close the vacuum pressure relief valve on the upper cover, and let it stand for 6 to 24 hours to ensure that the electrolyte fully infiltrates the tested battery cell; transfer the package body of the experimental lithium-ion battery to a normal atmosphere, connect the vacuum check valve on the upper cover and the vacuum pump, turn on the vacuum pump to evacuate the battery until the relative vacuum degree is below -95KPa, and disconnect the pipeline; at this point, the preparation of the experimental lithium-ion battery package body is completed, and finally the battery test and test data collation are carried out. The implementation process is as follows Figure 1 shown.

[0041] The present invention is further described in detail below through examples and drawings.

[0042] Embodiment 1:

[0043] In this embodiment, a preparation method for an experimental lithium-ion battery for studying a wide temperature range lithium iron phosphate positive electrode and a graphite negative electrode system is as follows:

[0044] (1) According to the design of wide temperature range lithium iron phosphate battery material system, the positive electrode uses three-dimensional carbon-coated lithium iron phosphate, and the negative electrode uses wide temperature range artificial graphite. The pulping, coating, rolling and die-cutting processes are completed in sequence to obtain positive and negative electrode sheets with the following dimensions: the positive electrode sheet has a length of 120 mm, a width of 62 mm, and a thickness of 183 μm; the negative electrode sheet has a length of 123 mm, a width of 65 mm, and a thickness of 117 μm.

[0045] (2) According to the design requirements, the positive and negative electrodes described in (1) are stacked with a double-layer polypropylene diaphragm with a width of 129 mm and a thickness of 20 μm using a stacking machine, and the positive and negative ears are led out on the same side. After the stacking is completed, the tested battery cell is fixed with green termination tape; the positive and negative ears of the tested battery cell protrude from the diaphragm by 8 mm and 16 mm, and the distance between the positive and negative ears is 20 mm. Aluminum tape and nickel tape are used to wrap the positive and negative ears of the tested battery cell once and press them tightly, and a hole puncher is used to make a Φ4 mm hole in the center of the protruding part of the positive and negative ears; the tested battery cell is transferred to the hot and cold press for pressing, and the parameters are set to 85°C for the upper plate, 65°C for the lower plate, 2MPa for the pressure, and 20 seconds for the pressure holding time; after the pressing is completed, the positive and negative electrodes of the battery cell are tested with a short circuit tester to confirm that there is no short circuit abnormality. At this point, the preparation of the tested battery cell is completed.

[0046] (3) The tested battery cell described in (2) is transferred to a high vacuum (vacuum pressure of 200 Pa) liquid bath oven at 86°C and baked until the water content of the positive electrode sheet is less than 260 ppm; the tested battery cell is cooled to room temperature after baking, and transferred to a low humidity environment for standby use.

[0047] (4) Figure 2 As shown, the battery test base mainly includes a positive electrode test terminal 1, a positive electrode test end rivet bolt 2, a negative electrode test terminal 4, a negative electrode test end rivet bolt 5, and a base 7. The specific structure is as follows:

[0048] A groove is provided in the middle of the rectangular base 7, and base through holes 11 are evenly provided around the top edge of the rectangular base 7. The grooves include groove 1 8, groove 2 9, and groove 3 10. The rectangular groove 1 8 is connected with the rectangular groove 2 9 to form a stepped base total groove. The length of the groove 1 8 is equal to the length of the groove 2 9, and the width and depth of the groove 1 8 are respectively greater than the width and depth of the groove 2 9. A rectangular groove 3 10 is provided on the periphery of the base total groove; the positive test terminal 1 and the negative test terminal 4 are relatively parallel installed on the same side of the base 7 perpendicular to the width direction of the groove 1 8, and the positive test terminal 1 and the negative test terminal 4 extend to the groove 1 One end inside 8 is the internal connection end 12 of the pole ear, and a positive test end rivet bolt 2 is provided on the internal connection end 12 of the pole ear of the positive test terminal 1, and a negative test end rivet bolt 5 is provided on the internal connection end 12 of the pole ear of the negative test terminal 4. The positive test terminal 1 and the negative test terminal 4 correspond to the positive pole ear and the negative pole ear of the tested battery cell respectively through the internal connection end 12 of the pole ear, and the positive test end rivet bolt 2 and the negative test end rivet bolt 5 are respectively connected to the central openings of the positive pole ear and the negative pole ear, and the positive test terminal 1 and the negative test terminal 4 extend to the ends outside the groove 8 to respectively open a positive test end through hole 3 and a negative test end through hole 6.

[0049] The size parameters of the battery test base of the experimental lithium-ion battery are as follows: the base 7 has a total length of 180 mm, a total width of 150 mm, and a total thickness of 15 mm; a rectangular groove (groove-8) is made 20 mm away from the left edge, with a length of 140 mm, a width of 80 mm, and a depth of 5 mm. An oriented polyethylene (OPS) expansion tape with the same length and width and a thickness of 0.5 mm is pasted at the bottom of the groove. The function of the OPS expansion tape is: after absorbing the electrolyte, it will expand by 150-200%, effectively filling the residual space in the thickness direction of the mold, exerting pressure on the positive and negative electrode sheets of the battery cell, and keeping the electrochemical reaction interface flat; in the groove A rectangular groove (groove two 9) with a length of 140mm, a width of 30mm and a depth of 2mm is made at the adjacent position on the right side of groove one 8; groove one 8 is connected with groove two 9 to form a stepped base total groove, and the outer dimensions of the base total groove are: length 140mm, width 110mm, and a rectangular semicircular sealing groove (groove three 10) with a groove width of 3mm, a groove length of 150mm, a groove width of 120mm, and an R3mm chamfer at the right angle position; a circle of Φ6mm through holes is made in the base 7.5mm away from the edge, 4 holes are set on one side in the length direction, and 2 holes are set on one side in the width direction, with a total of 12 holes in one circle.

[0050] (5) According to the size of the battery cell to be tested, the size parameters of the connecting piece of the battery test base of the experimental lithium-ion battery are as follows: the size of the protruding part of the internal connection terminal 12 of the pole ear of the base 7 is: length 5mm, width 16mm, the distance between the two internal connection terminals 12 of the pole ears is 20mm, the protruding part of the positive electrode is an aluminum sheet with a thickness of 2.5mm, and the negative electrode is a copper-plated nickel sheet with a thickness of 2.5mm. The center position of the protruding part is riveted and fixed with an M4 bolt with a thread length of 4mm. The material of the rivet bolt at the positive test end is aluminum, and the material of the rivet bolt at the negative test end is copper.

[0051] (6) According to the size of the battery cell being tested, the size parameters of the upper cover of the experimental lithium-ion battery are as follows: the total length of the upper cover is 180 mm, the total width is 150 mm, and the total thickness is 10 mm; a rectangular sealing groove is made 15 mm away from the edge of the upper cover, with a groove width of 3 mm, a groove length of 150 mm, and a groove width of 120 mm, and it is mirrored with the sealing groove of the base (groove three 10); a circle of 12 Φ6 mm through holes is set at 7.5 mm from the edge of the upper cover, and the position is the same as the position of the base through hole 11; two internal threaded through holes with a diameter of 20 mm are opened in the area corresponding to the upper cover and groove two 9 for installing the vacuum check valve and vacuum pressure relief valve.

[0052] (7) According to the size of the battery cell being tested, the sealing ring parameters of the experimental lithium-ion battery are as follows: the sealing ring is made of perfluoroether rubber, Φ3mm thick, 540mm in circumference, and can be completely embedded in the base sealing groove (groove 10) and the upper cover sealing groove.

[0053] (8) The parameters of the vacuum check valve and vacuum pressure relief valve of the experimental lithium-ion battery cover are as follows: the vacuum check valve body is made of pure copper, the lower end is a 4-point (Φ20mm) external thread, the thread length is 4.5mm, and the upper end is connected to a PP30 chrome-plated gas line C-type self-locking quick connector to facilitate the connection operation of the vacuum pump pipeline; the vacuum pressure relief valve is a pure copper metal disc ball valve, which starts to release pressure by rotating counterclockwise and closes clockwise.

[0054] (9) Place the components of the experimental lithium-ion battery described in (4)-(8) above in an ultrasonic cleaning machine, pour in anhydrous ethanol until the components are completely immersed, set the ultrasonic frequency to 50 Hz and the temperature to 30°C, and clean for 2 hours. Then wipe the surface of the component with a non-woven cloth and transfer it to a forced air oven at 85°C for 30 minutes. After baking and cooling, transfer it to a low-humidity environment and wait for installation and use.

[0055] (10) In a low humidity environment, paste 0.5 mm thick OPS expansion tape on the bottom of groove 8, then place the battery cell to be tested prepared in (3) in groove 8 with the positive electrode on the left and the negative electrode on the right, respectively insert the positive electrode ear and the negative electrode ear into the M4 bolts on the internal connection end 12 of the ear, and tighten them with nuts; use a pipette to inject the required volume of the electrolyte to be tested into groove 8, embed the perfluoroether rubber sealing ring into groove 3 10, cover the upper cover so that the sealing ring is embedded in the sealing groove of the upper cover at the same time; use M6 bolts and nuts to pass through the reserved through holes of the base 7 and the upper cover, and tighten them, repeat the above operation to complete the fixing of 12 bolts; at this point, the structural assembly process of the experimental lithium-ion battery is completed, keep the low humidity environment and let it stand for more than 12 hours until the electrolyte completely soaks the battery cell to be tested for use.

[0056] (11) Connect the vacuum check valve of the experimental lithium-ion battery described in (10) to the vacuum pump pipeline, turn on the vacuum pump to evacuate, and discharge the excess gas and electrolyte in the battery. When the relative vacuum reaches -95KPa, turn off the vacuum pump power. Insert the positive and negative copper noses of the blue electric test channel into the positive and negative studs on the outside of the experimental lithium-ion battery test base, and tighten them with M6 nuts; start the test cabinet setting program, and the battery begins to perform pre-formation. After completion, repeat the vacuum operation, disconnect the connecting pipeline, and clean the excess electrolyte at the interface.

[0057] (12) Figure 3 As shown in the figure, the battery was placed in a thermostat at different temperatures (50℃, 30℃, 25℃, 10℃, 0℃, -10℃, -20℃, -30℃, -40℃), and after standing for a period of time, it began to discharge, and the discharge performance data at different temperatures were obtained. After multiple high and low temperature discharges, the battery did not show any abnormalities such as damage or leakage, and had high reliability.

[0058] Embodiment 2:

[0059] In this embodiment, a preparation method for studying a power-type lithium iron phosphate experimental lithium-ion battery is as follows:

[0060] (1) According to the design of the power-type lithium iron phosphate battery material system, the positive electrode uses nano-sized three-dimensional carbon-coated lithium iron phosphate, and the negative electrode uses power-type soft carbon-coated modified artificial graphite. The pulping, coating, rolling and die-cutting processes are completed in sequence to obtain positive and negative electrode sheets with the following dimensions: the positive electrode sheet has a length of 113 mm, a width of 75 mm, and a thickness of 117 μm; the negative electrode sheet has a length of 116 mm, a width of 78 mm, and a thickness of 82 μm.

[0061] (2) According to the design requirements, the positive and negative electrodes described in (1) are stacked with a polypropylene double-sided ceramic coated diaphragm with a width of 122 mm and a thickness of 16 μm, and the positive and negative ears are led out on the opposite sides. After the stacking is completed, the tested battery cell is fixed with green termination tape; the positive and negative ears of the tested battery cell protrude from the diaphragm by a length of 8 mm and a width of 25 mm, and the positive and negative ears of the tested battery cell are respectively wrapped with aluminum tape and nickel tape once and pressed and fixed, and a Φ4 mm hole is made at the center of the protruding part of the positive and negative ears using a puncher; the tested battery cell is transferred to the hot and cold press for pressing, and the parameters are set to 85°C for the upper plate, 65°C for the lower plate, 2MPa for the pressure, and 20 seconds for the pressure holding time; after the pressing is completed, the positive and negative electrodes of the battery cell are tested with a short circuit tester to confirm that there is no short circuit abnormality. At this point, the preparation of the tested battery cell is completed.

[0062] (3) The tested battery cell described in (2) is transferred to a high vacuum (vacuum pressure of 200 Pa) liquid bath oven at 86°C and baked until the water content of the positive electrode sheet is less than 240 ppm; the tested battery cell is cooled to room temperature after baking, and transferred to a low humidity environment for standby use.

[0063] (4) Figure 4 As shown, the battery test base mainly includes a positive electrode test terminal 1, a positive electrode test end rivet bolt 2, a negative electrode test terminal 4, a negative electrode test end rivet bolt 5, and a base 7. The specific structure is as follows:

[0064] A groove is provided in the middle of the rectangular base 7, and base through holes 11 are evenly provided around the top edge of the rectangular base 7. The grooves include groove 1 8, groove 2 9, and groove 3 10. The rectangular groove 1 8 is connected with the rectangular groove 2 9 to form a stepped base total groove. The length of the groove 1 8 is equal to the length of the groove 2 9, and the width and depth of the groove 1 8 are respectively greater than the width and depth of the groove 2 9. A rectangular groove 3 10 is provided on the periphery of the base total groove; a positive test terminal 1 and a negative test terminal 4 are relatively installed on the opposite side of the base 7 perpendicular to the width direction of the groove 1 8, and the positive test terminal 1 and the negative test terminal 4 extend to the groove 1 One end inside 8 is the internal connection end 12 of the pole ear, and a positive test end rivet bolt 2 is provided on the internal connection end 12 of the pole ear of the positive test terminal 1, and a negative test end rivet bolt 5 is provided on the internal connection end 12 of the pole ear of the negative test terminal 4. The positive test terminal 1 and the negative test terminal 4 correspond to the positive pole ear and the negative pole ear of the tested battery cell respectively through the internal connection end 12 of the pole ear, and the positive test end rivet bolt 2 and the negative test end rivet bolt 5 are respectively connected to the central openings of the positive pole ear and the negative pole ear, and the positive test terminal 1 and the negative test terminal 4 extend to the ends outside the groove 8 to respectively open a positive test end through hole 3 and a negative test end through hole 6.

[0065] The size parameters of the battery test base of the experimental lithium-ion battery are as follows: the total length of the base is 170mm, the total width is 150mm, and the total thickness is 10mm; a rectangular groove (groove-8) is made at 20mm from the edge on the left side, with a length of 130mm, a width of 80mm, and a depth of 4mm. An OPS expansion tape with the same length and width and a thickness of 0.25mm is pasted at the bottom of the groove-1; another rectangular groove (groove-8) with a length of 130mm, a width of 30mm, and a depth of 2mm is made at the adjacent position on the right side of the groove. Groove two 9); Groove one and groove two are connected to form a stepped base total groove, the outer dimensions of the base total groove are: length 130mm, width 110mm, and a rectangular cross-section semicircular sealing groove (groove three 10) is made on the outermost side of the base total groove, the groove width is 3mm, the groove length is 150mm, the groove width is 130mm, and the R3mm chamfer is made at the right angle; a circle of Φ6mm through holes is made at a distance of 6mm from the edge of the base, 4 holes are set on one side in the length direction, and 2 holes are set on one side in the width direction, with a total of 12 holes in one circle.

[0066] (5) According to the size of the battery cell to be tested, the size parameters of the connecting piece of the battery test base of the experimental lithium-ion battery are as follows: the size of the protruding part of the internal connection terminal 12 of the pole ear of the base 7 is: length 5mm, width 25mm, the protruding part of the positive electrode is an aluminum sheet with a thickness of 3mm, and the negative electrode is a copper-plated nickel sheet with a thickness of 3mm. The center position of the protruding part is riveted and fixed with an M4 bolt with a thread length of 4mm. The material of the rivet bolt at the positive electrode test end is aluminum, and the material of the rivet bolt at the negative electrode test end is copper.

[0067] (6) According to the size of the battery cell being tested, the size parameters of the upper cover of the experimental lithium-ion battery are as follows: the total length of the upper cover is 170 mm, the total width is 150 mm, and the total thickness is 10 mm; a rectangular sealing groove is made 10 mm away from the edge of the upper cover, with a groove width of 3 mm, a groove length of 130 mm, and a groove width of 110 mm, and it is mirrored with the sealing groove of the base (groove three 10); a circle of 12 Φ6 mm through holes is set 6 mm away from the edge of the upper cover, and the position is the same as the position of the base through hole 11; two internal threaded through holes with a diameter of 20 mm are opened in the corresponding area of ​​the upper cover and groove two for installing the vacuum check valve and vacuum pressure relief valve.

[0068] (7) According to the size of the battery cell being tested, the sealing ring parameters of the experimental lithium-ion battery are as follows: the sealing ring is made of perfluoroether rubber, Φ3mm thick, 480mm in circumference, and can be completely embedded in the base sealing groove (groove 10) and the upper cover sealing groove.

[0069] (8) The parameters of the vacuum check valve and vacuum pressure relief valve of the experimental lithium-ion battery cover are as follows: the body of the vacuum check valve is made of pure copper, the lower end is a 4-point (Φ20mm) external thread, the thread length is 4.5mm, and the upper end is connected to a PP30 chrome-plated gas line C-type self-locking quick connector to facilitate the connection operation of the vacuum pump pipeline; the vacuum pressure relief valve is a pure copper metal disc ball valve, which starts to release pressure by rotating counterclockwise and closes clockwise.

[0070] (9) Place the components of the experimental lithium-ion battery described in (4)-(8) above in an ultrasonic cleaning machine, pour in anhydrous ethanol until the components are completely immersed, set the ultrasonic frequency to 50 Hz and the temperature to 30°C, and clean for 2 hours. Then wipe the surface of the component with a non-woven cloth and transfer it to a forced air oven at 85°C for 30 minutes. After baking and cooling, transfer it to a low-humidity environment and wait for installation and use.

[0071] (10) In a low humidity environment, paste 0.25 mm thick OPS expansion tape on the bottom of groove 8, then place the battery cell to be tested prepared in (3) in groove 8 with the positive electrode on the left and the negative electrode on the right, respectively insert the positive electrode ear and the negative electrode ear into the M4 bolts on the internal connection end 12 of the ear, and tighten them with nuts; use a pipette to inject the required volume of the electrolyte to be tested into groove 8, embed the perfluoroether rubber sealing ring into groove 3 10, cover the upper cover so that the sealing ring is embedded in the sealing groove of the upper cover at the same time; use M6 bolts and nuts to pass through the reserved through holes of the base 7 and the upper cover, and tighten them, repeat the above operation to complete the fixing of 12 bolts; at this point, the structural assembly process of the experimental lithium-ion battery is completed, keep the low humidity environment and let it stand for more than 12 hours until the electrolyte completely soaks the battery cell to be tested for use.

[0072] (11) Connect the vacuum check valve of the experimental lithium-ion battery described in (10) to the vacuum pump pipeline, turn on the vacuum pump to evacuate, and discharge the excess gas and electrolyte in the battery. When the relative vacuum reaches -95KPa, turn off the vacuum pump power. Insert the positive and negative copper noses of the blue electric test channel into the positive and negative studs on the outside of the experimental lithium-ion battery test base, and tighten them with M6 nuts; start the test cabinet setting program, and the battery begins to perform pre-formation. After completion, repeat the vacuum operation, disconnect the connecting pipeline, and clean the excess electrolyte at the interface.

[0073] (12) Figure 5 As shown in the figure, according to the test requirements, the experimental lithium-ion battery completed the discharge test at different rates (1C, 2C, 3C, 4C, 5C, 6C, 7C, 8C, 9C) at room temperature, and obtained the 1C to 9C discharge curve of the power-type design lithium iron phosphate experimental lithium-ion battery at room temperature. After multiple charge and discharge, the battery did not show abnormal phenomena such as melting, swelling, deformation, etc., and was strong and durable.

[0074] The implementation results show that the present invention makes the preparation and testing of experimental lithium-ion batteries faster and more convenient by designing the packaging shell structure of the tested battery cell without affecting the electrochemical reaction and performance of the lithium-ion battery. After the test is completed, the battery can be quickly disassembled, and the components can be reused after cleaning and drying. It is green, environmentally friendly, strong and durable. The present invention can meet the design verification of different electrode loads and different electrode sizes, and meet the functional verification of different components, different lithium salt types and concentrations of electrolytes, and has a wide range of applications.

Claims

1. A method for rapidly and repeatedly verifying the material system and process performance of a lithium-ion battery, characterized in that: The packaging body of the experimental lithium-ion battery consists of a battery test base, a sealing ring, an upper cover, a tested battery cell and fastening bolts. The battery test base, the sealing ring and the upper cover are injection molded with electrolyte-resistant materials. The tight connection between the three and the use of threaded connection or elastic bonding between the components form a closed space isolated from the outside world, providing a good electrochemical reaction environment. The upper cover plate and the battery test base are arranged opposite to each other in upper and lower parts. A groove one is opened on the left side of the battery test base for placing the battery cell under test. A groove two is opened close to the right side of the groove one for storage during battery formation and transition buffering during exhaust operation. A groove three is opened on the top of the battery test base and on the outer sides of the groove one and the groove two. A sealing groove corresponding to the groove three is opened on the bottom of the upper cover plate. The sealing ring is embedded in the groove three and the sealing groove and fits well.

2. The method for rapidly and repeatedly verifying the material system and process performance of a lithium-ion battery according to claim 1, characterized in that: Two internal threaded through holes are opened in the middle of the upper cover plate and the corresponding position of the groove 2, and a pure copper vacuum check valve and a vacuum pressure relief valve are installed respectively, which are used for vacuum exhaust of the battery after the battery is assembled and for vacuum relief operation when the battery is disassembled after the test is completed.

3. The method for rapidly and repeatedly verifying the material system and process performance of a lithium-ion battery according to claim 1, characterized in that: The outer sides of the battery test base and the upper cover are square, and the length and width of the outer sides of the battery test base and the upper cover are the same. Through holes are made at the edges of the battery test base and the upper cover, and are evenly distributed along a circle of the battery test base and the upper cover. Bolts are inserted into the through holes and tightened with nuts to achieve the connection between the base and the upper cover. A regular hexagonal groove is opened at the hole opening position on the bottom surface of the battery test base, and the nuts used are embedded in the groove and fixed with glue. The bolts are inserted into the through holes and tightened to make the battery test base fit with the upper cover. The bolts cooperate with the sealing ring to achieve isolation between the tested battery cell and the external environment.

4. The method for rapidly and repeatedly verifying the material system and process performance of a lithium-ion battery according to claim 1, characterized in that: The battery test base is provided with an aluminum positive test terminal and a copper negative test terminal. A vertical bolt structure is provided on the inner side of the groove where the positive test terminal and the negative test terminal are placed in the battery test base for placing the tested battery cell. The outside of the groove where the positive test terminal and the negative test terminal are placed in the battery test base for placing the tested battery cell is selected from sheet, line, stud, and metal table according to the test channel; the positive and negative ears of the tested battery cell are punched in advance, and the bolts on the positive and negative test terminals are respectively inserted during assembly, and are pressed with metal blocks of corresponding materials, and then tightened with nuts. The battery test base and the upper cover are tightened with bolts and nuts.

5. The method for rapidly and repeatedly verifying the material system and process performance of a lithium-ion battery according to any one of claims 1 to 4, characterized in that: The battery test base includes a positive test terminal, a positive test end rivet bolt, a negative test terminal, a negative test end rivet bolt, and a base. The specific structure is as follows: A groove is provided in the middle of the rectangular base, and base through holes are evenly provided around the top edge of the rectangular base. The grooves include groove one, groove two, and groove three. The rectangular groove one is connected to the rectangular groove two to form a stepped base total groove. The length of the groove one is equal to the length of the groove two, and the width and depth of the groove one are respectively greater than the width and depth of the groove two. A rectangular groove three is provided on the periphery of the base total groove; the ends of the positive test terminal and the negative test terminal extending into the groove one are the internal connection ends of the pole ears, and the positive test terminal A positive test terminal rivet bolt is provided on the internal connection end of the tab of the sub-electrode, and a negative test terminal rivet bolt is provided on the internal connection end of the tab of the negative test terminal. The positive test terminal and the negative test terminal correspond to the positive tab and the negative tab of the tested battery cell respectively through the internal connection end of the tab. The positive test end rivet bolt and the negative test end rivet bolt are respectively connected to the central openings of the positive tab and the negative tab. The positive test terminal and the negative test terminal are extended to the ends outside the groove to respectively open a positive test terminal through hole and a negative test terminal through hole.

6. The method for rapidly and repeatedly verifying the material system and process performance of a lithium-ion battery according to claim 5, characterized in that: The positive test terminal and the negative test terminal are installed relatively and parallelly on the same side of the base perpendicular to the width direction of the groove, or the positive test terminal and the negative test terminal are installed relatively and parallelly on the opposite side of the base perpendicular to the width direction of the groove.

7. The method for rapidly and repeatedly verifying the material system and process performance of a lithium-ion battery according to claim 5, characterized in that: Groove three is a sealing groove with a semicircular rectangular cross-section opened at the outermost side of the total groove of the base, and a sealing groove with a semicircular rectangular cross-section corresponding to groove three is opened at the bottom of the upper cover plate, so that the sealing ring is embedded in groove three and the sealing groove and fits tightly.

8. The method for rapidly and repeatedly verifying the material system and process performance of a lithium-ion battery according to claim 1, characterized in that: The battery cell under test is square in design. It consists of a positive electrode sheet, a negative electrode sheet and a separator, and is composed of a stacked or wound type. The positive electrode system is one or more of lithium iron phosphate, lithium iron manganese phosphate, lithium nickel cobalt manganese oxide, lithium manganese oxide, and metallic lithium. The negative electrode system is one or more of graphite, modified coated graphite, hard carbon, soft carbon, mesophase carbon microspheres, and lithium metal. The separator material is one of polyethylene and polypropylene, or a composite of both.

9. The method for rapidly and repeatedly verifying the material system and process performance of a lithium-ion battery according to claim 1, characterized in that: The battery test base, upper cover and sealing ring required for the packaging body of the experimental lithium-ion battery are all made of electrolyte-resistant materials. The battery test base and upper cover are made of resin polymer materials that are resistant to electrolytes and do not participate in electrochemical reactions, including one or more of polyvinyl chloride, polytetrafluoroethylene, polypropylene and polyethylene; an annular sealing ring is used between the battery test base and the upper cover, and the material of the sealing ring includes one or more of EPDM rubber, perfluoroether rubber and silicone.

10. The method for rapidly and repeatedly verifying the material system and process performance of a lithium-ion battery according to claim 1, characterized in that: The method is to open circular holes at the top of the positive and negative ears of the tested battery cell in a low humidity environment with an ambient dew point temperature less than -45°C, and place the tested battery cell in a rectangular slotted space of a battery test base; insert the positive ear of the tested battery cell into the positive test end rivet bolt on the positive test terminal, and then use a nut made of aluminum or aluminum alloy to lock and connect it with the positive test terminal on the battery test base; in the same way, insert the negative ear of the tested battery cell into the negative test end rivet bolt on the negative test terminal, and then use a nut made of copper or copper-plated nickel to connect it with the negative test terminal on the battery test base; inject the required electrolyte into the groove of the battery test base where the tested battery cell is located, and then put a sealing ring in the sealing groove at the top of the base, cover the upper cover, and align the upper cover with the edge of the battery test base; Use bolts and nuts to penetrate the through holes of the upper cover and the base, and tighten the bolts to ensure that the upper cover and the battery test base are well sealed; close the vacuum relief valve on the upper cover, and let it stand for 6 to 24 hours to ensure that the electrolyte fully infiltrates the tested battery cell; transfer the package body of the experimental lithium-ion battery to a normal atmosphere, connect the vacuum check valve on the upper cover and the vacuum pump, turn on the vacuum pump to evacuate the battery until the relative vacuum degree is below -95KPa, and disconnect the pipeline; at this point, the preparation of the experimental lithium-ion battery package body is completed, and the battery test and test data are sorted. After the battery test is completed, the tested battery cell and the battery test base are disassembled non-destructively, and the battery test base is reused after cleaning and drying.