Glue uniformizing method
By using the glue uniform method in semiconductor manufacturing, the backing film is pasted and the photoresist is spin-coated, the problem of photoresist edge accumulation is solved, the accuracy and yield of the wafer chip are improved, and the wafer area is fully utilized. Reduced production costs.
Patent Information
- Application Number
- CN202411150401.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-21
- Publication Date
- 2024-11-08
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
During semiconductor manufacturing, photoresist is prone to build up at the edge of the wafer, resulting in reduced production accuracy and irregular graphics, while traditional edge de-edge processes lead to reduced available wafer area and cost loss.
Using the glue uniform method, paste the back adhesive film to the back of the wafer, spin-coat the photoresist to the front, and remove the back adhesive film by exposure to solve the problem of edge glue stacking and avoid defects in the edge removal process.
Improve the production accuracy and yield of chips on the wafer, make full use of the wafer area, reduce production costs, and avoid the area reduction and cost loss caused by the edge removal process.
Smart Images

Figure CN118915393A_ABST
Abstract
Description
Technical Field
[0001] The present application belongs to the technical field of semiconductor manufacturing, and specifically relates to a method for coating. Background Art
[0002] In the field of semiconductor manufacturing, the photolithography process is undoubtedly the core link, which directly determines the manufacturing accuracy of the graphic size of each functional area on the chip. At the same time, the quality of the photolithography process will also have a direct impact on the yield and output of the chip on the wafer. During the photolithography process, photoresist is coated on the surface of the wafer. However, the photoresist near the edge of the wafer is often prone to glue accumulation on the front and back of the wafer. This edge glue accumulation problem will cause the edge of the wafer to reduce the manufacturing accuracy during exposure, and defects such as irregular graphics or glue layer detachment will appear after development.
[0003] In the current photolithography process, in order to eliminate defects caused by edge photoresist, a de-edging process is usually used to remove the photoresist accumulated on the edge of the wafer. However, this process will make several millimeters or even larger areas of the wafer edge unusable, thereby reducing the output of chips on a single wafer and causing certain cost losses. Summary of the invention
[0004] Therefore, the technical problem to be solved by the present application is to provide a method for uniform coating, aiming to overcome the adverse effects of the wafer edge coating problem in the existing photolithography process, while avoiding the reduction in wafer available area and cost loss caused by the traditional edge removal process.
[0005] In order to solve the above problems, the present application provides a method for coating, comprising:
[0006] Paste the adhesive film to the back of the wafer;
[0007] Spin-coat photoresist onto the front side of the wafer;
[0008] Remove the adhesive backing.
[0009] Optionally, remove the adhesive backing film, including:
[0010] Expose the adhesive film.
[0011] Optionally, the thickness of the wafer is 300um to 800um.
[0012] Optionally, the thickness of the adhesive film is 50um to 100um.
[0013] Optionally, the axis lines of the wafer and the backing film coincide with each other.
[0014] Optionally, the diameter of the wafer is A, 50mm≤A≤150mm, and the diameter of the backing film is B, 5mm≤BA≤15mm.
[0015] Optionally, the adhesive backing film is composed of a polymer substrate, a photosensitive resin, a photoinitiator and additives.
[0016] Optionally, the rotation speed during spin coating of the photoresist is 1000RPM to 6000RPM.
[0017] Optionally, the light intensity of the adhesive film exposure is greater than 20mW / cm 2 .
[0018] Optionally, the total exposure energy required for debonding the adhesive backing film is greater than 1000mJ / cm 2 .
[0019] Beneficial Effects
[0020] The coating method provided in the embodiment of the present invention first adheres the adhesive backing film to the back side of the wafer, then spin-coats the photoresist to the front side of the wafer, and finally removes the adhesive backing film. This effectively solves the problem of adhesive accumulation at the edge of the photoresist without using an edge removal process, improves the manufacturing accuracy and yield of the chip on the wafer, and at the same time fully utilizes the area of the wafer to reduce production costs. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 A flow chart of a method for coating a film according to an optional embodiment of the present application;
[0022] Figure 2 A flow chart of a method for coating abrasives according to another optional embodiment of the present application;
[0023] Figure 3 This is a schematic diagram of the structure of the wafer of this application being pasted with a backing film during the adhesive bonding process.
[0024] The reference numerals are as follows:
[0025] 1. Wafer; 2. Adhesive film. DETAILED DESCRIPTION
[0026] In the description of the present application, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present invention.
[0027] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.
[0028] In this application, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be an indirect connection through an intermediate medium, or it can be the internal communication of two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0029] The preferred embodiments of the present invention are described below in conjunction with the accompanying drawings. It should be understood that the preferred embodiments described herein are only used to illustrate and explain the present invention, and are not used to limit the present invention.
[0030] See also Figure 1 and Figure 3 As shown, according to an embodiment of the present application, a method for coating is provided. First, a backing film 2 is pasted to the back of a wafer 1, then, a photoresist is spin-coated to the front of the wafer 1, and finally, the backing film 2 is removed. This method effectively solves the problem of photoresist edge coating without using an edge removal process, improves the manufacturing accuracy and yield of the chip on the wafer 1, and at the same time makes full use of the area of the wafer 1 to reduce production costs. This coating method provides an innovative solution for the photolithography process in the field of semiconductor manufacturing, and has broad application prospects.
[0031] Please follow the steps below to implement:
[0032] Step S1: Paste the adhesive film 2 to the back side of the wafer 1 .
[0033] The wafer 1 may be a thin circular substrate made of semiconductor materials such as silicon, with a specific thickness range, such as 300um to 800um. The wafer 1 is the core material for semiconductor chip manufacturing, and its surface needs to be processed by high-precision photolithography and other processes to produce various circuit patterns.
[0034] Specifically, in this embodiment, the coating method is applicable to a wafer 1 with a thickness of 300um to 800um.
[0035] The adhesive film 2 may be composed of a polymer substrate, a photosensitive resin, a photoinitiator, and additives, etc. Its thickness is generally 50um to 100um, and it has specific physical and chemical properties, and can be tightly combined with the wafer 1 under specific conditions, and can be controllably removed by exposure or other methods in subsequent processes.
[0036] It is understandable that the polymer substrate can be polyethylene, polypropylene, polyester, etc., which provide basic physical support and flexibility for the film; the photosensitive resin can be acrylic resin, epoxy resin, etc., to achieve the exposure removal function; the photoinitiator triggers a photochemical reaction when exposed to ultraviolet light of a specific wavelength, causing the resin to cross-link or decompose, thereby changing the viscosity or solubility of the film; additives may include plasticizers to increase the flexibility of the film, antioxidants to prevent film aging, leveling agents to improve the surface flatness of the film, etc.
[0037] Specifically, in this embodiment, the adhesive film 2 is a purple UV film.
[0038] It is understandable that when pasting the adhesive film 2 to the back of the wafer 1, first, ensure that the back of the wafer 1 is clean, dry, and free of dust, oil and other impurities to ensure that the adhesive film 2 can be well pasted. At the same time, check the quality and integrity of the adhesive film 2 to ensure that it is not damaged or contaminated. Then, mechanical pasting or manual pasting can be used. In mechanical pasting, automated equipment is usually used to accurately paste the adhesive film 2 to the back of the wafer 1 through precise positioning and pressure control. Manual pasting requires the operator to have high skills and experience to ensure that the position of the adhesive film 2 is accurate, flat and free of bubbles.
[0039] It should be noted that during the pasting process, it is necessary to ensure that the axis of the wafer 1 and the adhesive film 2 coincide. This can be achieved through a precise positioning device or a visual system to ensure the accuracy and stability of the subsequent process. At the same time, the diameter of the wafer 1 is A, 50mm≤A≤150mm, and the diameter of the adhesive film 2 is B, which must meet 5mm≤BA≤15mm. This size design can ensure that the adhesive film 2 effectively supports the wafer 1 without causing too much interference in the subsequent process.
[0040] In addition, in the present application, the adhesive film 2 is pasted to the back of the wafer 1, which not only solves the problem of photoresist edge accumulation, but also provides a more stable base for the spin coating of the photoresist on the front of the wafer 1, ensuring that the photoresist is not broken and the photoresist is evenly coated. At the same time, due to the supporting effect of the adhesive film 2, the wafer 1 is not easily deformed or vibrated during the spin coating process, so that a more uniform photoresist coating can be obtained.
[0041] Step S2: Spin-coat photoresist onto the front side of the wafer 1 .
[0042] The photoresist may be a light-sensitive chemical material composed of resin, photosensitizer, solvent, etc.
[0043] Specifically, by spin coating the photoresist onto the front side of the wafer 1, a uniform photoresist film with a specific thickness and good performance can be formed on the front side of the wafer 1, preparing for the subsequent photolithography process so as to accurately transfer the circuit pattern onto the wafer 1. Different types of photoresists have different characteristics and are suitable for different photolithography process requirements.
[0044] Among them, when spin coating the photoresist to the front of the wafer 1, the wafer 1 can be first fixed on the chuck of the spin coating equipment to ensure that the wafer 1 is stable and horizontal, and then a dropper or nozzle is used to drop an appropriate amount of photoresist on the center of the wafer 1, and then the spin coating equipment is started to make the wafer 1 start to rotate at a specific speed. During the rotation process, the centrifugal force spreads the photoresist evenly on the front of the wafer 1, and finally the spin coating time and the rotation speed are controlled to achieve the desired photoresist thickness and uniformity. Generally, a higher rotation speed can obtain a thinner glue layer, and a longer spin coating time can improve the uniformity of the glue layer.
[0045] It should be noted that the rotation speed directly affects the thickness and uniformity of the photoresist. A lower rotation speed may cause the glue layer to be too thick and uneven, while a too high rotation speed may make the glue layer too thin, or even cause no glue in some areas. It is necessary to select a suitable rotation speed range according to the size of the wafer 1, the photoresist characteristics and the process requirements. In this embodiment, the rotation speed is 1000RPM to 6000RPM, which can effectively control the thickness of the glue layer and ensure that the photoresist thickness on the entire surface of the wafer 1 is consistent, thereby improving the accuracy of the subsequent photolithography process.
[0046] Specifically, in the present application, since a larger backing film 2 is pasted on the back of the wafer 1, after the photoresist is rotated and evenly spread on the front of the wafer 1, the deposited area is the area outside the positive projection of the wafer 1 on the backing film 2, thereby solving the problem of deposited glue on the edge of the wafer 1 during uniform glue application. It can be achieved that the pattern on the edge of the wafer 1 is consistent with the middle and intact without affecting the photolithography process, and the area of the wafer 1 is utilized to the maximum extent to produce chips, thereby improving the chip output on a single wafer 1; at the same time, it can solve the problem of defects in the photolithography pattern produced on the edge of the wafer 1.
[0047] Step S3: removing the adhesive film 2.
[0048] As mentioned above, in the photolithography process, the presence of the adhesive film 2 can avoid the problem of adhesive accumulation at the edge of the wafer 1, thereby improving the effective area utilization of the wafer 1. When the adhesive film 2 is removed, the area at the edge of the wafer 1 can be fully used for chip production, further improving the overall utilization of the wafer 1.
[0049] Specifically, the adhesive film 2 can be removed by mechanical peeling, chemical solvent treatment, exposure, etc.
[0050] See also Figure 2 As shown, in some specific examples, the above step S3, removing the adhesive film 2, includes:
[0051] Step S301: exposing the adhesive film 2.
[0052] Among them, in the semiconductor manufacturing process, the main purpose of exposing the backing film 2 is to achieve controllable dissolution of the backing film 2, so that the backing film 2 can be smoothly removed from the wafer 1 at a specific time without affecting the photoresist and the formed circuit pattern on the wafer 1.
[0053] When the adhesive film 2 is a light-sensitive material, such as a UV film, it can be exposed using an ultraviolet lamp, laser, etc. with a specific wavelength and intensity. For example, the light intensity of the adhesive film 2 is greater than 20 mW / cm 2 , and the total exposure energy required for debonding the adhesive film 2 is greater than 1000mJ / cm 2 The exposure process can cause the light-sensitive resin in the adhesive film 2 to undergo a chemical reaction, changing its physical properties and making it easier to remove.
[0054] Specifically, when exposing the adhesive film 2, first place the wafer 1 with the adhesive film 2 on the workbench of the exposure equipment, ensure that the position and angle of the wafer 1 and the light source are correct, then start the exposure equipment, and the light emitted by the light source is irradiated onto the adhesive film 2 through the optical system. During the exposure process, it is necessary to ensure uniform illumination to avoid local underexposure or overexposure, and finally control the duration of the exposure process according to the preset exposure time and total exposure energy. The exposure time can be adjusted according to the actual situation to ensure that the adhesive film 2 can fully absorb enough energy and undergo a debonding reaction.
[0055] The following is an example of the values of various parameters in the glue spreading method:
[0056] For example: a wafer 1 with a thickness of 500um is selected. This thickness is within the range of 300um to 800um, which is suitable for this coating method. In actual production, wafers 1 of different thicknesses can be selected according to different chip manufacturing requirements and process requirements. For example, for some high-performance chips, a thinner wafer 1 may be required to improve heat dissipation performance and integration; while for some applications with higher requirements for mechanical strength, a thicker wafer 1 may be required.
[0057] For example, a backing film 2 is used, and its thickness is 80um. This thickness is within the range of 50um to 100um, which meets the requirements of this coating method. Backing films 2 of different thicknesses may have different effects on the support effect of the wafer 1 and the coating of the photoresist. A thinner backing film 2 may be more suitable for chip manufacturing processes with strict thickness requirements, while a thicker backing film 2 may provide better support and stability.
[0058] For example: Assume that the diameter of wafer 1 is 100mm (A=100mm), and select a backing film 2 with a diameter of 110mm (B=110mm). At this time, BA=10mm, which meets the size requirement of 5mm≤BA≤15mm. In practical applications, the backing film 2 with a suitable diameter can be selected according to the size and process requirements of wafer 1. For example, if the size of wafer 1 is small, a backing film 2 with a smaller diameter difference can be selected to reduce material waste and process complexity.
[0059] For example, when spin coating photoresist, set the rotation speed to 3000RPM. This rotation speed is within the range of 1000RPM to 6000RPM. Different rotation speeds will affect the thickness and uniformity of the photoresist. For a specific photoresist and wafer 1 combination, the best spin coating speed can be determined by experiment. For example, for a photoresist with a higher viscosity, a lower rotation speed may be required to avoid a thin or uneven layer; for a photoresist with better fluidity, a higher rotation speed may be used to obtain a thinner layer.
[0060] For example, when exposing the adhesive film 2, a light source with a light intensity of 25 mW / cm 2 , total exposure energy is 1200mJ / cm 2 These parameters meet the requirement that the light intensity is greater than 20mW / cm 2 and total exposure energy greater than 1000mJ / cm 2 Different materials of the adhesive film 2 may require different exposure parameters to achieve the best debonding effect. In practical applications, the light intensity and exposure time can be adjusted through experiments to ensure that the adhesive film 2 can be fully debonded without damaging the photoresist and circuit pattern on the wafer 1.
[0061] It should be noted that total exposure energy = light intensity × exposure time. It is known that the total exposure energy is required to be greater than 1000mJ / cm 2 , here we assume that we need to achieve a total exposure energy of 1200mJ / cm 2 , light intensity is 25mW / cm 2 The formula is: exposure time = total exposure energy / light intensity = 1200mJ / cm 2 ÷25mW / cm 2= 48 seconds. If the light intensity is increased to 30mW / cm 2 , keep the total exposure energy at 1200mJ / cm 2 If the exposure time is 1200 mJ / cm 2 ÷30mW / cm 2 = 40 seconds. Conversely, if the light intensity is reduced, the exposure time needs to be extended accordingly to achieve the same total exposure energy.
[0062] The coating method provided in the embodiment of the present application first adheres the adhesive film 2 to the back of the wafer 1, then spin-coats the photoresist to the front of the wafer 1, and finally removes the adhesive film 2. This effectively solves the problem of photoresist edge buildup without using an edge removal process, improves the manufacturing accuracy and yield of the chip on the wafer 1, and at the same time fully utilizes the area of the wafer 1 to reduce production costs.
[0063] It is easy for those skilled in the art to understand that, under the premise of no conflict, the above-mentioned advantageous methods can be freely combined and superimposed.
[0064] The above are only preferred embodiments of the present application and are not intended to limit the present application. Any modifications, equivalent replacements and improvements made within the spirit and principles of the present application shall be included in the protection scope of the present application. The above are only preferred implementations of the present application. It should be pointed out that for ordinary technicians in this technical field, several improvements and variations can be made without departing from the technical principles of the present application, and these improvements and variations should also be regarded as the protection scope of the present application.
Claims
1. A method for coating, It is characterized in that include: Pasting a backing film (2) to the back side of the wafer (1); Spin coating photoresist onto the front side of the wafer (1); Remove the adhesive backing (2).
2. The method for coating according to claim 1, It is characterized in that Remove the adhesive film (2), including: Expose the adhesive film (2).
3. The method for coating according to claim 1, It is characterized in that The thickness of the wafer (1) is 300um to 800um.
4. The method for coating according to claim 1, It is characterized in that The thickness of the back adhesive film (2) is 50um to 100um.
5. The method for coating according to claim 1, It is characterized in that The axis lines of the wafer (1) and the backing film (2) coincide with each other.
6. The method for coating according to claim 1, It is characterized in that The diameter of the wafer (1) is A, 50mm≤A≤150mm, and the diameter of the backing film (2) is B, 5mm≤BA≤15mm.
7. The method for coating according to claim 1, It is characterized in that The back adhesive film (2) is composed of a polymer substrate, a photosensitive resin, a photoinitiator and additives.
8. The method for coating according to claim 1, It is characterized in that The rotation speed during spin coating of the photoresist is 1000RPM to 6000RPM.
9. The method for coating according to claim 2, It is characterized in that The light intensity of the adhesive film (2) exposed is greater than 20mW / cm 2 .
10. The method for coating according to claim 2, It is characterized in that The total exposure energy required for debonding the adhesive backing film (2) is greater than 1000 mJ / cm 2 .
Citation Information
Patent Citations
Reinforcing treatment method of thinned wafer in glue uniformizing process
CN116149142A
Preparation method for reducing wafer exposure standing wave effect
CN117148681A
Polymer back film layer for alleviating substrate warpage
CN119301737A
UV lamp exposure dispergator
CN213340296U
Method for coating photo-resist of semiconductor device
KR1020050115678A