Preparation method of high-performance lead type supercapacitor

By setting the inlet hole and connection hole in the lead-type supercapacitor, and cutting off the welded section after aging, releasing impurity gas, and fixing the battery cell with the shell positioning groove, the problem of reducing sealing caused by electrolyte exudation and vibration is solved. It improves the sealing and vibration resistance of the capacitor and extends the service life.

CN118919314AActive Publication Date: 2024-11-08FUJIAN TORCH ELECTRON TECH CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411281891.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-13
Publication Date
2024-11-08
Estimated Expiration
2044-09-13

AI Technical Summary

Technical Problem

The existing lead-type supercapacitors have sealing problems during assembly and use. The electrolyte is prone to seep out and the battery cell is prone to shake under vibration conditions, resulting in a decrease in sealing and shortening service life.

Method used

Set a liquid inlet hole in the lead wire, and set a connection hole at the connection between the connecting tongue and the connecting column. A seal is formed by high-temperature welding to prevent the electrolyte from oozing out. After aging, the welding section is cut off to release impurity gas and reduce the internal air pressure , in conjunction with a positioning groove on the outer periphery of the housing, the battery cell is fixed to improve vibration resistance.

Benefits of technology

Improves the sealing properties of the capacitor, extends the service life, reduces internal resistance and improves the vibration resistance of the supercapacitor.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118919314A_ABST
    Figure CN118919314A_ABST
Patent Text Reader

Abstract

According to the preparation method of the high-performance lead-type supercapacitor, the supercapacitor comprises a shell, a battery cell arranged in the shell, two leads connected with the battery cell respectively, and a sealing rubber plug arranged in the shell and used for sealing the battery cell, the lead comprises a connecting tongue connected with the battery cell, a connecting column connected with the connecting tongue and located above the battery cell, a lead column connected with the upper end of the connecting column and extending upwards out of the shell, and a liquid inlet hole extending downwards into the connecting column from the upper end of the lead column, and a plurality of connecting holes communicated with the liquid inlet hole are formed in the joint of the connecting tongue and the connecting column; through a mechanism for limiting the lead, the liquid inlet hole is formed in the lead, the connecting hole connected with the liquid inlet hole is formed in the connecting position of the connecting tongue and the connecting column, and liquid injection is performed after the capacitor is assembled, so that electrolyte is prevented from seeping into a gap between the sealing rubber plug and the inner wall of the shell from the interior of the shell in the assembling process, and the assembling quality of the capacitor is improved. And the sealing performance of the capacitor is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of supercapacitor preparation, and in particular relates to a method for preparing a high-performance lead-type supercapacitor. Background Art

[0002] As an emerging advanced energy storage device, supercapacitors have both the high power characteristics of traditional capacitors and the high energy characteristics of batteries. Due to its unique high specific power, large current discharge capability, ultra-low temperature characteristics, high reliability and green environmental protection, it has been widely used and developed in many fields such as electricity, transportation, communications, energy, aviation, etc.

[0003] In the existing lead-type supercapacitors, the cell diameter is usually set smaller than the inner diameter of the shell during assembly. This is to increase the empty space inside the shell to reduce the internal air pressure of the capacitor and improve the performance of the capacitor. However, the premise of more free space is to increase the gap between the cell and the shell. Due to the small size of the lead-type supercapacitor, it is not suitable to perform vibration-resistant waisting on the shell at the cell position. Therefore, the cell is usually in a suspended state inside the shell. When the capacitor is used under conditions of long-term vibration, the stress of the cell shaking is transferred from the guide pin to the contact position between the sealing rubber plug and the guide pin aluminum stem. Long-term vibration reduces the sealing of this position, resulting in capacitor leakage.

[0004] At the same time, the existing lead-type supercapacitors are assembled and packaged with the battery cell, sealing rubber plug, and shell after injecting or soaking the electrolyte. This process will cause the electrolyte to be squeezed and seep out to the contact point between the side of the sealing rubber plug and the inner wall of the shell and the R corner of the seal. The electrolyte attached to the gap between the sealing rubber plug and the shell due to capillary action cannot be cleaned by one cleaning. In the subsequent use process, the electrolyte will still slowly seep out, affecting the appearance of the capacitor and posing a risk of reduced sealing. Summary of the invention

[0005] The purpose of the present invention is to overcome the shortcomings of the prior art and provide a method for preparing a high-performance lead-type supercapacitor.

[0006] The present invention adopts the following technical solution:

[0007] A method for preparing a high-performance lead-type supercapacitor, the supercapacitor comprising a shell, a battery cell arranged in the shell, two leads respectively connected to the battery cells, and a sealing rubber plug arranged in the shell for sealing the battery cell, the lead comprising a connecting tongue connected to the battery cell, a connecting column connected to the connecting tongue and located above the battery cell, a lead column connected to the upper end of the connecting column and extending upward to the outside of the shell, and a liquid inlet hole extending downward from the upper end of the lead column to the connecting column, and a plurality of connecting holes connected to the liquid inlet holes are formed at the connection between the connecting tongue and the connecting column;

[0008] The preparation method specifically comprises the following steps:

[0009] Step 1, lead forming;

[0010] Step 2, capacitor molding: the battery cell is dried, and then assembled with the sealing rubber plug and the outer shell through the rubber, the electrolyte is injected from the liquid inlet hole, flows into the battery cell through the connection hole, and then the upper end of the lead column is subjected to high temperature to weld the upper end of the lead column to form a seal;

[0011] Step 3, charge and age the capacitor, then cut off the welded section at the upper end of the lead column to release the impurity gas generated inside the capacitor due to the first high-temperature aging, and then apply high temperature to the root position of the lead column near the connecting column to weld the root position to form a seal, so as to obtain the supercapacitor.

[0012] Furthermore, in step 2, the high temperature applied for welding the upper end of the lead column is 250-270° C. and the time is 3-5 seconds.

[0013] Furthermore, in step 1, the specific operation of lead forming is as follows: splice the connecting column and the lead column, then insert the metal fixing column into the liquid inlet hole, braze the connection between the connecting column and the lead column, take out the metal fixing column, and then use the electroplating process to copper-plate and tin-coat the inner and outer walls of the lead column; then insert a tin-resistant metal column into the liquid inlet hole, use capillary action to infiltrate the molten solder into the inner wall of the lead column, and after cooling, take out the metal column to obtain the lead.

[0014] Furthermore, in step 3, the high temperature applied for welding the root of the lead column is 250-270° C. and the time is 3-5 seconds.

[0015] Furthermore, the supercapacitor also includes a plurality of positioning grooves which are circumferentially distributed on the outer circumference of the shell and are recessed inwardly.

[0016] Furthermore, the upper end of the connecting tongue extends into the connecting column and is connected to the inner wall of the liquid inlet hole, and the connecting hole is arranged to extend inwardly from the outer side surface of the lower end of the connecting column.

[0017] Furthermore, the connecting tongue is arranged in a strip shape.

[0018] Furthermore, the connecting tongue and the connecting column are integrally formed.

[0019] Furthermore, the diameter of the connecting column is greater than the diameter of the lead column.

[0020] Furthermore, a solder layer connected to the upper end of the connecting column is arranged on the outer periphery of the lower end of the lead column, a chamfered surface is formed on the upper end of the solder layer, and the diameter of the lower end is consistent with the diameter of the connecting column.

[0021] From the above description of the present invention, it can be seen that compared with the prior art, the present invention has the following beneficial effects: the present application defines the mechanism of the lead wire, sets a liquid inlet hole in the lead wire, and sets a connecting hole connected to the liquid inlet hole at the connection between the connecting tongue and the connecting column. After the capacitor is assembled, liquid injection is performed to avoid the electrolyte from seeping out of the shell to the gap between the sealing rubber plug and the inner wall of the shell during the assembly process, thereby improving the sealing of the capacitor. At the same time, by performing local high-temperature heating at the end of the lead column to weld the solder to seal, and cutting the pins after aging, when the inner wall of the capacitor is aged for the first time, the oxygen-containing functional groups on the electrode surface react with trace water in the electrolyte under high voltage to generate impurity gases that can be released, thereby reducing the internal gas pressure of the capacitor and inhibiting the collapse and blockage of the electrode pore structure caused by gas particles, thereby improving the accessibility of the ion pair pores, reducing the internal resistance and increasing the service life of the supercapacitor.

[0022] By arranging a plurality of inwardly recessed positioning grooves on the outer peripheral surface of the shell, the insertion and fixation of the battery cell are facilitated, thereby improving the vibration resistance of the prepared supercapacitor. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 It is a structural schematic diagram of a supercapacitor;

[0024] Figure 2 It is a structural cross-sectional view of a supercapacitor;

[0025] Figure 3 It is a schematic diagram of the structure of the lead;

[0026] Figure 4 It is a structural cross-sectional view of the lead;

[0027] In the figure, 1-housing, 2-battery core, 3-lead, 4-sealing rubber plug, 5-positioning groove, 21-liquid injection channel, 31-connecting tongue, 32-connecting column, 33-lead column, 34-liquid inlet hole, 35-connecting hole, 36-soldering material layer, 37-chamfered surface. DETAILED DESCRIPTION

[0028] The present invention is further described below through specific implementation modes.

[0029] Reference Figures 1 to 4 As shown, a high-performance lead-type supercapacitor comprises a shell 1, a battery cell 2 arranged in the shell 1, two leads 3 respectively connected to the battery cell 2, a sealing rubber plug 4 arranged in the shell 1 for sealing the battery cell 2, and a plurality of positioning grooves 5 circumferentially distributed on the outer circumference of the shell 1 and recessed inwardly, wherein the corners of the contact surfaces between the positioning grooves 5 and the battery cell 2 are all smooth arc designs to prevent the battery cell 2 from being damaged when entering the shell; specifically, the two leads 3 are respectively used as a positive electrode lead and a negative electrode lead.

[0030] The battery cell 2 is formed by stacking and winding a negative electrode sheet, an inner separator, a positive electrode sheet and an outer separator in sequence, and has an injection channel 21 extending downward from the top thereof. Two leads 3 used as positive electrode leads and negative electrode leads are connected to the positive electrode sheet or the negative electrode sheet respectively.

[0031] The lead 3 includes a connecting tongue 31 connected to the battery cell 2, a connecting post 32 connected to the connecting tongue 31 and located above the battery cell 2, a lead post 33 connected to the upper end of the connecting post 32 and extending upward to the outside of the housing 1, and a liquid inlet hole 34 extending downward from the upper end of the lead post 33 to the connecting post 32, wherein a plurality of connecting holes 35 connected to the liquid inlet hole 34 are formed at the connection between the connecting tongue 31 and the connecting post 32. When injecting liquid, the electrolyte is injected through the liquid inlet hole 34 and then flows downward through the connecting hole 35 to infiltrate the battery cell.

[0032] The lead post 33 is made of a hollow iron or steel post, wherein the diameter of the connecting post 32 is larger than the diameter of the lead post 33, and a solder layer 36 connected to the upper end of the connecting post 32 is provided on the outer periphery of the lower end of the lead post 33; specifically, a chamfered surface 37 is formed on the upper end of the solder layer 36, and the diameter of its lower end is consistent with the diameter of the connecting post 32.

[0033] The connecting tongue 31 is arranged in a strip shape, and its upper end extends into the connecting column 32 and is connected to the inner wall of the liquid inlet hole 34, wherein the connecting tongue 31 and the connecting column 32 are integrally formed, and specifically, the connecting hole 35 extends inwardly from the outer side surface of the lower end of the connecting column 32.

[0034] The preparation method specifically comprises the following steps:

[0035] Step 1, lead forming: splice the connecting column 32 and the lead column 33, then insert the metal fixing column into the liquid inlet hole 34, braze the connection between the connecting column 32 and the lead column 33, take out the metal fixing column, and then use the electroplating process to copper-plated and tin-coated the inner and outer walls of the lead column 33; then insert a tin-free metal column with a diameter smaller than the diameter of the liquid inlet hole 34 into the liquid inlet hole 34, use capillary action to infiltrate the molten solder into the inner wall of the lead column 33, and after cooling, take out the metal column to obtain the lead;

[0036] Step 2, capacitor molding: prepare the battery cell 2 according to the existing battery cell 2 preparation method and dry the battery cell 2, then assemble it with the sealing rubber plug 4 and the shell through the rubber, inject the electrolyte from the liquid inlet 34, flow into the battery cell 2 through the connecting hole 35, and then apply a high temperature of 250-270°C to the upper end of the lead post 33 for 3-5 seconds to weld the upper end of the lead post 33 to form a seal;

[0037] Step 3, charge and age the capacitor at 60-70°C for 5-7h, then cut off the upper welded section of the lead column 33 to release the impurity gas generated inside the capacitor due to the first high-temperature aging, and then apply a high temperature of 250-270°C to the root position of the lead column 33 near the connecting column 33 for 3-5s to weld the root position to form a seal to obtain a supercapacitor.

[0038] The present application defines the lead structure, sets a liquid inlet hole 34 in the lead 3, and sets a connecting hole 35 connected to the liquid inlet hole 34 at the connection between the connecting tongue 31 and the connecting column 32. After the capacitor is assembled, liquid is injected to avoid the electrolyte from extending from the shell 1 to the gap between the sealing rubber plug 4 and the inner wall of the shell 1 during the assembly process, thereby improving the sealing of the capacitor. At the same time, local high-temperature heating is performed on the end of the lead column 33 to make the solder melt and seal, and the pins are trimmed after aging, so that when the inner wall of the capacitor is aged for the first time, the oxygen-containing functional groups on the electrode surface react with trace water in the electrolyte under high voltage to generate impurity gases that are released, thereby reducing the internal air pressure of the capacitor and inhibiting the collapse and blockage of the electrode pore structure caused by gas particles, thereby improving the accessibility of the ion pair pores, reducing the internal resistance and increasing the service life of the supercapacitor.

[0039] The above description is only a preferred embodiment of the present invention, and therefore cannot be used to limit the scope of implementation of the present invention. That is, equivalent changes and modifications made according to the scope of the patent application of the present invention and the contents of the specification should still fall within the scope covered by the patent of the present invention.

Claims

1. A method for preparing a high-performance lead-type supercapacitor, characterized in that: The supercapacitor comprises a shell, a battery cell arranged in the shell, two leads respectively connected to the battery cells, and a sealing rubber plug arranged in the shell for sealing the battery cell, wherein the leads comprise a connecting tongue connected to the battery cell, a connecting column connected to the connecting tongue and located above the battery cell, a lead column connected to the upper end of the connecting column and extending upward to the outside of the shell, and a liquid inlet hole extending downward from the upper end of the lead column to the connecting column, and a plurality of connecting holes connected to the liquid inlet holes are formed at the connection between the connecting tongue and the connecting column; The preparation method specifically comprises the following steps: Step 1, lead forming; Step 2, capacitor molding: the battery cell is dried, and then assembled with the sealing rubber plug and the outer shell through the rubber, the electrolyte is injected from the liquid inlet hole, flows into the battery cell through the connection hole, and then the upper end of the lead column is subjected to high temperature to weld the upper end of the lead column to form a seal; Step 3, charge and age the capacitor, then cut off the welded section at the upper end of the lead column to release the impurity gas generated inside the capacitor due to the first high-temperature aging, and then apply high temperature to the root position of the lead column near the connecting column to weld the root position to form a seal, so as to obtain the supercapacitor.

2. A high performance lead-type supercapacitor according to claim 1, characterized in that: In step 2, the high temperature applied to the upper end of the lead column for welding is 250-270° C. and the time is 3-5 seconds.

3. A high performance lead-type supercapacitor according to claim 1, characterized in that: In step 1, the specific operation of lead forming is as follows: splice the connecting column and the lead column, then insert the metal fixing column into the liquid inlet hole, braze the connection between the connecting column and the lead column, take out the metal fixing column, and then use the electroplating process to copper-plate and tin-coat the inner and outer walls of the lead column; then insert a tin-resistant metal column into the liquid inlet hole, use capillary action to infiltrate the molten solder into the inner wall of the lead column, and after cooling, take out the metal column to obtain the lead.

4. A high performance lead-type supercapacitor according to claim 1, characterized in that: In step 3, the high temperature applied for welding the root of the lead column is 250-270°C for 3-5 seconds.

5. The method for preparing a high-performance lead-type supercapacitor according to claim 1, characterized in that: The supercapacitor further comprises a plurality of positioning grooves which are circumferentially distributed on the outer circumference of the shell and are recessed inwardly.

6. The method for preparing a high-performance lead-type supercapacitor according to claim 1, characterized in that: The upper end of the connecting tongue extends into the connecting column and is connected to the inner wall of the liquid inlet hole. The connecting hole is obliquely extended inward from the outer side surface of the lower end of the connecting column.

7. The method for preparing a high-performance lead-type supercapacitor according to claim 1, characterized in that: The connecting tongue is arranged in a strip shape.

8. The method for preparing a high-performance lead-type supercapacitor according to claim 1, characterized in that: The connecting tongue and the connecting column are integrally formed.

9. The method for preparing a high-performance lead-type supercapacitor according to claim 1, characterized in that: The diameter of the connecting column is greater than the diameter of the lead column.

10. The method for preparing a high-performance lead-type supercapacitor according to claim 1, characterized in that: A solder layer connected to the upper end of the connection column is arranged on the outer periphery of the lower end of the lead column, a chamfered surface is formed on the upper end of the solder layer, and the diameter of the lower end is consistent with the diameter of the connection column.

Citation Information

Patent Citations

  • Production method of small square capacitor

    CN108305787A

  • Sealing element for electrolytic capacitor, and electrolytic capacitor using the same

    JP2008251980A

  • Capacitor and method of manufacturing the same

    JP2010098025A

  • Super capacitor of surface mount type and manufacturing method thereof

    KR101549814B1