Method for improving voltage resistance of MOS (Metal Oxide Semiconductor) device

By selecting high-energy bandgap materials and insulating layers in MOS devices, adjusting the gate structure and voltage configuration, combining doping process and simulation design, the problem of insufficient voltage resistance of MOS devices in the existing technology is solved, and the high voltage is achieved Stable improvement in performance.

CN118919411APending Publication Date: 2024-11-08WUXI LIGHTLEI ELECTRONIC TECH CO LTD
View PDF 0 Cites 2 Cited by

Patent Information

Application Number
CN202411014830.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-26
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

When the existing methods improve the voltage withstand capacity of MOS devices, increasing the channel length will affect the performance of the device, and the voltage withstand adjustment effect is not obvious, making it difficult to maintain stability at high voltages.

Method used

By selecting high-energy bandgap material as substrate material, setting the first and second insulating layers, adjusting the gate width and distance, performing hierarchical voltage configuration and doping process optimization, combining electromagnetic simulation and test optimization design, adjusting multi-stage The distance and wiring connection of the MOS structure.

Benefits of technology

It realizes flexible improvement in voltage resistance and performance stability of MOS devices, ensuring that the device performs more reliable under high voltage and avoiding the risk of performance degradation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118919411A_ABST
    Figure CN118919411A_ABST
Patent Text Reader

Abstract

The invention discloses a method for improving voltage resistance of an MOS (Metal Oxide Semiconductor) device. The method comprises the following steps: S1, selecting a substrate material; s2, selecting a gate material and preparing a gate; s3, hierarchical voltage configuration is carried out; s4, adjusting doping process parameters when the source electrode and the drain electrode are set; s5, adjusting the distance between the multiple stages of MOS structures; and S6, carrying out a withstand voltage test on the MOS device. The method for improving the voltage endurance capability of the MOS device comprises the steps of arranging a first insulating layer and a second insulating layer, selecting a substrate material and a grid material, carrying out voltage grading configuration, adjusting a doping process and adjusting the distance between multiple stages of MOS structures. The MOS device voltage-withstanding modification operation is more flexible, and the modification implementation effect of the MOS device is more obvious by using multiple adjustment modes, so that the MOS device prepared by the scheme is more stable in performance under high-voltage use.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of MOS devices, and in particular to a method for improving the withstand voltage of MOS devices. Background Art

[0002] MOS devices are semiconductor devices widely used in electronic circuits. They are widely used in digital, analog and radio frequency circuits due to their high performance, low power consumption and miniaturization. In order to increase the application of MOS devices under high voltage and improve their reliability during use, the voltage resistance of MOS devices will be improved.

[0003] Existing methods for improving the withstand voltage capability of MOS devices are mostly to increase the channel length. However, simply increasing the channel length will result in an upper limit to the withstand voltage adjustment of the MOS device, and blindly increasing the channel length will also affect the performance of the MOS device. Such a voltage-increasing method makes the modification effect on the MOS device not obvious. Therefore, a method for improving the withstand voltage of MOS devices is proposed. Summary of the invention

[0004] The object of the present invention is to provide a method for improving the withstand voltage of a MOS device to solve the problems raised in the above background technology.

[0005] To achieve the above object, the present invention provides the following technical solution: a method for improving the withstand voltage of a MOS device, the method comprising the following steps:

[0006] S1, firstly, selecting a substrate material, that is, selecting a high energy bandgap material as the substrate material, and setting a first insulating layer;

[0007] S2, selecting a gate material and preparing the gate, and setting a second insulating layer between the gate and the channel, and adjusting the width of the gate;

[0008] S3, perform hierarchical voltage configuration, combine materials from S1 and S2 to prepare a multi-level MOS structure, adjust the distance between adjacent gates, simulate the gate electric field distribution after the adjustment is completed, and then use circuit simulation to test the voltage of each level of MOS structure;

[0009] S4, adjusting doping process parameters when setting the source and drain, and using a high temperature annealing process to control the conductivity of the source and drain;

[0010] S5, adjusting the distance between the multi-level MOS structures, and adjusting the wiring connection in combination with the distance setting, and performing electromagnetic simulation after the adjustment is completed;

[0011] S6, perform voltage withstand test on MOS devices, and then further optimize the design based on the test data.

[0012] Preferably, the substrate material includes one or more of silicon, silicon germanium, silicon on insulator, gallium nitride, silicon carbide, indium gallium oxide and gallium oxide.

[0013] Preferably, the preparation material of the first insulating layer in S1 includes one or more of hafnium oxide, aluminum oxide, titanium oxide, chromium oxide, silicon nitride and aluminum nitride, and the thickness of the first insulating layer is set to 3-9 nm.

[0014] Preferably, the gate is prepared using one or more materials selected from the group consisting of polysilicon, metal gate, silicon oxide and high-k dielectric, and during the preparation of the gate, gate shape and layout are optimized and doping treatment is performed, wherein the gate structure adopts a planarized structure design, and the adjustment of the gate width and spacing includes the design of the gate's own width and the distance between adjacent gates, and the second insulating layer is aluminum oxide.

[0015] Preferably, the gate and the second insulating layer are combined using a thin film deposition technique.

[0016] Preferably, the second insulating layer is provided to reduce the width of the channel, and the calculation formula for the width of the channel is:

[0017] W=W A -2W D (1);

[0018] Among them, W A Represents the distance between adjacent gates, W D Indicates the distance between the second insulating layer and the gate.

[0019] Preferably, the multi-level MOS structure is designed to disperse the voltage to multiple levels. During the design, the voltage of each level is calculated and the corresponding substrate material, gate material and structure are selected. After the design is completed, circuit simulation is performed to verify the calculated voltage.

[0020] Preferably, the dopants used for the source and drain are phosphorus and boron, and are selected according to the type of device;

[0021] A low doping concentration is used in the middle region of the source and drain, a buffer region with a high doping concentration is designed near the source and drain, and a gradient doping method is used in the source and drain settings to gradually increase the doping concentration.

[0022] Preferably, the restrictions on the multi-level MOS structure distance adjustment and wiring adjustment include electrical characteristics, process limitations, thermal management, hierarchical layout, use of through holes, signal integrity, differential pair wiring and power grounding layout.

[0023] Preferably, the withstand voltage test method of the MOS device includes a static withstand voltage test method and a dynamic withstand voltage test;

[0024] The withstand voltage test parameters of the MOS device include voltage range, test time and environmental conditions.

[0025] Technical effects and advantages of the present invention:

[0026] The method for improving the voltage resistance of MOS devices disclosed in the present invention includes setting a first insulating layer and a second insulating layer, selecting a substrate material and a gate material, performing voltage grading configuration, adjusting a doping process, and adjusting a distance between multi-level MOS structures. By combining the above methods, the voltage resistance modification operation of the MOS device is more flexible, and a variety of adjustment methods are used to make the MOS device modification implementation effect more obvious. By using the method of the present invention, the voltage resistance modification can be completed as much as possible while ensuring the functional integrity of the MOS device, so that the performance of the MOS device prepared by the present solution is more stable under high-voltage use. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] Figure 1 The present invention is an operational flow chart of the method for improving the performance of the present invention.

[0028] Figure 2 This is a schematic diagram of the channel width calculation of the present invention. DETAILED DESCRIPTION

[0029] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0030] The present invention provides Figure 1 A method for improving the withstand voltage of a MOS device shown in the figure comprises the following steps:

[0031] S1, firstly, selecting a substrate material, that is, selecting a high-energy bandgap material as the substrate material, using the high-energy bandgap material, and setting a first insulating layer to increase the withstand voltage;

[0032] Specifically, the substrate material includes one or more of silicon, silicon germanium, silicon on insulator, gallium nitride, silicon carbide, indium gallium oxide and gallium oxide.

[0033] It should be noted that selecting a suitable substrate material can significantly improve the voltage resistance of MOS devices, improve the switching speed, power consumption and heat dissipation capacity of the device. When selecting the above materials, it is necessary to comprehensively consider the material properties, cost and application requirements to achieve the best device performance. The characteristics of the above materials are:

[0034] Silicon (Si), low cost, mature technology, easy processing, with a lot of manufacturing experience and equipment support, and suitable for most standard MOS devices;

[0035] Silicon germanium (SiGe), which can adjust the band gap and improve device performance, is suitable for high-frequency and high-power applications, and has good thermal conductivity, which helps to dissipate heat;

[0036] Silicon on insulator (SOI) significantly reduces leakage current, improves withstand voltage performance, and can improve device switching speed and reduce power consumption. Due to the presence of the insulating layer, the electric field coupling effect is reduced;

[0037] Gallium nitride (GaN), with a high energy bandgap, excellent high-temperature performance and high-voltage capability, is suitable for high-frequency and high-power applications such as RF and power converters, and has excellent heat dissipation performance, which helps improve device reliability;

[0038] Silicon carbide (SiC), with extremely high voltage and high temperature resistance, suitable for extreme conditions, low on-resistance, can improve power conversion efficiency, and excellent radiation resistance, suitable for aerospace and automotive applications;

[0039] Indium gallium oxide (InGaO), which has a wide bandgap, is suitable for high-power and high-frequency applications, and can operate at higher voltages without breakdown, helping to improve the overall performance of the device;

[0040] Gallium oxide (Ga2O3), with its extremely high bandgap (about 4.8 eV), has excellent withstand voltage characteristics and is suitable for high-voltage applications such as power switches, enabling high-performance devices at relatively low cost.

[0041] Specifically, the preparation material of the first insulating layer in S1 includes one or more of hafnium oxide, aluminum oxide, titanium oxide, chromium oxide, silicon nitride and aluminum nitride, and the thickness of the first insulating layer is set to 3-9 nm.

[0042] It should be noted that the material used for the above-mentioned insulating layer is a high dielectric constant material. The use of these high dielectric constant materials can effectively increase the thickness of the insulating layer while maintaining the same capacitance, so as to improve the performance of the insulating layer and reduce the leakage current. The characteristics of the above-mentioned materials are:

[0043] Hafnium oxide (HfO2) is one of the most commonly used high dielectric constant materials. Its dielectric constant is about 25, which is much higher than that of traditional silicon dioxide (SiO2). HfO2 has good thermal stability and is compatible with silicon materials.

[0044] Aluminum oxide (Al2O3) has a dielectric constant of about 9 and has excellent chemical stability and good interface properties;

[0045] The dielectric constant of titanium oxide (TiO2) can be as high as 100;

[0046] Chromium oxide (CrO3) exhibits good electrical properties as a high dielectric constant material;

[0047] Silicon nitride (Si3N4) has a dielectric constant of about 7, but it is used as an insulating material in some applications;

[0048] Aluminum nitride (AlN) has a dielectric constant of about 8 and has good thermal conductivity and electrical insulation properties.

[0049] S2, selecting a gate material and preparing the gate, and setting a second insulating layer between the gate and the channel, and adjusting the width of the gate to ensure uniform electric field distribution;

[0050] Specifically, the gate is used to control the switching state of the MOSFET, and the formation of the conductive channel is regulated by applying voltage. Ideally, the gate material should be insulating (such as SiO2) to form a good electrical isolation between the gate and the channel. However, the conductivity of the gate may be affected in some high-frequency and high-power applications. In order to optimize the performance of the gate, high-k materials (such as HfO2) are usually used to replace SiO2 to improve the capacitance effect and reduce the gate leakage current.

[0051] The gate preparation material includes one or more of polysilicon, metal gate, silicon oxide and high-k dielectric, and the gate shape and layout are optimized and doping treatment is performed during the gate preparation process. The gate structure adopts a flattened structure design, and the adjustment of the gate width and spacing includes the design of the gate's own width and the distance between adjacent gates. The second insulating layer is aluminum oxide.

[0052] It should be noted that polysilicon is a traditional MOSFET gate material with good stability. Its conductivity can be adjusted using doping technology during the optimization process; Metal Gate: In advanced semiconductor technology, metal gate has better electric field control capability and lower resistance than polysilicon gate. The use of metal gate (such as tungsten, tantalum, etc.) can improve the electric field distribution; Silicon oxide (SiO2) is a traditional gate dielectric material, and the electric field distribution can be optimized by controlling its thickness and quality; High-k dielectrics are used in modern MOSFETs, such as HfO2, to reduce gate leakage current and enhance gate control capability.

[0053] Design a flat gate structure to ensure uniform electric field distribution, avoid sharp structures or uneven thickness; optimize the doping concentration in the gate material to ensure uniform electric field distribution. Different doping concentrations will affect the conductivity and electric field distribution of the gate.

[0054] Furthermore, the gate and the second insulating layer are combined using thin film deposition technology to ensure the uniformity and integrity of each layer.

[0055] For further reference, Figure 2 As shown, the second insulating layer is provided to reduce the width of the channel, and the calculation formula for the width of the channel is:

[0056] W=W A -2W D (1);

[0057] Among them, W A Represents the distance between adjacent gates, W D Indicates the distance between the channel and the gate of the second insulating layer. As shown in the figure, the smooth curved surface design allows the second insulating layer to be set at a longer distance within a certain length space, thereby allowing more second insulating layers to be set, thereby stabilizing the channel structure.

[0058] S3, perform hierarchical voltage configuration, combine materials from S1 and S2 to prepare a multi-level MOS structure, adjust the distance between adjacent gates, simulate the gate electric field distribution after the adjustment is completed, and then use circuit simulation to test the voltage of each level of MOS structure;

[0059] It should be noted that when designing a multi-level MOS structure, it is necessary to clearly define the maximum voltage that needs to be withstood in the design, as well as the rated voltage of each level of MOS devices. At the same time, according to the application requirements, select nMOS, pMOS or CMOS structures; design multiple cascaded MOS devices, each device bears a part of the voltage, and the source can be connected to the drain of the next level in a cascade manner; according to the required total voltage, it is distributed to the MOS devices of each level. For example, if the total voltage is 100V, it can be designed as 10 levels, each level withstands 10V;

[0060] Specifically, the design of the multi-level MOS structure is used to disperse the voltage to multiple levels. During the design, the voltage of each level is calculated and the corresponding substrate material, gate material and structure are selected. After the design is completed, circuit simulation is performed to verify the calculated voltage.

[0061] S4, adjusting doping process parameters when setting the source and drain, reducing the electric field strength, and using a high temperature annealing process to control the conductivity of the source and drain;

[0062] Specifically, the dopants used for the source and drain are phosphorus and boron, and are selected according to the type of device;

[0063] It should be noted that the source is the injection source of carriers (electrons or holes). In n-type MOSFET, the source is usually an n-type doped region, while in p-type MOSFET it is a p-type doped region; the conductivity of the source is usually high to ensure that sufficient carriers can be effectively injected. The doping concentration and doping process of the source have an important influence on its conductivity. A higher doping concentration can increase the conductivity, thereby reducing the contact resistance of the source.

[0064] The drain is the collector of carriers. In n-type MOSFET, the drain is also an n-type doped region, while in p-type MOSFET it is a p-type doped region. The conductivity of the drain also needs to be kept high in order to effectively collect the carriers injected from the source. The design of the drain also needs to take into account factors such as breakdown voltage, and a higher doping concentration is usually used to improve its conductivity.

[0065] A low doping concentration is used in the middle area of ​​the source and drain to reduce the electric field strength, which can be achieved by controlling the concentration of the dopant and the injection time. A high doping concentration buffer zone is designed near the source and drain to concentrate the electric field in a smaller area of ​​the device under high voltage working conditions. At the same time, a gradient doping method is used in the source and drain settings to gradually increase the doping concentration. This method can locally reduce the electric field strength and avoid the electric field being concentrated at a certain point, thereby reducing the risk of breakdown.

[0066] It should be noted that after adjusting the doping concentration, electrical testing is performed to measure the device's withstand voltage, leakage current, and switching characteristics to verify the effectiveness of the doping adjustment. The operating principle is:

[0067] Electric field distribution, the electric field distribution of MOS devices is closely related to the doping concentration. Higher doping concentration will lead to enhanced electric fields in the source and drain regions, thereby increasing the risk of breakdown;

[0068] Reducing the electric field strength. By reducing the doping concentration of the source and drain, the electric field strength generated in these areas can be reduced. This is because the electric field strength is proportional to the doping concentration. When the doping concentration is low, the electric field strength is relatively small.

[0069] Improve the withstand voltage performance. The lower electric field strength helps to prevent the breakdown phenomenon and improve the withstand voltage capability of the device. In addition, the lower doping concentration can reduce the leakage current and improve the overall performance and reliability of the device.

[0070] Current control, by adjusting the doping concentration of the source and drain, can effectively control the on-current characteristics of the MOS device and avoid unnecessary current leakage under high voltage working conditions.

[0071] S5, adjusting the distance between the multi-level MOS structures, and adjusting the wiring connection in combination with the distance setting, and performing electromagnetic simulation after the adjustment is completed;

[0072] Specifically, the restrictions on distance adjustment and wiring adjustment of multi-level MOS structures include electrical characteristics, process limitations, thermal management, hierarchical layout, use of through holes, signal integrity, differential pair wiring, and power grounding layout.

[0073] It should be noted that the distance adjustment includes: electrical characteristics, the adjustment of distance will affect capacitance and inductance, and thus affect signal delay and noise. A larger distance may reduce interference, but it will also increase signal propagation delay; process limitations, the resolution and controllability of the manufacturing process will limit the minimum distance between MOS structures. The appropriate spacing needs to be determined based on the process node used; thermal management, multi-level MOS structures will generate heat, and appropriately increasing the distance can help dissipate heat and reduce the impact of temperature on circuit performance;

[0074] The wiring connection methods are as follows: hierarchical layout. In multi-level MOS structures, hierarchical layout is usually adopted to place MOS tubes of different levels on different metal layers to reduce the complexity of interconnection; through-holes (Via) are used between different metal layers to achieve electrical connection between different levels. This method can effectively save space while maintaining good electrical connection; signal integrity. When wiring, the integrity of the signal needs to be considered, such as avoiding long-distance routing, reducing corners, and avoiding cross interference; differential pair wiring. For high-speed signals, differential pair wiring can be used to reduce noise and improve the signal's anti-interference ability; power and ground layout. Ensure a good layout of power and ground to reduce the impact of power noise on the performance of the MOS structure. Large-area power and ground layers are usually used to reduce impedance.

[0075] S6, perform voltage withstand test on MOS devices, and then further optimize the design based on the test data.

[0076] Specifically, the withstand voltage test method of MOS devices includes a static withstand voltage test method and a dynamic withstand voltage test. The withstand voltage test can help determine the working ability of the device under extreme conditions and prevent failures in actual applications.

[0077] It should be noted that the static withstand voltage test is to connect the gate, power supply and source (or drain) of the device to a high voltage source, gradually increase the voltage until the withstand voltage limit of the device is reached or failure occurs, and monitor the leakage current to determine whether the device has breakdown or other failures;

[0078] Dynamic withstand voltage test tests the response capability of a device by applying a pulse voltage or a rapidly changing voltage, and observes the performance of the device under different frequencies and waveforms.

[0079] The withstand voltage test parameters of MOS devices include voltage range, test time and environmental conditions.

[0080] It should be noted that the test voltage range is determined according to the device specification, which is usually set to 1.5 to 2 times the rated operating voltage. The test duration can affect the measurement results, usually ranging from a few seconds to a few minutes. The temperature and humidity during the test should be controlled within the standard range to ensure the reliability of the test results. During the test, record the changes in leakage current to determine whether there is a current surge or breakdown. Determine the breakdown voltage of the device, usually at the point where the leakage current increases significantly. Analyze the failure mode of the device in the withstand voltage test to understand the cause of the failure.

[0081] Finally, it should be noted that the above is only a preferred embodiment of the present invention and is not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments or to make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A method for improving the withstand voltage of a MOS device, characterized in that: The improvement method comprises the following steps: S1, firstly, selecting a substrate material, that is, selecting a high energy bandgap material as the substrate material, and setting a first insulating layer; S2, selecting a gate material and preparing the gate, and setting a second insulating layer between the gate and the channel, and adjusting the width of the gate; S3, perform hierarchical voltage configuration, combine materials from S1 and S2 to prepare a multi-level MOS structure, adjust the distance between adjacent gates, simulate the gate electric field distribution after the adjustment is completed, and then use circuit simulation to test the voltage of each level of MOS structure; S4, adjusting doping process parameters when setting the source and drain, and using a high temperature annealing process to control the conductivity of the source and drain; S5, adjusting the distance between the multi-level MOS structures, and adjusting the wiring connection in combination with the distance setting, and performing electromagnetic simulation after the adjustment is completed; S6, perform voltage withstand test on MOS devices, and then further optimize the design based on the test data.

2. A method for improving the withstand voltage of a MOS device according to claim 1, characterized in that: The substrate material includes one or more of silicon, silicon germanium, silicon on insulator, gallium nitride, silicon carbide, indium gallium oxide and gallium oxide.

3. A method for improving the withstand voltage of a MOS device according to claim 1, characterized in that: The preparation material of the first insulating layer in S1 includes one or more of hafnium oxide, aluminum oxide, titanium oxide, chromium oxide, silicon nitride and aluminum nitride, and the thickness of the first insulating layer is set to 3-9nm.

4. A method for improving the withstand voltage of a MOS device according to claim 1, characterized in that: The gate is prepared using materials selected from the group consisting of polysilicon, metal gate, silicon oxide, and high-k dielectrics. During the preparation of the gate, gate shape and layout are optimized and doping treatment is performed. The gate structure adopts a planarized structure design. The gate width and spacing adjustment includes the design of the gate width itself and the distance between adjacent gates. The second insulating layer is aluminum oxide.

5. A method for improving the withstand voltage of a MOS device according to claim 4, characterized in that: The gate and the second insulating layer are combined by using a thin film deposition technology.

6. A method for improving the withstand voltage of a MOS device according to claim 5, characterized in that: The second insulating layer is provided to reduce the width of the channel, and the calculation formula of the width of the channel is: W=W A -2W D (1); Among them, W A Represents the distance between adjacent gates, W D Indicates the distance between the second insulating layer and the gate.

7. A method for improving the withstand voltage of a MOS device according to claim 1, characterized in that: The multi-level MOS structure is designed to disperse the voltage to multiple levels. During the design, the voltage of each level is calculated and the corresponding substrate material, gate material and structure are selected. After the design is completed, circuit simulation is performed to verify the calculated voltage.

8. The method for improving the withstand voltage of a MOS device according to claim 1, characterized in that: The dopants used in the source and drain are phosphorus and boron, and are selected according to the type of device; A low doping concentration is used in the middle region of the source and drain, a buffer region with a high doping concentration is designed near the source and drain, and a gradient doping method is used in the source and drain settings to gradually increase the doping concentration.

9. The method for improving the withstand voltage of a MOS device according to claim 1, characterized in that: The restrictions of the multi-level MOS structure distance adjustment and wiring adjustment include electrical characteristics, process limitations, thermal management, hierarchical layout, use of through holes, signal integrity, differential pair wiring and power grounding layout.

10. The method for improving the withstand voltage of a MOS device according to claim 1, characterized in that: The voltage withstand test method of the MOS device includes a static voltage withstand test method and a dynamic voltage withstand test; The withstand voltage test parameters of the MOS device include voltage range, test time and environmental conditions.

Citation Information

Cited By

  • Design and preparation method of modified diamond with multi-signal sensing function

    CN119245743A

  • SiC MOS dynamic characteristic prediction method and system and medium

    CN120671618A