Adjustable carrier for producing plastic package type IPM module and welding method

By using adjustable vehicles and adjusting structures in the production of plastic-sealed IPM modules, the problems of low production efficiency and poor welding quality caused by different vehicles in the prior art are solved, and efficient screen printing and patch welding are achieved. Reduces costs and improves product quality.

CN118919466APending Publication Date: 2024-11-08XIAN YONGDIAN ELECTRIC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410855216.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-28
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

In the production of plastic-sealed IPM modules, different vehicles are required to use screen printing and patch welding, resulting in low production efficiency, high cost and poor soldering quality, which is prone to damage solder paste pattern and material collision damage.

Method used

Adoptable vehicles, with multiple sets of temporary storage units on the vehicle, including grooves for placing PCBs and DBCs, and a pull-pull or press-type adjustment structure is installed in the grooves, and the adjustment structure is used to print on screen and Maintain the correct height of the PCB and DBC during patch welding to avoid replacing the vehicle.

Benefits of technology

Improve production efficiency, avoid solder paste pattern damage and material bumps, simplify operation steps, reduce production costs, and improve soldering quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118919466A_ABST
    Figure CN118919466A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of semiconductor devices, and particularly discloses an adjustable carrier for producing a plastic package type IPM module and a welding method. The adjustable carrier comprises a carrier body, and multiple sets of temporary storage units arranged on the upper surface of the carrier body at intervals in the length direction; each set of temporary storage unit comprises a first groove and a second groove which are formed in the carrier body, are arranged in rows in the width direction of the carrier body and have different depths, and the first groove and the second groove are used for placing a PCB and a DBC respectively; wherein all the second grooves are arranged in a row and are communicated with one another to form a track groove, any end of the track groove penetrates through the carrier body, and a drawing type or pressing type adjusting structure used for adjusting the depth of the second grooves is installed in the track groove. By adopting the adjustable carrier provided by the invention, the silk-screen printing process and the patch welding process can be completed in sequence, so that various quality problems such as solder paste pattern damage and product collision caused by material transfer are avoided, the operation steps are simplified, the efficiency of producing the plastic package type IPM module is greatly improved, and the competitiveness is brought to enterprises.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of semiconductor devices, and in particular relates to an adjustable carrier and a welding method for producing a plastic-sealed IPM module. Background Art

[0002] Plastic-encapsulated IPM (Intelligent Power Module) is a new type of control module that integrates IGBT chip and its drive circuit, control circuit and overcurrent, undervoltage, short circuit, overheating and other protection circuits. It is called a highly integrated semiconductor device and can be used to control and drive high-power electronic equipment, such as AC motor drivers, frequency converters, inverters, etc. Therefore, it is widely used in frequency conversion home appliances, inverter power supplies, industrial control and other fields, with considerable social and economic benefits.

[0003] The structure of a general plastic-encapsulated IPM module is mainly composed of "lead frame + printed circuit board (hereinafter referred to as PCB) + ceramic copper-clad substrate (hereinafter referred to as DBC)". The combination of IGBT, FRD chip and DBC, as well as the combination of DBC, PCB and lead frame of this product uses solder paste welding process. Since the copper layer on the back of DBC must be fully exposed outside the injection molded body as a heat sink, the PCB and DBC are in different height planes. In the existing process, when producing plastic-encapsulated IPM modules, two different carriers are used for screen printing and surface mount welding respectively. This is because screen printing requires that the PCB and DBC are located on the same plane of the carrier tray and the surface of the carrier tray is flat and has no protrusions, while surface mount welding requires the use of carriers with grooves of different depths to assemble the PCB, DBC and lead frame according to structural requirements. This leads to the following defects in the existing technology when producing plastic-encapsulated IPM modules:

[0004] First, because screen printing and patch welding use different carriers, when performing patch welding after screen printing, PCB and DBC need to be transferred one by one, which seriously restricts production efficiency and requires multiple carriers, increasing production costs;

[0005] Second, after screen printing, the solder paste covers the soldering area on the surface of PCB and DBC, the contact area is too small, and the edge of DBC is a ceramic layer. Therefore, it is easy to cause the solder paste pattern to be damaged and the material to be damaged by collision during the transfer process, which affects the quality of welding and even causes the product to be scrapped in severe cases.

[0006] In view of this, this invention is proposed. Summary of the invention

[0007] The purpose of the present invention is to overcome the shortcomings of the above-mentioned prior art and provide an adjustable carrier and a welding method for producing plastic-sealed IPM modules. The method is mainly used to solve the problem that two different carriers need to be used in the existing process for producing plastic-sealed IPM modules by screen printing and chip welding, resulting in the need to transfer PCBs and DBCs one by one after screen printing. By adopting the adjustable carrier provided by the present invention, there is no need to replace the carrier during the two processes of screen printing and chip welding, which not only avoids various quality problems such as damage to the solder paste pattern and product bumps caused by the transfer of materials, but also simplifies the operation steps and greatly improves production efficiency, thereby bringing competitiveness to the enterprise.

[0008] The purpose of the present invention is to be solved by the following technical solutions:

[0009] On the one hand, the present invention provides an adjustable carrier for producing a plastic-encapsulated IPM module, comprising a carrier body, wherein a plurality of temporary storage units are arranged at intervals along the length direction of the upper surface of the carrier body, each set of the temporary storage units comprises a first groove and a second groove which are opened on the carrier body and arranged in a row along the width direction thereof, and the depth of the second groove is greater than the depth of the first groove, the first groove is used to place a PCB, and the second groove is used to place a DBC;

[0010] Among them, the second grooves in multiple sets of the temporary storage units are arranged in a row and connected to each other to form a track groove. Either end of the track groove passes through the carrier body. An adjustment structure for adjusting the depth of the second groove is installed in the track groove, and the adjustment structure is a pull-out type or a press-type.

[0011] Furthermore, the pull-out type adjustment structure includes a support plate, which is arranged in the track groove, and the length of the support plate is greater than the distance between the first and last second grooves, and the width of the support plate is smaller than the width of the second grooves.

[0012] Further, the thickness of the support plate+the thickness of the DBC=the depth of the second groove, and the depth of the first groove=the thickness of the PCB.

[0013] Furthermore, a through hole is provided on the support plate at one end of the track groove penetrating the carrier body, and the through hole cooperates with an auxiliary line to horizontally pull the support plate.

[0014] Furthermore, the carrier body is made of aluminum alloy, and the support plate is made of resin.

[0015] Furthermore, the push-type adjustment structure includes a bearing plate and a plurality of ball spring pins, the plurality of ball spring pins are evenly embedded on the opposite side walls of the track groove, each of the ball spring pins includes a cylindrical shell, a spring is arranged in the inner cavity of the cylindrical shell, one end of the spring is fixedly connected to the bottom of the cylindrical shell, and the other end is connected to the ball embedded in the top of the cylindrical shell;

[0016] Among them, the cylindrical shell is completely embedded in the side wall of the track groove, and the ball extends out of the cylindrical shell into the track groove in a natural state, the supporting plate is mounted on the ball, and the height from the upper surface of the supporting plate to the bottom of the second groove + the thickness of DBC = the depth of the second groove.

[0017] Furthermore, a mounting hole for mounting the lead frame is respectively opened on the upper surface of the carrier body and on both sides of the multiple sets of temporary storage units, and the two mounting holes are arranged diagonally, and the lead frame is assembled by inserting a pin into the mounting hole.

[0018] On the other hand, the present invention provides a welding method for producing a plastic-encapsulated IPM module based on the above-mentioned adjustable carrier, which specifically includes the following steps:

[0019] Step 1: Assemble PCB and DBC

[0020] First, install the pull-out or push-type adjustment structure in the track groove of the carrier body, and then respectively install the PCB in the first groove and the DBC in the second groove, and the DBC is located on the upper part of the adjustment structure. At this time, the upper surfaces of the PCB and the DBC are located on the same horizontal plane;

[0021] Step 2: Screen printing

[0022] Put the PCB and DBC assembled in step 1 together with the adjustable carrier into the screen printing equipment so that the upper surfaces of the PCB and DBC are printed with solder paste;

[0023] Step 3: Adjust the depth of the second groove

[0024] After the screen printing in step 2 is completed, the adjustment structure in the adjustable carrier is pulled out or pressed down, so that the DBC with screen printing completed in the second groove falls to the bottom thereof, so that the DBC and the PCB form the height difference required by the product structure;

[0025] Step 4: Patching

[0026] After the adjustment in step 3 is completed, the PCB and DBC as well as the adjustable carrier are placed in the chip mounting equipment to mount the chip;

[0027] Step 5: Assemble the lead frame

[0028] Assemble the lead frame on the adjustable carrier completed in step 4, and assemble the lead frame, PCB and DBC according to the requirements of the product structure;

[0029] Step 6: Soldering

[0030] The adjustable carrier of the lead frame assembled in step 5 is placed in a vacuum welding furnace for welding.

[0031] Further, in step 1, the pull-out adjustment structure is a support plate, the thickness of the support plate + the thickness of the DBC = the depth of the second groove, and the depth of the first groove = the thickness of the PCB;

[0032] In step 3, when adjusting the depth of the second groove, the support plate is pulled out along the length direction of the carrier body to increase the depth of the second groove and make the DBC fall.

[0033] Further, in step 1, the push-type adjustment structure includes a bearing plate and a plurality of ball spring pins embedded along the two opposite side walls of the track groove, the bearing plate is mounted on the ball spring pins, and at this time, the height from the upper surface of the bearing plate to the bottom of the second groove + the thickness of DBC = the depth of the second groove;

[0034] Step 3: When adjusting the depth of the second groove, press the bearing plate in the vertical direction. At this time, the ball spring pin contracts under the force, and the DBC moves downward with the bearing plate, thereby adjusting the depth of the second groove.

[0035] Compared with the prior art, the present invention has the following beneficial effects:

[0036] The present invention is mainly composed of a carrier body and an adjustment structure; wherein, a plurality of temporary storage units are provided on the carrier body, and each temporary storage unit includes a first groove and a second groove for accommodating PCB and DBC, so that multiple sets of products can be processed at one time; at the same time, the second groove for accommodating DBC is connected in series to form a track groove, and a pull-out or press-type adjustment structure is installed in the groove, through which the depth of the second groove can be adjusted, so that when the screen printing process is performed, the upper surface of the PCB and DBC is in the same horizontal plane. At the same time, when the patch welding process is performed, there is no need to replace the carrier, and only the adjustment structure needs to be pulled out or pressed to meet the height difference requirement of the PCB and DBC in the product. Compared with the prior art, the present invention can perform screen printing and patch welding processes respectively through a set of adjustable carriers, thereby avoiding quality problems such as solder paste pattern damage and product bumps caused by transferring materials (PCB, DBC), and at the same time greatly improves the efficiency of producing plastic-sealed IPM modules, and reduces the number of carriers, providing competitiveness for enterprises. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] The accompanying drawings are incorporated in and constitute a part of this specification and, together with the description, serve to explain the principles of the present invention.

[0038] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, for ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.

[0039] Figure 1 This is a process flow chart of a welding method for producing a plastic-sealed IPM module according to the present invention;

[0040] Figure 2 is a schematic diagram of the structure of an adjustable carrier according to Embodiment 1 of the present invention;

[0041] Figure 3 It is a cross-sectional schematic diagram of the assembly of an adjustable carrier (pull-out adjustment structure) during screen printing in Embodiment 1 of the present invention;

[0042] Figure 4 It is a top view schematic diagram of the adjustable carrier assembly (pull-out type adjustment structure) during screen printing in Embodiment 1 of the present invention;

[0043] Figure 5 It is a cross-sectional schematic diagram of the assembly of an adjustable carrier (pull-out type adjustment structure) during patch welding in Example 1 of the present invention;

[0044] Figure 6 It is a cross-sectional schematic diagram of the assembly of an adjustable carrier (press-type adjustment structure) during screen printing in Embodiment 2 of the present invention;

[0045] Figure 7 It is a cross-sectional schematic diagram of the assembly of an adjustable carrier (press-type adjustment structure) during patch welding in Example 2 of the present invention;

[0046] Figure 8 It is a schematic cross-sectional view of the ball spring pin in the push-type adjustment structure of Example 2 of the present invention.

[0047] in:

[0048] 1 is the carrier body; 11 is the temporary storage unit; 12 is the track groove; 13 is the mounting pin hole; 111 is the first groove; 112 is the second groove;

[0049] 2 is PCB;

[0050] 3 for DBC;

[0051] 4 is a support plate; 41 is a through hole;

[0052] 5 is a bearing plate;

[0053] 6 is a ball spring pin; 61 is a cylindrical housing; 62 is a spring; and 63 is a ball. DETAILED DESCRIPTION

[0054] Exemplary embodiments will be described in detail herein, examples of which are shown in the accompanying drawings. When the following description refers to the drawings, the same numbers in different drawings represent the same or similar elements unless otherwise indicated. The embodiments described in the following exemplary embodiments do not represent all embodiments consistent with the present invention. Instead, they are merely examples of devices consistent with some aspects of the present invention as detailed in the appended claims.

[0055] In order to enable those skilled in the art to better understand the technical solution of the present invention, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments.

[0056] Example 1

[0057] See also Figures 2 to 5 An adjustable carrier for producing a plastic-encapsulated IPM module provided by an embodiment of the present invention comprises a rectangular carrier body 1, and four sets of temporary storage units 11 are arranged at intervals along the length direction of the carrier body 1 on the upper surface thereof. The number of the temporary storage units 11 can be increased or decreased according to actual conditions. Each set of the temporary storage units 11 comprises a first groove 111 and a second groove 112 which are opened on the carrier body 1 and arranged in a row along the width direction thereof, and the depth of the second groove 112 is greater than the depth of the first groove 111. The first groove 111 is used to place a PCB 2, and the second groove 112 is used to place a DBC 3. All the second grooves 112 are arranged in a row and connected to each other to form a track groove 12, and either end of the track groove 12 passes through the carrier body 1, as shown in the attached figure of this embodiment. Figure 2 , 4 As shown, the track groove 12 penetrates from the left end, and an adjustment structure for adjusting the depth of the second groove 112 is installed in the track groove 12. In this embodiment, the adjustment structure is a pull-out type.

[0058] Specifically, the pull-out adjustment structure of the embodiment of the present invention includes a support plate 4, which is arranged in the track groove 12. The length of the support plate 4 should be greater than the distance between the first and last second grooves 112, so as to be able to support the DBC 3 in all the second grooves 112. Preferably, the length of the support plate 4 should be greater than the length of the track groove 12, that is, there is a margin after the support plate 4 is fully extended into the track groove 12. More preferably, a through hole 41 is opened at the margin to facilitate the support plate 4 to be horizontally pulled out of the track groove 12 in coordination with the auxiliary line; at the same time, the width of the support plate 4 is smaller than the width of the second groove 112, so that when the support plate 4 is pulled out after screen printing, the DBC 3 can be prevented from being pulled out together.

[0059] Furthermore, in the embodiment of the present invention, when screen printing is performed, it is required that the thickness of the support plate 4 + the thickness of the DBC 3 = the depth of the second groove 112, and the depth of the first groove 111 = the thickness of the PCB 2, that is, the upper surfaces of the PCB 2 and the DBC 3 are located on the same horizontal plane. Figure 3 When the patch soldering process is performed after the screen printing is completed, the support plate 4 is evacuated, and the PCB 2 and DBC 3 are formed as shown Figure 5 The height difference shown should meet the product design requirements.

[0060] In addition, if Figure 2 As shown, in order to facilitate the assembly of the lead frame, an installation pin hole 13 for installing the lead frame is opened on the upper surface of the carrier body 1 and on both sides of the multiple sets of temporary storage units 11, and the two installation pin holes 13 are arranged diagonally. When assembling the lead frame, a pin is inserted into the installation pin hole 13. During specific assembly, the lead frame is placed on the carrier body 1, and then the pin is inserted into the installation pin hole 13 to fix the lead frame. Each adjustable carrier is equipped with two pins, which can be inserted diagonally, and the operation is simple.

[0061] In the embodiment of the present invention, the carrier body 1 is made of an aluminum alloy material with strong thermal conductivity and high hardness, such as 7075 aluminum alloy; the support plate 4 is made of a wear-resistant but relatively low hardness resin material, such as polytetrafluoroethylene, to avoid the copper layer on the lower surface of the DBC 3 being worn during the extraction process and causing appearance defects.

[0062] like Figure 1 As shown, the present invention provides a welding method for producing a plastic-encapsulated IPM module based on the adjustable carrier of the pull-out adjustment structure, which specifically includes the following steps:

[0063] 1) Assemble PCB 2 and DBC 3

[0064] First, the support plate 4 of set specifications is installed in the track groove 12 opened in the carrier body 1, and then the PCB 2 is assembled in the first groove 111, and the DBC 3 is assembled in the second groove 112, and the DBC 3 is located on the upper part of the support plate 4. At this time, the upper surfaces of the PCB 2 and the DBC 3 are located in the same horizontal plane, that is, the thickness of the support plate 4 plus the thickness of the DBC 3 is exactly equal to the depth of the second groove 112, and the depth of the first groove 111 is equal to the thickness of the PCB 2;

[0065] 2) Screen printing

[0066] Put the PCB 2 and DBC 3 assembled in step 1) together with the adjustable carrier into a screen printing device so that the upper surfaces of the PCB 2 and DBC 3 are printed with solder paste;

[0067] 3) Adjust the depth of the second groove 112

[0068] After the screen printing of step 2) is completed, the support plate 4 is pulled out along the length direction of the carrier body 1 (left side in the figure). After the support plate 4 is pulled out, the depth of the second groove 112 becomes larger, and the DBC 3 immediately falls to the bottom of the second groove 112, thereby forming a height difference required by the product structure with the PCB 2;

[0069] Step 4) Patching

[0070] After the adjustment in step 3) is completed, the PCB 2 and the DBC 3 as well as the adjustable carrier are placed in a chip mounting device to mount the chip;

[0071] Step 5) Assemble the lead frame

[0072] Assemble the lead frame on the adjustable carrier completed in step 4, so that the lead frame, PCB 2 and DBC 3 are assembled according to the requirements of the product structure;

[0073] Step 6) Soldering

[0074] The adjustable carrier with the lead frame assembled in step 5) is placed in a vacuum welding furnace for welding.

[0075] Example 2

[0076] like Figures 6 to 8 As shown, the adjustable carrier provided by the embodiment of the present invention is different from the embodiment 1 only in that the adjustment structure in this embodiment is a press-type, and the track groove 12 completely passes through both ends of the carrier body 1.

[0077] Specifically, the push-type adjustment structure includes a bearing plate 5 and a plurality of ball spring pins 6. The plurality of ball spring pins 6 are evenly embedded on the opposite side walls of the track groove 12. Only the telescopic head portion of the ball spring pin 6 is exposed in the track groove 12. During screen printing, the bearing plate 5 is mounted on the ball spring pin 6. At this time, the height from the upper surface of the bearing plate 5 to the bottom of the second groove 112 + the thickness of the DBC 3 = the depth of the second groove 112. At the same time, the upper surfaces of the PCB 2 and the DBC 3 are located on the same horizontal plane. Figure 6 When the screen printing is completed and the patch welding process is performed, the carrier plate 5 is vertically squeezed, and the head of the ball spring pin 6 shrinks due to the squeezing force, so the DBC 3 will follow the carrier plate 5 and fall to the bottom of the second groove 112, as shown Figure 7 shown.

[0078] Specifically, Figure 8As shown, each ball spring pin 6 includes a cylindrical shell 61, an inner cavity of which is provided with a spring 62, one end of the spring 62 is fixedly connected to the bottom of the cylindrical shell 61, and the other end is connected to a ball 63 embedded in the top of the cylindrical shell 61; when installed, the cylindrical shell 61 is completely embedded in the side wall of the track groove 12, and in a natural state, only the ball 63 extends out of the cylindrical shell 61 into the track groove 12, and the bearing plate 5 is carried on the ball 63.

[0079] In the embodiment of the present invention, the carrier plate 5 does not need to be pulled out, thus greatly reducing the friction with the DBC 3. Therefore, in the embodiment of the present invention, both the carrier body 1 and the carrier plate 5 can be made of aluminum alloy material with strong thermal conductivity to ensure welding quality.

[0080] like Figure 1 As shown, the present invention provides a welding method for producing a plastic-encapsulated IPM module based on the adjustable carrier with the above-mentioned press-type adjustment structure, which specifically includes the following steps:

[0081] 1) Assemble PCB 2 and DBC 3

[0082] First, the carrier plate 5 of set specifications is installed in the track groove 12 opened in the carrier body 1, and is placed on the upper part of the ball 63 in the ball spring pin 6 on both sides of the track groove 12, and then the PCB 2 is respectively assembled in the first groove 111, and the DBC 3 is assembled in the second groove 112, and the DBC 3 is located on the upper part of the carrier plate 5. In the natural state, the upper surfaces of the PCB 2 and the DBC 3 are located in the same horizontal plane, that is, the height from the upper surface of the carrier plate 5 to the bottom of the second groove 112 plus the thickness of the DBC 3 is equal to the depth of the second groove 112;

[0083] 2) Screen printing

[0084] Put the PCB 2 and DBC 3 assembled in step 1) together with the adjustable carrier into a screen printing device so that the upper surfaces of the PCB 2 and DBC 3 are printed with solder paste;

[0085] 3) Adjust the depth of the second groove 112

[0086] After the screen printing in step 2) is completed, the carrier plate 5 is pressed in the vertical direction, at which time the ball spring pin 6 is forced to contract, and the DBC 3 moves downward along with the carrier plate 5 and falls to the bottom of the second groove 112, thereby forming a height difference with the PCB 2 required by the product structure;

[0087] Explanation: Since the ball spring pin 6 is embedded in the side wall of the track groove 12, when the supporting plate 5 is pressed, the head ball 63 of the ball spring pin 6 is forced to shrink, so that the supporting plate 5 can move downward, thereby achieving the purpose of adjusting the depth of the second groove 112. Conversely, the supporting plate 5 can be lifted up to be removed, and at the same time, the ball 63 of the ball spring pin 6 rebounds and protrudes.

[0088] Step 4) Patching

[0089] After the adjustment in step 3) is completed, the PCB 2 and the DBC 3 as well as the adjustable carrier are placed in a chip mounting device to mount the chip;

[0090] Step 5) Assemble the lead frame

[0091] Assemble the lead frame on the adjustable carrier completed in step 4, so that the lead frame, PCB 2 and DBC 3 are assembled according to the requirements of the product structure;

[0092] Step 6) Soldering

[0093] The adjustable carrier with the lead frame assembled in step 5) is placed in a vacuum welding furnace for welding.

[0094] To sum up, since the carrier provided by the present invention adopts a pull-out or push-type adjustment structure, screen printing and patch welding processes can be completed successively in the same set of adjustable carriers, thereby solving the various problems caused by the prior art that PCB 2 and DBC3 need to be transferred one by one after screen printing. It not only avoids the damage to the solder paste pattern caused by touching the product after screen printing, resulting in poor welding, and quality problems such as DBC breakage caused during operation, thereby improving product quality; it also simplifies the operating steps, improves the efficiency of producing plastic-sealed IPM modules, and at the same time reduces the number of carriers used, thereby reducing production costs.

[0095] The above description is only a specific embodiment of the present invention, so that those skilled in the art can understand or implement the present invention. Various modifications to these embodiments will be apparent to those skilled in the art, and the general principles defined herein can be implemented in other embodiments without departing from the spirit or scope of the present invention.

[0096] It should be understood that the present invention is not limited to what has been described above and that various modifications and changes may be made without departing from its scope. The scope of the present invention is limited only by the appended claims.

Claims

1. An adjustable carrier for producing plastic-encapsulated IPM modules, characterized in that: The carrier body (1) comprises a plurality of temporary storage units (11) arranged at intervals on the upper surface of the carrier body (1) along the length direction thereof, each set of the temporary storage units (11) comprising a first groove (111) and a second groove (112) which are opened on the carrier body (1) and arranged in a row along the width direction thereof, and the depth of the second groove (112) is greater than the depth of the first groove (111), the first groove (111) is used for placing a PCB (2), and the second groove (112) is used for placing a DBC (3); The second grooves (112) in the plurality of temporary storage units (11) are arranged in a row and connected to each other to form a track groove (12). Either end of the track groove (12) passes through the carrier body (1). An adjustment structure for adjusting the depth of the second groove (112) is installed in the track groove (12). The adjustment structure is a pull-out type or a press-type.

2. The adjustable carrier for producing plastic-encapsulated IPM modules according to claim 1, characterized in that: The pull-out type adjustment structure comprises a support plate (4), wherein the support plate (4) is arranged in the track groove (12), the length of the support plate (4) is greater than the distance between the first and last second grooves (112), and the width of the support plate (4) is less than the width of the second grooves (112).

3. The adjustable carrier for producing plastic-encapsulated IPM modules according to claim 2, characterized in that: The thickness of the support plate (4) + the thickness of the DBC (3) = the depth of the second groove (112), and the depth of the first groove (111) = the thickness of the PCB (2).

4. The adjustable carrier for producing plastic-encapsulated IPM modules according to claim 2, characterized in that: A through hole (41) is provided on the support plate (4) at one end of the track groove (12) penetrating the carrier body (1), and the through hole (41) cooperates with the auxiliary line to horizontally pull the support plate (4).

5. The adjustable carrier for producing plastic-encapsulated IPM modules according to claim 2, characterized in that: The material of the carrier body (1) is aluminum alloy, and the material of the support plate (4) is resin.

6. The adjustable carrier for producing plastic-encapsulated IPM modules according to claim 1, characterized in that: The push-type adjustment structure comprises a bearing plate (5) and a plurality of ball spring pins (6), wherein the plurality of ball spring pins (6) are evenly embedded on opposite side walls of the track groove (12), and each of the ball spring pins (6) comprises a cylindrical shell (61), wherein a spring (62) is arranged in the inner cavity of the cylindrical shell (61), wherein one end of the spring (62) is fixedly connected to the bottom of the cylindrical shell (61), and the other end is connected to a ball (63) embedded in the top of the cylindrical shell (61); The cylindrical shell (61) is completely embedded in the side wall of the track groove (12), and the ball (63) extends out of the cylindrical shell (61) into the track groove (12) in a natural state, the bearing plate (5) is mounted on the ball (63), and the height from the upper surface of the bearing plate (5) to the bottom of the second groove (112) + the thickness of the DBC (3) = the depth of the second groove (112).

7. The adjustable carrier for producing plastic-encapsulated IPM modules according to claim 1, characterized in that: A mounting pin hole (13) for mounting a lead frame is provided on the upper surface of the carrier body (1) and on both sides of the plurality of temporary storage units (11), and the two mounting pin holes (13) are arranged diagonally. When assembling the lead frame, a pin is inserted into the mounting pin hole (13).

8. A welding method for producing a plastic-encapsulated IPM module, characterized in that: The welding method is based on the adjustable carrier according to claim 1, and specifically comprises the following steps: Step 1: Assemble PCB (2) and DBC (3) First, the pull-out or push-type adjustment structure is installed in the track groove (12) provided in the carrier body (1), and then the PCB (2) is respectively installed in the first groove (111), and the DBC (3) is installed in the second groove (112), and the DBC (3) is located on the upper part of the adjustment structure, and at this time, the upper surfaces of the PCB (2) and the DBC (3) are located on the same horizontal plane; Step 2: Screen printing The PCB (2) and DBC (3) assembled in step 1 are placed together with the adjustable carrier into a screen printing device, so that the upper surfaces of the PCB (2) and DBC (3) are printed with solder paste; Step 3: Adjust the depth of the second groove (112) After the screen printing in step 2 is completed, the adjustment structure in the adjustable carrier is pulled out or pressed down, so that the DBC (3) that has been screen-printed in the second groove (112) falls to the bottom thereof, so that the DBC (3) and the PCB (2) form a height difference required by the product structure; Step 4: Patching After the adjustment in step 3 is completed, the PCB (2) and the DBC (3) together with the adjustable carrier are placed in a chip mounting device to mount the chip; Step 5: Assemble the lead frame Assemble the lead frame on the adjustable carrier completed in step 4, so that the lead frame, PCB (2) and DBC (3) are assembled according to the requirements of the product structure; Step 6: Soldering The adjustable carrier of the lead frame assembled in step 5 is placed in a vacuum welding furnace for welding.

9. The welding method for producing a plastic-encapsulated IPM module according to claim 8, characterized in that: In step 1, the pull-out adjustment structure is a support plate (4), the thickness of the support plate (4) + the thickness of the DBC (3) = the depth of the second groove (112), and the depth of the first groove (111) = the thickness of the PCB (2); In step 3, when adjusting the depth of the second groove (112), the support plate (4) is pulled out along the length direction of the carrier body (1) to increase the depth of the second groove (112) and make the DBC (3) fall.

10. The welding method for producing a plastic-encapsulated IPM module according to claim 8, characterized in that: In step 1, the push-type adjustment structure comprises a bearing plate (5) and a plurality of ball spring pins (6) embedded along the opposite side walls of the track groove (12), the bearing plate (5) is mounted on the ball spring pins (6), and at this time, the height from the upper surface of the bearing plate (5) to the bottom of the second groove (112) + the thickness of DBC (3) = the depth of the second groove (112); Step 3: When adjusting the depth of the second groove (112), the support plate (5) is pressed in the vertical direction. At this time, the ball spring pin (6) is forced to contract, and the DBC (3) moves downward following the support plate (5), thereby adjusting the depth of the second groove (112).