Micro through hole filling method, application and product

By opening through holes on the HDI board and performing two electroplating micro-through holes, the problem of inadequate convection of toner residue and plating solution in small-size blind holes in micro-blind buried holes is solved, and the HDI board is realized Excellent conductivity and high yield rate.

CN118921888APending Publication Date: 2024-11-08MFS TECH HUNAN
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411004316.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-25
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The existing micro-blind buried hole technology is difficult to completely remove the toner residue and insufficient convection of the plating solution in small-size blind holes, resulting in a decrease in the conductivity of the HDI board and prone to plating layering and gap problems.

Method used

By using the micro-through hole filling method, by opening 30-70μm through holes on the HDI plate, using dispersed carbon powder suspension to treat the hole walls, and performing two electroplating: the first electroplating is reduced in the through hole diameter, and the second The plating completely encloses the through holes to form a flat plane.

Benefits of technology

The toner residue and plating layer are avoided at the bottom of the blind hole, the conductivity and product yield of the HDI board are improved, and the sealing of the interconnection channels between layers and the tightness of the electroplated copper layer is ensured.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118921888A_ABST
    Figure CN118921888A_ABST
Patent Text Reader

Abstract

In order to realize interlayer interconnection on an HDI (High Density Interconnection) board, when the required hole diameter is 30-70 microns, the invention provides a micro through hole filling and leveling method, which comprises the following steps of: directly forming a through hole of 30-70 microns on the HDI board, reducing the aperture of the through hole to be less than 25 microns through primary electroplating, and filling and leveling the through hole through secondary electroplating to realize interlayer interconnection. And a flat bonding pad plane is formed on the surface of the HDI plate. Compared with a traditional micro blind buried hole technology, the method has the advantages that plating layer layering caused by residual carbon powder at the bottom of the blind hole and cracks at the bottom of the blind hole caused by insufficient convection exchange of copper plating liquid medicine in the hole burying process due to the fact that the hole diameter of the blind hole is too small are avoided; according to the HDI board interlayer interconnection obtained by adopting the micro through hole filling and leveling method, the phenomenon that the product performance is affected by resistance abrupt change points due to the fact that cavities exist in the electroplating copper layer is avoided, the method can be used for preparing the HDI board, and the prepared HDI board product is high in yield.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of circuit board preparation, and in particular relates to a micro-through hole filling method and application thereof. Background Art

[0002] HDI (High Density Interconnector) board, that is, high-density interconnect board, is a circuit board with a high circuit distribution density. HDI board has inner and outer layers of circuits, and usually uses micro blind buried hole technology to connect the circuits between layers, such as Figure 1 As shown, the micro blind buried via technology is usually to drill a blind hole 020 on the HDI board 010 to penetrate the insulating layer 011, and then treat the hole wall of the blind hole 020 with a dispersed carbon powder suspension to deposit carbon powder 030 on the hole wall (this step is called black hole), and then electroplate the blind hole 020 to fill it with metal copper 040 to connect the copper-plated layer 012 on the surface of the HDI board 010 (this step is called filling hole), so that the internal connection of each layer of circuit is achieved. As the current HDI board design is becoming more and more sophisticated and the product area is getting smaller and smaller, the blind hole aperture is also gradually getting smaller, from the common 80μm-100μm blind hole aperture to 30-50μm blind hole aperture. When the blind hole with a smaller aperture uses the above-mentioned micro blind buried hole technology, carbon powder will accumulate at the bottom of the blind hole in the black hole step. When the blind hole aperture is too small, the carbon powder at the bottom of the blind hole cannot be cleaned up, which will cause the electroplated copper at the bottom of the hole to be delaminated. In addition, since the plating solution is not easy to fully convect and diffuse in the small-diameter blind hole in the hole filling step, there are often gaps at the bottom of the blind hole, which affects the conductivity of the HDI board. When the HDI board is used later, the large resistance at the blind hole buried hole is easy to cause heat and performance degradation. Summary of the invention

[0003] In view of this, the purpose of the present invention is to provide a micro-through hole filling method to replace the micro blind buried hole technology to achieve the connection of each layer of the HDI board, avoid the phenomenon of plating layer delamination and cracking in the connection path of each layer of the circuit, and the obtained HDI board has excellent conductivity.

[0004] A micro-through hole filling method of the present invention comprises the following steps:

[0005] S100, opening a through hole on the HDI board, wherein the through hole has an aperture of 30-70 μm;

[0006] S200, treating the hole wall of the through hole with a dispersed carbon powder suspension so that the carbon powder is attached to the hole wall of the through hole;

[0007] S300, the first electroplating, plating the first copper layer on the surface of the HDI board and plating a thin layer of copper on the wall of the through hole, so that the through hole diameter is reduced;

[0008] S400, the second electroplating, plating a second copper layer on the surface of the HDI board and filling the through holes with copper plating, so that the HDI board can achieve inter-layer interconnection and form a flat surface on the surface of the HDI board.

[0009] Furthermore, the through hole opened in step S100 is a laser opening.

[0010] Furthermore, step S110 is included between step S100 and step S200, and in step S110, the HDI board is processed by a plasma surface cleaning process.

[0011] Furthermore, the electroplating solution for the first electroplating in step S300 includes: copper sulfate pentahydrate: 110-150 g / L, sulfuric acid: 160-200 g / L, chloride ion: 40-70 ppm, 125-T Additive: 1.0-5.0 ml / L, 125-TCarrier: 15-35 ml / L.

[0012] Furthermore, in the step S300, the current of the first electroplating is 16-20 ASF, and the electroplating time is 14-24 min.

[0013] Furthermore, the aperture of the through hole in step S300 is reduced to less than 25 μm.

[0014] Furthermore, the electroplating solution for the second electroplating in step S400 includes: copper sulfate pentahydrate: 200-250 g / L, sulfuric acid: 30-60 g / L, chloride ion: 50-90 ppm, VL200-A: 10-30 ml / L, VL200-B: 0.5-1.6 ml / L, VL200-C: 10-20 ml / L.

[0015] Furthermore, in the step S400, the current of the second electroplating is 10-18 ASF, and the electroplating time is 30-50 min.

[0016] Another aspect of the present invention further provides an application of a micro-via filling method, and the micro-via filling method is applied in the field of HDI board manufacturing.

[0017] Another aspect of the present invention further provides an HDI board product, which is prepared according to the above-mentioned micro-through hole filling method.

[0018] The present invention has the following beneficial effects:

[0019] In order to realize the interlayer interconnection on the HDI board, when the required opening diameter is 30-70μm, the present invention provides a micro-through hole filling method, which directly opens a 30-70μm through hole on the HDI board, reduces the through hole diameter to less than 25μm by the first electroplating, and fills the through hole by the second electroplating to realize the interlayer interconnection, and forms a flat pad plane on the surface of the HDI board. Compared with the traditional micro blind buried hole technology, this method avoids the plating layer stratification caused by the carbon powder residue at the bottom of the blind hole and the cracks at the bottom of the blind hole caused by the insufficient convection exchange of the copper plating solution during the buried hole process due to the small aperture of the blind hole. The micro-through hole filling method adopts two electroplating methods, that is, the first electroplating reduces the aperture of the through hole and the second electroplating completely closes the through hole to fill the channel of the interconnection between the layers of the HDI board, and optimizes the electroplating parameters related to the first electroplating and the second electroplating, avoiding the situation that the use of one electroplating filling easily leads to the closure of one end of the through hole. The interconnection between layers of the HDI board obtained by the micro-through hole filling method will not have resistance mutation points affecting product performance due to the presence of voids in the electroplated copper layer, and can be used to prepare HDI boards with a high yield rate. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1 This is a schematic diagram of the steps of micro blind buried via technology.

[0021] Figure 2 is a schematic diagram of the steps of a micro-through hole filling method provided in some embodiments of the present application,

[0022] Figure 3 is an appearance diagram of a through-hole sample provided in Example 1 of the present application,

[0023] Figure 4 is an electron microscope image of a cross-section of a through-hole sample provided in Example 1 of the present application,

[0024] Figure 5 This is the appearance diagram of the sample after the through hole is sealed provided in Example 1 of the present application.

[0025] Figure 6 This is an electron microscope image of the cross section of the sample after the through hole is closed as provided in Example 1 of the present application.

[0026] Description of reference numerals:

[0027] 010.HDI board,

[0028] 011. Insulation layer,

[0029] 012. Copper plating,

[0030] 020. Blind hole,

[0031] 030.Toner,

[0032] 040.Metallic copper. DETAILED DESCRIPTION

[0033] In order to more clearly and completely describe the technical solution of the present invention, the present invention is further described in detail through specific embodiments below. It should be understood that the specific embodiments described herein are only used to explain the present invention, and are not used to limit the present invention. Various changes can be made within the scope of the rights of the present invention.

[0034] The terms "vertical", "horizontal", "left", "right" and similar expressions used herein are for illustrative purposes only and are not intended to be the only implementation method. Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art to which the present invention belongs. The terms used herein in the specification of the present invention are only for the purpose of describing specific implementation methods and are not intended to limit the present invention. The term "and / or" used herein includes any and all combinations of one or more of the relevant listed items.

[0035] like Figure 2 As shown, the present invention provides a micro-through hole filling method, comprising the following steps

[0036] S100, open a through hole on the HDI board, the through hole diameter is 30-70μm;

[0037] S200, treating the hole wall of the through hole with a dispersed carbon powder suspension so that the carbon powder is attached to the hole wall of the through hole;

[0038] S300, the first electroplating, plating the first copper layer on the surface of the HDI board and plating a thin layer of copper on the wall of the through hole, so that the through hole diameter is reduced;

[0039] S400, the second electroplating, plating a second copper layer on the surface of the HDI board and filling the through holes with copper plating, so that the HDI board can achieve inter-layer interconnection and form a flat surface on the surface of the HDI board.

[0040] As mentioned in the background technology, in order to achieve interlayer interconnection on the HDI board, the traditional micro blind buried hole technology is used to connect the lines between the layers. The micro blind buried hole technology has a better connection effect when the blind hole aperture is 80-100μm. When the blind hole aperture is lower than 80μm, the carbon powder remaining at the bottom of the blind hole during the black hole process cannot be cleaned up due to the small aperture, which causes the bottom of the hole to be delaminated during the subsequent copper plating and filling. Moreover, when the aperture is too small, the exchange effect of the electroplating solution in the blind hole becomes poor, which affects the electroplating effect and causes cracks in the electroplating layer at the bottom of the blind hole. In order to avoid the above situation, the present invention adopts The method of opening a through hole on the HDI board is to open a through hole with a required aperture of 30-70μm on the HDI board, and the through hole directly penetrates the HDI board. Then the hole wall of the through hole is also treated with a black hole so that carbon powder is attached to the hole wall of the through hole. Then the through hole is electroplated for the first time, and the first copper layer is plated on the surface of the HDI board and a thin layer of copper is plated on the hole wall of the through hole, so that the hole diameter of the through hole is reduced; then the second electroplating is performed, and the second copper layer is plated on the surface of the HDI board and the through hole is filled with copper plating, so that the HDI board can achieve inter-layer interconnection and form a flat surface on the surface of the HDI board. The micro-through hole filling method provided by the present invention uses through holes to replace blind holes, so that carbon powder in black holes will not be deposited in the holes, and the convective exchange effect of the plating solution in the through holes during electroplating is better than that of the blind holes, and the attached electroplated copper layer does not have delamination and cracking; the use of copper plating twice can avoid the high current density at the hole mouth during copper plating once, which causes one end of the hole mouth to be closed or both ends to be closed at the same time. When one end is closed, the electroplating process is similar to the blind hole filling process, the convective exchange effect of the plating solution in the hole is not good, and cracks exist in the electroplating layer; if both ends are closed, it means that a cavity is formed in the hole during the filling process, and the product performance is greatly reduced.

[0041] In some embodiments provided by the present invention, the through hole diameter is reduced to less than 25 μm in step S300. The first electroplating reduces the through hole diameter to less than 25 μm, so that the hole diameter in the hole can be continuously reduced to completely closed during the second electroplating to achieve interlayer interconnection and form a flat surface on the surface of the HDI board.

[0042] In some embodiments of the present invention, the through hole formed in step S100 is formed by laser drilling.

[0043] In some embodiments of the present invention, step S110 is further included between step S100 and step S200. In step S110, the HDI board is processed by a plasma surface cleaning process.

[0044] In some embodiments provided by the present invention, the plating solution for the first electroplating in step S300 includes: copper sulfate pentahydrate: 110-150 g / L, sulfuric acid: 160-200 g / L, chloride ion: 40-70 ppm, 125-T Additive: 1.0-5.0 ml / L, 125-TCarrier: 15-35 ml / L.

[0045] In some embodiments provided by the present invention, the current of the first electroplating in step S300 is 16-20ASF, and the electroplating time is 14-24min. The electroplating current and the electroplating time are adjusted accordingly according to the aperture of the laser opening in step S100, so that the copper layer can be plated on the through-hole wall to reduce the aperture of the through-hole but not to close the through-hole: specifically, when the electroplating current of the first electroplating is 16-20ASF, the aperture of the through-hole is 30μm, and the electroplating time is 14-16min; when the aperture of the through-hole is 70μm, the electroplating time is 20-24min.

[0046] In some embodiments provided by the present invention, the plating solution for the second electroplating in step S400 includes: copper sulfate pentahydrate: 200-250 g / L, sulfuric acid: 30-60 g / L, chloride ion: 50-90 ppm, VL200-A: 10-30 ml / L, VL200-B: 0.5-1.6 ml / L, VL200-C: 10-20 ml / L.

[0047] In some embodiments provided by the present invention, the current of the second electroplating in step S400 is 10-18ASF, and the electroplating time is 30-50min. In the second electroplating, in order to seal the through hole densely, the electroplating current is smaller than the current of the first electroplating, but the electroplating time is also extended accordingly. Specifically, when the electroplating current of the second electroplating is 10-18ASF, the original aperture of the through hole is 30μm, and the electroplating time is 30min; when the original aperture of the through hole is 70μm, the electroplating time is 50min.

[0048] The present invention is described in detail below through specific embodiments.

[0049] Example 1

[0050] The soft board is cut into pieces. The soft board is a copper-clad board with three layers of 12μm copper layer, 25μm Pi (polyimide) layer and 12μm copper layer. Through holes are opened on the soft board by laser. The through hole diameter is 60μm. Then the soft board with through holes is treated by plasma surface cleaning process. The hole wall of the through hole is treated with dispersed carbon powder suspension so that carbon powder is attached to the hole wall of the through hole. The soft board is electroplated for the first time. The plating solution comes from Rohm and Haas 125-T series plating The composition of the plating solution is: copper sulfate pentahydrate: 120g / L, sulfuric acid: 180g / L, chloride ion: 50ppm, 125-TAdditive: 3.0ml / L, 125-TCarrier: 25ml / L; the electroplating current is 18ASF, the electroplating time is 20min, and sampling is carried out on the obtained soft board, taking a through hole on any four corners and a through hole at the center of the board surface as sampling points. The appearance of the through holes at the above two sampling points is as follows Figure 3 As shown, the through holes at the above two sampling points were vertically sliced, and the cross sections were examined by electron microscope. The obtained electron microscope photos are shown in Figure 4 As shown by Figure 4 It can be seen that the apertures of the through holes are 17.06μm and 20.79μm, respectively, which are less than 25μm. Then the soft board is electroplated for the second time. The plating solution comes from Hongtai Da's VL200 series. The composition of the plating solution is: copper sulfate pentahydrate: 230g / L, sulfuric acid: 50g / L, chloride ion: 70ppm, VL200-A: 20ml / L, VL200-B: 1.2ml / L, VL200-C: 15ml / L; the electroplating current is 14ASF, and the electroplating time is 40min. The obtained soft board takes two through holes on any four corners and one through hole at the center of the board as sampling points. The appearance of the through holes at the three sampling points is as follows Figure 5 As shown, the through holes at the three sampling points were vertically sliced, and the cross sections were examined by electron microscope. The obtained electron microscope photos are shown in Figure 6 As shown. Figure 5 It can be seen that the through hole on the soft board is filled and there is no obvious gap between the hole and the board surface. Figure 6 It can be seen that the electroplated copper layer in the through hole is tight, without gaps, delamination and voids, and the copper layer on the upper and lower soft board surfaces forms a flat plane, which is conducive to the subsequent use of the board surface as a solder pad.

[0051] Another aspect of the present invention further provides an application of a micro-via filling method, and the micro-via filling method is applied in the field of HDI board manufacturing.

[0052] Another aspect of the present invention further provides an HDI board product, which is prepared according to the above-mentioned micro-through hole filling method, which will not be described in detail here.

[0053] The above is a detailed introduction to a micro-via filling method, application and product provided by the present invention. This article uses specific examples to illustrate the principles and implementation methods of the present invention. The description of the above embodiments is only used to help understand the core idea of ​​the present invention. It should be pointed out that for ordinary technicians in this technical field, without departing from the principles of the present invention, the present invention can also be improved and modified, and these improvements and modifications also fall within the scope of protection of the claims of the present invention.

Claims

1. A method for filling a micro-through hole, characterized in that: The following steps are involved: S100, opening a through hole on the HDI board, wherein the through hole has an aperture of 30-70 μm; S200, treating the hole wall of the through hole with a dispersed carbon powder suspension so that the carbon powder is attached to the hole wall of the through hole; S300, the first electroplating, plating the first copper layer on the surface of the HDI board and plating a thin layer of copper on the wall of the through hole, so that the through hole diameter is reduced; S400, the second electroplating, plating a second copper layer on the surface of the HDI board and filling the through holes with copper plating, so that the HDI board can achieve inter-layer interconnection and form a flat surface on the surface of the HDI board.

2. The micro-through hole filling method according to claim 1, characterized in that: The step S100 of opening the through hole is laser drilling.

3. The micro-through hole filling method according to claim 1, characterized in that: The step S110 is further included between the step S100 and the step S200. In the step S110, the HDI board is processed by a plasma surface cleaning process.

4. The micro-through hole filling method according to claim 1, characterized in that: The electroplating solution for the first electroplating in step S300 includes: copper sulfate pentahydrate: 110-150 g / L, sulfuric acid: 160-200 g / L, chloride ion: 40-70 ppm, 125-T Additive: 1.0-5.0 ml / L, 125-T Carrier: 15-35 ml / L.

5. The micro-through hole filling method according to claim 1, characterized in that: In the step S300, the current of the first electroplating is 16-20 ASF, and the electroplating time is 14-24 minutes.

6. The micro-through hole filling method according to claim 1, characterized in that: In the step S300 , the diameter of the through hole is reduced to less than 25 μm.

7. The micro-through hole filling method according to claim 1, characterized in that: The electroplating solution for the second electroplating in step S400 includes: copper sulfate pentahydrate: 200-250 g / L, sulfuric acid: 30-60 g / L, chloride ion: 50-90 ppm, VL200-A: 10-30 ml / L, VL200-B: 0.5-1.6 ml / L, VL200-C: 10-20 ml / L.

8. The micro-through hole filling method according to claim 1, characterized in that: The current of the second electroplating in step S400 is 10-18 ASF, and the electroplating time is 30-50 min.

9. Application of a micro-through hole filling method, characterized in that: Application of the micro-through hole filling method according to any one of claims 1 to 8 in the field of HDI board manufacturing.

10. An HDI board product, characterized in that: The micro-through hole is prepared according to the micro-through hole filling method according to any one of claims 1 to 8.