Paint door production process for changing paint-free door processing mode
By modifying white latex adhesive composite veneer and density board and performing UV roll coating, combined with cold press assembly, the production process of leather painted wooden doors is simplified, the problems of cumbersome and low efficiency of traditional processes are solved, and the product pass rate is significantly improved and Process efficiency.
Patent Information
- Application Number
- CN202411152676.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-21
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2044-08-21
AI Technical Summary
The production process of traditional leather painted wooden doors is cumbersome, with a long production cycle, low efficiency, low pass rate, high labor intensity for workers, and wood products can easily lead to product quality decline when humidity changes.
Modified white latex is used to bond the wood veneer with polypropylene fiber cloth to make a composite wood veneer, and hot pressed and bonded with the density board, then UV rolling is performed to obtain a painted panel, and finally cold pressed and assembled with the core material to simplify the process flow.
It significantly shortened the production cycle and improved the paint end qualification rate from 75% to 99%, reducing the labor intensity of workers and improving product quality and market competitiveness.
Smart Images

Figure SMS_1
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of wooden paint products, and in particular relates to a paint door production process which improves the paint-free door processing method. Background Art
[0002] At present, paint products in the industry generally make components first, assemble the products into shape, and then paint the surface; while paint-free products use surface-treated decorative panels and are directly assembled with other components to form products. Therefore, the production efficiency, quality stability and cost-effectiveness of paint-free products are higher than those of paint products. However, compared with paint-free products, paint products have many high-quality properties such as brighter colors, stronger visual impact, better surface finish, easier scrubbing, and better moisture resistance. Even though paint-free products have obvious advantages in production efficiency and other aspects, paint products are still the main choice in many scenarios.
[0003] Based on the above, simplifying and shortening the production process of paint products is the current research focus in the industry. Taking the veneer painted wooden door as an example, its traditional production process is very cumbersome, including: material preparation-cold pressing-sanding-hot pressing veneer-edge punching-edge sealing-key hole opening-grinding-roll coating-door inspection-packaging. This process has obvious defects such as many production processes, long cycle, low efficiency, low qualified rate of finished products, and high labor intensity of workers. The more prominent problem is that wood products will shrink or expand due to changes in humidity in the air during the production process, resulting in a significant reduction in the qualified rate of the product at the paint end. At the same time, due to the continuous assembly of parts during the entire manufacturing process, the labor cost required for the subsequent production will rise sharply.
[0004] In view of this, in order to improve product quality, improve production efficiency, and reduce the labor intensity of workers, it is of great significance to improve and study a new production process for veneer paint wooden doors. Summary of the invention
[0005] In view of the cumbersome traditional production process, the purpose of the present invention is to provide a paint door production process that changes the paint-free door processing method. The present invention combines the paint-free product processing method, uses a special modified white latex to first bond the veneer and polypropylene fiber cloth as a composite veneer, and then applies glue to the density board to further hot-press and bond it with the composite veneer, and then UV roller coating is performed to obtain a paint panel, and finally the paint panel and the core material are directly pressed and assembled to form a door leaf. The new process provided by the present invention shortens the full-line production cycle by 8-10 days compared to the traditional production process of veneered paint wooden doors. It can not only significantly reduce the labor intensity of workers, but also increase the paint end qualification rate from the traditional 75% to 99%. The product quality has risen sharply and has good market competitiveness.
[0006] To achieve the above object, the present invention specifically adopts the following scheme: The present invention provides a paint door production process for improving the paint-free door processing method, comprising the following steps: Step 1: Select core materials, density boards and veneers without obvious defects, and steam and dry the selected raw materials for later use; Step 2: Take the veneer obtained in step 1, bond it with polypropylene fiber cloth to make composite veneer, then glue the composite veneer and density board through hot pressing to obtain veneer density board; Step 3: UV roller coating the laminated density board obtained in step 2 to obtain a painted panel; Step 4: Take the paint panel and core material obtained in step 3, and assemble them by cold pressing to obtain a semi-finished product; Step 5: Cut, edge-seal, unlock and package the semi-finished product in sequence to obtain the veneered painted wooden door.
[0007] Preferably, the core material in step 1 is solid wood or a solid wood frame plus filler; the density board is high-density fiberboard or medium-density fiberboard with a density of 0.7-0.9 g / cm 3 The veneer material is black walnut or cherry wood with a thickness of 0.08-0.12 mm; the moisture content is controlled to 10%-12% by steaming and drying.
[0008] Preferably, in step 2, the veneer and polypropylene fiber cloth are bonded and the composite veneer and density board are hot-pressed and laminated using modified white latex. The preparation method of the modified white latex is as follows: chitosan is added to the polyvinyl alcohol solution and mixed and stirred evenly as an emulsifier system; ethylene vinyl acetate, versatate vinyl carbonate and initiator solution are slowly added dropwise to the diluted emulsifier system at 75-85°C; after the addition is completed, the temperature is kept high for full polymerization; then the temperature is cooled to room temperature, dibutyl phthalate and octanol are added and stirred evenly to obtain an emulsion; finally, melamine formaldehyde resin is added to the obtained emulsion and fully dispersed to obtain the modified white latex.
[0009] Preferably, the raw materials for preparing the modified white latex are as follows by weight: 3-9 parts of polyvinyl alcohol, 0.5-2 parts of chitosan, 45-68 parts of ethylene vinyl acetate, 7-14 parts of vinyl versatate, 0.2-0.5 parts of initiator (ammonium persulfate), 2-6 parts of dibutyl phthalate, 1-3 parts of octanol, 6-12 parts of melamine formaldehyde resin, and sufficient water.
[0010] The present invention uses natural veneer and polypropylene fiber cloth to make composite veneer, which not only retains the beauty, touch and texture of the surface veneer, but also can reduce the thickness of the veneer used to reduce costs; and the polypropylene fiber cloth has high tensile strength and elastic modulus, which can effectively enhance the strength of the veneer and improve the overall stability of the door leaf. For the bonding between the veneer and the polypropylene fiber cloth and the composite veneer and the density board, the present invention uses ethylene vinyl acetate as the main monomer and versatate vinyl acetate as the cross-linking monomer to prepare modified white latex, the combination of the two can greatly improve the adhesive force and water resistance and durability of the glue, chitosan and melamine formaldehyde resin can further enhance the bonding strength and heat resistance, and the prepared high-performance modified white latex can provide good stability and strong bonding force for the composite veneer and the veneer density board.
[0011] Preferably, the thickness of the composite veneer in step 2 is 0.16-0.2 mm, and hot pressing bonding refers to bonding one side of the composite veneer polypropylene fiber cloth to the density board.
[0012] Preferably, the parameters of the hot pressing bonding are: temperature 120-135° C., pressure 5-6 MPa, and time 10-15 min.
[0013] Preferably, the hardness of the paint used for UV roller coating in step three is not less than 3H.
[0014] Preferably, in step 4, the paint panel and the core material are cold pressed using a two-component plywood glue.
[0015] Preferably, the cold pressing parameters in step 4 are: pressure 7.4-8 MPa, and processing time 10-14 h.
[0016] Compared with the prior art, the present invention has the following beneficial effects: The present invention combines the processing technology of paint-free products, improves the current cumbersome production process of veneer paint wooden doors, and obtains a new production process, which is: material preparation-hot pressing veneer-roll coating-cold pressing-new line (edge punching-edge sealing-unlocking connection)-door inspection-packaging. The present invention forms a composite veneer by bonding veneer with polypropylene fiber cloth, and at the same time, a modified white latex is used to form a veneer density board with good stability with the composite veneer and density board; polypropylene fiber cloth and veneer can significantly improve the mechanical properties and processability of woodworking components, while reducing the thickness of the veneer used to reduce costs. The present invention first uses the panel to paint and then assembles, which significantly shortens the traditional more than a dozen processing steps, and the production cycle of the whole line is shortened by 8-10 days year-on-year; at the same time, the veneer process is changed from the original whole door press to the panel press, which greatly reduces the labor intensity of workers, and the change from the whole door to the panel also reduces the labor intensity of workers, and the qualified rate of the paint end is also increased from 75% of the traditional process to 99%. The process turnover of the present invention is reduced, the product quality is directly improved, the yield rate is greatly improved, and the quality of the product is further guaranteed. DETAILED DESCRIPTION
[0017] In order to make the purpose, technical scheme and advantages of the present invention clearer, the technical scheme of the present invention will be clearly and completely described below in conjunction with the embodiments. If the specific conditions are not specified in the embodiments, they are carried out according to the conventional conditions or the conditions recommended by the manufacturer. If the manufacturer of the reagents or instruments is not specified, they are all conventional products that can be purchased commercially.
[0018] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art of the present invention. The terms used in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The term "and / or" used herein includes any and all combinations of one or more related listed items.
[0019] In view of the complicated traditional process, the new process adopted by the present invention is: material preparation - hot pressing lamination - roller coating - cold pressing - new line (edge punching - edge sealing - unlocking connection) - door inspection - packaging. The new process of the present invention is combined with the paint-free product processing method. The panel is first painted and then assembled. At the same time, higher hardness paint is used, and the middle section of the semi-finished product contact surface rubber strip is added to isolate and reduce friction. Plastic tracks and rubber wheels are used to solve the problem of embossing to prevent defects such as scratches on the paint surface and broken edges.
[0020] Example 1 A production process for a veneer painted wooden door, comprising: 1. Choose solid wood boards and medium-density fiberboards (0.7 g / cm 3), black walnut veneer (processed to a thickness of 0.1 mm), the selected raw materials are spray-steamed and dried to a moisture content of 10% for later use.
[0021] 2. Weigh 6 parts of polyvinyl alcohol (PVA1799, the same below), 1.2 parts of chitosan, 55 parts of ethylene vinyl acetate, 11 parts of vinyl ester carbonate, 0.35 parts of ammonium persulfate, 4 parts of dibutyl phthalate, 2 parts of octanol, 10 parts of melamine formaldehyde resin, and sufficient water by weight. Add chitosan to the polyvinyl alcohol solution (85°C) and mix well as the emulsifier system. Slowly drop ethylene vinyl acetate, vinyl ester carbonate and ammonium persulfate solution into the diluted emulsifier system at 80°C. After the drop is completed, continue to keep warm for full polymerization, then cool to room temperature, add dibutyl phthalate and octanol, stir well, adjust pH (7.5) and viscosity (9000 mPa·s) to obtain an emulsion, and finally add melamine formaldehyde resin to the obtained emulsion to fully disperse, so as to obtain a modified white latex.
[0022] 3. Take the treated veneer and use the modified white latex to mix it with polypropylene fiber cloth (fiber diameter not exceeding 12μm, surface density 44 g / m 2 , the same below) bonding (glue amount 0.02 g / cm 2 ), and composite veneer (thickness 0.18 mm) was made; then modified white latex (coating amount 0.03 g / cm) was evenly applied on one side of the medium density fiberboard. 2 ), bond one side of the composite veneer polypropylene fiber cloth to the glue-coated side of the medium density fiberboard, put them into a hot press, and perform hot pressing and bonding at 5.5 MPa and 125°C for 12 minutes to obtain a veneer density board.
[0023] 4. The obtained laminated density board was UV-rolled (using silicon-modified polyurethane resin SJ-5021, Jining, Shandong) to obtain a painted panel.
[0024] 5. Take the obtained painted panel and solid wood board, and evenly apply two-component plywood glue (BAINIAN ZBL-A803, solid content 53%, glue coating amount 0.045 g / cm 2 ), assemble the glue-coated side of the paint panel with the solid wood board, put the assembled workpiece into a cold press, and cold press for 12 h under 7.6 MPa to form a semi-finished product; 6. The semi-finished products are cut, edge-sealed, unlocked and packaged in sequence to obtain the veneered painted wooden door.
[0025] Example 2 A production process for a veneer painted wooden door, comprising: 1. Choose solid wood boards and medium-density fiberboards (0.7 g / cm3 ), black walnut veneer (processed to a thickness of 0.1 mm), the selected raw materials are spray-steamed and dried to a moisture content of 12% for later use.
[0026] 2. Weigh 5 parts of polyvinyl alcohol, 1.5 parts of chitosan, 45 parts of ethylene vinyl acetate, 7 parts of tert-butyl carbonate, 0.2 parts of ammonium persulfate, 2 parts of dibutyl phthalate, 1 part of octanol, 6 parts of melamine formaldehyde resin, and sufficient water by weight. Add chitosan to the polyvinyl alcohol solution (85°C) and mix well as the emulsifier system. Slowly drop ethylene vinyl acetate, tert-butyl carbonate and ammonium persulfate solution into the diluted emulsifier system at 80°C. After the drop is completed, continue to keep warm for full polymerization. Then cool to room temperature, add dibutyl phthalate and octanol, stir well, adjust pH (7.5) and viscosity (9000 mPa·s) to obtain an emulsion. Finally, add melamine formaldehyde resin to the obtained emulsion and fully disperse it to obtain a modified white latex.
[0027] 3. Take the treated veneer and glue it to the polypropylene fiber cloth using the modified white latex (glue coating amount 0.02 g / cm 2 ), and composite veneer (thickness 0.18 mm) was made; then modified white latex (coating amount 0.03 g / cm) was evenly applied on one side of the medium density fiberboard. 2 ), bond one side of the composite veneer polypropylene fiber cloth to the glue-coated side of the medium density fiberboard, put them into a hot press, and perform hot pressing and bonding at 6 MPa and 120°C for 15 min to obtain a veneer density board.
[0028] 4. The obtained laminated density board was UV-rolled (using silicon-modified polyurethane resin SJ-5021, Jining, Shandong) to obtain a painted panel.
[0029] 5. Take the obtained painted panel and solid wood board, and evenly apply two-component plywood glue (BAINIAN ZBL-A803, solid content 53%, glue coating amount 0.045 g / cm 2 ), assemble the glue-coated side of the paint panel with the solid wood board, put the assembled workpiece into a cold press, and cold press for 14 h under 7.4 MPa to form a semi-finished product; 6. The semi-finished products are cut, edge-sealed, unlocked and packaged in sequence to obtain the veneered painted wooden door.
[0030] Example 3 A production process for a veneer painted wooden door, comprising: 1. Choose solid wood boards and medium-density fiberboards (0.8 g / cm 3), black walnut veneer (processed to a thickness of 0.12 mm), the selected raw materials are spray-steamed and dried to a moisture content of 10% for later use.
[0031] 2. Weigh 6 parts of polyvinyl alcohol, 1 part of chitosan, 68 parts of ethylene vinyl acetate, 14 parts of vinyl ester carbonate, 0.5 parts of ammonium persulfate, 6 parts of dibutyl phthalate, 3 parts of octanol, 12 parts of melamine formaldehyde resin, and sufficient water by weight. Add chitosan to the polyvinyl alcohol solution (85°C) and mix well as the emulsifier system. Slowly drop ethylene vinyl acetate, vinyl ester carbonate and ammonium persulfate solution into the diluted emulsifier system at 80°C. After the drop is completed, continue to keep warm for full polymerization. Then cool to room temperature, add dibutyl phthalate and octanol, stir well, adjust pH (7.5) and viscosity (9500 mPa·s) to obtain an emulsion. Finally, add melamine formaldehyde resin to the obtained emulsion and fully disperse it to obtain a modified white latex.
[0032] 3. Take the treated veneer and glue it to the polypropylene fiber cloth using the modified white latex (glue coating amount 0.02 g / cm 2 ), to make composite veneer (thickness 0.2 mm); then evenly apply modified white latex (glue coating amount 0.03 g / cm 2 ), bond one side of the composite veneer polypropylene fiber cloth to the glue-coated side of the medium density fiberboard, put them into a hot press, and perform hot pressing and bonding at 5 MPa and 130°C for 10 min to obtain a veneer density board.
[0033] 4. The obtained laminated density board was UV-rolled (using silicon-modified polyurethane resin SJ-5021, Jining, Shandong) to obtain a painted panel.
[0034] 5. Take the obtained painted panel and solid wood board, and evenly apply two-component plywood glue (BAINIAN ZBL-A803, solid content 53%, glue coating amount 0.045 g / cm 2 ), assemble the side of the paint panel coated with glue with the solid wood board, put the assembled workpiece into a cold press, and cold press for 10 h under 8 MPa to form a semi-finished product; 6. The semi-finished products are cut, edge-sealed, unlocked and packaged in sequence to obtain the veneered painted wooden door.
[0035] Comparative Example 1 Refer to the step parameters of Example 1, except that white latex prepared from the following raw materials is used instead of bonding to prepare the composite veneer and hot pressing to prepare the veneer density board.
[0036] No versatate vinyl carbonate is added, that is, the raw materials for preparation are: 6 parts of polyvinyl alcohol, 1.2 parts of chitosan, 55 parts of ethylene vinyl acetate, 0.35 parts of ammonium persulfate, 4 parts of dibutyl phthalate, 2 parts of octanol, 10 parts of melamine formaldehyde resin, and sufficient water.
[0037] Comparative Example 2 Refer to the step parameters of Example 1, except that white latex prepared from the following raw materials is used instead of bonding to prepare the composite veneer and hot pressing to prepare the veneer density board.
[0038] No chitosan and melamine formaldehyde resin are added, that is, the raw materials are: 6 parts of polyvinyl alcohol, 55 parts of ethylene vinyl acetate, 11 parts of vinyl versatate, 0.35 parts of ammonium persulfate, 4 parts of dibutyl phthalate, 2 parts of octanol, and sufficient water.
[0039] Comparative Example 3 The parameters of the steps in Example 1 are referred to, except that black walnut veneer (processed to a thickness of 0.18 mm) is used to directly bond the glue-coated side of the medium-density fiberboard and hot-press the veneer to prepare the veneer board.
[0040] Test example The samples prepared in the above Examples 1-3 and Comparative Examples 1-3 were subjected to performance testing (GB / T 17657-2022 "Test methods for physical and chemical properties of wood-based panels and veneer wood-based panels"), and the results are as follows.
[0041] Table 1
[0042] It can be seen that the present invention significantly shortens the production process and greatly improves the mechanical properties and stability of the obtained product. The process of the present invention significantly improves production efficiency, reduces the labor intensity of workers, and improves product quality, and has good application prospects.
[0043] The embodiments described above only express several preferred embodiments of the present invention, and the descriptions thereof are relatively specific and detailed, but are not intended to limit the present invention. It should be noted that for those skilled in the art, the present invention may also have various changes and modifications, and any modifications, equivalent substitutions, improvements, etc. made within the concept and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. A paint door production process that changes the paint-free door processing method, characterized in that: The steps include: Step 1: Select core materials, density boards and veneers without obvious defects, and steam and dry the selected raw materials for later use; Step 2: Take the veneer obtained in step 1, bond it with polypropylene fiber cloth to make composite veneer, then glue the composite veneer and density board through hot pressing to obtain veneer density board; Step 3: UV roller coating the laminated density board obtained in step 2 to obtain a painted panel; Step 4: Take the paint panel and core material obtained in step 3, and assemble them by cold pressing to obtain a semi-finished product; Step 5: Cut, edge-seal, unlock and package the semi-finished product in sequence to obtain the veneered painted wooden door.
2. The paint door production process according to claim 1 is characterized in that: Step 1: The core material is solid wood or solid wood frame plus filler; the density board is high-density fiberboard or medium-density fiberboard with a density of 0.7-0.9 g / cm 3 The veneer material is black walnut or cherry wood with a thickness of 0.08-0.12 mm; the moisture content is controlled to 10%-12% by steaming and drying.
3. The paint door production process according to claim 1 is characterized in that: In step 2, modified white latex is used for bonding the veneer to the polypropylene fiber cloth and for hot pressing the composite veneer to the density board. The preparation method of the modified white latex is as follows: chitosan is added to the polyvinyl alcohol solution and mixed and stirred evenly as an emulsifier system; ethylene vinyl acetate, versatate vinyl carbonate and initiator solution are slowly added dropwise to the diluted emulsifier system at 75-85°C; after the addition is completed, the temperature is kept warm for full polymerization; then the temperature is cooled to room temperature, dibutyl phthalate and octanol are added and stirred evenly to obtain an emulsion; finally, melamine formaldehyde resin is added to the obtained emulsion and fully dispersed to obtain the modified white latex.
4. The paint door production process according to claim 3 is characterized in that: The raw materials for preparing the modified white latex are as follows by weight: 3-9 parts of polyvinyl alcohol, 0.5-2 parts of chitosan, 45-68 parts of ethylene vinyl acetate, 7-14 parts of versatate vinyl carbonate, 0.2-0.5 parts of initiator, 2-6 parts of dibutyl phthalate, 1-3 parts of octanol, 6-12 parts of melamine formaldehyde resin and sufficient water.
5. The paint door production process according to claim 1 is characterized in that: The thickness of the composite veneer in step 2 is 0.16-0.2 mm, and hot pressing bonding refers to bonding one side of the composite veneer polypropylene fiber cloth to the density board.
6. The paint door production process according to claim 5 is characterized in that: The parameters of the hot pressing bonding are: temperature 120-135° C., pressure 5-6 MPa, and time 10-15 min.
7. The paint door production process according to claim 1 is characterized in that: The hardness of the paint used for UV roller coating in step 3 is not less than 3H.
8. The paint door production process according to claim 1 is characterized in that: In step 4, the paint panel and core material are cold pressed using two-component plywood glue.
9. The paint door production process according to claim 1, characterized in that: The cold pressing parameters in step 4 are: pressure 7.4-8 MPa, processing time 10-14 h.
Citation Information
Patent Citations
Method for prolonging refreshing time of yellow peach slices
CN102669266A
Preparation method of titanium dioxide-graphene composite nano paper
CN103086373A
Method of improving removal rate of gummy substances in waste cardboard paper
CN103669066A
sealing interface for an air drying cartridge and a base for an air drying cartridge