Method for treating and recycling waste acid in perfume synthesis process
By using liquid sulfur dioxide for blow-off treatment and multi-stage spray treatment during fragrance synthesis, combined with special adsorbents, the problem of poor waste acid treatment during fragrance synthesis is solved, and efficient waste acid separation and concentration is achieved , improves the purity and yield of nitric acid, reduces costs, and promotes green and clean production.
Patent Information
- Application Number
- CN202411119892.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-15
- Publication Date
- 2024-11-12
AI Technical Summary
The prior art has poor treatment effect of waste acid during the fragrance synthesis process, resulting in poor concentration effect and difficulty in ensuring purity.
By adding liquid sulfur dioxide to the pretreatment kettle for blow-off treatment, nitrogen oxide gas is generated and adsorbed. Combined with multi-stage spraying treatment, high concentration of sulfuric acid and concentrated nitric acid are obtained respectively, and special adsorbents are prepared to minimize the The interference of sulfur dioxide gas on nitric acid.
It realizes efficient separation and concentration of waste acid, improves the yield and purity of nitric acid, reduces the cost of waste acid treatment, and has a more environmentally friendly and clean process.
Smart Images

Figure CN118929585A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field related to the recycling of perfume production waste, and in particular to a method for treating and reusing waste acid in a perfume synthesis process. Background Art
[0002] Commonly used nitro musks include xylene musk and ketone musk. Ketone musk is 3,5-dinitro-2,6-dimethyl-4-tert-butylacetophenone, a type of nitro musk, with a soft musk aroma, elegant fragrance, and long-lasting fragrance. Therefore, it is widely used in daily chemical products such as perfumes, cosmetics, and detergents.
[0003] In industrial production, the synthesis of nitromusk requires acetylation and nitration. In the nitration process, fuming nitric acid is used as a nitrating agent and sulfuric acid is used as a catalyst. After the nitration reaction, a large amount of waste acid is generated, mainly including unreacted nitric acid and sulfuric acid and some solid residues. At present, the general treatment method of waste acid is to separate sulfuric acid and nitric acid from the waste acid by steam stripping, distillation, etc., and then process and concentrate them separately. The sulfuric acid and nitric acid obtained by these methods have poor concentration effects and the purity is difficult to guarantee.
[0004] The treatment of spice waste acid urgently requires the design of a treatment method with good concentration effect and high purity of recovered materials. Summary of the invention
[0005] 1. Technical issues to be resolved
[0006] In view of the deficiencies of the prior art, the present invention provides a method for treating and reusing waste acid in a fragrance synthesis process.
[0007] (II) Technical solution
[0008] To achieve the above objectives, the present invention is implemented through the following technical solutions:
[0009] The method for treating and reusing waste acid in the fragrance synthesis process comprises the following steps:
[0010] S1: By weight, 100 parts of 3% dilute sulfuric acid and 200 parts of waste acid liquid produced in the fragrance synthesis process are pumped into the pretreatment kettle, and then mixed evenly, and the temperature in the pretreatment kettle is controlled to be 40-60°C;
[0011] S2: Open the inlet valve of liquid sulfur dioxide, slowly add liquid sulfur dioxide into the pretreatment kettle of S1, control the pressure in the pretreatment kettle to 0.3-0.5Mpa, stir evenly until nitrogen oxide gas is generated, and perform stripping treatment. The nitrogen oxide gas is adsorbed through the transmission channel, and the transmission channel is filled with adsorbent;
[0012] S3: When no gas is generated in the pretreatment kettle in S2, the reaction is finished, the inlet valve is closed, and a sulfuric acid solution is obtained in the pretreatment kettle. The obtained sulfuric acid solution is pumped into a primary sulfuric acid concentration kettle, concentrated into concentrated sulfuric acid after flash evaporation, and then enters a secondary sulfuric acid concentration kettle to obtain high-concentration sulfuric acid, and the mass concentration of the high-concentration sulfuric acid is 99.2%;
[0013] S4: The nitrogen oxide gas adsorbed in S2 is sent to a spray tower for multi-stage spray treatment. The spray liquid is clean water. The spray treatment temperature is 20-45°C. Finally, dilute nitric acid is obtained in the absorption kettle. A small amount of residual nitrogen oxide gas is introduced into the spray tower again to form dilute nitric acid. All the formed dilute nitric acid is sent to a nitric acid concentration kettle for concentration. After concentration, it is pumped into a concentrated nitric acid storage tank to obtain concentrated nitric acid with a mass concentration of 99.0%.
[0014] Furthermore, the preparation method of the adsorbent comprises the following steps:
[0015] A1: Dissolve 3-5 parts of ferric nitrate, 0.2-0.4 parts of copper nitrate and 0.06-0.1 parts of calcium chloride in 50 parts of water to obtain a mixed salt solution.
[0016] A2: Pour 0.4-0.6 parts of dextrin, 20-30 parts of modified zeolite powder and 0.6-1 parts of modified pulverized coal powder into the mixed salt solution obtained in A1 in sequence, and stir until the mixture is uniform to form a primary mixture;
[0017] A3: The primary mixture obtained in A2 is pressed and transferred to a sintering furnace, and argon protection is introduced. The heating rate is set to 1-3°C / min, the temperature is increased to 400-500°C, maintained for 1-2h, and naturally cooled to room temperature. The mixture is crushed to a particle size of less than 0.3mm to obtain an adsorbent.
[0018] Furthermore, the preparation method of the modified zeolite powder includes the following steps: adding 1 part of zeolite powder with a particle size not greater than 40 meshes to 2 to 4 parts of a potassium carbonate solution with a mass fraction of 20 to 30%, stirring evenly, hydrothermally crystallizing at 140 to 160° C. for 2 to 3 hours, filtering and drying to obtain the modified zeolite powder.
[0019] Furthermore, the preparation method of the modified fly ash comprises the following steps: by weight, adding 1 part of fly ash to 2 to 4 parts of 1.2 to 1.8% sodium carboxymethyl cellulose solution, heating to 80 to 95° C., soaking for 0.5 to 1.5 hours, filtering, and obtaining modified fly ash.
[0020] Furthermore, the particle size of the modified pulverized coal is ≤2 mm.
[0021] After adopting the above technical solution, the present invention has the following beneficial effects compared with the prior art:
[0022] 1. The present invention effectively separates sulfuric acid and nitric acid in waste acid by adding liquid sulfur dioxide, and further performs multiple spraying and cyclic spraying treatment on the generated nitrogen oxide gas, so that the nitrogen oxide gas is fully absorbed and converted by water, thereby effectively reducing the loss of nitrogen oxide gas and improving the yield of nitric acid.
[0023] 2. The present invention provides a special adsorbent for adsorbing nitrogen oxide gas so that a small amount of sulfur dioxide gas carried by the nitrogen oxide gas is fully adsorbed, thereby minimizing the interference of sulfur dioxide gas on nitric acid solution, and ultimately achieving the purpose of reducing the sulfuric acid content in concentrated nitric acid.
[0024] 3. The present invention provides an efficient treatment method for waste acid from nitration of synthetic fragrances, thereby obtaining high-concentration sulfuric acid and concentrated nitric acid, which is beneficial to green and clean production. At the same time, this treatment process reduces the cost of waste acid treatment and improves economic benefits. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] Figure 1 The present invention is a process flow chart of the method for treating and reusing waste acid generated in the fragrance synthesis process. DETAILED DESCRIPTION
[0026] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments. The following description of at least one exemplary embodiment is actually only illustrative and is by no means intended to limit the present invention and its application or use. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0027] Embodiment 1:
[0028] The method for treating and reusing waste acid in the fragrance synthesis process comprises the following steps:
[0029] S1: 100 parts by weight of 3% dilute sulfuric acid and 200 parts of waste acid liquid produced in the fragrance synthesis process are pumped into the pretreatment kettle, and then mixed evenly, and the temperature in the pretreatment kettle is controlled to be 50°C;
[0030] S2: Open the inlet valve of liquid sulfur dioxide, slowly add liquid sulfur dioxide into the pretreatment kettle of S1, control the pressure in the pretreatment kettle to 0.4Mpa, stir evenly until nitrogen oxide gas is generated, and perform stripping treatment. The nitrogen oxide gas is adsorbed through the transmission channel, and the transmission channel is filled with adsorbent.
[0031] S3: When no gas is generated in the pretreatment kettle in S2, the reaction is finished, the inlet valve is closed, and a sulfuric acid solution is obtained in the pretreatment kettle. The obtained sulfuric acid solution is pumped into a primary sulfuric acid concentration kettle, concentrated into concentrated sulfuric acid after flash evaporation, and then enters a secondary sulfuric acid concentration kettle to obtain high-concentration sulfuric acid, and the mass concentration of the high-concentration sulfuric acid is 99.2%;
[0032] S4: The adsorbed nitrogen oxide gas in S2 is sent to a spray tower for multi-stage spray treatment. The spray liquid is clean water. The spray treatment temperature is 30°C. Finally, dilute nitric acid is obtained in the absorption kettle. A small amount of residual nitrogen oxide gas is introduced into the spray tower again to form dilute nitric acid. All the formed dilute nitric acid is sent to a nitric acid concentration kettle for concentration. After concentration, it is pumped into a concentrated nitric acid storage tank to obtain concentrated nitric acid with a mass concentration of 99.0%.
[0033] The preparation method of the adsorbent comprises the following steps:
[0034] A1: Dissolve 4 parts of ferric nitrate, 0.3 parts of copper nitrate and 0.08 parts of calcium chloride in 50 parts of water to obtain a mixed salt solution.
[0035] A2: Pour 0.5 parts of dextrin, 25 parts of modified zeolite powder and 0.8 parts of modified pulverized coal powder into the mixed salt solution obtained in A1 in sequence, and stir until the mixture is uniform to form a primary mixture;
[0036] A3: The primary mixture obtained in A2 was pressed and transferred to a sintering furnace, and argon protection was introduced. The heating rate was set to 2°C / min, the temperature was increased to 450°C, maintained for 1 hour, and naturally cooled to room temperature. The mixture was crushed to a particle size of less than 0.3 mm to obtain an adsorbent.
[0037] The preparation method of modified zeolite powder comprises the following steps: adding 1 part of zeolite powder with a particle size not greater than 40 meshes to 3 parts of 25% potassium carbonate solution by weight, stirring evenly, hydrothermally crystallizing at 150° C. for 2 hours, filtering and drying to obtain modified zeolite powder.
[0038] The preparation method of modified fly ash comprises the following steps: adding 1 part of fly ash to 3 parts of 1.5% sodium carboxymethyl cellulose solution by weight, heating to 90°C, soaking for 1 hour, filtering, and crushing to a particle size of less than 2 mm to obtain modified fly ash.
[0039] Example 2
[0040] The method for treating and reusing waste acid in the fragrance synthesis process comprises the following steps:
[0041] S1: By weight, 100 parts of 3% dilute sulfuric acid and 200 parts of waste acid liquid produced in the fragrance synthesis process are pumped into the pretreatment kettle, and then mixed evenly, and the temperature in the pretreatment kettle is controlled to 40°C;
[0042] S2: Open the inlet valve of liquid sulfur dioxide, slowly add liquid sulfur dioxide into the pretreatment kettle of S1, control the pressure in the pretreatment kettle to 0.3Mpa, stir evenly until nitrogen oxide gas is generated, and perform stripping treatment. The nitrogen oxide gas is adsorbed through the transmission channel, and the transmission channel is filled with adsorbent.
[0043] S3: When no gas is generated in the pretreatment kettle in S2, the reaction is finished, the inlet valve is closed, and a sulfuric acid solution is obtained in the pretreatment kettle. The obtained sulfuric acid solution is pumped into a primary sulfuric acid concentration kettle, concentrated into concentrated sulfuric acid after flash evaporation, and then enters a secondary sulfuric acid concentration kettle to obtain high-concentration sulfuric acid, and the mass concentration of the high-concentration sulfuric acid is 98.7%;
[0044] S4: The adsorbed nitrogen oxide gas in S2 is sent to a spray tower for multi-stage spray treatment. The spray liquid is clean water. The spray treatment temperature is 20°C. Finally, dilute nitric acid is obtained in the absorption kettle. A small amount of residual nitrogen oxide gas is introduced into the spray tower again to form dilute nitric acid. All the formed dilute nitric acid is sent to a nitric acid concentration kettle for concentration. After concentration, it is pumped into a concentrated nitric acid storage tank to obtain concentrated nitric acid with a mass concentration of 98.9%.
[0045] The preparation method of the adsorbent comprises the following steps:
[0046] A1: Dissolve 3 parts of ferric nitrate, 0.2 parts of copper nitrate and 0.06 parts of calcium chloride in 50 parts of water to obtain a mixed salt solution.
[0047] A2: Pour 0.4 parts of dextrin, 20 parts of modified zeolite powder and 0.6 parts of modified pulverized coal powder into the mixed salt solution obtained in A1 in sequence, and stir until the mixture is uniform to form a primary mixture;
[0048] A3: The primary mixture obtained in A2 was pressed and transferred to a sintering furnace, and argon protection was introduced. The heating rate was set to 1°C / min, the temperature was increased to 400°C, maintained for 1 hour, and naturally cooled to room temperature. The mixture was crushed to a particle size of less than 0.3 mm to obtain an adsorbent.
[0049] The preparation method of modified zeolite powder comprises the following steps: adding 1 part of zeolite powder with a particle size not greater than 40 meshes to 2 parts of 20% potassium carbonate solution by weight, stirring evenly, hydrothermally crystallizing at 140° C. for 2 hours, filtering and drying to obtain modified zeolite powder.
[0050] The preparation method of modified fly ash comprises the following steps: adding 1 part of fly ash to 2 parts of 1.2% sodium carboxymethyl cellulose solution by weight, heating to 80°C, soaking for 0.5h, filtering, and crushing to a particle size of less than 2mm to obtain modified fly ash.
[0051] Example 3
[0052] The method for treating and reusing waste acid in the fragrance synthesis process comprises the following steps:
[0053] S1: 100 parts by weight of 3% dilute sulfuric acid and 200 parts of waste acid liquid produced in the fragrance synthesis process are pumped into the pretreatment kettle, and then mixed evenly, and the temperature in the pretreatment kettle is controlled to be 60°C;
[0054] S2: Open the inlet valve of liquid sulfur dioxide, slowly add liquid sulfur dioxide into the pretreatment kettle of S1, control the pressure in the pretreatment kettle to 0.5Mpa, stir evenly until nitrogen oxide gas is generated, and perform stripping treatment. The nitrogen oxide gas is adsorbed through the transmission channel, and the transmission channel is filled with adsorbent.
[0055] S3: When no gas is generated in the pretreatment kettle in S2, the reaction is finished, the inlet valve is closed, and a sulfuric acid solution is obtained in the pretreatment kettle. The obtained sulfuric acid solution is pumped into a primary sulfuric acid concentration kettle, concentrated into concentrated sulfuric acid after flash evaporation, and then enters a secondary sulfuric acid concentration kettle to obtain high-concentration sulfuric acid, and the mass concentration of the high-concentration sulfuric acid is 98.9%;
[0056] S4: The adsorbed nitrogen oxide gas in S2 is sent to a spray tower for multi-stage spray treatment. The spray liquid is clean water. The spray treatment temperature is 45°C. Finally, dilute nitric acid is obtained in the absorption kettle. A small amount of residual nitrogen oxide gas is introduced into the spray tower again to form dilute nitric acid. All the formed dilute nitric acid is sent to a nitric acid concentration kettle for concentration. After concentration, it is pumped into a concentrated nitric acid storage tank to obtain concentrated nitric acid with a mass concentration of 99.1%.
[0057] The preparation method of the adsorbent comprises the following steps:
[0058] A1: Dissolve 5 parts of ferric nitrate, 0.4 parts of copper nitrate and 0.1 parts of calcium chloride in 50 parts of water to obtain a mixed salt solution.
[0059] A2: Pour 0.6 parts of dextrin, 30 parts of modified zeolite powder and 1 part of modified pulverized coal powder into the mixed salt solution obtained in A1 in sequence, and stir until the mixture is uniform to form a primary mixture;
[0060] A3: The primary mixture obtained in A2 was pressed and transferred to a sintering furnace, and argon protection was introduced. The heating rate was set to 3°C / min, the temperature was increased to 500°C, maintained for 2h, and naturally cooled to room temperature. The mixture was crushed to a particle size of less than 0.3mm to obtain an adsorbent.
[0061] The preparation method of modified zeolite powder comprises the following steps: adding 1 part of zeolite powder with a particle size not greater than 40 meshes to 4 parts of 30% potassium carbonate solution by weight, stirring evenly, hydrothermally crystallizing at 160° C. for 3 hours, filtering and drying to obtain modified zeolite powder.
[0062] The preparation method of modified fly ash comprises the following steps: adding 1 part of fly ash to 4 parts of 1.8% sodium carboxymethyl cellulose solution by weight, heating to 95°C, soaking for 1.5 hours, filtering, and crushing to a particle size of less than 2 mm to obtain modified fly ash.
[0063] Comparative Example 1
[0064] Compared with Example 1, in the preparation of the adsorbent, the modified zeolite powder was replaced by unmodified zeolite powder.
[0065] The preparation method of the adsorbent comprises the following steps:
[0066] A1: Dissolve 4 parts of ferric nitrate, 0.3 parts of copper nitrate and 0.08 parts of calcium chloride in 50 parts of water to obtain a mixed salt solution.
[0067] A2: Pour 0.5 parts of dextrin, 25 parts of zeolite powder and 0.8 parts of modified pulverized coal powder into the mixed salt solution obtained in A1 in sequence, and stir until the mixture is uniform to form a primary mixture;
[0068] A3: The primary mixture obtained in A2 was pressed and transferred to a sintering furnace, and argon protection was introduced. The heating rate was set to 2°C / min, the temperature was increased to 450°C, maintained for 1 hour, and naturally cooled to room temperature. The mixture was crushed to a particle size of less than 0.3 mm to obtain an adsorbent.
[0069] Comparative Example 2
[0070] Compared with Example 1, in the preparation of the adsorbent, the modified fly ash is replaced by unmodified fly ash.
[0071] The preparation method of the adsorbent comprises the following steps:
[0072] A1: Dissolve 4 parts of ferric nitrate, 0.3 parts of copper nitrate and 0.08 parts of calcium chloride in 50 parts of water to obtain a mixed salt solution.
[0073] A2: Pour 0.5 parts of dextrin, 25 parts of modified zeolite powder and 0.8 parts of pulverized coal powder into the mixed salt solution obtained in A1 in sequence, and stir until the mixture is uniform to form a primary mixture;
[0074] A3: The primary mixture obtained in A2 was pressed and transferred to a sintering furnace, and argon protection was introduced. The heating rate was set to 2°C / min, the temperature was increased to 450°C, maintained for 1 hour, and naturally cooled to room temperature. The mixture was crushed to a particle size of less than 0.3 mm to obtain an adsorbent.
[0075] Comparative Example 3
[0076] Compared with Example 1, in the preparation of the adsorbent, the modified zeolite powder is replaced by unmodified zeolite powder, and the modified fly ash is replaced by unmodified fly ash.
[0077] The preparation method of the adsorbent comprises the following steps:
[0078] A1: Dissolve 4 parts of ferric nitrate, 0.3 parts of copper nitrate and 0.08 parts of calcium chloride in 50 parts of water to obtain a mixed salt solution.
[0079] A2: Pour 0.5 parts of dextrin, 25 parts of zeolite powder and 0.8 parts of pulverized coal powder into the mixed salt solution obtained in A1 in sequence, and stir until the mixture is uniform to form a primary mixture;
[0080] A3: The primary mixture obtained in A2 was pressed and transferred to a sintering furnace, and argon protection was introduced. The heating rate was set to 2°C / min, the temperature was increased to 450°C, maintained for 1 hour, and naturally cooled to room temperature. The mixture was crushed to a particle size of less than 0.3 mm to obtain an adsorbent.
[0081] The process diagram of the present invention is as follows Figure 1 .
[0082] The content of sulfuric acid in the concentrated nitric acid finally prepared and recovered is measured and shown in Table 1.
[0083] Table 1
[0084]
[0085]
[0086] The content of sulfuric acid in the concentrated nitric acid prepared in Examples 1 to 3 shows that the nitric acid prepared and recovered by the technical solution of the present invention has high purity.
[0087] Comparative Example 1 Compared with Example 1, in the preparation of the adsorbent, the modified zeolite powder was replaced by unmodified zeolite powder.
[0088] The content of sulfuric acid in the concentrated nitric acid in Example 1 is 0.08%, and the content of sulfuric acid in the concentrated nitric acid in Comparative Example 1 is 0.46%. It can be clearly seen that the content of sulfuric acid in the concentrated nitric acid obtained after the final treatment of the waste acid in Comparative Example 1 is higher than the content of sulfuric acid in the concentrated nitric acid obtained after the final treatment of the waste acid in Example 1.
[0089] The above results show that the zeolite powder modified by the technical solution of the present invention can improve the adsorption effect of the adsorbent and thus increase the recovery rate of concentrated nitric acid.
[0090] Comparative Example 2 Compared with Example 1, in the preparation of the adsorbent, the modified fly ash was replaced by unmodified fly ash.
[0091] The content of sulfuric acid in the concentrated nitric acid in Example 1 is 0.08%, and the content of sulfuric acid in the concentrated nitric acid in Comparative Example 2 is 0.51%. It can be clearly seen that the content of sulfuric acid in the concentrated nitric acid obtained after the final treatment of the waste acid in Comparative Example 2 is higher than the content of sulfuric acid in the concentrated nitric acid obtained after the final treatment of the waste acid in Example 1.
[0092] The above results show that the fly ash modified by the technical solution of the present invention can improve the adsorption effect of the adsorbent and thus increase the recovery rate of concentrated nitric acid.
[0093] Comparative Example 3 Compared with Example 1, in the preparation of the adsorbent, the modified zeolite powder is replaced by unmodified zeolite powder, and the modified fly ash is replaced by unmodified fly ash.
[0094] The content of sulfuric acid in the concentrated nitric acid in Example 1 is 0.08%, and the content of sulfuric acid in the concentrated nitric acid in Comparative Example 3 is 0.67%. It can be clearly seen that the content of sulfuric acid in the concentrated nitric acid obtained after the final treatment of the waste acid in Comparative Example 3 is higher than the content of sulfuric acid in the concentrated nitric acid obtained after the final treatment of the waste acid in Example 1.
[0095] Combining Comparative Examples 1 and 2, it can be concluded that the zeolite powder and fly ash modified by the technical solution of the present invention have a positive synergistic effect in enhancing the adsorption effect of the adsorbent.
[0096] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.
Claims
1. A method for treating and reusing waste acid in a fragrance synthesis process, characterized in that: The following steps are involved: S1: By weight, 100 parts of 3% dilute sulfuric acid and 200 parts of waste acid liquid produced in the fragrance synthesis process are pumped into the pretreatment kettle, and then mixed evenly, and the temperature in the pretreatment kettle is controlled to be 40-60°C; S2: Open the inlet valve of liquid sulfur dioxide, add liquid sulfur dioxide into the pretreatment kettle of S1, control the pressure in the pretreatment kettle to 0.3-0.5Mpa, stir evenly until nitrogen oxide gas is generated, and perform stripping treatment. The nitrogen oxide gas is adsorbed through the transmission channel, and the transmission channel is filled with adsorbent; S3: When no gas is generated in the pretreatment kettle in S2, the reaction is finished, the inlet valve of the liquid sulfur dioxide is closed, and a sulfuric acid solution is obtained in the pretreatment kettle. The obtained sulfuric acid solution is pumped into a sulfuric acid concentration kettle, and concentrated after flash evaporation to obtain high-concentration sulfuric acid; S4: The adsorbed nitrogen oxide gas in S2 is sent to a spray tower for multi-stage spray treatment. The spray liquid is clean water. The spray treatment temperature is 20-45°C. Finally, dilute nitric acid is obtained in the spray tower. The dilute nitric acid is sent to a nitric acid concentration kettle for concentration to obtain concentrated nitric acid, which is then pumped into a concentrated nitric acid storage tank.
2. The method for treating waste acid in the fragrance synthesis process according to claim 1, characterized in that: The preparation method of the adsorbent comprises the following steps: A1: Dissolve 3-5 parts of ferric nitrate, 0.2-0.4 parts of copper nitrate and 0.06-0.1 parts of calcium chloride in 50 parts of water to obtain a mixed salt solution. A2: Pour 0.4-0.6 parts of dextrin, 20-30 parts of modified zeolite powder and 0.6-1 parts of modified pulverized coal powder into the mixed salt solution obtained in A1 in sequence, and stir until the mixture is uniform to form a primary mixture; A3: The primary mixture obtained in A2 is pressed and transferred to a sintering furnace, and argon protection is introduced. The heating rate is set to 1-3°C / min, the temperature is increased to 400-500°C, maintained for 1-2h, and naturally cooled to room temperature. The mixture is crushed to a particle size of less than 0.3mm to obtain an adsorbent.
3. The method for treating waste acid in the fragrance synthesis process according to claim 2, characterized in that: The preparation method of the modified zeolite powder comprises the following steps: adding 1 part of zeolite powder with a particle size of no more than 40 meshes to 2-4 parts of potassium carbonate solution with a mass fraction of 20-30%, stirring evenly, hydrothermally crystallizing at 140-160° C. for 2-3 hours, filtering and drying to obtain the modified zeolite powder.
4. The method for treating waste acid in the fragrance synthesis process according to claim 2, characterized in that: The preparation method of the modified fly ash comprises the following steps: by weight, adding 1 part of fly ash to 2-4 parts of sodium carboxymethyl cellulose solution with a mass fraction of 1.2-1.8%, heating to 80-95° C., soaking for 0.5-1.5 hours, filtering, and crushing to obtain modified fly ash.
5. The method for treating waste acid in the fragrance synthesis process according to claim 4, characterized in that: The particle size of the modified fly ash is ≤2mm.
Citation Information
Patent Citations
Sulfur dioxide adsorbent and preparation method thereof
CN111545162A
Mixed acid waste liquid resource recycling system and process
CN111960392A
Perfluorohydrocarbon adsorption material as well as preparation method and application thereof
CN118403610A
Preparation method of compound absorbent for removing nitrogen oxide
CN1994554A
Method of reprocessing waste acid containing nitric and sulphuric acid