Method for treating wastewater containing high-concentration Cu (II)-EDTA (Ethylene Diamine Tetraacetic Acid) with high efficiency and low cost by ball-milling zero-valent manganese
The zero-valent manganese is modified by ball milling method to form ball milling zero-valent manganese (ZVMnbm), which solves the problems of low efficiency and high cost of Cu(II)-EDTA wastewater treatment in the prior art, and achieves high efficiency and low cost Cu(II) )-EDTA removal significantly improves removal efficiency and reduces energy consumption.
Patent Information
- Application Number
- CN202410995928.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-24
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2044-07-24
AI Technical Summary
The prior art is difficult to efficiently and at low cost to treat high concentrations of Cu(II)-EDTA wastewater, and in practical applications, zero-valent manganese is hindered by the oxide layer, resulting in low removal efficiency and high cost.
The commercial manganese powder is surface modified by ball milling to form ball mill zero-valent manganese (ZVMnbm). Using its large specific surface area and strong redox capacity, Cu(II)-EDTA was removed. The diameter of the ball mill beads was 2-6mm and the rotation speed was 200. -800rpm, ball milling time is 0.5-4 hours, add wastewater and stir, significantly weaken the oxide layer and improve electron transfer efficiency.
A Cu(II)-EDTA removal rate of 98% was achieved, reducing energy consumption and cost, significantly improving removal efficiency, simple operation, suitable for large-scale promotion, and has good environmental adaptability and economic benefits.
Smart Images

Figure CN118929883A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of environmental remediation of industrial heavy metal wastewater, and in particular to a method for efficiently and low-costly treating wastewater containing high-concentration Cu(II)-EDTA by ball milling zero-valent manganese. Background Art
[0002] This section merely provides background information related to the present disclosure and is not necessarily prior art.
[0003] With the progress of industry and the development of society, heavy metal pollution has become a hot spot and difficulty for national key governance. According to statistics, the heavy metal wastewater generated by the electroplating industry alone in my country is as high as about 4 billion tons per year, mainly including copper (Cu), nickel (Ni), cadmium (Cd), etc. The presence of complexing agents (pesticides, fertilizers, detergents, plasticizers, etc.) makes the composition of industrial heavy metal wastewater more complicated. Heavy metal ions are easily combined with organic ligands such as ethylenediaminetetraacetic acid (EDTA), nitrotriacetic acid (NTA), humic acid (HA), citric acid (CA), etc. to form stable metal complexes with different structures and toxicities. Therefore, in addition to existing in the form of ions, more than 90% of the heavy metals in wastewater are in the form of complexes. This stable heavy metal complex is not biodegradable, and at the same time has natural persistence and bioaccumulation. Once it enters higher organisms through bioaccumulation, it is difficult to be excreted naturally or completely eliminated from the organism. It will react with proteins or enzymes in the organism to make them inactive, damage internal organs, cause acute, subacute and chronic poisoning, and cause irreversible damage to the organism.
[0004] Cu(Ⅱ)-EDTA is a typical pollutant in electroplating wastewater. 2+ It forms a stable complex with EDTA in a molar ratio of 1:1. EDTA contains 4 carboxyl groups and 2 amine groups. 2+ The stability constant of the formed complex is as high as 18.7. As one of the essential elements for the human body, copper plays a vital role in the human body, but excessive intake can lead to acute copper poisoning, and in severe cases can lead to hepatitis, hypotension, acute renal failure and even death. Compared with metal ions, complex copper is more toxic to the environment and microorganisms due to the stable coordination bond formed with EDTA.
[0005] In previous studies, similar to the removal methods of most free heavy metals, the removal technologies of complexed heavy metals also include electrolysis, adsorption, photocatalysis, etc. However, in the actual operation process, it is necessary to consider the treatment effect and operating cost, and to avoid the introduction of secondary pollutants. Electrolysis technology consumes a lot of energy and is prone to residual organic ligands, leading to secondary pollution. The adsorption method is reliable and economical. It produces less sludge than the coagulation-filtration method. It has been widely used in the treatment and remediation of heavy metal-containing water bodies, but the adsorbent will reach adsorption saturation and must be regenerated. In addition, there are membrane separation methods such as reverse osmosis, but they all have disadvantages such as high cost, high energy consumption, and difficult operation to varying degrees.
[0006] As a green remediation material, zero-valent metals have large specific surface area and strong electron-donating ability, and are widely used in water purification processes. Manganese is one of the high-abundance elements in the first transition series and one of the most active and important geochemical elements. Mn has a rich valence state, ranging from 0 to +7, and its electronic structure is 3d 5 4s 2 , the redox potential is -1.18V, it has a strong affinity for oxygen, and has a reducing and fixing effect on most heavy metal ions in water. 0 The surface is easily oxidized to form MnO x @Mn 0 The core-shell structure has a more lasting catalytic activity than manganese oxide and has a strong adsorption capacity for heavy metals and organic matter.
[0007] However, in actual application, we found that zero-valent manganese also has many defects. The surface oxide layer will greatly hinder the outward transfer of internal electrons, resulting in reduced reduction activity for target pollutants. Compared with chemical modification, the method of surface modification of zero-valent manganese by mechanical ball milling is easy to promote and apply on a large scale because of its simple operation, low cost, and no waste liquid. Summary of the invention
[0008] Purpose of the invention: The technical problem to be solved by the present invention is to provide a method for treating wastewater containing high concentration of Cu(II)-EDTA with high efficiency and low cost by ball milling zero-valent manganese in view of the shortcomings of the prior art.
[0009] In order to solve the above technical problems, the present invention discloses the following technical solutions:
[0010] Application of zero-valent manganese in removing Cu(Ⅱ)-EDTA, specifically a ball-milled zero-valent manganese (ZVMn bm ) A method for efficiently and cost-effectively treating wastewater containing high concentration of Cu(Ⅱ)-EDTA.
[0011] Wherein, the zero-valent manganese is manganese powder obtained by ball milling; the manganese powder is commercial manganese powder.
[0012] Wherein, the ball milling beads are stainless steel ball milling beads.
[0013] The diameter of the ball milling beads is 2-6 mm, preferably 2-4 mm and 4.1-6 mm, and preferably 3 mm and 5 mm.
[0014] Furthermore, the ratio of the number of ball milling beads with a diameter of 2-4 mm to the number of ball milling beads with a diameter of 4.1-6 mm is 1-3:1, preferably 2:1.
[0015] Among them, 15-25 ball milling beads with a diameter of 4.1-6 mm and 35-45 ball milling beads with a diameter of 2-4 mm are used for every 4 g of manganese powder, preferably 20 ball milling beads with a diameter of 5 mm and 40 ball milling beads with a diameter of 3 mm.
[0016] Wherein, the total ball milling time is 0.5-4h, preferably 1.5-3h, preferably 2h.
[0017] Wherein, the rotation speed of the ball mill is 200-800 rpm, preferably 300-600 rpm, preferably 350-500 rpm.
[0018] The ball milling is performed using a planetary ball mill, and the direction of the ball milling is changed every 20-40 minutes, preferably every 30 minutes. The operating power of the ball mill is 20-46W, such as 25W, 30W, 35W, 40W, preferably 33.33W.
[0019] Among them, ball milled zero-valent manganese (ZVMn bm ) is added to wastewater containing Cu(II)-EDTA to remove Cu(II)-EDTA; wherein stirring, such as mechanical stirring, is performed during the process of removing Cu(II)-EDTA.
[0020] Wherein, the mass ratio of zero-valent manganese to Cu(II)-EDTA is 8-12:1, preferably 10:1.
[0021] Wherein, the zero-valent manganese removes Cu(II)-EDTA under the condition of an initial pH of 2-5, such as the initial pH of the reaction is 3.4.
[0022] The ball-milled zero-valent manganese (ZVMn bm ) Store in an inert gas until needed.
[0023] The ball-milled zero-valent manganese (ZVMn bm ) The removal rate of Cu(Ⅱ)-EDTA and Cu(Ⅱ) was as high as 98% within 5 minutes.
[0024] Beneficial effects:
[0025] 1. The method of the present invention utilizes ball milling to weaken the outer oxide layer of commercial manganese powder, and the electrons of the internal zero-valent manganese are efficiently transferred outward, and the pollutants adsorbed on the outside are captured and utilized, thereby reducing the pollutants.
[0026] 2. Ball-milled zero-valent manganese (ZVMn) synthesized by the method of the present invention bm )The removal effect of high-concentration Cu(Ⅱ)-EDTA is better than that of unmodified zero-valent manganese (ZVMn) material, which significantly improves the removal efficiency and reduces energy consumption.
[0027] 3. The method of the present invention is used to prepare ball-milled zero-valent manganese (ZVMn bm ) The reaction conditions are less restricted and can be carried out at room temperature and pressure.
[0028] 4. The method of the present invention is simple in technology, strong in practicability, mild in reaction conditions, easy in construction and operation, has low requirements on equipment, is conducive to large-scale promotion, and has significant economic and environmental benefits. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] The present invention will be further described in detail below in conjunction with the accompanying drawings and specific embodiments, and the above and / or other advantages of the present invention will become more clear.
[0030] Figure 1 is ZVMn in Example 1 bm XRD pattern of .
[0031] Figure 2 is ZVMn in Example 1 bm and SEM images of ZVMn.
[0032] Figure 3 is ZVMn in Example 2 bm Comparison of the removal effects of ZVMn and ZVMn on Cu(Ⅱ)-EDTA.
[0033] Figure 4 is ZVMn in Example 2 bm Comparison of the removal effects of ZVMn and ZVMn on Cu(Ⅱ).
[0034] Figure 5 is ZVMn in Example 2 bm Comparison of the recovery effects of ZVMn and ZVMn on Cu(Ⅱ).
[0035] Figure 6 is ZVMn in Example 2 bm SEM-mapping comparison chart before and after the reaction.
[0036] Figure 7 is ZVMn in Example 2 bm Energy consumption comparison chart with ZVMn.
[0037] Figure 8 The different inorganic anions in Example 3 are ZVMn bm Comparison of the effects of treating wastewater containing high concentration of Cu(Ⅱ)-EDTA.
[0038] Fig. 9 The natural organic matter (HA) in Example 4 is ZVMn bm Comparison of the effects of treating wastewater containing high concentration of Cu(Ⅱ)-EDTA.
[0039] Fig.10 The effect of different initial pH values on ZVMn in Example 5 bm Comparison of the effects of treating wastewater containing high concentration of Cu(Ⅱ)-EDTA. DETAILED DESCRIPTION
[0040] The present invention can be better understood according to the following examples. However, it is easy for those skilled in the art to understand that the contents described in the examples are only used to illustrate the present invention, and should not and will not limit the present invention described in detail in the claims.
[0041] The experimental methods described in the following examples are conventional methods unless otherwise specified; the reagents and materials described are commercially available unless otherwise specified.
[0042] The main raw materials involved in the following examples, such as zero-valent manganese (ZVMn), were all from MacLean (Shanghai, China), and all reagents were of analytical grade, with a particle size of 200 mesh.
[0043] Example 1
[0044] This embodiment provides a method for ball milling zero-valent manganese, and the specific steps are as follows:
[0045] Weigh 4.0g zero-valent manganese and use a planetary ball mill from Nanjing Boyuntong Instrument Technology Co., Ltd. with a rotation speed of 400rpm, a ball milling time of 2h, an operating power of 33.33W, and a turn every 30min. The ball mill jar is filled with 20 medium-sized ball milling beads (with a diameter of 5mm) and 40 small ball milling beads (with a diameter of 3mm). The ball milling treatment causes a mass loss of 10.1% of ZVMn, and the treated sample is recorded as ZVMn bm , stored in inert gas.
[0046] from Figure 1 It can be seen that ball milling does not change the main phase of the material, and still maintains Mn 0 The phase structure of Figure 2 It can be seen that ball milling reduces the particle size of ZVMn, increases the specific surface area of the material, and is beneficial to the removal of pollutants.
[0047] Example 2
[0048] Add 100 ppm (i.e. 100 mg / L) Cu(II)-EDTA aqueous solution to a 100 mL beaker. The total volume of the reaction solution is 50 mL and the initial pH is 3.4. Add 0.05 g ZVMn bm Or ZVMn to a concentration of 1g / L, use mechanical stirring to mix in an open aerobic environment, place it on a constant temperature rotary mixer, set the speed to 200r / min, and the temperature to 25°C. Sampling is performed at regular intervals to determine the residual amount of Cu(Ⅱ)-EDTA or Cu(Ⅱ) in the system.
[0049] The experimental results are as follows Figure 3 and Figure 4 As shown, ZVMn bm The removal rates of Cu(Ⅱ)-EDTA and Cu(Ⅱ) were 98% and 93% respectively within 5 min, which were higher than 54% and 38% of ZVMn. Figure 6 It can be seen that the copper element signal is significantly enhanced after the reaction, and copper recovery is achieved.
[0050] Energy consumption calculation: the unit price of commercial zero-price manganese is 1.01 yuan / gram, and the commercial electricity fee in Nanjing is 0.67 yuan / kWh. The calculation method is as follows: formula (1)(2)(3). Figure 7 The electricity cost of the ball mill running at 33.33W for 2 hours is 0.045 yuan. Considering the loss rate of 10.1% caused by ball milling, 4.45g of raw materials are needed to obtain 4g of processed samples. The material cost is 4.495 yuan. The total cost is 4.495+0.045=4.54 yuan (material cost + electricity cost). The unit sample processing fee is 4.54÷4=1.135 yuan / gram.
[0051] ZVMn bm Take 1L 100ppm Cu(Ⅱ)-EDTA wastewater as an example, using 1g / L ZVMn bm The removal rate of 100ppm Cu(Ⅱ)-EDTA in 5 minutes is 98%. Complete removal requires 1g / L×1L×100%÷98%=1.02g, and the cost is 1.02×1.135=1.158 yuan. The electricity cost of the constant temperature rotary mixer running at 860W for 5 minutes is 0.048 yuan. The above cost is calculated based on ZVMn bm The energy consumption required to treat 1L 100ppm Cu(Ⅱ)-EDTA wastewater is 1.158+0.048=1.206 yuan. It can be found that ball milling significantly reduces the energy consumption of the material and achieves low-cost treatment.
[0052]
[0053] After the reaction, ZVMnbm or ZVMn for recovery, dissolve in 0.1mol / L hydrochloric acid and dilute to 50mL, and measure the amount of Cu(II) recovered in the system. Figure 5 As shown, the recovery of Cu(II) by zero-valent manganese after ball milling can reach more than 90%, which is much higher than 35% of untreated zero-valent manganese.
[0054] Example 3
[0055] Add 100 ppm Cu(Ⅱ)-EDTA aqueous solution to a 100 mL beaker. The total volume of the reaction solution is 50 mL and the initial pH is 3.4. Add 0.029 g NaCl, 0.042 g NaNO 3 , 0.071 g NaSO 4 The initial concentration of the corresponding anion was 10 mM, and 0.05 g ZVMn was added. bm The concentration was 1 g / L, mechanically stirred and mixed in an open aerobic environment, and placed on a constant temperature rotary mixer with a speed of 200 r / min and a temperature of 25° C. Samples were taken at regular intervals to determine the residual amount of Cu(II)-EDTA in the system.
[0056] The experimental results are as follows Figure 8 As shown, the presence of inorganic anions has an important effect on ZVMn bm Removal of Cu(Ⅱ)-EDTA had little effect.
[0057] Example 4
[0058] Add 100 ppm Cu(II)-EDTA aqueous solution to a 100 mL beaker. The total volume of the reaction solution is 50 mL and the initial pH is 3.4. Add 5 mg humic acid (HA) to the reaction solution to make its initial concentration 10 ppm. Add 0.05 g ZVMn bm The concentration was 1 g / L, mechanically stirred and mixed in an open aerobic environment, and placed on a constant temperature rotary mixer with a speed of 200 r / min and a temperature of 25° C. Samples were taken at regular intervals to determine the residual amount of Cu(II)-EDTA in the system.
[0059] The experimental results are as follows Fig. 9 As shown in Figure 2, the presence of natural organic matter represented by HA has an important effect on ZVMn bm The removal of Cu(Ⅱ)-EDTA had little effect on ZVMn bm Have good environmental adaptability.
[0060] Example 5
[0061] Add 100 ppm Cu(Ⅱ)-EDTA aqueous solution to a 100 mL beaker, use 3 mM KOH to adjust the initial pH of the solution, the total volume of the reaction solution is 50 mL, and add 0.05 g ZVMn bm The concentration was 1 g / L, mechanically stirred and mixed in an open aerobic environment, and placed on a constant temperature rotary mixer with a speed of 200 r / min and a temperature of 25° C. Samples were taken at regular intervals to determine the residual amount of Cu(II)-EDTA in the system.
[0062] The experimental results are as follows Fig.10 As shown in the figure, different initial pH of the reaction has an effect on ZVMn bm The removal of Cu(Ⅱ)-EDTA had little effect on ZVMn bm Have good environmental adaptability.
[0063] The above-mentioned embodiments only express several implementation methods of the present invention, and the description thereof is relatively specific and detailed, but it cannot be understood as limiting the scope of the patent of the present invention. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, which all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be subject to the attached claims.
Claims
1. Application of zero-valent manganese in the removal of Cu(Ⅱ)-EDTA.
2. The use according to claim 1, characterized in that: The zero-valent manganese is obtained by ball milling manganese powder.
3. The use according to claim 2, characterized in that: The ball milling beads are stainless steel ball milling beads.
4. The use according to claim 3, characterized in that: The diameter of the ball milling beads is 2-6 mm, preferably 2-4 mm and 4.1-6 mm; preferably, the ratio of the number of ball milling beads with a diameter of 2-4 mm to the number of ball milling beads with a diameter of 4.1-6 mm is 1-3:1, preferably 2:
1.
5. The use according to claim 2, characterized in that: For every 4 g of manganese powder, 15-25 ball milling beads with a diameter of 4.1-6 mm and 35-45 ball milling beads with a diameter of 2-4 mm are used, preferably 20 ball milling beads with a diameter of 5 mm and 40 ball milling beads with a diameter of 3 mm are used.
6. The use according to claim 2, characterized in that: The total ball milling time is 0.5-4 h, preferably 1.5-3 h, preferably 2 h.
7. The use according to claim 2, characterized in that: The rotation speed of the ball mill is 200-800 rpm, preferably 300-600 rpm, preferably 350-500 rpm.
8. The use according to claim 2, characterized in that: The ball milling is performed using a planetary ball mill, and the direction of the ball milling is changed every 20-40 minutes.
9. The use according to any one of claims 1 to 8, characterized in that: The mass ratio of the zero-valent manganese to Cu(II)-EDTA is 8-12:1, preferably 10:
1.
10. The use according to claim 9, characterized in that: The zero-valent manganese removes Cu(II)-EDTA under the condition of pH 2-5.
Citation Information
Patent Citations
Method and apparatus for removing manganese from water
CA2122021A1
Method of removing pollutant in water with mechanical ball-milling activated zero-valent aluminum
CN110282717A
Method for removing pollutants through efficient reduction of ball-milled lignosulphonated zero-valent iron
CN114409051A
Method for directly reducing, decomplexing and recovering copper from complex copper wastewater
CN116789308A
Preparation method and application of manganese-doped micron iron modified material
CN117401801A