Integrated thinning and chamfering processing method for ultra-thin glass

Through the combination of laser internal engraving and chemical etching, the integration of thinning and chamfering processing of ultra-thin glass is achieved, solving the problems of extended production cycle and high cost caused by separate processing, improving efficiency and quality, and reducing environmental impact and equipment complexity.

CN118930062APending Publication Date: 2024-11-12BIEL OPTIC HUIZHOU +2

Patent Information

Application Number
CN202410996547.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-24
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

The thinning and chamfering processing process of existing ultra-thin glass is carried out separately, resulting in extended production cycles, increased costs, low efficiency, complex equipment, and great environmental impact. Multi-step processing increases material waste and quality control difficulty.

Method used

The chamfered structure is engraved inside the glass sheet by laser engraving, and then thinning through chemical etching to achieve an integrated process of thinning and chamfering processing, reducing production steps and working hours, improving production efficiency, and reducing equipment and operation complexity. Reduce energy consumption and chemical use.

Benefits of technology

It significantly improves production efficiency, reduces processing costs and environmental impact, improves product quality consistency and reliability, reduces equipment investment and maintenance costs, simplifies process flow, and reduces material losses and processing errors.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118930062A_ABST
    Figure CN118930062A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of glass processing, and particularly discloses an integrated thinning and chamfering processing method for ultra-thin glass, which is high in production efficiency, low in processing cost, high in product quality, less in equipment needing maintenance and operation and small in influence on the environment. The integrated thinning and chamfering processing method comprises the following steps: S1, cutting a glass incoming material into sheets with preset shapes and sizes; s2, a chamfer structure is engraved in a preset part in the sheet in a laser internal engraving mode; s3, performing chemical etching thinning on the sheet subjected to laser internal carving, wherein the chemical etching thinning thickness is greater than or equal to the minimum distance from the edge of the chamfering structure to the surface of the sheet; and S4, splitting the thinned sheet to obtain the ultra-thin glass with a chamfer at the edge.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of glass processing, and in particular to an integrated thinning and chamfering processing method for ultra-thin glass. Background Art

[0002] Ultra-thin glass (UTG) refers to glass with a thickness of ≤100μm, which is soft and can be bent and rolled. It integrates the advantages of plastic polymers into the glass. In addition to maintaining the various properties of glass, it also meets the requirements of easy bending. It is currently widely used in folding screens of smartphones, wearable devices and other electronic products. Because ultra-thin glass is very fragile and its edges are easily damaged, it is often necessary to process chamfers on the edges of ultra-thin glass to smooth the glass edges, thereby reducing cracks or breaks caused by edge stress concentration; at the same time, chamfered edges are more resistant to external impacts than straight edges, reducing damage caused by collisions or pressure changes; the smooth edges after chamfering are more user-friendly, especially in consumer electronic products such as smartphones, tablets and other devices, which can prevent users from being cut; chamfered glass is not prone to edge collapse due to collisions, and the edge strength of the glass can be greatly improved to avoid glass fragments; chamfered edges can be more easily installed in the device frame or housing, reducing the risk of damage during installation and reducing the difficulty of assembly; in addition, chamfers can help ultra-thin glass better adapt to other components, such as screen bonding, the combination of glass cover and body, etc., to improve the accuracy of the overall assembly. In view of the above advantages of chamfering, ultra-thin glass often needs to be chamfered while being thinned.

[0003] At present, the industry mainly uses physical grinding and / or chemical etching to thin ultra-thin glass; while mechanical grinding or other physical and chemical processing is used to chamfer ultra-thin glass. The processes involved in thinning and chamfering are completely different. Therefore, the thinning process and chamfering process of ultra-thin glass are usually carried out separately. In the case where the thinning process and chamfering process are carried out separately, firstly, due to the need for multi-step processing, each step not only requires separate equipment settings and operations, but also may involve different process links, such as grinding, cleaning and edging. This multi-stage process processing method will lead to an extension of the entire production cycle, thereby increasing manufacturing costs. Secondly, in the case of separate processing, the glass needs to be repositioned and adjusted after being transferred between different workstations, which is time-consuming, has low processing efficiency, and is prone to material waste or production defects caused by inaccurate or incorrect positioning. Thirdly, uneven material stress, microcracks or other structural defects may occur in different processing stages, especially quality problems in the edge area of ​​the glass. The increase in independent processing steps will increase the difficulty of controlling the quality of the final product. Furthermore, multi-step processing requires a variety of different machines and technologies, each of which requires specialized maintenance and operation, increasing operational complexity, maintenance costs and the risk of equipment failure. In addition, each step requires separate machine operation and resource investment, and multi-stage processing is usually accompanied by higher energy consumption. In addition, multi-step processing may involve more chemicals or physical wear, which puts a greater burden on the environment. Summary of the invention

[0004] Based on this, it is necessary to provide an integrated thinning and chamfering method for ultra-thin glass with high production efficiency, low processing cost, high product quality, less equipment to be maintained and operated, and little impact on the environment in order to address the above-mentioned shortcomings.

[0005] An integrated thinning and chamfering method for ultra-thin glass comprises the following steps:

[0006] S1. Cutting the glass material into sheets of preset shapes and sizes;

[0007] S2. Carve a chamfered structure at a preset position inside the sheet by laser engraving;

[0008] S3, chemically etching and thinning the sheet after laser engraving, wherein the thickness of the chemical etching thinning is greater than or equal to the minimum distance from the edge of the chamfered structure to the surface of the sheet;

[0009] S4. Splitting the thinned sheet to obtain ultra-thin glass with chamfered edges.

[0010] In one embodiment, before step S1, the method further includes:

[0011] S0. A protective layer is provided on the surface of the glass material; the protective layer is an oil film coated on the surface of the glass material, or a protective film covering the surface of the glass material.

[0012] In one embodiment, step S2 comprises:

[0013] S21, determining the laser inner engraving processing surface of the sheet, and removing the protective layer on the laser inner engraving processing surface;

[0014] S22, shaping the laser beam of the laser inner engraving machine to control the focal position and depth of the laser beam;

[0015] S23, carving a chamfered structure distributed along a circular path inside the sheet.

[0016] In one embodiment, step S3 comprises:

[0017] S31, removing the remaining protective layer on the surface of the sheet;

[0018] S32, immersing the sheet in an etching solution for etching;

[0019] S33, cleaning the etched sheet.

[0020] In one embodiment, the etching solution is an HF solution with a concentration of 10-40% and a temperature between 20-30°C, or the etching solution is a NaOH solution with a concentration of 10-40% and a temperature between 110-130°C; the etching time is 500-1000s, and the thickness of the sheet after etching is 25-40μm.

[0021] In one embodiment, in step S33, ultrasonic cleaning is used to remove the etching solution remaining on the surface of the sheet.

[0022] In one embodiment, after step S4, the method further includes: S5, chemically hardening the ultra-thin glass; step S5 includes:

[0023] S51, preheating the ultra-thin glass to a hardening temperature and keeping it warm for a preset time;

[0024] S52, preparing a hardening solution of a preset concentration and a preset temperature, and immersing the ultra-thin glass after heat preservation in the hardening solution to perform an ion exchange reaction;

[0025] S53. After the reaction is completed, the ultra-thin glass is slowly cooled to room temperature.

[0026] In one of the embodiments, the hardening temperature is 350-450°C; the insulation time of the ultra-thin glass is greater than 10 minutes; the hardening solution is a potassium chloride solution or a sodium nitrate solution with a concentration of 5-20%, and the hardening solution temperature is 350-450°C; the ion exchange reaction time is 3600-10000s; and the ultra-thin glass is slowly cooled at a rate less than 1°C / min.

[0027] In one embodiment, step S5 further includes:

[0028] S6, placing the hardened ultra-thin glass in a polishing liquid for polishing;

[0029] S7. Clean the ultra-thin glass after the polishing.

[0030] In one embodiment, the back-polishing liquid is a NaOH solution with a concentration of 10-30%, the back-polishing temperature is 60-90° C., and the back-polishing time is 60-300 s.

[0031] The integrated thinning and chamfering processing method of ultra-thin glass of the present invention is implemented by pre-laser engraving the sheet, forming a chamfered structure inside the sheet, and then chemically etching the sheet for thinning, thereby realizing an integrated process of thinning and chamfering processing, which can significantly reduce production steps and working hours, and improve overall production efficiency; the operation process is reduced, and the number of times the glass is transported and repositioned in the middle is reduced, while speeding up the production speed, reducing the risk of material loss, and reducing the processing errors introduced by multiple transports and repositioning of the product, thereby improving the consistency and reliability of the product; laser engraving provides high-precision edge processing, while chemical etching can be used for uniform and effective thinning. This combination can provide more refined processing effects while ensuring quality, and improve product processing quality; the processing involves less equipment and technology, which reduces equipment investment and maintenance costs, and the reduction of processing steps and equipment operating time will reduce overall energy consumption and reduce the processing cost of ultra-thin glass. The reduction of processing steps will also reduce the use of chemicals and the generation of their waste, and reduce the impact on the environment. BRIEF DESCRIPTION OF THE DRAWINGS

[0032] Figure 1 A flowchart of an integrated thinning and chamfering method for ultra-thin glass in one embodiment of the present invention;

[0033] Figure 2 It is a schematic diagram of the structure of a sheet after laser engraving in one embodiment of the present invention;

[0034] Figure 3 This is a schematic diagram of the structure of a sheet after chemical etching and thinning in one embodiment of the present invention;

[0035] Figure 4This is a schematic diagram of the structure of a sheet after being split in one embodiment of the present invention;

[0036] Figure 5 This is a microscopic structure diagram of a sheet after laser engraving in one embodiment of the present invention;

[0037] Figure 6 This is a schematic diagram of an embodiment of the present invention in which etching liquid enters the chamfer structure during chemical etching thinning of a sheet. DETAILED DESCRIPTION

[0038] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the specific embodiments of the present invention are described in detail below in conjunction with the accompanying drawings. In the following description, many specific details are set forth to facilitate a full understanding of the present invention. However, the present invention can be implemented in many other ways different from those described herein, and those skilled in the art can make similar improvements without violating the connotation of the present invention, so the present invention is not limited by the specific embodiments disclosed below.

[0039] Please combine Figure 1-4 The present invention discloses an integrated thinning and chamfering method for ultra-thin glass with high production efficiency, low processing cost, high product quality, less equipment to be maintained and operated, and little impact on the environment. The integrated thinning and chamfering method comprises the following steps:

[0040] S1. Cut the glass material into sheets of preset shapes and sizes.

[0041] Specifically, according to the design drawings and specification requirements of the product (the ultra-thin glass product to be processed and formed can be a smartphone screen, a wearable device, a car display, etc.), a high-precision cutting tool, such as a laser cutter or a water jet, is used to cut the original large piece of glass material into a predetermined shape and size. This step requires a high degree of precise control to ensure the accuracy of the cutting and the neatness of the edges. In addition, before step S1, it also includes: S0, setting a protective layer on the surface of the glass material; the protective layer is an oil film coated on the surface of the glass material, or a protective film covering the surface of the glass material. Preferably, the thickness of the protective layer on the surface of the glass material is uniform. By setting a protective layer on the surface of the glass material, the glass material can be prevented from being mechanically damaged or chemically corroded during subsequent processing, and dust and other particles can be prevented from adhering to the surface of the glass material to ensure the processing quality.

[0042] S2, engraving a chamfered structure 100 at a preset position inside the sheet by laser engraving. Step S2 includes:

[0043] S21, determining the laser inner engraving processing surface of the sheet, and removing the protective layer on the laser inner engraving processing surface.

[0044] In this embodiment, after the laser inner engraving processing surface of the sheet is determined, the laser inner engraving machine is located on the side of the sheet where the laser inner engraving processing surface is located when performing laser inner engraving on the sheet, and the laser beam emitted by the laser inner engraving machine enters the sheet through the laser inner engraving processing surface. By removing the protective layer on the laser inner engraving processing surface, the interference of the protective layer on the laser beam can be eliminated, so that the laser can process the laser inner engraving processing surface.

[0045] S22, shaping the laser beam of the laser inner engraving machine to control the focal position and depth of the laser beam.

[0046] By adjusting the optical components in the laser engraving machine (laser emitting equipment), such as using a spatial light modulator SLM or a diffractive optical element DOE, the shape and energy distribution of the laser beam can be changed to achieve the shaping of the laser beam of the laser engraving machine. The shaped laser beam can accurately control the focal position and depth of the laser, which is suitable for complex internal engraving or fine surface processing. The processing time is about 10s / pcs.

[0047] S23, carving a chamfered structure 100 distributed along a circular path inside the sheet, the microstructure of the chamfered structure 100 is as follows: Figure 5 In this embodiment, a high-precision, well-shaped laser beam is used to perform fine engraving inside the glass to form a predetermined chamfer shape. The laser accurately adjusts the depth and angle of the chamfer to ensure a smooth and uniform edge.

[0048] It should be noted that the laser internal chamfering technology uses a spatial light shaping device SLM (Spatial light Modulator) or a diffractive optical element DOE (Diffractive optical elements) to shape the laser beam into a desired chamfered beam, and then focuses it into the inside of the transparent glass, and engraves it in a one-time multi-focus manner inside the glass, so as to form a chamfered structure 100 inside the glass. The chamfer shape can be set arbitrarily and can be finely adjusted according to the final performance of the product. Laser focusing and engraving means that the shaped laser beam is focused into the inside of the transparent glass. Through precise focusing, the laser can perform one-time engraving in a multi-focus manner inside the glass, so that complex designs and patterns can be created inside without damaging the glass surface. The chamfered structure 100 is formed inside the sheet through laser internal engraving technology. The specific shape of the chamfer can be adjusted according to the final performance and requirements of the product. The shape and depth of the laser engraving can be flexibly set according to different application requirements, so as to achieve the best visual effect and physical performance.

[0049] S3. Chemically etch and thin the laser engraved sheet. The thickness of chemical etching is greater than or equal to the minimum distance from the edge of the chamfered structure 100 to the sheet surface. Figure 5as well as Figure 6 In this embodiment, by limiting the thickness of chemical etching thinning to be greater than or equal to the minimum distance from the edge of the chamfered structure 100 to the surface of the sheet, it is ensured that during the chemical etching thinning process of the sheet, the edge of the chamfered structure 100 formed on the sheet by laser inner engraving can be exposed, so that the etching liquid can penetrate into the gap of the chamfered structure 100, and the etching liquid reacts with the sheet in the gap, so that the two sides of the glass are connected, so as to provide conditions for subsequent splitting operations and reduce the difficulty of splitting. Figure 6 The arrows in FIG. 1 show the path of the etching liquid entering the gap of the chamfered structure 100 .

[0050] Further, step S3 includes:

[0051] S31, removing the remaining protective layer on the sheet surface. When the protective layer is a protective film, the protective film can be carefully removed to expose the sheet surface, which is convenient for chemical etching and thinning of the sheet surface. When the protective layer is an oil film, the oil film on the sheet surface can be removed by ultrasonic cleaning or detergent cleaning, so that the sheet surface is exposed, which is convenient for subsequent processing.

[0052] S32, immerse the sheet in the etching solution for etching. Further, the etching solution is an HF solution with a concentration of 10-40% and a temperature between 20-30°C, or the etching solution is a NaOH solution with a concentration of 10-40% and a temperature between 110-130°C; the etching time is 500-1000s, and the thickness of the sheet after etching is 25-40μm. In one embodiment, the etching solution is an HF solution with a concentration of 10% and a temperature of 20°C, and the etching time is 1000s. In one embodiment, the etching solution is an HF solution with a concentration of 30% and a temperature of 25°C, and the etching time is 800s. In one embodiment, the etching solution is an HF solution with a concentration of 40% and a temperature of 30°C, and the etching time is 500s. In one embodiment, the etching solution is a NaOH solution with a concentration of 10% and a temperature of 130°C, and the etching time is 1000s. In one embodiment, the etching solution is a NaOH solution with a concentration of 20% and a temperature of 110°C, and the etching time is 700s. In one embodiment, the etching solution is a NaOH solution with a concentration of 40% and a temperature of 120°C, and the etching time is 5000s. In actual processing, when an HF solution is selected, a HF solution with a concentration of 10-40% and a room temperature can be selected; the etching time can be further adjusted according to the thickness of the glass material, which will not be described in detail here.

[0053] S33, cleaning the etched sheet.

[0054] Since unreacted etching liquid often remains on the surface of the glass after chemical etching, it is necessary to remove the etching liquid remaining on the surface of the glass to avoid affecting subsequent operations. Preferably, in step S33, ultrasonic cleaning is used to remove the etching liquid remaining on the surface of the sheet. Specifically, the sheet is placed in a cleaning tank, and the etching liquid remaining on the surface of the sheet is removed by ultrasonic cleaning. The cleaned surface is based on the standard of no fogging residue visually observed.

[0055] S4. Splitting the thinned sheet to obtain ultra-thin glass with chamfered edges.

[0056] Specifically, a glass breaking machine is used to break the thinned glass. This process needs to be carefully designed according to the physical and chemical properties of the glass to ensure that the broken product has good structural integrity and edge quality.

[0057] In this solution, after laser engraving and chamfering the glass, liquid polishing is directly performed for thinning, which combines and reduces the complicated UTG chamfering process and chemical reduction process in the traditional process. The chamfered part and the glass surface are polished in an integrated manner through liquid polishing (chemical etching thinning) technology. Liquid polishing not only optimizes the surface texture of the chamfer, but also further thins the glass thickness without damaging the overall strength of the glass, and facilitates the etching liquid to penetrate into the pre-processed chamfered structure 100. While the glass surface is thickened, the inner surface of the glass chamfer is etched, so that the etching liquid reacts inside the chamfered structure 100 and finally connects the two sides of the glass. After the liquid polishing is completed, only the splitting process is required to obtain ultra-thin glass with chamfers, and no separate edge chamfering process is required. The combination of laser engraving and liquid polishing (liquid polishing) technology is used to simultaneously achieve chamfering processing and glass thinning. The way to improve processing efficiency and product quality is specifically reflected in the following aspects:

[0058] 1) Improve machining accuracy

[0059] Precise control: Laser engraving can control the shape, depth and angle of the chamfer very accurately, ensuring that each edge is processed precisely as required, avoiding later corrections.

[0060] Consistency and repeatability: The high repeatability of laser processing ensures the consistency of chamfers for each product in mass production and reduces quality fluctuations.

[0061] Parameter optimization: By optimizing parameters such as laser power, focal length, scanning speed, etc., we can ensure the best effect and efficiency during laser processing and reduce heat-affected zones and microcracks.

[0062] 2) Optimize the processing flow

[0063] Integrated operation: Traditional chamfering and thinning operations require multiple steps and equipment to complete, while the combination of laser engraving and liquid polishing technology can complete chamfering and thinning in one continuous process, significantly improving production efficiency.

[0064] Reduce process conversion: Reduce intermediate inspection and conversion processes, reduce transportation and waiting time, and make the entire production process more compact and efficient.

[0065] Furthermore, after step S4, the following step is further included: S5, chemically hardening the ultra-thin glass. By chemically hardening the ultra-thin glass, potassium, sodium ions, etc. are exchanged in the tank by using chemical deposition or infiltration process, thereby increasing the hardness and wear resistance of the glass surface. This process not only improves the physical properties of the glass, but also enhances its impact resistance to prevent it from being fragile or scratched in daily use. Specifically, step S5 includes:

[0066] S51, preheating the ultra-thin glass to a hardening temperature and keeping it warm for a preset time. The hardening temperature is 350-450°C, and the ultra-thin glass is kept warm for more than 10 minutes, so that the temperature of each part of the ultra-thin glass is uniform.

[0067] S52, configure a hardening solution with a preset concentration and a preset temperature, and immerse the ultra-thin glass after heat preservation in the hardening solution for ion exchange reaction. In this embodiment, the hardening solution is a potassium chloride KCl solution or a sodium nitrate NaNO3 solution with a concentration of 5-20%. During actual processing, the concentration of the hardening solution can be further adjusted according to specific conditions. The temperature of the hardening solution is 350-450°C, and the temperature of the hardening solution is the hardening temperature of chemical hardening. This temperature range is conducive to the ion exchange reaction. In this embodiment, the temperature control accuracy is required to be high, usually controlled within ±5°C. In one embodiment, the hardening temperature of the hardening solution is 350°C. In another embodiment, the hardening temperature of the hardening solution is 400°C. In another embodiment, the hardening temperature of the hardening solution is 450°C. The ion exchange reaction time is 3600-10000s. The length of the ion exchange reaction time depends on the thickness, shape and hardness index of the glass to be achieved. During actual processing, the ion exchange reaction time can be further adjusted as needed.

[0068] S53. After the reaction is completed, the ultra-thin glass is slowly cooled to room temperature, and the entire chemical hardening process is completed. Preferably, the ultra-thin glass is slowly cooled at a rate less than 1°C / min to avoid surface cracks caused by rapid cooling of the ultra-thin glass. By chemically hardening the ultra-thin glass, a compression layer composed of potassium ions or sodium ions will be formed on the surface of the ultra-thin glass. This compression layer can effectively prevent the expansion of cracks and improve the impact resistance and wear resistance of the glass. Compared with the glass before chemical hardening, the strength of the hardened glass is increased by 2-5 times. In the actual processing process, the hardening parameters and ion exchange reaction time can be further adjusted according to the thickness of the incoming glass, which will not be repeated here.

[0069] After step S5, the following steps are also included:

[0070] S6. Place the hardened ultra-thin glass in a polishing liquid for polishing. In this embodiment, after the chemical hardening treatment, the glass is polished again to eliminate tiny surface defects that may be formed during the hardening process, which not only improves the physical properties of the glass, but also enhances its impact resistance. In this embodiment, chemical polishing is adopted, and the polishing liquid is a NaOH solution with a concentration of 10-30%, the polishing temperature is 60-90°C, and the polishing time is 60-300s. Specifically, solid sodium hydroxide (NaOH) is dissolved in water to prepare a solution of the required concentration, and the hardened glass is immersed in the NaOH solution and maintained at a certain temperature. During this process, the NaOH solution will chemically react with the glass surface, causing ion exchange on the glass surface. The sodium ions Na in the NaOH solution + Will react with calcium ions Ca in the glass 2+ or potassium ion K + Exchange occurs. This process will form a compression layer composed of sodium ions on the surface of the glass, thereby increasing the surface compression stress of the glass. The increase in surface compression stress will inhibit the expansion of cracks, thereby improving the mechanical strength and impact resistance of the glass. Usually, after this chemical polishing treatment, the strength of the glass can be increased by 2-5 times.

[0071] S7. Clean the ultra-thin glass after polishing. Specifically, use appropriate cleaning agents and water flow to thoroughly clean the glass after various processing steps in an ultrasonic cleaning device to remove processing residues on the glass surface, such as cutting fluid, polishing paste, dust, etc. This step is the key to ensuring the final quality of the product and is used to eliminate the impact of residues on the cleanliness of the glass.

[0072] The above-mentioned integrated thinning and chamfering processing method of ultra-thin glass realizes an integrated process of thinning and chamfering processing by pre-laser engraving the sheet, forming a chamfer structure 100 inside the sheet, and then chemically etching the sheet for thinning, which can significantly reduce production steps and working hours and improve overall production efficiency; the operation process is reduced, and the number of times the glass is transported and repositioned in the middle is reduced, while speeding up production, reducing the risk of material loss, and reducing processing errors introduced by multiple transports and repositioning of products, thereby improving product consistency and reliability; laser engraving provides high-precision edge processing, while chemical etching can be used for uniform and effective thinning. This combination can provide more refined processing effects while ensuring quality, thereby improving product processing quality; the processing involves less equipment and technology, which reduces equipment investment and maintenance costs, and the reduction of processing steps and equipment operating time will reduce overall energy consumption and reduce the processing cost of ultra-thin glass. The reduction of processing steps will also reduce the use of chemicals and the generation of their waste, thereby reducing the impact on the environment.

[0073] The technical features of the above-described embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features in the above-described embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0074] The above-mentioned embodiments only express several implementation methods of the present invention, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the invention patent. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, and these all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be subject to the attached claims.

Claims

1. An integrated thinning and chamfering method for ultra-thin glass, characterized in that: The following steps are involved: S1. Cutting the glass material into sheets of preset shapes and sizes; S2. Carve a chamfered structure at a preset position inside the sheet by laser engraving; S3, chemically etching and thinning the sheet after laser engraving, wherein the thickness of the chemical etching thinning is greater than or equal to the minimum distance from the edge of the chamfered structure to the surface of the sheet; S4. Splitting the thinned sheet to obtain ultra-thin glass with chamfered edges.

2. The integrated thinning and chamfering method of ultra-thin glass according to claim 1, characterized in that: Before step S1, the method further includes: S0. A protective layer is provided on the surface of the glass material; the protective layer is an oil film coated on the surface of the glass material, or a protective film covering the surface of the glass material.

3. The integrated thinning and chamfering method of ultra-thin glass according to claim 2, characterized in that: Step S2 includes: S21, determining the laser inner engraving processing surface of the sheet, and removing the protective layer on the laser inner engraving processing surface; S22, shaping the laser beam of the laser inner engraving machine to control the focal position and depth of the laser beam; S23, carving a chamfered structure distributed along a circular path inside the sheet.

4. The integrated thinning and chamfering method of ultra-thin glass according to claim 2, characterized in that: Step S3 includes: S31, removing the remaining protective layer on the surface of the sheet; S32, immersing the sheet in an etching solution for etching; S33, cleaning the etched sheet.

5. The integrated thinning and chamfering method of ultra-thin glass according to claim 4, characterized in that: The etching solution is an HF solution with a concentration of 10-40% and a temperature between 20-30°C, or the etching solution is a NaOH solution with a concentration of 10-40% and a temperature between 110-130°C; the etching time is 500-1000s, and the thickness of the sheet after etching is 25-40μm.

6. The integrated thinning and chamfering method of ultra-thin glass according to claim 4, characterized in that: In step S33, ultrasonic cleaning is used to remove the etching solution remaining on the surface of the sheet.

7. The integrated thinning and chamfering method of ultra-thin glass according to claim 1, characterized in that: After step S4, the method further includes: S5, chemically hardening the ultra-thin glass; step S5 includes: S51, preheating the ultra-thin glass to a hardening temperature and keeping it warm for a preset time; S52, preparing a hardening solution of a preset concentration and a preset temperature, and immersing the ultra-thin glass after heat preservation in the hardening solution to perform an ion exchange reaction; S53. After the reaction is completed, the ultra-thin glass is slowly cooled to room temperature.

8. The integrated thinning and chamfering method of ultra-thin glass according to claim 7, characterized in that: The hardening temperature is 350-450°C; the ultra-thin glass insulation time is greater than 10 minutes; the hardening solution is a potassium chloride solution or a sodium nitrate solution with a concentration of 5-20%, and the hardening solution temperature is 350-450°C; the ion exchange reaction time is 3600-10000s; the ultra-thin glass slow cooling speed is less than 1°C / min.

9. The integrated thinning and chamfering method of ultra-thin glass according to claim 7, characterized in that: After step S5, the following steps are also included: S6, placing the hardened ultra-thin glass in a polishing liquid for polishing; S7. Clean the ultra-thin glass after the polishing.

10. The integrated thinning and chamfering method of ultra-thin glass according to claim 9, characterized in that: The back-throwing liquid is a NaOH solution with a concentration of 10-30%, the back-throwing temperature is 60-90°C, and the back-throwing time is 60-300s.

Citation Information

Patent Citations

  • Glass chamfering method and device

    CN112479582A

  • Processing method of ultrathin flexible glass edge R corner and production method of ultrathin flexible glass

    CN114180848A

  • Thinning process for float optical glass

    CN114213031A

  • Processing method for improving edge strength of ultra-thin glass

    CN116409944A

  • Monolithic processing method of ultra-thin glass, ultra-thin glass and flexible display device

    CN116874192A

Cited By

  • Processing method of AG (anti-glare) glass

    CN119609948A

  • Processing method of AG anti-dazzle glass

    CN119609948B