Ceramsite prepared by mixing metal tailings and steel slag and method thereof

Through hyperspectral data analysis, the mixing and stirring process of rare earth tailings and steel slag is determined, which solves the problem of inaccurate stirring time control in the prior art, improves the preparation efficiency of ceramic granules and reduces costs.

CN118930213AActive Publication Date: 2024-11-12YUELIDA (HEBEI) ENVIRONMENTAL TECHNOLOGY CO LTD

Patent Information

Application Number
CN202411177490.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-26
Publication Date
2024-11-12
Estimated Expiration
2044-08-26

AI Technical Summary

Technical Problem

The prior art cannot accurately control the mixing and stirring time of rare earth tailings and steel slag, resulting in insufficient strength of the ceramic granules or too long stirring time, low efficiency and high cost.

Method used

Hyperspectral data analysis is used to determine the stirring of the mixture, and determine whether to stop stirring by material similarity, permeability and movement complexity to ensure sufficient mixing uniformity and avoid unnecessary stirring time.

Benefits of technology

On the basis of ensuring the strength of the ceramite, timely stop stirring is achieved, the preparation efficiency is improved, the cost is reduced, and the preparation time and energy waste are avoided.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118930213A_ABST
    Figure CN118930213A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of redevelopment and utilization of rare earth metal tailings, in particular to ceramsite prepared by mixing metal tailings and steel slag and a method thereof, and the method comprises the following steps: crushing and grinding the metal tailings and the steel slag into powder to obtain a rare earth tailing mixture; carrying out solid-liquid separation on the petroleum drilling slurry to obtain petroleum drilling waste liquid, dipping a rare earth tailing mixture, and obtaining dipping liquid dipped by the petroleum drilling waste liquid and the rare earth tailing mixture; the preparation method comprises the following steps: mixing and stirring impregnation liquid obtained by impregnating the petroleum drilling waste liquid, a rare earth tailing mixture, industrial waste bricks, Suzhou soil, high bauxite, coal ash, silica fume, attapulgite, coal gangue, straw waste, industrial phosphoric acid, steel fibers, phosphogypsum, alumina sol, polypropylene fibers, sodium sulfate, citric acid, benzalkonium chloride, bentonite, river sand and graphite powder; and homogenizing the mixture, balling, coating, screening, standing and cooking to obtain the ceramsite. The ceramsite preparation efficiency can be improved, and the ceramsite preparation cost can be reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of rare earth metal tailings redevelopment and utilization, and in particular to ceramsite prepared by mixing metal tailings and steel slag and a method thereof. Background Art

[0002] Rare earth tailings contain important metal resources and have high economic value. During the development of mineral resources, the mining utilization rate often does not reach 100%, and a large amount of rare earth tailings will be produced. The production of rare earth tailings will not only waste resources, but also occupy land and easily cause soil erosion. Therefore, the treatment of rare earth tailings restricts the development of the rare earth industry, and its comprehensive utilization has become an important factor affecting the development of the rare earth industry.

[0003] At present, the development and utilization of rare earth tailings has important practical significance. In the existing technology of preparing ceramsite using rare earth tailings, in order to ensure the strength of the prepared ceramsite, it is often necessary to continuously mix and stir the mixture. However, the existing technology often cannot accurately control the mixing and stirring time. When the mixing and stirring time is short, it is easy to make the mixing uniformity of the mixture poor, resulting in weak strength of the prepared ceramsite, which cannot meet the strength requirements of ceramsite in practical applications.

[0004] In order to ensure the strength requirements of the prepared expanded clay in practical applications, a longer mixing time is usually set during the mixing and stirring process. When the mixture reaches the time of being fully mixed and uniform, the existing technology is unable to stop the mixing and stirring of the mixture in time on the basis of satisfying the requirement of fully mixing the mixture, resulting in excessively long mixing and stirring time for the mixture, resulting in a waste of preparation time and electric energy, and leading to the problems of low efficiency and high preparation cost of expanded clay. Summary of the invention

[0005] In order to solve the above technical problems, the purpose of this application is to provide a ceramsite prepared by mixing metal tailings and steel slag and a method thereof, and the technical scheme adopted is as follows:

[0006] The present application provides a method for preparing ceramsite mixed with metal tailings and steel slag, comprising the following steps:

[0007] crushing the metal tailings and steel slag, and grinding the crushed mixture into powder to obtain a rare earth tailings mixture;

[0008] Solid-liquid separation of oil drilling slurry to obtain oil drilling waste liquid, impregnation of the rare earth tailings mixture to obtain an impregnation liquid impregnated with the oil drilling waste liquid and the rare earth tailings mixture after impregnation;

[0009] Take the impregnation liquid impregnated with oil drilling waste liquid and the rare earth tailings mixture impregnated with it, industrial waste bricks, Suzhou soil, high-alumina bauxite, fly ash, silica ash, attapulgite, coal gangue, straw waste, industrial phosphoric acid, steel fiber, phosphogypsum, alumina sol, polypropylene fiber, sodium sulfate, citric acid, benzalkonium chloride, bentonite, river sand and graphite powder, mix and stir, and judge whether to stop stirring according to the high-spectral data analysis of the stirring process. The judgment process is as follows:

[0010] Collect hyperspectral images of the mixture during the mixing process and divide them into multiple sub-areas;

[0011] Based on the difference in reflectance between different pixels in each sub-region, the material similarity of each sub-region is constructed, and all material similarity thresholds are segmented to divide the sub-regions into material regions and non-material regions. The ratio of the number of non-material regions in the hyperspectral image at each moment to the total number of sub-regions is determined as the material mixing probability at each moment.

[0012] According to the average level of material similarity of all material regions at each moment and the correlation between the reflectivity of the pixels at the center of different material regions at each moment, the material penetration resistance at each moment is constructed, and the material movement complexity at each moment is obtained in combination with the material mixing probability;

[0013] The multiple moments closest to each moment are combined into a local moment set of each moment, and the material mixing change degree of each moment is determined according to the distribution disorder degree and range of the material movement complexity of all moments in the local moment set of each moment, so as to judge whether to stop stirring;

[0014] The fully mixed and stirred mixture is homogenized, balled, coated, sieved, rested, and steamed to obtain ceramsite.

[0015] Preferably, the weight ratio of the metal tailings to the steel slag is 1:1, and the grinding fineness is 10% on a 0.08 mm square hole sieve.

[0016] Preferably, the immersion temperature is 47° C. and the immersion time is 24 hours.

[0017] Preferably, 460 parts of a rare earth tailings mixture impregnated with oil drilling waste liquid, 250 parts of an impregnation liquid after impregnation, 10 parts of industrial waste bricks, 10 parts of Suzhou soil, 10 parts of high-alumina bauxite, 10 parts of fly ash, 10 parts of silica ash, 10 parts of attapulgite, 10 parts of coal gangue, 10 parts of straw waste, 3 parts of industrial phosphoric acid, 3 parts of steel fiber, 3 parts of phosphogypsum, 3 parts of alumina sol, 2 parts of polypropylene fiber, 2 parts of sodium sulfate, 2 parts of citric acid, 2 parts of benzalkonium chloride, 2 parts of bentonite, 2 parts of river sand, and 2 parts of graphite powder.

[0018] Preferably, the material similarity of each sub-region is calculated as follows:

[0019] In the formula, G i is the material similarity of the ith sub-region, n is the number of pixels in the sub-region, dtw() is the dtw distance, ∈ is the value to avoid the denominator being zero, g i,j and g i,j―1 is the reflectivity sequence of the jth and j-1th pixels in the i-th sub-region. The reflectivity of each pixel is arranged in ascending order of wavelength to form the reflectivity sequence of each pixel.

[0020] Preferably, the corresponding calculation formula of the material penetration resistance at each moment is:

[0021] Where D t is the material penetration resistance at time t, GX t is the mean of the material similarity of all material regions in the hyperspectral image at time t, m t is the number of material regions in the hyperspectral image at time t, cos() is the cosine similarity, and f t,d and f t,d―1 It is the reflectance sequence of the central pixels of the d-th and d-1-th material areas in the hyperspectral image at time t. The reflectance sequence of the central pixel is composed of the reflectance of the central pixel arranged in ascending order of wavelength.

[0022] Preferably, the material movement complexity at each moment is the ratio of the material mixing probability to the material penetration resistance at each moment.

[0023] Preferably, the step of determining the degree of material mixing change at each moment to determine whether to stop mixing and stirring further includes:

[0024] H t =norm(σV t × t ), where H t is the material mixing variation at time t, norm() is the normalization function, σV t is the information entropy of the material movement complexity corresponding to all the moments in the local moment set at moment t, zV t is the extreme difference of the material movement complexity corresponding to all moments in the local moment set at moment t;

[0025] If the material mixing change degree is less than the preset threshold, the stirring is stopped; otherwise, the stirring is continued until the material mixing change degree is less than the preset threshold.

[0026] Preferably, the discharge requirements of the homogenized mixture are a particle size of 0.6 mm and a sieve residue of 13%; the screening and curing is to screen out spheres smaller than 19 mm from the spheres and put them into a curing machine for curing for 24 hours; the cooking preparation is to autoclave the spheres after curing and react them under a saturated steam constant pressure of 1.0 MPa for 4.5 hours.

[0027] The embodiment of the present application also provides a ceramsite prepared by mixing metal tailings and steel slag, and the ceramsite is prepared by the steps of any one of the methods described above.

[0028] From the above, it can be seen that the ceramsite prepared by mixing metal tailings and steel slag and the method thereof provided in the present application have at least the following beneficial effects:

[0029] The present application constructs the material movement complexity between different material particles by analyzing the material mixing probability and the penetration resistance characteristics during the mixing process of different material particles. The material movement complexity can reflect the movement characteristics of strong collision, penetration and convection mixing between different material particles. The greater the material movement complexity, the more conducive to the uniformity of the mixed material mixing at this time; based on the material movement complexity, the material mixing variation degree of the mixing and stirring process is obtained. The material mixing variation degree reflects that the greater the change in the material movement complexity between the mixed materials, the smaller the material mixing variation degree, which indicates that the change in the material movement complexity between different material particles at this time will tend to be stable, and the more it can be explained that the mixed material is not fully mixed and uniform at this time, so the present invention determines whether to stop mixing and stirring by the material mixing variation degree. Compared with the prior art, the present invention can stop mixing and stirring the mixed material in time on the basis of ensuring that the mixed material is fully mixed and uniform, avoid the waste of preparation time and electric energy, effectively improve the efficiency of preparing ceramsite, and reduce the preparation cost of ceramsite. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] In order to more clearly illustrate the technical solutions and advantages in the embodiments of the present application or the prior art, the drawings required for use in the embodiments or the prior art descriptions are briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.

[0031] Figure 1 A flow chart of the steps of a method for preparing ceramsite mixed with metal tailings and steel slag provided in this application;

[0032] Figure 2 A schematic diagram of data collection during the mixing and stirring process provided in this application;

[0033] Figure 3Schematic diagram of material area and non-material area in the hyperspectral image provided in this application;

[0034] Figure 4 A flow chart for determining whether stirring should be stopped during mixing and stirring in the ceramsite preparation process provided in this application;

[0035] Figure 5 This is a schematic diagram comparing the effects of the 8 groups of implementation combinations provided in this application. DETAILED DESCRIPTION

[0036] In order to further explain the technical means and effects adopted by the present application to achieve the predetermined invention purpose, the following is a detailed description of the ceramsite and method thereof prepared by mixing a metal tailing and steel slag according to the present application, its specific implementation method, structure, characteristics and effects as follows in combination with the accompanying drawings and preferred embodiments. In the following description, different "one embodiment" or "another embodiment" does not necessarily refer to the same embodiment. In addition, the specific features, structures or characteristics in one or more embodiments may be combined in any suitable form.

[0037] Unless otherwise specified and limited, terms such as "comprises", "comprising" or any other variants thereof are intended to cover non-exclusive inclusion, so that a circuit structure, article or device including a series of elements includes not only those elements, but also includes other elements not explicitly listed, or also includes elements inherent to such articles or devices. In the absence of further restrictions, an element defined by the sentence "comprising a ..." does not exclude the presence of other identical elements in the article or device including the element. In addition, the term "and\or" used herein includes any and all combinations of one or more related listed items. All technical and scientific terms used herein have the same meaning as those commonly understood by technicians in the technical field of this application.

[0038] The specific scheme of ceramsite prepared by mixing metal tailings and steel slag and the method thereof provided in the present application is described in detail below with reference to the accompanying drawings.

[0039] See also Figure 1 , which shows a flow chart of the steps of a method for preparing ceramsite mixed with metal tailings and steel slag provided in one embodiment of the present application, specifically:

[0040] The purpose of this embodiment is to accurately control the mixing time during the mixing and stirring process of the ground mixture, and to stop mixing and stirring the mixture in time on the basis of ensuring that the mixture is fully mixed and uniform, so as to avoid the waste of preparation time and electric energy, resulting in low efficiency and high preparation cost of expanded clay.

[0041] In this embodiment, metal tailings and steel slag are used as basic raw materials to prepare ceramsite through the following process flow:

[0042] S1, crushing and screening: the metal tailings and steel slag are fed into a crusher in a weight ratio of 1:1 for crushing, and the crushed mixture is fed into a grinding mill for grinding into powder, with a fineness of 10% on a 0.08 mm square hole sieve to obtain a rare earth tailings mixture;

[0043] S2, impregnation with oil drilling waste liquid: performing solid-liquid separation on the oil drilling slurry to obtain oil drilling waste liquid, and impregnating the rare earth tailings mixture with the oil drilling waste liquid at a temperature of 47° C. for 24 h to obtain an impregnation liquid impregnated with the oil drilling waste liquid and a rare earth tailings mixture impregnated with the oil drilling waste liquid;

[0044] S3, mixing and stirring: taking the following materials in parts by weight for mixing and stirring, in this embodiment, 460 parts of rare earth tailings mixture after impregnation with oil drilling waste liquid, 10 parts of industrial waste bricks, 10 parts of Suzhou soil, 10 parts of high-alumina bauxite, 10 parts of fly ash, 10 parts of silica fume, 10 parts of attapulgite, 10 parts of coal gangue, 10 parts of straw waste, 3 parts of industrial phosphoric acid, 3 parts of steel fiber, 3 parts of phosphogypsum, 3 parts of alumina sol, 2 parts of polypropylene fiber, 2 parts of sodium sulfate, 2 parts of citric acid, 2 parts of benzalkonium chloride, 2 parts of bentonite, 2 parts of river sand, 2 parts of graphite powder, 250 parts of impregnation liquid after impregnation with oil drilling waste liquid, are sent into the mixing box of the mixer for mixing and stirring, and the original fixed stirring time is set to 40min. In order to be able to accurately control the mixing and stirring time, this embodiment will analyze the stirring condition of the mixture based on the hyperspectral data during the stirring process, specifically including the following steps:

[0045] Step 1: Collect the hyperspectral image of the mixture during the mixing process and divide it into multiple sub-areas.

[0046] In this embodiment, from the beginning of the mixing process, a hyperspectral camera is used to collect hyperspectral images of the mixture in real time during the mixing process to obtain hyperspectral images of the mixture at each moment in the mixing process. In this embodiment, the hyperspectral image at each moment is evenly divided into K rectangular grid areas, and each rectangular grid area is recorded as each sub-area. In this embodiment, K is 64, and the spectral reflectance of each pixel is arranged in ascending order of wavelength to form a sequence, which is recorded as the reflectance sequence of each pixel.

[0047] In this embodiment, the collection time interval is 2s, and the data collection diagram is as follows: Figure 2 As shown, Figure 2 Number 1 is the hyperspectral camera, number 2 is the acquisition window, and number 3 is the stirring box.

[0048] Step 2: Based on the difference in reflectance between different pixels in each sub-region, the material similarity of each sub-region is constructed, and all material similarity thresholds are segmented to divide the sub-regions into material regions and non-material regions. The ratio of the number of non-material regions in the hyperspectral image at each moment to the total number of sub-regions is determined as the material mixing probability at each moment.

[0049] Usually, at the beginning of the mixing process, the mixture is in the initial state of mixing. At this time, the mixing uniformity of the mixture is low, and the agglomeration of the mixture is obvious, indicating that the penetration between different materials is weak. At the same time, if the difference in spectral reflectance between pixels in different regions of the hyperspectral image at a certain moment is greater, and the difference in spectral reflectance between pixels in the same region is smaller, it can be explained to a certain extent that the penetration between different materials is weaker at this time.

[0050] In order to precisely control the mixing time, it is necessary to analyze the penetration characteristics between different materials during the mixing process.

[0051] Generally speaking, the smaller the difference in spectral reflectance between pixels in a sub-region, the more likely the material composition in the sub-region is to be of the same type, which means the material in the sub-region is more homogeneous, and to a certain extent, the worse the uniformity of the mixture.

[0052] Based on the above analysis, the material similarity of each sub-region is calculated based on the difference in reflectance between different pixels in each sub-region. The expression is:

[0053] In the formula, G i is the material similarity of the ith sub-region, n is the number of pixels in the sub-region, dtw() is the dtw distance, g i,j and g i,j―1 is the reflectivity sequence of the jth and j-1th pixels in the i-th sub-region, dtw(g i,j ,g i,j―1 ) is the reflectivity sequence g i,j and g i,j―1 The dtw distance between them, ∈ is a value to avoid the denominator being zero, and in this embodiment, the value is 1. The material similarity reflects the degree of uniformity of the material composition in the sub-region, that is, the smaller the material similarity, the more likely the material composition in the sub-region belongs to the same material, which to a certain extent indicates that the worse the uniformity of the mixed material, the higher the degree of uniformity of the material composition in the sub-region.

[0054] Normally, when a mixture undergoes strong penetration, particles of different materials will continuously collide with each other, thereby achieving uniform mixing between different materials. In order to analyze the characteristics of collision and mixing between different materials, all sub-regions in the hyperspectral image at each moment are used as inputs to the Otsu threshold algorithm to obtain a segmentation threshold. In this embodiment, the sub-regions corresponding to material similarities above the segmentation threshold are used as material regions, and the sub-regions corresponding to material similarities below the segmentation threshold are used as non-material regions, thereby obtaining all material regions and non-material regions in the hyperspectral image at each moment. The Otsu threshold algorithm is a well-known technology, and the specific process will not be repeated here. The schematic diagram of the material region and non-material region in the hyperspectral image is as follows: Figure 3 As shown, the black area in Figure 3 is all material areas, and the white area is all non-material areas.

[0055] The material area accounts for a large proportion in the hyperspectral image, while the non-material area accounts for a small proportion in the hyperspectral image, indicating that the mixing process is in the initial stage of mixing. At this time, the probability of collision and mixing between different materials is small, which is not conducive to the full and uniform mixing of the mixture.

[0056] Therefore, in this embodiment, the ratio of the number of all non-material areas in the hyperspectral image at each moment to the total number of sub-areas is recorded as the material mixing probability at each moment. The material mixing probability reflects the probability of collision and mixing between different material particles. That is, the larger the material mixing probability, the greater the probability of collision and mixing between different material particles at this time, and the more conducive it is to sufficient and uniform mixing of the mixture.

[0057] Step 3: Based on the average level of material similarity of all material areas at each moment and the correlation between the reflectivity of the pixels at the center of different material areas at each moment, the material penetration resistance at each moment is constructed, and the material movement complexity at each moment is obtained in combination with the material mixing probability.

[0058] In the mixing and stirring process, if you want to stop the mixing and stirring of the mixture in time to avoid the mixing and stirring time being too long, it is necessary to analyze the penetration effect between different material particles. The stronger the penetration effect between different material particles, the more it can be explained that it has been fully mixed at this time, and then stop the mixing and stirring of the mixture in time to avoid wasting preparation time and electric energy.

[0059] Generally speaking, the higher the material similarity in the material area, the higher the uniformity of the material composition in the material area. At the same time, if the difference between the spectral reflectance of pixels between different material areas is greater, it means to a certain extent that the penetration between different materials in the mixing process is smaller, reflecting that the uniformity of the mixture is worse at this time.

[0060] Based on the above analysis, the material penetration resistance at each moment is calculated according to the average level of material similarity of all material areas at each moment and the correlation between the reflectivity of the pixels at the center of different material areas at each moment. The specific expression is:

[0061] Where D t is the material penetration resistance at time t, GX t is the mean of the material similarity of all material regions in the hyperspectral image at time t, m t is the number of material regions in the hyperspectral image at time t, cos() is the cosine similarity, and f t,d and f t,d―1 is the reflectance sequence of the central pixels of the d-th and d-1-th material areas in the hyperspectral image at time t, The purpose of adding 1 to the denominator is to avoid the situation where the denominator is zero. It can be understood that the larger the mean value of the material similarity and the larger the cosine similarity, to a certain extent, it means that the penetration effect of different material particles at the corresponding time is smaller, and the greater the material penetration resistance at this time, that is, the worse the uniformity of the mixed material at this time.

[0062] Generally speaking, the higher the probability of collision and mixing between particles of different materials during the mixing process, and the smaller the barrier characteristics of penetration between particles of different materials, to a certain extent, it explains that the complexity of the mixing movement between particles of different materials is higher. For example, the mixed particles will experience strong collision, penetration, convection mixing and other mixing movement phenomena, which is more conducive to the uniformity of the mixing of the mixture. When the mixing movement between the mixed particles tends to be stable, it means that the mixture has been fully mixed and evenly mixed, and the mixing and stirring of the mixture should be stopped in time.

[0063] Based on the above analysis, the material movement complexity at each moment is obtained according to the material penetration resistance at each moment and the material mixing probability, wherein the material movement complexity at each moment is the ratio of the material mixing probability at each moment to the material penetration resistance. It should be noted that in the process of calculating the ratio, in order to avoid the denominator being zero, a value to avoid the denominator being zero needs to be added to the denominator, which is set to 0.01 in this embodiment.

[0064] It can be understood that the complexity of material movement reflects the complexity of the movement of different material particles in the mixture. The greater the complexity of material movement, the stronger the movement characteristics of collision, penetration and convection mixing between different material particles, which is more conducive to the uniformity of the mixture.

[0065] Step 4: Combine multiple moments closest to each moment into a local moment set. According to the distribution disorder and range of the material movement complexity of all moments in the local moment set of each moment, determine the material mixing change degree at each moment to determine whether to stop stirring.

[0066] Generally, as the mixing time continues, the material movement complexity between different material particles at each moment will change to a large extent, and the uniformity of the mixture will become higher and higher. When the uniformity of the mixture tends to be stable, the change in the material movement complexity between different material particles will tend to be stable, indicating that the mixture has been fully mixed and uniform, and the mixing of the mixture is stopped in time. Therefore, in order to identify the moment when the mixture is fully mixed and uniform, so as to accurately control the mixing time, it is necessary to further analyze the changes in the material movement complexity.

[0067] In order to analyze the change of material movement complexity in local time, in this embodiment, the 20 moments closest to each moment are used to form a local moment set for each moment. Then, according to the distribution disorder and range of the material movement complexity of all moments in the local moment set of each moment, the material mixing change degree at each moment is calculated. The calculation formula in this embodiment is:

[0068] H t =norm(σV t × t ), where H t is the material mixing variation at time t, norm() is the normalization function, σV t is the information entropy of the material movement complexity corresponding to all the moments in the local moment set at moment t, zV t is the range of the material movement complexity corresponding to all moments in the local moment set at time t, where the calculation of information entropy and range value are both well-known technologies, and the specific process is not repeated here. The larger the information entropy and the larger the range, the greater the change in the material movement complexity between the same material particles, and the more it can be explained that the mixture is not fully mixed at this time, and the greater the material mixing change.

[0069] Generally, when the mixture is fully mixed, the change in the complexity of material movement between different material particles tends to be stable, and the material mixing variation is at a low level. Therefore, this embodiment calculates the material mixing variation at each moment in real time to analyze the mixing condition during the stirring process.

[0070] Furthermore, in this embodiment, whether to stop stirring is judged based on the degree of change of material mixing. Specifically, if the degree of change of material mixing corresponding to the current moment is less than the preset threshold value, it is judged that the mixture is fully mixed and uniform at this time, and the mixing and stirring is stopped at this time to enter the next process; if the degree of change of material mixing corresponding to the current moment is greater than the preset threshold value, it is judged that the mixture is not fully mixed and uniform at this time, and the mixing and stirring is continued until the mixture is fully mixed and uniform, that is, the degree of change of material mixing is less than the preset threshold value. In this embodiment, the preset threshold value is 0.1.

[0071] Specifically, the flow chart of judging whether stirring is stopped during mixing and stirring in the ceramsite preparation process in this embodiment is as follows: Figure 4 shown.

[0072] S4, homogenizing, balling and coating the mixed material after being fully mixed and stirred, screening, resting and steaming to obtain ceramsite.

[0073] Preferably, the homogenization process in this embodiment is as follows: the fully mixed and stirred mixture is fed into a homogenizing device, and the discharge requirements of the homogenized mixture are controlled as follows: the particle size is controlled at 0.6 mm, the sieve residue is 13%, and the homogenized mixture is obtained;

[0074] Preferably, the balling and coating process in this embodiment is: the homogenized mixture is sent into a balling machine for balling treatment, and then sent into a coating machine for coating treatment to obtain coated spheres, and the balling machine is equipped with a water spraying device;

[0075] Preferably, the specific process of screening and curing in this embodiment is as follows: in this embodiment, spheres smaller than 19 mm are screened out from the spheres, and the screened spheres are placed in a curing machine for curing for 24 hours. In this embodiment, the curing temperature is 45 degrees and the humidity is 95 degrees for the first six hours, and spraying is performed during the subsequent curing time until the surface of the spheres is visually moistened;

[0076] Preferably, the specific process of cooking preparation in this embodiment is: putting the spheres after resting into a pressure cooker for autoclave treatment, and reacting for 4.5 hours under a saturated steam constant pressure of 1.0 MPa. In this embodiment, the height of the spheres entering the pressure cooker is 3 meters to obtain unfired ceramsite.

[0077] In order to reflect the efficiency brought by using this embodiment to determine the stirring time, further, the difference between the original fixed stirring time and the stirring time of this embodiment is analyzed, and the ratio of the difference to the original fixed stirring time is used as the improvement rate, and multiple groups of implementation combinations are used for comparison. Specifically, Figure 5 As shown in the figure, it is a schematic diagram comparing the effects of 8 groups of implementation combinations using this embodiment and the original fixed stirring time, Figure 5The bar chart without slash marks indicates the original fixed stirring time, the bar chart with slash marks indicates the stirring time of this embodiment, and the black broken line indicates the change of the boost rate, corresponding to the corresponding boost rate in different implementation combinations.

[0078] Compared with the prior art of mixing and stirring the ground mixture, the present embodiment can stop mixing and stirring the mixture in time on the basis of ensuring that the mixture is fully mixed and uniform, thereby avoiding waste of preparation time and electric energy, and can effectively improve the efficiency of preparing expanded clay and reduce the preparation cost of expanded clay.

[0079] Based on the same inventive concept as the above method, an embodiment of the present application also provides a ceramsite prepared by mixing metal tailings and steel slag, and the ceramsite is prepared using the steps of any one of the above methods.

[0080] It is to be understood that the sequence of the embodiments of the present application described above is for description only and does not represent the advantages and disadvantages of the embodiments. The above describes specific embodiments of the present specification. In addition, the processes depicted in the accompanying drawings do not necessarily require the specific order or continuous order shown to achieve the desired results. In some embodiments, multitasking and parallel processing are also possible or may be advantageous.

[0081] The various embodiments in this specification are described in a progressive manner, and the same or similar parts between the various embodiments can be referenced to each other, and each embodiment focuses on the differences from other embodiments.

[0082] The above content is only an implementation method of the present application and is not intended to limit the scope of the present application. Any equivalent structure or equivalent process transformation made using the contents of the present application specification and drawings, or directly or indirectly used in other related technical fields, are also included in the protection scope of the present application.

Claims

1. A method for preparing ceramsite mixed with metal tailings and steel slag, characterized in that: The following steps are involved: crushing the metal tailings and steel slag, and grinding the crushed mixture into powder to obtain a rare earth tailings mixture; Solid-liquid separation of oil drilling slurry to obtain oil drilling waste liquid, impregnation of the rare earth tailings mixture to obtain an impregnation liquid impregnated with the oil drilling waste liquid and the rare earth tailings mixture after impregnation; Take the impregnation liquid impregnated with oil drilling waste liquid and the rare earth tailings mixture impregnated with it, industrial waste bricks, Suzhou soil, high-alumina bauxite, fly ash, silica ash, attapulgite, coal gangue, straw waste, industrial phosphoric acid, steel fiber, phosphogypsum, alumina sol, polypropylene fiber, sodium sulfate, citric acid, benzalkonium chloride, bentonite, river sand and graphite powder, mix and stir, and judge whether to stop stirring according to the high-spectral data analysis of the stirring process. The judgment process is as follows: Collect hyperspectral images of the mixture during the mixing process and divide them into multiple sub-areas; Based on the difference in reflectance between different pixels in each sub-region, the material similarity of each sub-region is constructed, and all material similarity thresholds are segmented to divide the sub-regions into material regions and non-material regions. The ratio of the number of non-material regions in the hyperspectral image at each moment to the total number of sub-regions is determined as the material mixing probability at each moment. According to the average level of material similarity of all material regions at each moment and the correlation between the reflectivity of the pixels at the center of different material regions at each moment, the material penetration resistance at each moment is constructed, and the material movement complexity at each moment is obtained in combination with the material mixing probability; The multiple moments closest to each moment are combined into a local moment set of each moment, and the material mixing change degree of each moment is determined according to the distribution disorder degree and range of the material movement complexity of all moments in the local moment set of each moment, so as to judge whether to stop stirring; The fully mixed and stirred mixture is homogenized, balled, coated, sieved, rested, and steamed to obtain ceramsite.

2. The method for preparing ceramsite mixed with metal tailings and steel slag as claimed in claim 1, characterized in that: The weight ratio of the metal tailings to the steel slag is 1:1, and the grinding fineness is 10% of the residue on a 0.08 mm square hole sieve.

3. The method for preparing ceramsite mixed with metal tailings and steel slag as claimed in claim 1, characterized in that: The immersion temperature is 47° C. and the immersion time is 24 hours.

4. The method for preparing ceramsite mixed with metal tailings and steel slag as claimed in claim 1, characterized in that: 460 parts of rare earth tailings mixture after impregnation with oil drilling waste liquid, 250 parts of impregnation liquid after impregnation, 10 parts of industrial waste bricks, 10 parts of Suzhou soil, 10 parts of high-alumina bauxite, 10 parts of fly ash, 10 parts of silica ash, 10 parts of attapulgite, 10 parts of coal gangue, 10 parts of straw waste, 3 parts of industrial phosphoric acid, 3 parts of steel fiber, 3 parts of phosphogypsum, 3 parts of alumina sol, 2 parts of polypropylene fiber, 2 parts of sodium sulfate, 2 parts of citric acid, 2 parts of benzalkonium chloride, 2 parts of bentonite, 2 parts of river sand, and 2 parts of graphite powder.

5. The method for preparing ceramsite mixed with metal tailings and steel slag as claimed in claim 1, characterized in that: The corresponding calculation formula for the material similarity of each sub-region is: In the formula, G i is the material similarity of the ith sub-region, n is the number of pixels in the sub-region, dtw() is the dtw distance, ∈ is the value to avoid the denominator being zero, g i,j and g i,j―1 is the reflectivity sequence of the jth and j-1th pixels in the i-th sub-region. The reflectivity of each pixel is arranged in ascending order of wavelength to form the reflectivity sequence of each pixel.

6. The method for preparing ceramsite mixed with metal tailings and steel slag as claimed in claim 1, characterized in that: The corresponding calculation formula for the material penetration resistance at each moment is: Where D t is the material penetration resistance at time t, GX t is the mean of the material similarity of all material regions in the hyperspectral image at time t, m t is the number of material regions in the hyperspectral image at time t, cos() is the cosine similarity, and f t,d and f t,d―1 It is the reflectance sequence of the central pixels of the d-th and d-1-th material areas in the hyperspectral image at time t. The reflectance sequence of the central pixel is composed of the reflectance of the central pixel arranged in ascending order of wavelength.

7. The method for preparing ceramsite mixed with metal tailings and steel slag as claimed in claim 1, characterized in that: The material movement complexity at each moment is the ratio of the material mixing probability to the material penetration resistance at each moment.

8. The method for preparing ceramsite mixed with metal tailings and steel slag as claimed in claim 1, characterized in that: Determining the degree of change of material mixing at each moment to determine whether to stop mixing and stirring further includes: H t =norm(σV t × t ), where H t is the material mixing variation at time t, norm() is the normalization function, σV t is the information entropy of the material movement complexity corresponding to all the moments in the local moment set at moment t, zV t is the extreme difference of the material movement complexity corresponding to all moments in the local moment set at moment t; If the material mixing change degree is less than the preset threshold, the stirring is stopped; otherwise, the stirring is continued until the material mixing change degree is less than the preset threshold.

9. The method for preparing ceramsite mixed with metal tailings and steel slag as claimed in claim 1, characterized in that: The discharge requirements of the homogenized mixture are a particle size of 0.6 mm and a sieve residue of 13%; the screening and curing is to screen out spheres smaller than 19 mm from the spheres and put them into a curing machine for curing for 24 hours; the cooking preparation is to autoclave the spheres after curing and react them under a saturated steam constant pressure of 1.0 MPa for 4.5 hours.

10. A ceramsite prepared by mixing metal tailings and steel slag, characterized in that: The ceramsite is prepared by the steps of any one of the methods of claims 1-9.

Citation Information

Patent Citations

  • Preparation method of ion type rare earth tailing porous ceramsite

    CN105801161A

  • Petroleum resin production process separation method and system

    CN117205590A

  • High-performance filter ultrafiltration membrane and preparation method thereof

    CN117753219A

  • Preparation method of energy-saving and heat-insulating wall material

    CN118181794A

  • High-rate sodium ferric phosphate positive electrode material and preparation method thereof

    CN118405680A

Cited By

  • Efficient preparation process of continuous fiber reinforced silicon carbide ceramic-based composite material

    CN122059712A

  • A high-efficiency preparation process of continuous fiber reinforced silicon carbide ceramic matrix composite

    CN122059712B