Atomization fixing agent capable of settling radioactive aerosol and preparation method thereof

By using a combination of a polymer solution of carboxymethylcellulose and polyvinyl alcohol and a surfactant, an efficient biomass atomization fixative was prepared, which solved the low efficiency and toxicity of aerosol removal in the prior art. The problem has achieved efficient and harmless purification and degradation effects of radioactive aerosols.

CN118930739APending Publication Date: 2024-11-12NANHUA UNIV
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411123820.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-15
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

The existing aerosol atomization fixative has low removal efficiency and is toxic, and has secondary pollution problems, making it difficult to meet the purification needs of nuclear facilities for decommissioning and nuclear accident emergency response.

Method used

Using a polymer solution with carboxymethyl cellulose and polyvinyl alcohol as matrix, combined with rhamnolipid and sophoralipid as surfactants, atomized fixation with a network structure and high viscosity is prepared through a free radical polymerization mechanism. to achieve efficient capture and settlement of radioactive aerosols.

Benefits of technology

The biomass atomizing fixative can settle at a rate of 90.80% in 30 minutes, which is non-toxic and harmless, and is biodegradable. It solves the problem of secondary pollution and maintains high viscosity to prevent aerosol flow, achieving Efficient radioaerosol purification.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
  • Figure SMS_2
    Figure SMS_2
  • Figure SMS_3
    Figure SMS_3
Patent Text Reader

Abstract

The invention discloses an atomization fixing agent capable of settling radioactive aerosol and a preparation method thereof.The atomization fixing agent is prepared from, by weight, 100 parts of a high-molecular polymer solution and 1-5 parts of a surfactant, and the high-molecular polymer solution is prepared from, by weight, 1-4 parts of carboxymethylcellulose, 1-4 parts of polyvinyl alcohol, 0.01-0.03 part of an initiator, 0-0.08 part of a cross-linking agent and 200-400 parts of water; the surfactant is prepared from rhamnolipid and sophorolipid. According to the atomization fixing agent capable of settling the radioactive aerosol and the preparation method of the atomization fixing agent, the radioactive aerosol atomization fixing agent has low surface tension, has better wetting and capturing performance on the radioactive aerosol in the air, is more beneficial to pressing of the radioactive aerosol, and can be used for fixing the radioactive aerosol. And meanwhile, the aerosol atomization fixing agent also has the advantage of high viscosity of the existing aerosol atomization fixing agent, and the aerosol pressed by the atomization fixing agent cannot flow everywhere after falling onto the surface of an object, so that secondary pollution caused by radioactive aerosol is prevented.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of aerosol suppression, and particularly relates to an atomizing fixative capable of settling radioactive aerosols and a preparation method thereof. Background Art

[0002] While the development of nuclear science and technology has brought enormous economic benefits to society, it has also inevitably led to numerous unforeseen problems. This is particularly true during nuclear accidents and the decommissioning of nuclear facilities, where large amounts of radioactive aerosols are generated and suspended in the air. These aerosols not only severely impact the environment but can also be inhaled by construction workers, causing irreparable radiation damage. Furthermore, national laws and regulations are increasingly stringent regarding occupational health and environmental protection. Consequently, radioactive aerosols, as a significant hazard in the nuclear energy industry's workplace, have garnered widespread attention, and the purification of these aerosols has become a key research focus in the field of radioactive waste gas treatment.

[0003] Aerosol purification technologies are primarily categorized into four types based on the interaction mechanisms between particles: mechanical dust removal, filtration-based dust removal, wet dust removal, and electrostatic dust removal. Currently, nuclear power plant air purification systems mostly utilize high-efficiency air filters. This mature physical filtration purification technology is highly efficient for aerosols within a large particle size range, but its efficiency is very low for smaller particle sizes, and its use also generates large amounts of radioactive solid waste. Furthermore, due to the unpredictable location and sudden timing of nuclear accident emergencies, more mobile, flexible, and easy-to-operate dust removal technologies are required. Among these technologies, atomization-based fixed-point aerosols containing a specific composition are atomized to produce microscopic droplets, which are then delivered to the treatment area to purify the air. Therefore, wet atomization spray dust removal technology can generally meet these requirements. This decontamination method is not only simple and convenient to operate, generates relatively little waste, but also requires no operator access to the contaminated area, significantly minimizing the radioactive hazard to workers.

[0004] Aerosol fixatives are primarily composed of one or more components, including polymers, polyols, surfactants, and glycerol. However, most current aerosol fixatives are toxic, causing secondary pollution and resistance to degradation after use. Therefore, developing an environmentally friendly aerosol fixative that can efficiently remove radioactive aerosols is of great significance. Summary of the Invention

[0005] The present invention aims to provide an aerosol fixative capable of settling radioactive aerosols and its preparation method, addressing the current problems of low removal efficiency and inherent toxicity of aerosol fixatives. The present invention also provides a method for preparing and using a biomass aerosol fixative for rapid control of radioactive aerosol contamination. While highly effective in purifying radioactive aerosols, the agent is non-toxic and harmless to humans, poses no secondary contamination risk, and is biodegradable. This solution addresses the issue of aerosol contamination during nuclear facility decommissioning and nuclear accident emergency response.

[0006] To achieve the above objectives, the first aspect of the present invention provides an aerosol fixative capable of settling radioactive aerosols, the aerosol fixative comprising, by weight, 100 parts of a polymer solution and 1 to 5 parts of a surfactant, the polymer solution comprising, by weight, 1 to 4 parts of carboxymethyl cellulose, 1 to 4 parts of polyvinyl alcohol, 0.01 to 0.03 parts of an initiator, 0 to 0.08 parts of a cross-linking agent, and 200 to 400 parts of water, the surfactant comprising rhamnolipid and sophorolipid.

[0007] The invention uses carboxymethyl cellulose as a matrix, polyvinyl alcohol as a modified functional monomer, water as a solvent, adopts a free radical polymerization mechanism to prepare a high molecular polymer solution, and then adds a surfactant to modify the high molecular polymer solution.

[0008] The high-molecular-weight polymer solution of the present invention is formed by graft copolymerization of carboxymethyl cellulose and polyvinyl alcohol through aqueous solution polymerization. A biomass surfactant is subsequently added to produce an atomized fixative solution with a network structure, high viscosity, and low surface tension. This novel radioactive aerosol atomized fixative exhibits low surface tension, providing improved wetting and capture of radioactive aerosols in the air, further facilitating their suppression. While also combining the high viscosity advantages of existing aerosol atomized fixatives, the aerosols suppressed by the atomized fixative will not flow freely after landing on surfaces, preventing secondary contamination caused by the radioactive aerosols.

[0009] Preferably, the mass ratio of rhamnolipid to sophorolipid is 9:1.

[0010] Preferably, the initiator is potassium persulfate.

[0011] Preferably, the cross-linking agent is N'N-methylenebisacrylamide.

[0012] A second aspect of the present invention provides a method for preparing an atomized fixative capable of settling radioactive aerosols, comprising the following steps: (1) Mix polyvinyl alcohol and water, heat and stir until completely dissolved to obtain a colorless transparent solution, which is component 1; (2) Carboxymethyl cellulose and water are mixed, heated and stirred until the solution is uniform, then the temperature is raised, an initiator is added and stirred until completely dissolved, to obtain combination 2; (3) Add component 1 to component 2, then add the cross-linking agent, stir evenly, heat to react, and cool to obtain a polymer solution; (4) stirring the rhamnolipid and sophorolipid uniformly at room temperature to obtain a surfactant; (5) Add the surfactant to the polymer solution and stir at room temperature for 1 to 2 hours to obtain an atomized fixative.

[0013] Preferably, the heating temperature in step (1) is 80-90°C.

[0014] Preferably, the heating temperature in step (2) is 40°C, and the heating temperature is 60-80°C.

[0015] Preferably, the heating temperature in step (3) is 60-80° C., and the reaction time is 1-3 h.

[0016] A third aspect of the present invention provides an application of an atomized fixative capable of settling radioactive aerosols, and an application of the atomized fixative in settling radioactive aerosols.

[0017] The radioactive aerosol atomizing fixative of the present invention can be used in general occasions and in nuclear facility decommissioning or nuclear accidents to mitigate accident consequences, prevent pollution spread, and protect the safety of workers and the environment.

[0018] Preferably, the method comprises the following steps: (1) Adding the atomized fixative to water to form a biomass atomized fixative solution with a concentration of 1-5 g / L; (2) Spray the biomass atomized fixative solution onto the radioactive aerosol contaminated area using a siphon atomizing spray gun. The spraying time is 1 minute. After spraying, the solution is left to stand for 30 minutes to complete the sedimentation of the radioactive aerosol.

[0019] The biomass atomized fixative solution of the present invention captures radioactive dust particles and settles on the surface of the object after atomization spraying. As the solvent evaporates, the dust particles are wrapped therein and fixed. The film body is then recovered and processed mechanically to achieve the purpose of decontamination.

[0020] Preferably, the speed of the siphon atomizing spray gun is 200 mL / min and the pressure is 0.1-0.3 MPa.

[0021] Therefore, the present invention adopts an atomized fixative capable of settling radioactive aerosols and a preparation method thereof, which has the following beneficial effects: (1) The biomass atomization sedimentation agent prepared by the present invention uses abundant and renewable biomass materials as raw materials, and the biomass sedimentation agent is environmentally friendly and biodegradable, solving the problem of secondary pollution caused by the adsorption and sedimentation of existing radioactive aerosols; (2) The biomass sedimentation agent prepared by the present invention has a sedimentation efficiency of up to 90.80% for radioactive aerosol dust within 30 minutes after spraying and sedimentation.

[0022] The technical solution of the present invention is further described in detail below through examples. DETAILED DESCRIPTION

[0023] The present invention will be further described below. It should be noted that this embodiment is based on the technical solution and provides a detailed implementation method and specific operation process, but the present invention is not limited to this embodiment.

[0024] Example 1 A biomass atomization fixative for adsorption, precipitation and fixation of radioactive aerosols, the materials of which are selected as follows: 10g carboxymethyl cellulose, 40g polyvinyl alcohol, 0.5g potassium persulfate, 0.75g N'N-methylenebisacrylamide, 2g mixed solution of rhamnolipid and sophorolipid. The mass ratio of rhamnolipid to sophorolipid is 9:1.

[0025] The preparation method of the biomass atomization fixative is specifically as follows: (1) Preparation of polymer solution Dissolve 40 g of polyvinyl alcohol in 2500 ml of deionized water, heat to 90°C, stir until the polyvinyl alcohol is completely dissolved, cool to 60°C, and keep warm for later use.

[0026] 10 g of carboxymethyl cellulose and 2500 ml of deionized water were placed in a three-necked beaker, heated to 40°C, and stirred until the carboxymethyl cellulose was completely dissolved. Subsequently, 0.5 g of potassium persulfate was added, and the temperature was gradually raised to 60°C, and stirred until dissolved.

[0027] The polyvinyl alcohol solution was added to a three-necked beaker containing dissolved carboxymethyl cellulose, followed by the addition of 0.75 g of N'N-methylenebisacrylamide. The mixture was heated and stirred at 60° C. for 2 h, and then cooled and discharged to obtain a high molecular weight polymer solution.

[0028] (2) Preparation of radioactive aerosol pressurized preparations Measure 100 g of the high molecular weight polymer solution, add 2 g of the mixed solution of surfactant rhamnolipid and sophorolipid, stir evenly, seal and refrigerate for use.

[0029] Example 2 A biomass atomization fixative for adsorption, precipitation and fixation of radioactive aerosols, the materials of which are selected as follows: 40g carboxymethyl cellulose, 10g polyvinyl alcohol, 0.5g potassium persulfate, 0.75g N'N-methylenebisacrylamide, 2g mixed solution of rhamnolipid and sophorolipid. The mass ratio of rhamnolipid to sophorolipid is 9:1.

[0030] The preparation method of the biomass atomization fixative is specifically as follows: (1) Preparation of polymer solution Dissolve 10 g of polyvinyl alcohol in 2500 ml of deionized water, heat to 90°C, stir until the polyvinyl alcohol is completely dissolved, cool to 60°C, and keep warm for later use.

[0031] 40 g of carboxymethyl cellulose and 2500 ml of deionized water were placed in a three-necked beaker, heated to 40°C, and stirred until the carboxymethyl cellulose was completely dissolved. Subsequently, 0.5 g of potassium persulfate was added, and the temperature was gradually raised to 60°C, and stirred until dissolved.

[0032] The polyvinyl alcohol solution was added to a three-necked beaker containing dissolved carboxymethyl cellulose, followed by the addition of 0.75 g of N'N-methylenebisacrylamide. The mixture was heated and stirred at 80° C. for 1 h, and then cooled and discharged to obtain a high molecular weight polymer solution.

[0033] (2) Preparation of radioactive aerosol pressurized preparations Measure 100 g of the high molecular weight polymer solution, add 2 g of the mixed solution of surfactant rhamnolipid and sophorolipid, stir evenly, seal and refrigerate for use.

[0034] Example 3 A biomass atomization fixative for adsorption, precipitation and fixation of radioactive aerosols, the materials of which are selected as follows: 30g carboxymethyl cellulose, 20g polyvinyl alcohol, 0.5g potassium persulfate, 0.75g N'N-methylenebisacrylamide, 2g mixed solution of rhamnolipid and sophorolipid. The mass ratio of rhamnolipid to sophorolipid is 9:1.

[0035] The preparation method of the biomass atomization fixative is specifically as follows: (1) Preparation of polymer solution Dissolve 20 g of polyvinyl alcohol in 2500 ml of deionized water, heat to 90°C, stir until the polyvinyl alcohol is completely dissolved, cool to 60°C, and keep warm for later use.

[0036] 30 g of carboxymethyl cellulose and 2500 ml of deionized water were placed in a three-necked beaker, heated to 40°C, and stirred until the carboxymethyl cellulose was completely dissolved. Subsequently, 0.5 g of potassium persulfate was added, and the temperature was gradually raised to 60°C, and stirred until dissolved.

[0037] The polyvinyl alcohol solution was added to a three-necked beaker containing dissolved carboxymethyl cellulose, and then 0.75 g of N'N-methylenebisacrylamide was added. The mixture was heated and stirred at 70° C. for 2 h, and then cooled and discharged to obtain a high molecular weight polymer solution.

[0038] (2) Preparation of radioactive aerosol pressurized preparations Measure 100 g of the high molecular weight polymer solution, add 2 g of the mixed solution of surfactant rhamnolipid and sophorolipid, stir evenly, seal and refrigerate for use.

[0039] Example 4 A biomass atomization fixative for adsorption, precipitation and fixation of radioactive aerosols, the materials of which are selected as follows: 20g carboxymethyl cellulose, 30g polyvinyl alcohol, 0.5g potassium persulfate, 0.75g N'N-methylenebisacrylamide, 2g mixed solution of rhamnolipid and sophorolipid. The mass ratio of rhamnolipid to sophorolipid is 9:1.

[0040] The preparation method of the biomass atomization fixative is specifically as follows: (1) Preparation of polymer solution Dissolve 30 g of polyvinyl alcohol in 2500 ml of deionized water, heat to 90°C, stir until the polyvinyl alcohol is completely dissolved, cool to 60°C, and keep warm for later use.

[0041] 20 g of carboxymethyl cellulose and 2500 ml of deionized water were placed in a three-necked beaker, heated to 40°C, and stirred until the carboxymethyl cellulose was completely dissolved. Subsequently, 0.5 g of potassium persulfate was added, and the temperature was gradually raised to 60°C, and stirred until dissolved.

[0042] The polyvinyl alcohol solution was added to a three-necked beaker containing dissolved carboxymethyl cellulose, and then 0.75 g of N'N-methylenebisacrylamide was added. The mixture was heated and stirred at 65° C. for 2 h, and then cooled and discharged to obtain a high molecular weight polymer solution.

[0043] (2) Preparation of radioactive aerosol pressurized preparations Measure 1 L of the polymer solution, add 2 g of the mixed solution of surfactant rhamnolipid and sophorolipid, stir evenly, seal and refrigerate for use.

[0044] Example 5 A biomass atomization fixative for adsorption, precipitation and fixation of radioactive aerosols, the materials of which are selected as follows: 25g carboxymethyl cellulose, 25g polyvinyl alcohol, 0.5g potassium persulfate, 0.75g N'N-methylenebisacrylamide, 2g mixed solution of rhamnolipid and sophorolipid. The mass ratio of rhamnolipid to sophorolipid is 9:1.

[0045] The preparation method of the biomass atomization fixative is specifically as follows: (1) Preparation of polymer solution Dissolve 25 g of polyvinyl alcohol in 2500 ml of deionized water, heat to 90°C, stir until the polyvinyl alcohol is completely dissolved, cool to 60°C, and keep warm for later use.

[0046] 25 g of carboxymethyl cellulose and 2500 ml of deionized water were placed in a three-necked beaker, heated to 40°C, and stirred until the carboxymethyl cellulose was completely dissolved. Subsequently, 0.5 g of potassium persulfate was added, and the temperature was gradually raised to 60°C, and stirred until dissolved.

[0047] The polyvinyl alcohol solution was added to a three-necked beaker containing dissolved carboxymethyl cellulose, and then 0.75 g of N'N-methylenebisacrylamide was added. The mixture was heated and stirred at 75° C. for 2 h, and then cooled and discharged to obtain a high molecular weight polymer solution.

[0048] (2) Preparation of radioactive aerosol pressurized preparations Measure 100 g of the high molecular weight polymer solution, add 2 g of the mixed solution of surfactant rhamnolipid and sophorolipid, stir evenly, seal and refrigerate for use.

[0049] Comparative Example 1 The difference from Example 1 is that the added amount of polyvinyl alcohol is 50g.

[0050] Comparative Example 2 The difference from Example 1 is that the surfactant is sodium dodecylbenzenesulfonate.

[0051] Comparative Example 3 The difference from Example 1 is that carboxymethyl cellulose is replaced by gelatin.

[0052] Comparative Example 4 The difference from Example 1 is that the mass ratio of rhamnolipid to sophorolipid is 7:3.

[0053] Test Example 1 Analysis of film-forming effect of radioactive aerosol atomized fixative The atomized fixatives prepared in Examples 1-5 were prepared into solutions with a concentration of 5 g / L. These solutions were evenly coated on various substrates (glass, metal, plastic, etc.) and left at room temperature. The curing time and film-forming properties were observed. The curing time was within 48 hours, and continuous film formation was achieved. Mechanical peeling revealed peeling rates exceeding 95%. This demonstrates that the atomized fixatives prepared in this invention can form films that encapsulate aerosols, enabling aerosol removal.

[0054] Test Example 2 Viscosity Adjustment of Radioactive Aerosol Fixatives The atomized fixatives prepared in Examples 1-5 were prepared into solutions with a concentration of 5 g / L. The viscosity was tested at room temperature and found to be between 30 and 450 mPa·s. The solutions were then sealed and stored in a cool, dry place. This demonstrates that the viscosity of the solutions can be controlled by adjusting the monomer ratio in the present invention.

[0055] Test Example 3 Test the dust removal effect of atomized fixative The method for determining the dust removal efficiency of aerosol press agents (atomized fixatives) is as follows: in a confined space with a volume of 1m³, cutting concrete blocks generates aerosols. The concentration of aerosol particles generated is detected by a dust concentration meter. When the aerosol concentration in the confined space reaches 300mg / m³, cutting is stopped. A certain amount of aerosol atomized fixative is taken and sprayed in the contaminated area. The changes in aerosol concentration are recorded in real time by an aerosol detection instrument. The dust removal efficiency of the aerosol press agent can be calculated based on this. The dust removal efficiency calculation formula of the aerosol press agent is as follows:

[0056] The dust reduction efficiency of the aerosol atomized fixative prepared in the examples and comparative examples was tested, and the specific test process is as follows: Step 1: Prepare 5 types of atomized fixatives according to the above Examples 1-5.

[0057] Step 2: Build the test platform. The manual spray gun is connected to the air compressor through a hose. Compressed air is used as the power source of the spray gun. The manual spray gun is equipped with a sample tank (2L). A movable circular opening with a diameter of 10 cm is set on the top of the enclosed space box to facilitate the spray gun to spray samples into the box. The sampling port of the aerosol detection equipment is placed inside the box at a height of half the box height to continuously detect the aerosol concentration value.

[0058] Step 3: Aerosol generation: Use a cutting machine to cut the concrete blocks, and use the aerosol detection system to detect the real-time aerosol concentration. Once the aerosol concentration stabilizes, proceed to step 4.

[0059] Step 4: The aerosol atomized fixative (0.5 g / L) is atomized and introduced into the box through the circular hole on the top of the box. The spray volume is 200 ml, the spray time is 1 min, the pressure is 0.2 MPa, and it is kept still for 30 minutes after spraying. During this process, the changes in aerosol concentration are detected in real time.

[0060] Step 5: Calculation of aerosol deposition efficiency.

[0061] The test results are shown in Tables 1 and 2.

[0062]

[0063] From Table 1, it can be seen that the total suppression efficiency of the aerosols with different viscosities for the 2-105 μm band is between 82% and 88%.

[0064]

[0065] It can be seen from Table 2 that the comparative examples did not adopt the technical solution defined in the present invention, and the pressing efficiency of the prepared atomized fixative decreased to varying degrees.

[0066] Therefore, the present invention adopts an atomizing fixative with the above-mentioned structure capable of settling radioactive aerosols and a preparation method thereof. The present invention not only efficiently purifies aerosols but also has the advantages of high viscosity of existing aerosol pressing agents. After the aerosols are pressed by the pressing agent and fall onto the surface of an object, they will not flow everywhere. In addition, the biomass settling agent prepared by the present invention uses abundant and renewable biomass materials as raw materials. The biomass settling agent is environmentally friendly and biodegradable, and solves the problem of secondary pollution caused by the adsorption and settling of existing radioactive aerosols.

[0067] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention rather than to limit the same. Although the present invention has been described in detail with reference to the preferred embodiments, those skilled in the art should understand that they can still modify or replace the technical solutions of the present invention with equivalents, and these modifications or equivalent replacements cannot cause the modified technical solutions to deviate from the spirit and scope of the technical solutions of the present invention.

Claims

1. An atomizing fixative capable of settling radioactive aerosols, characterized in that: The atomizing fixative comprises 100 parts of a high molecular polymer solution and 1-5 parts of a surfactant in parts by weight, the high molecular polymer comprises 1-4 parts of carboxymethyl cellulose, 1-4 parts of polyvinyl alcohol, 0.01-0.03 parts of an initiator, 0-0.08 parts of a cross-linking agent and 200-400 parts of water in parts by weight, and the surfactant comprises rhamnolipid and sophorolipid.

2. The atomized fixative capable of settling radioactive aerosols according to claim 1, characterized in that: The mass ratio of rhamnolipid to sophorolipid was 9:

1.

3. The atomized fixative capable of settling radioactive aerosols according to claim 1, characterized in that: The initiator is potassium persulfate.

4. The atomized fixative capable of settling radioactive aerosols according to claim 1, characterized in that: The crosslinking agent is N'N-methylenebisacrylamide.

5. The method for preparing an atomized fixative capable of settling radioactive aerosol according to any one of claims 1 to 4, characterized in that: The following steps are involved: (1) Mix polyvinyl alcohol and water, heat and stir until they are completely dissolved to obtain a colorless transparent solution, which is component 1; (2) mixing carboxymethyl cellulose and water, heating and stirring until the solution is uniform, then raising the temperature, adding an initiator and stirring until it is completely dissolved, to obtain combination 2; (3) Add component 1 to component 2, then add a cross-linking agent, stir evenly, heat to react, and cool to obtain a polymer solution; (4) stirring the rhamnolipid and sophorolipid uniformly at room temperature to obtain a surfactant; (5) Add the surfactant to the polymer solution and stir at room temperature for 1 to 2 hours to obtain an atomized fixative.

6. The method for preparing an atomized fixative capable of settling radioactive aerosols according to claim 5, characterized in that: The heating temperature in step (1) is 80-90°C.

7. The method for preparing an atomized fixative capable of settling radioactive aerosols according to claim 5, characterized in that: The heating temperature in step (2) is 40°C, and the heating temperature is 60-80°C.

8. The method for preparing an atomized fixative capable of settling radioactive aerosols according to claim 5, characterized in that: The heating temperature in step (3) is 60-80°C and the reaction time is 1-3h.

9. Use of an atomized fixative capable of settling radioactive aerosols according to any one of claims 1 to 4, characterized in that: Application of aerosolized fixatives in settling radioactive aerosols.

10. The use of an atomized fixative capable of settling radioactive aerosols according to claim 9, characterized in that: The following steps are involved: (1) adding the atomized fixative into water to form a biomass atomized fixative solution with a concentration of 1 to 5 g / L; (2) Spray the biomass atomized fixative solution on the radioactive aerosol contaminated area through a siphon atomizing spray gun. The spraying time is 1 minute. After spraying, let it stand for 30 minutes to complete the sedimentation of the radioactive aerosol.

Citation Information

Cited By

  • Graphene / iron oxyhydroxide-doped pressed preparation as well as preparation method and application thereof