Low-HOMO energy level polythiophene polymer as well as preparation method and application thereof
Low HOMO level polythiophene polymers were prepared by Stille coupling polymerization, which solved the problem of poor miscibility between polythiophene polymers and non-fullerene acceptors, and achieved high-efficiency light energy conversion of organic solar cells with low synthesis cost and excellent performance.
Patent Information
- Application Number
- CN202411051240.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-01
- Publication Date
- 2024-11-12
AI Technical Summary
The high HOMO energy level and active layer morphology of polythiophene polymers result in poor miscibility and compatibility with high-performance non-fullerene acceptors, limiting their application in organic solar cells.
Low HOMO level polythiophene polymers were prepared by Stille coupling polymerization, and side chain modification with thiazole-thiazole units was introduced to reduce the HOMO level. Solar cell thin films were then prepared by spin coating.
A polymer with suitable HOMO and LUMO energy levels and good carrier transport capability was obtained, which improved the light energy conversion efficiency of organic solar cells to 2.99%. Moreover, the synthesis route is simple and low in cost.
Smart Images

Figure CN118930820A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of organic photoelectric functional materials, and in particular to a low HOMO energy level polythiophene polymer and a preparation method and application thereof. Background Art
[0002] Polythiophene polymers are the earliest, most classic and most widely studied class of polymer donor materials at the time. This type of structure has the advantages of simple modification, good planarity and self-assembly performance, and strong carrier transport ability. A PCE of 2.8% was obtained in the blend device of the classic polythiophene polymer, poly 3-hexylthiophene (P3HT) and the fullerene acceptor PC618M. In the following period, by regulating the device morphology and replacing more efficient non-fullerene acceptors such as ICBA, BTP-4Cl and ZY-4Cl, the PCE of the device with poly 3-hexylthiophene (P3HT) also gradually exceeded 10%.
[0003] However, polythiophene polymers have an obvious defect, namely, a high HOMO energy level (-4.9 eV) and an over-mixed active layer morphology, which greatly limits their miscibility and compatibility with most high-performance non-fullerene acceptors currently on the market. Summary of the invention
[0004] In order to reduce the HOMO energy level of a polythiophene polymer, the present invention provides a low HOMO energy level polythiophene polymer and a preparation method thereof.
[0005] The first aspect of the present invention is to provide a low HOMO energy level polythiophene polymer using the following technical solution: a low HOMO energy level polythiophene polymer, the general structure of the low HOMO energy level polythiophene polymer is as follows: Where n is 0-1, and m is 1-n.
[0006] The second aspect of the present invention is to provide a method for preparing a low HOMO energy level polythiophene polymer, comprising the following steps: adding 2,5-bis(5-bromo-4-((2-butyloctyl)thio)thiophene-2-yl)thiazolo[5,4-d]thiazole, 2,5-bis(3-((2-hexyldecyl)oxy)-5-(trimethylstannyl)thiophene-2-yl)thiazolo[5,4-d]thiazole and 2,5-bis(trimethylstannyl)thiophene to a toluene solvent, and obtaining a low HOMO energy level polythiophene polymer through a Stille coupling polymerization reaction under the catalytic action of a catalyst.
[0007] Preferably, the molar ratio of 2,5-bis(5-bromo-4-((2-butyloctyl)thio)thiophene-2-yl)thiazolo[5,4-d]thiazole, 2,5-bis(3-((2-hexyldecyl)oxy)-5-(trimethylstannyl)thiophene-2-yl)thiazolo[5,4-d]thiazole and 2,5-bis(trimethylstannyl)thiophene is 1:a:1-a, wherein a is 0-1.
[0008] Preferably, the temperature of the Stille coupling polymerization reaction is 90-110° C., and the reaction time is 8-24 h.
[0009] Preferably, the catalyst is tetrakis(triphenylphosphine)palladium.
[0010] Preferably, the amount of tetrakis(triphenylphosphine)palladium used is 1-10% of the total mass of 2,5-bis(5-bromo-4-((2-butyloctyl)thio)thiophene-2-yl)thiazolo[5,4-d]thiazole, 2,5-bis(3-((2-hexyldecyl)oxy)-5-(trimethylstannyl)thiophene-2-yl)thiazolo[5,4-d]thiazole and 2,5-bis(trimethylstannyl)thiophene.
[0011] Preferably, the mass ratio of toluene to 2,5-bis(5-bromo-4-((2-butyloctylthio)thiophen-2-yl)thiazolo[5,4-d]thiazole is 50-100:1.
[0012] The third aspect of the present invention is to provide an application of a low HOMO energy level polythiophene polymer in the preparation of an organic solar cell.
[0013] In summary, the present invention has the following beneficial effects: 1. The preparation method of the low HOMO energy level polythiophene polymer provided in the present application has a simple synthesis route. The three raw materials are dissolved in a solvent. Under the catalytic action of the catalyst, only one step of Stille coupling polymerization reaction is required to obtain the low HOMO energy level polythiophene polymer. The post-processing is simple, the synthesis cost is reduced, and it has good application prospects.
[0014] 2. In the present application, 2,5-bis(5-bromo-4-((2-butyloctyl)thio)thiophene-2-yl)thiazo[5,4-d]thiazole (sulfane chain-substituted dithienylthiazo[thiazole]thiazole unit), 2,5-bis(3-((2-hexyldecyl)oxy)-5-(trimethylstannyl)thiophene-2-yl)thiazo[5,4-d]thiazole (oxyane chain-substituted dithienylthiazo[thiazole]thiazole unit) and 2,5-bis(trimethylstannyl)thiophene unit are randomly copolymerized to obtain a side chain The modified thiazolyl thiazole unit is introduced into the polythiophene main chain. Since the thiazolyl thiazole unit contains two electron-withdrawing unsaturated nitrogen-substituted imines (-C=NR), the obtained thiophene-dithiophenyl thiazolyl thiazole polymer POSTTz-Th(n) acquires a certain electron-withdrawing ability, which provides a certain electron density to the conjugated polymer POSTTz-Th(n), thereby reducing the HOMO energy level of the thiophene-dithiophenyl thiazolyl thiazole polymer POSTTz-Th.
[0015] 3. The thiophene-dithienyl thiazolyl thiazole polymer POSTTz-Th obtained in the present application has a suitable HOMO energy level, LUMO energy level and a suitable optical band gap, and has good carrier transport ability. Since oxyalkyl side chains and sulfanyl side chains are introduced at positions 2 and 3 of different thiophenes in the polymer obtained in the present application, respectively, they have strong electron donating ability, can extend absorption, and reduce the optical band gap. Under their synergistic effect, the HOMO energy level of the donor material can be further effectively reduced, reaching -5.21 to -5.28 eV.
[0016] 4. The thiophene-dithiophenylthiazolyl thiazole polymer POSTTz-Th obtained in the present application has good thermal stability and can be widely used in the preparation of organic solar cells. The organic solar cell prepared by blending the polymer obtained in the present application as a donor material with the non-fullerene acceptor Y6 can achieve a device light energy conversion efficiency of 2.99% without annealing or additive optimization.
[0017] 5. The thiophene-dithiophenylthiazolyl thiazole polymer POSTTz-Th obtained in the present application is easily soluble in organic solvents such as dichloromethane and chloroform, so it can be used to prepare solar cell films by spin coating. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 It is the TGA chart of the polymers POSTTz-Th (n=1, m=0) and POSTTz-Th (n=0.9, m=0.1) of Examples 1 and 2 of the present application.
[0019] Figure 2 This is the cyclic voltammetry curve of the polymer POSTTz-Th (n=1, m=0) of Example 1 of the present application.
[0020] Figure 3 This is the cyclic voltammetry curve of the polymer POSTTz-Th (n=0.9, m=0.1) of Example 2 of the present application.
[0021] Figure 4 It is an energy level comparison diagram of the polymers POSTTz-Th (n=1, m=0) and POSTTz-Th (n=0.9, m=0.1) of Examples 1 and 2 of the present application and the polythiophene polymer P3HT.
[0022] Figure 5 This is the J–V curve of the non-fullerene solar cell prepared using the polymer POSTTz-Th (n=1, m=0) in Example 1 of the present application. DETAILED DESCRIPTION
[0023] The present invention is further described in detail below in conjunction with the accompanying drawings.
[0024] Example 1 The synthetic route of thiophene-dithienyl thiazolyl thiazole polymer POSTTz-Th (n=1, m=0) is as follows: The specific preparation method of thiophene-dithiophenyl thiazolyl thiazole polymer POSTTz-Th (n=1, m=0) comprises the following steps: under nitrogen protection, 159.26 mg (0.15 mmol) of 2,5-bis (5-bromo-4- ((2-butyloctyl) thio) phen-2-yl) thiazolyl [5,4-d] thiazole, 62.05 mg (0.15 mol) of 2,5-bis (trimethylstannyl) thiophene, 20 mg of tetrakis (triphenylphosphine) ) Palladium and 11 mL toluene were added to a 25 mL two-necked round-bottom flask, and the reaction was refluxed at 110 ° C for 24 hours until the reaction system became viscous, and then the mixture was poured into 100 mL of anhydrous methanol and precipitated. Soxhlet extraction was used to separate low molecular weight oligomers to purify the polymer. Acetone, ether, dichloromethane and chloroform were used as extractants in turn. The collected chloroform solution was concentrated and precipitated with anhydrous methanol, and vacuum dried to obtain 70 mg of blue-black solid. GPC: number average molecular weight (Mn) = 35.57 kDa; weight average molecular weight (Mw) = 68.39 kDa, polydispersity index (PDI) = 1.92.
[0025] Example 2 The synthetic route of thiophene-dithienyl thiazolyl thiazole polymer POSTTz-Th (n=0.9, m=0.1) is as follows: The specific preparation method of thiophene-dithienyl thiazolyl thiazole polymer POSTTz-Th (n=0.9, m=0.1) comprises the following steps: Under nitrogen protection, 216.24 mg (0.25 mmol) of 2,5-bis (5-bromo-4- ((2-butyloctyl) thio) thiophene-2-yl) thiazolo [5,4-d] thiazole, 27.82 mg (0.025 mmol) of 2,5-bis (3- ((2-hexyldecyl) oxy) -5- (trimethylstannyl) thiophene-2-yl) thiazolo [5,4-d] thiazole, 93.08 mg (0.225 mol) of 2,5-bis (trimethylstannyl) Thiophene, 20 mg of tetrakis(triphenylphosphine)palladium and 15 mL of toluene were added to a 25 mL two-necked round-bottom flask, and the mixture was refluxed at 110°C for 8 h until the reaction system became viscous. The mixture was then poured into 100 mL of anhydrous methanol and precipitated. After filtration, the polymer was thermally dissolved in chloroform and rapidly filtered through a silica gel column (eluent: chloroform) to separate low molecular weight oligomers. The collected chloroform solution was concentrated and precipitated with anhydrous methanol, and vacuum dried to obtain 110 mg of a blue-black solid. GPC: number average molecular weight (Mn) = 17.31 kDa; weight average molecular weight (Mw) = 30.81 kDa, polydispersity index (PDI) = 1.78.
[0026] Example 3 The synthetic route of thiophene-dithienyl thiazolyl thiazole polymer POSTTz-Th (n=0.8, m=0.2) is as follows: The specific preparation method of thiophene-dithienyl thiazolyl thiazole polymer POSTTz-Th (n=0.8, m=0.2) comprises the following steps: Under nitrogen protection, 216.24 mg (0.25 mmol) of 2,5-bis (5-bromo-4- ((2-butyloctyl) thio) thiophene-2-yl) thiazolo [5,4-d] thiazole, 27.82 mg (0.05 mmol) of 2,5-bis (3- ((2-hexyldecyl) oxy) -5- (trimethylstannyl) thiophene-2-yl) thiazolo [5,4-d] thiazole, 93.08 mg (0.2 mmol) of 2,5-bis (trimethylstannyl) thiophene Phthene, 20 mg tetrakis(triphenylphosphine)palladium and 15 mL toluene were added to a 25 mL two-necked round-bottom flask, refluxed at 90 ° C for 24 h until the reaction system became viscous, then the mixture was poured into 100 mL of anhydrous methanol and precipitated, the polymer was thermally dissolved in chloroform after filtration, and quickly filtered through a silica gel column (eluent: chloroform) to separate low molecular weight oligomers, the collected chloroform solution was concentrated and precipitated with anhydrous methanol, and vacuum dried to obtain 123 mg of blue-black solid. GPC: number average molecular weight (Mn) = 19.53 kDa; weight average molecular weight (Mw) = 35.82 kDa, polydispersity index (PDI) = 1.83.
[0027] Example 4 The synthetic route of thiophene-dithienyl thiazolyl thiazole polymer POSTTz-Th (n=0.7, m=0.3) is as follows: The specific preparation method of thiophene-dithienyl thiazolyl thiazole polymer POSTTz-Th (n=0.7, m=0.3) comprises the following steps: Under nitrogen protection, 216.24 mg (0.25 mmol) of 2,5-bis(5-bromo-4-((2-butyloctyl)thio)thiophen-2-yl)thiazolo[5,4-d]thiazole, 27.82 mg (0.075 mmol) of 2,5-bis(3-((2-hexyldecyl)oxy)-5-(trimethylstannyl)thiophen-2-yl)thiazolo[5,4-d]thiazole, 93.08 mg (0.175 mmol) of 2,5-bis(trimethylstannyl)thiophene, 20 mg of tetrakis(triphenylphosphine)palladium and 15 mL of toluene were added into a 25 mL two-necked round-bottom flask, and the mixture was refluxed at 110° C. for 24 h until the reaction system became viscous. The mixture was then poured into 100 mL of anhydrous methanol and precipitated. After filtration, the polymer was thermally dissolved in chloroform and quickly filtered through a silica gel column (eluent: chloroform) to separate low molecular weight oligomers. The collected chloroform solution was concentrated and precipitated with anhydrous methanol and vacuum dried to obtain 107 mg of a blue-black solid.
[0028] Example 5 The synthetic route of thiophene-dithienyl thiazolyl thiazole polymer POSTTz-Th (n=0.6, m=0.4) is as follows: The invention discloses a method for preparing a thiophene-dithiophenyl thiazolyl thiazole polymer POSTTz-Th (n=0.6, m=0.4), comprising the following steps: under nitrogen protection, 216.24 mg (0.25 mmol) of 2,5-bis(5-bromo-4-((2-butyloctyl)thio)thiophene-2-yl)thiazolyl[5,4-d]thiazole, 27.82 mg (0.1 mmol) of 2,5-bis(3-((2-hexyldecyl)oxy)-5-(trimethylstannyl)thiophene-2-yl)thiazolyl[5,4-d]thiazole, 93.08 mg (0.15 mmol) of 2,5-bis(trimethylstannyl)thiophene, 20 mg of tetrakis(triphenylphosphine)palladium and 15 mL of toluene are added into a 25 mL two-necked round-bottom flask, and the mixture is refluxed at 110° C. for 24 h until the reaction system becomes viscous. The mixture was then poured into 100 mL of anhydrous methanol and precipitated. After filtration, the polymer was thermally dissolved in chloroform and quickly filtered through a silica gel column (eluent: chloroform) to separate low molecular weight oligomers. The collected chloroform solution was concentrated and precipitated with anhydrous methanol and vacuum dried to obtain 112 mg of a blue-black solid.
[0029] Performance Testing 1. Thermal stability test: The thermal stability of the thiophene-dithienyl thiazolyl thiazole polymer POSTTz-Th obtained in Examples 1-5 was tested using a thermal analyzer TGA Q50 V20.8 Build34. The test conditions were: in a dry nitrogen atmosphere, the temperature was increased at a rate of 20°C / min to test the thermal stability. The corresponding thermal weight loss curve is shown in FIG. Figure 1 As shown, Figure 1 The results show that the thermal decomposition temperature of the thiophene-dithiophenyl thiazolyl polymer POSTTz-Th prepared in Example 1 is 390°C, and the thermal decomposition temperature of the thiophene-dithiophenyl thiazolyl polymer POSTTz-Th prepared in Example 2 is 349°C, indicating that the two polymers obtained in Examples 1 and 2 have good thermal stability and can be applied to organic solar cells. The thermal decomposition temperature of the thiophene-dithiophenyl thiazolyl polymer POSTTz-Th prepared in Example 3 is 290°C, the thermal decomposition temperature of the thiophene-dithiophenyl thiazolyl polymer POSTTz-Th prepared in Example 4 is 284°C, and the thermal decomposition temperature of the thiophene-dithiophenyl thiazolyl polymer POSTTz-Th prepared in Example 5 is 25°C. It can be seen that the thermal stability of the thiophene-dithiophenyl thiazolyl polymer POSTTz-Th obtained in Examples 3-5 is relatively poor.
[0030] 2. HOMO and LUMO energy level test: Cyclic voltammetry (CV) was used to measure the HOMO and LUMO energy levels of the thiophene-dithiophenyl thiazolyl thiazole polymer POSTTz-Th obtained in Example 1 and Example 2. Since the thiophene-dithiophenyl thiazolyl thiazole polymer POSTTz-Th prepared in Example 3 and Comparative Examples 1-2 had too good solubility and was difficult to form a film, it could not be tested. The test conditions were: 0.1 mol / L tetrabutylammonium hexafluorophosphate in acetonitrile solution, Pt as the working electrode, Ag / AgCl as the reference electrode, ferrocene (Fc / Fc + ) is the internal standard; the calculation of the electron energy level refers to the following empirical formula: E HOMO =-e(E ox +4.80), E LUMO =-e(E red +4.80), where E g opt is the optical band gap. The cyclic voltammetry curves of the two copolymers are shown in Figure 2 and Figure 3 As shown, the initial oxidation potential (E ox ) are 1.82V and 1.73V respectively. In fact, the reduction potential (E red ) are 0.48V and 0.41V respectively. According to the above empirical formula, the HOMO energy level of the thiophene-dithiophenyl thiazolyl thiazole polymer POSTTz-Th of Example 1 is calculated to be -5.28eV, the HOMO energy level of the thiophene-dithiophenyl thiazolyl thiazole polymer POSTTz-Th of Example 2 is -5.21eV, the LUMO energy level of the thiophene-dithiophenyl thiazolyl thiazole polymer POSTTz-Th of Example 1 is -3.52eV, and the LUMO energy level of the thiophene-dithiophenyl thiazolyl thiazole polymer POSTTz-Th of Example 2 is -3.68eV. The results show that: Figure 4 The HOMO energy levels of the two prepared polymers are significantly lower than the HOMO energy level of the traditional polythiophene polymer P3HT (about -4.90 eV), which is conducive to obtaining a high open circuit voltage. At the same time, it proves that introducing side chain modified thiazole and thiazole units into polythiophene is an effective strategy to lower its HOMO energy level.
[0031] 3. Photovoltaic performance test: Since the thiophene-dithiophenyl thiazolyl thiazole polymer POSTTz-Th obtained in Examples 2-5 is difficult to form a film during the photovoltaic performance test, only the thiophene-dithiophenyl thiazolyl thiazole polymer POSTTz-Th (n=1, m=0) obtained in Example 1 was tested for photovoltaic performance. The current-voltage curve of the bulk heterojunction organic solar cell based on the thiophene-dithiophenyl thiazolyl thiazole polymer POSTTz-Th (n=1, m=0) is shown in FIG. Figure 5 As shown, when the thiophene-dithiophenyl thiazolyl thiazole polymer POSTTz-Th (n=1, m=0) is blended with Y6 at a ratio of 1:1.2, the photovoltaic performance results are shown in Table 1.
[0032] Table 1 Photovoltaic performance results of polymers PBF-STTz1 and PBSiCl-STTz1 Active layer <![CDATA[V oc (V)]]> <![CDATA[J sc (mA / cm 2 )]]> FF(%) PCE(%) PSTTz-Th:Y6 0.654 10.96 41.81 2.99 From the results in Table 1, it can be seen that when thiophene-dithienyl thiazolyl thiazole polymer POSTTz-Th (n=1, m=0) is blended with Y6, the short-circuit current J sc =10.96mAcm -2 , open circuit voltage V oc =0.654V, fill factor FF=41.81%, energy conversion efficiency PCE=2.99%, and it has good photovoltaic characteristics.
[0033] The embodiments of this specific implementation method are all preferred embodiments of the present invention, and are not intended to limit the protection scope of the present invention. Therefore, any equivalent changes made based on the structure, shape, and principle of the present invention should be included in the protection scope of the present invention.
Claims
1. A low HOMO level polythiophene polymer, Features: The general structure of the low HOMO energy level polythiophene polymer is as follows: Where n is 0-1, and m is 1-n.
2. The method for preparing a low HOMO level polythiophene polymer according to claim 1, It is characterized in that The method comprises the following steps: adding 2,5-bis(5-bromo-4-((2-butyloctyl)thio)thiophene-2-yl)thiazolyl[5,4-d]thiazole, 2,5-bis(3-((2-hexyldecyl)oxy)-5-(trimethylstannyl)thiophene-2-yl)thiazolyl[5,4-d]thiazole and 2,5-bis(trimethylstannyl)thiophene into a toluene solvent, and obtaining a low HOMO energy level polythiophene polymer through a Stille coupling polymerization reaction under the catalytic action of a catalyst.
3. The method for preparing a low HOMO level polythiophene polymer according to claim 2, Features: The molar ratio of the 2,5-bis(5-bromo-4-((2-butyloctyl)thio)thiophene-2-yl)thiazolo[5,4-d]thiazole, 2,5-bis(3-((2-hexyldecyl)oxy)-5-(trimethylstannyl)thiophene-2-yl)thiazolo[5,4-d]thiazole and 2,5-bis(trimethylstannyl)thiophene is 1:a:1-a, wherein a is 0-1.
4. The method for preparing a low HOMO level polythiophene polymer according to claim 2, Features: The temperature of the Stille coupling polymerization reaction is 90-110°C and the reaction time is 8-24h.
5. The method for preparing a low HOMO level polythiophene polymer according to claim 2, Features: The catalyst is tetrakis(triphenylphosphine)palladium.
6. The method for preparing a low HOMO level polythiophene polymer according to claim 5, Features: The amount of tetrakis(triphenylphosphine)palladium used is 1-10% of the total mass of 2,5-bis(5-bromo-4-((2-butyloctyl)thio)thiophen-2-yl)thiazolo[5,4-d]thiazole, 2,5-bis(3-((2-hexyldecyl)oxy)-5-(trimethylstannyl)thiophen-2-yl)thiazolo[5,4-d]thiazole and 2,5-bis(trimethylstannyl)thiophene.
7. The method for preparing a low HOMO level polythiophene polymer according to claim 2, Features: The mass ratio of toluene to 2,5-bis(5-bromo-4-((2-butyloctyl)thio)thiophene-2-yl)thiazolo[5,4-d]thiazole is 50-100:
1.
8. Use of the low HOMO energy level polythiophene polymer according to claim 1 in preparing an organic solar cell.
Citation Information
Patent Citations
Preparation and application of A2-pi-A1-pi-A2 type small molecule receptor materials taking thiazolothiazole as core
CN108794509A
Thiazolothiazole linear conjugated polymer as well as preparation method and application thereof
CN114409878A
Novel polythiophene derivatives and organic thin film transistor using the same
KR1020100086197A