PVC lubricant and preparation process thereof

By optimizing the PVC lubricant formulation and preparation process, the problems of poor fluidity and insufficient environmental friendliness of traditional lubricants in PVC product manufacturing have been solved, achieving more efficient processing and environmentally friendly production, and improving product quality and mold life.

CN118931209AInactive Publication Date: 2024-11-12YUNLIAN HI-TECH (JIANGXI) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410987822.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-23
Publication Date
2024-11-12
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Traditional PVC lubricants are inadequate in terms of performance and environmental friendliness, leading to problems such as poor flowability, difficulty in demolding, and poor surface quality in PVC products during production, and they do not meet the requirements of sustainable development.

Method used

A PVC lubricant formula containing specific proportions of mineral oil, soybean oil, lemon essential oil, and other ingredients is used, and precise preparation process steps, including mixing, heating, pressurization, and microwave treatment, are employed to ensure that the raw materials are fully mixed and reacted in the reaction vessel.

Benefits of technology

It improves the fluidity and compatibility of PVC materials, enhances surface quality and appearance, strengthens stability, reduces energy consumption, minimizes environmental hazards, extends mold life, and meets environmental protection requirements.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention relates to the technical field of homopolymers or copolymers of vinyl chloride, and discloses a PVC (polyvinyl chloride) lubricant. The lubricating oil is prepared from the following components in parts by weight: 28 to 50 parts of mineral oil, 20 to 30 parts of soybean oil, 6 to 9 parts of lemon essential oil, 3 to 11 parts of epoxy resin, 5 to 6 parts of fatty alcohol ester, 20 to 32 parts of glycerol ricinoleate, 32 to 60 parts of epoxidized soybean oil, 23 to 35 parts of pentaerythritol ester, 8 to 16 parts of white calcium stearate, 10 to 15 parts of organic amino compound, 3 to 7 parts of epoxy compound, 1 to 5 parts of zinc soap, 11 to 20 parts of tin thioglycolate, 3 to 6 parts of organic pentaphosphorus and 3 to 5 parts of octadecanol. The invention discloses a PVC (polyvinyl chloride) lubricant and a preparation process thereof, the PVC lubricant comprises the following components in parts by weight: 13-16 parts of calcium stearate, 7-11 parts of fumaric acid, 2.5-4 parts of alkyd resin, 3-8 parts of white calcium stearate, 4-7 parts of lead stearate, 2-7 parts of acetic ether, 3-5 parts of cetearyl alcohol, 0.5-2 parts of ethylene glycol and 0.1-1.5 parts of cetyl alcohol, according to the PVC lubricant and the preparation process thereof, by adopting an optimized formula and an advanced preparation process, the flowability of a PVC material can be remarkably improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of homopolymers or copolymers of vinyl chloride, in particular to a PVC lubricant and a preparation process thereof. Background Art

[0002] In the processing of PVC materials, the use of lubricants is crucial. Traditional PVC lubricants often have certain limitations in performance, such as unsatisfactory lubrication, poor compatibility with PVC materials, and insufficient stability. This may lead to problems such as poor fluidity, difficulty in demoulding, and poor surface quality in the production process of PVC products, affecting product quality and production efficiency.

[0003] In addition, with the continuous improvement of environmental protection requirements, some ingredients that may be contained in traditional lubricants are not friendly to the environment and do not conform to the trend of sustainable development of modern industry. Therefore, it is urgent to develop an improved version of PVC lubricant with better performance, environmental protection and high efficiency. Summary of the invention

[0004] 1. Technical issues to be resolved

[0005] In view of the deficiencies in the prior art, the present invention provides a PVC lubricant and a preparation process thereof, which have the advantages of high surface quality and aesthetic appearance of the product and solve the problem of poor surface quality.

[0006] (II) Technical solution

[0007] To achieve the above object, the present invention provides the following technical scheme: a PVC lubricant, comprising the following specific formula and proportion: mineral oil: 28-50 parts, soybean oil: 20-30 parts, lemon essential oil: 6-9 parts, epoxy resin: 3-11 parts, fatty alcohol: 5-6 parts, glycerol ricinoleate: 20-32 parts, epoxy soybean oil: 32-60 parts, pentaerythritol: 23-35 parts, calcium stearate: 8-16 parts, organic amino compound: 10- 15 parts, epoxy compound: 3-7 parts, zinc soap: 1-5 parts, tin thioglycolate: 11-20 parts, organic pentaphosphorus: 3-6 parts, octadecyl alcohol: 3-5 parts, calcium stearate: 13-16 parts, fumaric acid: 7-11 parts, alkyd resin: 2.5-4 parts, white calcium stearate: 3-8 parts, lead stearate: 4-7 parts, ethyl acetate: 2-7 parts, spermaceti alcohol: 3-5 parts, ethylene glycol: 0.5-2 parts and hexadecanol: 0.1-1.5 parts.

[0008] Preferably, a PVC lubricant preparation process comprises the following specific steps: step 1: accurately measuring the formulated amount of epoxy soybean oil, pentaerythritol fat, calcium stearate, organic amino compound, epoxy compound and zinc soap, and placing them in a mixer;

[0009] Step 2: Accurately measure the formula amount of tin thioglycolate, organic pentaphosphorus, octadecyl alcohol, calcium stearate, fumaric acid, alkyd resin, white calcium stearate and lead stearate, and place them in a heating mixer;

[0010] Step 3: Open the reactor and preheat to 45-70 degrees;

[0011] Step 4: Accurately measure the formulated amount of mineral oil, soybean oil, lemon essential oil, epoxy resin, fatty alcohol, glycerol ricinoleate, ethyl acetate, cetearyl alcohol, ethylene glycol and hexadecanol, and place them into the preheated reactor;

[0012] Step 5: Slowly add the mixture in step 1 into the reactor, raise the temperature of the reactor to 140-155 degrees, and continue stirring for 10 minutes;

[0013] Step 6: Add the mixture heated and stirred in step 2 into the reactor, mix it with the original raw materials in the reactor, and stir the reactor under pressure, maintaining the pressure between 0.1-0.25MPa;

[0014] Step 7: taking out the mixed material after heating, pressurizing and stirring in step 6, and putting it into a microwave processor for microwave heating treatment;

[0015] Step 8: Filter the mixed material processed in step 7, cool it down and condense it into crystals through the cooling system, and then inspect it by slicing. If it is qualified, it will be packaged as a finished product

[0016] Preferably, in step 1, the mixer rotates at a constant speed of 60-75 revolutions per minute for thorough mixing.

[0017] Preferably, in the step 2, heating and stirring are heated to 90-120 degrees, and stirring is continued at a speed of 300-350 revolutions per minute for 10-20 minutes.

[0018] Preferably, in step 4, the temperature of the reactor is slowly raised to 120-140 degrees while stirring at 300-450 revolutions per minute.

[0019] Preferably, in step seven, the microwave treatment frequency is set to 750-920 MHZ, the temperature is set to 50-75 degrees, and the heating treatment is performed for 3-6 minutes.

[0020] (III) Beneficial effects

[0021] Compared with the prior art, the present invention provides a PVC lubricant and a preparation process thereof, which have the following beneficial effects:

[0022] 1. The PVC lubricant and its preparation process, by adopting an optimized formula and an advanced preparation process, can significantly improve the fluidity of the PVC material, making it easier to form during the processing, thereby improving production efficiency, enhancing compatibility with the PVC material, ensuring that the lubricant can be evenly distributed, effectively reducing defects on the surface of the product, improving the surface quality and appearance of the product, having excellent stability, maintaining good lubrication performance under different processing conditions, reducing the risk of unstable product quality caused by fluctuations in lubricant performance, and the selected raw materials pay more attention to environmental protection, reducing potential harm to the environment, meeting the requirements of sustainable development, improving the demoulding performance of PVC products, reducing resistance and damage during demoulding, and extending the service life of the mold. The optimized lubricant can reduce energy consumption during processing and save production costs. DETAILED DESCRIPTION

[0023] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0024] The invention provides a technical method, a PVC lubricant and a preparation process thereof. The PVC lubricant comprises the following specific formula and proportion: mineral oil: 28-50 parts, soybean oil: 20-30 parts, lemon essential oil: 6-9 parts, epoxy resin: 3-11 parts, fatty alcohol fat: 5-6 parts, glycerol ricinoleate: 20-32 parts, epoxy soybean oil: 32-60 parts, pentaerythritol fat: 23-35 parts, calcium stearate: 8-16 parts, organic amino compound: 1 0-15 parts, epoxy compound: 3-7 parts, zinc soap: 1-5 parts, tin thioglycolate: 11-20 parts, organic pentaphosphorus: 3-6 parts, octadecyl alcohol: 3-5 parts, calcium stearate: 13-16 parts, fumaric acid: 7-11 parts, alkyd resin: 2.5-4 parts, white calcium stearate: 3-8 parts, lead stearate: 4-7 parts, ethyl acetate: 2-7 parts, spermaceti alcohol: 3-5 parts, ethylene glycol: 0.5-2 parts and hexadecanol: 0.1-1.5 parts;

[0025] A PVC lubricant preparation process comprises the following specific steps: step 1: accurately measuring the formulated amount of epoxy soybean oil, pentaerythritol fat, calcium stearate, organic amino compound, epoxy compound and zinc soap, placing them in a mixer, and rotating them at a uniform speed of 60-75 revolutions per minute to fully mix them;

[0026] Step 2: Accurately measure the formula amount of tin thioglycolate, organic pentaphosphorus, octadecyl alcohol, calcium stearate, fumaric acid, alkyd resin, white calcium stearate and lead stearate, place them in a heating mixer, heat to 90-120 degrees, and stir continuously at a speed of 300-350 revolutions per minute for 10-20 minutes;

[0027] Step 3: Open the reactor and preheat to 45-70 degrees;

[0028] Step 4: Accurately measure the formulated amount of mineral oil, soybean oil, lemon essential oil, epoxy resin, fatty alcohol, glyceryl ricinoleate, ethyl acetate, cetearyl alcohol, ethylene glycol and hexadecanol, place them in a preheated reactor, and slowly raise the temperature to 120-140 degrees while stirring at 300-450 revolutions per minute;

[0029] Step 5: Slowly add the mixture in step 1 into the reactor, raise the temperature of the reactor to 140-155 degrees, and continue stirring for 10 minutes;

[0030] Step 6: Add the mixture heated and stirred in step 2 into the reactor, mix it with the original raw materials in the reactor, and stir the reactor under pressure, maintaining the pressure between 0.1-0.25MPa;

[0031] Step 7: Take out the mixed material after heating, pressurizing and stirring in step 6, put it into a microwave processor for microwave heating treatment, set the microwave frequency to 750-920MHZ, set the temperature to 50-75 degrees, and heat for 3-6 minutes;

[0032] Step 8: Filter the mixed material processed in step 7, cool it down and condense it into crystals through a cooling system, and then inspect it by slicing. If it is qualified, package it as a finished product.

[0033] Furthermore, during the preparation process, the raw materials must be accurately weighed in strict accordance with the recipe ratio and the raw materials must be of high quality.

[0034] Furthermore, the temperature and pressure of the reactor must be precisely controlled within an appropriate range to ensure the smooth implementation of the reaction and the excellent quality of the product.

[0035] Furthermore, the frequency and temperature of the microwave processor should be flexibly adjusted according to actual conditions to achieve the best processing effect.

[0036] Furthermore, during the filtration and cooling condensation crystallization operations, the operating specifications must be strictly followed to prevent the product from being contaminated or damaged.

[0037] The PVC lubricant adopts an optimized formula and advanced preparation technology, which can significantly improve the fluidity of PVC materials, making it easier to form during the processing, thereby improving production efficiency, enhancing compatibility with PVC materials, ensuring that the lubricant can be evenly distributed, effectively reducing defects on the surface of products, improving the surface quality and appearance of products, and having excellent stability. It can maintain good lubrication performance under different processing conditions, reducing the risk of unstable product quality due to fluctuations in lubricant performance. The selected raw materials pay more attention to environmental protection, reduce potential harm to the environment, meet the requirements of sustainable development, improve the demoulding performance of PVC products, reduce resistance and damage during demoulding, and extend the service life of the mold. The optimized lubricant can reduce energy consumption in the processing process and save production costs.

[0038] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A PVC lubricant, characterized in that: The specific formula and proportion include: mineral oil: 28-50 parts, soybean oil: 20-30 parts, lemon essential oil: 6-9 parts, epoxy resin: 3-11 parts, fatty alcohol: 5-6 parts, glycerol ricinoleate: 20-32 parts, epoxy soybean oil: 32-60 parts, pentaerythritol: 23-35 parts, calcium stearate: 8-16 parts, organic amino compound: 10-15 parts, epoxy compound: 3-7 parts, Zinc soap: 1-5 parts, tin thioglycolate: 11-20 parts, organic pentaphosphorus: 3-6 parts, octadecyl alcohol: 3-5 parts, calcium stearate: 13-16 parts, fumaric acid: 7-11 parts, alkyd resin: 2.5-4 parts, white calcium stearate: 3-8 parts, lead stearate: 4-7 parts, ethyl acetate: 2-7 parts, spermaceti alcohol: 3-5 parts, ethylene glycol: 0.5-2 parts and hexadecanol: 0.1-1.5 parts.

2. A PVC lubricant preparation process, characterized in that: The method comprises the following specific steps: step 1: accurately measuring the formulated amounts of epoxy soybean oil, pentaerythritol fat, calcium stearate, organic amino compound, epoxy compound and zinc soap, and placing them in a mixer; Step 2: Accurately measure the formula amount of tin thioglycolate, organic pentaphosphorus, octadecyl alcohol, calcium stearate, fumaric acid, alkyd resin, white calcium stearate and lead stearate, and place them in a heating mixer; Step 3: Open the reactor and preheat to 45-70 degrees; Step 4: Accurately measure the formulated amount of mineral oil, soybean oil, lemon essential oil, epoxy resin, fatty alcohol, glycerol ricinoleate, ethyl acetate, cetearyl alcohol, ethylene glycol and hexadecanol, and place them into the preheated reactor; Step 5: Slowly add the mixture in step 1 into the reactor, raise the temperature of the reactor to 140-155 degrees, and continue stirring for 10 minutes; Step 6: Add the mixture heated and stirred in step 2 into the reactor, mix it with the original raw materials in the reactor, and stir the reactor under pressure, maintaining the pressure between 0.1-0.25MPa; Step 7: taking out the mixed material after heating, pressurizing and stirring in step 6, and putting it into a microwave processor for microwave heating treatment; Step 8: Filter the mixed material processed in step 7, cool it down and condense it into crystals through a cooling system, and then inspect it by slicing. If it is qualified, package it as a finished product.

3. A PVC lubricant preparation process according to claim 2, characterized in that: In the step 1, the mixer is rotated at a constant speed of 60-75 revolutions per minute to perform thorough mixing.

4. A process for preparing a PVC lubricant according to claim 1, characterized in that: The second step is heating and stirring to 90-120 degrees, and stirring continuously at a speed of 300-350 revolutions per minute for 10-20 minutes.

5. A process for preparing a PVC lubricant according to claim 1, characterized in that: In the step 4, the temperature of the reactor is slowly raised to 120-140 degrees under stirring at 300-450 revolutions per minute.

6. A process for preparing a PVC lubricant according to claim 1, characterized in that: In the step 7, the microwave treatment frequency is set to 750-920 MHZ, the temperature is set to 50-75 degrees, and the heating treatment is performed for 3-6 minutes.