Foam acidizing fluid system, preparation method and performance verification test
By adding weak acid and corrosion inhibitor to the acidizing liquid, and using foaming agent and foam stabilizer to form foam acidification liquid, the problems of small acidification distance and high corrosion risk are solved, and efficient production increase and equipment protection of dolomite thermal storage are achieved .
Patent Information
- Application Number
- CN202411002712.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-25
- Publication Date
- 2024-11-12
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing acidification liquid system has a small acidification distance in dolomite thermal storage, which is prone to retention, resulting in poor thermal storage and production increase effect, and has a high risk of corrosion to downhole equipment.
Using foam acidification liquid system, the acidification liquid with slow and corrosion inhibition is formed by combining acid solution (combination of strong acid and weak acid), foaming agent, foam stabilizing agent and corrosion inhibitor, and is used to increase the acidification distance. and reduce the risk of corrosion.
It effectively increases the acidification distance of the acidification liquid, reduces corrosion to the reservoir and equipment, enhances the reservoir permeability, and ensures efficient production increase of heat storage.
Smart Images

Figure CN118931522A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of thermal storage development, and in particular to a foam acidizing liquid system, a preparation method and a performance verification test. Background Art
[0002] Geothermal energy stored in heat reservoirs is a clean and sustainable energy source with great potential. Carbonate rock heat reservoirs, such as limestone heat reservoirs and dolomite heat reservoirs, are one of the important target reservoirs for geothermal energy development. Taking the Wumishan Formation dolomite heat reservoir drilling as an example, the heterogeneity of the heat reservoir leads to poor communication between the heat reservoir pores and fractures, resulting in low production capacity of some wells.
[0003] At present, acid fracturing technology is generally used to increase the production of dolomite thermal reservoirs, that is, chemical acidizing fluid is injected into the reservoir section through geothermal wells to chemically dissolve the thermal reservoir rocks, so as to increase the fracture opening and porosity in the reservoir rocks, and the connectivity between the reservoir pores and fractures, so as to improve the reservoir permeability, thereby achieving increased production of thermal reservoirs.
[0004] As an important component of acid fracturing technology, the performance of the acidizing fluid system directly affects the effect of thermal reservoir production increase. The acidizing fluid systems usually used in geothermal wells are mainly conventional strong acid acidizing fluid systems and thickening acidizing fluid systems.
[0005] For conventional strong acid acidizing fluid systems, the acidizing fluid rapidly reacts with dolomite acid-rock, causing the acidizing fluid to dissolve the rock violently near the wellbore, resulting in excessive dissolution of the rock near the wellbore but unable to further acidize and dissolve the rock along the cracks. As a result, the effective acidizing distance is small, which is not conducive to connecting the reservoir pores and cracks and increases the risk of collapse near the wellbore.
[0006] For the thickened acidizing fluid system, although the mass transfer rate of hydrogen ions is reduced by the thickened acidizing fluid, thereby slowing down the acid-rock reaction rate and increasing the effective acidizing distance of the acidizing fluid, the acidizing fluid system has a large viscosity and is easily retained in the reservoir. The residual acidizing fluid retained in the reservoir will block the pores and cracks in the reservoir formation, reduce the formation permeability, cause reservoir damage, and is not conducive to efficient acidizing and production increase. Summary of the invention
[0007] 1. Technical issues to be resolved
[0008] In view of the above-mentioned shortcomings and deficiencies of the prior art, the present invention provides a foam acidizing fluid system, a preparation method and a performance verification test, wherein the acidizing fluid system has good retarding and corrosion inhibition, has the advantages of large acidizing distance and low corrosion, etc., and solves the technical problems in the prior art that the acidizing fluid system has a small acidizing distance and is easy to be retained in the reservoir, resulting in poor thermal energy storage acidizing production increase effect.
[0009] (II) Technical solution
[0010] In order to achieve the above object, the present invention provides a foam acidizing fluid system, a preparation method and a performance verification test. The specific technical scheme is as follows:
[0011] A foam acidizing liquid system, used for increasing the production of dolomite thermal reservoirs, the acidizing liquid system is in a foamy state, and includes a compound acid solution, a foaming agent, a foam stabilizer, a corrosion inhibitor, and an iron ion stabilizer;
[0012] Among them, the compound acid solution includes strong acid and weak acid.
[0013] Preferably, the strong acid is hydrochloric acid, and the weak acid is formic acid, acetic acid or a mixture thereof;
[0014] Calculated by the mass percentage of hydrochloric acid, the compound acid solution is a 20% compound acid solution, which includes 10% hydrochloric acid, 0-5% formic acid and 10%-5% acetic acid.
[0015] Preferably, in terms of mass percentage of hydrochloric acid, the 20% compound acid solution includes 10% hydrochloric acid, 5% formic acid and 5% acetic acid.
[0016] Preferably, based on the mass percentage of hydrochloric acid, the foaming agent includes 1.5% surfactant AGS-12; the foam stabilizer includes 0.6% xanthan gum and 1.5% modified nano-silica.
[0017] Preferably, based on the mass percentage of hydrochloric acid, the mass ratio of the corrosion inhibitor is 1%, and the mass ratio of the iron ion stabilizer is 0.5%.
[0018] A method for preparing a foam acidifying liquid system, which is used to prepare the foam acidifying liquid system, comprises the following steps:
[0019] S10, preparing compound acid solution;
[0020] S20, adding the compound acid solution prepared in step S10 into a stirring cup, and adding a corrosion inhibitor into the stirring cup;
[0021] S30, adding an iron ion stabilizer, a foam stabilizer and a foaming agent to the stirring cup in sequence to complete the preparation of a liquid acidifying liquid system;
[0022] S40, using a stirrer to stir the liquid acidified liquid system obtained in step S30 at a set speed for 5 minutes to foam the liquid acidified liquid system;
[0023] or;
[0024] The liquid acidifying liquid system obtained in step S30 is mixed with high-pressure gas to foam the liquid acidifying liquid system.
[0025] Furthermore, the preparation method of the compound acid solution comprises the following steps:
[0026] S11, using 36% hydrochloric acid solution and water as solvent, prepare 10% hydrochloric acid solution;
[0027] S12, adding 5% formic acid and 5% acetic acid in sequence to the 10% hydrochloric acid solution obtained in step S11 to complete the preparation of a 20% compound acid solution.
[0028] A foam acidizing fluid system performance verification test is used to verify the performance of the foam acidizing fluid system, comprising the following steps:
[0029] Four groups of foam acidizing liquid systems based on different acid solutions were set up, including Example 1, Example 2, Comparative Example 1 and Comparative Example 2, and a non-foam acidizing liquid system of Comparative Example 3 and a foam acidizing liquid system lacking a corrosion inhibitor of Comparative Example 4:
[0030] Based on Example 1, Example 2, Comparative Example 2 and Comparative Example 3, the apparent viscosity and density of the foamed acidizing liquid system and the non-foamed acidizing liquid system of the above examples and comparative examples were tested to determine the basic properties of the acidizing liquid system;
[0031] Based on Example 1, Example 2, Comparative Example 1 and Comparative Example 2, the foaming property and foam stability of the foam acidification system were tested to verify that the foaming time of the foam acid system can meet the requirements of on-site acidification operations;
[0032] Based on Example 1, Example 2, Comparative Example 1, Comparative Example 2 and Comparative Example 3, a static acid-rock reaction test was carried out at normal pressure at the hot storage temperature to verify the effect of foaming property on the retarding property of the acidizing fluid system;
[0033] Based on Example 1, Example 2, Comparative Example 1, Comparative Example 2 and Comparative Example 4, a static test at normal pressure was carried out at the hot storage temperature to verify the influence of the corrosion inhibitor and the acid type on the corrosion inhibition of the acidizing liquid system;
[0034] Based on Example 1, Example 2, Comparative Example 1 and Comparative Example 2, a system compatibility test was conducted to verify that the foam acidifying liquid would not cause performance degradation due to flocculation and precipitation due to system incompatibility under both normal temperature conditions and hot storage conditions.
[0035] Further, based on Example 1, Example 2, Comparative Example 1, Comparative Example 2 and Comparative Example 3, a static acid-rock reaction test at normal pressure was carried out at the hot storage temperature to verify the effect of foaming property on the retarding property of the acidizing fluid system, wherein the static acid-rock test at normal pressure comprises the following steps:
[0036] 1) Select dolomite cuttings with a particle size of 5-10 mm, clean them with deionized water, and then dry them in a drying oven at 60°C for 48 hours;
[0037] 2) Weigh out 5 groups of the dried cuttings, each group of cuttings weighing about 50g, and place them in 5 beakers respectively, preheat the beakers and the cuttings to the heat storage temperature, and after the cuttings are fully preheated, add the acidizing liquid systems of Example 1, Example 2, Comparative Example 1, Comparative Example 2 and Comparative Example 3 into the beakers containing the cuttings, keep the heat storage temperature constant, and react the cuttings with the acidizing liquid system for 4h;
[0038] 3) The rock chips after the reaction were slowly cleaned with deionized water, and then placed in a drying oven at 60°C for 48 hours, and the mass of each group of rock chips after drying was weighed;
[0039] 4) Calculate the cuttings mass loss rate and loss velocity based on the cuttings mass before and after reaction and reaction time.
[0040] Further, based on Example 1, Example 2, Comparative Example 1, Comparative Example 2 and Comparative Example 4, a static corrosion test at normal pressure was carried out at the hot storage temperature to verify the influence of the corrosion inhibitor and the acid type on the corrosion inhibition of the acidizing liquid system, wherein the static corrosion test at normal pressure includes the following steps:
[0041] 1) Select 5 sets of N80 metal sheets, the length of the metal sheets is 40mm, the width is 13mm, and the thickness is 2mm. After the metal sheets are washed and dried, the mass of the metal sheets before corrosion and the surface area of the metal sheets are weighed;
[0042] 2) Select 5 groups of spherical three-necked flasks as containers for placing metal sheets and acidifying liquid systems, and place the 5 groups of metal sheets at the bottom of the 5 groups of flasks respectively;
[0043] 3) Preheat the flask containing the metal sheet to the heat storage temperature, connect the condensed water in the condenser, and then add the acidified liquid systems of Example 1, Example 2, Comparative Example 1, Comparative Example 2 and Comparative Example 4 to the 5 groups of flasks respectively, keep the heat storage temperature constant, and make the metal sheet completely immersed in the foamed acidified liquid system for 4 hours;
[0044] 4) After 4 hours, stop heating and then stop passing condensed water. Take out the corroded metal sheet, wash and dry it, weigh the mass of the corroded metal sheet, calculate the corrosion rate of the metal sheet, and observe the corrosion condition of the metal sheet.
[0045] (III) Beneficial effects
[0046] The acidizing fluid system, preparation method and performance verification test provided by the present invention fill the gap in the existing geothermal acidizing fluid system technology.
[0047] The present invention provides a foam acidizing liquid system, wherein the acidizing liquid is in a foamy state and is foamed by a compound acid liquid, a foaming agent, a foam stabilizer, a corrosion inhibitor and an iron ion stabilizer. The compound acid liquid is a mixture of a strong acid and a weak acid. Compared with a simple strong acid, the corrosiveness of a weak acid is relatively weak. The addition of a weak acid and a corrosion inhibitor greatly improves the corrosion inhibition effect of the acidizing liquid system, and can reduce the corrosion of the acidizing liquid system to underground metal casings and metal acid injection construction equipment. The acidizing liquid is foamed by the addition of a foaming agent and a foam stabilizer, so that the acidizing liquid system after foaming has good retarding properties, which can increase the effective acidizing distance of the acidizing liquid to the thermal reservoir rock, and can effectively chemically dissolve the thermal reservoir rock, thereby improving the reservoir permeability to ensure the effect of increasing thermal reservoir production.
[0048] The present invention also provides a preparation method of the foam acidifying liquid system. The foam acidifying liquid system prepared according to the preparation method has the above-mentioned beneficial effects.
[0049] The present invention also provides a performance verification test of the foam acidizing liquid system, and the advantages and disadvantages of various performances of the foam acidizing liquid system of the present application are verified through comparative tests. BRIEF DESCRIPTION OF THE DRAWINGS
[0050] The drawings described herein are used to provide a further understanding of the present application and constitute a part of the present application. The illustrative embodiments of the present application and their descriptions are used to explain the present application and do not constitute an improper limitation on the present application. In the drawings:
[0051] Figure 1 This is a schematic diagram of the foam morphology in the foam acidifying liquid system just prepared in Example 1 and Example 2 of the present application;
[0052] Figure 2 It is a cuttings mass change rate curve diagram of Example 1, Example 2, Comparative Example 1, Comparative Example 2 and Comparative Example 3 in this application;
[0053] Figure 3 It is a liquid volume curve at 25°C, 70.6°C and 90°C of Example 1, Example 2, Comparative Example 1 and Comparative Example 2 in this application;
[0054] Figure 4 Schematic diagram of the corrosion of metal sheets in Example 1, Example 2, Comparative Example 1, Comparative Example 2 and Comparative Example 4. DETAILED DESCRIPTION
[0055] In order to make the purpose, technical scheme and advantages of the present invention clearer, the technical scheme in the embodiment of the present invention will be described in more detail below in conjunction with the drawings in the preferred embodiments of the present invention. In the drawings, the same or similar reference numerals throughout represent the same or similar elements or elements with the same or similar functions. The described embodiments are part of the embodiments of the present invention, not all of them. The embodiments described below with reference to the drawings are exemplary and are intended to be used to explain the present invention, and should not be construed as limitations on the present invention. Based on the embodiments in the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention. The embodiments of the present invention are described in detail below in conjunction with the drawings.
[0056] Based on the above-mentioned problems existing in the prior art, the present application provides a foam acidizing liquid system, a preparation method and a performance verification test.
[0057] In the disclosed embodiments, the foam acidizing fluid system is used for dolomite thermal storage acidizing and production enhancement, and is in a foamy state, including a compound acid solution, a foaming agent, a foam stabilizer, a corrosion inhibitor and an iron ion stabilizer, wherein the compound acid solution is a mixture of a strong acid and a weak acid.
[0058] During the acidification and production increase of thermal reservoirs, the foam acidizing fluid system is injected into the reservoir section of the geothermal well. The foam acidizing fluid system will dissolve the reservoir rock, increase the fracture opening and porosity of the reservoir rock, and make the reservoir have good permeability, so as to improve the heat exchange efficiency of the fluid injected into the geothermal reservoir in the reservoir, thereby improving the effect of thermal reservoir production increase.
[0059] It should be noted that in the acid fracturing technology, the foam acidizing fluid system mainly relies on the acidizing reaction between the compound acid and the rock to achieve thermal reservoir production increase. The compound acid in this embodiment uses a mixture of strong acid and weak acid. Compared with the pure strong acid, the addition of weak acid makes the compound acid have good retarding and corrosion inhibition. The retarding property relatively slows down the reaction speed of the acidizing fluid and the reservoir rock, effectively increasing the effective acidizing distance of the acidizing fluid; the corrosion inhibition can reduce the corrosion of the acidizing fluid to the underground metal casing and metal acid injection construction equipment.
[0060] Secondly, the foaming agent and foam stabilizer are used for foaming and stabilizing foam. The acidizing fluid system after foaming has good retarding properties, which further increases the effective acidizing distance of the acidizing fluid and avoids the problem of wellbore collapse caused by excessive reaction of the acidizing fluid with the rock near the well.
[0061] Specifically in this embodiment, the compound acid solution is a mixture of a strong acid and a weak acid, the strong acid is hydrochloric acid, and the weak acid is formic acid, acetic acid or a mixture thereof. In terms of the mass percentage of hydrochloric acid, the compound acid solution is a 20% compound acid solution, including a mixture of 10% hydrochloric acid, 0-5% formic acid and 10%-5% acetic acid.
[0062] In the preferred embodiment, the 20% compound acid solution includes 10% hydrochloric acid, 5% formic acid and 5% acetic acid. The components and proportions of this compound acid solution are the preferred embodiment obtained through verification of multiple groups of comparative tests. For details, please refer to the subsequent foam acidizing liquid system performance verification test.
[0063] In this embodiment, based on the mass percentage of hydrochloric acid, the foaming agent includes 1.5% surfactant, 0.6% tackifier and 1.5% inorganic nano-enhancer.
[0064] In the preferred embodiment, the surfactant is preferably an alkyl glycine surfactant AGS-12. AGS is the abbreviation of Alkyl Glycine Surfactant in English, and 12 represents that there are 12 carbon atoms in the carbon chain of dodecylamine in the synthetic substance. As an organic surfactant, AGS-12 has the advantages of being non-flammable, non-toxic and non-corrosive. It can be used for efficient foaming in a certain temperature range, high salt and high calcium environment, and can meet the application conditions of geothermal reservoirs. It is non-toxic, environmentally friendly, biodegradable (bacterial), does not pollute the environment, and does not leave residues, making the acidizing fluid easy to clean and not easy to be retained in the reservoir formation, thereby realizing thermal storage protection.
[0065] The tackifier is preferably xanthan gum, which is a biological glue that integrates thickening, suspension, emulsification, and stability. In this embodiment, the thickening property of xanthan gum is mainly used. The thickening property makes the foamy acidizing liquid have good viscosity, which can stabilize the foam in the system and slow down the mass transfer rate of hydrogen ions, thereby improving the foam stability of the acidizing liquid system, slowing down the reaction rate of the acidizing liquid system and dolomite, and further improving the effective acidizing distance of the acidizing liquid system.
[0066] The inorganic nano-enhancer is preferably modified nano-silica, because it can be adsorbed at the air-liquid interface and form hydrogen bonds with xanthan gum and surfactant AGS-12, thereby enhancing the foam stability by reducing the foam surface tension, enhancing the foam liquid film strength and preventing the foam from agglomerating.
[0067] The above is a preferred embodiment of the foaming agent and the foam stabilizer of this embodiment. By jointly foaming the surfactant AGS-12, xanthan gum and modified nano-silica, the acidified liquid after foaming has good retarding properties and is easy to clean, so that the residual liquid of the acidified liquid system is not easily retained in the reservoir formation, thereby achieving thermal storage protection.
[0068] In the embodiment of the present disclosure, the amount of corrosion inhibitor and iron ion stabilizer added is also calculated as a percentage of the mass of hydrochloric acid. The amount of corrosion inhibitor added is 1%, the amount of iron ion stabilizer added is 0.5%, and the ratio of the amount of corrosion inhibitor to the amount of iron ion stabilizer added is 2:1.
[0069] Among them, the corrosion inhibitor is preferably HC-Y-02, which is the commercial product code of the corrosion inhibitor. The corrosion inhibitor can significantly reduce the corrosion effect of the foam acidizing fluid on metals such as iron, and protect the acidizing equipment and downhole pipelines.
[0070] The combination of iron ion stabilizer and corrosion inhibitor can prevent the precipitation of iron ions in the acid solution at a lower pH value, thereby blocking the reservoir pores and cracks.
[0071] It should be noted that the addition amount of each component in the foam acidifying liquid system of this embodiment is calculated based on the mass percentage of hydrochloric acid in the compound acid solution, in order to facilitate the calculation of the addition amount of other components.
[0072] The above is a preferred solution for the composition and ratio of each component of the foam acidizing liquid system of this embodiment. Based on this, this embodiment also provides a method for preparing the foam acidizing liquid system, which specifically includes the following steps:
[0073] S10, preparing 20% compound acid solution, comprising the following steps:
[0074] S11, based on 36% hydrochloric acid, using water as solvent, dilute it to 10% hydrochloric acid solution;
[0075] S12. Add 5% formic acid and 5% acetic acid to the 10% hydrochloric acid solution in step S12 in sequence to complete the preparation of a 20% compound acid solution.
[0076] S20, adding the 20% compound acid solution prepared in step S10 into the stirring cup, and adding 1% corrosion inhibitor into the stirring cup;
[0077] S30, adding 0.5% iron ion stabilizer, 1.5% surfactant AGS-12, 0.6% xanthan gum and 1.5% modified nano-silica into the mixing cup of step S20 in sequence;
[0078] S40, using a stirrer to stir the mixed solution obtained in step S30 at a set speed for 5 minutes to fully foam it, so as to complete the preparation of the foam acid solution system;
[0079] Alternatively, the mixed liquid obtained in step S30 is mixed with high-pressure gas to fully foam it, thereby completing the preparation of the foamed acidifying liquid system of this embodiment.
[0080] The preparation method of 1.5% surfactant AGS-12 in step S30 comprises the following steps:
[0081] 1) Dissolve 54.9g dodecylamine in anhydrous ethanol, dissolve 24g sodium hydroxide in 75ml water, and then mix the two at 80°C;
[0082] 2) Take 72g of sodium chloroacetate and add it into 150ml of water and stir to prepare a sodium chloroacetate solution, and then add the sodium chloroacetate solution dropwise into the mixed solution prepared in step 1);
[0083] 3) heating the mixed solution obtained in step 2) to 85° C. and stirring for 2 hours;
[0084] 4) Dry and crush the product obtained in step 3) to obtain a powdered surfactant AGS-12, and then store the powdered surfactant at room temperature.
[0085] It should be noted that the mass of each raw material required for the above-mentioned surfactant AGS-12 is only an example. When the demand is large, it can be proportionally enlarged according to the ratio of each raw material.
[0086] The above is the preparation method of the foam acidizing liquid system of this embodiment. The foam acidizing liquid system prepared by the above method has the advantages of slow speed, corrosion inhibition, compatibility and easy cleaning.
[0087] Based on the foam acidizing liquid system prepared by the above method, this embodiment also provides a performance verification test of the foam acidizing liquid system of this embodiment to verify the various performance advantages of the foam acidizing liquid system.
[0088] The verification test of the foam acidizing liquid system in this embodiment is carried out according to the standard of "SY / T 5886-2018 Acidizing Liquid Working Performance Evaluation Method". By setting up 6 groups of acidizing liquid systems with different formulations (see Table 1 for details), including Example 1, Example 2, Comparative Example 1, Comparative Example 2, Comparative Example 3 and Comparative Example 4, the various properties of the acidizing liquid system are verified by comparative tests to determine the optimal ratio of each component of the foam acidizing liquid system.
[0089] Table 1: Acidizing fluid system formula
[0090]
[0091] As can be seen from Table 1, the components and ratios of the composite acid solution in the acidizing solution systems of Example 1, Example 2, Comparative Example 1 and Comparative Example 2 are different, the purpose of which is to verify the influence of different acid solution types on the performance indicators of the acidizing solution system; Comparative Example 3 is compared with Comparative Example 2, in which the acidizing solution system is not foamed, the purpose of which is to study the influence of foaming on the performance of the acidizing solution system; Comparative Example 4 is compared with Comparative Example 2, in which no corrosion inhibitor is added to the acidizing solution system of Comparative Example 4, the purpose of which is to verify the influence of the corrosion inhibitor on the performance of the acidizing solution system.
[0092] To illustrate the advantages of the foam acidizing liquid system of this embodiment, i.e., the foam acidizing liquid system of embodiment 1, the following comparative analysis will be conducted on the experimental data of the apparent viscosity and density, foaming property and foam stability, solubility, retarding property, corrosion inhibition and system compatibility of the acidizing liquid system with respect to the above embodiments and comparative examples, as follows:
[0093] 1. Apparent viscosity and density:
[0094] 1.1. The apparent viscosity of the acidizing liquid system is measured by a coaxial cylinder viscometer, which specifically includes the following steps:
[0095] 1) Add the acidified liquid system into the outer cylinder of the cylinder viscometer, lift the outer cylinder, and insert the inner cylinder into the acidified liquid system;
[0096] 2) Start the cylinder viscometer and rotate it at a set speed of 100r / min. Record the reading of the cylinder viscometer after it stabilizes.
[0097] 3) Calculate the apparent viscosity of the acidizing liquid system based on the cylinder viscometer reading.
[0098] 1.2. The density of the acidizing liquid system is measured by a density meter. The measurement process is as follows:
[0099] 1) Place the density meter sample cup on the weighing table, and then set the density meter reading to zero to remove the weight of the sample cup;
[0100] 2) Slowly add the acidified liquid system into the sample cup to the mouth of the cup, cover the cup lid and press down, then wipe off the overflowed acidified liquid system;
[0101] 4) Place the sample cup filled with the acidifying liquid system on the weighing table. The value displayed on the density meter is the density of the acidifying liquid system being tested.
[0102] The above is a method for measuring the apparent viscosity and density of the acidizing liquid system. According to the above method, the apparent viscosity coefficient and density of the above embodiments and comparative examples are measured and recorded, and the specific values are shown in Table 2.
[0103] Table 2 Apparent viscosity and density of acidizing fluid system
[0104]
[0105]
[0106] Combining the data in Table 1 and Table 2, firstly, it can be seen from the data of Comparative Examples 2 and 3 that, when the components of the compounded acid solution are the same, the apparent viscosity of the acidifying liquid system after foaming is significantly increased, and the density is smaller. The smaller density indicates that the gas content in the foaming acid system is increased, and the larger viscosity is conducive to the stability of the foam. Therefore, it can be indirectly proved that the foaming performance of the foaming acidifying liquid system is better.
[0107] Secondly, from the data of Example 1, Example 2, Comparative Example 1 and Comparative Example 2, it can be seen that the compounding method of strong acid and weak acid significantly increases the apparent viscosity of the acidizing liquid system, and the density is relatively small. The larger viscosity can slow down the migration rate of hydrogen ions, and the foam can hinder the migration of hydrogen ions. This can indirectly prove that the compounded acid solution of the combination of strong acid and weak acid makes the acidizing liquid system have good retarding properties.
[0108] 2. About foamability and foam stability
[0109] The foamability and foam stability of four groups of foam acidifying liquid systems based on different acid solutions, Example 1, Example 2, Comparative Example 1, and Comparative Example 2, were evaluated by foaming volume, foam characteristic value, and foam half-life of each group at the thermal storage temperature. The results are shown in Tables 3, 4, Figure 1 and Figure 3 shown.
[0110] Table 3: Foamability and stability of foam acidifying liquid system
[0111]
[0112] Table 4: Foam stability of foam acidizing liquid system
[0113]
[0114] It can be seen from Table 3 that the foaming volume and foam characteristic value of Example 1 and Example 2 are greater than those of Comparative Example 1 and Comparative Example 2, which can directly prove that Example 1 and Example 2 have better foaming properties.
[0115] As can be seen from Table 4, the foam stability of the foam acidifying liquid decreases with increasing temperature, Example 1>Comparative Example 1>Example 2>Comparative Example 2, which can directly prove that the compounding method of strong acid and weak acid significantly increases the foam stability of the foam acidifying liquid, and the foam stability of the foam acidifying liquid system based on the compounding acid solution of hydrochloric acid and two organic weak acids, formic acid and acetic acid, is the best.
[0116] 3. Rock chip dissolution and acidizing fluid system slowness
[0117] For the four groups of foamed acidizing liquid systems based on different acid solutions in Example 1, Example 2, Comparative Example 1 and Comparative Example 2, and the non-foamed acidizing liquid system based on 20% hydrochloric acid in Comparative Example 3, a static acid-rock reaction experiment at normal pressure was carried out at the thermal storage temperature, and the specific steps are as follows:
[0118] 1) Select dolomite cuttings with a particle size of 5-10 mm, clean them with deionized water, and then dry them in a drying oven at 60°C for 48 hours;
[0119] 2) Weigh out 5 groups of the dried cuttings, each group of cuttings weighing about 50g, and place them in 5 beakers respectively, preheat the beakers and the cuttings to the heat storage temperature, and after the cuttings are fully preheated, add the acidizing liquid systems of Example 1, Example 2, Comparative Example 1, Comparative Example 2 and Comparative Example 3 into the beakers containing the cuttings, keep the heat storage temperature constant, and react the cuttings with the acidizing liquid system for 4h;
[0120] 3) The rock chips after the reaction were slowly cleaned with deionized water, and then placed in a drying oven at 60°C for 48 hours, and the mass of each group of rock chips after drying was weighed;
[0121] 4) Calculate the cuttings mass loss rate and loss velocity based on the cuttings mass before and after reaction and reaction time.
[0122] It can be understood that the cuttings mass loss rate can characterize the dissolution of cuttings in the acidizing fluid system, and the mass loss rate can characterize the slowness of the acidizing fluid system. The test results are shown in Table 5 and Figure 2 shown.
[0123] Table 5: Rock chip dissolution
[0124]
[0125] From Table 5 and Figure 3 It can be seen that the cuttings mass change rate and mass change rate in Comparative Example 3 are significantly greater than those in Comparative Example 1, Comparative Example 2, Example 1 and Example 2, and compared with Comparative Example 3, the mass change rate decrease rates of the other four groups are about 50%, indicating that foamed acid has a significant retarding effect compared to non-foamed acid.
[0126] The rock cuttings mass change rate and mass change rate of Example 1 and Example 2 are slightly smaller than those of Comparative Example 1 and Comparative Example 2, indicating that the use of weak acid instead of strong acid in the acid solution has a certain retarding effect, but the retarding effect achieved by bubbling to form foam acid is significantly greater than that of weak acid instead of strong acid.
[0127] 4. Corrosion inhibition
[0128] Four groups of foamed acidizing liquid systems based on different acid solutions, namely, Example 1, Example 2, Comparative Example 1, and Comparative Example 2, and a non-foamed acidizing liquid system based on 20% hydrochloric acid without adding the corrosion inhibitor HC-Y-02 in Comparative Example 4, were subjected to a static corrosion test at normal pressure at the hot storage temperature. The specific steps are as follows:
[0129] 1) Select 5 sets of N80 metal sheets, the length of the metal sheets is 40mm, the width is 13mm, and the thickness is 2mm. After the metal sheets are washed and dried, the mass of the metal sheets before corrosion and the surface area of the metal sheets are weighed;
[0130] It should be noted that N80 is a steel-grade metal material for oil well pipes, which is selected according to the standard "SY / T 5886-2018 Acidizing Fluid Working Performance Evaluation Method".
[0131] 2) Select 5 groups of spherical three-necked flasks as containers for placing metal sheets and acidifying liquid systems, and place 5 metal sheets at the bottom of the 5 groups of flasks respectively;
[0132] It should be noted that the "SY / T 5886-2018 Acidizing Liquid Performance Evaluation Method" stipulates that the metal sheet should be placed in the flask in a suspended manner, but the metal sheet is placed at the bottom of the flask in this embodiment, the purpose is to make the metal sheet completely immersed in the acidizing liquid system. Since the embodiment and the comparative example in this comparative test are both foam acidizing liquid systems, the foam acidizing liquid system will defoam over time and cause the volume to decrease. If the metal sheet is placed in the flask in a suspended manner, the foam acidizing liquid system will defoam, resulting in partial exposure of the metal sheet, which will affect the accuracy of the test results.
[0133] At the same time, it can be understood that the "SY / T 5886-2018 Acidizing Fluid Performance Evaluation Method" stipulates that the metal sheet should be placed in the flask in a suspended manner, with the purpose of making all sides of the metal sheet corroded. However, the flask in this embodiment is spherical, and only the tip of the metal sheet is in contact with the flask, and it is assumed that all sides are corroded, which also achieves the effect of the suspension method.
[0134] 3) Preheat the flask containing the metal sheet to the heat storage temperature, connect the condensed water in the condenser, and then add the foam acidified liquid system of Example 1, Example 2, Comparative Example 1, Comparative Example 2 and Comparative Example 4 to the 5 groups of flasks respectively, keep the heat storage temperature constant, and allow the foam acidified liquid system to corrode the metal sheet for 4 hours;
[0135] 4) After reaching the set time of 4h, stop heating, then stop passing condensed water, take out the corroded metal sheet, wash and dry it, weigh the mass of the corroded metal sheet, calculate the corrosion rate of the metal sheet, and observe the corrosion of the metal sheet. The results are shown in Table 6 and Figure 4 shown.
[0136] Table 6: Corrosion inhibition of foam acidizing fluid
[0137]
[0138]
[0139] From Table 6 and Figure 4 It can be seen that the corrosion rate of the metal sheet in Comparative Example 4 is significantly greater than that in Comparative Example 2, indicating that the corrosion inhibitor HC-Y-02 has a significant corrosion inhibition effect in the foam acidification liquid system. The corrosion rate of the metal sheet in Comparative Example 3 is significantly greater than that in Example 1, Example 2 and Comparative Example 1, indicating that the use of weak acid instead of strong acid can have a significant corrosion inhibition effect. In addition, the corrosion rate of the metal sheet in Examples 1 and 2 is less than that in Comparative Example 1, indicating that increasing the amount of acetic acid in the compound acid solution can improve the corrosion inhibition effect to a certain extent.
[0140] 5. System compatibility
[0141] The compatibility of the four groups of foam acidizing fluid systems based on different acid solutions, namely Example 1, Example 2, Comparative Example 1 and Comparative Example 2, at heat storage temperature without adding formation water and with adding formation water, as well as at room temperature without adding formation water, was evaluated. The formation water was taken from the heat storage formation. The system compatibility results are shown in Table 7.
[0142] Table 7: Compatibility of foam acidizing liquid system
[0143]
[0144] As shown in Table 4, except for Comparative Example 2, the foam acidizing liquid system without formation water added in Example 1, Example 2 and Comparative Example 1 had no flocculation, precipitation or stratification after standing for 4 hours at the hot storage temperature and room temperature. At the hot storage temperature, flocculation, precipitation and stratification occurred in Comparative Examples 1 and 2 with formation water added after standing for 4 hours, while there was no flocculation, precipitation or stratification in Example 1 and Example 2.
[0145] This indicates that the bath acidifying liquid systems of Examples 1 and 2 have system compatibility that meets the requirements, and their performance will not decrease due to flocculation and precipitation due to system incompatibility at room temperature and under hot storage conditions.
[0146] The above is the entire process of the verification test of the foam acidifying liquid system of this embodiment. The above test proves that the acid solution in the foam acidifying liquid system of Example 1 and Example 2 uses 0-5% formic acid and 5-10% weak acid instead of 10% hydrochloric acid, which significantly improves the retarding and corrosion inhibition of the foam acidifying liquid; the foaming property and foam stability of the foam acidifying liquid system are significantly enhanced by foaming with surfactant AGS-12 and synergistic foam stabilization with xanthan gum and modified nano-silica; the addition of corrosion inhibitor HC-Y-02 makes the foam acidifying liquid system have excellent corrosion inhibition performance; in terms of foam stability, Example 1 is significantly better than Example 2, and then Example 1 can be selected as the preferred scheme of the foam acidifying liquid system of this embodiment.
[0147] In summary, the above test results fully verify that the foam acidizing fluid system of this embodiment has the advantages of slow speed, corrosion inhibition, compatibility and easy cleaning, and can be widely used in dolomite thermal reservoir production increase, and can effectively ensure the effect of acidizing production increase.
[0148] The above are only preferred specific embodiments of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical solutions and inventive concepts of the present invention within the technical scope disclosed by the present invention, which are all covered by the protection scope of the present invention.
Claims
1. A foam acidizing fluid system for increasing the production of dolomite thermal reservoirs, characterized in that: The acidizing liquid system is in a foamy state and includes a compound acid solution, a foaming agent, a foam stabilizer, a corrosion inhibitor and an iron ion stabilizer; Wherein, the compound acid solution includes a strong acid and a weak acid.
2. The foam acidizing liquid system according to claim 1, characterized in that The strong acid is hydrochloric acid, and the weak acid is formic acid, acetic acid or a mixture thereof; Calculated by the mass percentage of the hydrochloric acid, the compound acid solution is a 20% compound acid solution, including 10% hydrochloric acid, 0-5% formic acid and 10%-5% acetic acid.
3. The foam acidifying liquid system according to claim 2, characterized in that Calculated by mass percentage of the hydrochloric acid, the 20% compound acid solution includes 10% hydrochloric acid, 5% formic acid and 5% acetic acid.
4. The foam acidifying liquid system according to claim 2, characterized in that: The foam stabilizer includes 1.5% surfactant AGS-12 based on the mass percentage of the hydrochloric acid; The foam stabilizer comprises 0.6% xanthan gum and 1.5% modified nano silicon dioxide.
5. The foam acidizing liquid system according to claim 2, characterized in that: Calculated by mass percentage of the hydrochloric acid, the mass ratio of the corrosion inhibitor is 1%, and the mass ratio of the iron ion stabilizer is 0.5%.
6. A method for preparing a foam acidifying liquid system, characterized in that: The method for preparing the foam acidifying liquid system according to any one of claims 1 to 5 comprises the following steps: S10, preparing compound acid solution; S20, adding the compound acid solution prepared in step S10 into a stirring cup, and adding a corrosion inhibitor into the stirring cup; S30, adding an iron ion stabilizer, a foam stabilizer and a foaming agent to the stirring cup in sequence to complete the preparation of a liquid acidifying liquid system; S40, using a stirrer to stir the liquid acidified liquid system obtained in step S30 at a set speed for 5 minutes to foam the liquid acidified liquid system; or; The liquid acidifying liquid system obtained in step S30 is mixed with high-pressure gas to foam the liquid acidifying liquid system.
7. The method for preparing the foam acidifying liquid system according to claim 6, characterized in that: The preparation method of the composite acid solution comprises the following steps: S11, using 36% hydrochloric acid solution and water as solvent, prepare 10% hydrochloric acid solution; S12, adding 5% formic acid and 5% acetic acid in sequence to the 10% hydrochloric acid solution obtained in step S11 to complete the preparation of a 20% compound acid solution.
8. A foam acidizing fluid system performance verification test, characterized in that: The method is used to verify the performance of the foam acidizing liquid system according to any one of claims 1 to 5, comprising the following steps: Four groups of foam acidizing liquid systems based on different acid solutions were set up, including Example 1, Example 2, Comparative Example 1 and Comparative Example 2, and a non-foam acidizing liquid system of Comparative Example 3 and a foam acidizing liquid system lacking a corrosion inhibitor of Comparative Example 4: Based on the embodiment 1, the embodiment 2, the comparative example 2 and the comparative example 3, the apparent viscosity and density of the foamed acidizing liquid system and the non-foamed acidizing liquid system of the above embodiments and comparative examples are tested to determine the basic properties of the acidizing liquid system; Based on the embodiment 1, the embodiment 2, the comparative example 1 and the comparative example 2, the foaming property and the foam stability of the foam acidification system are tested to verify that the foaming time of the foam acidification system can meet the requirements of the on-site acidification operation; Based on the embodiment 1, embodiment 2, comparative example 1, comparative example 2 and comparative example 3, a static acid-rock reaction test at normal pressure was carried out at the hot storage temperature to verify the effect of foaming property on the retarding property of the acidizing fluid system; Based on the embodiment 1, embodiment 2, comparative example 1, comparative example 2 and comparative example 4, a static test at normal pressure was carried out at the hot storage temperature to verify the influence of the corrosion inhibitor and the acid type on the corrosion inhibition of the acidizing liquid system; Based on the Example 1, the Example 2, the Comparative Example 1 and the Comparative Example 2, a system compatibility test was conducted to verify that the foam acidifying liquid would not cause performance degradation due to flocculation and precipitation due to system incompatibility under both normal temperature conditions and hot storage conditions.
9. The foam acidizing fluid system performance verification test according to claim 8, characterized in that: Based on the embodiment 1, embodiment 2, comparative example 1, comparative example 2 and comparative example 3, a static acid-rock reaction test at normal pressure is carried out at the hot storage temperature to verify the influence of foaming property on the retarding property of the acidizing fluid system, wherein the static acid-rock test at normal pressure comprises the following steps: 1) Select dolomite cuttings with a particle size of 5-10 mm, wash the cuttings with deionized water, and then place them in a drying oven at 60° C. for 48 hours; 2) Weigh out 5 groups of the dried rock chips, each group of which has a mass of about 50 g, and place them in 5 beakers respectively. Preheat the beakers and the rock chips to the heat storage temperature. After the rock chips are fully preheated, add the acidizing liquid systems of Example 1, Example 2, Comparative Example 1, Comparative Example 2 and Comparative Example 3 into the beakers containing the rock chips respectively, keep the heat storage temperature constant, and react the rock chips with the acidizing liquid system for 4 hours; 3) The rock cuttings after the reaction were slowly cleaned with the deionized water, and then placed in the drying box to dry at 60° C. for 48 hours, and the mass of the rock cuttings in each group after drying was weighed; 4) Calculate the cuttings mass loss rate and loss velocity based on the cuttings mass before and after reaction and reaction time.
10. The foam acidizing fluid system performance verification test according to claim 8, characterized in that: Based on the embodiment 1, embodiment 2, comparative example 1, comparative example 2 and comparative example 4, a static corrosion test at normal pressure is carried out at the hot storage temperature to verify the influence of the corrosion inhibitor and the acid type on the corrosion inhibition of the acidizing liquid system, wherein the static corrosion test at normal pressure comprises the following steps: 1) Select 5 sets of N80 metal sheets, the length of the metal sheets is 40 mm, the width is 13 mm, and the thickness is 2 mm. After the metal sheets are washed and dried, the mass of the metal sheets before corrosion and the surface area of the metal sheets are weighed; 2) Select 5 groups of spherical three-necked flasks as containers for placing the metal sheets and the acidifying liquid system, and place the 5 groups of metal sheets at the bottom of the 5 groups of flasks respectively; 3) preheating the flask containing the metal sheet to the heat storage temperature, connecting the condensed water in the condenser, and then adding the acidified liquid systems of Example 1, Example 2, Comparative Example 1, Comparative Example 2 and Comparative Example 4 to the 5 groups of flasks respectively, keeping the heat storage temperature constant, so that the metal sheet is completely immersed in the foamed acidified liquid system for 4 hours; 4) After 4 hours, stop heating and then stop passing condensed water, take out the corroded metal sheet, wash and dry it, weigh the mass of the corroded metal sheet, calculate the corrosion rate of the metal sheet, and observe the corrosion condition of the metal sheet.
Citation Information
Patent Citations
High performance acidizing fracturing fluid and preparation method thereof
CN103756663A
Composite osmotic acid liquor and preparation method thereof
CN114437693A