Composite inert electrode, electrolytic cell comprising composite inert electrode and method for forming composite inert electrode

By using composite inert electrodes made of ceramic materials, the carbonaceous outer layer is composed of carbon-containing materials and corrosion-resistant metals, the loss problem of electrodes in corrosive electrolyte is solved, cost reduction and service life extension are achieved, and the Electrolytic reaction.

CN118932382APending Publication Date: 2024-11-12FULL CHAIN MATERIALS INTL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310534037.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-12
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

In electrolyte cells containing corrosive electrolytes, the electrode material continues to lose, resulting in increased manufacturing costs, and corrosion-resistant electrode materials are expensive and difficult to use on a large scale.

Method used

A composite inert electrode consisting of an electrode core made of ceramic material and a carbonaceous outer layer. The carbonaceous outer layer is composed of carbonaceous material and corrosion-resistant metal. The non-interpolated electrode material is formed through electroplating and deposition reaction, which reduces material costs and extends Service life.

Benefits of technology

It significantly reduces the material cost of composite inert electrodes, extends the service life of the electrode, simplifies the chemical reaction in electrolytic reactions, avoids electrode losses, and is simple in production, reducing manufacturing costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118932382A_ABST
    Figure CN118932382A_ABST
Patent Text Reader

Abstract

A composite inert electrode is substantially composed of an electrode core and a carbonaceous outer layer coating the electrode core. The electrode core is substantially composed of a ceramic material. The carbonaceous outer layer is substantially composed of a carbonaceous material and a corrosion resistant metal. The carbonaceous outer layer is made of a non-insertion type electrode material, and the corrosion-resistant metal is dispersed in the carbonaceous material.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a composite inert electrode, an electrolytic cell containing the composite inert electrode, and a method for forming the composite inert electrode. In particular, the present invention is directed to a corrosion-resistant composite inert electrode for an electrolytic cell containing a corrosive electrolyte, and a method for forming the corrosion-resistant composite inert electrode. Background Art

[0002] In the field of chemical engineering, electrolysis is often used to carry out non-spontaneous chemical reactions for manufacturing or refining purposes. Electrolysis is usually carried out in an electrolytic cell, especially an electrolytic cell containing a corrosive electrolyte.

[0003] However, corrosive electrolytes have potential damage to the electrodes in the electrolytic cell. For example, during the electrolysis process, the electrode material will continue to be consumed. Although the use of corrosion-resistant electrode materials can reduce the loss rate of electrode materials, due to their high price, if expensive corrosion-resistant electrode materials are used in large quantities, the corresponding increase in manufacturing costs remains a technical problem to be solved.

[0004] In the search for other effective solutions, the industry needs a corrosion-resistant electrolytic electrode and a manufacturing method thereof that is simple to manufacture, inexpensive, high-quality, stable and reliable. Summary of the invention

[0005] To achieve the above objectives, the inventors of this case, after exhausting their efforts in research and development, have proposed a breakthrough composite inert electrode, an electrolytic cell including the composite inert electrode, and a method for forming the composite inert electrode. This breakthrough composite inert electrode is conducive to solving the above technical problems currently faced by the industry.

[0006] The present invention first proposes a composite inert electrode. The composite inert electrode is substantially composed of an electrode core and a carbonaceous outer layer covering the electrode core. The electrode core is substantially composed of a ceramic material. The carbonaceous outer layer is a composite material, substantially composed of a carbonaceous material and a corrosion-resistant metal. The carbonaceous outer layer is a non-intercalation electrode material, and the corrosion-resistant metals are dispersed in the carbonaceous material separately from each other. The carbonaceous outer layer is conductive, and its resistivity is, for example, less than 1×10 -3 Ω·m.

[0007] The present invention further provides an electrolytic cell. The electrolytic cell comprises an electrolyte and the composite inert electrode. The electrolyte comprises at least one of a strong acid, a strong base and a fluoride. The carbonaceous outer layer in the composite inert electrode directly contacts the electrolyte to isolate the electrolyte from contacting the electrode core.

[0008] The present invention can also provide a method for forming a composite inert electrode. First, an electrode core is provided. The electrode core is substantially composed of a ceramic material. Next, an electroplating deposition reaction is performed in the presence of a carbon source precursor to form a carbonaceous outer layer covering the electrode core. The carbonaceous outer layer is substantially composed of a carbonaceous material and a corrosion-resistant metal. The carbonaceous outer layer is a non-insertion type electrode material, and the corrosion-resistant metal is dispersed in the carbonaceous material.

[0009] The composite inert electrode proposed by the present invention does not require a large amount of expensive corrosion-resistant electrode materials, so the material cost of the composite inert electrode of the present invention can be significantly reduced. The method for forming a composite inert electrode proposed by the present invention can further reduce the manufacturing cost of the composite inert electrode because of its simple manufacturing method. In addition, the carbonaceous outer layer produced by the method for forming a composite inert electrode of the present invention is a non-insertion type electrode material. This non-insertion type electrode material will not undergo an insertion reaction with metals or ions to produce an intercalation compound or an intercalation composite. Therefore, it can also simplify the chemical reaction between the electrode and the electrolyte in the electrolysis reaction. In addition, the carbonaceous outer layer is a composite material, comprising a carbonaceous material and a corrosion-resistant metal dispersed therein, and this corrosion-resistant metal can also increase the service life of the carbonaceous outer layer. In addition, the electrode core is a ceramic material, which has good support, is not easy to wear and has low cost. Therefore, the composite inert electrode, electrolytic cell and method for forming a composite inert electrode of this case are nothing less than a comprehensive technical solution that can demonstrate the advantages of multiple inventions. BRIEF DESCRIPTION OF THE DRAWINGS

[0010] Figure 1 FIG. 4 is a schematic flow chart of a method for forming a composite inert electrode according to an embodiment of the present invention.

[0011] Figures 2 to 4 FIG. 4 is a schematic diagram of a method for forming a composite inert electrode using electrodes according to an embodiment of the present invention.

[0012] Figure 5 to Figure 6 FIG. 4 is a schematic diagram of a method for regenerating a composite inert electrode according to an embodiment of the present invention.

[0013] Figures 7 to 9 FIG. 4 is a schematic diagram of the cross-sectional structure of a composite inert electrode according to an embodiment of the present invention.

[0014] Fig.10 The cross-sectional structure diagram of a composite inert electrode according to an embodiment of the present invention applied to an electrolytic cell is shown in FIG. DETAILED DESCRIPTION

[0015] In order to enable those skilled in the art to further understand the present invention, several preferred embodiments of the present invention are listed below, and the components and intended effects of the present invention are described in detail in conjunction with the accompanying drawings. Moreover, those skilled in the art can also refer to the following embodiments and replace, reorganize, and mix the features of several different embodiments to complete other embodiments without departing from the spirit of the present invention.

[0016] In the following description and claims, words such as "containing" and "including" are open-ended words, and therefore should be interpreted as "containing but not limited to..." In the following description and claims, "substantially consisting of certain components" or similar words are semi-closed words, which means that in the combination of components, ingredients or steps, components, ingredients or steps recorded in the description that do not substantially affect the components, ingredients or steps recorded in the claim are not excluded. For example, but not limited to, impurities, adulterants, contaminants or possible additives and precursors that are difficult to completely exclude in practice do not exclude components, ingredients or steps that are not recorded in the description and do not substantially affect the main technical features of the invention in the claim.

[0017] The terms "approximately", "equal to", "equal" or "same", "substantially" or "approximately" are generally interpreted as being within a range of plus or minus 20% of a given value, or within a range of plus or minus 10%, plus or minus 5%, plus or minus 3%, plus or minus 2%, plus or minus 1% or plus or minus 0.5% of a given value. In addition, the phrases "a given range is a first value to a second value", "a given range falls within the range of a first value to a second value" indicate that the given range includes the first value, the second value, and other values ​​therebetween.

[0018] Unless otherwise defined, all terms (including technical and scientific terms) used herein have the same meaning as commonly understood by those skilled in the art to which the present invention belongs. It is understood that these terms, such as those defined in commonly used dictionaries, should be interpreted as having a meaning consistent with the background or context of the relevant technology and the present invention, and should not be interpreted in an idealized or overly formal manner unless specifically defined in the embodiments of the present invention.

[0019] Figure 1 FIG. 4 is a schematic flow chart of a method for forming a composite inert electrode according to an embodiment of the present invention. Figure 2 FIG. 4 is a schematic diagram of a method for forming a composite inert electrode by electroplating according to an embodiment of the present invention. Figure 2In the method for forming a composite inert electrode shown in FIG. 1 , first, an electroplating chamber 10 is provided. The electroplating chamber 10 contains an electroplating solution 11, which can be used to form a passivation protective layer on the surface of the substrate to protect the substrate inside. Next, a substrate is provided and placed in the electroplating chamber 10. In one embodiment, as shown in FIG. Figure 3 As shown, the substrate can be an electrode core 110 of the composite inert electrode of the present invention. The electrode core 110 is substantially composed of a ceramic material. For example, an electrode core 110 substantially composed of a ceramic material is provided and placed in the electroplating tank 10.

[0020] In one embodiment, the ceramic material refers to a material other than an organic material and a metal material, such as an inorganic non-metallic material. The ceramic material may be a mixture formed by sintering silicon oxide and / or metal oxide, with inorganic nitride, inorganic boride and inorganic carbide added as needed. According to one embodiment, the Mohs hardness of the ceramic material is higher than 6.5.

[0021] like Figure 3 As shown, the electroplating solution 11 contains stable ions of corrosion-resistant metals, such as aluminum ions (composite ions) of corrosion-resistant metals, so that the corrosion-resistant metals are dissolved in and stably exist in the electroplating solution 11 through the aluminum ions. The ligands and aluminum ions of various corrosion-resistant metals suitable for electroplating are common knowledge in the art, so they are not described in detail. As needed, a sacrificial electrode 12 containing corrosion-resistant metals can be provided in the electroplating solution 11. By providing a sacrificial electrode 12 of corrosion-resistant metal and replacing a new sacrificial electrode 12, the sacrificial electrode 12 can continuously provide the ions and aluminum ions of the corrosion-resistant metal in the electroplating solution 11, so that the concentration of the ions and aluminum ions of the corrosion-resistant metal in the electroplating tank 10 can be maintained at a constant concentration. In addition, the carbon source precursor 13 is introduced into the electroplating tank 10 and dispersed in the electroplating solution 11. By continuously adding the carbon source precursor 13, the concentration of the carbon source precursor 13 in the electroplating tank 10 can be maintained at a constant concentration.

[0022] Please refer to Figure 4 As shown, in the presence of the carbon source precursor 13, the surface 110A of the electrode core 110 is subjected to a predetermined electroplating deposition reaction. Figure 4As shown, in the presence of the carbon source precursor 13, an appropriate voltage is provided to the electrode core 110 and the sacrificial electrode 12 connected in series, and a predetermined electroplating deposition reaction is performed on the surface 110A of the electrode core 110. The predetermined electroplating deposition reaction can be in the presence of the corrosion-resistant metal ions in the electroplating solution 11, so that the reduced carbon source precursor 130 and the first corrosion-resistant metal 111 obtained from the corrosion-resistant metal ions directly form a carbon outer layer 120 that completely covers the electrode core 110 on the surface 110A of the electrode core 110, thereby obtaining the composite inert electrode 100 of the present invention, and forming a protective effect on the electrode core 110, and there is no need to use an additional binder to assist in forming the carbon outer layer 120 on the surface 110A of the electrode core 110. The thickness of the carbon outer layer 120 can range from several nanometers to several micrometers as required. Therefore, compared with the electrode core 110, the thickness of the carbon outer layer 120 is much smaller than the thickness of the electrode core 110. According to one embodiment, the Mohs hardness of the carbon outer layer 120 is lower than the Mohs hardness of the electrode core 110 .

[0023] Graphite is an effective inert material. The graphite material can be a continuous layer that completely covers the electrode core 110. In one embodiment, the carbon outer layer 120 includes a carbonaceous material 121, such as a carbon material. In another embodiment, the carbon outer layer 120 is substantially composed of the carbonaceous material 121 and the first corrosion-resistant metal 111, wherein the carbon outer layer 120 is a non-insertion type electrode material. The carbon outer layer 120 is conductive, and its resistivity is, for example, less than 1X10 -3 Ω·m. Due to the presence of the corrosion-resistant metal ions in the electroplating solution 11, the first corrosion-resistant metal 111 is dispersed in the carbonaceous material 121, or the carbonaceous material 121 is dispersed in the first corrosion-resistant metal 111, so that the two together form the carbonaceous outer layer 120. In another embodiment, part of the first corrosion-resistant metal 111 and part of the carbonaceous material 121 form an alloy 123.

[0024] The carbon-containing material 121 includes, for example, a graphite-based carbon material. The graphite-based carbon material includes, for example, at least one of graphite, graphene, reduced graphene oxide, and graphene oxide. An appropriate carbon source precursor 13, such as at least one of graphite, graphene, reduced graphene oxide, and graphene oxide, can be reduced on the surface 110A of the electrode core 110 under the conditions of an electroplating deposition reaction to form a carbon-containing material 121 that covers the electrode core 110. The electroplating deposition reaction is a non-spontaneous redox reaction in the presence of an externally provided voltage and current. According to one embodiment, the electrode plating solution may include a carbon source precursor (for example), a metal salt (for example, a nickel salt), an additive (for example, boric acid), and / or a dispersant, but is not limited thereto.

[0025] In one embodiment, the corrosion-resistant metal may be a passive metal or a corrosion-resistant metal material, such as a group consisting of ruthenium, rhodium, palladium, silver, osmium, iridium, platinum, gold, nickel, tantalum, niobium, zirconium, titanium, or an alloy thereof, but not limited thereto. A passive metal material or a corrosion-resistant metal material may refer to a metal material or an alloy that is chemically stable to at least one of a strong acid, a strong base, and a halide. Corrosion resistance may refer to a chemically passive metal material whose thickness change value is less than or equal to 1 nanometer (nm) per minute under certain corrosion conditions. A strong acid may be, for example, perchloric acid, chloric acid, sulfuric acid, hydrochloric acid, nitric acid, phosphoric acid, or a mixture thereof, but not limited thereto. A strong base may be, for example, an organic quaternary ammonium base such as sodium hydroxide, potassium hydroxide, tetramethylammonium hydroxide, or a mixture thereof, but not limited thereto. A halide may be, for example, a fluoride, a fluoride salt, hydrogen fluoride, hydrofluoric acid, aqua regia, or a mixture thereof, but not limited thereto. For example, niobium can resist the corrosion of molten alkali, aqua regia, hydrochloric acid, sulfuric acid, nitric acid, or phosphoric acid. Silver, platinum, gold, or nickel (including nickel alloys) can resist corrosion by hydrogen fluoride or hydrofluoric acid.

[0026] In one embodiment, the carbonaceous outer layer 120 formed by the electroplating deposition reaction of the present invention can be a passive thin layer of carbonaceous material, and its thickness is, for example, 1 μm to 5 mm, but it is not limited thereto. For example, the carbonaceous outer layer 120 can be a non-insertion type thin layer of conductive electrode material. This passive carbonaceous material is passive to metals or ions, and will not undergo conventional insertion reactions with metals or ions to produce corresponding intercalation compounds or intercalation complexes. Therefore, the carbonaceous outer layer 120 of the present invention can also simplify the chemical reaction between the electrode and the electrolyte in the electrolysis reaction of the composite inert electrode of the present invention, avoid the electrode core 110 from being lost by the electrolyte, or reduce the rate at which the electrode core 110 is lost by the electrolyte, which is one of the technical features of the method for forming a composite inert electrode of the present invention. In addition, since the carbonaceous outer layer is a composite material, which includes a carbonaceous material and a corrosion-resistant metal dispersed therein, the carbonaceous outer layer containing the corrosion-resistant metal in this case has a longer service life than the carbonaceous outer layer containing only a carbonaceous material.

[0027] Please refer to Figure 5 to Figure 6 , which is a schematic diagram of a method for regenerating a composite inert electrode according to an embodiment of the present invention. The conductive carbon outer layer 120 covering the electrode core 110 may age after use, thereby affecting the long-term performance of the composite inert electrode 100. The present invention can regenerate the aged composite inert electrode 100 through a simple method. Please refer to Figure 5As shown, first, a composite inert electrode 100 having an aged conductive carbon outer layer 120 is provided. If necessary, a simple method can be used to strip off the aged conductive carbon outer layer 120, such as a heating process to oxidize the aged conductive carbon outer layer 120, or a grinding process to grind off the aged conductive carbon outer layer 120, and completely strip off the aged conductive carbon outer layer 120, but it is not limited thereto. Compared with nickel metal or other metals that can be used as electrolytic electrodes, ceramic materials are particularly suitable for regenerating the aged composite inert electrode 100 by heating and stripping because of their high heat resistance and mechanical strength.

[0028] Please refer to Figure 6 As shown, the aforementioned electrode electroplating deposition method can be used again to form a conductive carbon outer layer 121 on the surface 110A of the electrode core 110 to obtain the regenerated composite inert electrode 101 of the present invention, so that the composite inert electrode 101 provided by the present invention becomes a composite electrode that is easy to regenerate (re-rejuvenate) its corrosion resistance and restore its long-term performance. By stripping off the overused and aged conductive carbon outer layer 120 and then forming a cheap conductive carbon outer layer 121, the maintenance cost of the composite inert electrode 100 provided by the present invention can be reduced.

[0029] After the above-mentioned method for forming a composite inert electrode, a composite inert electrode 100 provided by the present invention can be obtained. Figures 7 to 9 , which is a schematic diagram of the cross-sectional structure of a composite inert electrode 100 according to an embodiment of the present invention. A composite inert electrode 100 provided by the present invention is substantially composed of an electrode core 110 and a carbonaceous outer layer 120. The carbonaceous outer layer 120 covers the electrode core 110. In one embodiment, the carbonaceous outer layer 120 is substantially composed of a carbonaceous material 121 and a corrosion-resistant metal 111, wherein the carbonaceous outer layer 120 is a non-insertion type electrode material, and the corrosion-resistant metal 111 is dispersed in the carbonaceous material 121 to form the carbonaceous outer layer 120. In another embodiment, part of the corrosion-resistant metal 111 and part of the carbonaceous material 121 form an alloy 123. In a preferred embodiment, the carbonaceous outer layer 120 directly and completely covers the electrode core 110 as a whole.

[0030] In one embodiment, the electrode core 110 is substantially made of ceramic material. The details of the ceramic material and the corrosion-resistant metal are as described above, so they are not repeated here. Depending on the situation, the electrode core 110 can be a single-layer structure, a double-layer structure, or a multi-layer composite structure. Figure 7FIG. 1 is a cross-sectional view of a composite inert electrode 100 having a single-layer electrode core 110 according to an embodiment of the present invention. The single-layer electrode core 110 may be substantially composed of a single corrosion-resistant metal, such as substantially composed of nickel, but not limited thereto.

[0031] In another embodiment, the double-layer electrode core 110 may be substantially composed of a first corrosion-resistant metal 111 with a smaller outer layer thickness encapsulating a second corrosion-resistant metal 112 with a larger inner layer thickness. Figure 8 The cross-sectional structure diagram of the composite inert electrode 100 of the double-layer structure electrode core 110 according to one embodiment of the present invention. The second corrosion-resistant metal 112 of the inner layer can be lower in price than the first corrosion-resistant metal 111 of the outer layer, which is beneficial to reduce the raw material cost of the electrode core 110. For example, the double-layer structure electrode core 110 can be substantially composed of an outer layer of gold encapsulating an inner layer of nickel, or substantially composed of an outer layer of silver encapsulating an inner layer of titanium, but is not limited thereto.

[0032] In another embodiment, the multi-layer electrode core 110 may be substantially composed of a first corrosion-resistant metal 111 with a smaller outer layer thickness wrapping a second corrosion-resistant metal 112 in the middle layer, and then the second corrosion-resistant metal 112 in the middle layer wrapping a third corrosion-resistant metal 113 with a larger inner layer thickness, and so on to form a composite electrode core structure with three or more layers. Fig. 9 The cross-sectional structure diagram of the composite inert electrode 100 of the three-layer structure electrode core 110 according to one embodiment of the present invention is shown. For example, the three-layer structure electrode core 110 may be substantially composed of an outer layer of gold wrapping a middle layer of silver, and the middle layer of silver wrapping an inner layer of nickel, which is beneficial to achieve a balance between reducing the raw material cost of the electrode core 110 and extending the service life of the composite inert electrode 100, but is not limited thereto.

[0033] In one embodiment, the carbonaceous outer layer 120 includes a carbonaceous material. The carbonaceous material includes at least one of graphene, reduced graphene oxide and graphene oxide. In another embodiment, the carbonaceous outer layer 120 may further include the aforementioned corrosion-resistant metal. For example, the carbonaceous outer layer 120 may include a mixture or compound of the aforementioned corrosion-resistant metal and the carbonaceous material. The mixture may be an alloy-like structure or a binary material in which layered graphite is dispersed in the corrosion-resistant metal. The compound may be a compound of a corrosion-resistant metal and carbon. In particular, the carbonaceous outer layer 120 formed by the electrode electroplating deposition method or the electrodeless electroplating deposition method of the present invention may be a passive carbonaceous material. For example, the carbonaceous outer layer 120 may be a non-insertion type electrode material, which is not suitable for use in primary batteries or secondary batteries. This passive carbonaceous material is passive to metals or ions, and will not undergo conventional insertion reactions with metals or ions to produce corresponding intercalation compounds or intercalation complexes, which is one of the technical features of the method of composite inert electrodes of the present invention.

[0034] Compared with a simple graphite electrode, the composite inert electrode 100 of the present invention still retains the advantages of the electrode core 110 of a metal material. For example, a simple method can be used to peel off the used and aged conductive carbonaceous outer layer 120 without damaging the electrode core 110 of a ceramic material. In addition, the composite inert electrode 100 of the present invention can be regenerated by forming a new conductive carbonaceous outer layer 121 on the surface 110A of the electrode core 110 after the used and aged conductive carbonaceous outer layer 120 is peeled off, thereby obtaining the regenerated composite inert electrode 101 of the present invention, making the composite inert electrode 100 provided by the present invention a composite electrode that is easy to regenerate and maintain.

[0035] The composite inert electrode 100 provided by the present invention can be used in an electrochemical device, such as an electrolytic cell. Fig.10 As shown, it is a schematic diagram of the cross-sectional structure of an electrolytic cell including a composite inert electrode 100 according to an embodiment of the present invention. The electrolytic cell 200 provided by the present invention comprises an electrolyte 210, a power supply structure 220, and at least one composite inert electrode 100 as described above (for example, two composite inert electrodes 100). The electrolyte 210 can be a chemical solution comprising at least one electrolyte. The electrolyte 210 can, for example, contain at least one of a strong acid, a strong base, and a fluoride. In one embodiment, the strong acid can be, for example, perchloric acid, chloric acid, sulfuric acid, hydrochloric acid, nitric acid, phosphoric acid, or a mixture thereof, but is not limited thereto. The strong base can be, for example, an organic quaternary ammonium base such as sodium hydroxide, potassium hydroxide, tetramethylammonium hydroxide, or a mixture thereof, but is not limited thereto. The halide can be, for example, a fluoride, a fluoride salt, hydrogen fluoride, hydrofluoric acid, aqua regia, or a mixture thereof, but is not limited thereto.

[0036] The power supply structure 220 can provide the composite inert electrode 100 with appropriate voltage and current to perform a predetermined electrolytic reaction. The composite inert electrode 100 will perform a predetermined electrolytic reaction when immersed in the electrolyte 210 under appropriate voltage conditions, current conditions and temperature conditions. In one embodiment, the carbonaceous outer layer 120 directly contacts the electrolyte 210 to isolate the electrolyte 210 from contacting the electrode core 110 and reduce the possibility of damage to the electrode core 110, and form a protective layer to extend the service life of the composite inert electrode 100. The composite inert electrode 110 is essentially composed of the electrode core 110 and the carbonaceous outer layer 120. Please refer to the above for the details of the carbonaceous outer layer 120 and the electrode core 110, so it will not be repeated. In a preferred embodiment, the carbonaceous outer layer 120 can be a non-insertion type electrode material, which is one of the technical features of the electrolytic cell 200 of the present invention.

[0037] During the electrolysis process, one (or some) of the composite inert electrodes 110 is configured to receive a positive voltage from the power structure 220, and another (or some) of the composite inert electrodes 110 is configured to receive a negative voltage from the power structure 220. By applying positive voltage and negative voltage to the composite inert electrodes 110, respectively, the electrolyte 210 will undergo an electrolysis reaction to generate corrosive gas and / or flammable gas. According to one embodiment, the composite inert electrode 110 as an anode will generate corrosive gas, such as fluorine-containing nitride, and the composite inert electrode 110 as a cathode will generate flammable gas, such as hydrogen, but is not limited thereto.

[0038] The above description is only a preferred embodiment of the present invention. All equivalent changes and modifications made according to the scope of the patent application of the present invention should fall within the scope of the present invention.

[0039] Description of Reference Numerals

[0040] 10. Plating tank

[0041] 11. Plating solution

[0042] 12. Sacrificial electrode

[0043] 13.Carbon source precursor

[0044] 100. Composite inert electrode

[0045] 101. Composite inert electrode

[0046] 110.Electrode core

[0047] 110A.Surface

[0048] 111.The first corrosion-resistant metal

[0049] 112. Second corrosion-resistant metal

[0050] 113. The third corrosion-resistant metal

[0051] 120. Carbon outer layer

[0052] 121. Carbonaceous materials

[0053] 123. Alloy

[0054] 200.Electrolyzer

[0055] 210. Electrolyte

[0056] 220. Power supply structure.

Claims

1. A composite inert electrode, substantially consisting of an electrode core and a carbonaceous outer layer covering the electrode core, wherein: The electrode core is substantially composed of a ceramic material; as well as The carbon outer layer is substantially composed of a carbon-containing material and a corrosion-resistant metal, wherein the carbon outer layer is a non-insertion type electrode material, and the corrosion-resistant metal is dispersed in the carbon-containing material.

2. The composite inert electrode as claimed in claim 1, wherein the corrosion-resistant metal is selected from a group consisting of ruthenium metal, rhodium metal, palladium metal, silver metal, osmium metal, iridium metal, platinum metal, gold, nickel metal, tantalum metal, and titanium metal.

3. The composite inert electrode as claimed in claim 1, wherein the carbon-containing material comprises at least one of carbon, graphene, reduced graphene oxide and graphene oxide.

4. The composite inert electrode as claimed in claim 1, wherein the corrosion-resistant metal and the carbon-containing material form an alloy. The composite inert electrode as claimed in claim 1 , wherein the carbon outer layer directly and entirely covers the electrode core.

6. The composite inert electrode of claim 1, wherein the carbonaceous outer layer is a composite layer covering the electrode core.

7. An electrolytic cell comprising: An electrolyte comprising at least one of a strong acid, a strong base and a fluoride; and The composite inert electrode as claimed in claim 1, wherein the carbonaceous outer layer directly contacts the electrolyte to isolate the electrolyte from contacting the electrode core.

8. The electrolytic cell of claim 7, wherein the number of the composite inert electrodes is greater than 1, and some of the composite inert electrodes are configured to receive a positive voltage, and other of the composite inert electrodes are configured to receive a negative voltage.

9. A method for forming a composite inert electrode, comprising: providing an electrode core, wherein the electrode core consists essentially of a ceramic material; and An electroplating deposition reaction is carried out in the presence of a carbon source material to form a carbon outer layer covering the electrode core, wherein the carbon outer layer is substantially composed of a carbon-containing material and the corrosion-resistant metal, the carbon outer layer is a non-insertion type electrode material, and the corrosion-resistant metal is dispersed in the carbon-containing material.

10. The method of forming a composite inert electrode as claimed in claim 9, wherein the Mohs hardness of the ceramic material is higher than the Mohs hardness of the carbonaceous outer layer.