Production process of electrolytic polishing line easy to clean and high in electrolytic efficiency

The current abnormality of the electrolytic polishing line is identified through the current monitoring system, and combined with the adjustment of the electrolytic solute concentration, the problem of uneven electrolytic reaction speed is solved, and the electrolytic efficiency and product quality stability are improved.

CN118932473AInactive Publication Date: 2024-11-12JIANGYIN TITANS HIGH VOLTAGE ELECTRIC CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411053933.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-02
Publication Date
2024-11-12
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

In the production process of electrolytic polishing lines, the system for monitoring current and identifying the degree of current abnormality is lacking, resulting in uneven electrolytic reaction speed, which in turn affects the production cycle, energy consumption and product quality stability.

Method used

The current monitoring system is adopted to obtain current value data, analyze abnormal characterization values, judge the degree of current abnormality, and adjust it according to the abnormal signal of the electrolyte solute concentration to ensure that the electrolysis process runs in an optimized state.

Benefits of technology

Real-time monitoring and handling of current abnormalities is realized, electrolytic efficiency and product quality are improved, current abnormalities are identified and adjusted in a timely manner, and the stability of the electrolytic process is ensured.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118932473A_ABST
    Figure CN118932473A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of electrolytic polishing line production, and discloses a production process of an easy-to-clean high-electrolytic-efficiency electrolytic polishing line, which comprises the following steps: putting a treated workpiece into an electrolytic bath, and performing electrolytic polishing treatment under the monitoring of a current monitoring system. The method comprises the following steps: firstly, acquiring a current value in an electrolysis process, judging the current value to obtain an electrolytic current abnormal signal, acquiring appearance data of the electrolytic current abnormal signal, calculating a current abnormal characterization value based on the appearance data, and finally comparing the current abnormal characterization value with a current abnormal characterization threshold value to judge the current abnormal degree. According to the method, a signal with low current abnormal degree or a signal with high current abnormal degree is generated, so that the system can quickly identify the current abnormal degree and timely detect and process the current abnormal degree by monitoring and judging the current value in the electrolysis process in real time, the electrolysis process can be operated in a better state, and the electrolysis efficiency and the product quality are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of electrolytic polishing line production, and in particular to a production process of an electrolytic polishing line that is easy to clean and has high electrolytic efficiency. Background Art

[0002] Electrolytic polishing is a process that uses electrochemical reactions to smooth and polish metal surfaces. In this process, the metal workpiece acts as an anode, immersed in an electrolyte containing a specific chemical composition, and a direct current is passed through it. When the current passes through, the surface of the workpiece will undergo anodic dissolution, that is, the raised parts of the metal surface will be dissolved first, thereby achieving a smooth surface effect.

[0003] In the production process of electrolytic polishing line, unstable current will lead to uneven electrolytic reaction speed, making it impossible to maintain the electrolytic process in an optimized state, which will lead to extended production cycle and increased energy consumption, thus affecting the output and quality stability of products. However, at present, there is a lack of current monitoring and current abnormality identification system in the process of electrolytic polishing line, so that the situation of high current abnormality cannot be handled in time;

[0004] In view of this, we proposed a production process for an easy-to-clean and high-electrolytic-efficiency electrolytic polishing line. Summary of the invention

[0005] The object of the present invention is to provide a production process for an easy-to-clean, high-electrolysis-efficiency electrolytic polishing line to solve the problem of lack of a system for monitoring current and identifying the degree of current abnormality in the above background.

[0006] The purpose of the present invention can be achieved through the following technical solutions:

[0007] A production process for an easy-to-clean high-electrolysis-efficiency electrolytic polishing line comprises the following steps:

[0008] The processed workpiece is placed in an electrolytic cell, and electrolytic polishing is performed under the monitoring of a current monitoring system. During the electrolysis process, the electrolyte circulates in the electrolytic cell; wherein the monitoring process of the current monitoring system specifically includes: S1: obtaining the current value data during the electrolysis process, and performing analysis and processing to obtain a current anomaly characterization value; S2: comparing the current anomaly characterization value with the current anomaly characterization threshold value, and if the current anomaly characterization value is greater than or equal to the current anomaly characterization threshold value, generating a current anomaly high degree signal; S3: based on the above-mentioned current anomaly high degree signal, obtaining the electrolyte solute concentration value data during the electrolysis process, and judging whether the electrolyte solute concentration is abnormal, and generating an electrolyte solute concentration abnormality signal; S4: based on the above-mentioned electrolyte solute concentration abnormality signal, calculating the synchronous correlation value of the current anomaly and the electrolyte solute concentration abnormality, and judging, if the synchronous correlation value is greater than or equal to the synchronous correlation threshold value, generating a correlation influence signal; S5: adjusting the electrolyte solute concentration value based on the above-mentioned correlation influence signal.

[0009] As a further solution of the present invention: the process of obtaining the current abnormality characterization value is:

[0010] Acquire data on the occurrence of abnormal current signals, wherein the data on the occurrence of abnormal current signals include a current abnormal time ratio and a current abnormal degree value;

[0011] The abnormal time ratio is multiplied by the current abnormality degree value to obtain the current abnormality characterization value.

[0012] As a further solution of the present invention: the process of obtaining the abnormal time ratio and the current abnormality degree value is as follows:

[0013] During the monitoring time period, the duration of each abnormal current signal is obtained, marked as the abnormal current time period, and all the abnormal current time periods obtained are summed to obtain the total duration of the abnormality. The total duration of the abnormality is ratioed with the total time of the detection time period to obtain the abnormal time ratio.

[0014] As a further solution of the present invention: the process of obtaining the current abnormality value is as follows:

[0015] During the monitoring period, the current value data of all abnormal time periods are obtained, the current values ​​in the abnormal time periods are respectively calculated with the current standard values, the absolute value of the difference is recorded as the abnormal current deviation value, the abnormal current deviation value is ratioed with the current standard value to obtain the abnormal current deviation ratio, all the abnormal current deviation ratios are summed and averaged to obtain the current abnormality degree value.

[0016] As a further solution of the present invention: the process of generating the abnormal electrolysis current signal is:

[0017] The total time of the electrolysis process is divided into a number of monitoring time nodes, and the time period between every two monitoring time nodes is marked as a monitoring time period;

[0018] Obtaining current value data for each monitoring time period, and comparing the current value data with the current threshold range respectively;

[0019] If the current value is not within the current threshold range, an electrolysis current abnormality signal is generated.

[0020] As a further solution of the present invention: the process of generating an abnormal electrolyte solute concentration signal is:

[0021] Acquire electrolyte solute concentration value data during the electrolysis process, and compare the electrolyte solute concentration value with the electrolyte solute concentration threshold range;

[0022] If the electrolyte solute concentration value is not within the electrolyte solute concentration threshold range, an electrolyte solute concentration abnormal signal is generated.

[0023] As a further solution of the present invention: the process of obtaining the synchronous association value is:

[0024] Get the effective percentage value and the total value of the target time period;

[0025] Multiply the effective proportion value by the total value of the target time period to obtain the synchronization correlation value.

[0026] As a further solution of the present invention: the process of obtaining the total value of the target time period is:

[0027] Obtain a time period in which an abnormal electrolyte solute concentration signal is generated, mark it as an abnormal concentration time period, and obtain an abnormal current time period;

[0028] Extract the overlapping time period of the concentration abnormal time period and the current abnormal time period, mark it as the target time period, sum all the target time periods, and obtain the total value of the target time period;

[0029] As a further solution of the present invention: the process of obtaining the effective ratio value is:

[0030] Divide each target time period into a number of target time points, and obtain the current value and electrolyte solute concentration value corresponding to each target time point within the target time period;

[0031] With time as the X-axis and current value as the Y-axis, a two-dimensional model is established, and the current value is substituted into the two-dimensional model to draw a current line graph;

[0032] With time as the X-axis and electrolyte solute concentration as the Y-axis, a two-dimensional model is established, and the electrolyte solute concentration value is substituted into the two-dimensional model to draw a line graph of the electrolyte solute concentration;

[0033] Mark the straight line segment connecting two adjacent target time points as the target sub-polyline;

[0034] Obtain the slope values ​​of all target sub-broken lines in the current broken line graph and the electrolyte solute concentration broken line graph respectively, and mark them as the current target sub-broken line slope value and the concentration target sub-broken line slope value respectively;

[0035] The current target sub-broken line slope value and the concentration target sub-broken line slope value corresponding to the same time are ratio-processed to obtain the target slope ratio;

[0036] All target slope ratios are summed and averaged to obtain the target slope ratio mean, and all target slope ratios are respectively subtracted from the target slope ratio mean to obtain the absolute value of the difference, which is marked as the target slope ratio deviation value;

[0037] comparing the target slope ratio deviation value with a target slope ratio deviation threshold;

[0038] If the target slope ratio deviation value is less than or equal to the target slope ratio deviation threshold, a valid target slope ratio is generated;

[0039] Obtain the number of valid target slope ratio values, perform ratio processing on the number of valid slope ratio values ​​and the number of target sub-broken lines in the target time period to obtain the valid proportion value;

[0040] As a further solution of the present invention: the process of adjusting the electrolyte solute concentration value is:

[0041] Obtaining the abnormal current deviation ratio within the current abnormal time period, summing up and averaging all the abnormal current deviation values, and obtaining the abnormal current deviation mean;

[0042] Obtaining a target slope ratio mean value, performing ratio processing on the abnormal current deviation mean value and the target slope ratio mean value, and obtaining an electrolyte solute concentration adjustment value;

[0043] Obtain the electrolyte solute concentration values ​​in the overlapping time period, sum and average them, and obtain the average value of abnormal electrolyte solute concentration;

[0044] The abnormal electrolyte solute concentration mean value and the electrolyte solute concentration adjustment value are summed to obtain the electrolyte solute concentration target value.

[0045] Beneficial effects of the present invention:

[0046] (1) The present invention first obtains the current value during the electrolysis process, and judges the current value to obtain an abnormal electrolysis current signal, and obtains the occurrence data of the abnormal electrolysis current signal, calculates the abnormal current characterization value based on the occurrence data, and finally compares the abnormal current characterization value with the abnormal current characterization threshold value to judge the degree of the abnormal current, and generates a low abnormal current degree signal or a high abnormal current degree signal, so that the system can quickly identify the abnormal current degree by real-time monitoring and judging the current value during the electrolysis process, and timely detect and process it, so that the electrolysis process can be operated in a better state, thereby improving the electrolysis efficiency and product quality;

[0047] (2) The present invention obtains electrolyte solute concentration value data and makes a judgment to generate an electrolyte solute concentration abnormality signal. Based on the electrolyte solute concentration value and the current value at the time of the abnormality, a synchronous correlation value is calculated. According to the synchronous correlation value, it is determined whether the electrolyte solute concentration has an effect on the electrolysis current. If an effect exists, the electrolyte solute concentration value is adjusted in a timely manner, thereby facilitating timely analysis of the cause of the current abnormality during the electrolysis process, rapid adjustment of the current abnormality during the electrolysis process, and improving the electrolysis efficiency and product quality. BRIEF DESCRIPTION OF THE DRAWINGS

[0048] The present invention will be further described below in conjunction with the accompanying drawings.

[0049] Figure 1 This is a schematic diagram of the production process of an easy-to-clean high-electrolysis efficiency electrolytic polishing line of the present invention;

[0050] Figure 2 It is a schematic flow chart of a production process current monitoring system of an easy-to-clean high-electrolysis efficiency electrolytic polishing line in the present invention;

[0051] Figure 3 It is a schematic diagram of the process of obtaining the current abnormality characterization value in the production process of an easy-to-clean high-electrolysis efficiency electrolytic polishing line in the present invention. DETAILED DESCRIPTION

[0052] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0053] Example 1

[0054] See also Figure 1 - Figure 3 As shown, the present invention is a production process for an easy-to-clean high-electrolysis efficiency electrolytic polishing line, comprising the following steps:

[0055] Step 1: Clean and deburr the surface of the metal workpiece to be processed to ensure that there is no dirt and burrs on the surface of the workpiece;

[0056] Step 2: Place the processed workpiece into the electrolytic cell and perform electrolytic polishing under the monitoring of the current monitoring system. During the electrolysis process, the electrolyte circulates in the electrolytic cell to ensure uniform and efficient electrolysis.

[0057] Step 3: After the electrolytic polishing is completed, the workpiece enters the liquid collecting tank, water washing tank, and hot water rinsing tank for cleaning in sequence. The liquid collecting tank collects the residual electrolyte, and the water washing tank and hot water rinsing tank perform preliminary water washing and hot water rinsing respectively, thereby removing the residual electrolyte and dirt for easy cleaning;

[0058] Step 4: Put the cleaned workpiece on the drying rack for drying. The hot air generated by the hot air generator quickly evaporates the moisture on the surface of the workpiece to ensure that the workpiece is dry without residue;

[0059] Step 5: Perform quality inspection on the dried workpieces to ensure that they meet the surface quality requirements before packaging and storage.

[0060] Example 2

[0061] Based on the above embodiments, unstable current will lead to uneven speed of electrolytic reaction, so that the electrolytic process cannot be maintained in an optimized state, which will lead to extended production cycle and increased energy consumption. At the same time, it will also affect the output and quality stability of the product. The present invention is a production process of an easy-to-clean high-electrolytic efficiency electrolytic polishing line. The monitoring process of the current monitoring system specifically includes:

[0062] S1: Obtain the current value data during the electrolysis process, and analyze and process it to obtain the current abnormality characterization value;

[0063] In some embodiments, the total time of the electrolysis process is divided into a number of monitoring time nodes, and the time period between every two monitoring time nodes is marked as a monitoring time period;

[0064] Obtain the current value data of each monitoring time period, and compare the current value data with the current threshold range (the current threshold range is set by a technician in this field based on historical experimental data);

[0065] If the current value is within the current threshold range, an electrolysis current normal signal is generated;

[0066] If the current value is not within the current threshold range, an electrolysis current abnormal signal is generated;

[0067] Based on the electrolysis current abnormal signal, data of the current abnormal signal is obtained, wherein the data of the current abnormal signal includes a current abnormal time ratio and a current abnormal degree value;

[0068] During the monitoring period, the duration of each abnormal current signal is obtained, marked as the abnormal current period, and all the abnormal current periods obtained are summed to obtain the total duration of the abnormality, and the total duration of the abnormality is processed with the total time of the detection period to obtain the abnormal time ratio;

[0069] It should be explained that the meaning of the abnormal time ratio is: the abnormal time ratio is calculated by the total duration of the current abnormality and the total duration of the detection period, that is, the larger the abnormal time ratio is, the larger the total duration of the current abnormality is, the higher the degree of current abnormality is during the electrolysis process, the lower the electrolysis efficiency is, and the lower the product quality is;

[0070] During the monitoring period, the current value data of all abnormal time periods are obtained, and the current values ​​in the abnormal time periods are respectively calculated with the current standard values ​​(the current standard value is the average of the maximum value and the minimum value of the current threshold range), and the absolute value of the difference is recorded as the abnormal current deviation value, and the abnormal current deviation value is processed with the current standard value to obtain the abnormal current deviation ratio, and all abnormal current deviation ratios are summed and averaged to obtain the current abnormality degree value;

[0071] It should be explained that the meaning reflected by the current abnormality value is: the current abnormality value is calculated by the abnormal current deviation ratio, that is, the larger the current abnormality value, the larger the mean value of the abnormal current deviation ratio, the larger the difference between the abnormal current value and the current standard value, and the higher the current abnormality during the electrolysis process, the lower the electrolysis efficiency and the lower the product quality;

[0072] The abnormal time ratio value is multiplied by the current abnormality degree value to obtain the current abnormality characterization value;

[0073] S2: comparing the current abnormality characterization value with the current abnormality characterization threshold, determining the degree of current abnormality, and generating a low current abnormality degree signal or a high current abnormality degree signal;

[0074] In some embodiments, a current anomaly characterization value is obtained, and the current anomaly characterization value is compared with a current anomaly characterization threshold value (the current anomaly characterization threshold value is summarized and set by a person skilled in the art based on historical experimental data);

[0075] If the current anomaly characterization value is less than the current anomaly characterization threshold, it means that although there are abnormal current fluctuations in the electrolysis process, these fluctuations have not reached a level that significantly affects the process effect. Therefore, the current anomaly in the electrolysis process is within an acceptable range, and a low current anomaly signal is generated;

[0076] If the current abnormality characterization value is greater than or equal to the current abnormality characterization threshold, it means that the abnormal current fluctuation in the electrolysis process has exceeded the acceptable range, which may have an adverse effect on the electrolysis efficiency and product quality. Therefore, there is a significant abnormality in the current in the electrolysis process, and a high current abnormality signal is generated;

[0077] The core technology of this embodiment is: first, the current value during the electrolysis process is obtained, and the current value is judged to obtain the electrolysis current abnormality signal, and the occurrence data of the electrolysis current abnormality signal is obtained, and the current abnormality characterization value is calculated based on the occurrence data, and finally the current abnormality characterization value is compared with the current abnormality characterization threshold, and the degree of current abnormality is judged to generate a low current abnormality signal or a high current abnormality signal. Therefore, by real-time monitoring and judging the current value during the electrolysis process, the system can quickly identify the degree of current abnormality, detect and process it in time, so that the electrolysis process can run in a better state, thereby improving the electrolysis efficiency and product quality.

[0078] Example 3

[0079] Based on the above embodiment, too high or too low concentration of the solute in the electrolyte may affect the change of the current during the electrolysis process. The monitoring process of the current monitoring system specifically includes:

[0080] S3: Based on the above-mentioned high current abnormality signal, obtaining electrolyte solute concentration value data during the electrolysis process, and determining whether the electrolyte solute concentration is abnormal, and generating an electrolyte solute concentration normal signal or an electrolyte solute concentration abnormal signal;

[0081] In some embodiments, the electrolyte solute concentration value data during the electrolysis process is obtained, and the electrolyte solute concentration value is compared with the electrolyte solute concentration threshold range (the electrolyte solute concentration threshold range is set by those skilled in the art based on historical experimental data summary);

[0082] If the electrolyte solute concentration value is within the electrolyte solute concentration threshold range, it means that the electrolyte solute concentration value is within the process standard range, and a normal electrolyte solute concentration signal is generated;

[0083] If the electrolyte solute concentration value is not within the electrolyte solute concentration threshold range, it means that the electrolyte solute concentration value is not within the process standard range, and an electrolyte solute concentration abnormality signal is generated;

[0084] S4: Based on the electrolyte solute concentration abnormality signal, calculate the synchronous correlation value between the current abnormality and the electrolyte solute concentration abnormality, make a judgment, and generate a correlation influence signal or an uncorrelated influence signal;

[0085] In some embodiments, a time period in which an abnormal electrolyte solute concentration signal is generated is obtained, marked as a concentration abnormal time period, and a current abnormal time period is obtained;

[0086] Extract the overlapping time period of the concentration abnormal time period and the current abnormal time period, mark it as the target time period, sum all the target time periods, and obtain the total value of the target time period;

[0087] Divide each target time period into a number of target time points, and obtain the current value and electrolyte solute concentration value corresponding to each target time point within the target time period;

[0088] With time as the X-axis and current value as the Y-axis, a two-dimensional model is established, and the current value is substituted into the two-dimensional model to draw a current line graph;

[0089] With time as the X-axis and electrolyte solute concentration as the Y-axis, a two-dimensional model is established, and the electrolyte solute concentration value is substituted into the two-dimensional model to draw a line graph of the electrolyte solute concentration;

[0090] Mark the straight line segment connecting two adjacent target time points as the target sub-polyline;

[0091] Obtain the slope values ​​of all target sub-broken lines in the current broken line graph and the electrolyte solute concentration broken line graph respectively, and mark them as the current target sub-broken line slope value and the concentration target sub-broken line slope value respectively;

[0092] The current target sub-broken line slope value and the concentration target sub-broken line slope value corresponding to the same time are ratio-processed to obtain the target slope ratio;

[0093] All target slope ratios are summed and averaged to obtain the target slope ratio mean, and all target slope ratios are respectively subtracted from the target slope ratio mean to obtain the absolute value of the difference, which is marked as the target slope ratio deviation value;

[0094] Compare the target slope ratio deviation value with the target slope ratio deviation threshold (the target slope ratio deviation threshold is set by a person skilled in the art based on historical experimental data summary);

[0095] If the target slope ratio deviation value is less than or equal to the target slope ratio deviation threshold, it means that the target slope ratio is close to the target slope ratio mean value, and a valid target slope ratio is generated;

[0096] If the target slope ratio deviation value is greater than the target slope ratio deviation threshold, it means that the target slope ratio differs greatly from the target slope ratio mean, and an invalid target slope ratio is generated;

[0097] Obtain the number of valid target slope ratio values, perform ratio processing on the number of valid slope ratio values ​​and the number of target sub-broken lines in the target time period to obtain the valid proportion value;

[0098] It should be explained that the meaning reflected by the effective proportion value is: the effective proportion value is calculated by the effective slope ratio value and the target sub-broken line value, that is, the larger the effective proportion value, the larger the effective slope ratio value. In the target period, the current target sub-broken line slope value and the concentration target sub-broken line slope value are in a certain proportional relationship, that is, there is a certain synchronization between the current change and the concentration change, and the greater the correlation between the current and the concentration;

[0099] Multiply the effective proportion value by the total value of the target time period to obtain the synchronization correlation value;

[0100] Compare the synchronization correlation value with the synchronization correlation threshold (the synchronization correlation threshold is set by a person skilled in the art based on historical experimental data);

[0101] If the synchronous correlation value is less than the synchronous correlation threshold, the electrolyte solute concentration has no effect on the current, and an uncorrelated influence signal is generated;

[0102] If the synchronous correlation value is greater than or equal to the synchronous correlation threshold, the electrolyte solute concentration has an influence on the current, and a correlation influence signal is generated;

[0103] S5: Based on the above correlation influence signal, adjusting the electrolyte solute concentration value;

[0104] In some embodiments, the abnormal current deviation ratio within the current abnormal time period is obtained, and all abnormal current deviation values ​​are summed and averaged to obtain the abnormal current deviation average;

[0105] Obtaining a target slope ratio mean value, performing ratio processing on the abnormal current deviation mean value and the target slope ratio mean value, and obtaining an electrolyte solute concentration adjustment value;

[0106] Obtain the electrolyte solute concentration values ​​in the overlapping time period, sum and average them, and obtain the average value of abnormal electrolyte solute concentration;

[0107] The average value of the abnormal electrolyte solute concentration is summed with the electrolyte solute concentration adjustment value to obtain the electrolyte solute concentration target value;

[0108] That is, the electrolyte solute concentration is adjusted to the electrolyte solute concentration target value.

[0109] The core technology of this embodiment is: first, the electrolyte solute concentration value data is obtained, and a judgment is made to generate an electrolyte solute concentration abnormality signal; based on the electrolyte solute concentration value and the current value at the time of the abnormality, a synchronous correlation value is calculated; based on the synchronous correlation value, it is determined whether the electrolyte solute concentration has an impact on the electrolysis current; based on the existence of an impact, the electrolyte solute concentration value is adjusted in time, which is conducive to timely analysis of the cause of the current abnormality during the electrolysis process, rapid adjustment of the current abnormality during the electrolysis process, and improvement of electrolysis efficiency and product quality.

[0110] The above is a detailed description of an embodiment of the present invention, but the content is only a preferred embodiment of the present invention and cannot be considered to limit the scope of implementation of the present invention. All equivalent changes and improvements made within the scope of the present invention should still fall within the scope of the patent coverage of the present invention.

Claims

1. A production process for an easy-to-clean high-electrolysis-efficiency electrolytic polishing line, characterized in that: The following steps are involved: The processed workpiece is placed in an electrolytic cell and electropolished under the monitoring of a current monitoring system. During the electrolysis process, the electrolyte circulates in the electrolytic cell. Among them, the monitoring process of the current monitoring system specifically includes: S1: Obtain the current value data during the electrolysis process, and analyze and process it to obtain the current abnormality characterization value; S2: comparing the current abnormality characterization value with the current abnormality characterization threshold, and generating a current abnormality high degree signal if the current abnormality characterization value is greater than or equal to the current abnormality characterization threshold; S3: Based on the above-mentioned current abnormality high degree signal, obtain the electrolyte solute concentration value data during the electrolysis process, and determine whether the electrolyte solute concentration is abnormal, and generate an electrolyte solute concentration abnormality signal; S4: Based on the electrolyte solute concentration abnormality signal, a synchronous correlation value between the current abnormality and the electrolyte solute concentration abnormality is calculated, and a judgment is made. If the synchronous correlation value is greater than or equal to a synchronous correlation threshold, a correlation influence signal is generated; S5: Based on the above-mentioned correlation influence signal, the electrolyte solute concentration value is adjusted.

2. The production process of an easy-to-clean high-electrolysis efficiency electrolytic polishing line according to claim 1, characterized in that: The process of obtaining the current anomaly characterization value is as follows: Acquire data on the occurrence of abnormal current signals, wherein the data on the occurrence of abnormal current signals include a current abnormal time ratio and a current abnormal degree value; The abnormal time ratio value is multiplied by the current abnormality degree value to obtain the current abnormality characterization value.

3. The production process of an easy-to-clean high-electrolysis efficiency electrolytic polishing line according to claim 2, characterized in that: The process of obtaining the abnormal time ratio and the current abnormality degree is as follows: During the monitoring time period, the duration of each abnormal current signal is obtained, marked as the abnormal current time period, and all the abnormal current time periods obtained are summed to obtain the total duration of the abnormality. The total duration of the abnormality is ratioed with the total time of the detection time period to obtain the abnormal time ratio.

4. The production process of an easy-to-clean high-electrolysis efficiency electrolytic polishing line according to claim 2, characterized in that: The process of obtaining the current abnormality value is as follows: During the monitoring period, the current value data of all abnormal time periods are obtained, the current values ​​in the abnormal time periods are respectively calculated with the current standard values, the absolute value of the difference is recorded as the abnormal current deviation value, the abnormal current deviation value is ratioed with the current standard value to obtain the abnormal current deviation ratio, all the abnormal current deviation ratios are summed and averaged to obtain the current abnormality degree value.

5. The production process of an easy-to-clean high-electrolysis-efficiency electrolytic polishing line according to claim 2, characterized in that: The process of generating an abnormal electrolysis current signal is: The total time of the electrolysis process is divided into a number of monitoring time nodes, and the time period between every two monitoring time nodes is marked as a monitoring time period; Obtaining current value data for each monitoring time period, and comparing the current value data with the current threshold range respectively; If the current value is not within the current threshold range, an electrolysis current abnormality signal is generated.

6. The production process of an easy-to-clean high-electrolysis efficiency electrolytic polishing line according to claim 1, characterized in that: The process of generating abnormal electrolyte solute concentration signal is as follows: Acquire electrolyte solute concentration value data during the electrolysis process, and compare the electrolyte solute concentration value with the electrolyte solute concentration threshold range; If the electrolyte solute concentration value is not within the electrolyte solute concentration threshold range, an electrolyte solute concentration abnormal signal is generated.

7. The production process of an easy-to-clean high-electrolysis-efficiency electrolytic polishing line according to claim 1, characterized in that: The process of obtaining the synchronous associated value is: Get the effective percentage value and the total value of the target time period; Multiply the effective proportion value by the total value of the target time period to obtain the synchronization correlation value.

8. The production process of an easy-to-clean high-electrolysis-efficiency electrolytic polishing line according to claim 7, characterized in that: The process of obtaining the total value of the target time period is as follows: Obtain a time period in which an abnormal electrolyte solute concentration signal is generated, mark it as an abnormal concentration time period, and obtain an abnormal current time period; The overlapping time period of the abnormal concentration time period and the abnormal current time period is extracted and marked as the target time period. All target time periods are summed to obtain the total value of the target time period.

9. The production process of an easy-to-clean high-electrolysis-efficiency electrolytic polishing line according to claim 8, characterized in that: The process of obtaining the effective percentage value is as follows: Divide each target time period into a number of target time points, and obtain the current value and electrolyte solute concentration value corresponding to each target time point within the target time period; With time as the X-axis and current value as the Y-axis, a two-dimensional model is established, and the current value is substituted into the two-dimensional model to draw a current line graph; With time as the X-axis and electrolyte solute concentration as the Y-axis, a two-dimensional model is established, and the electrolyte solute concentration value is substituted into the two-dimensional model to draw a line graph of the electrolyte solute concentration; Mark the straight line segment connecting two adjacent target time points as the target sub-polyline; Obtain the slope values ​​of all target sub-broken lines in the current broken line graph and the electrolyte solute concentration broken line graph respectively, and mark them as the current target sub-broken line slope value and the concentration target sub-broken line slope value respectively; The current target sub-broken line slope value and the concentration target sub-broken line slope value corresponding to the same time are ratio-processed to obtain the target slope ratio; All target slope ratios are summed and averaged to obtain the target slope ratio mean, and all target slope ratios are respectively subtracted from the target slope ratio mean to obtain the absolute value of the difference, which is marked as the target slope ratio deviation value; comparing the target slope ratio deviation value with a target slope ratio deviation threshold; If the target slope ratio deviation value is less than or equal to the target slope ratio deviation threshold, a valid target slope ratio is generated; Get the number of valid target slope ratios, and perform ratio processing on the number of valid slope ratios and the number of target sub-broken lines in the target time period to obtain the valid proportion value.

10. The production process of an easy-to-clean high-electrolysis-efficiency electrolytic polishing line according to claim 1, characterized in that: The process of adjusting the electrolyte solute concentration value is: Obtaining the abnormal current deviation ratio within the current abnormal time period, summing up and averaging all the abnormal current deviation values, and obtaining the abnormal current deviation mean; Obtaining a target slope ratio mean value, performing ratio processing on the abnormal current deviation mean value and the target slope ratio mean value, and obtaining an electrolyte solute concentration adjustment value; Obtain the electrolyte solute concentration values ​​in the overlapping time period, sum and average them, and obtain the average value of abnormal electrolyte solute concentration; The abnormal electrolyte solute concentration mean value and the electrolyte solute concentration adjustment value are summed to obtain the electrolyte solute concentration target value.

Citation Information

Cited By

  • Surface coating process for optical element product

    CN120470976A