Building material beneficial to improving 5G communication and processing method
By embedding communication divergence blocks and coating communication divergence coatings in building materials, the 5G signal attenuation problem is solved, signal propagation efficiency is improved, and organic pollutants are degraded in photocatalytic, enhancing the material applicability.
Patent Information
- Application Number
- CN202410985914.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-23
- Publication Date
- 2024-11-12
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing building materials have problems with attenuating signals to 5G communications, resulting in low signal propagation efficiency.
Cement bricks are used as the foundation material, filling holes are set up in the middle and communication divergence blocks are filled. The outer wall is coated with communication divergence coating. The coating consists of zinc acetate, anhydrous ethanol, ammonium phosphate and oxalic acid. The divergence block is a low-frequency microwave dielectric ceramic material. The surface photovoltaic signal-enhanced ZnO is prepared by a specific preparation method, and combined with a photocatalytic reaction to enhance signal propagation.
It effectively reduces signal attenuation, improves the propagation efficiency of 5G communication, and degrades organic pollutants in photocatalytics, enhancing the applicability of the material.
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of building materials, and specifically to a building material and a processing method that are beneficial to improving 5G communications. Background Art
[0002] Building materials are the foundation of construction projects, and concrete is the most widely used building material. Its main components include cement, admixtures and aggregates, which are hardened after adding water and mixing. It has the advantages of simple process and fire resistance.
[0003] With the development of 5G communication technology, there are some special requirements for building materials. These requirements are mainly reflected in the electromagnetic properties of the materials. Existing building materials have great limitations on the divergence of 5G communication signals, which accelerates the attenuation of 5G signals. Summary of the invention
[0004] 1. Technical issues to be solved
[0005] In view of the deficiencies in the prior art, the present invention provides a building material and a processing method that are beneficial to improving 5G communications, solving the problem that existing building materials accelerate 5G signal attenuation.
[0006] (II) Technical solution
[0007] To achieve the above objectives, the present invention is implemented through the following technical solutions: a building material and processing method that is beneficial to improving 5G communication, including cement bricks, a filling hole is provided in the middle of the cement bricks, the outer wall of the cement bricks is coated with communication divergent paint, and the interior of the filling hole is filled with a communication divergent block.
[0008] Preferably, the cement bricks are composed of cement, ceramsite, diatomaceous earth, water, expanded perlite and titanium dioxide.
[0009] Preferably, the mass fraction ratio of the cement, ceramsite, diatomaceous earth, water, expanded perlite and titanium dioxide is (30-40): (25-35): (23-32): (35-60): (12-15): (3-5).
[0010] Preferably, the communication divergent coating is composed of zinc acetate, anhydrous ethanol, ammonium phosphate, methanol solution and oxalic acid.
[0011] Preferably, the ratio of zinc acetate to anhydrous ethanol is set to 2.19 g: (100-150 mL), the ratio of ammonium phosphate to methanol solution is set to (0.0025-0.01 g): 20 mL, the molar ratio of zinc acetate to ammonium phosphate is 100: (0.5-3), and the ratio of oxalic acid to anhydrous ethanol is set to 2.51 g: (40-60 mL).
[0012] Preferably, the communication divergence block is made of low-frequency microwave dielectric ceramic material, and the low-frequency microwave dielectric ceramic material is made of BaO-Ln2O3-TiO2 (BLT) series with tungsten bronze structure.
[0013] Preferably, the preparation method of the communication divergent coating is:
[0014] S1, dissolving zinc acetate in anhydrous ethanol, and heating and stirring in a water bath, adding a methanol solution containing (NH4)3PO4 to the solution, dissolving oxalic acid in anhydrous ethanol, and then adding the mixture to the above-mentioned mixed solution of zinc acetate and ammonium phosphate, and stirring vigorously;
[0015] S2, transferring the mixed solution to an oven for drying, and grinding the dried solid;
[0016] S3, placing the ground solid into a muffle furnace for calcination to obtain a ZnO product;
[0017] S4. Use the prepared surface photovoltage signal enhanced ZnO to carry out photocatalytic reaction.
[0018] A method for processing building materials that is beneficial to improving 5G communications, comprising the following steps:
[0019] Step 1: Mix cement, ceramsite, diatomaceous earth, expanded perlite and titanium dioxide in a certain proportion;
[0020] Step 2: fully mix the prepared raw materials in a mixer and add water to the mixture from time to time;
[0021] Step 3, feeding the mixed raw materials into a mold of a molding machine, and pressing the molding machine into cement bricks with filling holes;
[0022] Step 4: embed the communication divergent block into the filling hole, and apply the communication divergent coating to the outer side wall of the cement brickwork;
[0023] Step 5: Place the formed cement bricks in a natural environment for water curing, and then dry and harden them.
[0024] (III) Beneficial effects
[0025] The present invention provides a building material and a processing method that are beneficial to improving 5G communication.
[0026] Beneficial effects:
[0027] 1. The building material has a communication divergent block embedded in the middle. The combination of the communication divergent block and cement bricks can effectively reduce the dielectric constant of the building material, thereby effectively reducing the attenuation of 5G signals during the propagation process, and further effectively improving the propagation efficiency of 5G communications.
[0028] 2. The outer wall of the building material is coated with a communication divergent coating, which has a stronger signal enhancement effect than traditional building materials, and can effectively degrade organic pollutants under photocatalysis, thereby improving the applicability of the building material. DETAILED DESCRIPTION
[0029] The technical solutions in the embodiments of the present invention are described clearly and completely below. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0030] Embodiment 1:
[0031] An embodiment of the present invention provides a building material that is beneficial to improving 5G communications, including cement bricks, a filling hole is provided in the middle of the cement bricks, the outer wall of the cement bricks is coated with communication divergent paint, and the interior of the filling hole is filled with a communication divergent block.
[0032] Cement bricks are composed of cement, ceramsite, diatomaceous earth, water, expanded perlite and titanium dioxide. The mass fraction ratio of cement, ceramsite, diatomaceous earth, water, expanded perlite and titanium dioxide is 30:25:23:35:12:3.
[0033] The communication divergent coating is composed of zinc acetate, anhydrous ethanol, ammonium phosphate, methanol solution and oxalic acid. The ratio of zinc acetate to anhydrous ethanol is set to 2.19g:100mL), the ratio of ammonium phosphate to methanol solution is set to 0.0025g:20mL, the molar ratio of zinc acetate to ammonium phosphate is 100:0.5, and the ratio of oxalic acid to anhydrous ethanol is set to 2.51g:40mL. The preparation method of the communication divergent coating is:
[0034] S1, dissolving zinc acetate in anhydrous ethanol, and heating and stirring in a water bath, adding a methanol solution containing (NH4)3PO4 to the solution, dissolving oxalic acid in anhydrous ethanol, and then adding the mixture to the above-mentioned mixed solution of zinc acetate and ammonium phosphate, and stirring vigorously;
[0035] S2, transferring the mixed solution to an oven for drying, and grinding the dried solid;
[0036] S3, placing the ground solid into a muffle furnace for calcination to obtain a ZnO product;
[0037] S4. Use the prepared surface photovoltage signal enhanced ZnO to carry out photocatalytic reaction.
[0038] The communication divergent block adopts low-frequency microwave dielectric ceramic material, and the low-frequency microwave dielectric ceramic material adopts BaO-Ln2O3-TiO2 (BLT) series with tungsten bronze structure.
[0039] A method for processing building materials that is beneficial to improving 5G communications, comprising the following steps:
[0040] Step 1: Mix cement, ceramsite, diatomaceous earth, expanded perlite and titanium dioxide in a certain proportion;
[0041] Step 2: fully mix the prepared raw materials in a mixer and add water to the mixture from time to time;
[0042] Step 3, feeding the mixed raw materials into a mold of a molding machine, and pressing the molding machine into cement bricks with filling holes;
[0043] Step 4: embed the communication divergent block into the filling hole, and apply the communication divergent coating to the outer side wall of the cement brickwork;
[0044] Step 5: Place the formed cement bricks in a natural environment for water curing, and then dry and harden them.
[0045] Embodiment 2:
[0046] An embodiment of the present invention provides a building material that is beneficial to improving 5G communications, including cement bricks, a filling hole is provided in the middle of the cement bricks, the outer wall of the cement bricks is coated with communication divergent paint, and the interior of the filling hole is filled with a communication divergent block.
[0047] Cement bricks are composed of cement, ceramsite, diatomaceous earth, water, expanded perlite and titanium dioxide. The mass fraction ratio of cement, ceramsite, diatomaceous earth, water, expanded perlite and titanium dioxide is 30:35:32:60:15:5.
[0048] The communication divergent coating is composed of zinc acetate, anhydrous ethanol, ammonium phosphate, methanol solution and oxalic acid. The ratio of zinc acetate to anhydrous ethanol is set to 2.19g:150mL, the ratio of ammonium phosphate to methanol solution is set to 0.01g:20mL, the molar ratio of zinc acetate to ammonium phosphate is 100:3, and the ratio of oxalic acid to anhydrous ethanol is set to 2.51g:60mL. The preparation method of the communication divergent coating is as follows:
[0049] S1, dissolving zinc acetate in anhydrous ethanol, and heating and stirring in a water bath, adding a methanol solution containing (NH4)3PO4 to the solution, dissolving oxalic acid in anhydrous ethanol, and then adding the mixture to the above-mentioned mixed solution of zinc acetate and ammonium phosphate, and stirring vigorously;
[0050] S2, transferring the mixed solution to an oven for drying, and grinding the dried solid;
[0051] S3, placing the ground solid into a muffle furnace for calcination to obtain a ZnO product;
[0052] S4. Use the prepared surface photovoltage signal enhanced ZnO to carry out photocatalytic reaction.
[0053] The communication divergent block adopts low-frequency microwave dielectric ceramic material, and the low-frequency microwave dielectric ceramic material adopts BaO-Ln2O3-TiO2 (BLT) series with tungsten bronze structure.
[0054] A method for processing building materials that is beneficial to improving 5G communications, comprising the following steps:
[0055] Step 1: Mix cement, ceramsite, diatomaceous earth, expanded perlite and titanium dioxide in a certain proportion;
[0056] Step 2: fully mix the prepared raw materials in a mixer and add water to the mixture from time to time;
[0057] Step 3, feeding the mixed raw materials into a mold of a molding machine, and pressing the molding machine into cement bricks with filling holes;
[0058] Step 4: embed the communication divergent block into the filling hole, and apply the communication divergent coating to the outer side wall of the cement brickwork;
[0059] Step 5: Place the formed cement bricks in a natural environment for water curing, and then dry and harden them.
[0060] Embodiment three:
[0061] An embodiment of the present invention provides a building material that is beneficial to improving 5G communications, including cement bricks, a filling hole is provided in the middle of the cement bricks, the outer wall of the cement bricks is coated with communication divergent paint, and the interior of the filling hole is filled with a communication divergent block.
[0062] Cement bricks are composed of cement, ceramsite, diatomaceous earth, water, expanded perlite and titanium dioxide. The mass fraction ratio of cement, ceramsite, diatomaceous earth, water, expanded perlite and titanium dioxide is 35:30:28:45:14:4.
[0063] The communication divergent coating is composed of zinc acetate, anhydrous ethanol, ammonium phosphate, methanol solution and oxalic acid. The ratio of zinc acetate to anhydrous ethanol is set to 2.19g:150mL, the ratio of ammonium phosphate to methanol solution is set to 0.01g:20mL, the molar ratio of zinc acetate to ammonium phosphate is 100:3, and the ratio of oxalic acid to anhydrous ethanol is set to 2.51g:60mL. The preparation method of the communication divergent coating is as follows:
[0064] S1, dissolving zinc acetate in anhydrous ethanol, and heating and stirring in a water bath, adding a methanol solution containing (NH4)3PO4 to the solution, dissolving oxalic acid in anhydrous ethanol, and then adding the mixture to the above-mentioned mixed solution of zinc acetate and ammonium phosphate, and stirring vigorously;
[0065] S2, transferring the mixed solution to an oven for drying, and grinding the dried solid;
[0066] S3, placing the ground solid into a muffle furnace for calcination to obtain a ZnO product;
[0067] S4. Use the prepared surface photovoltage signal enhanced ZnO to carry out photocatalytic reaction.
[0068] The communication divergent block adopts low-frequency microwave dielectric ceramic material, and the low-frequency microwave dielectric ceramic material adopts BaO-Ln2O3-TiO2 (BLT) series with tungsten bronze structure.
[0069] A method for processing building materials that is beneficial to improving 5G communications, comprising the following steps:
[0070] Step 1: Mix cement, ceramsite, diatomaceous earth, expanded perlite and titanium dioxide in a certain proportion;
[0071] Step 2: fully mix the prepared raw materials in a mixer and add water to the mixture from time to time;
[0072] Step 3, feeding the mixed raw materials into a mold of a molding machine, and pressing the molding machine into cement bricks with filling holes;
[0073] Step 4: embed the communication divergent block into the filling hole, and apply the communication divergent coating to the outer side wall of the cement brickwork;
[0074] Step 5: Place the formed cement bricks in a natural environment for water curing, and then dry and harden them.
[0075] Embodiment 4:
[0076] An embodiment of the present invention provides a building material that is beneficial to improving 5G communications, including cement bricks, a filling hole is provided in the middle of the cement bricks, the outer wall of the cement bricks is coated with communication divergent paint, and the interior of the filling hole is filled with a communication divergent block.
[0077] Cement bricks are composed of cement, ceramsite, diatomaceous earth, water, expanded perlite and titanium dioxide. The mass fraction ratio of cement, ceramsite, diatomaceous earth, water, expanded perlite and titanium dioxide is 30:25:23:35:12:3.
[0078] The communication divergent coating is composed of zinc acetate, anhydrous ethanol, ammonium phosphate, methanol solution and oxalic acid. The ratio of zinc acetate to anhydrous ethanol is set to 2.19g:125mL, the ratio of ammonium phosphate to methanol solution is set to 0.005g:20mL, the molar ratio of zinc acetate to ammonium phosphate is 100:2, and the ratio of oxalic acid to anhydrous ethanol is set to 2.51g:50mL. The preparation method of the communication divergent coating is:
[0079] S1, dissolving zinc acetate in anhydrous ethanol, and heating and stirring in a water bath, adding a methanol solution containing (NH4)3PO4 to the solution, dissolving oxalic acid in anhydrous ethanol, and then adding the mixture to the above-mentioned mixed solution of zinc acetate and ammonium phosphate, and stirring vigorously;
[0080] S2, transferring the mixed solution to an oven for drying, and grinding the dried solid;
[0081] S3, placing the ground solid into a muffle furnace for calcination to obtain a ZnO product;
[0082] S4. Use the prepared surface photovoltage signal enhanced ZnO to carry out photocatalytic reaction.
[0083] The communication divergent block adopts low-frequency microwave dielectric ceramic material, and the low-frequency microwave dielectric ceramic material adopts BaO-Ln2O3-TiO2 (BLT) series with tungsten bronze structure.
[0084] A method for processing building materials that is beneficial to improving 5G communications, comprising the following steps:
[0085] Step 1: Mix cement, ceramsite, diatomaceous earth, expanded perlite and titanium dioxide in a certain proportion;
[0086] Step 2: fully mix the prepared raw materials in a mixer and add water to the mixture from time to time;
[0087] Step 3, feeding the mixed raw materials into a mold of a molding machine, and pressing the molding machine into cement bricks with filling holes;
[0088] Step 4: embed the communication divergent block into the filling hole, and apply the communication divergent coating to the outer side wall of the cement brickwork;
[0089] Step 5: Place the formed cement bricks in a natural environment for water curing, and then dry and harden them.
[0090] Embodiment five:
[0091] An embodiment of the present invention provides a building material that is beneficial to improving 5G communications, including cement bricks, a filling hole is provided in the middle of the cement bricks, the outer wall of the cement bricks is coated with communication divergent paint, and the interior of the filling hole is filled with a communication divergent block.
[0092] Cement bricks are composed of cement, ceramsite, diatomaceous earth, water, expanded perlite and titanium dioxide. The mass fraction ratio of cement, ceramsite, diatomaceous earth, water, expanded perlite and titanium dioxide is 40:35:32:60:15:5.
[0093] The communication divergent coating is composed of zinc acetate, anhydrous ethanol, ammonium phosphate, methanol solution and oxalic acid. The ratio of zinc acetate to anhydrous ethanol is set to 2.19g:125mL, the ratio of ammonium phosphate to methanol solution is set to 0.005g:20mL, the molar ratio of zinc acetate to ammonium phosphate is 100:2, and the ratio of oxalic acid to anhydrous ethanol is set to 2.51g:50mL. The preparation method of the communication divergent coating is:
[0094] S1, dissolving zinc acetate in anhydrous ethanol, and heating and stirring in a water bath, adding a methanol solution containing (NH4)3PO4 to the solution, dissolving oxalic acid in anhydrous ethanol, and then adding the mixture to the above-mentioned mixed solution of zinc acetate and ammonium phosphate, and stirring vigorously;
[0095] S2, transferring the mixed solution to an oven for drying, and grinding the dried solid;
[0096] S3, placing the ground solid into a muffle furnace for calcination to obtain a ZnO product;
[0097] S4. Use the prepared surface photovoltage signal enhanced ZnO to carry out photocatalytic reaction.
[0098] The communication divergent block adopts low-frequency microwave dielectric ceramic material, and the low-frequency microwave dielectric ceramic material adopts BaO-Ln2O3-T iO2 (BLT) series with tungsten bronze structure.
[0099] A method for processing building materials that is beneficial to improving 5G communications, comprising the following steps:
[0100] Step 1: Mix cement, ceramsite, diatomaceous earth, expanded perlite and titanium dioxide in a certain proportion;
[0101] Step 2: fully mix the prepared raw materials in a mixer and add water to the mixture from time to time;
[0102] Step 3, feeding the mixed raw materials into a mold of a molding machine, and pressing the molding machine into cement bricks with filling holes;
[0103] Step 4: embed the communication divergent block into the filling hole, and apply the communication divergent coating to the outer side wall of the cement brickwork;
[0104] Step 5: Place the formed cement bricks in a natural environment for water curing, and then dry and harden them.
[0105] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A building material that is conducive to improving 5G communications, including cement brickwork, characterized in that: A filling hole is arranged in the middle of the cement brick, the outer side wall of the cement brick is coated with a communication diverging paint, and the inside of the filling hole is filled with a communication diverging block.
2. A building material that is beneficial to improving 5G communication according to claim 1, characterized in that: The cement bricks are composed of cement, ceramsite, diatomaceous earth, water, expanded perlite and titanium dioxide.
3. A building material that is beneficial to improving 5G communication according to claim 2, characterized in that: The mass fraction ratio of the cement, ceramsite, diatomaceous earth, water, expanded perlite and titanium dioxide is (30-40): (25-35): (23-32): (35-60): (12-15): (3-5).
4. A building material that is beneficial to improving 5G communication according to claim 1, characterized in that: The communication divergent coating is composed of zinc acetate, anhydrous ethanol, ammonium phosphate, methanol solution and oxalic acid.
5. A building material that is beneficial to improving 5G communication according to claim 4, characterized in that: The ratio of zinc acetate to anhydrous ethanol is set to 2.19 g: (100-150 mL), the ratio of ammonium phosphate to methanol solution is set to (0.0025-0.01 g): 20 mL, the molar ratio of zinc acetate to ammonium phosphate is 100: (0.5-3), and the ratio of oxalic acid to anhydrous ethanol is set to 2.51 g: (40-60 mL).
6. A building material that is beneficial to improving 5G communication according to claim 1, characterized in that: The communication divergence block is made of low-frequency microwave dielectric ceramic material, and the low-frequency microwave dielectric ceramic material is made of BaO-Ln2O3-TiO2 (BLT) series with tungsten bronze structure.
7. A building material that is beneficial to improving 5G communication according to claim 1, characterized in that: The preparation method of the communication divergent coating is: S1, dissolving zinc acetate in anhydrous ethanol, and heating and stirring in a water bath, adding a methanol solution containing (NH4)3PO4 to the solution, dissolving oxalic acid in anhydrous ethanol, and then adding the mixture to the above-mentioned mixed solution of zinc acetate and ammonium phosphate, and stirring vigorously; S2, transferring the mixed solution to an oven for drying, and grinding the dried solid; S3, placing the ground solid into a muffle furnace for calcination to obtain a ZnO product; S4. Use the prepared surface photovoltage signal enhanced ZnO to carry out photocatalytic reaction.
8. A method for processing a building material that is beneficial to improving 5G communication, applied to a building material that is beneficial to improving 5G communication as described in claims 1-7, comprising the following steps: Step 1: Mix cement, ceramsite, diatomaceous earth, expanded perlite and titanium dioxide in a certain proportion; Step 2: fully mix the prepared raw materials in a mixer and add water to the mixture from time to time; Step 3, feeding the mixed raw materials into a mold of a molding machine, and pressing the molding machine into cement bricks with filling holes; Step 4: embed the communication divergent block into the filling hole, and apply the communication divergent coating to the outer side wall of the cement brickwork; Step 5: Place the formed cement bricks in a natural environment for water curing, and then dry and harden them.