Slow tensile corrosion test fixture in liquid medium, test machine and test method
By designing a slow tensile corrosion test fixture including corrosion box, inlet tube, outlet tube and clamping part in the liquid medium, the complex and inconvenient problems of slow tensile corrosion test in liquid medium in the prior art are solved, and the problem of slow tensile corrosion test in liquid medium is realized. Simple structure, easy use and improved experimental practicality.
Patent Information
- Application Number
- CN202410978903.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-22
- Publication Date
- 2024-11-12
AI Technical Summary
The prior art is difficult to effectively carry out slow tensile corrosion tests in liquid media, resulting in complex structure, inconvenient use, and lack of practicality.
A slow tensile corrosion test fixture in liquid medium including corrosion box, liquid inlet tube, liquid outlet tube, first clamp and second clamp are designed, and corrosion-resistant materials and sealing gaskets are used to ensure the safety of the test. and provide corresponding experimental methods.
It realizes a slow tensile corrosion test in liquid media with simple structure and easy to use, improves the practicality and safety of the test, and ensures the stability of the corrosion liquid and the reliability of the test.
Smart Images

Figure CN118937048A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of mechanical property detection, in particular to a slow tensile corrosion test fixture in a liquid medium. Background Art
[0002] Stress corrosion is one of the important factors affecting the life and safe service of mechanical structures, involving multiple engineering fields such as transportation, chemical industry, machinery, and energy.
[0003] Constant (slow) strain tensile is a tensile test method designed to evaluate the stress corrosion sensitivity of materials in specific media with a tensile rate less than a certain critical value. It applies stress to the specimen placed in a corrosive environment at a constant or relatively slow strain rate in order to obtain the stress corrosion characteristics and stress corrosion sensitivity of the material in a specific corrosive environment.
[0004] Therefore, in order to achieve the above goals, it is necessary to develop a slow tensile corrosion test fixture in liquid medium to address the above problems. Summary of the invention
[0005] The purpose of the present invention is to provide a slow tensile corrosion test fixture, a testing machine and an experimental method in a liquid medium to solve the problems existing in the above-mentioned prior art, with simple structure, convenient use and good practicality.
[0006] To achieve the above object, the present invention provides the following solutions:
[0007] The present invention provides a slow tensile corrosion test fixture in a liquid medium, comprising: a corrosion box, a liquid inlet pipe, a liquid outlet pipe, a first clamping piece and a second clamping piece. The corrosion box is a top-opening structure, and the corrosion box is used to place the corrosion liquid; one end of the liquid inlet pipe is connected and communicated with the corrosion box, and the other end is connected and communicated with the liquid outlet of a circulation pump in an external liquid storage tank; one end of the liquid outlet pipe is connected and communicated with the corrosion box, and the other end is connected and communicated with the external liquid storage tank; the top end of the first clamping piece is used for being detachably fixedly connected to the upper clamp of a testing machine, and the other end is used for being detachably fixedly connected to the top end of a tensile specimen; the top end of the first clamping piece passes through the bottom of the corrosion box and is sealed with the corrosion box, the top end of the second clamping piece is used for being detachably fixedly connected to the bottom end of the tensile specimen, and the bottom end of the second clamping piece is used for being detachably fixedly connected to the lower clamp of the testing machine.
[0008] Preferably, the first clamping member includes a first connecting portion and a first specimen fastening device, the first connecting portion is integrally fixedly connected to the first specimen fastening device, the first connecting portion is used to be detachably fixedly connected to the upper chuck of the testing machine, the first specimen fastening device is provided with a first internal threaded hole, the top of the tensile specimen is provided with a first external thread, and the first external thread is used to be threadedly connected to the first internal threaded hole.
[0009] Preferably, the second clamping member includes a second connecting portion, a second sample fastening device, a fixing nut and a support, the second connecting portion is integrally fixedly connected to the second sample fastening device, the second connecting portion is used to be detachably fixedly connected to the lower chuck of the testing machine, a second threaded hole is provided at the top of the second sample fastening device, a second external thread is provided at the bottom of the tensile test, the second external thread is used to be threadedly connected to the second threaded hole, the support is vertically fixedly connected to the connection between the second connecting portion and the second sample fastening device, the support is used to contact the bottom of the corrosion box and support the corrosion box, the outer side wall of the second sample fastening device is provided with a third external thread, the bottom of the top view box is provided with a through hole, the second sample fastening device is used to pass through the through hole and be threadedly connected to the fixing nut, and tightening the fixing nut can enable the second sample fastening device to seal the through hole.
[0010] Preferably, it also includes an upper sealing gasket and a lower sealing gasket, the upper sealing gasket is sleeved on the outside of the second sample fixing device and is located between the fixing nut and the corrosion box, and the lower sealing gasket is sleeved on the outside of the second sample fixing device and is located between the support and the corrosion box.
[0011] Preferably, the upper sealing gasket and the lower sealing gasket are both made of rubber material.
[0012] Preferably, the connection position between the liquid outlet pipe and the corrosion box is located at the designed liquid level position of the corrosion box so that the corrosion liquid in the corrosion box is maintained at the designed liquid level position.
[0013] Preferably, the first clamping piece is integrally processed from corrosion-resistant stainless steel, and the surface of the first clamping piece is coated with a corrosion-resistant coating, the second clamping piece is integrally processed from corrosion-resistant stainless steel, and the surface of the second clamping piece is coated with a corrosion-resistant coating, and the corrosion box is integrally processed from corrosion-resistant stainless steel, and the surface of the corrosion box is coated with a corrosion-resistant coating.
[0014] The present invention also provides a slow tensile corrosion testing machine, comprising the slow tensile corrosion testing fixture in liquid medium as described in any one of the above items.
[0015] The present invention also provides a method for performing a slow tensile corrosion test using the tensile corrosion testing machine as described above, comprising the following steps:
[0016] The bottom of the second clamping piece which is sealed and connected to the corrosion box is clamped on the lower clamp of the testing machine, and the two ends of the tensile specimen are respectively connected to the first clamping piece and the second clamping piece, and then the crossbeam of the testing machine is moved to a suitable position so that the upper clamp of the testing machine clamps the first clamping piece, and the corrosion liquid is transported into the corrosion box from the liquid inlet pipe. After the corrosion liquid meets the experimental requirements in the corrosion box, the tensile program in the computer of the testing machine is started, and the constant strain tensile test parameters are set, and then the test can be started.
[0017] Compared with the prior art, the present invention has achieved the following technical effects:
[0018] The invention provides a slow tensile corrosion test fixture in a liquid medium, a testing machine and an experimental method. The bottom of a second clamping piece sealed with the corrosion box is clamped on a lower clamp of the testing machine, and the two ends of the tensile specimen are respectively connected to the first clamping piece and the second clamping piece. Then, the crossbeam of the testing machine is moved to a suitable position, so that the upper clamp of the testing machine clamps the first clamping piece, and the corrosion liquid is transported into the corrosion box from a liquid inlet pipe. After the corrosion liquid meets the experimental requirements in the corrosion box, the tensile program in the computer of the testing machine is started, and the constant strain tensile test parameters are set, and then the test can be started. The structure is simple and easy to use. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0020] Figure 1 A schematic diagram of the structure of a slow tensile corrosion test fixture in a liquid medium provided by the present invention;
[0021] Figure 2 A side view of a slow tensile corrosion test fixture in a liquid medium provided by the present invention;
[0022] Figure 3 A schematic diagram of the structure of a second sample fastening device and a support platform in a slow tensile corrosion test fixture in a liquid medium provided by the present invention;
[0023] Figure 4 This is a schematic diagram of the structure of the slow tensile corrosion test fixture in liquid medium provided by the present invention when in use;
[0024] In the figure: 1. first clamping member; 2. first sample fastening device; 3. first threaded hole; 4. liquid outlet pipe; 5. fixing nut; 6. upper sealing gasket; 7. lower sealing gasket; 8. support platform; 9. second sample fastening device; 10. second clamping member; 11. liquid inlet pipe; 12. corrosion box; 13. liquid level; 14. third external thread; 15. second threaded hole; 16. tensile specimen; 17. upper chuck; 18. lower chuck. DETAILED DESCRIPTION
[0025] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0026] The purpose of the present invention is to provide a slow tensile corrosion test fixture, a testing machine and an experimental method in a liquid medium to solve the problems existing in the above-mentioned prior art, with simple structure, convenient use and good practicality.
[0027] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the present invention is further described in detail below with reference to the accompanying drawings and specific embodiments.
[0028] The present invention provides a slow tensile corrosion test fixture in a liquid medium, such as Figures 1 to 4As shown, it includes: a corrosion box 12, a liquid inlet pipe 11, a liquid outlet pipe 4, a first clamping member 1 and a second clamping member 10. The corrosion box 12 is a top-opening structure, and the corrosion box 12 is used to place the corrosion liquid; one end of the liquid inlet pipe 11 is connected and communicated with the corrosion box 12, and the other end is connected and communicated with the liquid outlet of the circulation pump in the external liquid storage tank; one end of the liquid outlet pipe 4 is connected and communicated with the corrosion box 12, and the other end is connected and communicated with the external liquid storage tank; the top end of the first clamping member 1 is used to be detachably fixedly connected to the upper clamp 17 of the testing machine, and the other end is used to be detachably fixedly connected to the top end of the tensile specimen 16; the top end of the first clamping member 1 passes through the bottom of the corrosion box 12 and is sealed with the corrosion box 12, and the top of the second clamping member 10 The first end is used for being detachably fixedly connected to the bottom end of the tensile specimen 16, and the bottom end of the second clamping member 10 is used for being detachably fixedly connected to the lower chuck 18 of the testing machine. The bottom of the second clamping member 10 which is sealed with the corrosion box 12 is clamped on the lower chuck 18 of the testing machine, and the two ends of the tensile specimen 16 are respectively connected to the first clamping member 1 and the second clamping member 10. Then, the crossbeam of the testing machine is moved to a suitable position so that the upper chuck 17 of the testing machine clamps the first clamping member 1, and the corrosive liquid is transported from the liquid inlet pipe 11 to the corrosion box 12. After the corrosive liquid meets the experimental requirements in the corrosion box 12, the tensile program in the computer of the testing machine is started, and the constant strain tensile test parameters are set before the test can be started. The structure is simple and easy to use.
[0029] In a preferred solution of the present embodiment, the first clamping member 1 includes a first connecting portion and a first sample fastening device 2, the first connecting portion is integrally fixedly connected to the first sample fastening device 2, the first connecting portion is used to be detachably fixedly connected to the upper clamp 17 of the testing machine, the first sample fastening device 2 is provided with a first internal threaded hole, the top of the tensile specimen 16 is provided with a first external thread, the first external thread is used to be threadedly connected to the first internal threaded hole, the structure is simple, and it is easy to use, and it is convenient to disassemble and connect with the tensile specimen 16.
[0030] In a preferred solution of the present embodiment, the second clamping member 10 comprises a second connecting portion, a second sample fastening device 9, a fixing nut 5 and a support platform 8. The second connecting portion is integrally fixedly connected with the second sample fastening device 9. The second connecting portion is used to be detachably fixedly connected with the lower clamp 18 of the testing machine. A second threaded hole 15 is provided on the top of the second sample fastening device 9. A second external thread is provided on the bottom of the tensile tester. The second external thread is used to be threadedly connected to the second threaded hole 15. The support platform 8 is vertically fixedly connected to the connection between the second connecting portion and the second sample fastening device 9. The table 8 is used to contact with the bottom of the corrosion box 12 and can support the corrosion box 12. The outer wall of the second sample fastening device 9 is provided with a third external thread 14. The bottom of the top view box is provided with a through hole. The second sample fastening device 9 is used to pass through the through hole and be threadedly connected with the fixing nut 5. Tightening the fixing nut 5 can make the second sample fastening device 9 seal the through hole. It has a simple structure and is easy to use. It is convenient to support the corrosion box 12 while being convenient to disassemble and connect with the tensile sample 16. The tensile sample 16 can be placed in the corrosion liquid in the corrosion box 12 and can be stretched.
[0031] In a preferred solution of the present embodiment, the slow tensile corrosion test fixture in liquid medium also includes an upper sealing gasket 6 and a lower sealing gasket 7. The upper sealing gasket 6 is sleeved on the outside of the second sample fixing device and is located between the fixing nut 5 and the corrosion box 12. The lower sealing gasket 7 is sleeved on the outside of the second sample fixing device and is located between the support 8 and the corrosion box 12. It has a simple structure and can effectively seal the connection between the second sample fastening device 9 and the corrosion box 12.
[0032] In a preferred solution of this embodiment, the upper sealing gasket 6 and the lower sealing gasket 7 are both made of rubber material, which effectively prevents the leakage of corrosive liquid media.
[0033] In a preferred scheme of the present embodiment, the connection position between the liquid outlet pipe 4 and the corrosion box 12 is located at the designed liquid level 13 position of the corrosion box 12 so that the corrosive liquid in the corrosion box 12 is maintained at the designed liquid level 13 position. The corrosion box 12 is provided with a liquid inlet pipe 11 at the bottom and a liquid outlet pipe 4 at the top. The liquid inlet pipe 11 is connected to the liquid outlet of the circulation pump installed in the external liquid storage tank. The liquid outlet pipe 4 is connected to the external liquid storage tank with a plastic pipe to ensure that the solution in the corrosion box 12 is replaced at least once per minute to keep the concentration of the corrosive liquid in the corrosion box 12 stable.
[0034] In a preferred scheme of the present embodiment, the first clamping member 1 is integrally processed with corrosion-resistant stainless steel, and the surface of the first clamping member 1 is coated with a corrosion-resistant coating, the second clamping member 10 is integrally processed with corrosion-resistant stainless steel, and the surface of the second clamping member 10 is coated with a corrosion-resistant coating, the corrosion box 12 is integrally processed with corrosion-resistant stainless steel, and the surface of the corrosion box 12 is coated with a corrosion-resistant coating, the structure is simple, and the corrosive liquid can be effectively prevented from corroding the device, thereby ensuring the durability of the device.
[0035] Embodiment 2
[0036] This embodiment also provides a slow tensile corrosion testing machine, including the slow tensile corrosion testing fixture in liquid medium as in the first embodiment.
[0037] This embodiment also provides a method for performing a slow tensile corrosion test using the tensile corrosion testing machine of the second embodiment, comprising the following steps:
[0038] Clamp the second clamping part 10 of the second sample fastening device 9 which is fastened to the corrosion box 12 onto the lower chuck 18 of the testing machine, and then screw the tensile specimen 16 which is respectively provided with the first external thread and the second external thread at both ends into the second threaded hole 15 and the first threaded hole 3 respectively, and fasten them, and then move the crossbeam of the testing machine to a suitable position so that the upper chuck 17 of the testing machine clamps the first clamping part 1, prepare the corrosion liquid, load it into the external liquid storage tank, heat it to the required temperature, start the circulation pump, make the corrosion box 12 reach the height of the liquid level 13, start the tensile program in the computer, set the constant (slow) strain tensile test parameters, and then start the test.
[0039] The present invention uses specific examples to illustrate the principles and implementation methods of the present invention. The above examples are only used to help understand the method and core ideas of the present invention. At the same time, for those skilled in the art, according to the ideas of the present invention, there will be changes in the specific implementation methods and application scope. In summary, the content of this specification should not be understood as limiting the present invention.
Claims
1. A slow tensile corrosion test fixture in a liquid medium, characterized by: include: A corrosion box, wherein the corrosion box has an open top structure and is used to place the corrosion liquid; A liquid inlet pipe, one end of which is connected and communicated with the corrosion box, and the other end of which is connected and communicated with the liquid outlet of the circulation pump in the external liquid storage tank; A liquid outlet pipe, one end of which is connected to and communicated with the corrosion tank, and the other end of which is connected to and communicated with the external liquid storage tank; a first clamping member, wherein the top end of the first clamping member is used to be detachably fixedly connected to the upper clamp of the testing machine, and the other end of the first clamping member is used to be detachably fixedly connected to the top end of the tensile specimen; and A second clamping member, the top end of the first clamping member passes through the bottom of the corrosion box and is sealed and connected to the corrosion box, the top end of the second clamping member is used to be detachably fixedly connected to the bottom end of the tensile specimen, and the bottom end of the second clamping member is used to be detachably fixedly connected to the lower clamp of the testing machine.
2. The slow tensile corrosion test fixture in liquid medium according to claim 1, characterized in that: The first clamping member includes a first connecting portion and a first sample fastening device, the first connecting portion is integrally fixedly connected to the first sample fastening device, the first connecting portion is used to be detachably fixedly connected to the upper clamp of the testing machine, the first sample fastening device is provided with a first internal threaded hole, the top of the tensile specimen is provided with a first external thread, and the first external thread is used to be threadedly connected to the first internal threaded hole.
3. The slow tensile corrosion test fixture in liquid medium according to claim 1, characterized in that: The second clamping member includes a second connecting portion, a second sample fastening device, a fixing nut and a support. The second connecting portion is integrally fixedly connected to the second sample fastening device. The second connecting portion is used to be detachably fixedly connected to the lower chuck of the testing machine. A second threaded hole is provided at the top of the second sample fastening device. A second external thread is provided at the bottom of the tensile test. The second external thread is used to be threadedly connected to the second threaded hole. The support is vertically fixedly connected to the connection between the second connecting portion and the second sample fastening device. The support is used to contact the bottom of the corrosion box and support the corrosion box. A third external thread is provided on the outer side wall of the second sample fastening device. A through hole is provided at the bottom of the top-view box. The second sample fastening device is used to pass through the through hole and be threadedly connected to the fixing nut. Tightening the fixing nut can enable the second sample fastening device to seal the through hole.
4. The slow tensile corrosion test fixture in liquid medium according to claim 3, characterized in that: It also includes an upper sealing gasket and a lower sealing gasket. The upper sealing gasket is sleeved on the outside of the second sample fixing device and is located between the fixing nut and the corrosion box. The lower sealing gasket is sleeved on the outside of the second sample fixing device and is located between the support platform and the corrosion box.
5. The slow tensile corrosion test fixture in liquid medium according to claim 4, characterized in that: The upper sealing gasket and the lower sealing gasket are both made of rubber material.
6. The slow tensile corrosion test fixture in liquid medium according to claim 5, characterized in that: The connection position between the liquid outlet pipe and the corrosion box is located at the designed liquid level position of the corrosion box so that the corrosion liquid in the corrosion box is maintained at the designed liquid level position.
7. The slow tensile corrosion test fixture in liquid medium according to claim 6, characterized in that: The first clamping piece is integrally processed from corrosion-resistant stainless steel, and the surface of the first clamping piece is coated with a corrosion-resistant coating. The second clamping piece is integrally processed from corrosion-resistant stainless steel, and the surface of the second clamping piece is coated with a corrosion-resistant coating. The corrosion box is integrally processed from corrosion-resistant stainless steel, and the surface of the corrosion box is coated with a corrosion-resistant coating.
8. A slow tensile corrosion testing machine, characterized in that: It comprises the slow tensile corrosion test fixture in liquid medium as described in any one of claims 1 to 7.
9. A method for performing a slow tensile corrosion test using the tensile corrosion testing machine as claimed in claim 8, characterized in that: The following steps are involved: The bottom of the second clamping piece which is sealed and connected to the corrosion box is clamped on the lower clamp of the testing machine, and the two ends of the tensile specimen are respectively connected to the first clamping piece and the second clamping piece, and then the crossbeam of the testing machine is moved to a suitable position so that the upper clamp of the testing machine clamps the first clamping piece, and the corrosion liquid is transported into the corrosion box from the liquid inlet pipe. After the corrosion liquid meets the experimental requirements in the corrosion box, the tensile program in the computer of the testing machine is started, and the constant strain tensile test parameters are set, and then the test can be started.
Citation Information
Cited By
Device and method for testing stress corrosion sensitivity of material
CN121298394A
Apparatus and method for testing stress corrosion susceptibility of materials
CN121298394B