Semiconductor device and manufacturing method thereof

By grinding the substrate crystal rod into a rod-shaped body and lithography and electroplating, multiple chips are formed, which solves the packaging complexity and heat dissipation problems in multi-chip cooperation, and achieves efficient integration and precision control, reducing production difficulty and cost. .

CN118943080APending Publication Date: 2024-11-12SHANGHAI WONSUNG ALLOY MATERIAL CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411001066.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-25
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

The existing technology faces packaging complexity and heat dissipation problems in multi-chip collaboration, resulting in large space occupancy and high production process difficulty.

Method used

The substrate crystal rod is grinded into a rod-shaped body, lithography and electroplating are performed to form multiple chips, and the processing accuracy is improved through the self-tension support frame and position adjustment mechanism, reducing diffraction phenomena, and achieving efficient integration of the chip.

Benefits of technology

It solves the problem of multi-chip heat dissipation, reduces the cost of coating and the equipment's dependence on thermal expansion and contraction, improves the coating and grinding accuracy, simplifies the control system, and reduces manufacturing and maintenance costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118943080A_ABST
    Figure CN118943080A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of semiconductors, and particularly relates to a manufacturing method of a semiconductor device and the semiconductor device. The method comprises the steps that a substrate crystal bar is provided, the substrate crystal bar is ground to obtain a rod-shaped body, the rod-shaped body is provided with a cross section in a preset shape, and impurities on the surface of the rod-shaped body are removed; photoetching the circumferential surface of the rod-shaped body, and plating a functional film layer; performing electroplating treatment at a preset position of the functional film layer, forming an electroplating electrode on the surface of the semiconductor functional film layer, and performing electroplating at a preset position of the rod-shaped body to form a conductive circuit, thereby forming a plurality of chips on the circumferential surface of the rod-shaped body; residual impurities and photoresist on the surface of the rod-shaped body are stripped; testing the plurality of chips formed on the rod-shaped body; and electrically connecting the chips with the circuit board to obtain the semiconductor device with a plurality of chips formed on the circumferential surface. According to the application, the plurality of chips are formed on the circumferential surface of the rod-shaped body, and heat is dissipated to the periphery when the chips work, so that the problem of heat dissipation of the plurality of chips can be solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of chip manufacturing technology, and in particular to a semiconductor device and a method for manufacturing the same. Background Art

[0002] With the rapid development of technology, multi-chip collaboration is often required to achieve more advanced functions or larger-scale processing capabilities. The following are some common devices and applications that require multi-chip collaboration. For example, supercomputers are usually composed of thousands or even millions of processor chips for large-scale parallel computing tasks at the same time. Data center servers require multiple processor chips to support high-performance and high-capacity data processing and storage. Artificial intelligence and machine learning systems often require multiple chips for parallel computing and model training to provide faster and more accurate results. Network switches and routers require multiple chips to handle network data traffic, routing forwarding, and security functions. Automotive electronic systems: Electronic systems in modern cars require multiple chips to support vehicle control, safety features, entertainment systems, etc.

[0003] Currently, for devices that require multiple chips, a single chip is often packaged first and then integrated onto a circuit board. The circuit becomes complicated, which takes up a larger plane space. Alternatively, multiple chips are packaged in a stacked manner, but heat dissipation is also a problem that needs to be faced. This poses a higher challenge to the multi-chip manufacturing process. Summary of the invention

[0004] In order to solve the above problems, the present application provides a method for manufacturing a semiconductor device.

[0005] The present application provides a method for manufacturing a semiconductor device using the following technical solution: Grinding: providing a substrate crystal rod, grinding the circumferential surface of the substrate crystal rod to obtain a rod-shaped body, wherein the rod-shaped body has a cross-section of a predetermined shape, and the surface of the rod-shaped body after grinding is a smooth surface; Cleaning: removing impurities on the surface of the rod-shaped body; Coating: photolithography the circumferential surface of the rod-shaped body, and coating a functional film layer; Electroplating: performing electroplating at a preset position of the functional film layer, forming an electroplating electrode on the surface of the semiconductor functional film layer, and electroplating a conductive circuit at a preset position of the rod-shaped body, thereby obtaining a rod-shaped body with multiple chips formed on the circumferential surface; Surface treatment: stripping off the impurities and photoresist remaining on the surface of the rod; Testing: testing the plurality of chips formed on the rod-shaped body; and Welding: providing a circuit board, electrically connecting the chip to the circuit board, and obtaining a semiconductor device with multiple chips distributed in the circumferential direction.

[0006] In one embodiment, the cross-section of the predetermined shape is semicircular, circular, square, quasi-circular or quasi-square.

[0007] In one of the embodiments, after the grinding step, a self-tensioning support frame is provided, wherein the self-tensioning support frame includes a base and support heads located at opposite ends of the base, the substrate crystal rod is fixed to the self-tensioning support frame, and the opposite ends of the substrate crystal rod are respectively clamped on the two support heads.

[0008] By adopting the above solution, the self-tensioning support frame can keep the substrate crystal rod in a straightened state all the time, avoiding the problem of reduced processing accuracy caused by stress concentration.

[0009] In one embodiment, providing the carrier also includes providing a position adjustment mechanism, wherein the position adjustment mechanism is configured to drive the self-tensioning support frame to move parallely and rotate.

[0010] In one of the embodiments, in the coating step, the provided lithography equipment includes a laser, a mask and a projection lens group, the mask is arranged between the laser and the projection lens group, the projection lens group includes at least 3 concave mirrors, and the diameters of the 3 concave mirrors decrease successively on the light output path of the laser.

[0011] By adopting the above solution, the diffraction phenomenon generated during the photolithography process can be reduced and the processing accuracy can be improved.

[0012] In one embodiment, the functional film layer is used to form any one or a combination of multiple of an LED light-emitting chip, a storage chip, a sensor chip or a control chip.

[0013] In one embodiment, the circumferential surface of the rod-shaped body is defined as a first region and a second region, and the first region and the second region are used to form a face-up chip and a flip-chip, respectively.

[0014] In one embodiment, the diameter of the substrate crystal rod is 0.1 mm-300 mm.

[0015] In summary, the present application includes at least one of the following beneficial technical effects: 1. The present application forms multiple chips on the circumferential surface of the rod-shaped body through a chip manufacturing process. When the chips are working, the heat is dissipated to the surroundings. Compared with the semiconductor device formed by stacking multiple chips in the prior art, the solution of the present application is more conducive to solving the problem of heat dissipation of multiple chips; 2. The substrate for manufacturing the chip structure in this application is a substrate crystal rod. Since the diameter is much smaller than that of a conventional wafer, a small vacuum space is required during coating, which facilitates achieving a vacuum degree in a smaller space and reduces the coating cost; 3. The substrate for manufacturing the chip structure of the present application is a rod-shaped body formed by grinding a substrate crystal rod. Compared with the wafer sheet in the prior art, the rod-shaped body is less dependent on the thermal expansion and contraction of the equipment; 4. The substrate for manufacturing the chip structure in this application is a substrate crystal rod. Compared with the wafer in the prior art, the curved surface is easier to meet the grinding accuracy requirements; or in other words, for the curved surface, the accuracy will only affect part of the chip; 5. The substrate for manufacturing the chip structure in the present application is a substrate crystal rod. When moving, only two dimensions, namely the rotation and axial movement of the substrate crystal rod, need to be controlled. Compared with the related technology of using wafers to manufacture chips, which requires control of three dimensions, the coating accuracy and grinding accuracy of the present application are easier to control. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 is a flow chart of a method for manufacturing a semiconductor device according to Embodiment 1 of the present application; Figure 2 is a structural diagram of a grinding device provided in an embodiment of the present application; Figure 3 yes Figure 1 A structural diagram of a self-tensioning support frame used in the semiconductor device manufacturing method provided; Figure 4 yes Figure 1 A schematic diagram of a photolithography method for manufacturing a semiconductor device is provided; Figure 5 is to use Figure 1 A structural diagram of a semiconductor device formed by the provided semiconductor device manufacturing method; Figure 6 (A)-6(D) is adopted Figure 1 A schematic structural diagram of a semiconductor device formed by a semiconductor device manufacturing method is provided.

[0017] Description of reference numerals: 1. Rod-shaped body; 2. First chip; 3. Second chip; 4. Circuit board; 5. Self-tensioning support frame; 50. Base; 52. Support head; 6. Photolithography equipment; 60. Laser; 64. Projection lens group; 62. Mask; 40. Gold wire; 7. Workbench; 8. Grinding head; 9. Ultrasonic probe; 10. Microfluidic channel; 11. Phase change material. DETAILED DESCRIPTION

[0018] The following is combined with Figure 1-6 This application is described in further detail.

[0019] The embodiments of the present application disclose a method for manufacturing a semiconductor device and a semiconductor device manufactured by the method.

[0020] See also Figure 1, the method for manufacturing a semiconductor device provided in the present application includes: S1. Polishing and grinding: provide a substrate crystal rod, and polish and grind the substrate crystal rod to obtain a rod-shaped body 1. The rod-shaped body 1 has a cross-section of a predetermined shape, and the surface of the rod-shaped body 1 after grinding is a smooth surface, and the grinding flatness difference at each position is less than or equal to 3nm; the diameter of the rod-shaped body 1 finally obtained is 0.1mm-300mm, preferably 10-60mm. Compared with the large-diameter layer structure required for manufacturing wafers, rods with smaller diameters are less likely to break and are easier to produce, reducing the difficulty of production. In this embodiment, the substrate crystal rod provided is any one of a silicon-based crystal rod, a gallium arsenide crystal rod, or a sapphire crystal rod.

[0021] In this application, please refer to Figure 2 The grinding device includes a workbench 7, and a plurality of grinding heads 8 fixed to the workbench 7, and the plurality of grinding heads are distributed along the same circumference. The grinding heads 8 are telescopically adjustable to adapt to the grinding of substrate crystal rods of different diameters. In a possible embodiment, the grinding heads 8 can also be evenly distributed on the same circumference. The grinding heads 8 are evenly distributed on the circumference, which can provide more consistent grinding pressure and speed, avoid local over-grinding or under-grinding, and improve the grinding quality; in addition, the plurality of grinding heads can more evenly distribute the heat generated during the grinding process, which helps to prevent local overheating and protect the crystal rod material. In the present application, an ultrasonic probe 9 is also provided on the workbench 7, and the ultrasonic probe 9 can measure the grinding accuracy of the substrate crystal rod. The substrate crystal rod can rotate around the axis so that the ultrasonic probe 9 can detect the grinding accuracy in real time. In actual grinding, the telescopic mechanism of the grinding head 8 and the measurement data of the ultrasonic probe 9 are integrated into a closed-loop control system. During the grinding process, the ultrasonic probe 9 measures the grinding accuracy of the substrate crystal rod in real time and feeds the data back to the control system. The control system automatically adjusts the pressure, speed and telescopic position of the grinding head according to the measurement results of the ultrasonic probe to achieve the best grinding effect. The telescopic mechanism of the grinding head is designed to ensure that it can move accurately according to the instructions of the control system to achieve micron-level or even nano-level adjustments.

[0022] In order to meet the needs of grinding substrate crystal rods with different cross-sectional shapes, the shape of the grinding head 8 can be adjusted according to actual needs.

[0023] In this embodiment, the provided substrate crystal rod is made of semiconductor material, and before coating, ion implantation is performed on a preset position of the substrate crystal rod.

[0024] Please also read Figure 6(A)-6 (D), in this embodiment, the cross-section of the rod-shaped body 1 obtained after grinding the substrate crystal rod provided can be semicircular, circular, square, quasi-circular or quasi-square. The cross-sectional shape of the rod-shaped body 1 can be selected according to the actual scenario to achieve the maximum full utilization of the substrate crystal rod. For example, in Figure 6 In (A), the cross-sectional shape of the rod-shaped body 1 is circular; Figure 6 In (B), the cross-section of the rod is quasi-circular; Figure 6 In (C), the cross-sectional shape of the rod-shaped body 1 is a square; Figure 6 In (D), the cross-sectional shape of the rod-shaped body 1 is a square.

[0025] See also Figure 3 In this embodiment, after step S1, a self-tensioning support frame 5 is further provided, wherein the self-tensioning support frame 5 includes a base 50 and support heads 52 located at opposite ends of the base 50, and the substrate crystal rod is fixed to the self-tensioning support frame 5, and the opposite ends of the substrate crystal rod are respectively clamped on the two support heads 52. The substrate crystal rod is fixed by the self-tensioning support frame 5, and the substrate crystal rod can rotate relative to the self-tensioning support frame 5, so that the substrate crystal rod can be processed by a chip process. The self-tensioning support frame 5 can always keep the substrate crystal rod in a straightened state.

[0026] When providing the self-tensioning support frame 5, a position adjustment mechanism (not shown) is also provided, and the position adjustment mechanism is configured to drive the self-tensioning support frame 5 to move in parallel and rotate. In each link of lithography, coating, and electroplating, it is necessary to use a position adjustment mechanism to rotate and translate the substrate crystal rod. Compared with related technologies, traditional three-dimensional position adjustment mechanisms need to control multiple axes at the same time, which requires the control system to be able to accurately synchronize and coordinate the actions of multiple motion axes. To achieve lithography, the position adjustment mechanism needs to move in three-dimensional space and needs to control the movement of three dimensions of XYZ; the technical solution of the present application only requires two dimensions, one is the translation dimension, and the other is the rotation dimension. The control dimension is one less, and the difficulty will be reduced by one level. This simplification not only makes the control algorithm more intuitive and easy to implement, but also reduces the complexity of the electronic and mechanical systems, thereby reducing the manufacturing cost and maintenance cost of the overall system.

[0027] Semiconductor wafers are typically available in standard wafer sizes and / or thicknesses. For example, a standard wafer diameter may be 2 inches (50 mm), 4 inches (100 mm), or 6 inches (150 mm). For silicon carbide wafers, the standard wafer thickness may be, for example, at least 0.1% or at least 0.15% of the standard wafer diameter (e.g., 350 μm for a 6-inch wafer).

[0028] In the related art, when using wafers to manufacture chips, due to the small thickness of the wafers, the difference in grinding flatness at each position of the entire wafer needs to be less than 3nm. The control of grinding accuracy directly determines the quality of the chip, which makes the process of semiconductor wafers more complicated and affects the yield. In this embodiment, since a rod-shaped wafer is used to make chips, the shape of the required grinding head can be an arc-shaped or semicircular grinding head that matches the size of the rod-shaped body 1. The arc-shaped or semicircular grinding head can completely wrap the outer circumferential surface of the rod-shaped body 1 for grinding, and can grind vertically, and the grinding accuracy can be more clearly judged from the imaging mechanism, thereby achieving higher accuracy.

[0029] S2, cleaning, removing impurities on the surface of the rod; S3, coating, photolithography and coating of functional film on the circumferential surface of the rod-shaped body; the coating method includes chemical vapor deposition and / or physical vapor deposition, please refer to Figure 4 In this embodiment, the photolithography device 6 includes a laser 60, a mask 62 and a projection lens group 64. The mask 62 is arranged between the laser 60 and the projection lens group 64. In this embodiment, the projection lens group 64 includes at least three concave reflectors. In this embodiment, the schematic projection lens group 64 includes a first, a second and a third concave reflector in sequence along the light-emitting optical path. The diameters of the three concave reflectors are successively reduced on the light-emitting optical path of the laser 60. The first concave reflector among the three concave reflectors converges the light beam emitted by the laser 60, and then the second concave reflector and the third concave reflector gradually converge the light beam further, and finally form a focusing point on the rod-shaped body 1 to process the rod-shaped body 1. The material of the concave reflector is a silicon-molybdenum concave mirror.

[0030] The use of a concave reflector can effectively reduce diffraction when processing the rod-shaped body 1, and can improve the accuracy of photolithography. Because the rod-shaped body 1 is preferably a convex surface or a convex curved surface, the convex surface or the convex curved surface is less likely to diffract than a flat wafer. This is because on a convex or curved surface, the propagation path of light is more complicated than on a flat surface, and there are usually more reflections and refractions. These processes make the phase distribution of light more complicated and weaken the effect of diffraction. In addition, for curved surfaces, the incident angle of the incident light will change with the change of position, which will cause the light at different positions to experience different optical path differences, thereby reducing the impact of the diffraction effect. Therefore, compared with a flat surface, the diffraction effect on a convex or curved surface is usually smaller. During photolithography, diffraction will cause blurring and distortion of the pattern, limiting the resolution of the photolithography, so diffraction should be avoided during photolithography.

[0031] The light beam emitted by the laser 60 passes through the projection lens group 64, and the lens further focuses and reduces the pattern on the light to form extreme ultraviolet light. The extreme ultraviolet light is irradiated onto the rod-shaped body 1, that is, the light passing through the projection lens group 64 exposes the pattern on the mask 62 to the rod-shaped body, and finally forms a corresponding pattern on the rod-shaped body.

[0032] The functional film layer is used to form any one or a combination of LED light-emitting chips, storage chips, sensor chips or control chips. In other words, the material or method or number of layers required for coating can be selected according to the type of chip to be formed.

[0033] S4, electroplating, performing electroplating treatment at the preset position of the functional film layer, forming an electrode layer and a conductive circuit at the preset position of the rod-shaped body 1, so that each chip can establish a communication connection with the outside world.

[0034] See also Figure 5 and Figure 6 (A)-6 (D), the semiconductor device obtained by the scheme of the present application, the circumferential surface of the rod-shaped body can form an array chip, in this embodiment, the chip includes a first chip 2 and a second chip 3, the first chip 2 can be soldered to the circuit board 4 by flip-chip, and the second chip 3 can be mounted on the circuit board 4 by gold wire 40. Since the positive projection of the first chip 2 and the positive projection of the second chip 3 fall on the same surface, the surface area occupied by the circuit board 4 can be reduced, the integration of the chip can be improved, and the gold wire 40 can be used as a heat dissipation channel for the second chip 3. Of course, it can be understood that the first chip 2 or the second chip 3 can also be connected in series or in parallel through electroplated conductive lines or gold wires.

[0035] S5, surface treatment, stripping the impurities and photoresist remaining on the surface of the rod-shaped body 1; S6, testing, testing the multiple chips formed on the rod-shaped body 1 to determine the yield of each chip; S7, welding, please refer to Figure 6 (A)-6 (D), provide a circuit board 4, flip-chip solder the first chip 2 to the circuit board 4, and mount the second chip 3 on the circuit board 4 through a gold wire, so as to obtain a semiconductor device having a plurality of first chips 2 and second chips 3 formed on the circumferential surface. This semiconductor device realizes a high degree of integration of multiple chips. Later, the substrate crystal rod can also be cut to obtain a desired length or number of chips.

[0036] Specifically, in a specific embodiment, the substrate crystal rod is made of sapphire. The diameter of the substrate crystal rod is 10 mm. Within this diameter range, firstly, the processing yield requirement is met, and secondly, the space requirement for chip manufacturing can be further reduced on the basis of meeting the processing yield, for example, the size of the vacuum space can be reduced.

[0037] In this embodiment, the cleaning method may be reagent cleaning or ultrasonic cleaning, etc. In this embodiment, for example, a metal-organic chemical vapor deposition device MOCVD may be used to perform surface cleaning on a sapphire substrate under high temperature conditions, and the chamber temperature may be optionally raised to 1050° C. in a hydrogen atmosphere and maintained at that temperature for 10 minutes, to finally obtain a semiconductor device.

[0038] The present application also relates to a semiconductor device, which includes a circuit board 4 and a rod-shaped body 1. A plurality of chips are formed on the surface of the rod-shaped body 1, and the chips include a first chip 2 and a second chip 3, and the orthographic projection of the first chip 2 can fall on the same surface as the orthographic projection of the second chip 3; and / or the first chip 2 and the second chip 3 are arranged in an array respectively; the first chip 2 is flip-chip soldered to the circuit board 4, and the second chip 3 is mounted on the circuit board 4 through a gold wire 40.

[0039] The first chip 2 and the second chip 3 are of different types. The first chip 2 includes a clock distributor, a power management chip and a radio frequency distributor, and the second chip 3 includes a data processing chip and a storage chip. By using a film forming process, a plurality of chips are formed on the surface of the rod-shaped body 1, and the chips are directly integrated on the circumferential surface of the rod-shaped body, which reduces additional packaging steps and materials, thereby reducing the size and weight of the device, and facilitating integration into smaller devices.

[0040] In this embodiment, the orthographic projection of the first chip 2 can fall on the same surface as the orthographic projection of the second chip 3. The first chip 2 is a signal distribution center, such as clock distribution, data cache, etc., which provides necessary support for the orthographic chip and reasonably distributes signals to the second chip 3, thereby reducing signal cross-interference and improving signal processing efficiency.

[0041] The cross-sectional shape of the rod-shaped body 1 can be selected according to the actual scenario to achieve the maximum utilization of the substrate crystal rod. Figure 6 In (A), the cross-sectional shape of the rod-shaped body 1 is circular, and an arc-shaped bearing portion is correspondingly provided on the circuit board 4, and a solder pad is formed on the bearing portion. The first chip is flip-chip soldered on the bearing portion of the circuit board, and the bearing portion has a limiting effect on the chip, so that the rod-shaped body 1 can be stably fixed on the circuit board 4; Figure 6 In (B), the cross-section of the rod is quasi-circular; Figure 6 In (C), the cross-sectional shape of the rod-shaped body 1 is a square; Figure 6 In (D), the cross-sectional shape of the rod-shaped body 1 is a square.

[0042] In this embodiment, 6 (C) is used as an example for explanation. A microchannel 10 is also provided on the surface of the rod-shaped body 1. The microchannel 10 is distributed along the circumference of the rod-shaped body and extends from the first chip 2 at the edge to the second chip 3 at the edge on the same side. The microchannel 10 is filled with a phase change material 11, but the phase change material 11 does not fill the microchannel 10. When the semiconductor device is heated, the phase change material 11 in the microchannel 10 absorbs heat and begins to melt, and the phase change material 11 expands and rises along the microchannel 10. The phase change material 11 transfers heat from the heat source area to the colder area during the rising process. When the phase change material flows to a colder area, it releases heat and re-solidifies because the microchannel 10 extends from the first chip 2 at the edge to the second chip 3 at the edge on the same side. This allows the phase change material to expand due to heat, taking away heat, and to flow back under the action of gravity. It can then return to the heat source area through capillary action and gravity. The phase change material 11 circulates between solid and liquid states, continuously absorbing and releasing heat, thereby achieving thermal management of semiconductor devices.

[0043] The above are all preferred embodiments of the present application, and the protection scope of the present application is not limited thereto. Therefore, any equivalent changes made according to the structure, shape, and principle of the present application should be included in the protection scope of the present application.

Claims

1. A method for manufacturing a semiconductor device, It is characterized in that include: Grinding: providing a substrate crystal rod, the diameter of the substrate crystal rod being 0.1 mm to 200 mm, grinding the circumferential surface of the substrate crystal rod (1) to obtain a rod-shaped body (1), the rod-shaped body (1) having a cross section of a predetermined shape, and the surface of the rod-shaped body after grinding is a smooth surface; Cleaning: removing impurities on the surface of the lining rod-shaped body (1); Coating: photolithography the circumferential surface of the rod-shaped body (1), and coating a semiconductor functional film layer to form a chip on the circumferential surface of the rod-shaped body (1); Electroplating: performing electroplating treatment at a preset position of the functional film layer, forming an electroplating electrode on the surface of the semiconductor functional film layer, and electroplating to form a conductive circuit at a preset position of the rod-shaped body (1), thereby obtaining a rod-shaped body (1) having a plurality of chips formed on the circumferential surface, wherein the conductive circuit enables the chips to establish a communication connection; Surface treatment: stripping off impurities and photoresist remaining on the circumferential surface of the rod-shaped body (1); Testing: testing the plurality of chips formed on the rod-shaped body (1); and Welding: providing a circuit board (4), electrically connecting the chip to the circuit board (4), and obtaining a semiconductor device with a plurality of chips distributed in a circumferential direction.

2. The method for manufacturing a semiconductor device according to claim 1, It is characterized in that The chip comprises a first chip (2) and a second chip (3), and the orthographic projection of the first chip (2) and the orthographic projection of the second chip (3) can fall on the same surface; and / or The first chip (2) and the second chip (3) are arranged in an array respectively; and The first chip (2) is flip-chip soldered to the circuit board (4), and the second chip (3) is face-mounted on the circuit board (4) via gold wires.

3. The method for manufacturing a semiconductor device according to claim 1, It is characterized in that The cross section of the predetermined shape is semicircular, circular, square, polygonal, quasi-circular, quasi-square or quasi-polygonal.

4. The method for manufacturing a semiconductor device according to claim 2, It is characterized in that After the grinding step, a self-tensioning support frame (5) and a position adjustment mechanism are also provided, wherein the self-tensioning support frame (5) includes a base (50) and support heads (52) located at opposite ends of the base (50), the substrate crystal rod is fixed to the self-tensioning support frame (5), and the opposite ends of the substrate crystal rod are respectively clamped on the two support heads (52); the position adjustment mechanism is configured to drive the self-tensioning support frame (5) to move parallel to and rotate along the axial direction.

5. The method for manufacturing a semiconductor device according to claim 4, It is characterized in that In the grinding step, the provided grinding device includes a workbench (7) and a plurality of grinding heads (8) fixed to the workbench (7), the plurality of grinding heads (8) are evenly distributed along the same circumference, and the grinding heads (8) can be telescopically adjustable through a precision mechanism.

6. The method for manufacturing a semiconductor device according to claim 5, It is characterized in that An ultrasonic probe (9) and a closed-loop control system are also provided on the workbench (7). The ultrasonic probe (9) measures the grinding accuracy of the substrate crystal rod in real time and feeds back the data to the closed-loop control system. The closed-loop control system automatically adjusts the pressure, grinding speed and telescopic position of each grinding head (8) according to the measurement results of the ultrasonic probe (9).

7. The method for manufacturing a semiconductor device according to any one of claims 1 to 6, It is characterized in that After the testing step and before the welding step, the method further comprises arranging a microchannel (10) on the surface of the rod-shaped body (1), wherein the microchannel (10) is distributed along the circumference of the rod-shaped body (1) and extends at least from the first chip (2) at the outermost edge to the second chip (3) at the outermost edge on the same side, and the microchannel (10) is filled with a phase change material (11).

8. The method for manufacturing a semiconductor device according to claim 7, It is characterized in that In the coating step, a photolithography device is provided, comprising a laser (60), a mask (62) and a projection lens group (64), wherein the mask (62) is arranged between the laser (60) and the projection lens group (64), and the projection lens group (64) comprises at least three concave reflection mirrors, wherein the diameters of the three concave reflection mirrors decrease in sequence on the light output path of the laser (60).

9. A semiconductor device, It is characterized in that include: Circuit board (4); as well as A rod-shaped body (1), wherein a plurality of chips are formed on the surface of the rod-shaped body (1), wherein the chips include a first chip (2) and a second chip (3), wherein the orthographic projection of the first chip (2) and the orthographic projection of the second chip (3) can fall on the same surface; and / or the first chip (2) and the second chip (3) are arranged in an array; and The first chip (2) is flip-chip soldered to the circuit board (4), and the second chip (3) is face-mounted on the circuit board (4) via a gold wire (40).

10. The semiconductor device according to claim 9, It is characterized in that A microchannel (10) is also provided on the surface of the rod-shaped body (1), the microchannel (10) is distributed along the circumference of the rod-shaped body (1) and extends at least from the first chip (2) at the outermost edge to the second chip (3) at the outermost edge on the same side, and the microchannel is filled with a phase change material.

Citation Information

Cited By

  • Semiconductor device and manufacturing method therefor

    WO2026020851A1