Redox flow battery electrolyte with stable circulation and preparation method thereof
By preparing a liquid-flow battery electrolyte containing lead methylsulfonate, maleic anhydride, acrylamide, triethyl phosphate water, boric acid and hydrogen peroxide, the problems of conduction efficiency and battery life of the liquid-flow battery electrolyte are solved, and the problem of the liquid-flow battery electrolyte is achieved. High efficiency and stable battery performance and low cost preparation.
Patent Information
- Application Number
- CN202411369720.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-29
- Publication Date
- 2024-11-12
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing liquid-flow battery electrolyte has shortcomings in conduction efficiency and working stability, and the battery life is short.
A liquid-flow battery electrolyte composed of lead methylsulfonate, maleic anhydride, acrylamide, triethyl phosphate water, boric acid and hydrogen peroxide is prepared through specific stirring and heating steps, and the pH value and temperature are adjusted to form Cycling stable electrolyte.
The high conduction efficiency, working stability and long battery life of the electrolyte are achieved, and the cost of preparation equipment is reduced.
Smart Images

Figure CN118943444A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the technical field of liquid flow batteries, and relates to a liquid flow battery electrolyte and a preparation method thereof, in particular to a liquid flow battery electrolyte with stable circulation and a preparation method thereof. Background Art
[0002] Liquid flow battery is an electrochemical energy storage technology proposed by Thaller in 1974. It is a new type of battery. Liquid flow battery consists of a battery stack unit, electrolyte, electrolyte storage and supply unit, and management control unit. It is a high-performance battery that separates the positive and negative electrolytes and circulates them separately. It has the characteristics of high capacity, wide application field, and long cycle life. It is a new energy product.
[0003] After searching, for example, Chinese patent documents disclose a seasonal electrolyte for lead liquid flow batteries and a preparation method thereof [Application No.: 201910283866.0; Publication No.: CN 109873191 B]. This seasonal electrolyte for lead liquid flow batteries and a preparation method thereof, the electrolyte is a mixture of lead fluoroborate, fluoroboric acid and boric acid, wherein the concentration of lead fluoroborate is 2-3 mol / L, the concentration of fluoroboric acid is 0-1 mol / L, the concentration of boric acid is 0.1-0.5 mol / L and an appropriate amount of additives. The electrolyte can make the lead liquid flow battery recyclable in the temperature range of -50℃-60℃, the coulomb efficiency is basically above 90%, the energy efficiency is above 70%, and the energy density is about 35Wh / L.
[0004] Although the electrolyte disclosed in this patent can make the lead liquid flow battery recyclable in the temperature range of -50℃-60℃, the coulomb efficiency is basically above 90%, the energy efficiency is above 70%, and the energy density is around 35Wh / L, it cannot make the conduction efficiency fast, the operation stable, and the battery life long. Summary of the invention
[0005] The purpose of the present invention is to address the above-mentioned problems in the existing technology and propose a cyclically stable liquid flow battery electrolyte and a preparation method thereof. The technical problem to be solved by the invention is: how to achieve fast electrolyte conduction efficiency, stable operation and long battery life.
[0006] The purpose of the present invention can be achieved by the following technical solutions: A circulation-stable liquid flow battery electrolyte is prepared from the following raw materials in parts by weight: 6-18 parts of lead methanesulfonate, 10-30 parts of maleic anhydride, 6-20 parts of acrylamide, 20-30 parts of triethyl phosphate water, 20-35 parts of boric acid, 1-10 parts of hydrogen peroxide and 20-30 parts of deionized water.
[0007] The liquid flow battery electrolyte is made of the following raw materials in parts by weight: 8-12 parts of lead methyl sulfonate, 12-18 parts of maleic anhydride, 10-16 parts of acrylamide, 20-25 parts of triethyl phosphate water, 30-35 parts of boric acid, 3-6 parts of hydrogen peroxide and 10-15 parts of deionized water.
[0008] The flow battery electrolyte is made of the following raw materials in parts by weight: 15 parts of lead methyl sulfonate, 20 parts of maleic anhydride, 13 parts of acrylamide, 25 parts of triethyl phosphate water, 27 parts of boric acid, 5 parts of hydrogen peroxide and 25 parts of ionized water.
[0009] A method for preparing a cyclically stable liquid flow battery electrolyte comprises the following steps: S1, maleic anhydride, acrylamide and half of the lead methyl sulfonate are mixed and stirred to obtain a first mixed solution, and the first mixed solution is mixed and stirred with triethyl phosphate water to obtain a second mixed solution; S2, half of the lead methyl sulfonate is mixed with boric acid to obtain a third mixed solution, the third mixed solution is dissolved in deionized water, and stirred until clear; S3, adjusting the pH value of the second mixed solution to 10-11 to obtain a fourth mixed solution, stirring the third mixed solution and the fourth mixed solution evenly, slowly heating to 70° C.-90° C., and dropping hydrogen peroxide to obtain a fifth mixed solution after the dropping is complete; S4. Heat the fifth mixed solution to a temperature of 75°C-95°C. After the reaction is completed, stop heating and cool the mixed solution while stirring to obtain a lead-vanadium liquid flow battery electrolyte.
[0010] The stirring speed in step S1 and step S2 is between 30-300 rpm, the stirring speed in S3 is between 50-200 rpm, and the stirring speed in S4 is between 15-48 rpm.
[0011] The heating time in step S3 is 20 minutes, the heating time in step S4 is 12 minutes, and the cooling time is 25 minutes.
[0012] The device used in steps one to four is an integrated preparation device, which includes: the integrated preparation device includes a mixing barrel one and a mixing barrel two, a rotating groove is provided in the mixing barrel one, a rotating drum is rotatably connected in the rotating groove, a gear ring is fixed to the outer wall of the rotating drum, a motor two is fixed on the mixing barrel one, a gear one is fixed to the output shaft end of the motor two, the gear one is meshed with the gear ring, a hollow shaft is rotatably connected in the rotating drum, a motor one is fixed in the mixing barrel one, the output shaft end of the motor one is fixedly connected to the hollow shaft, two stirring rods one are fixed on the hollow shaft, a stirring rod two is rotatably connected on the hollow shaft, the stirring rod two is fixedly connected to the inner wall of the rotating drum, a feeding port is provided in the mixing barrel one, the hollow shaft and the mixing barrel two are connected by a suction pipe, and a water pump is fixed in the suction pipe.
[0013] The above structure is adopted, maleic anhydride, acrylamide and half of lead methyl sulfonate are poured into a stirring barrel 1, motor 2 is started, gear 1 is driven to rotate, gear 1 drives the gear ring to drive the rotating drum to rotate, so that the rotating drum drives the stirring rod 2 to rotate, so that the stirring rod 2 and the stirring rod 1 rotate in the opposite direction, and the stirring is more uniform, motor 1 is started, the hollow shaft is driven to rotate, the stirring rod 1 on the hollow shaft stirs the maleic anhydride, acrylamide and half of the lead methyl sulfonate, the stirring rod 2 rotates in the opposite direction of the stirring rod 1 with the rotating drum, the stirring efficiency is improved, and the stirring is more uniform, after the first mixed liquid is stirred, triethyl phosphate water is poured into the stirring barrel 1 for stirring to obtain a second mixed liquid, the second mixed liquid is pumped into the second stirring barrel through a suction pipe, half of the lead methyl sulfonate and boric acid are poured into the stirring barrel 1 for stirring to obtain a third mixed liquid, and then ion water is poured into the third mixed liquid and stirred until it is clarified, the pH value of the second mixed liquid in the stirring barrel 2 is adjusted to - to obtain a fourth mixed liquid, and the third mixed liquid in the stirring barrel 1 is pumped into the stirring barrel 2.
[0014] A water inlet is provided on the lower side of the hollow shaft, and the suction tube extends into the water inlet. A piston ring is slidably connected inside the hollow shaft, and a connecting ring is slidably connected to the outer wall of the hollow shaft. The connecting ring and the piston ring are connected by two ropes. A connecting rod extending from the mixing barrel is fixed on the connecting ring, and the two connecting rods are connected by a threaded plate. A motor three is fixed on the mixing barrel one, and a screw is fixed on the output shaft end of the motor three, and the screw is threadedly connected to the threaded plate.
[0015] With the above structure, the motor three is started to drive the lead screw to rotate, and the threaded plate on the lead screw drives the connecting ring on the connecting rod to move up and down. When the connecting ring moves downward on the hollow shaft, the piston ring is driven to slide upward through the rope, so that the water inlet is opened, and the mixed liquid in the rotating drum enters the hollow shaft through the water inlet, and then the mixed liquid is pumped into the mixing barrel two through the suction tube.
[0016] A mounting column is fixed on the hollow shaft, and a mounting groove connected to the inside of the hollow shaft is provided on the mounting column. A rotating column is rotatably connected in the mounting groove, and a second gear is fixed on the rotating column. A gear rod is fixed on the piston ring, and the second gear is meshed with the gear rod. A torsion spring is fixed in the mounting groove, and the other end of the torsion spring is fixedly connected to the gear.
[0017] With the above structure, when the connecting ring moves upward on the hollow shaft, there is no more traction on the piston ring through the rope, and the elastic force of the torsion spring causes gear two to rotate, and gear two drives the piston ring on the gear rod to move downward, thereby enabling the piston ring to block the water inlet.
[0018] A fixed shaft is fixed in the mixing barrel two, a sleeve is slidably connected to the fixed shaft, a stirring rod three is fixed on the sleeve, a moving ring is slidably connected to the fixed shaft, the moving ring is rotatably connected to the sleeve, an electric telescopic rod is fixed to the mixing barrel two, the telescopic end of the electric telescopic rod is fixedly connected to the moving ring, a spiral groove is provided on the inner wall of the mixing barrel two, a sliding ball is fixed on the stirring rod three, the sliding ball is slidably connected to the spiral groove, a heating groove is provided on the inner wall of the mixing barrel two, and a heater is fixed in the heating groove.
[0019] With the above structure, the third mixed liquid and the fourth mixed liquid are in the stirring barrel 2, and the heater and the electric telescopic rod are started. While the heater heats the third mixed liquid and the fourth mixed liquid, the electric telescopic rod drives the moving ring to move up and down, and the stirring rod 3 on the sleeve rotatably connected to the moving ring moves up and down in the stirring barrel 2, and the sliding ball on the stirring rod 3 slides in the spiral groove to rotate the stirring rod 3, thereby achieving uniform stirring of the third mixed liquid and the fourth mixed liquid.
[0020] Compared with the prior art, the present cyclically stable liquid flow battery electrolyte and its preparation method have the following advantages: 1. The stable circulation liquid flow battery electrolyte and the preparation method thereof of the present invention have fast electrolyte conduction efficiency, stable operation, and long battery life. In addition, the existing stable circulation liquid flow battery electrolyte preparation process adopts integrated preparation equipment, and the required equipment cost is low.
[0021] 2. Pour maleic anhydride, acrylamide and half of the lead methylsulfonate into a stirring barrel, start motor 2, drive gear 1 to rotate, gear 1 drives the gear ring to drive the drum to rotate, so that the drum drives the stirring rod 2 to rotate, so that the stirring rod 2 and the stirring rod 1 rotate in the opposite direction, and the stirring is more uniform. Start motor 1, drive the hollow shaft to rotate, and the stirring rod 1 on the hollow shaft stirs maleic anhydride, acrylamide and half of the lead methylsulfonate. The stirring rod 2 rotates with the drum in the opposite direction to the stirring rod 1, thereby improving the stirring efficiency and making the stirring more uniform. After the first mixed solution is stirred, triethyl phosphate water is poured into the stirring barrel 1 for stirring to obtain a second mixed solution. The second mixed solution is pumped into the second stirring barrel through a suction tube, and half of the lead methylsulfonate and boric acid are poured into the stirring barrel 1 for stirring to obtain a third mixed solution. Then, ionized water is poured into the third mixed solution and stirred until it is clarified. The second mixed solution in the stirring barrel 2 is adjusted to a pH value of - to obtain a fourth mixed solution, and the third mixed solution in the stirring barrel 1 is pumped into the stirring barrel 2.
[0022] 3. The third mixed liquid and the fourth mixed liquid are in the stirring barrel 2, and the heater and the electric telescopic rod are started. While the heater heats the third mixed liquid and the fourth mixed liquid, the electric telescopic rod drives the moving ring to move up and down, and the stirring rod 3 on the sleeve rotatably connected to the moving ring moves up and down in the stirring barrel 2, and the sliding ball on the stirring rod 3 slides in the spiral groove to make the stirring rod 3 rotate, thereby achieving uniform stirring of the third mixed liquid and the fourth mixed liquid.
[0023] 4. Start motor three to drive the lead screw to rotate. The threaded plate on the lead screw drives the connecting ring on the connecting rod to move up and down. When the connecting ring moves downward on the hollow shaft, the piston ring is driven to slide upward through the rope to open the water inlet. The mixed liquid in the rotating drum enters the hollow shaft through the water inlet, and then the mixed liquid is pumped into the mixing barrel two through the suction tube. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Figure 1 It is a work flow chart of the present invention.
[0025] Figure 2 It is a schematic diagram of the overall structure of the integrated preparation device in the present invention.
[0026] Figure 3 It is an overall cross-sectional view of the integrated preparation device in the present invention.
[0027] Figure 4 It is a cross-sectional view of a stirring barrel 1 of the integrated preparation device of the present invention.
[0028] Figure 5 yes Figure 4 A is an enlarged view of the middle image.
[0029] Figure 6 yes Figure 3 Enlarged view of B.
[0030] Figure 7 It is a cross-sectional view of the stirring barrel 2 of the integrated preparation device in the present invention.
[0031] Figure 8 This is the formula diagram of the electrolyte of the liquid flow battery in the present invention In the figure, 1, mixing barrel one; 2, mixing barrel two; 3, rotating trough; 4, rotating drum; 5, gear ring; 6, motor one; 7, gear one; 8, piston ring; 9, connecting ring; 10, rope; 11, suction tube; 12, connecting rod; 13, threaded plate; 14, motor three; 15, lead screw; 16, fixed shaft; 17, sleeve; 18, stirring rod three; 19, moving ring; 20, electric telescopic rod; 21, spiral groove; 22, sliding ball; 23, heating trough; 24, heater; 25, mounting column; 26, mounting groove; 27, rotating column; 28, gear two; 29, gear rod; 30, torsion spring; 31, hollow shaft; 32, stirring rod two; 33, stirring rod one; 34, motor four. DETAILED DESCRIPTION
[0032] The following are specific embodiments of the present invention and the accompanying drawings to further describe the technical solution of the present invention, but the present invention is not limited to these embodiments.
[0033] Embodiment 1 A circulation-stable liquid flow battery electrolyte is prepared from the following raw materials in parts by weight: 15 parts of lead methyl sulfonate, 20 parts of maleic anhydride, 13 parts of acrylamide, 25 parts of triethyl phosphate water, 27 parts of boric acid, 5 parts of hydrogen peroxide and 25 parts of ionized water.
[0034] like Figure 1 As shown, a method for preparing a cyclically stable liquid flow battery electrolyte comprises the following steps: S1, maleic anhydride, acrylamide and half of lead methyl sulfonate are mixed and stirred to obtain a first mixed solution, and the first mixed solution is mixed and stirred with triethyl phosphate water to obtain a second mixed solution; S2, half of the lead methyl sulfonate is mixed with boric acid to obtain a third mixed solution, the third mixed solution is dissolved in deionized water, and stirred until clear; S3, adjusting the pH value of the second mixed solution to 11 to obtain a fourth mixed solution, stirring the third mixed solution and the fourth mixed solution evenly, slowly heating to 80° C., and dropping hydrogen peroxide to obtain a fifth mixed solution after the dropping is complete; S4. Heat the fifth mixed solution to 85° C. After the reaction is completed, stop heating and cool the mixed solution while stirring to obtain a lead-vanadium liquid flow battery electrolyte.
[0035] The stirring speed in step S1 and step S2 is between 300 rpm, the stirring speed in S3 is between 200 rpm, and the stirring speed in S4 is between 50 rpm.
[0036] The heating time in step S3 is 20 minutes, the heating time in step S4 is 12 minutes, and the cooling time is 25 minutes.
[0037] The preparation equipment used in this embodiment are all existing equipment on the market, among which, the one used in step 1 is: cantilever electric stirrer, model: LC-OES-200SH; the one used in step 2 is: electric stirrer, model: GH-2021; the ones used in steps 3 and 4 are: magnetic heating stirrer, model: Australian KEWLAB.
[0038] Embodiment 2 A circulation-stable liquid flow battery electrolyte is made from the following raw materials in parts by weight: The liquid flow battery electrolyte is made from the following raw materials in parts by weight: 15 parts of lead methanesulfonate, 20 parts of maleic anhydride, 13 parts of acrylamide, 25 parts of triethyl phosphate water, 27 parts of boric acid, 5 parts of hydrogen peroxide and 25 parts of ionized water.
[0039] like Figure 1 As shown, a method for preparing a cyclically stable liquid flow battery electrolyte comprises the following steps: S1, maleic anhydride, acrylamide and half of lead methyl sulfonate are mixed and stirred evenly to obtain a first mixed solution, and the first mixed solution is mixed and stirred evenly with triethyl phosphate water to obtain a second mixed solution.
[0040] S2. Mix half of the lead methyl sulfonate with boric acid to obtain a third mixed solution, dissolve the third mixed solution in deionized water, and stir until it is clear.
[0041] S3. Adjust the pH value of the second mixed solution to 11 to obtain a fourth mixed solution. Evenly stir the third mixed solution and the fourth mixed solution, slowly heat to 80° C., dropwise add hydrogen peroxide, and obtain a fifth mixed solution after the dropwise addition is complete.
[0042] S4. Heat the fifth mixed solution to 85° C. After the reaction is completed, stop heating and cool the mixed solution while stirring to obtain a lead-vanadium liquid flow battery electrolyte.
[0043] The stirring speed in step S1 and step S2 is between 300 rpm, the stirring speed in S3 is between 200 rpm, and the stirring speed in S4 is between 50 rpm.
[0044] The heating time in step S3 is 20 minutes, the heating time in step S4 is 12 minutes, and the cooling time is 25 minutes.
[0045] like Figure 4As shown, the device used in step 1 to step 4 is an integrated preparation device, which includes a mixing barrel 1 and a mixing barrel 2, a rotating groove 3 is provided in the mixing barrel 1, a rotating drum 4 is rotatably connected in the rotating groove 3, a gear ring 5 is fixed to the outer wall of the rotating drum 4, a motor 2 34 is fixed on the mixing barrel 1, a gear 7 is fixed to the output shaft end of the motor 2 34, the gear 7 is meshed with the gear ring 5, a hollow shaft 31 is rotatably connected in the rotating drum 4, a motor 6 is fixed in the mixing barrel 1, the output shaft end of the motor 6 is fixedly connected to the hollow shaft 31, two stirring rods 1 33 are fixed on the hollow shaft 31, a stirring rod 2 32 is rotatably connected on the hollow shaft 31, the stirring rod 2 32 is fixedly connected to the inner wall of the rotating drum 4, a feeding port is provided on the mixing barrel 1, the hollow shaft 31 and the mixing barrel 2 2 are connected by a suction pipe 11, and a water pump is fixed in the suction pipe 11.
[0046] With the above structure, maleic anhydride, acrylamide and half of the lead methyl sulfonate are poured into the stirring barrel 1, the motor 2 34 is started, the gear 1 7 is driven to rotate, the gear 1 7 drives the gear ring 5 to drive the rotating drum 4 to rotate, so that the rotating drum 4 drives the stirring rod 2 32 to rotate, so that the stirring rod 2 32 and the stirring rod 1 33 rotate in opposite directions, and the stirring is more uniform. The motor 1 6 is started to drive the hollow shaft 31 to rotate, and the stirring rod 1 33 on the hollow shaft 31 stirs the maleic anhydride, acrylamide and half of the lead methyl sulfonate, and the stirring rod 2 32 moves with the rotating drum 4 in the direction opposite to the stirring rod 1 33 rotates in the opposite direction to improve the stirring efficiency and make the stirring more uniform. After the first mixed liquid is stirred, triethyl phosphate water is poured into the stirring barrel 1 for stirring to obtain a second mixed liquid. The second mixed liquid is pumped into the second stirring barrel through the suction tube 11, and half of the lead methylsulfonate and boric acid are poured into the stirring barrel 1 for stirring to obtain a third mixed liquid. Then, ionized water is poured into the third mixed liquid and stirred until it is clarified. The pH value of the second mixed liquid in the stirring barrel 2 is adjusted to - to obtain a fourth mixed liquid. The third mixed liquid in the stirring barrel 1 is pumped into the stirring barrel 2.
[0047] like Figure 4-6 As shown, a water inlet is provided on the lower side of the hollow shaft 31, and a suction tube 11 extends into the water inlet. A piston ring 8 is slidably connected inside the hollow shaft 31, and a connecting ring 9 is slidably connected to the outer wall of the hollow shaft 31. The connecting ring 9 is connected to the piston ring 8 by two ropes 10. A connecting rod 12 extending from the mixing barrel 1 is fixed to the connecting ring 9, and the two connecting rods 12 are connected by a threaded plate 13. A motor 3 14 is fixed to the mixing barrel 1, and a screw 15 is fixed to the output shaft end of the motor 3 14. The screw 15 is threadedly connected to the threaded plate 13.
[0048] With the above structure, the motor 3 14 is started to drive the lead screw 15 to rotate, and the threaded plate 13 on the lead screw 15 drives the connecting ring 9 on the connecting rod 12 to move up and down. When the connecting ring 9 moves downward on the hollow shaft 31, the piston ring 8 is driven to slide upward through the rope 10, so that the water inlet is opened, and the mixed liquid in the rotating drum 4 enters the hollow shaft 31 through the water inlet, and then the mixed liquid is pumped into the mixing barrel 2 through the suction tube 11.
[0049] like Figure 4-5 As shown, a mounting column 25 is fixed on the hollow shaft 31, and a mounting groove 26 connected to the inside of the hollow shaft 31 is formed on the mounting column 25. A rotating column 27 is rotatably connected in the mounting groove 26, and a gear 28 is fixed on the rotating column 27. A gear rod 29 is fixed on the piston ring 8, and the gear 28 is meshingly connected with the gear rod 29. A torsion spring 30 is fixed in the mounting groove 26, and the other end of the torsion spring 30 is fixedly connected to the gear.
[0050] With the above structure, when the connecting ring 9 moves upward on the hollow shaft 31, there is no more traction on the piston ring 8 through the rope 10, and the elastic force of the torsion spring 30 causes the gear 28 to rotate, and the gear 28 drives the piston ring 8 on the gear rod 29 to move downward, so that the piston ring 8 blocks the water inlet.
[0051] like Figure 7 As shown, a fixed shaft 16 is fixed in the mixing barrel 2, a sleeve 17 is slidably connected to the fixed shaft 16, a stirring rod 3 18 is fixed to the sleeve 17, a moving ring 19 is slidably connected to the fixed shaft 16, the moving ring 19 is rotatably connected to the sleeve 17, an electric telescopic rod 20 is fixed to the mixing barrel 2, the telescopic end of the electric telescopic rod 20 is fixedly connected to the moving ring 19, a spiral groove 21 is provided on the inner wall of the mixing barrel 2, a sliding ball 22 is fixed on the stirring rod 3 18, the sliding ball 22 is slidably connected to the spiral groove 21, a heating groove 23 is provided on the inner wall of the mixing barrel 2, and a heater 24 is fixed in the heating groove 23.
[0052] With the above structure, the third mixed liquid and the fourth mixed liquid are in the stirring barrel 2, and the heater 24 and the electric telescopic rod 20 are started. While the heater 24 heats the third mixed liquid and the fourth mixed liquid, the electric telescopic rod 20 drives the moving ring 19 to move up and down, and the stirring rod 3 18 on the sleeve 17 that is movably connected to the moving ring 19 moves up and down in the stirring barrel 2, and the sliding ball 22 on the stirring rod 3 18 slides in the spiral groove 21 to rotate the stirring rod 3 18, thereby achieving uniform stirring of the third mixed liquid and the fourth mixed liquid.
[0053] Example 3 A circulation-stable liquid flow battery electrolyte is prepared from the following raw materials in parts by weight: 18 parts of lead methyl sulfonate, 10 parts of maleic anhydride, 20 parts of acrylamide, 20 parts of triethyl phosphate water, 35 parts of boric acid, 1 part of hydrogen peroxide and 30 parts of ionized water.
[0054] like Figure 1 As shown, a method for preparing a cyclically stable liquid flow battery electrolyte comprises the following steps: S1, maleic anhydride, acrylamide and half-lead methylsulfonate are mixed and stirred evenly to obtain a first mixed solution, and the first mixed solution is mixed and stirred evenly with triethyl phosphate water to obtain a second mixed solution; S2, half of the lead methylsulfonate is mixed with boric acid to obtain a third mixed solution, the third mixed solution is dissolved in deionized water, and stirred until clear; S3, adjusting the pH value of the second mixed solution to 11 to obtain a fourth mixed solution, stirring the third mixed solution and the fourth mixed solution evenly, slowly heating to 85° C., and dropping hydrogen peroxide to obtain a fifth mixed solution after the dropping is complete; S4. Heat the fifth mixed solution to 90° C. After the reaction is completed, stop heating and cool the mixed solution while stirring to obtain a lead-vanadium liquid flow battery electrolyte.
[0055] The stirring speed in step S1 and step S2 is between 300 rpm, the stirring speed in S3 is between 200 rpm, and the stirring speed in S4 is between 50 rpm.
[0056] The heating time in step S3 is 20 minutes, the heating time in step S4 is 12 minutes, and the cooling time is 25 minutes.
[0057] The preparation equipment used in the method for preparing a circulation-stable liquid flow battery electrolyte in this embodiment is the same as the equipment in Example 2, and the difference lies in the different ratios of the raw materials in the process.
[0058] Example 4 A circulation-stable liquid flow battery electrolyte is prepared from the following raw materials in parts by weight: 6 parts of lead methyl sulfonate, 30 parts of maleic anhydride, 6 parts of acrylamide, 30 parts of triethyl phosphate water, 20 parts of boric acid, 10 parts of hydrogen peroxide and 20 parts of ionized water.
[0059] like Figure 1 As shown, a method for preparing a cyclically stable liquid flow battery electrolyte comprises the following steps: S1, maleic anhydride, acrylamide and half-lead methylsulfonate are mixed and stirred evenly to obtain a first mixed solution, and the first mixed solution is mixed and stirred evenly with triethyl phosphate water to obtain a second mixed solution; S2, half of the lead methylsulfonate is mixed with boric acid to obtain a third mixed solution, the third mixed solution is dissolved in deionized water, and stirred until clear; S3, adjusting the pH value of the second mixed solution to 11 to obtain a fourth mixed solution, stirring the third mixed solution and the fourth mixed solution evenly, slowly heating to 85° C., and dropping hydrogen peroxide to obtain a fifth mixed solution after the dropping is complete; S4. Heat the fifth mixed solution to 90° C. After the reaction is completed, stop heating and cool the mixed solution while stirring to obtain a lead-vanadium liquid flow battery electrolyte.
[0060] The stirring speed in step S1 and step S2 is between 300 rpm, the stirring speed in S3 is between 200 rpm, and the stirring speed in S4 is between 50 rpm.
[0061] The heating time in step S3 is 20 minutes, the heating time in step S4 is 12 minutes, and the cooling time is 25 minutes.
[0062] The preparation equipment used in the method for preparing a circulation-stable liquid flow battery electrolyte in this embodiment is the same as the equipment in Example 2, and the difference lies in the different ratios of the raw materials in the process.
[0063] Experimental example The flow battery electrolytes prepared in Examples 1-4 were subjected to comparative experiments: the comparative criteria were: the conductivity of the flow battery electrolyte; battery life; stirring efficiency; the data was more intuitive. The experimental table is as follows (Table 1):
[0064] In summary, the conduction efficiency, battery life and stirring efficiency of the flow battery electrolyte prepared by the cycle-stable flow battery electrolyte and the preparation method thereof of the present invention are superior to the cycle-stable flow battery electrolyte in the prior art.
[0065] In Example 1 and Example 2, only the molding equipment of S1 to S4 is different. The conduction efficiency, battery life and stirring efficiency in Example 2 are significantly better than those in Example 1. Therefore, the use of the circulating stable liquid flow battery electrolyte and the preparation method thereof in the present invention can improve the electrolyte conduction efficiency, battery life and stirring efficiency of the liquid flow battery.
[0066] Compared with Example 2, Example 3 and Example 4 only have different ratios of raw materials in the process, and the equipment used in the processing steps are the same. The conduction efficiency of Example 2 is lower than that of Example 3 and Example 4, the battery life of Example 3 is lower than that of Example 2 and Example 4, and the stirring efficiency of Example 4 is lower than that of Example 2 and Example 3. It can be seen that different ratios of raw materials will also affect the conduction efficiency, battery life and stirring efficiency of the liquid flow battery electrolyte.
[0067] The specific embodiments described herein are merely examples of the spirit of the present invention. Those skilled in the art may make various modifications or additions to the specific embodiments described or replace them in similar ways, but they will not deviate from the spirit of the present invention or exceed the scope defined by the appended claims.
Claims
1. A cyclically stable liquid flow battery electrolyte, characterized in that: The flow battery electrolyte is prepared from the following raw materials in parts by weight: 6-18 parts of lead methyl sulfonate, 10-30 parts of maleic anhydride, 6-20 parts of acrylamide, 20-30 parts of triethyl phosphate water, 20-35 parts of boric acid, 1-10 parts of hydrogen peroxide and 20-30 parts of deionized water.
2. A cyclically stable liquid flow battery electrolyte according to claim 1, characterized in that: The liquid flow battery electrolyte is made of the following raw materials in parts by weight: 8-12 parts of lead methyl sulfonate, 12-18 parts of maleic anhydride, 10-16 parts of acrylamide, 20-25 parts of triethyl phosphate water, 30-35 parts of boric acid, 3-6 parts of hydrogen peroxide and 10-15 parts of deionized water.
3. A cyclically stable liquid flow battery electrolyte according to claim 1, characterized in that: The flow battery electrolyte is made of the following raw materials in parts by weight: 15 parts of lead methyl sulfonate, 20 parts of maleic anhydride, 13 parts of acrylamide, 25 parts of triethyl phosphate water, 27 parts of boric acid, 5 parts of hydrogen peroxide and 25 parts of ionized water.
4. A method for preparing a cyclically stable liquid flow battery electrolyte according to claims 1-3, characterized in that: The following steps are involved: S1, maleic anhydride, acrylamide and half of the lead methyl sulfonate are mixed and stirred to obtain a first mixed solution, and the first mixed solution is mixed and stirred with triethyl phosphate water to obtain a second mixed solution; S2, half of the lead methyl sulfonate is mixed with boric acid to obtain a third mixed solution, the third mixed solution is dissolved in deionized water, and stirred until clear; S3, adjusting the pH value of the second mixed solution to 10-11 to obtain a fourth mixed solution, stirring the third mixed solution and the fourth mixed solution evenly, slowly heating to 70° C.-90° C., and dropping hydrogen peroxide to obtain a fifth mixed solution after the dropping is complete; S4. Heat the fifth mixed solution to a temperature of 75°C-95°C. After the reaction is completed, stop heating and cool the mixed solution while stirring to obtain a lead-vanadium liquid flow battery electrolyte.
5. The method for preparing a cyclically stable liquid flow battery electrolyte according to claim 4, characterized in that: The stirring speed in step S1 and step S2 is between 30-300 rpm, the stirring speed in S3 is between 50-200 rpm, and the stirring speed in S4 is between 15-48 rpm.
6. The method for preparing a cyclically stable liquid flow battery electrolyte according to claim 4, characterized in that: The heating time in step S3 is 20 minutes, the heating time in step S4 is 12 minutes, and the cooling time is 25 minutes.
7. The method for preparing a cyclically stable liquid flow battery electrolyte according to claim 4, characterized in that: The device used in step 1 to step 4 is an integrated preparation device, which comprises a mixing barrel 1 (1) and a mixing barrel 2 (2). A rotating groove (3) is provided in the mixing barrel 1 (1), a rotating drum (4) is rotatably connected in the rotating groove (3), a gear ring (31) is fixed to the outer wall of the rotating drum (4), a motor 2 (34) is fixed to the mixing barrel 1 (1), a gear 1 (7) is fixed to the output shaft end of the motor 2 (34), the gear 1 (7) is meshed with the gear ring (31), and the rotating drum (4) is rotated. A hollow shaft (5) is connected, a motor (6) is fixed in the mixing barrel (1), the output shaft end of the motor (6) is fixedly connected to the hollow shaft (5), two stirring rods (33) are fixed on the hollow shaft (5), a stirring rod (32) is rotatably connected to the hollow shaft (5), the stirring rod (32) is fixedly connected to the inner wall of the rotating drum (4), a feeding port is opened on the mixing barrel (1), the hollow shaft (31) and the mixing barrel (2) are connected through a suction pipe (11), and a water pump is fixed in the suction pipe (11).
8. The method for preparing a cyclically stable liquid flow battery electrolyte according to claim 7, characterized in that: A water inlet is provided at the lower side of the hollow shaft (5), and the suction pipe (11) extends into the water inlet. A piston ring (8) is slidably connected inside the hollow shaft (5), and a connecting ring (9) is slidably connected to the outer wall of the hollow shaft (5). The connecting ring and the piston ring (8) are connected by two ropes (10). A connecting rod (12) extending from the mixing barrel (1) is fixed on the connecting ring (9), and the two connecting rods (12) are connected by a threaded plate (13). A motor (14) is fixed on the mixing barrel (1), and a lead screw (15) is fixed to the output shaft end of the motor (14), and the lead screw (15) is threadedly connected to the threaded plate (13).
9. The method for preparing a cyclically stable liquid flow battery electrolyte according to claim 1, characterized in that: A mounting column (25) is fixed on the hollow shaft (5), and a mounting groove (26) is formed on the mounting column (25) and is communicated with the interior of the hollow shaft (5). A rotating column (27) is rotatably connected in the mounting groove (26), and a second gear (28) is fixed on the rotating column (27). A gear rod (29) is fixed on the piston ring (8), and the second gear (28) is meshingly connected with the gear rod (29). A torsion spring (30) is fixed in the mounting groove (26), and the other end of the torsion spring (30) is fixedly connected to the gear.
10. The method for preparing a cyclically stable liquid flow battery electrolyte according to claim 1, characterized in that: A fixed shaft (16) is fixed inside the mixing barrel (2), a sleeve (17) is slidably connected to the fixed shaft (16), a stirring rod (18) is fixed to the sleeve (17), a moving ring (19) is slidably connected to the fixed shaft (16), the moving ring (19) is rotatably connected to the sleeve (17), an electric telescopic rod (20) is fixed to the mixing barrel (2), the telescopic end of the electric telescopic rod (20) is fixedly connected to the moving ring (19), a spiral groove (21) is provided on the inner wall of the mixing barrel (2), a sliding ball (22) is fixed to the stirring rod (18), the sliding ball (22) is slidably connected to the spiral groove (21), a heating groove (23) is provided on the inner wall of the mixing barrel (2), and a heater (24) is fixed inside the heating groove (23).
Citation Information
Patent Citations
A weather-resistant electrolyte for lead-acid flow batteries and its preparation method
CN109873191B