Manufacturing method, film forming apparatus, and film forming method
By designing the convex shape holding surface on the electrostatic chuck and adjusting the film forming conditions using the film thickness measurement part, the problem of substrate deflection affecting the retention force is solved, and fast and low-voltage substrate holding is achieved, and production efficiency and finished product rate are improved. .
Patent Information
- Application Number
- CN202410558581.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-05-11
- Filing Date
- 2024-05-08
- Publication Date
- 2024-11-12
AI Technical Summary
When the electrostatic chuck holds the substrate, the deflection of the substrate will affect the holding force of the electrostatic chuck, resulting in the inability to effectively adsorb the substrate, and applying a high voltage may damage the component-forming area, and the power removal will take a long time, affecting production efficiency.
By designing a convex-shaped surface on the holding surface of the electrostatic chuck, matching the flexural shape of the substrate, to improve adsorption force, and using the film thickness measuring part in the passage chamber to measure the film thickness, adjust the film formation conditions to achieve fast and low voltage substrate retaining.
Effective maintenance under the condition of substrate deflection is achieved, component damage is avoided and power removal time is extended, and production efficiency and yield is improved.
Smart Images

Figure CN118946227A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a manufacturing method, a film forming device and a film forming method. Background Art
[0002] Organic EL display devices (OLEDs) are suitable for use in smartphones, televisions, and automobile displays as well as VR HMDs (Virtual Reality Head Mount Displays). When manufacturing an organic EL display device, it is necessary to form an organic light-emitting element (OLED) that constitutes the organic EL display device.
[0003] As a manufacturing device for such an organic EL display device, a film forming line having a device (film forming device) for conveying a substrate to a film forming chamber and performing film formation (film forming treatment) on the substrate is proposed (see Patent Document 1). Patent Document 1 proposes a group-type film forming device that conveys substrates from a conveying chamber to a plurality of film forming chambers in sequence and performs film formation treatment on the substrates in each film forming chamber. In addition, in Patent Document 1, in a conveying chamber, the thickness of a film (organic film or metal film) formed on the substrate, i.e., the film thickness, is measured while the substrate that has undergone film formation treatment is held (adsorbed) by an electrostatic chuck.
[0004] Prior Art Literature
[0005] Patent Literature
[0006] Patent Document 1: U.S. Patent Application No. 2021 / 0226183 Summary of the invention
[0007] Problems to be solved by the invention
[0008] However, when a substrate that has been subjected to film forming treatment is held by an electrostatic chuck as in the prior art, if the substrate is warped (e.g., warped (deformed) into a convex shape), the holding of the substrate by the electrostatic chuck may sometimes be affected. For example, due to the deflection of the substrate, the electrostatic chuck cannot exert sufficient holding force (adsorption force) on the substrate, and cannot match the substrate with the chuck surface (plane).
[0009] Thus, in the case where the substrate is deflected, in order to exert a sufficient holding force on the substrate, for example, it is conceivable to increase the voltage applied to the electrostatic chuck. However, when the deflection of the substrate becomes larger, even if the maximum voltage is applied to the electrostatic chuck, the substrate cannot be adsorbed, and it becomes difficult to hold the substrate itself with the electrostatic chuck. In addition, by applying a high voltage to the electrostatic chuck, it is possible that the element formation area (active area) where the element on the substrate is to be formed is damaged. In addition, it takes time to remove the high voltage (charged) applied to the electrostatic chuck, resulting in a longer cycle time, which is the time required for manufacturing a product.
[0010] The present invention provides a new technology which is beneficial for an electrostatic chuck to hold a substrate.
[0011] Solutions to Solve Problems
[0012] A manufacturing method as one embodiment of the present invention is a manufacturing method for manufacturing an electronic device, characterized in that the manufacturing method comprises: a first step of forming a film on a first surface of a substrate; a second step of sealing the film after the first step; and a third step of measuring the thickness of the film after the first step and before the second step while holding the substrate with the first surface of the substrate on which the film is formed in the first step facing the direction of gravity using a first electrostatic chuck, the first electrostatic chuck comprising a first holding surface that holds the substrate on a second surface of the substrate opposite to the first surface, the first holding surface having a surface shape that is convex on one side in the direction of gravity.
[0013] A manufacturing method as another embodiment of the present invention is a manufacturing method for manufacturing an electronic device, characterized in that the manufacturing method includes: a first step of forming a film on a first surface of a substrate; a second step of sealing the film after the first step; and a third step of measuring the thickness of the film after the first step and before the second step, while the substrate is held by a first electrostatic chuck in a state where the first surface of the substrate on which the film is formed in the first step faces the gravity direction, wherein in the first step, the film is formed on the first surface of the substrate while the substrate is held by a second electrostatic chuck different from the first electrostatic chuck in a state where the first surface of the substrate faces the gravity direction, the substrate having a deflection shape that is convex on one side in the gravity direction, the first electrostatic chuck including a first holding surface that holds the substrate on a second surface of the substrate on the opposite side to the first surface, the second electrostatic chuck including a second holding surface that holds the substrate on a second surface of the substrate on the opposite side to the first surface, the first holding surface of the first electrostatic chuck having a surface shape closer to the deflection shape of the substrate than the second holding surface of the second electrostatic chuck.
[0014] As another embodiment of the present invention, a film forming device is characterized in that the film forming device comprises: a film forming chamber for forming a film on a first surface of a substrate; an electrostatic chuck for holding the substrate in a manner such that the first surface of the substrate faces the direction of gravity; and a measuring unit for measuring the thickness of the film formed on the first surface of the substrate while the substrate is held by the electrostatic chuck before sealing the film formed on the first surface of the substrate, the electrostatic chuck comprising a holding surface for holding the substrate on a second surface of the substrate on an opposite side to the first surface, the holding surface having a surface shape that is convex on one side in the direction of gravity.
[0015] As another embodiment of the present invention, the film forming method is characterized in that the film forming method comprises: a first step of forming a film on a first surface of a substrate; a second step of sealing the film after the first step; and a third step of measuring the thickness of the film after the first step and before the second step while holding the substrate with the first surface of the substrate on which the film is formed in the first step facing the direction of gravity by an electrostatic chuck, the electrostatic chuck comprising a holding surface which holds the substrate on a second surface of the substrate opposite to the first surface, the holding surface having a surface shape which is convex on one side in the direction of gravity.
[0016] Effects of the Invention
[0017] According to the present invention, for example, a new technology which is advantageous for holding a substrate by an electrostatic chuck can be provided.
[0018] Further objects or other aspects of the present invention will become apparent from the following embodiments described with reference to the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 FIG. 1 is a diagram schematically showing a configuration of a film forming system including a film forming apparatus as one embodiment of the present invention.
[0020] Figure 2 It is a diagram schematically showing the structure of a film forming apparatus.
[0021] Figure 3 It is a diagram schematically showing the structure of a passage chamber.
[0022] Figure 4 This is a diagram showing an example of an alignment mark provided on a substrate.
[0023] Figure 5 It is a diagram for explaining the principle of measurement processing by the film thickness measurement unit.
[0024] Figure 6This is a diagram showing a state where a deflected substrate is held by a substrate holding portion.
[0025] 7(A) and (B) are diagrams showing the structure of a substrate holding portion in this embodiment.
[0026] Figure 8 It is a diagram schematically showing the structure of a film thickness control system in a film forming system.
[0027] Fig. 9 (A) and (B) are diagrams for explaining an organic EL display device as an electronic device. DETAILED DESCRIPTION
[0028] Hereinafter, the embodiments are described in detail with reference to the accompanying drawings. In addition, the following embodiments do not limit the invention involved in the claims. Although multiple features are described in the embodiments, these multiple features are not all necessary for the invention, and multiple features can be combined arbitrarily. Moreover, in the accompanying drawings, the same or similar structures are marked with the same figure numbers, and repeated descriptions are omitted.
[0029] Figure 1 1 is a diagram schematically showing the structure (layout) of a film forming system 100 having a film forming device as one embodiment of the present invention. The film forming system 100 is a system that performs film forming processing on a substrate that has been brought in, and carries out the substrate that has been film-formed. The film forming system 100 is configured as a manufacturing line for electronic devices, for example, and a plurality of film forming systems 100 may be arranged in parallel. In addition, in each of the following figures, arrow Z indicates the up-down direction (direction of gravity), and arrows X and Y indicate mutually orthogonal horizontal directions.
[0030] The film forming system 100 (film forming device) is particularly suitable as a system for manufacturing organic light-emitting elements such as OLEDs and organic photoelectric conversion elements such as organic thin-film solar cells. As electronic devices, for example, light-emitting elements, photoelectric conversion elements, touch panels, etc. can be listed. In this embodiment, the electronic device includes a display device having a light-emitting element (such as an organic EL display device), a lighting device (such as an organic EL lighting device), a sensor having a photoelectric conversion element (such as an organic COMS image sensor), etc.
[0031] In this embodiment, the film forming system 100 is implemented as a system for manufacturing a display panel of an organic EL display device for a smartphone or a display panel of an organic EL display device for a VR HMD. In the case of manufacturing a display panel for a smartphone, a 4.5-generation substrate (about 700 mm×about 900 mm), a 6-generation full-size substrate (about 1500 mm×about 1850 mm), or a half-cut size substrate (about 1500 mm×about 925 mm) is used. On such a substrate, film formation is performed to form an organic EL element, and the substrate is punched to manufacture a plurality of small-sized panels. In addition, in the case of manufacturing a display panel for a VR HMD, a silicon wafer of a specified size (for example, 300 mm) is used. On such a silicon wafer, film formation is performed to form an organic EL element, and the silicon wafer is punched along the area between the element formation areas (the scribe area) to manufacture a plurality of small-sized panels. However, the size and type of the substrate are not particularly limited and can be set appropriately.
[0032] like Figure 1 As shown, the film forming system 100 has a structure in which a plurality of group-type units (hereinafter also referred to as "units") CU1 to CU3 are connected via a connecting chamber. Here, the group-type unit refers to a film forming unit having a structure in which a plurality of film forming devices are arranged around a substrate conveying robot serving as a substrate conveying unit. In addition, in the present embodiment, the film forming system 100 has three units CU1 to CU3, but the number of units is not limited. Hereinafter, in the description common to all units and the description of uncertain units, reference numerals marked with "x" instead of numbers are used, such as "CUx", and in the description of individual units, reference numerals marked with numbers are used, such as "CU1". In addition, the same applies to the reference numerals for structures other than the marked units.
[0033] In addition, Figure 1 , a film forming system 100 as a part of the entire manufacturing line of electronic devices including a film forming device is shown. Upstream of the film forming system 100 (film forming device), for example, a substrate storage tank, a heating device, a cleaning device and other pre-processing devices may be provided. In addition, downstream of the film forming system 100 (film forming device), for example, a sealing device, a processing device, a storage tank for processed substrates and the like may be provided.
[0034] Unit CUx has a transfer chamber TRx arranged in the center, a plurality of film forming chambers EVx1 to EVx4 (film forming devices) and mask chambers MSx1 to MSx2 arranged around the transfer chamber TRx. Two adjacent units CUx and CUx+1 are connected by a connecting chamber CNx. In unit CUx, the transfer chamber TRx, the film forming chambers EVx1 to EVx4, the mask chambers MSx1 to MSx2 and the connecting chamber CNx are spatially connected, and the interior thereof is maintained in a vacuum or inert gas atmosphere such as nitrogen. In the present embodiment, each chamber constituting unit CUx and connecting chamber CNx is connected to a vacuum pump (not shown), and each chamber can be independently evacuated. Each chamber is also referred to as a "vacuum chamber" or simply a "chamber". In the present embodiment, "vacuum" (state) refers to a state filled with a gas having a pressure lower than the atmospheric pressure, that is, a decompressed state.
[0035] In the transport chamber TRx, a transport robot RRx is provided as a transport unit for transporting the substrate S and the mask M. The transport robot RRx is, for example, a multi-joint robot having a structure in which a manipulator for holding the substrate S or the mask M is mounted on a multi-joint arm. In the unit CUx, the substrate S is transported by transport units such as the transport robot RRx and the transport robot RCx while maintaining a horizontal state in which the film forming surface S1 (first surface) of the film forming the substrate S is oriented in the direction of gravity (-Z direction (downward)). The manipulator constituting the transport robot RRx or the transport robot RCx holds, for example, the peripheral area of the film forming surface S1 of the substrate S. The transport robot RRx transports the substrate S between the passage chamber PSx-1 on the upstream side, the film forming chambers EVx1 to EVx4, and the buffer chamber BCx on the downstream side. In addition, the transport robot RRx transports the mask M between the mask chamber MSx1 and the film forming chambers EVx1 and EVx2, and transports the mask M between the mask chamber MSx2 and the film forming chambers EVx3 and EVx4. The manipulator constituting the transport robot RRx or the transport robot RCx performs the prescribed actions respectively according to the program stored in the transport control unit. The prescribed actions are set to efficiently transport the plurality of substrates S when the film forming process is performed on the plurality of substrates S sequentially or simultaneously in parallel in the plurality of film forming chambers or units. In addition, the position of the substrate S on the transport path may deviate from the ideal transport position due to errors in the movement of the manipulator, for example, caused by changes in the degree of deflection of the multi-joint arm. In this case, it is sufficient to fine-tune the movement of the manipulator by correcting the program for controlling the movement of the manipulator as needed.
[0036] The mask chambers MSx1 and MSx2 are chambers provided with mask stockers for storing masks M for film forming processing and masks M for film forming processing, respectively. Mask chamber MSx1 stores masks M used in film forming chambers EVx1 and EVx3, for example, and mask chamber MSx2 stores masks M used in film forming chambers EVx2 and EVx4, for example. As the mask M, for example, a metal mask having a plurality of openings is used.
[0037] The film forming chambers EVx1 to EVx4 are chambers for performing a process of forming a film (material layer) by evaporating (attaching) an evaporation substance on the film forming surface S1 of the substrate S, that is, a film forming process (evaporation process). In the present embodiment, the film forming chamber EVx1 and the film forming chamber EVx3 are chambers with the same function (chambers capable of performing the same film forming process), and the film forming chamber EVx2 and the film forming chamber EVx4 are chambers with the same function. Thus, the film forming process of the first path from the film forming chamber EVx1 to the film forming chamber EVx2 and the film forming process of the second path from the film forming chamber EVx3 to the film forming chamber EVx4 can be performed in parallel.
[0038] The connection chamber CNx has the function of connecting the unit CUx and the unit CUx+1, and delivering the substrate S that has been film-formed by the unit CUx to the subsequent unit CUx+1. In the present embodiment, the connection chamber CNx is composed of a buffer chamber BCx, a vortex chamber TCx, and a passage chamber PSx in sequence from the upstream side. Such a structure of the connection chamber CNx is advantageous from the perspective of productivity and availability of the film-forming device. However, the connection chamber CNx is not limited to such a structure, and the connection chamber CNx may also be composed of only the buffer chamber BCx or the passage chamber PSx.
[0039] The buffer chamber BCx is a chamber for conveying (handing over) substrates S between the conveying robot RRx provided in the unit CUx and the conveying robot RCx provided in the connection chamber CNx. The buffer chamber BCx temporarily accommodates a plurality of substrates S when there is a difference in processing speed between the unit CUx and the subsequent unit CUx+1, or when the substrates S cannot be conveyed due to a failure on the downstream side. Thus, the buffer chamber BCx realizes the function of adjusting the conveying speed and conveying time of the substrates S relative to the subsequent unit CUx+1. By providing the buffer chamber BCx having such a function in the connection chamber CNx, it is possible to realize high flexibility in laminated film formation corresponding to various layer structures while realizing high productivity. For example, a substrate storage rack (also called a "box") having a multi-stage structure may be provided in the buffer chamber BCx. The multi-stage structure is capable of accommodating a plurality of substrates S while maintaining a horizontal state in which the film forming surface S1 of the substrate S is oriented in the direction of gravity (-Z direction (downward). In addition, a lifting mechanism may be provided in the buffer chamber BCx. The lifting mechanism lifts and lowers the substrate storage rack in order to match the stage of the substrate S being carried in or out with the transport position.
[0040] The vortex chamber TCx is a chamber for rotating the orientation of the substrate S by 180 degrees. A conveying robot RCx for conveying (handing over) the substrate S from the buffer chamber BCx to the passage chamber PSx is provided in the vortex chamber TCx. Here, the end on the upstream side of the substrate S is referred to as the "rear end" and the end on the downstream side is referred to as the "front end". The conveying robot RCx rotates 180 degrees while maintaining the state of the substrate S received by the buffer chamber BCx and hands it over to the passage chamber PSx, thereby exchanging the front end and the rear end of the substrate S between the buffer chamber BCx and the passage chamber PSx. Therefore, since the unit CUx on the upstream side and the unit CUx+1 on the downstream side have the same orientation relative to the orientation when the substrate S is carried into the film forming chamber, the scanning direction of the film forming process relative to the substrate S and the orientation of the mask M can be made consistent in each unit CUx. Therefore, in each unit CUx, the orientation of the mask M set in the mask chambers MSx1~MSx2 can be made consistent, which can simplify the management of the mask M and improve the usability.
[0041] The passage chamber PSx is a chamber (handover chamber) for conveying (handing over) the substrate S between the conveying robot RCx provided in the connection chamber CNx and the conveying robot RRx+1 provided in the unit CUx+1 on the downstream side. In the present embodiment, in the passage chamber PSx, an alignment (positioning) process of the substrate S and a measurement process of measuring the thickness (film thickness) of the film formed on the film forming surface S1 of the substrate S are performed. Therefore, an alignment mechanism for performing the alignment process of the substrate S and a film thickness measuring unit for performing the measurement process are provided in the same chamber (passage chamber PSx).
[0042] Between the film forming chambers EVx1 to EVx4, the mask chambers MSx1 to MSx2, the transfer chamber TRx, the buffer chamber BCx, the swirl chamber TCx, and the passage chamber PSx, doors (gate valves or gate valves) that can be opened and closed may be provided, or they may be always open.
[0043] Figure 2 : is a diagram schematically showing the structure of a film forming device 200 arranged in film forming chambers EVx1 to EVx4. The film forming device 200 is implemented as a vacuum evaporation device for performing a film forming process, in which the evaporation material emitted from the evaporation source is evaporated on the film forming surface S1 of the substrate S to form a film. The film forming device 200 can form a thin film of the evaporation material of a predetermined pattern on the substrate S via a mask M. In the present embodiment, the substrate S has a rectangular shape. As the material of the substrate S, glass, resin, metal, etc. can be appropriately selected, and a material having a resin layer such as polyimide formed on glass is particularly preferred. As the evaporation material, an organic material or an inorganic material (such as a metal, a metal oxide), etc. can be used.
[0044] like Figure 2As shown, the film forming apparatus 200 includes: a mask holding portion 201 for holding a mask M; a substrate holding portion 202 for holding a substrate S; a vapor deposition source unit 203; a moving mechanism 204; a film forming rate monitor 205; and a film forming control portion 206. The mask holding portion 201, the substrate holding portion 202, the vapor deposition source unit 203, the moving mechanism 204, and the film forming rate monitor 205 are accommodated in a vacuum chamber 207. The film forming apparatus 200 further includes an alignment mechanism (not shown) that moves at least one of the mask holding portion 201 and the substrate holding portion 202 to perform an alignment process on the mask M held by the mask holding portion 201 and the substrate S held by the substrate holding portion 202.
[0045] The substrate holding portion 202 holds the substrate S in such a manner that the film forming surface S1 (first surface) of the film formed on the substrate S faces the gravity direction (-Z direction (downward direction)). In the present embodiment, the substrate holding portion 202 is configured as an electrostatic chuck (second electrostatic chuck) that adsorbs the substrate S using electrostatic force. The substrate S held by the substrate holding portion 202 is placed on the upper surface of the mask M held in a horizontal state by the mask holding portion 201 with the film forming surface S1 facing downward. However, as long as the structure is such that the substrate S and the mask M are sufficiently close to each other, the substrate S does not need to be placed on the upper surface of the mask M. In addition, a magnet (not shown) may be arranged close to the back side S2 (second surface) on the opposite side of the film forming surface S1 of the substrate S, and the mask M (mask foil) may be attracted to the substrate S by the magnetic force of the magnet, thereby improving the closeness of the mask M to the substrate S.
[0046] A vapor deposition source unit 203 is provided below the mask M. The vapor deposition source unit 203 includes, for example, a container (crucible) for containing vapor deposition materials, a heater for heating the vapor deposition materials contained in the container, etc. In addition, the vapor deposition source unit 203 also includes a reflector, a heat transfer member, a baffle, etc. for improving the heating efficiency of the vapor deposition materials contained in the container as needed.
[0047] The moving mechanism 204 supports the vapor deposition source unit 203 and moves (scans) it in a direction (Y direction) parallel to the film forming surface S1 of the substrate S. The moving mechanism 204 is configured as a one-axis moving mechanism in this embodiment, but may be configured as a two-axis or more moving mechanism.
[0048] In addition, in this embodiment, if Figure 2 As shown in the figure, the evaporation source unit 203 is set to one, but a plurality of evaporation source units (containers for accommodating evaporation materials) can also be arranged and configured to move as a whole. According to this structure, since different evaporation materials can be accommodated and released for each evaporation source unit (container), a mixed film or a laminated film can be formed on the film forming surface S1 of the substrate S.
[0049] The film formation rate monitor 205 is a sensor for monitoring the film formation speed of a thin film formed (filmed) on the film formation surface S1 of the substrate S. The film formation rate monitor 205 is, for example, a crystal oscillation film formation rate monitor, including a crystal oscillator that moves together with the evaporation source unit 203. The film formation rate monitor 205 estimates the film formation rate (evaporation rate) based on the change in the resonant frequency (natural vibration number) caused by the evaporation material discharged from the evaporation source unit 203 accumulating on the surface of the crystal oscillator (giving mass). The film formation rate is the amount of evaporation material attached to the substrate S per unit time.
[0050] The film forming control unit 206 controls (the operation of) each component of the film forming apparatus 200. The film forming control unit 206 is composed of, for example, a computer (information processing device) including a processor represented by a CPU, a memory such as a RAM and a ROM, and various interfaces. The film forming control unit 206 realizes various operations and processes in the film forming apparatus 200 by reading out the program stored in the ROM in the RAM and executing it.
[0051] The film forming control unit 206 controls the film forming rate based on the film forming rate estimated by the film forming rate monitor 205. Or the thickness of the film (film thickness) measured by the film thickness measuring unit 310, adjust (control) the film forming time [s] so that the thickness of the film formed on the film forming surface S1 of the substrate S becomes the target value. The film forming time is adjusted by changing the moving speed (scanning speed) of the evaporation source unit 203 performed by the moving mechanism 204. However, the release amount (evaporation amount) of the evaporation material can also be adjusted (controlled) by changing the heater temperature, the shutter opening, etc. in the evaporation source unit 203 so that the thickness of the film formed on the film forming surface S1 of the substrate S becomes the target value. In addition, the film forming control unit 206 can also combine the adjustment of the film forming time and the adjustment of the release amount so that the thickness of the film formed on the film forming surface S1 of the substrate S becomes the target value. In other words, the film forming control unit 206 adjusts (controls) at least one of the scanning speed, the heater temperature and the shutter opening of the evaporation source unit 203 so that the thickness of the film formed on the film forming surface S1 of the substrate S becomes the target value.
[0052] Figure 3 is a diagram schematically showing the structure of the passage chamber PSx, corresponding to Figure 1AA section shown. As described above, an alignment mechanism for performing alignment processing of the substrate S is provided in the passage chamber PSx. The substrate S transported to the passage chamber PSx via the transfer chamber TRx or the cyclotron chamber TCx has a deviation (position offset) caused by the position accuracy of the robot used in the transport of the substrate S. In the present embodiment, the position offset of the substrate S can be reduced (suppressed) by the alignment mechanism provided in the passage chamber PSx. The alignment mechanism includes: a driving unit 302 for driving the substrate holding unit 301 provided in the vacuum chamber 300 in the X direction, the Y direction and the θ direction (rotation direction around the Z axis); a camera 305; and an alignment control unit 306. The camera 305 captures the substrate S (alignment mark 304) through a window 303 provided at the lower part (bottom surface) of the vacuum chamber 300 and obtains image data. The alignment control unit 306 obtains the position information (position offset) of the substrate S arranged in the vacuum chamber 300 based on the image data obtained by the camera 305. In addition, the alignment control unit 306 moves the substrate S through the driving unit 302 based on the position information of the substrate S.
[0053] like Figure 3 As shown, the substrate holding portion 301 includes a base material 3011 (main body member) and a holding portion 3012, and holds the substrate S in a manner such that the film forming surface S1 of the substrate S faces the gravity direction (-Z direction (downward)). The base material 3011 has a rectangular shape when viewed from above, and supports the holding portion 3012. The holding portion 3012 is a member including a holding surface 3012A (first holding surface), and the holding surface 3012A holds the substrate S on the back side S2 on the opposite side of the film forming surface S1 of the substrate S. In the present embodiment, the holding portion 3012 is configured as an electrostatic chuck (first electrostatic chuck) that adsorbs the substrate S using electrostatic force.
[0054] When the substrate S is held by the substrate holding part 301 by the transfer robot RCx provided in the cyclotron chamber TCx, the alignment mark 304 of the substrate S is photographed by the camera 305 to obtain image data. The alignment control part 306 detects the position and inclination of the alignment mark 304 based on the image data obtained by the camera 305, thereby obtaining the position offset and rotation offset of the substrate S. Then, the alignment control part 306 controls the driving part 302 to move the substrate S so as to reduce the position offset and rotation offset of the substrate S, thereby performing the alignment process of the substrate S.
[0055] Here, when the substrate S is subjected to film forming processing in the film forming chambers EVx1 to EVx4, it is necessary to align the substrate S and the mask M with high precision. Therefore, in the film forming chambers EVx1 to EVx4, the substrate S is subjected to ultra-high precision alignment processing called fine alignment. In the present embodiment, as described above, by pre-aligning the substrate S in the passage chamber PSx (rough alignment), the initial positional deviation when the substrate S is transported to the film forming chamber of the subsequent unit CUx+1 is suppressed. Thus, the time required for fine alignment in the film forming chamber can be shortened.
[0056] Figure 4 : is a diagram showing an example of an alignment mark 304 provided on a substrate S. The alignment mark 304 is provided, for example, at two corners on the rear end side of the substrate S, respectively. However, the alignment mark 304 may be provided at a corner on the front end side of the substrate S, or at two or four diagonal corners, or at a position along the edge of the substrate S instead of at a corner of the substrate S. In addition, the number of the alignment mark 304 is not limited and is arbitrary. In addition, instead of providing the alignment mark 304 on the substrate S, the position offset and rotation offset of the substrate S may be obtained by detecting the edge or corner of the substrate S.
[0057] In addition, a film thickness measuring unit 310 is provided in the passage chamber PSx. The film thickness measuring unit 310 is used to measure the thickness (film thickness) of the film formed on the film forming surface S1 of the substrate S. Figure 3 As shown, the film thickness measuring unit 310 is provided as one, but a plurality of film thickness measuring units 310 may be provided. By using a plurality of film thickness measuring units 310 to measure the film thickness of a plurality of locations at once, it is possible to evaluate the deviation of the film thickness within the substrate surface or to collectively evaluate a plurality of films formed in a plurality of film forming chambers.
[0058] In this embodiment, the film thickness measurement unit 310 measures the thickness of the film formed on the substrate S by detecting the reflectivity of the surface of the substrate S using an optical sensor. Figure 3 As shown in FIG. 1 , the sensor head 312 includes a film thickness evaluation unit 311, a sensor head 312, and an optical fiber 313 connecting the sensor head 312 and the film thickness evaluation unit 311. The sensor head 312 is disposed below the substrate holding portion 301 provided in the vacuum chamber 300, and is connected to the optical fiber 313 via a vacuum flange 314 installed on the lower part (bottom surface) of the vacuum chamber 300. The sensor head 312 has a function of setting the irradiation area of the light guided via the optical fiber 313 to a predetermined area, and is composed of optical components such as an optical fiber, a pinhole, and a lens.
[0059] Figure 5This is a diagram for explaining the principle of the measurement process based on the film thickness measurement unit 310. The film thickness evaluation unit 311 includes a light source 320, a spectrometer 321, and a measurement control unit 322. The light source 320 is a device including, for example, a deuterium lamp, a xenon lamp, or a halogen lamp, and outputs measurement light having a wavelength in the range of 200nm to 1μm. The spectrometer 321 is a device that detects the spectrum (intensity of each wavelength) by spectroscopically analyzing the reflected light from the substrate S (film formed on the substrate S) input from the sensor head 312. The spectrometer 321 is composed of, for example, a spectroscopic element (grating, prism, etc.), a detector that performs photoelectric conversion, and the like. The measurement control unit 322 performs control based on the light source 320, calculations for calculating the film thickness based on the spectrum detected by the spectrometer 321, and the like.
[0060] The measurement light output from the light source 320 is guided to the sensor head 312 via the optical fiber 313, and irradiated to the substrate S from the sensor head 312. The reflected light (measurement light) reflected by the substrate S is input to the spectrometer 321 from the sensor head 312 via the optical fiber 313. Here, the light reflected from the surface of the film formed on the film-forming surface S1 of the substrate S and the light reflected at the interface between the film and its base layer interfere with each other. In this way, due to the influence of the interference (and absorption) generated by the film formed on the film-forming surface S1 of the substrate S, the spectrum of the reflected light is affected by the difference in optical path length, that is, the thickness (film thickness) of the film formed on the film-forming surface S1 of the substrate S. Therefore, in the measurement control unit 322, by analyzing the spectrum of the reflected light detected by the spectrometer 321, the thickness (film thickness) of the film formed on the film-forming surface S1 of the substrate S can be calculated.
[0061] Such a film thickness measurement (evaluation) based on the reflection spectroscopy method can be performed in a short time and with high precision for organic films with a thickness of several nm to several hundred nm, and therefore can also be used for organic films (organic layers) of organic EL display devices, etc. Here, as materials for the organic film, hole transport materials such as αNPD: α-naphthylphenylbenzenediamine, and luminescent materials such as Ir(ppy)3: iridium-phenylpyrimidine complexes can be listed. In addition, as materials for the organic film, electron transport materials such as Alq3: tris(8-quinolinone)aluminum, Liq: 8-hydroxyquinolinone-lithium can also be listed. In addition, the film thickness measurement based on the reflection spectroscopy method can also be applied to mixed films of the above materials.
[0062] In addition, in this embodiment, if Figure 4As shown, the film thickness measuring section 310 measures the thickness (film thickness) of the film for film thickness measurement formed in the film thickness measurement region 330, that is, the measurement patch 331. On the substrate S (film forming surface S1), the film thickness measurement region 330 is provided at a position different from the element forming region 340 where electronic devices such as a display panel are formed, for example, at the front end of the substrate S. When film forming is performed in each film forming chamber, the film thickness measurement region 330 (predetermined portion) is also film-formed in parallel with the film forming in the element forming region 340, so that the measurement patch 331 as a film for film thickness measurement is formed in the film thickness measurement region 330. This can be easily achieved by forming an opening for forming the measurement patch 331 in the mask M used in each film forming chamber.
[0063] The film thickness measurement region 330 can be set to an area in which a plurality of measurement patches 331 can be formed, and the formation position of the measurement patches 331 can be changed according to the film unit to be measured for the film thickness. For example, when it is desired to measure the thickness (film thickness) of a film (a laminated film in which a single film or a plurality of films are laminated) formed in one film forming chamber, only the film (a single film or a laminated film) formed in one film forming chamber is formed in the film thickness measurement region 330 as the measurement patch 331. In addition, when it is desired to measure the thickness (film thickness) of a laminated film formed through a plurality of film forming chambers, a laminated film identical to the laminated film to be measured is formed in the film thickness measurement region 330 as the measurement patch 331. In this way, by making the measurement patch 331 different (formed) for each film to be measured, the thickness (film thickness) of the film to be measured can be accurately measured.
[0064] Here, as described above, consider the state where the substrate S is held by the substrate holding portion 301 in the passage chamber PSx ( Figure 3 ) and measuring the thickness of the film formed on the substrate S by the film thickness measuring unit 310. The substrate S that has been subjected to the film forming process sometimes has a curved shape that is convex on one side in the direction of gravity. The holding force (adsorption force) of the electrostatic chuck depends on the distance between the electrostatic chuck and the object to be held (substrate). If the distance between the electrostatic chuck and the substrate is wide, the holding force for holding (adsorption) the substrate is small, and it is difficult to hold the substrate. When the substrate S having a curved shape is held by the holding unit 3012 of the substrate holding unit 301, as Figure 6 As shown, sufficient holding force (adsorption force) cannot be applied to the substrate S. In this case, in order to match the substrate S with the holding surface 3012A of the holding portion 3012, it is necessary to gradually adsorb the substrate S from the end portion onto the holding surface 3012A, which takes time. In addition, there is also the possibility that the substrate S itself cannot be held. Figure 6 This is a diagram showing a state in which the deflected substrate S is held by the substrate holding portion 301 (holding portion 3012 ).
[0065] Therefore, in the present embodiment, as shown in FIG. 7(A) and FIG. 7(B), in the holding portion 3012, a holding surface 3012A having a surface shape that is convex on one side in the direction of gravity is specified based on the substrate S having a curved shape that is convex on one side in the direction of gravity. For example, in the holding portion 3012, a holding surface 3012A having a surface shape that is closer to the curved shape of the substrate S than the holding surface 202A (second holding surface) specified by the substrate holding portion 202 provided in the film forming chamber (film forming device 200) (i.e., compared to the holding surface 202A) is specified. More preferably, in the holding portion 3012, a holding surface 3012A having a surface shape that is consistent with the curved shape of the substrate S is specified.
[0066] By defining the holding surface 3012A having such a surface shape, as shown in FIG. 7(A) and FIG. 7(B), the distance between the substrate S and the electrostatic chuck (holding surface 3012A) becomes closer, and a sufficient holding force (adsorption force) can be applied to the substrate S. Thus, even if the substrate S has a curved shape, the substrate S can be matched with the holding surface 3012A in a short time (quickly). Therefore, in the present embodiment, in the passage chamber PSx, the substrate S can be reliably and quickly held at a low voltage by the substrate holding portion 301. FIG. 7(A) and FIG. 7(B) are diagrams showing the structure of the substrate holding portion 301 in the present embodiment.
[0067] As described above, the holding portion 3012 is configured as an electrostatic chuck that attracts the substrate S by electrostatic force. Specifically, as shown in FIG7(A), the chuck region CR (electrostatic chuck) that functions as the holding portion 3012 and attracts the back side S2 of the substrate S by electrostatic force may be provided to cover the entire surface of the holding surface 3012A (base material 3011). In addition, as shown in FIG7(B), a plurality of chuck regions CR that function as the holding portion 3012 and attract the back side S2 of the substrate S by electrostatic force may be provided in a matrix on the holding surface 3012A.
[0068] Thus, in this embodiment, the holding surface 3012A having a surface shape that is convex on one side in the direction of gravity is defined in the holding portion 3012 of the substrate holding portion 301. Thus, even a substrate S having a curved shape that is convex on one side in the direction of gravity can be held by the substrate holding portion 301 (holding portion 3012) without increasing the voltage applied to the electrostatic chuck. Therefore, the element forming region 340 forming electronic devices such as a display panel will not be damaged due to the high voltage applied to the electrostatic chuck, and it does not take time to remove the charge, which is advantageous in terms of cycle time.
[0069] In addition, in the measurement process of measuring the thickness of the film formed on the substrate S, it is sufficient as long as the reflected light from the substrate S can be detected (monitored) by the film thickness measuring unit 310. Therefore, the holding surface 3012A defined by the holding portion 3012 of the substrate holding portion 301 may also have a surface shape close to the bending shape of the substrate S. On the other hand, in the film forming process, within the range of ensuring the uniformity of the thickness of the film formed on the substrate S, the substrate holding portion 301 may be used instead of the substrate holding portion 202 that holds the substrate S. In other words, the holding surface 202A defined by the substrate holding portion 202 may also have a surface shape that is convex on one side in the direction of gravity within the range of ensuring the uniformity of the thickness of the film formed on the substrate S.
[0070] In addition, the surface shape to be specified as the holding surface 3012A of the holding portion 3012 of the substrate holding portion 301, that is, the deflection shape of the substrate S can be obtained by experimentally performing a film forming process or simulation in advance to form a film on the substrate S. Since the deflection shape of the substrate S varies depending on the type (material) or thickness of the film formed on the substrate S, the film forming conditions, the type or thickness of the substrate S, etc., it is necessary to obtain the deflection shape according to these conditions.
[0071] In each film forming chamber (film forming device 200), as described above, the thickness (film forming rate) of the film formed using the film forming rate monitor 205 is controlled to a target value of the film forming rate. However, the film forming rate monitor 205 does not directly measure the thickness of the film formed on the substrate S, but indirectly measures the film forming rate through a crystal oscillator arranged at a position different from the substrate S. Therefore, depending on various error factors such as the amount of deposited material deposited on the crystal oscillator, the temperature of the crystal oscillator, etc., the film thickness of the film deposited on the crystal oscillator of the film forming rate monitor 205 and the film thickness of the film deposited on the substrate S are sometimes different. In addition, the film forming rate estimated by the film forming rate monitor 205 itself sometimes produces an error. In this case, a deviation in the film thickness occurs in the film formed on the substrate S, resulting in a decrease in quality and a decrease in yield.
[0072] Therefore, in this embodiment, the thickness of the measuring patch 331 formed on the substrate S (film thickness measurement area 330) is measured by the film thickness measurement unit 310, and the film forming conditions of each film forming chamber are controlled according to the measurement result, thereby achieving high-precision film thickness control. Here, the film forming conditions include, for example, the scanning speed of the evaporation source unit 203, the heater temperature, and the shutter opening. When controlling the film forming conditions, both the film forming rate estimated by the film forming rate monitor 205 and the measurement result obtained by the film thickness measurement unit 310 can also be used. The film forming rate monitor 205 that evaluates the accumulation amount of the evaporated material deposited on the crystal oscillator and the film thickness measurement unit 310 that optically evaluates the thickness of the film formed on the substrate S have different measurement principles, so the evaluation results obtained for interference, environment, changes in the film forming state, etc. are different. By combining such different evaluation results, more reliable film thickness control can be performed.
[0073] Figure 8 : is a diagram schematically showing the structure of a film thickness control system in the film forming system 100. The film thickness control unit 350 sends a control instruction for controlling the film forming conditions to the film forming control unit 206 of each film forming chamber based on the measurement result of the film thickness measuring unit 310. The control of the film forming conditions is roughly divided into feedback control and feedforward control. Feedback control is a control in which the film thickness control unit 350 controls the film forming conditions in the film forming chamber on the upstream side of the film thickness measuring unit 310 to adjust the thickness (film thickness) of the film formed on the subsequent substrate Ss. Feedforward control is a control in which the film thickness control unit 350 controls the film forming conditions in the film forming chamber on the downstream side of the film thickness measuring unit 310 to adjust the thickness (film thickness) of the film formed on the substrate S through the subsequent film forming process. The film thickness control unit 350 can implement only one of the feedback control and the feedforward control, or can implement both of the controls. In addition, it can also be set for each film forming chamber or each unit whether to implement feedback control or feedforward control.
[0074] Next, a method for manufacturing an electronic device using the film forming apparatus 200 (film forming system 100 including the film forming apparatus 200) in this embodiment will be described. Here, an organic EL display device will be described as an example of an electronic device.
[0075] First, an organic EL display device will be described. Fig. 9 (A) is a diagram showing the overall structure of an organic EL display device 50 . Fig. 9 (B) is a diagram showing a cross-sectional structure of one pixel of the organic EL display device 50 .
[0076] like Fig. 9As shown in (A), the organic EL display device 50 has a display area 51 in which pixels 52 including a plurality of light-emitting elements are arranged in a matrix. As described later, each of the plurality of light-emitting elements has a structure having an organic layer (organic film) clamped by a pair of electrodes. In addition, in the present embodiment, a pixel refers to the smallest unit capable of displaying a specified color in the display area 51. For example, in the organic EL display device 50, a pixel 52 is composed of a combination of a first light-emitting element 52R, a second light-emitting element 52G and a third light-emitting element 52B capable of displaying colors different from each other. The pixel 52 is generally composed of a combination of a red light-emitting element, a green light-emitting element and a blue light-emitting element, but is not limited thereto. For example, it can be composed of a combination of a yellow light-emitting element, a cyan light-emitting element and a white light-emitting element, or it can be composed of light-emitting elements of at least one color.
[0077] Fig. 9 (B) Yes Fig. 9 (A) is a partial cross-sectional view of the AB line shown. The pixel 52 is composed of an organic EL element having an anode 54, a hole transport layer 55, any one of the light-emitting layers 56R, 56G and 56B, an electron transport layer 57 and a cathode 58 on a substrate 53. Among them, the hole transport layer 55, the light-emitting layers 56R, 56G and 56B and the electron transport layer 57 are equivalent to organic layers. In addition, in the present embodiment, the light-emitting layer 56R is an organic EL layer that emits red light, the light-emitting layer 56G is an organic EL layer that emits green light, and the light-emitting layer 56B is an organic EL layer that emits blue light. The light-emitting layers 56R, 56G and 56B are respectively formed into patterns corresponding to light-emitting elements (sometimes also recorded as organic EL elements) that emit red light, green light and blue light. In addition, the anode 54 is formed separately for each light-emitting element. The hole transport layer 55, the electron transport layer 57 and the cathode 58 can be formed together with a plurality of light-emitting layers 56R, 56G and 56B, or can be formed for each light-emitting element. In order to prevent the anode 54 and the cathode 58 from being short-circuited by foreign matter, an insulating layer 59 is provided between the electrodes. Furthermore, since the organic EL layer is degraded by moisture or oxygen, a protective layer PL is provided to protect the organic EL element from moisture or oxygen.
[0078] exist Fig. 9 In (B), the hole transport layer 55 and the electron transport layer 57 are shown as one layer, but they can also be formed by a plurality of layers including a hole blocking layer and an electron blocking layer according to the structure of the organic EL element. In addition, a hole injection layer having an energy band structure for smoothly injecting holes from the anode 54 to the hole transport layer 55 can also be formed between the anode 54 and the hole transport layer 55. Similarly, an electron injection layer can also be formed between the cathode 58 and the electron transport layer 57.
[0079] Hereinafter, a method for manufacturing an organic EL display device will be described.
[0080] First, a circuit (not shown) for driving the organic EL display device and a substrate 53 on which an anode 54 is formed are prepared.
[0081] Next, an acrylic resin is formed by spin coating on the substrate 53 with the anode 54 formed thereon, and patterned by photolithography to form an opening in the portion of the acrylic resin with the anode 54 formed thereon, thereby forming an insulating layer 59. This opening corresponds to a light emitting region where the light emitting element actually emits light.
[0082] The substrate 53 patterned with the insulating layer 59 is carried into the film forming device 200 (first film forming chamber) of the film forming system 100, and the hole transport layer 55 is formed as a common layer on the anode 54 of the display area 51. The hole transport layer 55 is formed by vacuum evaporation, for example. The hole transport layer 55 is actually formed in a larger size than the display area 51, so a high-precision mask is not required.
[0083] Next, the substrate 53 formed up to the hole transport layer 55 is carried into the film forming apparatus 200 (second film forming chamber). The substrate 53 and the mask are aligned, and the red light emitting layer 56R is formed on the portion of the substrate 53 where the red light emitting element is formed via the mask.
[0084] Similar to the film formation of the light-emitting layer 56R, the light-emitting layer 56G emitting green light is formed in the film forming device 200 (third film forming chamber), and the light-emitting layer 56B emitting blue light is formed in the film forming device 200 (fourth film forming chamber). After the light-emitting layers 56R, 56G, and 56B are formed, the electron transport layer 57 is formed on the entire display region 51 in the film forming device 200 (fifth film forming chamber). The electron transport layer 57 is formed as a common layer of the three light-emitting layers 56R, 56G, and 56B.
[0085] Next, the substrate 53 on which the electron transport layer 57 has been formed is carried into the film forming apparatus 200 (sixth film forming chamber), and the cathode 58 is formed into a film.
[0086] Then, the substrate 53 formed up to the cathode 58 is carried into a sealing device, and a protective layer PL is formed by plasma CVD (sealing process), thereby completing the organic EL display device 50. Here, the protective layer PL is formed by CVD, but the present invention is not limited thereto. For example, the protective layer PL may be formed by ALD or inkjet.
[0087] In addition, if the substrate 53 is exposed to an atmosphere containing moisture or oxygen during the period from when the substrate 53 having the insulating layer 59 patterned thereon is carried into the film forming apparatus 200 to when the protective layer PL is formed, the light-emitting layer composed of the organic EL material may be degraded. Therefore, it is preferable to carry the substrate 53 into or out of the film forming apparatus in a vacuum atmosphere or an inert gas atmosphere.
[0088] The present invention is not limited to the above-described embodiments, and various changes and modifications can be made without departing from the spirit and scope of the invention. Therefore, claims are appended to disclose the scope of the invention.
[0089] Description of Reference Numerals
[0090] CU1, CU2, CU3: group type units; EV11~EV14, EV21~EV24, EV31~EV34: film forming chambers; RR1, RR2, RR3: transfer robots; CN1, CN2: connection chambers; PS1, PS2: passage chambers; S: substrate; 100: film forming system; 200: film forming device; 301: substrate holding portion; 3012: holding portion; 3012A: holding surface.
Claims
1. A manufacturing method is a manufacturing method for manufacturing an electronic device, characterized in that: The manufacturing method has the following features: In a first step, a film is formed on a first surface of a substrate; a second step of sealing the film after the first step; as well as a third step of measuring the thickness of the film after the first step and before the second step, while holding the substrate by a first electrostatic chuck in a state where the first surface of the substrate on which the film is formed in the first step faces the direction of gravity, The first electrostatic chuck includes a first holding surface, the first holding surface holding the substrate on a second surface of the substrate opposite to the first surface. The first holding surface has a surface shape that is convex on one side in the direction of gravity.
2. The manufacturing method according to claim 1, characterized in that: In the third step, the thickness of the film is measured in a delivery chamber for delivering the substrate carried out from a film forming chamber for forming the film.
3. The manufacturing method according to claim 1, characterized in that: In the first step, the film is formed on the first surface of the substrate while the substrate is held by a second electrostatic chuck different from the first electrostatic chuck so that the first surface of the substrate faces the gravity direction.
4. The manufacturing method according to claim 3, characterized in that: The second electrostatic chuck includes a second holding surface that holds the substrate at a second surface of the substrate opposite to the first surface.
5. The manufacturing method according to claim 4, characterized in that: The substrate has a curved shape that is convex on one side in the direction of gravity, The first holding surface of the first electrostatic chuck has a surface shape closer to a deflected shape of the substrate than the second holding surface of the second electrostatic chuck.
6. The manufacturing method according to claim 1, characterized in that: The first holding surface of the first electrostatic chuck is provided with a region for adsorbing the second surface of the substrate by electrostatic force so as to cover the entire surface of the first holding surface.
7. The manufacturing method according to claim 1, characterized in that: A plurality of regions for adsorbing the second surface of the substrate by electrostatic force are provided in a matrix on the first holding surface of the first electrostatic chuck.
8. The manufacturing method according to claim 1, characterized in that: The film comprises an organic film, The electronic device includes an organic EL element.
9. A manufacturing method, which is a manufacturing method for manufacturing an electronic device, characterized in that: The manufacturing method has the following features: In a first step, a film is formed on a first surface of a substrate; a second step of sealing the film after the first step; as well as a third step of measuring the thickness of the film after the first step and before the second step, while holding the substrate by a first electrostatic chuck in a state where the first surface of the substrate on which the film is formed in the first step faces the direction of gravity, In the first step, the film is formed on the first surface of the substrate while the substrate is held by a second electrostatic chuck different from the first electrostatic chuck so that the first surface of the substrate faces the gravity direction. The substrate has a curved shape that is convex on one side in the direction of gravity, The first electrostatic chuck includes a first holding surface, the first holding surface holding the substrate on a second surface of the substrate opposite to the first surface. The second electrostatic chuck includes a second holding surface for holding the substrate on a second surface of the substrate opposite to the first surface. The first holding surface of the first electrostatic chuck has a surface shape closer to a deflected shape of the substrate than the second holding surface of the second electrostatic chuck.
10. A film forming device, characterized in that: The film forming device comprises: a film forming chamber, for forming a film on a first surface of a substrate; an electrostatic chuck for holding the substrate in a manner that the first surface of the substrate faces a direction of gravity; as well as a measuring unit that measures a thickness of the film formed on the first surface of the substrate while the substrate is held by the electrostatic chuck before the film formed on the first surface of the substrate is sealed, The electrostatic chuck includes a holding surface that holds the substrate on a second surface of the substrate opposite to the first surface. The holding surface has a surface shape that is convex on one side in the direction of gravity.
11. A film forming method, characterized in that: The film forming method has the following features: In a first step, a film is formed on a first surface of a substrate; a second step of sealing the film after the first step; as well as a third step of measuring the thickness of the film after the first step and before the second step, while holding the substrate with the first surface of the substrate on which the film is formed in the first step facing the direction of gravity by an electrostatic chuck; The electrostatic chuck includes a holding surface that holds the substrate on a second surface of the substrate opposite to the first surface. The holding surface has a surface shape that is convex on one side in the direction of gravity.