Washable crease-free shirt and manufacturing method thereof

By using double-sided adhesive lining strips in the shirt for stitching bonding and high-temperature flat pressing, combining high-iron-iron yarn and formaldehyde-free fabric finishing technology, the problem of shrinkage and wrinkling of shirts after washing is solved, achieving high-reliance Hot and crisp shirt design.

CN118947978APending Publication Date: 2024-11-15LUTAI TEXTILE
View PDF 0 Cites 2 Cited by

Patent Information

Application Number
CN202411057365.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-02
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

Existing non-iron shirts are prone to shrink and wrinkle after multiple washes, and the wrinkle problem caused by sutures has not been effectively solved, making it difficult to maintain a flat and crisp appearance, affecting the performance and quality of taking.

Method used

Double-sided adhesive lining is used for sewing bonding, and flat pressing it through a high-temperature three-dimensional flat press, combining tightly spun high-iron-iron yarn, low-reducing strength bleaching and dyeing technology, formaldehyde-free fabric free ironing and finishing technology, and environmentally friendly ready-to-wear No-ironing and atomization finishing treatment to ensure that the seams of the shirt are flat and wrinkle-free.

Benefits of technology

It achieves the high degree of ironing, deformation and wrinkle of the shirt. It can wash it up to 50-100 times, and has the effect of high clarity, high wear resistance, soft and comfortable, beautiful and generous.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118947978A_ABST
    Figure CN118947978A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of textile fabrics, and particularly relates to a washable crease-free shirt and a manufacturing method thereof. The washable and crease-free shirt comprises a garment piece, shoulder pieces, sleeves, sleeve caps, a collar and sleeve qis, and double-faced adhesive tape lining strips are arranged at the sewing parts and are flatly pressed and bonded; the double-faced adhesive tape lining cloth is adhered to the top fly, so that all sewing seam parts of the shirt are smooth, wrinkle-free and soft. The fabric adopts compact spinning high non-ironing yarns, a bleaching and dyeing process with low drop strength and a formaldehyde-free non-ironing finishing process with high capillary effect and high permeability and instantaneous water absorption. The sewn shirt is subjected to environment-friendly, safe and formaldehyde-free garment non-ironing atomization finishing, a non-ironing finishing agent is added into 30-40 times of water to be evenly mixed, and the non-ironing finishing agent is atomized and sprayed to the shirt through an atomizer; baking the shirt sprayed with the non-ironing treatment agent by using a baking machine; the washable and crease-free shirt can be obtained. According to the manufacturing method of the washable and wrinkle-free shirt, the manufactured shirt is comfortable to touch, elastic, green, environmentally friendly and renewable.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of textile fabrics, and in particular relates to a washable and wrinkle-free shirt and a manufacturing method thereof. Background Art

[0002] With the progress of society, the development of science and technology and the improvement of living standards, people's clothing consumption concepts and market demands have changed significantly. The requirements for shirts are not only durable, beautiful, but also pursue the comfort, health, safety and environmental protection of textiles. Non-iron shirts have good flatness, but the existing non-iron shirts have the disadvantages of large shrinkage, easy wrinkling and poor shape retention after repeated washing, and cannot maintain a flat and crisp appearance, which greatly affects the wearing performance and quality of the shirts.

[0003] Patent CN109577004A discloses a method for processing shirts containing linen or regenerated cellulose fibers, including fabric processing and garment processing. Fabric processing includes: yarn preparation, yarn dyeing, yarn softening, drying, winding, warping, sizing, weaving, cloth preparation, singeing, desizing, mercerizing, shaping, and preshrinking; garment processing includes: cloth preparation, cutting, sewing, pre-washing, drying, spraying, pre-drying, pressing, baking, moisture regain, washing, drying, buttoning, ironing, and packaging; the yarn is too soft and the dyed fabric is treated with polyethylene wax emulsion.

[0004] Patent CN111074631A discloses a method for free-ironing finishing of cotton and linen garments, including the steps of alkali washing, stacking, dispensing, preparing, dipping, squeezing, pre-drying and moisture setting, shaping and pressing, baking and shaping, and free-ironing finishing post-processing of the cotton and linen garments.

[0005] Patent CN106436298A discloses a water-absorbing, moisture-conducting, environmentally friendly, wrinkle-resistant and non-ironing finishing liquid for shirts, which is used to finish shirt fabrics. The finishing liquid is prepared from the following raw materials: butane tetracarboxylic acid, ammonium citrate, triethanolamine, malic acid, sodium hypochlorite, tackified acid, diphenyl disulfonic acid derivatives, amino silicone oil, silane coupling agent KH550, chitosan, N,N-dimethylformamide, fatty alcohol polyoxyethylene-5-ether, an appropriate amount of maleic anhydride, an appropriate amount of sodium dodecyl sulfate, and an appropriate amount of deionized water.

[0006] Patent CN108618221A discloses a method for preparing a non-ironing, washable, shrink-resistant knitted garment, comprising: cleaning the knitted fabric until the surface is smooth and hair-free, and then making the garment; treating the garment with a resin finishing liquid; pre-drying the garment, and controlling the moisture content of the garment after pre-drying; positioning ironing the garment; baking the garment after positioning ironing to obtain a non-ironing, washable, shrink-resistant knitted garment. The knitted garment has the advantages of ultra-low shrinkage, no fading, excellent appearance flatness after washing, anti-pilling and precise control of garment size.

[0007] The above methods only involve wrinkle-free finishing of fabrics or ready-made garments, but do not mention the wrinkle problem caused by the seams of shirts, and the number of washable times cannot be guaranteed. Summary of the invention

[0008] The technical problem to be solved by the present invention is to overcome the above-mentioned defects of the prior art and provide a method for making a washable and wrinkle-free shirt. The produced shirt is comfortable to touch, elastic, green, environmentally friendly and renewable.

[0009] The washable and wrinkle-free shirt of the present invention comprises a garment piece, a shoulder piece, a sleeve, a sleeve head, a collar, and a sleeve flap. The bottom edge of the stitching parts of the garment piece, the shoulder piece, and the sleeve are bonded with a double-sided adhesive lining strip with a width of 0.5-1.2 cm; the two stitching parts of the sleeve head, the collar, and the sleeve flap are bonded with a double-sided adhesive lining strip with a width of 0.5-1.0 cm; the stitching parts are all bonded by a high-temperature three-dimensional flat press, the temperature is 150-170°C, the time is 6-12s, and the pressure is 3.0-4.5mpa; the garment piece comprises a front piece and a back piece, the shoulder piece comprises a shoulder surface and a shoulder lining, and the front piece is divided into two parts by a placket, and the placket is bonded with a double-sided adhesive lining cloth. All the stitching parts of the shirt are smooth, wrinkle-free, and soft. The fabric adopts compactly spun high-iron-free yarn, a low-strength-reducing bleaching and dyeing process, high-wool efficiency, high-penetration instantaneous water absorption, and a formaldehyde-free fabric iron-free finishing process. After sewing, the shirt is then subjected to environmentally friendly and safe formaldehyde-free ready-made garment non-ironing atomization finishing. The non-ironing finishing agent is added to 30-40 times of water and mixed evenly, and then sprayed on the shirt with an atomizer; the shirt sprayed with the non-ironing treatment agent is baked in a baking machine; and a washable and wrinkle-free shirt can be obtained. The washable and wrinkle-free shirt is completed by the steps of non-ironing yarn, non-ironing fabric, ready-made garment non-ironing, and wrinkle-free treatment of ready-made garment seams. It adopts a green and environmentally friendly formaldehyde-free non-ironing process, saves water, energy, and reduces emissions, and achieves the best washable and wrinkle-free functionality; the shirt made by the present invention has a simple structure, beautiful appearance, safety and environmental protection, and the production method is scientific, reasonable, simple and easy.

[0010] The method for making the washable and wrinkle-free shirt comprises sewing and ironing-free atomization finishing of the ready-made garment.

[0011] Sewing involves the following steps:

[0012] ① The front placket is sewn with a sewing machine with a tug, and the trumpet with double-sided adhesive lining is sewn. The width of the double-sided adhesive lining is consistent with the width of the placket, 2-5cm;

[0013] ② Use an automatic over-shoulder machine to sew the back piece, over-shoulder surface and over-shoulder lining together. The over-shoulder machine is equipped with a speaker with a double-sided adhesive lining strip. The width of the double-sided adhesive lining strip is 0.5-1.2cm;

[0014] ③Add 0.8-1.2cm double-sided adhesive lining strips to the shoulder seams of the front and back pieces and sew them together;

[0015] ④ Use a sleeve sewing machine to sew the sleeves at the armhole, and add a 0.5-1.2cm double-sided adhesive lining strip at the armhole;

[0016] ⑤ The sleeve side seams and body side seams are sewn with a corbel fitting machine. The corbel fitting machine is equipped with a trumpet with a double-sided adhesive lining strip. The sleeve seams and body side seams are added with a double-sided adhesive lining strip, and the lining strip width is 0.5-1.2cm;

[0017] ⑥ The bottom edge rolling process uses Durkopp bottom edge equipment. The Durkopp equipment is equipped with a speaker with a double-sided adhesive lining strip. The bottom edge is added with a double-sided adhesive lining strip with a width of 0.5-1.0cm;

[0018] ⑦ The collar and sleeves are made by automatic template machine, and 0.5-1.0 double-sided adhesive lining strips are added around the collar and sleeves;

[0019] ⑧ For large sleeves, double-sided adhesive lining is used, and for small sleeves, 0.5-1.0 double-sided adhesive lining strip is added.

[0020] The steps of the non-ironing atomization finishing of ready-made clothes are: firstly, the non-ironing finishing liquid is used to make the liquid carrying rate reach 15-20%, and then baking is performed to obtain a washable and wrinkle-free shirt.

[0021] The non-ironing finishing liquid is used to treat the ready-made clothes in a spray finishing manner.

[0022] The baking is done using a shirt baking machine.

[0023] The baking temperature is 120-150°C and the baking time is 3-5 minutes.

[0024] The non-ironing finishing liquid includes modified N-hydroxymethyl dihydroxyethylene urea formaldehyde-free resin, 90-150g / L, preferably Raycare CR-ZFF (Lurui Fine Chemicals); non-ironing finishing resin synergist 50-80g / L, preferably heat-reactive polyurethane Hydroperm RPU-N.CN n (Archroma Chemicals); catalyst 20-50g / L, preferably metal salt mixture Raycare CT-FF (Lurui Fine Chemicals), used in conjunction with formaldehyde-free resin Raycare CR-ZFF, can achieve zero formaldehyde addition non-ironing effect on pure cotton and blended fabrics; softener 15-60g / L, preferably Raysoft-LR9960.

[0025] Specifically, the method for making the washable and wrinkle-free shirt includes sewing and ironing-free atomization finishing of the ready-made garment;

[0026] Sewing involves the following steps:

[0027] ① The front placket is sewn with a sewing machine with a tug, and the trumpet with double-sided adhesive lining is sewn. The width of the double-sided adhesive lining is consistent with the width of the placket, 2-5cm;

[0028] ② Use an automatic over-shoulder machine to sew the back piece, over-shoulder surface and over-shoulder lining together. The over-shoulder machine is equipped with a speaker with a double-sided adhesive lining strip. The width of the double-sided adhesive lining strip is 0.5-1.2cm;

[0029] ③Add 0.8-1.2cm double-sided adhesive lining strips to the shoulder seams of the front and back pieces and sew them together;

[0030] ④ Use a sleeve sewing machine to sew the sleeves at the armhole, and add a 0.5-1.2cm double-sided adhesive lining strip at the armhole;

[0031] ⑤ The sleeve side seams and body side seams are sewn with a corbel fitting machine. The corbel fitting machine is equipped with a trumpet with a double-sided adhesive lining strip. The sleeve seams and body side seams are added with a double-sided adhesive lining strip, and the lining strip width is 0.5-1.2cm;

[0032] ⑥ The bottom edge rolling process uses Durkopp bottom edge equipment. The Durkopp equipment is equipped with a speaker with a double-sided adhesive lining strip. The bottom edge is added with a double-sided adhesive lining strip with a width of 0.5-1.0cm;

[0033] ⑦ The collar and sleeves are made by automatic template machine, and 0.5-1.0 double-sided adhesive lining strips are added around the collar and sleeves;

[0034] ⑧ For large sleeves, double-sided adhesive lining is used, and for small sleeves, 0.5-1.0 double-sided adhesive lining strip is added.

[0035] The steps for the non-ironing atomization finishing of ready-made garments are as follows:

[0036] ① Use a non-ironing finishing liquid to spray finish, so that the liquid rate reaches 15-20%, and then bake to obtain a washable and wrinkle-free shirt; the non-ironing finishing liquid includes 90-150g / L of modified N-hydroxymethyl dihydroxyethylene urea formaldehyde-free resin; 50-80g / L of resin synergist; 20-50g / L of catalyst; and 15-60g / L of softener.

[0037] ② Bake the shirt sprayed with the non-ironing treatment agent in a baking machine at 120-150℃ for 3-5 minutes.

[0038] Compared with the prior art, the present invention has the following beneficial effects:

[0039] (1) The method for making a washable and wrinkle-free shirt of the present invention is simple, easy to implement, scientific and reasonable, green, safe, environmentally friendly, and water-saving and energy-saving.

[0040] (2) The washable and wrinkle-free shirt prepared by the method of the present invention can achieve a non-ironing property of the seams and the fabric of level 4 or above, and can be washed 50-100 times without deformation or wrinkling. It has high non-ironing property, high stiffness, high wear resistance, and is soft, comfortable, and beautiful. BRIEF DESCRIPTION OF THE DRAWINGS

[0041] Figure 1 Schematic diagram of a washable and wrinkle-free shirt according to the present invention. DETAILED DESCRIPTION

[0042] The present invention will be further described below in conjunction with specific embodiments.

[0043] The raw materials and additives used in the following examples and comparative examples are all commercially available products.

[0044] Example 1

[0045] The washable and wrinkle-free shirt includes a garment piece, a shoulder piece, a sleeve, a sleeve head, a collar, and a sleeve flap. The bottom edge of the stitching parts of the garment piece, shoulder piece, and sleeve are bonded with a double-sided adhesive lining strip with a width of 0.5 cm; the two stitching parts of the sleeve head, collar, and sleeve flap are bonded with a double-sided adhesive lining strip with a width of 0.5 cm; the stitching parts are all bonded by a high-temperature three-dimensional flat press at a temperature of 150°C, a time of 12s, and a pressure of 4.5MPa; the garment piece includes a front piece and a back piece, the shoulder piece includes a shoulder surface and a shoulder lining, and the front piece is divided into two parts by a placket, and the placket is bonded with a double-sided adhesive lining cloth. This makes all the stitching and seams of the shirt smooth, wrinkle-free, and soft. The fabric uses compactly spun high-iron-free yarn, a low-strength bleaching and dyeing process, high wool efficiency, high penetration instant water absorption, and a formaldehyde-free fabric iron-free finishing process.

[0046] The method for making the washable and wrinkle-free shirt includes sewing and ironing-free atomization finishing of the ready-made shirt;

[0047] Sewing involves the following steps:

[0048] ① The front placket is sewn with a sewing machine with a tug, and the trumpet with double-sided adhesive lining is sewn. The width of the double-sided adhesive lining is consistent with the width of the placket, 2cm;

[0049] ② Use an automatic shoulder-pulling machine to sew the back piece, shoulder surface and shoulder lining together. The shoulder-pulling machine is equipped with a speaker with a double-sided adhesive lining strip. The width of the double-sided adhesive lining strip is 0.5cm;

[0050] ③Add 0.8cm double-sided adhesive lining strips to the shoulder seams of the front and back pieces and sew them together;

[0051] ④ Use a sleeve sewing machine to sew the sleeves at the armhole, and add a 0.5cm double-sided adhesive lining strip at the armhole;

[0052] ⑤ The sleeve side seams and body side seams are sewn with a corbel fitting machine. The corbel fitting machine is equipped with a trumpet with a double-sided adhesive lining. The sleeve seams and body side seams are equipped with a double-sided adhesive lining, and the lining width is 0.5cm;

[0053] ⑥ The bottom edge rolling process uses the Durkopp bottom edge equipment. The Durkopp equipment is equipped with a speaker with a double-sided adhesive lining strip. The bottom edge is added with a double-sided adhesive lining strip with a width of 0.5cm;

[0054] ⑦ The collar and sleeves are made by automatic template machine, and 0.5mm double-sided adhesive lining strips are added around the collar and sleeves;

[0055] ⑧ The large sleeves are bonded with double-sided adhesive lining cloth, and the small sleeves are added with 0.5 double-sided adhesive lining strip.

[0056] For the shirts made in the above steps, all the parts with lining or lining strips must be pressed and bonded by a high-temperature three-dimensional flat press at a temperature of 150°C, a time of 12 seconds, and a pressure of 4.5 MPa. This will make the double-sided adhesive lining or double-sided adhesive lining strip completely melted. The seams will be smooth, wrinkle-free and soft.

[0057] The steps for the non-ironing atomization finishing of ready-made garments are as follows:

[0058] ① Use a non-ironing finishing liquid to spray finish, so that the liquid rate reaches 15%, and then bake to obtain a washable and wrinkle-free shirt; the non-ironing finishing liquid includes modified N-hydroxymethyl dihydroxyethylene urea formaldehyde-free resin CR-ZFF 90g / L; resin enhancer RPU-N 50g / L; catalyst Raycare CT-FF 20g / L; softener Raysoft-LR996015g / L.

[0059] ② Bake the shirt sprayed with the non-ironing treatment agent in a baking machine at 150°C for 3 minutes.

[0060] The shirt made with the above steps is washable and wrinkle-free, the ironing resistance of the seams and fabrics can reach above level 4, and it can be washed up to 50 times without losing its shape or wrinkles.

[0061] Example 2

[0062] The washable and wrinkle-free shirt includes a garment piece, a shoulder piece, a sleeve, a sleeve head, a collar, and a sleeve flap. The bottom edge of the stitching parts of the garment piece, shoulder piece, and sleeve are bonded with a double-sided adhesive lining strip with a width of 1.0 cm; the two stitching parts of the sleeve head, collar, and sleeve flap are bonded with a double-sided adhesive lining strip with a width of 1.0 cm; the stitching parts are all bonded by a high-temperature three-dimensional flat press at a temperature of 160°C, a time of 7 seconds, and a pressure of 3.5 MPa; the garment piece includes a front piece and a back piece, the shoulder piece includes a shoulder surface and a shoulder lining, and the front piece is divided into two parts by a placket, and the placket is bonded with a double-sided adhesive lining cloth. This makes all the stitching and seams of the shirt smooth, wrinkle-free, and soft. The fabric uses compactly spun high-iron-free yarn, a low-strength bleaching and dyeing process, high wool efficiency, high penetration instant water absorption, and a formaldehyde-free fabric iron-free finishing process.

[0063] The method for making the washable and wrinkle-free shirt includes sewing and ironing-free atomization finishing of the ready-made shirt;

[0064] Sewing involves the following steps:

[0065] ① The front placket is sewn with a sewing machine with a tug, and the trumpet with double-sided adhesive lining is sewn. The width of the double-sided adhesive lining is consistent with the width of the placket, 3.5cm;

[0066] ② Use an automatic shoulder-pulling machine to sew the back piece, shoulder surface and shoulder lining together. The shoulder-pulling machine is equipped with a speaker with a double-sided adhesive lining strip. The width of the double-sided adhesive lining strip is 1.0cm;

[0067] ③Add 1.0cm double-sided adhesive lining strips to the shoulder seams of the front and back pieces and sew them together;

[0068] ④ Use a sleeve sewing machine to sew the sleeves at the armhole, and add a 1.0 cm double-sided adhesive lining at the armhole;

[0069] ⑤ The sleeve side seams and body side seams are sewn with a corbel fitting machine. The corbel fitting machine is equipped with a trumpet with a double-sided adhesive lining. The sleeve seams and body side seams are equipped with a double-sided adhesive lining, and the lining width is 1.0cm;

[0070] ⑥ The bottom edge rolling process uses the Durkopp bottom edge equipment. The Durkopp equipment is equipped with a speaker with a double-sided adhesive lining strip. The bottom edge is added with a double-sided adhesive lining strip with a width of 0.8cm;

[0071] ⑦ The collar and sleeves are made by automatic template machine, and 0.8 double-sided adhesive lining strips are added around the collar and sleeves;

[0072] ⑧ The large sleeves are bonded with double-sided adhesive lining cloth, and the small sleeves are added with 0.8 double-sided adhesive lining strip.

[0073] For the shirts made in the above steps, all the parts with lining or lining strips must be pressed and bonded by a high-temperature three-dimensional flat press at a temperature of 160°C, a time of 7 seconds, and a pressure of 3.5 MPa. This will make the double-sided adhesive lining or double-sided adhesive lining strip completely melted. The seams will be smooth, wrinkle-free and soft.

[0074] The steps for the non-ironing atomization finishing of ready-made garments are as follows:

[0075] ① Use a non-ironing finishing liquid to spray finish, so that the liquid rate reaches 18%, and then bake to obtain a washable and wrinkle-free shirt; the non-ironing finishing liquid includes modified N-hydroxymethyl dihydroxyethylene urea formaldehyde-free resin CR-ZFF 120g / L; resin enhancer RPU-N 60g / L; catalyst Raycare CT-FF 30g / L; softener Raysoft-LR996040g / L.

[0076] ② Bake the shirt sprayed with the non-ironing treatment agent in a baking machine at 140°C for 4 minutes.

[0077] The shirt made with the above steps is washable and wrinkle-free, the ironing resistance of the seams and fabrics can reach above level 4, and it can be washed up to 80 times without losing shape or wrinkling.

[0078] Example 3

[0079] The washable and wrinkle-free shirt includes a garment piece, a shoulder piece, a sleeve, a sleeve head, a collar, and a sleeve flap. The bottom edge of the stitching parts of the garment piece, shoulder piece, and sleeve are bonded with a double-sided adhesive lining strip with a width of 1.2 cm; the two stitching parts of the sleeve head, collar, and sleeve flap are bonded with a double-sided adhesive lining strip with a width of 1.0 cm; the stitching parts are all bonded by a high-temperature three-dimensional flat press at a temperature of 170°C, a time of 6 seconds, and a pressure of 4.5 MPa; the garment piece includes a front piece and a back piece, the shoulder piece includes a shoulder surface and a shoulder lining, and the front piece is divided into two parts by a placket, and the placket is bonded with a double-sided adhesive lining cloth. This makes all the stitching and seams of the shirt smooth, wrinkle-free, and soft. The fabric uses compactly spun high-iron-free yarn, a low-strength bleaching and dyeing process, high wool efficiency, high penetration instantaneous water absorption, and a formaldehyde-free fabric iron-free finishing process.

[0080] The method for making the washable and wrinkle-free shirt includes sewing and ironing-free atomization finishing of the ready-made shirt;

[0081] Sewing involves the following steps:

[0082] ① The front placket is sewn with a sewing machine with a tug, and the trumpet with double-sided adhesive lining is sewn. The width of the double-sided adhesive lining is consistent with the width of the placket, 5cm;

[0083] ② Use an automatic over-shoulder machine to sew the back piece, over-shoulder surface and over-shoulder lining together. The over-shoulder machine is equipped with a speaker with a double-sided adhesive lining strip. The width of the double-sided adhesive lining strip is 1.2cm;

[0084] ③Add 1.2cm double-sided adhesive lining strips to the shoulder seams of the front and back pieces and sew them together;

[0085] ④ Use a sleeve sewing machine to sew the sleeves at the armhole, and add a 1.2cm double-sided adhesive lining at the armhole;

[0086] ⑤ The sleeve side seams and body side seams are sewn with a corbel fitting machine. The corbel fitting machine is equipped with a trumpet with a double-sided adhesive lining. The sleeve seams and body side seams are equipped with a double-sided adhesive lining, and the lining width is 1.2cm;

[0087] ⑥ The bottom edge rolling process uses the Durkopp bottom edge equipment. The Durkopp equipment is equipped with a speaker with a double-sided adhesive lining. The bottom edge is added with a double-sided adhesive lining, and the lining width is 1.0cm;

[0088] ⑦ The collar and sleeves are made by automatic template machine, and 1.0 double-sided adhesive lining strips are added around the collar and sleeves;

[0089] ⑧ The large sleeves are bonded with double-sided adhesive lining cloth, and the small sleeves are added with 1.0 double-sided adhesive lining strip.

[0090] For the shirts made in the above steps, all the parts with lining or lining strips must be pressed and bonded by a high-temperature three-dimensional flat press at a temperature of 170°C, a time of 6 seconds, and a pressure of 3.0 MPa. This will make the double-sided adhesive lining or double-sided adhesive lining strip completely melted. The seams will be smooth, wrinkle-free and soft.

[0091] The steps for the non-ironing atomization finishing of ready-made garments are as follows:

[0092] ① The method comprises spraying a non-ironing finishing liquid to make the liquid carrying rate reach 20%, and then baking to obtain a washable and wrinkle-free shirt; the non-ironing finishing liquid comprises 150 g / L of modified N-hydroxymethyl dihydroxyethylene urea formaldehyde-free resin CR-ZFF; 80 g / L of resin synergist RPU-N; 50 g / L of catalyst Raycare CT-FF; and 60 g / L of softener Raysoft-LR9960.

[0093] ② Bake the shirt sprayed with the non-ironing treatment agent in a baking machine at 150°C for 3 minutes.

[0094] The shirt made with the above steps is washable and wrinkle-free, and the ironing resistance of the seams and fabrics can reach level 4. It can be washed up to 100 times without losing its shape or wrinkles.

[0095] Of course, the above contents are only preferred embodiments of the present invention and cannot be considered to limit the scope of the embodiments of the present invention. The present invention is not limited to the above examples, and equal changes and improvements made by ordinary technicians in the technical field within the essential scope of the present invention should all fall within the scope of the patent coverage of the present invention.

Claims

1. A washable and wrinkle-free shirt, characterized by: It comprises a garment piece, a yoke piece, a sleeve, a sleeve head, a collar and a sleeve flap. The bottom edges of the stitching parts of the garment piece, the yoke piece and the sleeve are bonded with a double-sided adhesive lining strip with a width of 0.5-1.2 cm; the two stitching parts of the sleeve head, the collar and the sleeve flap are bonded with a double-sided adhesive lining strip with a width of 0.5-1.0 cm; the stitching parts are bonded by flat pressing with a three-dimensional flat press at a temperature of 150-170°C, a time of 6-12s and a pressure of 3.0-4.5MPa; the garment piece comprises a front piece and a back piece, the yoke piece comprises a yoke surface and a yoke lining, the front piece is divided into two parts by a placket, and the placket is bonded with a double-sided adhesive lining cloth.

2. A method for making a washable and wrinkle-free shirt according to claim 1, characterized in that: Including sewing and non-ironing atomization finishing of ready-made garments.

3. The method for making a washable and wrinkle-free shirt according to claim 2, characterized in that: Sewing involves the following steps: ① The front placket is sewn with a sewing machine with a tug, and the trumpet with double-sided adhesive lining is sewn. The width of the double-sided adhesive lining is consistent with the width of the placket, 2-5cm; ② Use an automatic over-shoulder machine to sew the back piece, over-shoulder surface and over-shoulder lining together. The over-shoulder machine is equipped with a speaker with a double-sided adhesive lining strip. The width of the double-sided adhesive lining strip is 0.5-1.2cm; ③Add 0.8-1.2cm double-sided adhesive lining strips to the shoulder seams of the front and back pieces and sew them together; ④ Use a sleeve sewing machine to sew the sleeves at the armhole, and add a 0.5-1.2cm double-sided adhesive lining strip at the armhole; ⑤ The sleeve side seams and body side seams are sewn with a corbel fitting machine. The corbel fitting machine is equipped with a trumpet with a double-sided adhesive lining strip. The sleeve seams and body side seams are added with a double-sided adhesive lining strip, and the lining strip width is 0.5-1.2cm; ⑥ The bottom edge rolling process uses the Durkopp bottom edge equipment. The Durkopp equipment is equipped with a speaker with a double-sided adhesive lining strip. The bottom edge is added with a double-sided adhesive lining strip with a width of 0.5-1.0cm; ⑦ The collar and sleeves are hooked with an automatic template machine, and 0.5-1.0 double-sided adhesive lining strips are added around the collar and sleeves; ⑧ For large sleeves, double-sided adhesive lining is used, and for small sleeves, 0.5-1.0 double-sided adhesive lining strip is added.

4. The method for making a washable and wrinkle-free shirt according to claim 2, characterized in that: The steps of the non-ironing atomization finishing of ready-made clothes are: firstly, the non-ironing finishing liquid is used to make the liquid carrying rate reach 15-20%, and then baking is performed to obtain a washable and wrinkle-free shirt.

5. The method for making a washable and wrinkle-free shirt according to claim 4, characterized in that: The non-ironing finishing liquid is used to treat the ready-made clothes in a spray finishing manner.

6. The method for making a washable and wrinkle-free shirt according to claim 4, characterized in that: The baking is done using a shirt baking machine.

7. The method for making a washable and wrinkle-free shirt according to claim 4, characterized in that: The baking temperature is 120-150°C and the baking time is 3-5 minutes.

8. The method for making a washable and wrinkle-free shirt according to claim 4, characterized in that: The non-ironing finishing liquid comprises 90-150 g / L of modified N-methylol dihydroxy ethylene urea formaldehyde-free resin, 50-80 g / L of resin synergist, 20-50 g / L of catalyst, and 15-60 g / L of softener.

Citation Information

Cited By

  • Production process for preventing easy-care shirts from bubbling

    CN120021813A

  • Production technology for preventing blistering of iron-free shirts

    CN120021813B