Preparation method of corn stigma extract
Through a method including crushing, water extraction, filtration, fine filtration, concentration and spray drying, the problems of corn shaving resource waste and extract stability are solved, efficient and natural corn shaving extract preparation is achieved, and market products are improved categories and health benefits.
Patent Information
- Application Number
- CN202411010579.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-26
- Publication Date
- 2024-11-15
AI Technical Summary
Corn shavings are underutilized as by-products, resulting in waste of resources. At the same time, the market demand for food raw materials with physiological functions has increased, and there is a lack of effective utilization methods.
A method of preparing corn styre extract, including crushing, water extraction, filtration, fine filtration, concentration, ingredients and ultra-high temperature sterilization, improve the extraction efficiency and purity by modifying the reverse osmosis membrane, and finally obtain corn styres by spray drying. Extract.
It realizes efficient utilization of corn silk resources, improves the yield and total flavonoids of the extract, ensures the naturalness of the extract and the retention of active ingredients, and enhances the stability and ease of use of the product.
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of plant extract preparation and relates to a method for preparing a corn silk extract. Background Art
[0002] Corn silk is the dried style and stigma of corn, a grass plant. It is listed as a commonly used medicinal material in the 1985 edition of the "Medicinal Material Standards of the Ministry of Health of the People's Republic of China". Studies have found that corn silk contains a variety of functional ingredients such as polysaccharides, flavonoids, saponins, alkaloids, phytosterols, cryptoxanthin and organic acids, and has a variety of biological activities, such as lowering blood sugar, lowering blood lipids, regulating immunity, anti-oxidation, antibacterial, and diuretic.
[0003] my country is a major agricultural producer with an annual corn output that is very abundant. However, corn silk, a by-product of corn, is not fully utilized and is usually discarded as waste, resulting in a large amount of resource waste.
[0004] With the acceleration of modern life pace, unreasonable eating habits have caused many physiological and metabolic diseases. In addition, people's demands for their own health are increasing day by day. Some food ingredients with physiological functions have become the hot spots of research and development in the food industry, and corn silk is one of them.
[0005] Based on the current status of development and utilization of corn silk resources and consumers' health demands, it is planned to use corn silk as raw material to develop corn silk extract products, and apply them to food, beverages and health products. This not only solves the problem of corn silk resource waste, but also enriches the product categories in the market, which is of great benefit to people's health. Summary of the invention
[0006] The purpose of the present invention is to provide a method for preparing a corn silk extract, which has the characteristics of simple process and high yield of the prepared product.
[0007] The purpose of the present invention can be achieved through the following technical solutions:
[0008] A method for preparing a corn silk extract comprises the following steps:
[0009] S1. Crushing: crushing the corn silk raw material by a crusher;
[0010] S2, extraction: at a temperature of 95-98 ° C, the crushed corn silk and reverse osmosis drinking pure water in a mass ratio of 1:12 were mixed and extracted once, and the mixture was filtered through a 300-mesh stainless steel filter after 2 hours of extraction, and the filtrate was collected once, and the temperature was cooled to ≤40 ° C, and reverse osmosis drinking pure water was continued to be added to make the material-liquid ratio 1:8, and a second extraction was performed, and the mixture was filtered through a 300-mesh stainless steel filter after 2 hours of extraction, and the second filtrate was collected, and the two filtrates were combined to obtain the material after the extraction was completed, and the temperature was cooled to ≤40 ° C;
[0011] S3, filtration: After the extraction is completed, the material is filtered through a stainless steel filter and centrifuged to remove slag to obtain an extraction liquid;
[0012] S4, fine filtration: the leaching liquid is filtered through a fine filter membrane with a pore size of 10 μm and 2 μm or ultrafiltered through an ultrafiltration membrane with a pore size of 200 nm to obtain a fine filtrate;
[0013] S5, concentration: the refined filtrate is concentrated through a modified reverse osmosis membrane RO membrane, and the concentration is completed when the concentration reaches 2.0-8.0 Brix to obtain a concentrated solution;
[0014] S6. Compounding: Add maltodextrin in an amount of 4 times the mass of the solid content of the concentrated solution to the concentrated solution to obtain a concentrated prepared solution;
[0015] S7, ultra-high temperature sterilization: sterilize the above concentrated preparation liquid through ultra-high temperature sterilization equipment;
[0016] S8, spray drying: drying the sterilized concentrated formulation into powder through a spray drying device to obtain the corn silk extract.
[0017] As a preferred technical solution of the present invention, in step S1, the corn silk raw material is crushed to a particle size of 60 meshes.
[0018] As a preferred technical solution of the present invention, in step S3, the pore size of the stainless steel filter is 100 mesh, and the centrifugal speed is 4000 rpm.
[0019] As a preferred technical solution of the present invention, in step S5, during the concentration process, the feed liquid temperature is controlled at ≤40°C.
[0020] As a preferred technical solution of the present invention, in step S5, the preparation process of the modified reverse osmosis membrane is as follows:
[0021] The urea was heated in a muffle furnace, the heating rate of the muffle furnace was set to 5°C / min, the final temperature was 550°C and maintained for 2h, and then cooled to room temperature to obtain g-C3N4; at 25°C, the g-C3N4 with a mass ratio of 1:10 was fully mixed with a mixed solution of concentrated sulfuric acid and concentrated nitric acid with a volume ratio of 1:2, and stirred in a stirrer at a speed of 300r / min for 15 to 18h, and then the mixed solution with a volume ratio of 1:(1 to 1.2) was mixed with deionized water, and a precipitate was obtained by filtering and centrifuging, and dried at room temperature to prepare graphite oxide phase carbon nitride CNO;
[0022] Dissolve tannic acid in water to prepare a tannic acid solution with a concentration of 5 to 9 mg / mL, and mix 10 to 15 parts of CNO and 30 to 35 parts of the tannic acid solution at 30 to 35° C., filter, dry, and grind through a 200-mesh sieve to obtain modified CNO;
[0023] Dopamine is added to a Tris-HCl buffer solution to prepare a 6 mg / mL dopamine buffer solution. In parts by weight, 15 to 20 parts of modified CNO are added to 30 to 45 parts of dopamine buffer solution. After fully stirring, the reverse osmosis membrane is immersed in the dopamine buffer solution for self-polymerization reaction for 10 to 14 hours. After the reaction is completed, it is immersed in ethanol for 20 minutes, washed with deionized water, and dried to prepare the modified reverse osmosis membrane.
[0024] As a preferred technical solution of the present invention, in step S7, the parameters of the ultra-high temperature sterilization are a sterilization temperature of 120-125° C. and a sterilization time of 10-15 s.
[0025] As a preferred technical solution of the present invention, in step S8, the inlet air temperature of the spray drying equipment during drying is 180-210°C, and the exhaust air temperature is 100-110°C.
[0026] As a preferred technical solution of the present invention, the pH of the Tris-HCl buffer solution is 8.5 and the concentration is 10 mM.
[0027] Beneficial effects of the present invention:
[0028] (1) Graphite oxide phase carbon nitride (CNO) has a structure and chemical properties similar to graphene, and a structure similar to g-C3N4, so it can provide a channel for the transport of water molecules. Tannic acid can stabilize the structure of CNO. Through solution impregnation, tannic acid can be directly adsorbed on the surface of CNO, forming a stable covering layer through the action of hydrogen bonds and van der Waals forces, and can maintain the lamellar structure of CNO, thereby achieving surface modification of CNO; tannic acid, as a polyphenol compound, has good chelating ability and hydrophilicity, which can improve the surface hydrophilicity of CNO. The modified CNO used to prepare the modified polydopamine membrane layer can effectively combine with pollutants, reduce the adsorption and accumulation of pollutants on the membrane surface, thereby improving the water flux and pollution resistance of the reverse osmosis membrane. CNO modified by tannic acid can enhance the interaction between the substrate and the polymer when used to prepare the membrane. The modified CNO is mixed with the dopamine solution by doping, and dopamine undergoes self-polymerization under alkaline conditions, thereby forming a layer of polydopamine film on the surface of the reverse osmosis membrane. Polydopamine can improve the interfacial compatibility between the reverse osmosis membrane matrix and the inorganic material modified CNO, thereby avoiding the overflow of inorganic nanoparticles. At the same time, hydrophilic groups such as carboxyl, hydroxyl and amino groups can be introduced on the membrane surface, thereby improving the hydrophilicity of the reverse osmosis membrane surface. The hydrophilic membrane can attract water molecules on the membrane surface to form a hydration layer, thereby resisting the attachment of organic matter and bacteria, further improving the pollution resistance of the reverse osmosis membrane, reducing membrane pollution and the frequency of membrane cleaning, so as to remove metal particles generated by the crushing operation in the preparation process of corn silk extract, trace solid particles and microorganisms remaining in the filtration operation, etc., thereby increasing the yield of the corn silk extract preparation process.
[0029] (2) The present invention uses water as the extraction solvent, which ensures the naturalness of the extraction process, avoids the residue and pollution problems that may be caused by chemical solvents, and can better retain the active ingredients in corn silk, such as flavonoids, polysaccharides, alkaloids, etc. Compared with other solvents, the water extraction method can reduce the damage to the active ingredients and ensure the effectiveness of the extract. The extract obtained by the water extraction method has good water solubility and is easy to be absorbed and utilized by the human body. Compared with single extraction, through secondary extraction, the remaining active ingredients can be further extracted from corn silk, and the concentration of the extract and the overall extraction efficiency can be improved. The initial extraction may not be able to completely extract all the target components. The secondary extraction can make full use of the raw materials and avoid waste. The clarity of the extract is further improved by filtering and fine filtration. The modified reverse osmosis membrane can effectively distinguish the active ingredients and impurities in corn silk, improve the purity of the extract, and more easily protect the active ingredients in the extract. Adding maltodextrin to the concentrated extract can make the corn silk extract more easily form a solid form, which is convenient for storage, transportation and use. At the same time, maltodextrin can also expand the volume of the extract. Maltodextrin itself contains a large amount of polysaccharides, and also contains trace elements and minerals such as calcium and iron that are beneficial to the human body, so it can improve the appearance and taste of the product. In addition, maltodextrin has good solubility, stability and thickening properties, and can improve the solubility and stability of corn silk extract, making it easier to be absorbed and utilized by the human body. The corn silk extract obtained by the method of the present invention has a high yield, and the total flavonoid content in the corn silk extract is high. DETAILED DESCRIPTION
[0030] In order to further illustrate the technical means and effects adopted by the present invention to achieve the predetermined invention purpose, the specific implementation methods, structures, features and effects of the present invention are described in detail below in combination with the embodiments.
[0031] In the following examples and comparative examples:
[0032] Urea: purchased from Shanghai Aladdin Biochemical Technology Co., Ltd., product number: U432960;
[0033] Tannic acid: purchased from Shanghai Aladdin Biochemical Technology Co., Ltd., product number: T291741;
[0034] Dopamine: purchased from Shanghai MacLean Biochemical Technology Co., Ltd., product number: A902400;
[0035] Reverse osmosis membrane: purchased from Wharton Technology Co., Ltd., model: LP22-8040;
[0036] Maltodextrin: purchased from Baolingbao Biotechnology Co., Ltd.;
[0037] Corn silk raw materials: purchased from Xinshao Nan Stranger Technology Co., Ltd., the crushed particle size is 60 mesh;
[0038] The pH of the Tris-HCl buffer solution was 8.5 and the concentration was 10 mM.
[0039] Example 1
[0040] Preparation of modified reverse osmosis membrane:
[0041] The urea was heated in a muffle furnace, the heating rate of the muffle furnace was set to 5°C / min, the final temperature was 550°C and maintained for 2h, and then cooled to room temperature to obtain g-C3N4; at 25°C, the g-C3N4 with a mass ratio of 1:10 was fully mixed with a mixed solution of concentrated sulfuric acid and concentrated nitric acid with a volume ratio of 1:2, and stirred in a stirrer at a speed of 300r / min for 15h, and then the mixed solution with a volume ratio of 1:1 was mixed with deionized water, and a precipitate was obtained by filtering and centrifuging, and dried at room temperature to prepare oxidized graphite phase carbon nitride CNO;
[0042] Tannic acid was dissolved in water to prepare a tannic acid solution with a concentration of 5 mg / mL. By weight, 10 parts of CNO and 30 parts of the tannic acid solution were fully mixed at 30° C., and the mixture was filtered, dried, and crushed through a 200-mesh sieve to obtain modified CNO.
[0043] Dopamine was added to a Tris-HCl buffer solution to prepare a 6 mg / mL dopamine buffer solution. In parts by weight, 15 parts of modified CNO were added to 30 parts of dopamine buffer solution. After fully stirring, the reverse osmosis membrane was immersed in the dopamine buffer solution for self-polymerization reaction for 10 hours. After the reaction was completed, it was immersed in ethanol for 20 minutes, washed with deionized water, and dried to prepare a modified reverse osmosis membrane.
[0044] S1. Crushing: crushing the corn silk raw material by a crusher;
[0045] S2, extraction: at a temperature of 95 ° C, weigh 0.7 kg of crushed corn silk and 8.4 kg of reverse osmosis drinking pure water, mix and perform a primary extraction, extract for 2 hours, filter through a 300-mesh stainless steel filter, collect the primary filtrate, cool the temperature to ≤40 ° C, continue to add 5.6 kg of reverse osmosis drinking pure water, perform a secondary extraction, extract for 2 hours, filter through a 300-mesh stainless steel filter, collect the secondary filtrate, combine the two filtrates to obtain the material after the extraction, and cool the temperature to ≤40 ° C;
[0046] S3, filtration: After the extraction, the material is filtered through a stainless steel filter and centrifuged to remove slag to obtain an extraction liquid. The centrifuge speed is 4000r / min and the centrifugation time is 10min;
[0047] S4, fine filtration: the leaching liquid is ultrafiltered through an ultrafiltration membrane with a pore size of 200 nm to obtain a fine filtrate;
[0048] S5, concentration: the refined filtrate is concentrated by a modified reverse osmosis membrane RO membrane, and the concentration is completed when the concentration reaches 2.0 Brix to obtain a concentrated solution;
[0049] S6. Compounding: Add maltodextrin in an amount of 4 times the mass of the solid content of the concentrated solution to the concentrated solution to obtain a concentrated prepared solution;
[0050] S7, ultra-high temperature sterilization: sterilize the above concentrated preparation liquid through ultra-high temperature sterilization equipment, the sterilization temperature is 120°C, and the sterilization time is 15s;
[0051] S8. Spray drying: The sterilized concentrated formulation liquid is dried into powder by spray drying equipment, the inlet air temperature is controlled at 180° C., and the exhaust air temperature is controlled at 100° C., to obtain 205 g of dry corn silk extract, wherein the total flavonoid content is 1.3%.
[0052] Example 2
[0053] Preparation of modified reverse osmosis membrane:
[0054] The urea was heated in a muffle furnace, the heating rate of the muffle furnace was set to 5°C / min, the final temperature was 550°C and maintained for 2 hours, and then cooled to room temperature to obtain g-C3N4; at 25°C, the g-C3N4 with a mass ratio of 1:10 was fully mixed with a mixed solution of concentrated sulfuric acid and concentrated nitric acid with a volume ratio of 1:2, and stirred in a stirrer at a speed of 300r / min for 16 hours, and then the mixed solution with a volume ratio of 1:1.1 was mixed with deionized water, filtered and centrifuged to obtain a precipitate, and dried at room temperature to prepare oxidized graphite phase carbon nitride CNO;
[0055] Tannic acid was dissolved in water to prepare a tannic acid solution with a concentration of 7 mg / mL. By weight, 13 parts of CNO and 31 parts of tannic acid solution were fully mixed at 32°C, and the mixture was filtered, dried, and crushed through a 200-mesh sieve to obtain modified CNO.
[0056] Dopamine was added to a Tris-HCl buffer solution to prepare a 6 mg / mL dopamine buffer solution. In parts by weight, 17 parts of modified CNO were added to 35 parts of dopamine buffer solution. After fully stirring, the reverse osmosis membrane was immersed in the dopamine buffer solution for self-polymerization reaction for 12 hours. After the reaction was completed, it was immersed in ethanol for 20 minutes, washed with deionized water, and dried to prepare a modified reverse osmosis membrane.
[0057] S1. Crushing: crushing the corn silk raw material by a crusher;
[0058] S2, extraction: at a temperature of 98 ° C, weigh 20 kg of crushed corn silk and 240 kg of reverse osmosis drinking pure water, mix and perform a primary extraction, extract for 2 hours, filter through a 300-mesh stainless steel filter, collect the primary filtrate, cool the temperature to ≤40 ° C, continue to add 160 kg of reverse osmosis drinking pure water, perform a secondary extraction, extract for 2 hours, filter through a 300-mesh stainless steel filter, collect the secondary filtrate, combine the two filtrates to obtain the material after the extraction, and cool the temperature to ≤40 ° C;
[0059] S3, filtration: After the extraction, the material is filtered through a stainless steel filter and centrifuged to remove slag to obtain an extraction liquid. The centrifuge speed is 4000r / min and the centrifugation time is 10min;
[0060] S4, fine filtration: filter the extract solution through 10μm and 2μm fine filtration membranes in sequence to obtain fine filtrate;
[0061] S5, concentration: the refined filtrate is concentrated by a modified reverse osmosis membrane RO membrane, and the concentration is completed when the concentration reaches 3.5 Brix to obtain a concentrated solution;
[0062] S6. Compounding: Add maltodextrin in an amount of 4 times the mass of the solid content of the concentrated solution to the concentrated solution to obtain a concentrated prepared solution;
[0063] S7, ultra-high temperature sterilization: sterilize the above concentrated preparation liquid through ultra-high temperature sterilization equipment, the sterilization temperature is 122°C, and the sterilization time is 13s;
[0064] S8. Spray drying: The sterilized concentrated formulation liquid is dried into powder by spray drying equipment, the inlet air temperature is controlled at 190° C., and the exhaust air temperature is controlled at 105° C. to obtain 4.5 kg of dry corn silk extract, of which the total flavonoid content is 1.43%.
[0065] Example 3
[0066] Preparation of modified reverse osmosis membrane:
[0067] The urea was heated in a muffle furnace, the heating rate of the muffle furnace was set to 5°C / min, the final temperature was 550°C and maintained for 2h, and then cooled to room temperature to obtain g-C3N4; at 25°C, the g-C3N4 with a mass ratio of 1:10 was fully mixed with a mixed solution of concentrated sulfuric acid and concentrated nitric acid with a volume ratio of 1:2, and stirred in a stirrer at a speed of 300r / min for 18h, and then the mixed solution with a volume ratio of 1:1.2 was mixed with deionized water, filtered and centrifuged to obtain a precipitate, and dried at room temperature to prepare oxidized graphite phase carbon nitride CNO;
[0068] Tannic acid was dissolved in water to prepare a tannic acid solution with a concentration of 9 mg / mL. By weight, 15 parts of CNO and 35 parts of the tannic acid solution were fully mixed at 35° C., and the mixture was filtered, dried, and crushed through a 200-mesh sieve to obtain modified CNO.
[0069] Dopamine was added to a Tris-HCl buffer solution to prepare a 6 mg / mL dopamine buffer solution. In parts by weight, 20 parts of modified CNO were added to 45 parts of the dopamine buffer solution. After fully stirring, the reverse osmosis membrane was immersed in the dopamine buffer solution for self-polymerization reaction for 14 hours. After the reaction was completed, it was immersed in ethanol for 20 minutes, washed with deionized water, and dried to prepare the modified reverse osmosis membrane.
[0070] S1. Crushing: crushing the corn silk raw material by a crusher;
[0071] S2, extraction: at a temperature of 96 ° C, weigh 400 kg of crushed corn silk, feed in two batches, each feeding 200 kg, and mix with 2400 kg of reverse osmosis drinking pure water for one extraction, extract after 2 hours through a 300-mesh stainless steel filter, collect the first filtrate, cool the temperature to ≤40 ° C, continue to add 1600 kg of reverse osmosis drinking pure water, extract after 2 hours through a 300-mesh stainless steel filter, collect the second filtrate, combine the two filtrates to obtain the material after the extraction, and cool the temperature to ≤40 ° C;
[0072] S3, filtration: After the extraction, the material is filtered through a stainless steel filter and centrifuged to remove slag to obtain an extraction liquid. The centrifuge speed is 4000r / min and the centrifugation time is 10min;
[0073] S4, fine filtration: filter the extract solution through 10μm and 2μm fine filtration membranes in sequence to obtain fine filtrate;
[0074] S5, concentration: the refined filtrate is concentrated by a modified reverse osmosis membrane RO membrane, and the concentration is completed when the concentration reaches 8.0 Brix to obtain a concentrated solution;
[0075] S6. Compounding: Add maltodextrin in an amount of 4 times the mass of the solid content of the concentrated solution to the concentrated solution to obtain a concentrated prepared solution;
[0076] S7, ultra-high temperature sterilization: sterilize the above concentrated preparation liquid through ultra-high temperature sterilization equipment, the sterilization temperature is 125°C, and the sterilization time is 10s;
[0077] S8. Spray drying: The sterilized concentrated formulation liquid is dried into powder by spray drying equipment, the inlet air temperature is controlled at 210° C., and the exhaust air temperature is controlled at 110° C., to obtain 176.5 kg of dry corn silk extract, of which the total flavonoid content is 1.42%.
[0078] Comparative Example 1
[0079] The difference between Comparative Example 1 and Example 1 is that the reverse osmosis membrane in Comparative Example 1 has not been subjected to any modification treatment, and the other operations are the same, and 190 g of dry corn silk extract is obtained, wherein the total flavonoid content is 1.08%.
[0080] Comparative Example 2
[0081] The difference between Comparative Example 2 and Example 1 is that in Comparative Example 2, CNO is not modified with tannic acid, and the other operations are the same, and 197 g of dry corn silk extract is obtained, wherein the total flavonoid content is 1.16%.
[0082] Comparative Example 3
[0083] The difference between Comparative Example 3 and Example 1 is that the preparation process of the modified reverse osmosis membrane in Comparative Example 3 is:
[0084] Dopamine was added to a Tris-HCl buffer solution to prepare a 6 mg / mL dopamine buffer solution, and the reverse osmosis membrane was immersed in the dopamine buffer solution for self-polymerization reaction for 14 hours. After the reaction was completed, the reverse osmosis membrane was immersed in ethanol for 20 minutes, washed with deionized water, and dried to prepare the modified reverse osmosis membrane.
[0085] The remaining operations were the same, and 194 g of dry corn silk extract was obtained, of which the total flavonoid content was 1.11%.
[0086] The above description is only a preferred embodiment of the present invention and does not limit the present invention in any form. Although the present invention has been disclosed as a preferred embodiment as above, it is not used to limit the present invention. Any technical personnel in this field can make some changes or modify the technical contents disclosed above into equivalent embodiments without departing from the scope of the technical solution of the present invention. However, any brief modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention without departing from the content of the technical solution of the present invention are still within the scope of the technical solution of the present invention.
Claims
1. A method for preparing a corn silk extract, characterized in that: The steps include: S1. Crushing: crushing the corn silk raw material by a crusher; S2, extraction: at a temperature of 95-98 ° C, the crushed corn silk and reverse osmosis drinking pure water in a mass ratio of 1:12 were mixed and extracted once, and the mixture was filtered through a 300-mesh stainless steel filter after 2 hours of extraction, and the filtrate was collected once, and the temperature was cooled to ≤40 ° C, and reverse osmosis drinking pure water was continued to be added to make the material-liquid ratio 1:8, and a second extraction was performed, and the mixture was filtered through a 300-mesh stainless steel filter after 2 hours of extraction, and the second filtrate was collected, and the two filtrates were combined to obtain the material after the extraction was completed, and the temperature was cooled to ≤40 ° C; S3, filtration: After the extraction is completed, the material is filtered through a stainless steel filter and centrifuged to remove slag to obtain an extraction liquid; S4, fine filtration: the leaching liquid is filtered through a fine filter membrane with a pore size of 10 μm and 2 μm or ultrafiltered through an ultrafiltration membrane with a pore size of 200 nm to obtain a fine filtrate; S5, concentration: the refined filtrate is concentrated through a modified reverse osmosis membrane RO membrane, and the concentration is completed when the concentration reaches 2.0-8.0 Brix to obtain a concentrated solution; S6. Compounding: Add maltodextrin in an amount of 4 times the mass of the solid content of the concentrated solution to the concentrated solution to obtain a concentrated prepared solution; S7, ultra-high temperature sterilization: sterilize the above concentrated preparation liquid through ultra-high temperature sterilization equipment; S8, spray drying: drying the sterilized concentrated formulation into powder through a spray drying device to obtain the corn silk extract.
2. The method for preparing the corn silk extract according to claim 1, wherein: In step S1, the corn silk raw material is crushed into a particle size of 60 mesh.
3. The method for preparing the corn silk extract according to claim 1, characterized in that: In step S3, the pore size of the stainless steel filter is 100 mesh, and the centrifugal speed is 4000 rpm.
4. The method for preparing the corn silk extract according to claim 1, characterized in that: In step S5, during the concentration process, the temperature of the feed liquid is controlled at ≤40°C.
5. The method for preparing the corn silk extract according to claim 1, characterized in that: In step S5, the preparation process of the modified reverse osmosis membrane is as follows: The urea was heated in a muffle furnace, the heating rate of the muffle furnace was set to 5°C / min, the final temperature was 550°C and maintained for 2h, and then cooled to room temperature to obtain g-C3N4; at 25°C, the g-C3N4 with a mass ratio of 1:10 was fully mixed with a mixed solution of concentrated sulfuric acid and concentrated nitric acid with a volume ratio of 1:2, and stirred in a stirrer at a speed of 300r / min for 15 to 18h, and then the mixed solution with a volume ratio of 1:(1 to 1.2) was mixed with deionized water, and a precipitate was obtained by filtering and centrifuging, and dried at room temperature to prepare graphite oxide phase carbon nitride CNO; Dissolve tannic acid in water to prepare a tannic acid solution with a concentration of 5 to 9 mg / mL, and mix 10 to 15 parts of CNO and 30 to 35 parts of the tannic acid solution at 30 to 35° C., filter, dry, and grind through a 200-mesh sieve to obtain modified CNO; Dopamine is added to a Tris-HCl buffer solution to prepare a 6 mg / mL dopamine buffer solution. In parts by weight, 15 to 20 parts of modified CNO are added to 30 to 45 parts of dopamine buffer solution. After fully stirring, the reverse osmosis membrane is immersed in the dopamine buffer solution for self-polymerization reaction for 10 to 14 hours. After the reaction is completed, it is immersed in ethanol for 20 minutes, washed with deionized water, and dried to prepare the modified reverse osmosis membrane.
6. The method for preparing the corn silk extract according to claim 1, characterized in that: In step S7, the parameters of the ultra-high temperature sterilization are a sterilization temperature of 120-125° C. and a sterilization time of 10-15 seconds.
7. The method for preparing the corn silk extract according to claim 1, characterized in that: In step S8, the inlet air temperature of the spray drying equipment during drying is 180-210°C, and the exhaust air temperature is 100-110°C.
8. The method for preparing the corn silk extract according to claim 5, characterized in that: The pH of the Tris-HCl buffer solution is 8.5, and the concentration is 10 mM.