Device and method for preparing silicon fertilizer mixture with soil improvement effect
Through the one-step method of medium and low temperature alkali melting hydrothermal catalysis, the problems of high energy consumption, high cost and great environmental impact in silicon fertilizer production are solved, and the preparation of fully water-soluble silicon fertilizers and soluble silicon fertilizers with high conversion rates is realized, which improves the Crop growth and soil quality meet the requirements of green and environmental protection, and promote the industrial promotion of silicon fertilizers.
Patent Information
- Application Number
- CN202411114381.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-14
- Publication Date
- 2024-11-15
AI Technical Summary
The existing silicon fertilizer production methods have problems such as high energy consumption, high cost, poor product stability and great environmental impact. In particular, high temperature and high pressure reactions do not meet the requirements of low-carbon and high-efficiency green transformation, making it difficult to achieve industrial promotion.
By using a one-step process of medium and low temperature alkali melting hydrothermal catalysis, a fully water-soluble silicon fertilizer and soluble silicon fertilizer with stable performance and reliable quality are prepared to achieve high conversion rate and step of silicon ore Utilization, no waste emissions, meets green and environmental protection requirements.
It realizes rapid and low-cost conversion of silicon ore, reduces energy consumption and production costs, safe and environmentally friendly production process, solves the problems of low conversion rate of silicon fertilizer and soil slab formation, improves crop growth and soil quality, and meets the green circular economy production Require.
Smart Images

Figure CN118955221A_ABST
Abstract
Description
Technical Field
[0001] The application number of this invention is 201910713832.0, and the invention name is a series of applications entitled "A method for preparing fully water-soluble silicon fertilizer using silicon ore", which relates to agricultural fertilizers and soil conditioners, with a classification number of C05G3 / 00, and in particular to a preparation device and method for a silicon fertilizer mixture with a soil improvement function. Background Art
[0002] Silicon fertilizer has been successfully applied to the cultivation of rice and other crops in agricultural production. Silicon fertilizer has a significant effect on increasing the mechanical strength of rice stalks and improving lodging resistance. Silicon is one of the important nutrient elements in plant composition. In addition to improving crop lodging resistance, it can also enhance crop photosynthesis, improve crop resistance to pests and diseases, drought, dry hot winds, cold and other stress resistance. At the same time, silicon acts on the cell wall to enhance the air permeability of crops, prevent root rot and premature aging, and silicon fertilizer can enhance the pollen vitality of melon and fruit crops and increase the yield rate; silicon can significantly improve the quality of agricultural products and extend the shelf life; adding silicon fertilizer to the soil can not only improve the utilization rate of phosphorus fertilizer and regulate the balanced absorption of nitrogen, phosphorus and potassium; it can also improve the soil, promote the decomposition of organic fertilizers, inhibit soil pathogens and reduce heavy metal pollution. Due to the above-mentioned significant effects, silicon fertilizer has been listed as the fourth largest element fertilizer after nitrogen, phosphorus and potassium by the international soil community.
[0003] Nitrogen, phosphorus and potassium are the three essential nutrients for crops, and silicon, as an important intermediate element for crop growth, has received increasing attention in agriculture both at home and abroad.
[0004] Silicon fertilizer, as a health fertilizer and plant regulating fertilizer, is a new type of multifunctional fertilizer that cannot be compared with other chemical fertilizers. Silicon fertilizer can be used as fertilizer to provide nutrients, and can also be used as a soil conditioner to improve the soil. In addition, it also has the functions of preventing diseases, insects and reducing toxicity. With its outstanding advantages such as non-toxic, tasteless, non-deteriorating, non-loss and pollution-free, it will become a high-efficiency and high-quality fertilizer for the development of green ecological agriculture.
[0005] High yield and high quality are the development goals for evaluating crop planting levels. With the improvement of fertilization levels, the application of large amounts of chemical fertilizers must be accompanied by silicon fertilizers. Only by scientifically balanced fertilization of "nitrogen, phosphorus, potassium + silicon" can the effect of high quality and high yield be achieved. Silicon fertilizers can change the quality of crops and are attracting the attention of soil and fertilizer and plant nutrition circles around the world.
[0006] At present, silicon fertilizers in the agricultural market are all implemented in accordance with the silicon fertilizer industry standard NY / T 797-2004 of the Ministry of Agriculture and Rural Affairs, indicating that after years of research, testing and promotion, silicon fertilizer has become a new type of fertilizer in my country in the 21st century.
[0007] At present, silicon-deficient soils account for more than 50-80% of the total cultivated land in my country. Taking rice as an example, the area of rice cultivation in my country reaches more than 33.33 million hectares per year, and silicon-deficient soils account for more than 50%. If silicon fertilizers are fully applied, the yield can be increased by 10%, and this alone should increase the yield of rice by 1 million tons per year. The promotion of the production and application of silicon fertilizers has very obvious social and economic benefits.
[0008] At present, most of the silicon fertilizer production uses steel slag, ironmaking slag, yellow phosphorus slag, potassium feldspar, sea ore, red mud and other materials as the main raw materials, and is prepared by calcination, crushing and other processes, with effective silicon (measured by dissolution in dilute hydrochloric acid) as the main indicated amount of fertilizer. Although this part of soluble silicon has increased its specific surface area and solubility through mechanical activation, it is still an acid-soluble silicate, which is not conducive to direct absorption by plants. Domestic and foreign studies have shown that water-soluble monosilicic acid components can be directly absorbed by plants, and play a decisive role in promoting crop development, improving crop stress resistance, and especially reducing crop diseases. Therefore, monosilicic acid-type water-soluble silicon fertilizers should be the direction of silicon fertilizer development in the future. Soluble silicon fertilizers that can meet the requirements of NY / T797-2004 as slow-release silicon fertilizers have a long-term effect on soil and crops. The production of water-soluble silicon fertilizer is mainly prepared by mechanically mixing potassium silicate with various water-soluble trace element fertilizers. Water-soluble silicon fertilizer is also produced by adding activators to silicon-containing tailings such as steel slag using hot water. However, since the activation effect is affected by many factors, the product quality, that is, the water-soluble silicon content, fluctuates greatly.
[0009] The above methods mainly focus on the use of raw materials such as steel slag, which are crushed and physically mixed with other reagents, or the preparation of water-soluble silicon through hot water and other complex multi-step reactions, but these methods have the problem of difficult to ensure product stability or too high cost. There are also patents that use silicon ore and sodium hydroxide to melt at high temperatures of 1200-1600°C to prepare water-soluble silicon, or use silicon ore and soda ash solution to react under high temperature and high pressure to prepare. Whether it is a high-temperature melting reaction exceeding 1000°C or a high-temperature and high-pressure reaction, there are problems of high energy consumption and safety and environmental protection. It does not meet the current requirements of high-quality development for low-carbon, high-efficiency and green transformation. At the same time, the requirements for temperature-resistant materials are also extremely high, and the prospects for industrial promotion and economic feasibility are poor.
[0010] For example, Chinese patent document CN104761332A records a kind of medical stone water-soluble mineral silicon fertilizer, the mesh number of medical stone mineral powder is 600-800 mesh, the medical stone mineral powder accounts for 65-70% of the total weight ratio of the two, and potassium oxide accounting for 30-35% is added and burned at a high temperature of 1200-200 for 1 hour. It is quenched in water while hot, precipitated, and concentrated to obtain silicate crystals containing multiple minerals. The silicate crystals are determined by microspectroscopy and X-ray diffractometer to contain more than 60% silicon dioxide, and contain boron, selenium, and rare earth elements such as mace, antimony, etc. More than 50 trace elements required by plants, 600 kg of medical stone silicate crystals are put into a reactor, 400 kg of water is added, and the pressure (MP) is 80-120°C for more than 3 times to make it completely melt, and the insoluble matter is filtered out and cooled to room temperature before use. In this scheme, although water-soluble silicon fertilizer can be obtained, its production process requires high temperature and high pressure reaction, which consumes a lot of energy. It is useless in actual production and is a conceptual patent.
[0011] This patent is an upgrade based on the previous 1.0 version of the method of fully water-soluble silicon fertilizer. After special treatment of silicon ore in various processes and the addition of flux and other substances, the problem of low-temperature melting of silicon ore is further solved, energy consumption and production costs are greatly reduced, and melting conversion below 500°C is achieved. This patented technology is an internationally leading technology. With the excessive use of fertilizers in rural land in China and the widespread promotion of greenhouse planting, the threat to my country's agricultural planting land soil is increasing day by day, and the phenomenon of soil compaction is becoming more and more serious. It can be foreseen that through the vigorous promotion of this patent, it is hoped that the problem of soil compaction in rural cultivated land in my country will be greatly alleviated in the next few years. Because it is very energy-saving and environmentally friendly, it meets the relevant national policy requirements. Summary of the invention
[0012] The object of the present invention is to provide a device and method for preparing a silicon fertilizer mixture having a soil improvement effect by chemically reacting, rapidly, at low cost, and completely water-soluble silicon ore alkali melting to prepare water-soluble silicon fertilizer and simultaneously co-producing soluble silicon fertilizer.
[0013] The present invention adopts a one-step method of medium-low temperature alkali melt hydrothermal catalysis to make silicon ore react quickly with alkaline compounds to prepare fully water-soluble monosilicon fertilizer and soluble silicon fertilizer with stable performance and reliable quality. The present invention has the outstanding characteristics of high silicon conversion rate in raw materials, cascade utilization of silicon ore, no three wastes discharge, green environmental protection, low production cost, safe and environmentally friendly production process, etc., and realizes circular economy and energy conservation and emission reduction in the production process.
[0014] In order to solve the above technical problems, a method for preparing fully water-soluble silicon fertilizer using silicon ore of the present invention adopts the following steps: Silicon ore powder containing 5%-90% silicon (W / W) and having a fineness of 40-1500 meshes is used, firstly mixed with flux and alkaline compounds such as sodium hydroxide, then added with appropriate amount of water and allowed to stand for pre-hydration mixing, and then subjected to melting reaction, the weight percentage (wt) of silicon ore powder, flux, alkaline compound and water is 100 / (0.5-3.5) / (5-30) / (10-20), the standing pre-hydration mixing time is 10-30min, the reaction temperature is 50℃-600℃, the reaction time is 0.5h-4h, the reactant is dissolved in water, and then separated into solid and liquid, the separated liquid is the fully water-soluble silicon fertilizer, the separated liquid can also be dried to form powder particles, and the separated solid residue is dried to obtain solid soluble silicon fertilizer.
[0015] The silicon ore contains 30%-80% silicon (W / W), the fineness is 80 mesh-1200 mesh, the weight percentage of silicon ore and alkaline compound is 40-70:6-18, the reaction temperature is 150℃-500℃, and the reaction time is 1h-3h.
[0016] The silicon ore mainly exists in the form of silicon oxides and silicates. The silicon oxide ores mainly include sand, quartz, crystal, purple quartz, agate, flint and opal; the silicate ores mainly include granite, amphibole, asbestos, feldspar, clay and mica, etc. The dry basis silicon dioxide content in the silicon ore is 30%-80% (W / W).
[0017] The pulverization process of the silicon ore powder includes crushing-screening-grinding.
[0018] The flux is one of calcium fluoride, borax and urea, or a mixture of two or three thereof, and the added amount (wt) of the flux is 1.5%-3%.
[0019] The alkaline compound includes one or more of sodium hydroxide, potassium hydroxide, calcium oxide, magnesium oxide, sodium carbonate, potassium carbonate, sodium peroxide, calcium carbonate and magnesium carbonate.
[0020] The preparation process is as follows: Figure 1 As shown: Silicon ore - crushing - mixing with other solid materials - mixing with water and letting it stand - alkali molten water heat catalytic reaction - hydrolysis - solid-liquid separation - clear liquid - finished product 1 - liquid fully water-soluble silicon fertilizer Clear liquid--drying--finished product 2-solid fully water-soluble silicon fertilizer Residue (solid) - drying - finished product 3 - solid fully water-soluble silicon fertilizer The quality indicators of the liquid fully water-soluble silicon fertilizer are: water-soluble SiO2≥25%; water-insoluble matter≤0.5%; moisture≤60%.
[0021] The quality indicators of the solid fully water-soluble silicon fertilizer are: water-soluble SiO2≥50%; water-insoluble matter≤2%; moisture≤3%.
[0022] The quality indicators of the solid fully water-soluble silicon fertilizer are: moisture ≤3%; effective SiO2 ≥20%; fineness (passing 250μm sieve) ≥80%.
[0023] The preparation device is as follows Figure 2-4 shown.
[0024] Silicon ore powder containing 5%-90% silicon (W / W) and a fineness of 40-1500 meshes is used, first mixed evenly with flux and alkaline compounds such as sodium hydroxide, and then added with an appropriate amount of water to stand for pre-hydration mixing, with molecular sieve as a water absorbent, under the catalytic action of alkali molten water, the pre-hydrated mixed solution is fed in the form of spray into the reaction chamber of a reactor body equipped with a spray-based reaction device, and ultrasonication is performed using an ultrasonic device provided with the spray-based reaction device, accompanied by stirring, to perform melting reaction The weight percentage of silicon ore powder, flux, alkaline compound and water is 100 / (0.5-3.5) / (5-30) / (10-20), the standing prehydration mixing time is 10-30min, the reaction temperature is 50℃-600℃, the reaction time is 0.5h-4h, the obtained reactant is dissolved in water, and then separated into solid and liquid. The separated liquid is fully water-soluble silicon fertilizer. The obtained liquid can also be dried to form powder particles. The separated solid residue is dried to obtain soluble silicon fertilizer.
[0025] When feeding, water is added into the reaction chamber by using a spray device, ultrasonic stirring is performed by using an ultrasonic device provided in the reaction device based on spray injection, and then the mixture is allowed to stand for stratification, the oily layer is introduced into a sample collector through an introduction pipeline, and the co-solvent is recovered by vacuum distillation. After a white transparent liquid is obtained, the vacuum distillation is stopped, and the remaining liquid is cooled to room temperature. Meanwhile, the mixture is vigorously stirred in the sample collector, and finally a white solid powder of soluble silicon fertilizer is obtained; It should be understood that since water is added to the reaction chamber by the spray device, the residual feed in the spray device is equivalent to being cleaned to prevent clogging. Due to the ultrasound and stirring, these residual feeds will still react, so that a large amount of unreacted feed will not be introduced.
[0026] The reaction device based on spray injection includes a reaction kettle, a sample collector connected to the reaction kettle and having a discharge port with a switch door installed, and the switch door is used to close or open the discharge port according to whether discharge is required, and A plurality of nanobubble generating devices are arranged around the reactor, each of which is connected to a corresponding spray device arranged on the reactor body wall, and sprays a mist feed containing nanobubbles into the reaction chamber of the reactor body, and an ultrasonic device is arranged on the reactor body wall near the bottom of the reactor body; A first exhaust port is provided on the top of the reactor body, connected to a reflux device during the reaction; A first stirring motor is eccentrically installed on the top of the reactor, and a first output shaft of the first stirring motor is connected to a first stirring rod, so that a first blade at the end of the first stirring rod rotates to achieve stirring; the molecular sieve is arranged at the bottom of the reactor body; The reactor body of the reactor is provided with a first exhaust port connected to a reflux device at the top thereof, and a first motor connected and installed via a motor bracket, a thermocouple is installed at the bottom of the outer wall of the reactor body, and a semiconductor refrigeration device is installed closely around the outer wall. The first output shaft of the first motor is connected to a first stirring rod, a first blade is installed at the end of the first stirring rod, and two additional sets of blades are installed, and each blade is provided with a curved protrusion.
[0027] A window for measuring the level of the oily layer is installed on the inner wall of the reactor body, and position scales marked with the highest position H and the lowest position L are arranged on one side of the window. An active 4Å molecular sieve is arranged at the bottom of the reactor body.
[0028] The spray device includes a spray pipe and a spray head. Three spray devices are installed at three equal points on the inner wall of the reactor body, and three ultrasonic devices are installed near the bottom of the reactor body. The projections of each ultrasonic device and each spray device on the inner wall of the bottom of the reactor body are close to each other, and the projection of one spray device is between the projection of the thermocouple on the inner wall of the bottom of the reactor body and the projection of the corresponding ultrasonic device, and the three projections are close to each other.
[0029] It can be understood that the eccentrically mounted first stirring motor not only enables the first stirring rod to avoid the feed sprayed by the spray device, but also can create an asymmetric vortex, thereby achieving a strong mixing effect and making the reaction more uniform and thorough.
[0030] Preferably, the nanobubble generating device includes a feed pump and a venturi tube connected in sequence by pipelines along the feeding direction, and a multi-head carrier gas manifold connected to the venturi tube, and the multi-head carrier gas manifold is connected to a carrier gas source through an air inlet pipe; the spray device includes a spray head and a spray pipe connected to the spray head, and the spray pipe is connected to the inner wall of the reactor body.
[0031] Preferably, the number of the nano bubble generating devices is 3-6. Each nano bubble generating device includes a feed pump and a venturi tube arranged once in the injection direction, and a spray pipe is connected by a pipeline. Specifically, the spray pipe and the pipeline with external threads can be connected according to the first connecting sleeve with a polytetrafluoroethylene internal thread to realize the connection between the nano bubble generating device and the spray device, that is, the outflow end of the venturi tube is provided with an externally threaded pipeline at one end, and the end is used to connect the spray pipe in the spray device. Specifically, the spray pipe is connected to one end of the first connecting sleeve, and the other end of the first connecting sleeve is connected to the end of the pipeline with external threads through its polytetrafluoroethylene internal thread.
[0032] Preferably, the carrier gas comprises nitrogen or argon.
[0033] Optionally, the number of the ultrasonic devices matches the number of the nanobubble generating devices, that is, the number of the ultrasonic devices is equal to the number of the nanobubble generating devices, and the projections of each ultrasonic device and one of the spray devices at the bottom of the reactor body are close to each other.
[0034] Preferably, the spray devices are evenly distributed on the wall of the reactor.
[0035] The number of the multi-head carrier gas manifolds is an even multiple of 2, and they are distributed on both sides of a symmetry axis perpendicular to the symmetry axis of the Venturi tube along the feeding direction, and are arranged on the middle thin straight tube of the Venturi tube, and an acute angle is formed between the inlet direction of the carrier gas manifold and the feeding direction, and carrier gas is input into the Venturi tube through the inlet pipe through the carrier gas manifold, so that nano-scale bubbles are generated in the feed; Preferably, the acute angle is in the range of (45°, 75°). If the acute angle is too small, less than 45°, the diameter of the bubbles generated is generally larger and the total number is smaller. If it is too large, greater than 75°, the feed speed is slowed down.
[0036] More preferably, the acute angle is (55°, 65°) A polytetrafluoroethylene joint is provided at one end of the shell, and three connecting sleeves with polytetrafluoroethylene internal threads are installed on the outer wall of the reactor body. The ultrasonic transducer rod passes through the center of the polytetrafluoroethylene joint and is arranged according to Figure 2 The device is screwed in the direction of the middle arrow and extends into the reaction chamber inside the reactor body to form an installation position with an acute orientation angle.
[0037] It is understandable that due to the multi-head manifold, bubbles can be generated efficiently, and more abundant and delicate bubbles can be produced than a single manifold. When a single manifold is used, after the bubbles are generated, they are output through the bell mouth of the venturi tube, and the stability of the total number of bubbles cannot be guaranteed. However, with a multi-head manifold, bubbles begin to be generated at the end where the capillary enters, and are bubbled again at the end where the capillary enters the bell mouth. Because an acute angle is formed between the inlet direction of the carrier gas manifold and the feed direction, the feed is pushed out to a certain extent, achieving the stability of the total number of bubbles, the refinement of bubbles, and the speed of feeding.
[0038] When bubbles burst, cavitation effect will be generated in the reaction system. The bursting of dense bubbles in the space will lead to random vibration waves in all directions, thereby achieving sufficient microscopic mixing of the reaction system. In addition, the auxiliary superposition effect of ultrasound accelerates the additional generation of bubbles and the interaction between them, further strengthening the cavitation effect and making the reaction more uniform and sufficient.
[0039] The reactor and the sample collector are connected by a pipeline, and the end connected to the reactor is the lowest end allowed by the oil layer; a second exhaust port with a pressure relief valve is installed on the top of the sample collector, and a steam outlet pipe is arranged near the top of the sample collector wall to connect the condensation reflux device and the solvent collector; A second stirring motor is also installed on the top of the sample collector, and the second output shaft of the second stirring motor is connected to the second stirring rod, so that the second blade at the end of the second stirring rod rotates to achieve strong stirring of the white transparent liquid. As the temperature decreases, white solid powder of soluble silicon fertilizer is obtained. After the distillation is completed, the steam duct outlet is closed. The pressure relief valve is used to relieve pressure on the sample collector when the strong stirring ends after the distillation.
[0040] A heating device is installed at the bottom of the sample collector, and the recovered oily layer is heated and distilled under reduced pressure to obtain the white transparent liquid. Preferably, the ultrasonic device comprises an ultrasonic transducer rod, and a shell which encloses one end of the ultrasonic transducer rod and is detachably sealed to the outer wall of the reactor body, and which forms an acute angle with the central axis of the reactor so that the rod head penetrates deeply into the reaction chamber inside the reactor body.
[0041] Preferably, the outer wall detachable sealed connection is achieved through an outer wall detachable sealed connection structure, which includes a second connecting sleeve with a polytetrafluoroethylene internal thread installed on the outer wall of the reactor body and a polytetrafluoroethylene joint that can be threadedly connected to the second connecting sleeve, the polytetrafluoroethylene joint is threadedly connected to the end of the second connecting sleeve away from the outer shell, and the ultrasonic transducer rod passes through the center of the polytetrafluoroethylene joint and extends into the reaction chamber inside the reactor body.
[0042] Preferably, the end of the polytetrafluoroethylene joint away from the reactor body has a skirt, which is used to limit the sealing ring when the sealing ring is sleeved on the polytetrafluoroethylene joint. When the polytetrafluoroethylene joint and the polytetrafluoroethylene internal thread are screwed into the bottom, the second connecting sleeve abuts against the sealing ring and the sealing ring presses against the skirt to achieve sealing.
[0043] Preferably, solenoid valves are provided on the pipeline between the Venturi tube and the spray device, on the second exhaust port, on the steam outlet pipe, and on the multi-head manifold, and the solenoid valve provided between the Venturi tube and the spray device is a high-frequency pulse solenoid valve.
[0044] Due to pulse injection, micro-injection can diffuse in the larger reaction wall to easily achieve uniform mixing, and multiple micro-injection reactions can achieve reaction integration in the entire reaction process.
[0045] The two ends of the symmetry axis perpendicular to the feeding direction of the middle thin straight tube of the Venturi tube are provided with a 60° manifold and a 55° manifold for nitrogen carrier gas delivery, that is, the angles between the axes of the two manifolds and the symmetry axis are 60° and 55° respectively.
[0046] The top of the sample collector is provided with a second exhaust port of a pressure relief valve for pressure relief during strong stirring. A steam outlet pipe is arranged near the top of the outer wall of the sample collector to connect the condensation reflux device and the flux collector.
[0047] A second motor is also installed on the top of the sample collector. Similarly, the second output shaft of the second motor is connected to the second stirring rod. A second paddle is installed at the end of the second stirring rod, as well as an additional set of paddles. Each paddle is also provided with a curved protrusion.
[0048] A heating device is installed at the bottom of the sample collector, and a discharge port with a switch door is arranged on the outer wall close to the bottom.
[0049] Preferably, at least one set of paddles is additionally installed on the first stirring rod and the second stirring rod in addition to the ends, and all the paddles, including the first paddle and the second paddle, are provided with curved linear protrusions to enhance the stirring effect. An observation window is installed on the outer wall of the reactor body, and a position scale indicating the position of the oily layer, including the minimum and maximum height limit indicating liquid levels, is provided next to the observation window to confirm the height reached by the oily layer.
[0050] Preferably, a semiconductor refrigeration device is closely attached to the outer wall of the reactor body along the lower end of the observation window, and a thermocouple is installed on the reactor body wall at the lower end of the semiconductor refrigeration device. The precise constant temperature of the reaction temperature inside the reactor body is achieved by controlling the thermocouple and the semiconductor refrigeration device.
[0051] The silicon ore contains 30%-80% silicon (W / W), the fineness is 80 mesh-1200 mesh, the weight percentage of silicon ore and alkaline compound is 40-70:6-18, the reaction temperature is 150℃-500℃, and the reaction time is 1h-3h.
[0052] The beneficial effects of the present invention are: Due to the pretreatment of silicon-containing ore, i.e. micronization, water is added to expel the air in the pores of the solid mixture, making the material more uniform. During the melting reaction, water can increase the bubbles inside the silicon ore powder, and together with the flux, greatly reduce the melting temperature, achieve rapid alkali melting, and quickly convert the total silicon in the silicon ore into water-soluble silicon, with a conversion rate of 75%-85%. At the same time, the remaining total silicon is converted into citric acid-soluble silicon that can be absorbed by 2% citric acid, realizing the reasonable and efficient conversion of silicon in the silicon ore, and quick-acting fertilizer and effective slow-release fertilizer are obtained at the same time. The use of the two silicon fertilizers promotes crop growth and greatly improves crop quality. It can also improve the physical and chemical properties of the soil, increase soil bulk density, reduce soil compaction, and increase soil ventilation, water and fertilizer retention. It solves the current problems of low conversion rate of water-soluble silicon in mechanical mixing method, high cost of thermal method, and unstable product quality in production, and realizes the one-step process to produce high-conversion water-soluble silicon fertilizer and co-produce soluble silicon fertilizer, greatly reducing production costs, saving water and energy in the process, and no three wastes are discharged, meeting the green circular economy production.
[0053] While improving the soil, the present invention also has a good physiological stimulation effect on crops, which can enhance the vitality of the crop root system. The good development of the root system has a good improvement effect on the looseness, porosity and air permeability of the soil structure. It can increase the germination rate of wheat, corn and soybeans by more than 10%, and the emergence rate by more than 5%, ensuring the normal growth of crops throughout their life cycle until harvest.
[0054] The present invention has the outstanding characteristics of high silicon conversion rate in raw materials, cascade utilization of silicon ore, no discharge of three wastes, green environmental protection, low production cost, etc., and realizes circular economy and energy conservation and emission reduction in the production process. BRIEF DESCRIPTION OF THE DRAWINGS
[0055] Figure 1 A process flow chart of preparing fully water-soluble silicon fertilizer using silicon ore according to a specific embodiment of the present invention; Figure 2 This is a schematic diagram of the structure of a reaction device for preparing fully water-soluble silicon fertilizer from silicon ore according to a specific embodiment of the present invention; Figure 3 A top view of a reactor of a reaction device for preparing fully water-soluble silicon fertilizer from silicon ore according to a specific embodiment of the present invention; Figure 4The present invention is a schematic structural diagram of a nano bubble generating device for a reaction device for preparing fully water-soluble silicon fertilizer from silicon ore according to a specific embodiment of the present invention.
[0056] Figure 5 This is a comparison chart of the results of a wheat pot test using silicon ore to prepare a fully water-soluble silicon fertilizer according to a specific embodiment of the present invention. Figure 5 5(a), 5(b), 5(c), and 5(d) are comparison diagrams of the wheat pot test results of Examples 1-4, respectively. DETAILED DESCRIPTION
[0057] Example 1
[0058] Take 100g of silicon ore containing 50% total silicon, grind it to 80 mesh, mix it evenly with 5g of calcium fluoride and borax mixture (w / w=1:1), 10g of potassium hydroxide, and 2g of sodium hydroxide, add 15ml of water to the solid mixture, mix it evenly, place it for 15min, put the mixture into a heating furnace and react it at 500℃ for 1h, take it out, put it into 100mL of hot water, fully dissolve it, vacuum filter it, and the clear liquid is liquid water-soluble silicon fertilizer. The filter residue is dried and crushed to pass through a 200μm sieve, which is solid soluble silicon fertilizer. According to the relevant provisions of NY / T797-2004 and HG / T2830-2009, the sample test results are: liquid water-soluble silicon fertilizer is water-soluble SiO2=26.2%; water-insoluble matter is 0.3%; water content is 48.5%; solid soluble silicon fertilizer has a water content of 3%; effective SiO2=20.5%; fineness (passing a 250μm sieve) ≥80%.
[0059] The sample of Example 1 was taken and Xinjiang loam was used as the test material to carry out a wheat pot test. Figure 5 a) Compared with the control, wheat biomass yield increased by 7.5%, chlorophyll content increased by 12%, and soil bulk density increased by 8.7%.
[0060] Example 2 Take 100g of silicon ore containing 80% total silicon, grind it to 120 mesh, mix it with 3g of urea, 10g of potassium hydroxide, and 1g of sodium peroxide, add 10mL of water to the solid mixture, mix it evenly, place it for 15min, put it in a heating furnace and react at 400℃ for 0.5h, take it out, put it in 100mL of hot water, fully dissolve it, vacuum filter it, and the clear liquid is liquid water-soluble silicon fertilizer. Dry the filter residue and crush it to pass through a 200μm sieve, which is solid soluble silicon fertilizer. According to the relevant provisions of NY / T797-2004 and HG / T2830-2009, the sample test results are: liquid water-soluble silicon fertilizer is water-soluble SiO2=31.5%; water insoluble matter 0.4%; water 58.5%; solid soluble silicon fertilizer water 3%; effective SiO2=21.0%; fineness (passing 250μm sieve) ≥80%.
[0061] The sample of Example 2 was taken and soil from Xinjiang was used as the test material to carry out a rice pot test. Figure 5 b) Compared with the control, the rice biomass yield increased by 15%, the chlorophyll content increased by 20%, the soil bulk density increased by 8.7%, and the rice straw weight increased by 4.8%.
[0062] Example 3 Take 100g of silicon ore containing 30% total silicon, grind it to 1200 mesh, mix it evenly with 1g of borax, 1g of urea, 3g of sodium hydroxide, 10g of potassium hydroxide, and 1g of sodium peroxide, add 20mL of water to the solid mixture, mix it evenly, put it in a heating furnace at 200℃ for 4h after 20min, take it out, put it in 100mL of hot water, fully dissolve it, vacuum filter it, and the clear liquid is liquid water-soluble silicon fertilizer. The filter residue is dried and crushed to pass through a 200μm sieve, which is solid soluble silicon fertilizer. According to the relevant provisions of NY / T797-2004 and HG / T2830-2009, the sample test results are: liquid water-soluble silicon fertilizer is water-soluble SiO2=26.2%; water-insoluble matter is 0.3%; water content is 48.5%; solid soluble silicon fertilizer has a water content of 3%; effective SiO2=25.0%; fineness (passing a 250μm sieve) ≥80%.
[0063] The sample of Example 3 was taken and Xinjiang loam was used as the test material to carry out a rapeseed pot test. Figure 5 c) Compared with the control, the rapeseed biomass yield increased by 10%, the chlorophyll content increased by 12%, and the soil bulk density increased by 10%.
[0064] Example 4 Take 100g of silicon ore containing 60% total silicon, grind it to 200 mesh, mix it evenly with 1.5g of a mixture of calcium fluoride, borax, and urea (w / w / w=1:1:1) and 30g of a mixture of potassium hydroxide, sodium hydroxide, calcium oxide, sodium carbonate, and magnesium carbonate (mixing ratio 1:1:0.5:0.5:0.5), add 20mL of water to the solid mixture, mix it evenly, place it in a heating furnace for 30min, react at 300℃ for 2.5h, take it out, put it in 100mL of hot water, fully dissolve it, and filter it under vacuum. The clear liquid is liquid water-soluble silicon fertilizer. Dry the filter residue and crush it to pass a 200μm sieve, which is solid soluble silicon fertilizer. The test was carried out in accordance with the relevant regulations of NY / T797-2004 and HG / T2830-2009. The sample test results are as follows: liquid water-soluble silicon fertilizer has water-soluble SiO2 = 25%; water-insoluble matter 0.3%; moisture 46%; solid soluble silicon fertilizer has moisture 2.5%; effective SiO2 = 20.0%; fineness (passing 250μm sieve) ≥80%.
[0065] Samples from Example 4 were taken and soil from Xinjiang was used as the test material to carry out a rice pot test. Test results (see Figure 5 d) Compared with the control, the rice biomass yield increased by 20%, the chlorophyll content increased by 24.5%, the soil bulk density increased by 12.8%, and the rice straw weight increased by 8.6%.
[0066] The above descriptions are merely embodiments of the present invention and are not intended to limit the patent scope of the present invention. Any equivalent structure or equivalent process transformation made using the contents of the present invention specification and drawings, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present invention.
Claims
1. A method for preparing a silicon fertilizer mixture for soil improvement, characterized in that: The method comprises the following steps: using silicon ore powder containing 5%-90% (W / W) silicon and having a fineness of 40-1500 meshes, firstly mixing it with flux, alkaline compounds such as sodium hydroxide and a small amount of water, mixing evenly, standing and premixing, and then reacting, the weight percentage of silicon ore powder, flux, alkaline compound and water is 100 / (0.5-3.5) / (5-30) / (10-20), the standing time is 5-30 minutes, the reaction temperature is 50-600°C, the reaction time is 0.5h-4h, the reactant is dissolved in water, and then solid-liquid separation is performed, and the separated liquid is the fully water-soluble silicon fertilizer.
2. The method according to claim 1, characterized in that The silicon ore contains 30%-80% silicon (W / W), the fineness is 80 mesh-1200 mesh, the weight percentage of silicon ore powder, flux, alkaline compound and water is 100 / (1.5-3.5) / (10-30) / (10-20), the standing time is 10-30min, the reaction temperature is 150℃-500℃, and the reaction time is 1h-3h.
3. The method according to claim 1 or 2, characterized in that: The flux is one or a mixture of calcium fluoride, borax and urea, and the amount of the flux added is 1.5%-3% (wt).
4. The method according to claim 1 or 2, characterized in that: The silicon ore mainly exists in the form of silicon oxides and silicates. The silicon oxide ores mainly include sand, quartz, crystal, purple quartz, agate, flint and opal; the silicate ores mainly include granite, amphibole, asbestos, feldspar, clay and mica. The dry silicon dioxide content in the silicon ore is 10%-90% (W / W).
5. The method according to claim 1 or 2, characterized in that: The alkaline compound includes one or more of sodium hydroxide, potassium hydroxide, calcium oxide, magnesium oxide, sodium carbonate, potassium carbonate, sodium peroxide, calcium carbonate and magnesium carbonate.
6. The method according to claim 1 or 2, characterized in that: The quality indexes (wt) of the liquid silicon fertilizer are: water-soluble SiO2≥20%; water-insoluble matter≤0.5%; water content≤70%.
7. The method according to claim 1 or 2, characterized in that The fully water-soluble silicon fertilizer obtained by separation is dried to obtain powder particles, and the solid residue obtained by separation is dried to obtain solid soluble silicon fertilizer.
8. The method according to claim 7, characterized in that The quality indexes (wt) of the solid silicon fertilizer are: moisture ≤ 3%; effective SiO2 ≥ 20%; fineness passing through a 250 μm sieve ≥ 5%.
9. A device for preparing a silicon fertilizer mixture for soil improvement, using the method according to claims 1-8, characterized in that: The reaction device used in the reaction includes a reactor, a sample collector connected to the reactor and having a discharge port with a switch door, the switch door is used to close or open the discharge port according to whether unloading is required, and a plurality of nano bubble generating devices arranged around the reactor, each of which is connected to a corresponding spray device arranged on the wall of the reactor body, and sprays a mist feed containing nano bubbles into the reaction chamber of the reactor body; an ultrasonic device is arranged on the wall of the reactor body near the bottom of the reactor body; a first exhaust port is arranged on the top of the reactor body for connecting a reflux device during the reaction, a first stirring motor is eccentrically installed on the top of the reactor, and a first output shaft of the first stirring motor is connected to a first stirring rod, so that a first paddle at the end of the first stirring rod rotates to achieve stirring; in the reactor A molecular sieve is arranged at the bottom of the reactor body; the reactor and the sample collector are connected by a pipeline, and the end connected to the reactor is the lowest end allowed by the oily layer; a second exhaust port with a pressure relief valve is arranged on the top of the sample collector, and a steam outlet pipe is arranged near the top of the sample collector wall to connect the condensation reflux device and the solvent collector; a second stirring motor is also arranged on the top of the sample collector, and the second output shaft of the second stirring motor is connected to the second stirring rod, so that the second blade at the end of the second stirring rod rotates to achieve strong stirring of the white transparent liquid, and the steam conduit outlet is closed after the distillation is completed. The pressure relief valve is used to relieve the pressure on the sample collector when the strong stirring is completed after the distillation; a heating device is installed at the bottom of the sample collector, and the white transparent liquid is obtained by heating the recovered oily layer to perform reduced pressure distillation.
10. The device according to claim 9, characterized in that The nano bubble generating device comprises a feed pump and a venturi tube which are sequentially connected by pipelines along a feed direction, and a multi-head carrier gas manifold connected to the venturi tube, wherein the multi-head carrier gas manifold is connected to a carrier gas source via an air inlet pipe; the spray device comprises a spray head and a spray pipe connected to the spray head, wherein the spray pipe is connected to the outer wall of the reactor body; the ultrasonic device comprises an ultrasonic transducer rod, and a shell which closes one end of the ultrasonic transducer rod and is detachably sealed and connected to the outer wall of the reactor body, wherein the shell forms an acute angle with the central axis of the reactor body and extends the rod head deeply into the reaction chamber inside the reactor body.
Citation Information
Patent Citations
Method for treating flying ash through low-temperature molten sintering
CN103230924A
Medical stone water-soluble mineral silicon fertilizer
CN104761332A
Method for preparing fully-water-soluble silicon fertilizer from silicon ore
CN111116241A
Synthesis method of 2-chloronicotinic acid based on precious metal spinning catalytic cloth