Organic metal iridium complex, preparation method and organic electroluminescent device containing organic metal iridium complex

By introducing dibenzofuran into the organometallic iridium complex, the spatial symmetry is increased, and the problem of insufficient comprehensive characteristics of organic electroluminescent devices in terms of high efficiency, long life and low voltage is solved, and higher luminescence efficiency is achieved and lifespan and reduce the driving voltage.

CN118955568APending Publication Date: 2024-11-15JILIN OPTICAL & ELECTRONICS MATERIALS CO LTD
View PDF 0 Cites 2 Cited by

Patent Information

Application Number
CN202410989302.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-23
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

Existing organic electroluminescent devices have problems with insufficient comprehensive characteristics in terms of high efficiency, long life and low voltage.

Method used

An organic metal iridium complex is used, which increases its spatial symmetry and reduces molecular polarity by introducing dibenzofuran, thereby improving material stability, and preparing organic electroluminescent devices through specific synthetic methods.

Benefits of technology

Reduces the device's starting voltage and improves luminous efficiency and life.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118955568A_ABST
    Figure CN118955568A_ABST
Patent Text Reader

Abstract

The invention belongs to the field of organic electroluminescence, and provides an organic metal iridium complex, a preparation method and an organic electroluminescent device containing the organic metal iridium complex. The structural general formula of the organic metal iridium complex is as shown in formula L: # imgabs0. The invention provides the iridium complex, and after the organic metal compound is applied to the organic electroluminescent device, the starting voltage of the device is reduced, the luminous efficiency of the device is improved, and the service life of the device is prolonged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of organic electroluminescence, and in particular relates to an organic metal iridium complex, a preparation method and an organic electroluminescent device containing the same. Background Art

[0002] Organic electroluminescence (OLED) and related research As early as 1963, Pope et al. first discovered the electroluminescence phenomenon of organic compound single crystal anthracene. In 1987, Kodak Company in the United States used the method of evaporating organic small molecules to make an amorphous device, which reduced the driving voltage to less than 20V. OLED is a double-injection light-emitting device of holes and electrons, which directly converts electrical energy into light energy of organic semiconductor material molecules. Compared with traditional display devices such as CRT, LCD, PDP, OLED takes into account all the advantages of existing displays and has its own unique advantages. It has high brightness, high contrast, high definition, wide viewing angle, wide color gamut, etc. to achieve high-quality images, and has ultra-thin, ultra-light, low driving voltage, low power consumption, wide temperature and other characteristics to meet the needs of portable devices for lightness, power saving, and outdoor operation. Moreover, self-luminescence, high luminous efficiency, short response time, transparency, flexibility, etc. are the unique characteristics of OLED display. Therefore, OLED has been widely studied, developed and used.

[0003] In 1998, Forrest et al. from Princeton University in the United States found that by doping the phosphorescent dye octaethylporphyrin platinum into the main luminescent material, a light-emitting device with an external quantum efficiency of 4% and an internal quantum efficiency of 23% was prepared, which opened up a new field of phosphorescent electroluminescence, and in the following years, organic electrophosphorescence research has developed rapidly. As phosphorescent materials, precious metal complexes make full use of singlet and triplet excitons. Compared with fluorescent materials that only use singlet excitons, the effective utilization of triplet excitons, which accounts for up to 75%, enables PhOLED based on phosphorescent materials to achieve an internal quantum efficiency of 100%. Therefore, the research on high-efficiency phosphorescent organic electroluminescent devices has provided an important driving force for the development of flat panel and portable display industries.

[0004] Therefore, how to develop a high-performance phosphorescent material that enables an organic electroluminescent device to have comprehensive characteristics such as high efficiency, long life and low voltage is a technical problem that people in this field need to solve urgently. Summary of the invention

[0005] In view of this, the present invention provides an organic metal iridium complex, a preparation method and an organic electroluminescent device comprising the same. After the organic metal iridium complex is used in an organic electroluminescent device, it not only reduces the starting voltage of the device, but also improves the luminous efficiency and life of the device.

[0006] It should be noted that the present invention introduces dibenzofuran to give it a certain spatial symmetry, reduce the polarity between molecules and thus improve the stability of the material.

[0007] In order to achieve the above object, the present invention adopts the following technical solution:

[0008] The first technical purpose of the present invention is to provide an organometallic iridium complex, the general structural formula of the organometallic iridium complex is formula L:

[0009]

[0010] Among them, R 1 ~R 22 is a monosubstituted group, a disubstituted group, a trisubstituted group, a tetrasubstituted group or no substituted group; R 1 ~R 22 Each independently selected from -H, -D, -CN, -F, -CH 3 、-CD 3 , -CT 3 , -CF 3 、-CH 2 F, -CHF 2 , substituted or unsubstituted C1-C20 alkyl, substituted or unsubstituted C6-C12 aryl, substituted or unsubstituted methoxy, silane, germanium and combinations thereof.

[0011] Furthermore, the C1-C20 alkyl groups are each independently selected from a substituted or unsubstituted straight-chain alkyl group, a substituted or unsubstituted branched-chain alkyl group, and a substituted or unsubstituted cycloalkyl group.

[0012] Furthermore, the C1-C20 alkyl groups are partially or completely deuterated.

[0013] R 1 To R 22 Each independently selected from methyl, ethyl, CD 3 , propyl, butyl, pentyl, hexyl, C1-C6 alkyl substituted in whole or in part by deuterium, cyclopentyl, cyclohexyl, phenyl, -D, -CN, -F, -CT 3 , -CF 3 、-CH 2 F, -CHF 2 , methoxy, silane, germanium.

[0014] Ligand A is selected from one of the following structures LA-1 to LA-100:

[0015]

[0016]

[0017]

[0018]

[0019] In the above technical solution, the organometallic iridium complex is any one of the following structures, but is not limited thereto:

[0020]

[0021]

[0022]

[0023]

[0024]

[0025]

[0026]

[0027]

[0028]

[0029]

[0030]

[0031]

[0032]

[0033]

[0034]

[0035]

[0036]

[0037]

[0038]

[0039]

[0040]

[0041]

[0042]

[0043]

[0044]

[0045]

[0046]

[0047]

[0048]

[0049]

[0050]

[0051]

[0052]

[0053]

[0054]

[0055]

[0056]

[0057]

[0058]

[0059]

[0060]

[0061]

[0062]

[0063]

[0064]

[0065]

[0066]

[0067]

[0068]

[0069]

[0070]

[0071]

[0072]

[0073] Only some specific structural forms are listed above, but this series of organometallic iridium complexes are not limited to the above molecular structures. Other specific molecular structures can be obtained by simple changes of some simple groups and their substituted groups and substitution positions, which will not be described one by one here.

[0074] The second technical purpose of the present invention is to provide a method for preparing the organometallic iridium complex. The organometallic iridium complex of the present invention can be prepared by a synthetic method known to those skilled in the art, or preferably prepared by the following reaction process. The specific synthetic route is as follows:

[0075]

[0076] In the above formula, R 1 -R 22 As defined in formula I above.

[0077] For the synthesis of intermediate J, refer to patents KR1020170096769A and CN113121584A.

[0078] The specific preparation method is as follows:

[0079] Under nitrogen conditions, weigh raw material A, chloroform and acetic acid, and stir for 5 minutes; add NBS at room temperature and stir for 2 hours; add saturated brine, and obtain intermediate B by column chromatography.

[0080] Add raw material C, tetrakistriphenylphosphine palladium, potassium carbonate, tetrahydrofuran and water to intermediate B under nitrogen, and react at 90° C. for 24 h; separate the liquids, and perform spin-drying column chromatography to obtain intermediate D.

[0081] Potassium phosphate, xylene and dimethylformamide were added to intermediate D under nitrogen and refluxed for 12 h; the mixture was spin-dried, filtered through a funnel and recrystallized to obtain intermediate E.

[0082] Under nitrogen conditions, potassium carbonate and N-N-dimethylformamide were added to intermediate E and raw material F to react at 140° C. for 12 h; water and ethanol were added, and intermediate G was obtained by suction filtration and recrystallization.

[0083] Under nitrogen conditions, N-N-dimethylformamide, palladium acetate, and tricyclohexylphosphine were added to the intermediate G, and the mixture was reacted at 120° C. for 12 h. Water and ethanol were added, and the intermediate H was obtained by column chromatography and recrystallization.

[0084] Raw material I, tetrakistriphenylphosphine palladium, toluene, ethanol, water and potassium carbonate were added to intermediate H under nitrogen, and the mixture was reacted at 90° C. for 24 h. The liquid was separated and dried by rotary evaporation, and intermediate J was obtained by column chromatography.

[0085] Under nitrogen conditions, iridium trichloride, ethylene glycol ethyl ether and water were added to the intermediate J-1, reacted at 120°C for 48 hours, filtered and washed, and dried to obtain the intermediate J-2.

[0086] Silver trifluoromethanesulfonate, dichloromethane and isopropanol were added to the intermediate J-2 under nitrogen conditions, and the mixture was reacted at 25°C for 48 hours. The mixture was filtered through a silica gel funnel and dried by spin drying to obtain the intermediate J-3.

[0087] Under nitrogen conditions, intermediate J-3 and intermediate J were reacted in ethanol at 90° C. for 48 h, filtered, and column chromatography was performed to obtain formula L.

[0088] The third technical purpose of the present invention is to provide an organic electroluminescent device, which comprises an organic layer; the organic layer contains the organic metal iridium complex as described above.

[0089] Furthermore, the organic electroluminescent device further comprises a first electrode and a second electrode; the organic layer is disposed between the first electrode and the second electrode; wherein,

[0090] The organic layer comprises at least one of a hole injection layer, a hole transport layer, an electron blocking layer, a luminescence auxiliary layer, a luminescent layer, a hole blocking layer, an electron transport layer and an electron injection layer; and the luminescent layer comprises the organic metal iridium complex.

[0091] Specifically, the light-emitting layer comprises a host material and a doping material, and the organic metal iridium complex serves as the doping material.

[0092] Compared with the prior art, the present invention has the following beneficial effects:

[0093] The compound of the present invention adds dibenzofuran to the original dibenzofuran, so that the compound has a certain spatial symmetry, reduces the polarity between molecules, thereby improving the stability of the material, reducing the driving voltage of the device, and significantly improving the luminous efficiency and lifespan. DETAILED DESCRIPTION

[0094] The technical solutions in the embodiments of the present invention are described clearly and completely below. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0095] The embodiments of the present invention disclose a method for preparing an organic metal iridium complex and an organic electroluminescent device containing the same.

[0096] In addition, it should be noted that the numerical values ​​given in the following examples are as accurate as possible, but those skilled in the art understand that due to unavoidable measurement errors and experimental operation problems, each number should be understood as an approximate number rather than an absolutely accurate value.

[0097] Example 1: Preparation of organometallic compound L-181

[0098] The specific operation and process route are as follows:

[0099]

[0100] Step 1: Under nitrogen conditions, weigh raw material A-181 (CAS No.: 582-17-2625mmol), 1.5L of chloroform, and 600mL of acetic acid, and stir for 5 minutes; add NBS (635mmol) at room temperature and stir for 2 hours; add saturated brine (700mL) and obtain intermediate B-181 (120g, yield 81%) by column chromatography.

[0101] HPLC purity:>99.0%

[0102] Mass spectrum: Test value 237.96

[0103]

[0104] Step 2: Under nitrogen conditions, weigh the intermediate B-181 (502 mmol), raw material C-181 (CAS number: 1993-03-9502 mmol), tetrakistriphenylphosphine palladium (5 mmol), potassium carbonate (1.5 mol), tetrahydrofuran (1.2 L), and water (600 mL) and react at 90°C for 24 hours; separate the liquids, and spin dry column chromatography to obtain the intermediate D-181 (72 g, yield 57%).

[0105] HPLC purity:>99.0%

[0106] Mass spectrum: Test value 254.08

[0107] Step 3: Under nitrogen conditions, weigh the intermediate D-181 (283 mmol), potassium phosphate (0.85 mol), xylene 720 mL, and dimethylformamide 360 ​​mL, and reflux for 12 hours; spin dry, pass through a funnel, and recrystallize to obtain the intermediate E-181 (37 g, yield 52%).

[0108] HPLC purity:>99.0%

[0109] Mass spectrum: Test value 234.09

[0110] The second and third steps refer to patent KR1020170096769A

[0111]

[0112] Step 4: Under nitrogen conditions, weigh the intermediate E-181 (158 mmol), F-181 (CAS No.: 883499-24-9158 mmol), potassium carbonate (237 mmol), NN dimethylformamide 560 mL, react at 140 ° C for 12 hours; add water and ethanol, filter and recrystallize to obtain the intermediate G-181 (34 g, yield 52%).

[0113] HPLC purity:>99.0%

[0114] Mass spectrum: Test value 421.99

[0115] Step 5: Under nitrogen conditions, weigh the intermediate G-181 (80.1 mmol), NN dimethylformamide 340 mL, palladium acetate (1.6 mmol), tricyclohexyl phosphine (1.7 mmol), and react at 120°C for 12 h; add water, ethanol, column chromatography, and recrystallize to obtain the intermediate H-181 (19 g, yield 56%).

[0116] Mass spectrum: Test value 342.05

[0117] Step 4 Step 5 Reference Patent CN113121584A

[0118]

[0119] Step 6: Under nitrogen, weigh the intermediate H-181 (55 mmol), I-181 (CAS No.: 197958-29-582.9 mmol), tetrakistriphenylphosphine palladium (1.1 mmol), toluene 190 mL, ethanol 190 mL, water 95 mL, potassium carbonate (166 mmol), react at 90 ° C for 24 hours, separate and dry, and column chromatography to obtain intermediate J-181 (14.9 g, yield 70%)

[0120] HPLC purity:>99.0%

[0121] Mass spectrum: Test value 385.12

[0122]

[0123] Step 7: Under nitrogen conditions, weigh the raw material J-181-1 (CAS No.: 1622235-49-7 59.8 mmol), iridium trichloride (27.2 mmol), ethylene glycol ether 200 mL, and water 67 mL, react at 120°C for 48 hours, filter and wash, and dry to obtain the intermediate J-181-2 (12.5 g, yield 80%).

[0124] Step 8: Under nitrogen conditions, weigh the raw material J-181-2 (10.6 mmol), silver trifluoromethanesulfonate (23.3 mmol), 242 mL of dichloromethane, and 60 mL of isopropanol, react at 25°C for 48 hours, pass through a silica gel funnel, and spin dry to obtain the intermediate J-181-3 (12 g, yield 75%).

[0125]

[0126] Step 9: Under nitrogen conditions, weigh the raw materials J-181-3 (14.4 mmol), J-181 (36 mmol), and 220 mL of ethanol, react at 90°C for 48 hours, and filter and column chromatograph to obtain the final product L-181 (7.97 g, yield 60%).

[0127] HPLC purity:>99.3%

[0128] Mass spectrum: Test value 919.28

[0129] Elemental Analysis:

[0130] Calculated values: C, 66.65%; H, 4.39%; N, 4.57%; O, 3.48%.

[0131] Measured values: C, 66.54%; H, 4.38%; N, 4.55%; O, 3.47%

[0132] NMR: 1H NMR(400MHz,Chloroform-d)δ8.68(dd,1H),8.33(d,z,2H),8.11(dd,2H),7.99(dd,,1H),7.93(dd,1H),7.76(dd,,1H),7.68(dt,,3H) ,7.67-7.62(m,2H),7.62-7.54(m,3H),7.50(d,1H),7.49-7.40(m,3H),7.39-7.30(m,3H),7.28(td,2H),7.23(td,,1H),7.13(td,2H).

[0133] Example 2: Preparation of organometallic compound L-379

[0134] The single ligand synthesis process, steps 1 to 6, is the same as that of L-181 and will not be repeated here.

[0135]

[0136] Step 7: Under nitrogen conditions, weigh the raw material J-379-1 (CAS No.: 1008-89-5 96.6mmol), iridium trichloride (32.2mmol), ethylene glycol ether 220mL, water 73mL, react at 120℃ for 48h, filter and wash, and dry to obtain the intermediate J-379-2 (14.1g, yield 82%).

[0137] Step 8: Under nitrogen conditions, weigh the raw material J-379-2 (11.2 mmol), silver trifluoromethanesulfonate (24.6 mmol), 240 mL of dichloromethane, and 60 mL of isopropanol, react at 25°C for 48 hours, pass through a silica gel funnel, and spin dry to obtain the intermediate J-379-3 (12.9 g, yield 81%).

[0138]

[0139] Step 9: Under nitrogen conditions, weigh the raw materials J-379-3 (14.5 mmol), J-379 (36 mmol), and 220 mL of ethanol, react at 90°C for 48 hours, and filter and column chromatograph to obtain the final product L-379 (8.36 g, 65% yield).

[0140] HPLC purity:>99.3%

[0141] Mass spectrum: Test value 885.21

[0142] Elemental Analysis:

[0143] Calculated values: C, 66.65%; H, 3.42%; %; N, 4.57%; O, 3.62%.

[0144] Measured values: C, 66.67%; H, 3.44%; N, 4.58%; O, 3.68%

[0145] NMR: 1 H NMR(400MHz,Chloroform-d)δ8.68(dd,1H),8.66-8.62(m,2H),8.09(dd,2H),7.99(dd,1H),7.93(dd,1H),7.79-7.64(m,6H) ,7.62-7.54(m,3H),7.49-7.42(m,3H),7.43(d,1H),7.39-7.27(m,3H),7.31-7.21(m,4H),7.25-7.20(m,1H),7.13(td,2H).

[0146] Example 3: Preparation of organometallic compound L577

[0147] The single ligand synthesis process, steps 1 to 6, is the same as that of L-181 and will not be repeated here.

[0148]

[0149] Step 7: Under nitrogen conditions, weigh the raw material J-577-1 (CAS No.: 27012-22-2 96.3mmol), iridium trichloride (32.1mmol), ethylene glycol ethyl ether 218mL, and water 71mL, react at 120℃ for 48h, filter and wash, and dry to obtain the intermediate J-577-2 (13.8g, yield 82%).

[0150] Step 8: Under nitrogen conditions, weigh the raw material J-577-2 (11.1 mmol), silver trifluoromethanesulfonate (24.4 mmol), 238 mL of dichloromethane, and 60 mL of isopropanol, react at 25°C for 48 hours, pass through a silica gel funnel, and spin dry to obtain the intermediate J-577-3 (12.5 g, yield 78%).

[0151]

[0152] Step 9: Under nitrogen conditions, weigh the raw materials J-577-3 (14.2 mmol), J-577 (35.8 mmol), and 219 mL of ethanol, react at 90°C for 48 hours, and filter and column chromatograph to obtain the final product L-577 (7.87 g, yield 59%).

[0153] HPLC purity:>99.3%

[0154] Mass spectrum: Test value 913.26

[0155] Elemental Analysis:

[0156] Calculated values: C, 67.09%; H, 3.75%; N, 4.60%; O, 3.50%.

[0157] Measured values: C, 67.10%; H, 43.76%; N, 4.61%; O, 3.51%

[0158] NMR: 1 H NMR(400MHz,Chloroform-d)δ8.68(dd,1H),8.41(d,2H),8.11(dd,J=7.4,1.5Hz,2H),7.99(dd,1H),7.93(dd,1H),7. 76(dd,,1H),7.71-7.64(m,3H),7.62-7.54(m,5H),7.49-7.40(m,4H),7.39-7.20(m,6H),7.13(td,2H),2.28(s,6H).

[0159] Example 4: Preparation of organometallic compound L-595

[0160] The single ligand synthesis process, steps 1 to 6, is the same as that of L-181 and will not be repeated here.

[0161]

[0162] Step 7: Under nitrogen, weigh J-595-1 (CAS No.: 27012-22-2 73.2 mmol), dimethyl sulfoxide 123 mL, sodium hydroxide (146 mmol), react at 90 ° C for 48 h, separate and spin dry through a funnel to obtain intermediate J-595-2 (17 g, yield 85%)

[0163] Step 8: Under nitrogen, weigh the raw material J-595-2 (60.2 mmol), iridium trichloride (27.4 mmol), ethylene glycol ether 192 mL, water 64 mL, react at 120 ° C for 48 hours, filter and wash, and dry to obtain the intermediate J-595-3 (16.9 g, yield 78%).

[0164] Step 9: Under nitrogen conditions, weigh the raw material J-595-3 (10.1 mmol), silver trifluoromethanesulfonate (22.4 mmol), 320 mL of dichloromethane, and 59 mL of isopropanol, react at 25°C for 48 hours, pass through a silica gel funnel, and spin dry to obtain the intermediate J-595-4 (14.1 g, yield 68%)

[0165]

[0166] Step 10: Under nitrogen conditions, weigh the raw materials J-595-4 (14.5 mmol), J-595 (36 mmol), and 219 mL of ethanol, react at 90°C for 48 hours, and filter and column chromatograph to obtain the final product L-595 (10.93 g, 63% yield).

[0167] HPLC purity:>99.3%

[0168] Mass spectrum: Test value 1139.49

[0169] Elemental Analysis:

[0170] Calculated values: C, 70.62%; H, 6.01%; N, 3.69%; O, 2.81%.

[0171] Measured values: C, 70.64%; H, 6.03%; N, 3.70%; O, 2.82%

[0172] NMR: 1 H NMR(400MHz,Chloroform-d)δ8.68(dd,1H),8.29(s,2H),7.98(d,1H),7.94(dd,J=7.6,1H),7.77(ddd,2H),7.67(td ,1H),7.60-7.54(m,5H),7.53-7.45(m,4H),7.47-7.38(m,5H),7.38-7.30(m,5H),7.30-7.24(m,4H),7.23(td,1H).

[0173] Example 5: Preparation of organometallic compound L-757

[0174] The single ligand synthesis process, steps 1 to 6, is the same as that of L-181 and will not be repeated here.

[0175]

[0176] Step 7: Weigh the raw materials J-757-1 (CAS No.: 701261-35-0 490mmol), J-757-2 (CAS No.: 53939-30-3 490mmol), potassium carbonate (1.4mol), toluene 500mL, ethanol 250mL, react at 70℃ for 8h, spin dry column chromatography to obtain intermediate J-757-3 (63g, yield 70%).

[0177] HPLC purity:>99%

[0178] Mass spectrum: Test value 183.09

[0179]

[0180] Step 8: Weigh the raw materials J-757-3 (342 mmol), J-757-4 (CAS No.: 5720-05-8 342 mmol), potassium carbonate (1.02 mol), 630 mL of toluene, 315 mL of ethanol, and 315 mL of water, react at 90°C for 12 h, and spin dry column chromatography to obtain the intermediate J-757-5 (53 g, yield 65%).

[0181] HPLC purity:>99%

[0182] Mass spectrum: Test value 239.18

[0183] Step 9: Weigh the raw material J-757-5 (221 mmol), potassium hydroxide (442 mmol), and dimethyl sulfoxide 280 mL, react at 90°C for 48 h, separate the liquids, and spin dry the column to obtain the intermediate J-757-6 (27.5 g, yield 50.9%).

[0184]

[0185] Step 10: Under nitrogen conditions, weigh the raw material J-757-6, iridium trichloride (50.3 mmol), ethylene glycol ethyl ether 514 mL, and water 171 mL, react at 120°C for 48 hours, filter and wash, and dry to obtain the intermediate J-757-7 (22.2 g, yield 60%).

[0186] Step 11: Under nitrogen conditions, weigh the raw material J-757-7 (15.3 mmol), silver trifluoromethanesulfonate (33.8 mmol), 440 mL of dichloromethane, and 89 mL of isopropanol, react at 25°C for 48 hours, pass through a silica gel funnel, and spin dry to obtain the intermediate J-757-8 (17.5 g, yield 60%).

[0187]

[0188] Step 12: Under nitrogen conditions, weigh the raw materials J757-8 (14.5 mmol), J-757 (36 mmol), and 219 mL of ethanol, react at 90°C for 48 hours, and filter and column chromatograph to obtain the final product L-757 (9.54 g, 62% yield).

[0189] HPLC purity:>99.3%

[0190] Mass spectrum: Test value 1063.46

[0191] Elemental Analysis:

[0192] Calculated values: C, 68.90%; H, 6.06%; N, 3.95%; O, 3.01%.

[0193] Measured values: C, 68.92%; H, 6.07%; N, 3.96%; O, 3.03%

[0194] NMR: 1 H NMR(400MHz,Chloroform-d)δ8.70(dd,,1H),8.25(d,,2H),8.21(d,1H),8.13(s,1H),8.05-8.02(m,1H),8.00(d,1H),7.96-7.85(m,5H),7. 83(d,,2H),7.65(dd,1H),7.57(dd,,2H),7.49-7.42(m,2H),7.35(d,3H),7.32(dd2H),7.31-7.28(m,1H),7.28-7.22(m,1H),1.19(s,18H).

[0195] The synthesis methods of other organometallic iridium complexes L-217, L-398, L-542, L-614, and L-848 are the same as those in the above embodiments and are not described in detail here. The molecular formula and mass spectrum of the synthesized organometallic iridium complexes are shown in Table 1 below.

[0196] Table 1

[0197]

[0198]

[0199] Device Embodiment

[0200] Device Example 1: Preparation of an organic electroluminescent device using an organometallic compound of formula L-181

[0201] The coating thickness is The ITO glass substrate was cleaned twice in distilled water and ultrasonically washed for 30 minutes. After the distilled water cleaning, it was ultrasonically cleaned in sequence with isopropanol, acetone, methanol and other solvents, and then dried and transferred to a plasma cleaning machine. The above substrate was washed for 5 minutes and sent to a vapor deposition machine.

[0202] First, the thickness of the ITO (anode) vapor deposition is 4,4',4"-tri[2-naphthylphenylamino]triphenylamine ("2-TNATA") is used as a hole injection layer, and then a layer with a thickness of 1000 nm is deposited on the hole injection layer. N,N'-diphenyl-N,N'-(1-naphthyl)-1,1'-biphenyl-4,4'-diamine (NPB) is used as the hole transport layer, followed by evaporation with a thickness of The main material 4,4'-N,N'-biphenyl dicarbazole ("CBP") and the dopant material compound L-181 weight ratio of 90:10 are then evaporated on the light-emitting layer with a thickness of ALq 3 As the electron transport layer, a layer with a thickness of The electron injection layer material Liq is finally deposited on the electron injection layer with a thickness of By adding Al as cathode material, an organic electroluminescent device can be obtained.

[0203] The performance luminescence characteristics of the obtained device were tested using a KEITHLEY 2400 source measurement unit and a CS-2000 spectroradiometer to evaluate the driving voltage, lifespan, and luminous efficiency.

[0204] Device Comparative Example 1: An organic electroluminescent device was prepared in the same manner as in Device Example L-181, and the structure of the green light-emitting doping compound in the light-emitting layer was as follows:

[0205]

[0206] Device Comparative Example 2: An organic electroluminescent device was prepared in the same manner as in Device Example L-181, and the structure of the green light-emitting doping compound in the light-emitting layer was as follows:

[0207]

[0208] Device Comparative Example 3: An organic electroluminescent device was prepared in the same manner as in Device Example L-181. The structure of the green light-emitting doping compound in the light-emitting layer is as follows:

[0209]

[0210] Device Comparative Example 4: An organic electroluminescent device was prepared in the same manner as in Device Example L-181. The structure of the green light-emitting doping compound in the light-emitting layer is as follows:

[0211]

[0212] Device Comparative Example 5: An organic electroluminescent device was prepared in the same manner as in Device Example L-181. The structure of the green light-emitting doping compound in the light-emitting layer is as follows:

[0213]

[0214] Device Comparative Example 6: An organic electroluminescent device was prepared in the same manner as in Device Example L-181. The structure of the green light-emitting doping compound in the light-emitting layer is as follows:

[0215]

[0216] Device Comparative Example 7: An organic electroluminescent device was prepared in the same manner as in Device Example L-181. The structure of the green light-emitting doping compound in the light-emitting layer is as follows:

[0217]

[0218] Device Example 2: Refer to the method of the above device example L-181, the only difference is that the doping material L-181 is replaced by L-379.

[0219] Device Example 3: Refer to the method of the above device example L-181, the only difference is that the doping material L-181 is replaced by L-577.

[0220] Device Example 4: Refer to the method of the above device example L-181, the only difference is that the doping material L-181 is replaced by L-595.

[0221] Device Example 5: Refer to the method of the above device example L-181, the only difference is that the doping material L-181 is replaced by L-757.

[0222] Device Example 6: Refer to the method of the above device example L-181, the only difference is that the doping material L-181 is replaced by L-217.

[0223] Device Example 7: Refer to the method of the above-mentioned device example L-181, the only difference is that the doping material L-181 is replaced by L-398.

[0224] Device Example 8: Refer to the method of the above-mentioned device example L-181, the only difference is that the doping material L-181 is replaced by L-542.

[0225] Device Example 9: Refer to the method of the above device example L-181, the only difference is that the doping material L-181 is replaced by L-614.

[0226] Device Example 10: Refer to the method of the above-mentioned device example L-181, the only difference is that the doping material L-181 is replaced by L-848.

[0227] The driving voltage, luminous efficiency and life of the organic electroluminescent devices obtained from the above device embodiments and device comparative examples were characterized at a brightness of 2000 (nits). The test results are shown in Table 2 below.

[0228] Table 2

[0229] Devices Driving voltage(V) Luminous efficiency (cd / A) <![CDATA[T 95 (h)]]> Comparative Example 1 4.05 40.4 527 Comparative Example 2 3.95 48.5 613 Comparative Example 3 4.10 46.2 588 Comparative Example 4 3.99 49.6 609 Comparative Example 5 3.89 47.3 596 Comparative Example 6 3.88 48.6 588 Comparative Example 7 3.79 49.3 590 Device Example 1 3.43 73.4 ,854 Device Example 2 3.35 66.1 802 Device Example 3 3.54 62.6 756 Device Example 4 3.49 78.3 796 Device Example 5 3.34 72.6 873 Device Example 6 3.50 68.1 795 Device Example 7 3.48 67.4 783 Device Example 8 3.55 67.8 793 Device Example 9 3.42 68.8 789 Device Example 10 3.51 69.2 778

[0230] It can be seen from Table 2 that, when the dual ligands are the same and at the same brightness, by adding dibenzofuran to the original dibenzofuran, a certain spatial symmetry is obtained, the polarity between the molecules is reduced, and the stability of the material is improved. As a result, the organic electroluminescent device prepared by using the compound of the present application as a doping material for the light-emitting layer has a significantly lower driving voltage, and the luminous efficiency and life are significantly improved compared with the organic electroluminescent device prepared in the comparative example.

[0231] The above description of the disclosed embodiments enables one skilled in the art to implement or use the present invention. Various modifications to these embodiments will be apparent to one skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but rather to the widest scope consistent with the principles and novel features disclosed herein.

Claims

1. An organometallic iridium complex, characterized in that: The general structural formula of the organometallic iridium complex is Formula L: Among them, R1~R 22 is a monosubstituted group, a disubstituted group, a trisubstituted group, a tetrasubstituted group or no substituted group; R1~R 22 Each is independently selected from -H, -D, -CN, -F, -CH3, -CD3, -CT3, -CF3, -CH2F, -CHF2, substituted or unsubstituted C1-C20 alkyl, substituted or unsubstituted C6-C12 aryl, substituted or unsubstituted methoxy, silane, germanium and combinations thereof.

2. The organometallic iridium complex according to claim 1, characterized in that The C1-C20 alkyl groups are each independently selected from a substituted or unsubstituted straight-chain alkyl group, a substituted or unsubstituted branched-chain alkyl group, and a substituted or unsubstituted cycloalkyl group.

3. The organometallic iridium complex according to claim 1 or 2, characterized in that: The C1-C20 alkyl groups are partially or completely deuterated.

4. The organometallic iridium complex according to claim 1 or 2, characterized in that R1~R 22 Each is independently selected from methyl, ethyl, CD3, propyl, butyl, pentyl, hexyl, C1-C6 alkyl fully or partially substituted by deuterium, cyclopentyl, cyclohexyl, phenyl, -D, -CN, -F, -CT3, -CF3, -CH2F, -CHF2, methoxy, silanyl, germanium.

5. The organometallic iridium complex according to claim 4, characterized in that Ligand A is selected from one of the following structures LA-1 to LA-100: 。 6. The organometallic iridium complex according to claim 1, characterized in that The organometallic iridium complex is any one of the following structures, but is not limited thereto:

7. A method for preparing an organometallic iridium complex as claimed in claim 1, characterized in that: The method specifically comprises the following steps: (1): The specific synthetic route is as follows: Under nitrogen conditions, weigh raw material A, chloroform, and acetic acid, and stir for 5 minutes; add NBS at room temperature and stir for 2 hours; add saturated brine, and obtain intermediate B by column chromatography; Add raw material C, tetrakistriphenylphosphine palladium, potassium carbonate, tetrahydrofuran and water to intermediate B under nitrogen and react at 90°C for 24h; Separate the liquid, spin dry and column chromatography to obtain intermediate D; Potassium phosphate, xylene and dimethylformamide were added to intermediate D under nitrogen and refluxed for 12 hours; The product was spin-dried, passed through a funnel, and recrystallized to obtain intermediate E; Under nitrogen conditions, potassium carbonate and N-N-dimethylformamide were added to the intermediate E and the raw material F to react at 140°C for 12 hours; water and ethanol were added, and the intermediate G was obtained by suction filtration and recrystallization; Add N-N-dimethylformamide, palladium acetate, and tricyclohexylphosphine to the intermediate G under nitrogen conditions, and react at 120°C for 12 hours; add water and ethanol, column chromatography, and recrystallize to obtain the intermediate H; Add raw material I, tetrakistriphenylphosphine palladium, toluene, ethanol, water, potassium carbonate to intermediate H under nitrogen, react at 90°C for 24h, separate the liquid and dry it by spin drying, and obtain intermediate J by column chromatography; Add iridium trichloride, ethylene glycol ethyl ether and water to the intermediate J-1 under nitrogen, react at 120°C for 48h, filter and wash, and dry to obtain the intermediate J-2; Silver trifluoromethanesulfonate, dichloromethane, and isopropanol were added to the intermediate J-2 under nitrogen conditions, and the mixture was reacted at 25°C for 48 hours. The mixture was filtered through a silica gel funnel and dried by spin drying to obtain the intermediate J-3. Under nitrogen conditions, intermediate J-3 and intermediate J were reacted in ethanol at 90° C. for 48 h, filtered, and column chromatography was performed to obtain formula L. Among them, R 1- R 22 Having the definition as claimed in claim 1.

8. An organic electroluminescent device, characterized in that: The organic electroluminescent device comprises an organic layer; the organic layer contains the organic metal iridium complex as claimed in claim 1.

Citation Information

Cited By

  • Organic metal iridium complex, preparation method thereof, luminescent material and organic electroluminescent device

    CN120504701A

  • Organometallic iridium complexes, methods for their preparation, luminescent materials and organic electroluminescent devices

    CN120504701B