Wire drawing lubricant powder with high lubricating activity
By adding mica powder and animal and plant oil and fat to the brushed lubricant, and performing step-by-step grinding and drying during the preparation process, the problem of insufficient temperature and corrosion resistance of finished products in the prior art is solved, and the lubricant is improved physical properties and finished product quality.
Patent Information
- Application Number
- CN202411009364.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-26
- Publication Date
- 2024-11-15
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing brushed lubricant has no mica formula in the raw materials, which cannot improve the overall temperature and corrosion resistance of the finished product. At the same time, the preparation process does not perform step-by-step grinding of raw materials with different particle diameters, affecting the quality of the finished product.
Use animal and plant mixture formulas to mix oils, mica powder, paraffin, talc, microsilicon powder, stearic acid, mineral powder and preservatives, and improve particle fineness through specific mixing and grinding steps, including controlling temperature in the mixing device and mixing rate, grind and sieved powder, add preservative and drying.
It improves the high temperature resistance, corrosion resistance and adhesion properties of lubricating powder, ensures high lubricating activity, and improves the raw material grinding effect and finished product quality through particle size.
Smart Images

Figure CN118956475A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of lubricating powders, and in particular relates to a wire drawing lubricating powder with high lubricating activity. Background Art
[0002] Lubricating powder is a powdered lubricating material that can reduce friction and wear of mechanical equipment. Lubricating powder is usually a mixture of metal powder, graphite and other additives. It can be divided into oil powder and water powder according to the type of mixed oil. Lubricating powder can maintain stable running under high temperature and high pressure environment, and can withstand heavy loads and high-speed movement. The main use of lubricating powder is in manufacturing and industrial fields, such as bearing lubrication, machine parts assembly, metal forming and forging, etc. Lubricating powder is also needed when drawing metal wire.
[0003] China's patent discloses (CN111748397A) a wire drawing powder for metal wire and its preparation method. Nano silica powder and diatom mud are added to calcium stearate to prepare wire drawing powder. It can not only ensure the lubrication performance of wire drawing powder and reduce the friction coefficient of metal wire drawing process, but also make wire drawing powder have high temperature resistance, which can ensure that the surface of metal wire does not coke for a long time, prolong the drawing and lubrication performance. At the same time, on the basis of traditional wire drawing powder, the amount of wire drawing powder raw material used is reduced, and the cost is reduced; combined with the addition of sodium nitrite, the surface film forming efficiency of metal wire is high, the adhesion and anti-rust ability of wire drawing powder are enhanced, and the drawing quality of metal wire is improved. Although the current wire drawing lubricating powder can also play a good lubricating role, its raw material does not have a mica formula, and the overall temperature resistance and corrosion resistance of the finished product cannot be improved. At the same time, during the preparation, the raw materials with different particle diameters are not ground step by step, and the particle fineness of the raw materials cannot be improved, which affects the quality of the finished product. In order to solve this problem, a wire drawing lubricating powder with high lubrication activity is urgently needed. Summary of the invention
[0004] The purpose of the present invention is to propose a wire drawing lubricating powder with high lubrication activity to solve the problem that although the current wire drawing lubricating powder can also play a good lubricating role, its raw materials do not contain a mica formula, and the overall temperature resistance and corrosion resistance of the finished product cannot be improved. At the same time, during the preparation, the raw materials with different particle diameters are not ground in steps, and the particle fineness of the raw materials cannot be improved, which affects the quality of the finished product.
[0005] In order to achieve the above purpose, the present invention adopts the following technical scheme: a wire drawing lubricating powder with high lubricating activity, comprising the following materials: mixed animal and plant oils, mica powder, paraffin, talcum powder, microsilica powder, stearic acid, mineral powder and preservatives.
[0006] As a further description of the above technical solution:
[0007] The weight proportions of the animal fat, sodium soap, vegetable fat, stearic acid, brightener, anti-wear extreme pressure agent, antioxidant and dispersant are 12-15 parts, 5-8 parts, 6-7 parts, 4-7 parts, 5-6 parts, 8-10 parts, 6-8 parts and 2-5 parts respectively.
[0008] This article also discloses a method for preparing a wire drawing lubricating powder with high lubricating activity, comprising the following steps:
[0009] S1, taking animal and plant mixed fats and paraffin and placing them in a mixing device, raising the temperature in the mixing device, and waiting for the animal and plant mixed fats and paraffin to melt;
[0010] S2, add stearic acid and mica powder into the mixing device, control the mixing rate of the mixing device, and keep warm and mix for a period of time;
[0011] S3, taking mineral powder, talcum powder and microsilica powder and placing them in a grinding device in sequence, grinding the mixed materials, and keeping a certain time interval between grinding and adding the raw materials;
[0012] S4, sieving the grinding material, taking the grinding material into a mixing device, adding a preservative into the mixing device, and mixing for a period of time;
[0013] S5, gradually increase the temperature in the mixing device to gradually dry the mixture until the humidity of the mixture is maintained at a certain level, stop heating, and wait for the mixture to cool and be taken out;
[0014] S6, putting the mixed material obtained in S2 and the mixed material obtained in S5 into a mixing device at the same time, raising the temperature in the mixing device, and mixing for a period of time;
[0015] S7, after mixing, filtering the mixed material and collecting the solid mixed material;
[0016] S8, placing the solid mixture in a drying device and providing a certain temperature to quickly dry it into a powder form;
[0017] S9. Collect and store the finished products.
[0018] As a further description of the above technical solution:
[0019] In S1, the animal and plant mixed fats and paraffin are placed in a mixing device, the temperature in the mixing device is increased to 120-140° C., and the animal and plant mixed fats and paraffin are melted.
[0020] As a further description of the above technical solution:
[0021] In S2, stearic acid and mica powder are added into a mixing device, the mixing speed of the mixing device is controlled to 100-120 r / min, and the mixture is mixed at a temperature-insulated temperature for 5-10 minutes.
[0022] As a further description of the above technical solution:
[0023] In S3, mineral powder, talcum powder and microsilica powder are placed in a grinding device in sequence, and the mixed material is ground. The time interval between grinding and adding the raw materials is 5-8 minutes.
[0024] As a further description of the above technical solution:
[0025] In S4, the ground material is sieved, and the ground material is placed in a mixing device, and a preservative is added to the mixing device, and mixed for 15-20 minutes.
[0026] As a further description of the above technical solution:
[0027] In S5, the temperature in the mixing device is gradually increased at a rate of 10-15°C / min, so that the mixed material is gradually dried until the humidity of the mixed material is maintained at a certain level and the temperature is stopped to wait for the mixed material to be cooled and taken out.
[0028] As a further description of the above technical solution:
[0029] In S6, the mixed material obtained in S2 and the mixed material obtained in S5 are simultaneously put into a mixing device, the temperature in the mixing device is increased to 130-150r / min, and mixing is performed for 30-35min.
[0030] As a further description of the above technical solution:
[0031] In S8, the solid mixed material is placed in a drying device and provided with a temperature of 75-85° C. to be quickly dried into a powder.
[0032] In summary, due to the adoption of the above technical solution, the beneficial effects of the present invention are:
[0033] The lubricating powder adopts mica in the formula. Mica has good high temperature resistance and corrosion resistance, and can effectively improve the physical properties of the finished product. At the same time, the mica powder also has strong adhesion, can be closely combined with other materials, and provide good adhesion performance, so that the lubricating powder can effectively maintain high lubrication activity. At the same time, the formula is also provided with animal and plant mixed oils and fats, which have better lubrication effect and can also ensure the environmental protection of the finished product. At the same time, in the preparation method, the particle size of the powder to be ground is distinguished, and different powders are put into the grinding device for grinding by setting the adding time sequence, which can improve the grinding effect and uniformity of the raw materials and improve the quality of the final product. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] Figure 1 The present invention is a flow chart of a method for preparing a wire drawing lubricating powder with high lubricating activity. DETAILED DESCRIPTION
[0035] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0036] Example 1
[0037] See also Figure 1 The present invention provides a technical solution: a wire drawing lubricating powder with high lubricating activity, comprising the following materials: mixed animal and plant oils, mica powder, paraffin, talcum powder, microsilica powder, stearic acid, mineral powder and preservatives, with the weight proportions being 12-15 parts, 5-8 parts, 6-7 parts, 4-7 parts, 5-6 parts, 8-10 parts, 6-8 parts and 2-5 parts respectively.
[0038] This article also discloses a method for preparing a wire drawing lubricating powder with high lubricating activity, comprising the following steps:
[0039] S1, take animal and plant mixed fats and paraffin and place them in a mixing device, increase the temperature in the mixing device to 120°C, and wait for the animal and plant mixed fats and paraffin to melt;
[0040] S2, add stearic acid and mica powder into the mixing device, control the mixing speed of the mixing device to 100r / min, and keep warm and mix for 5min;
[0041] S3, taking mineral powder, talcum powder and microsilica powder and placing them in a grinding device in sequence, grinding the mixed materials, and keeping a time interval of 5-8 minutes between grinding and adding the raw materials;
[0042] S4, sieve the ground material, put the ground material into a mixing device, add the preservative into the mixing device, and mix for 15 minutes;
[0043] S5, gradually increase the temperature in the mixing device at a rate of 10°C / min, so that the mixed material is gradually dried, and the temperature is stopped when the mixed material humidity is maintained at a certain level, and the mixed material is cooled and taken out;
[0044] S6, putting the mixed material obtained in S2 and the mixed material obtained in S5 into a mixing device at the same time, raising the temperature in the mixing device to 130r / min, and mixing for 30min;
[0045] S7, after mixing, filtering the mixed material and collecting the solid mixed material;
[0046] S8, placing the solid mixture in a drying device and providing a temperature of 75° C. to quickly dry it into a powder form;
[0047] S9. Collect and store the finished products.
[0048] In this embodiment, the lubricating powder uses mica in the formula. Mica has good high temperature resistance and corrosion resistance, and can effectively improve the physical properties of the finished product. At the same time, mica powder also has strong adhesion and can be tightly combined with other materials to provide good adhesion performance, thereby effectively enabling the lubricating powder to continue to maintain high lubrication activity.
[0049] Example 2
[0050] See also Figure 1 The present invention provides a technical solution: a wire drawing lubricating powder with high lubricating activity, comprising the following materials: mixed animal and plant oils, mica powder, paraffin, talcum powder, microsilica powder, stearic acid, mineral powder and preservatives, with the weight proportions being 12-15 parts, 5-8 parts, 6-7 parts, 4-7 parts, 5-6 parts, 8-10 parts, 6-8 parts and 2-5 parts respectively.
[0051] This article also discloses a method for preparing a wire drawing lubricating powder with high lubricating activity, comprising the following steps:
[0052] S1, take animal and plant mixed fats and paraffin and place them in a mixing device, increase the temperature in the mixing device to 130°C, and wait for the animal and plant mixed fats and paraffin to melt;
[0053] S2, add stearic acid and mica powder into the mixing device, control the mixing speed of the mixing device to 110r / min, and keep warm and mix for 8min;
[0054] S3, taking mineral powder, talcum powder and microsilica powder and placing them in a grinding device in sequence, grinding the mixed materials, and keeping a time interval of 7 minutes between grinding and adding the raw materials;
[0055] S4, sieve the ground material, put the ground material into a mixing device, add the preservative into the mixing device, and mix for 16 minutes;
[0056] S5. Gradually increase the temperature in the mixing device at a rate of 12°C / min to gradually dry the mixed material until the humidity of the mixed material is maintained at a certain level, stop heating, and wait for the mixed material to cool and be taken out;
[0057] S6, putting the mixed material obtained in S2 and the mixed material obtained in S5 into a mixing device at the same time, raising the temperature in the mixing device to 140r / min, and mixing for 32min;
[0058] S7, after mixing, filtering the mixed material and collecting the solid mixed material;
[0059] S8, placing the solid mixture in a drying device and providing a temperature of 80° C. to quickly dry it into a powder form;
[0060] S9. Collect and store the finished products.
[0061] In this embodiment, the formula also includes animal and plant mixed oils and fats, which have a better lubricating effect and can also ensure the environmental friendliness of the finished product.
[0062] Example 3
[0063] See also Figure 1 The present invention provides a technical solution: a wire drawing lubricating powder with high lubricating activity, comprising the following materials: mixed animal and plant oils, mica powder, paraffin, talcum powder, microsilica powder, stearic acid, mineral powder and preservatives, with the weight proportions being 12-15 parts, 5-8 parts, 6-7 parts, 4-7 parts, 5-6 parts, 8-10 parts, 6-8 parts and 2-5 parts respectively.
[0064] This article also discloses a method for preparing a wire drawing lubricating powder with high lubricating activity, comprising the following steps:
[0065] S1, take animal and plant mixed fats and paraffin and place them in a mixing device, increase the temperature in the mixing device to 140°C, and wait for the animal and plant mixed fats and paraffin to melt;
[0066] S2, add stearic acid and mica powder into the mixing device, control the mixing speed of the mixing device to 120r / min, and keep warm and mix for 10min;
[0067] S3, taking mineral powder, talcum powder and microsilica powder and placing them in a grinding device in sequence, grinding the mixed materials, and keeping an interval of 8 minutes between grinding and adding the raw materials;
[0068] S4, sieve the ground material, put the ground material into a mixing device, add the preservative into the mixing device, and mix for 20 minutes;
[0069] S5. Gradually increase the temperature in the mixing device at a rate of 15°C / min to gradually dry the mixture until the humidity of the mixture is maintained at a certain level, stop heating, and wait for the mixture to cool and be taken out;
[0070] S6, putting the mixed material obtained in S2 and the mixed material obtained in S5 into a mixing device at the same time, raising the temperature in the mixing device to 150r / min, and mixing for 35min;
[0071] S7, after mixing, filtering the mixed material and collecting the solid mixed material;
[0072] S8, placing the solid mixture in a drying device and providing a temperature of 85° C. to quickly dry it into a powder form;
[0073] S9. Collect and store the finished products.
[0074] In this embodiment, the powders to be ground are differentiated by particle size in the preparation method, and different powders are put into the grinding device for grinding respectively by setting a time sequence, which can improve the grinding effect and uniformity of the raw materials and improve the quality of the final product.
[0075] Example 4
[0076] See also Figure 1 The present invention provides a technical solution: a wire drawing lubricating powder with high lubricating activity, comprising the following materials: mixed animal and plant oils, mica powder, paraffin, talcum powder, microsilica powder, stearic acid, mineral powder and preservatives, with the weight proportions being 12-15 parts, 5-8 parts, 6-7 parts, 4-7 parts, 5-6 parts, 8-10 parts, 6-8 parts and 2-5 parts respectively.
[0077] This article also discloses a method for preparing a wire drawing lubricating powder with high lubricating activity, comprising the following steps:
[0078] S1, take animal and plant mixed fats and paraffin and place them in a mixing device, increase the temperature in the mixing device to 140°C, and wait for the animal and plant mixed fats and paraffin to melt;
[0079] S2, add stearic acid and mica powder into the mixing device, control the mixing speed of the mixing device to 120r / min, and keep warm and mix for 10min;
[0080] S3, taking mineral powder, talcum powder and microsilica powder and placing them in a grinding device in sequence, grinding the mixed materials, and keeping a time interval of 6 minutes between grinding and adding the raw materials;
[0081] S4, sieve the ground material, put the ground material into a mixing device, add the preservative into the mixing device, and mix for 20 minutes;
[0082] S5. Gradually increase the temperature in the mixing device at a rate of 13°C / min to gradually dry the mixture until the humidity of the mixture is maintained at a certain level, stop heating, and wait for the mixture to cool and be taken out;
[0083] S6, putting the mixed material obtained in S2 and the mixed material obtained in S5 into a mixing device at the same time, raising the temperature in the mixing device to 150r / min, and mixing for 35min;
[0084] S7, after mixing, filtering the mixed material and collecting the solid mixed material;
[0085] S8, placing the solid mixture in a drying device and providing a temperature of 80° C. to quickly dry it into a powder form;
[0086] S9. Collect and store the finished products.
[0087] In this embodiment, the lubricating powder uses mica in the formula. Mica has good high temperature resistance and corrosion resistance, and can effectively improve the physical properties of the finished product. At the same time, mica powder also has strong adhesion, can be closely combined with other materials, and provide good adhesion performance, so that the lubricating powder can effectively maintain high lubrication activity. At the same time, the formula is also provided with animal and plant mixed oils and fats. The oils and fats have better lubrication effects and can also ensure the environmental protection of the finished product. At the same time, in the preparation method, the particle size of the powder to be ground is distinguished, and different powders are put into the grinding device for grinding by adding a time sequence setting, which can improve the grinding effect and uniformity of the raw materials and improve the quality of the final product.
[0088] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.
Claims
1. A wire drawing lubricating powder with high lubrication activity, Features: Includes the following materials: mixed animal and plant oils, mica powder, paraffin, talc, microsilica powder, stearic acid, mineral powder and preservatives.
2. A wire drawing lubricating powder with high lubrication activity according to claim 1, Features: The weight proportions of the animal and plant mixed oil, mica powder, paraffin, talc, microsilica powder, stearic acid, mineral powder and preservative are 12-15 parts, 5-8 parts, 6-7 parts, 4-7 parts, 5-6 parts, 8-10 parts, 6-8 parts and 2-5 parts respectively.
3. A method for preparing a wire drawing lubricating powder with high lubricating activity, Features: The steps include: S1, taking animal and plant mixed fats and paraffin and placing them in a mixing device, raising the temperature in the mixing device, and waiting for the animal and plant mixed fats and paraffin to melt; S2, add stearic acid and mica powder into the mixing device, control the mixing rate of the mixing device, and keep warm and mix for a period of time; S3, taking mineral powder, talcum powder and microsilica powder and placing them in a grinding device in sequence, grinding the mixed materials, and keeping a certain time interval between grinding and adding the raw materials; S4, sieving the grinding material, taking the grinding material into a mixing device, adding a preservative into the mixing device, and mixing for a period of time; S5, gradually increase the temperature in the mixing device to gradually dry the mixture until the humidity of the mixture is maintained at a certain level, stop heating, and wait for the mixture to cool and be taken out; S6, putting the mixed material obtained in S2 and the mixed material obtained in S5 into a mixing device at the same time, raising the temperature in the mixing device, and mixing for a period of time; S7, after mixing, filtering the mixed material and collecting the solid mixed material; S8, placing the solid mixture in a drying device and providing a certain temperature to quickly dry it into a powder form; S9. Collect and store the finished products.
4. A method for preparing a wire drawing lubricating powder with high lubricating activity according to claim 3, It is characterized in that In S1, the animal and plant mixed fats and paraffin are placed in a mixing device, the temperature in the mixing device is increased to 120-140° C., and the animal and plant mixed fats and paraffin are melted.
5. The method for preparing a wire drawing lubricating powder with high lubricating activity according to claim 3, It is characterized in that In S2, stearic acid and mica powder are added into a mixing device, the mixing speed of the mixing device is controlled to 100-120 r / min, and the mixture is mixed at a temperature-insulated temperature for 5-10 minutes.
6. A method for preparing a wire drawing lubricating powder with high lubricating activity according to claim 3, It is characterized in that In S3, mineral powder, talcum powder and microsilica powder are placed in a grinding device in sequence, and the mixed material is ground. The time interval between grinding and adding the raw materials is 5-8 minutes.
7. The method for preparing a wire drawing lubricating powder with high lubricating activity according to claim 3, It is characterized in that In S4, the ground material is sieved, and the ground material is placed in a mixing device, and a preservative is added to the mixing device, and mixed for 15-20 minutes.
8. The method for preparing a wire drawing lubricating powder with high lubricating activity according to claim 3, It is characterized in that In S5, the temperature in the mixing device is gradually increased at a rate of 10-15°C / min, so that the mixed material is gradually dried until the humidity of the mixed material is maintained at a certain level and the temperature is stopped to wait for the mixed material to be cooled and taken out.
9. The method for preparing a wire drawing lubricating powder with high lubricating activity according to claim 3, It is characterized in that In S6, the mixed material obtained in S2 and the mixed material obtained in S5 are simultaneously put into a mixing device, the temperature in the mixing device is increased to 130-150r / min, and mixing is performed for 30-35min.
10. The method for preparing a wire drawing lubricating powder with high lubricating activity according to claim 3, It is characterized in that In S8, the solid mixed material is placed in a drying device and provided with a temperature of 75-85° C. to be quickly dried into a powder.