Local gold plating process for laser pumping source chip base not prone to peeling
Through ultrasonic cleaning, plasma treatment and base layer plating and electroplating processes, the problem of easy peeling of the plating layer of the laser pump source chip base is solved, the adhesion and durability of the plating are improved, and the aesthetics and durability of the product are improved.
Patent Information
- Application Number
- CN202411427515.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-14
- Publication Date
- 2024-11-15
AI Technical Summary
The coating of the existing laser pump source chip base is easy to peel off, affecting its aesthetics and durability.
Ultrasonic cleaning, plasma treatment, base plating and electroplating processes are adopted to ensure the adhesion and durability of the plating layer, and the base plating is added before gold plating and sealing treatment after gold plating.
It improves the adhesion and corrosion resistance of the coating, enhances the aesthetics and durability of the laser pump source chip base, and extends its service life.
Smart Images

Figure KFUUWPJQSZ9SCI8NJHSHT9Y5QXRTZUZALVQPCGCE
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of gold plating technology, and in particular to a local gold plating process for a laser pump source chip base which is not prone to peeling. Background Art
[0002] The laser pump source chip base is a component used in laser technology. Its purpose is to facilitate the increase or decrease of the number of chip bases as needed, and to quickly replace damaged chip bases to avoid scrapping all chip bases at once and causing waste of resources. The laser pump source chip base also involves a local gold plating process in the production process, which avoids the waste of gold plating liquid through local gold plating.
[0003] The existing local gold plating technology mainly includes the following steps: surface treatment, pre-plating cleaning, plating pretreatment, metal electroplating and post-plating treatment. However, the laser pump source chip base prepared by the above technology has the problem of easy peeling of the plating layer, which affects the aesthetics and durability of the laser pump source chip base.
[0004] Therefore, in order to solve the problem that the above-mentioned coating is easy to peel off, a local gold plating process for the base of the laser pump source chip which is not easy to peel off can be designed. Summary of the invention
[0005] In order to overcome the problem of easy peeling of the coating.
[0006] The technical solution of the present invention is: a local gold plating process for a laser pump source chip base that is not prone to peeling, and the steps are as follows: S1: Surface preparation Pour clean water into the ultrasonic cleaning machine, then put in the laser pump source chip base, set the parameters of the ultrasonic cleaning machine, start the ultrasonic cleaning machine, take out the laser pump source chip base after cleaning and drain the sewage, then clean it with alkaline solution and acid solution in turn, and finally clean it again with clean water; S2: Pre-treat the surface, place the laser pump source chip base on a fixture in the processing chamber to ensure that its position is stable, turn on the plasma generator, and control the generation of plasma by adjusting parameters so that the plasma reacts fully with the surface of the laser pump source chip base, further clean the surface of the laser pump source chip base, remove fine oxides and organic matter, and improve the activity of the laser pump source chip base; S3: Block the non-gold-plated area; S4: Base plating: coating a base layer on the surface of the laser pump source chip base, the base layer is copper or nickel; S5: placing the laser pump source chip base into an electroplating tank containing a gold particle electrolyte, and controlling the current density and the temperature of the electrolyte so that the gold ions are reduced to metallic gold in the electrolyte and deposited in the area requiring electroplating; S6: After the electroplating is completed, the non-gold-plated area is shielded and cleaned to remove the residual electrolyte and other impurities to improve the finish and durability of the coating; S7: Apply the sealant evenly on the gold-plated area and cure it under visible light for 10 to 20 seconds; S8: Inspection and Packaging The laser pump source chip base that has been electroplated is inspected to ensure that the quality and thickness of the coating meet the requirements, and the qualified products are packaged.
[0007] Preferably, the parameters set during the clean water cleaning are a time of 3 to 5 minutes and a temperature of 30° C. to 35° C.
[0008] Preferably, the alkaline solution is a 2% to 5% sodium hydroxide solution, and the parameters set for alkaline washing are a temperature of 30 to 35° C. and a time of 5 to 10 minutes.
[0009] Preferably, the acid solution is a 5% to 10% hydrochloric acid solution or a 3% to 5% sulfuric acid solution, and the pickling parameters are set as a temperature of 30 to 35° C. and a time of 10 to 20 minutes.
[0010] Preferably, the input gas of the plasma generator is oxygen and nitrogen, wherein the ratio of oxygen to nitrogen is 1:7, and the adjusted parameters are: processing chamber pressure 80-120Pa, processing chamber temperature 40°C-60°C, gas flow rate 1-10L / min, and processing time 1-3min.
[0011] Preferably, the method for shielding the non-gold-plated area is: using a covering material to cover the part of the laser pump source chip base that does not require plating, and the covering material includes but is not limited to aluminum foil, tape, glue and wax.
[0012] Preferably, the method for shielding the non-gold-plated area is: using a shielding agent to coat the portion of the laser pump source chip base that does not require plating.
[0013] Preferably, the current density is 1.5 to 3 A / d , the temperature of the electrolyte is 30℃~35℃.
[0014] Preferably, the inspection includes visual inspection, thickness measurement and corrosion resistance testing.
[0015] The beneficial effects of the present invention are as follows: before gold plating, a base plating process is added, so that the bonding force between the laser pump source chip base and the plating layer can be improved, which is more conducive to the deposition of the surface plating layer, making the adhesion of the gold plating layer stronger and less prone to peeling, thereby improving the aesthetics and durability of the laser pump source chip base, and after the local gold plating is completed, further sealing treatment is performed, which greatly improves the corrosion resistance of the plating layer, increases the surface finish, improves the adhesion, and has good decorative effect and wear resistance and scratch resistance, protects the plating layer from the external environment, and extends its service life. DETAILED DESCRIPTION
[0016] The present invention will be further described below in conjunction with the embodiments.
[0017] Example 1 The present invention provides an embodiment: a local gold plating process for a laser pump source chip base that is not prone to peeling, and the steps are as follows: S1: Surface preparation Pour clean water into the ultrasonic cleaning machine, then put in the laser pump source chip base, set the parameters of the ultrasonic cleaning machine, start the ultrasonic cleaning machine, take out the laser pump source chip base after cleaning and drain the sewage, then clean it with alkaline solution and acid solution in turn, and finally clean it with clean water again. The parameters set for clean water cleaning are 3 minutes and 35°C, the alkaline solution is 2% sodium hydroxide solution, the parameters set for alkaline cleaning are 35°C and 5 minutes, the acid solution is 10% hydrochloric acid solution, and the parameters set for acid cleaning are 35°C and 10 minutes; S2: Pre-treat the surface, place the laser pump source chip base on the fixture in the processing chamber to ensure its stable position, turn on the plasma generator, and control the generation of plasma by adjusting parameters so that the plasma reacts fully with the surface of the laser pump source chip base, further clean the surface of the laser pump source chip base, remove fine oxides and organic matter, and improve the activity of the laser pump source chip base. The input gas of the plasma generator is oxygen and nitrogen, where the ratio of oxygen to nitrogen is 1:7. The adjusted parameters are: processing chamber pressure 80Pa, processing chamber temperature 40℃, gas flow rate 3L / min, and processing time 1min; S3: shielding the non-gold-plated area. The method of shielding the non-gold-plated area is: using aluminum foil to cover the part of the laser pump source chip base that does not need to be plated; S4: Base layer plating: coating a layer of base layer on the surface of the laser pump source chip base, and the base layer is copper; S5: Place the laser pump source chip base into the electroplating tank containing gold particle electrolyte and control the current density to 3A / d 1. The temperature of the electrolyte is 35°C, so that the gold ions are reduced to metallic gold in the electrolyte and deposited in the area to be electroplated; S6: After the electroplating is completed, the non-gold-plated area is shielded and cleaned to remove the residual electrolyte and other impurities to improve the finish and durability of the coating; S7: Apply the sealant evenly on the gold-plated area and cure it under visible light for 20 seconds; S8: Inspection and Packaging The laser pump source chip base that has been electroplated is inspected, including appearance inspection, thickness measurement and corrosion resistance test to ensure that the quality and thickness of the coating meet the requirements. Products that pass the inspection are packaged.
[0018] Example 2 The present invention provides an embodiment: a local gold plating process for a laser pump source chip base that is not prone to peeling, and the steps are as follows: S1: Surface preparation Pour clean water into the ultrasonic cleaning machine, then put in the laser pump source chip base, set the parameters of the ultrasonic cleaning machine, start the ultrasonic cleaning machine, take out the laser pump source chip base after cleaning and drain the sewage, then clean it with alkaline solution and acid solution in turn, and finally clean it with clean water again. The parameters set for clean water cleaning are time 5 minutes and temperature 35°C, the alkaline solution is 3% sodium hydroxide solution, the parameters set for alkaline cleaning are temperature 30°C and time 8 minutes, the acid solution is 5% sulfuric acid solution, and the parameters set for acid cleaning are temperature 35°C and time 12 minutes; S2: Pre-treat the surface, place the laser pump source chip base on the fixture in the processing chamber to ensure its stable position, turn on the plasma generator, and control the generation of plasma by adjusting the parameters so that the plasma reacts fully with the surface of the laser pump source chip base, further clean the surface of the laser pump source chip base, remove fine oxides and organic matter, and improve the activity of the laser pump source chip base. The input gas of the plasma generator is oxygen and nitrogen, where the ratio of oxygen to nitrogen is 1:7. The adjusted parameters are: processing chamber pressure 85Pa, processing chamber temperature 50℃, gas flow 6L / min, and processing time 1.5min; S3: shielding the non-gold-plated area. The method of shielding the non-gold-plated area is: using a shielding agent to coat the part of the laser pump source chip base that does not require plating; S4: Base layer plating, coating a layer of base layer on the surface of the laser pump source chip base, the base layer is nickel; S5: Place the laser pump source chip base into the electroplating tank containing gold particle electrolyte and control the current density to 3A / d 1. The temperature of the electrolyte is 35°C, so that the gold ions are reduced to metallic gold in the electrolyte and deposited in the area to be electroplated; S6: After the electroplating is completed, the non-gold-plated area is shielded and cleaned to remove the residual electrolyte and other impurities to improve the finish and durability of the coating; S7: Apply the sealant evenly on the gold-plated area and cure it under visible light for 20 seconds; S8: Inspection and Packaging The laser pump source chip base that has been electroplated is inspected, including appearance inspection, thickness measurement and corrosion resistance test to ensure that the quality and thickness of the coating meet the requirements. Products that pass the inspection are packaged.
[0019] Example 3 The present invention provides an embodiment: a local gold plating process for a laser pump source chip base that is not prone to peeling, and the steps are as follows: S1: Surface preparation Pour clean water into the ultrasonic cleaning machine, then put in the laser pump source chip base, set the parameters of the ultrasonic cleaning machine, start the ultrasonic cleaning machine, take out the laser pump source chip base after cleaning and drain the sewage, then clean it with alkaline solution and acid solution in turn, and finally clean it with clean water again. The parameters set for clean water cleaning are time 4 minutes and temperature 35°C, the alkaline solution is 4% sodium hydroxide solution, the parameters set for alkaline cleaning are temperature 35°C and time 7 minutes, the acidic solution is 6% hydrochloric acid solution, and the parameters set for acid cleaning are temperature 35°C and time 15 minutes; S2: Pre-treat the surface, place the laser pump source chip base on the fixture in the processing chamber to ensure its stable position, turn on the plasma generator, and control the generation of plasma by adjusting the parameters so that the plasma reacts fully with the surface of the laser pump source chip base, further clean the surface of the laser pump source chip base, remove fine oxides and organic matter, and improve the activity of the laser pump source chip base. The input gas of the plasma generator is oxygen and nitrogen, where the ratio of oxygen to nitrogen is 1:7. The adjusted parameters are: processing chamber pressure 100Pa, processing chamber temperature 40℃, gas flow 5L / min, and processing time 2min; S3: shielding the non-gold-plated area. The method of shielding the non-gold-plated area is: using a covering material to cover the part of the laser pump source chip base that does not need to be plated, and the covering material includes but is not limited to aluminum foil, tape, glue and wax; the method of shielding the non-gold-plated area is: using a shielding agent to apply to the part of the laser pump source chip base that does not need to be plated; S4: Base plating: coating a base layer on the surface of the laser pump source chip base, the base layer is copper or nickel; S5: Place the laser pump source chip base into the electroplating tank containing gold particle electrolyte and control the current density to 2.2A / d 1. The temperature of the electrolyte is 35°C, so that the gold ions are reduced to metallic gold in the electrolyte and deposited in the area to be electroplated; S6: After the electroplating is completed, the non-gold-plated area is shielded and cleaned to remove the residual electrolyte and other impurities to improve the finish and durability of the coating; S7: Apply the sealant evenly on the gold-plated area and cure it under visible light for 15 seconds; S8: Inspection and Packaging The laser pump source chip base that has been electroplated is inspected, including appearance inspection, thickness measurement and corrosion resistance test to ensure that the quality and thickness of the coating meet the requirements. Products that pass the inspection are packaged.
[0020] Comparative Example The laser pump source chip base is partially gold plated using a conventional process, the steps of which include surface treatment, pre-plating cleaning, plating pretreatment, metal electroplating and post-plating treatment.
[0021] Table 1 is a performance analysis table of local gold plating of the laser pump source chip base prepared by using Example 1, Example 2, Example 3 and the comparative example.
[0022] Table 1 The embodiments of the present invention are described in detail above, but the present invention is not limited to the above embodiments, and various changes can be made within the knowledge scope of those skilled in the art without departing from the spirit of the present invention.
Claims
1. A local gold plating process for a laser pump source chip base that is not prone to peeling, characterized in that: The steps are as follows: S1: Surface preparation Pour clean water into the ultrasonic cleaning machine, then put in the laser pump source chip base, set the parameters of the ultrasonic cleaning machine, start the ultrasonic cleaning machine, take out the laser pump source chip base after cleaning and drain the sewage, then clean it with alkaline solution and acid solution in turn, and finally clean it again with clean water; S2: Pre-treat the surface, place the laser pump source chip base on a fixture in the processing chamber to ensure that its position is stable, turn on the plasma generator, and control the generation of plasma by adjusting parameters so that the plasma reacts fully with the surface of the laser pump source chip base, further clean the surface of the laser pump source chip base, remove fine oxides and organic matter, and improve the activity of the laser pump source chip base; S3: Block the non-gold-plated area; S4: Base plating: coating a base layer on the surface of the laser pump source chip base, the base layer is copper or nickel; S5: placing the laser pump source chip base into an electroplating tank containing a gold particle electrolyte, and controlling the current density and the temperature of the electrolyte so that the gold ions are reduced to metallic gold in the electrolyte and deposited in the area requiring electroplating; S6: After the electroplating is completed, the non-gold-plated area is shielded and cleaned to remove the residual electrolyte and other impurities to improve the finish and durability of the coating; S7: Apply the sealant evenly on the gold-plated area and cure it under visible light for 10 to 20 seconds; S8: Inspection and Packaging The laser pump source chip base that has been electroplated is inspected to ensure that the quality and thickness of the coating meet the requirements, and the qualified products are packaged.
2. The local gold plating process for the laser pump source chip base that is not prone to peeling according to claim 1 is characterized in that: The parameters set for clean water cleaning are 3 to 5 minutes and a temperature of 30°C to 35°C.
3. The local gold plating process for the laser pump source chip base that is not prone to peeling according to claim 1 is characterized in that: The alkaline solution is a 2% to 5% sodium hydroxide solution, and the parameters set for alkaline washing are a temperature of 30 to 35°C and a time of 5 to 10 minutes.
4. The local gold plating process for the laser pump source chip base that is not prone to peeling according to claim 1 is characterized in that: The acid solution is a 5% to 10% hydrochloric acid solution or a 3% to 5% sulfuric acid solution, and the pickling setting parameters are a temperature of 30 to 35°C and a time of 10 to 20 minutes.
5. The local gold plating process for the laser pump source chip base that is not prone to peeling according to claim 1 is characterized in that: The input gas of the plasma generator is oxygen and nitrogen, wherein the ratio of oxygen to nitrogen is 1:7, and the adjusted parameters are: processing chamber pressure 80-120Pa, processing chamber temperature 40℃-60℃, gas flow rate 1-10L / min, and processing time 1-3min.
6. The non-peeling laser pump source chip base local gold plating process according to claim 1 is characterized in that: The method of shielding the non-gold-plated area is: using a covering material to cover the part of the laser pump source chip base that does not need to be plated, and the covering material includes but is not limited to aluminum foil, tape, glue and wax.
7. The local gold plating process for the laser pump source chip base that is not prone to peeling according to claim 1 is characterized in that: The method of shielding the non-gold-plated area is to use a shielding agent to coat the portion of the laser pump source chip base that does not require plating.
8. The non-peeling laser pump source chip base local gold plating process according to claim 1 is characterized in that: Current density is 1.5~3A / d , the temperature of the electrolyte is 30℃~35℃.
9. The non-peeling laser pump source chip base local gold plating process according to claim 1, characterized in that: Inspection includes visual inspection, thickness measurement and corrosion resistance testing.
Citation Information
Cited By
Electroplating method of plug shielding piece
CN119615317A
A method of electroplating a plug shield
CN119615317B