Longitudinal variable doping IGBT (Insulated Gate Bipolar Translator) structure and preparation method thereof
By introducing an electric field slow-changing layer and a field cut-off layer on the back of the substrate of the IGBT device, combined with the design of the transition zone, the failure problem caused by the electric field raised during short circuit of the IGBT device is solved, and its short-circuit robustness and switching losses are improved.
Patent Information
- Application Number
- CN202411013548.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-26
- Publication Date
- 2024-11-15
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
IGBT devices are prone to failure due to electric field raising in the case of short circuit. The drift region of the traditional trench gate IGBT devices with field cut-off layer is low, resulting in the device being extremely prone to failure during short circuit.
The longitudinally variable doped IGBT structure includes forming an electric field slow-changing layer and a field cut-off layer on the back of the semiconductor substrate, and covering the collector structure on the back of the field cut-off layer, and introducing variable doping in the transition region between the substrate and the collector. The electric field is slow to reduce the electric field to avoid the electric field raising.
It effectively avoids device failure caused by electric field elevation, reduces short-circuit saturation current and tailing current, and improves the short-circuit robustness and switching losses of IGBT.
Smart Images

Figure CN118969825A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and in particular to a longitudinal variable doping IGBT structure and a preparation method thereof. Background Art
[0002] The Insulated Gate Bipolar Transistor (IGBT) is a new type of composite power device developed on the basis of the Metal Oxide Semiconductor Field Effect Transistor (MOSFET) and the Bipolar Junction Transistor (BJT). It has the characteristics of MOSFET input and bipolar output. Load short circuit is a common abnormality in IGBT application systems. In this state, the current flowing through the circuit may reach several times or even dozens of times the saturation current of the device. The switching behavior of the IGBT device during the short circuit process may also cause transient failure. During the short circuit, the IGBT needs to withstand the impact of the short circuit and provide reaction time for the system protection circuit. Otherwise, the short circuit abnormality will cause damage to the system circuit. This shows the importance of the short circuit robustness of the IGBT device.
[0003] At present, the traditional trench gate IGBT device with a field stop layer has a low doping in the drift region, and the initial electric field is high when the electric field reaches the back stop layer. When a short circuit occurs in the device, the back electric field rises, which can easily cause the device to fail. Summary of the invention
[0004] The technical problem to be solved by the present invention is to provide a longitudinal variable doping IGBT structure and a preparation method thereof, wherein the IGBT structure can avoid device failure caused by subsequent electric field elevation.
[0005] In order to solve the above problems, the following technical solutions are provided:
[0006] The longitudinal variable doping IGBT structure of the present invention comprises a semiconductor substrate of the first conductivity type. The front side of the semiconductor substrate has a cell region. The characteristic is that there is a transition region between the back side of the semiconductor substrate and the collector structure. The transition region comprises an electric field gradual change layer and a field stop layer sequentially covering the back side of the semiconductor substrate, and the collector structure covers the back side of the field stop layer. The electric field gradual change layer is a variable doping layer of the first conductivity type, and the field stop layer is a heavily doped layer of the first conductivity type.
[0007] The cell region contains at least two gate trenches arranged side by side, a gate oxide layer is grown on the sidewalls and bottom walls of the gate trenches, the gate trenches with the gate oxide layer are filled with gate polysilicon, and the gate polysilicon is insulated and isolated from the metal layer deposited on the front side of the semiconductor substrate by an interlayer oxide layer arranged at the notch of the gate trenches. An emitter structure is provided between the two connected gate trenches.
[0008] The emitter structure comprises a first emitter region of a first conductivity type and a second emitter region of a second conductivity type from top to bottom, the first emitter region and the second emitter region are both in contact with the corresponding gate trench sidewalls, and the depth of the second emitter region is less than the depth of the gate trench. A contact hole penetrating the first emitter region is provided at the top of the second emitter region, the contact hole is filled with metal, the filling metal is connected to the metal layer, and the filling metal is in ohmic contact with the first emitter region and the second emitter region.
[0009] The collector structure comprises a collector electrode of the second conductivity type formed by implantation on the back side of the field stop layer, and a metal layer is deposited on the back side of the collector electrode to form a back electrode.
[0010] The collector of the second conductivity type is heavily doped.
[0011] The method for preparing the vertical variable doping IGBT structure is characterized by comprising the following steps:
[0012] In the first step, a heavily doped epitaxial layer of the first conductivity type is epitaxially grown on the front side of the single crystal silicon substrate as a field stop layer of the device; then, a variable doping epitaxial layer of the first conductivity type is grown on the front side of the heavily doped epitaxial layer as an electric field gradual change layer of the device; thereafter, a low doped epitaxial layer of the first conductivity type is grown on the front side of the variable doping epitaxial layer as a voltage-resistant layer of the device, and the low doped epitaxial layer is the semiconductor substrate, thereby obtaining a blank after epitaxial growth.
[0013] In the second step, an oxide layer is grown on the outer layer of the blank after epitaxial growth, and the redundant area is selectively etched away by photolithography to form a gate trench etching window, and the gate trench of the device is etched to obtain a blank with a gate trench.
[0014] In the third step, an oxide layer is first grown on the front side of the blank with the gate trench, so that a gate oxide layer is formed on the sidewalls and bottom walls of the gate trench; then, polysilicon is deposited on the whole, and only the polysilicon in the gate trench is retained by Etch Back, forming a blank with a complete gate trench structure.
[0015] The fourth step is to grow a thin oxide layer as a barrier layer for the second conductivity type injection as a whole on the blank containing a complete gate trench structure. Next, the second conductivity type is injected into the front side and a thermal process is performed to form a second emitter region. After that, the oxide layer thickened by the thermal process on the front side is thinned to form a new thin oxide layer as a barrier layer for the first conductivity type injection. Through photolithography, the first conductivity type injection region is selected. After the injection is completed, the photoresist is removed and a thermal process is performed to form a first emitter region. After that, an oxide layer is deposited on the surface to form an interlayer oxide layer.
[0016] The fifth step is to selectively etch contact holes through photolithography and fill them with metal to ensure that the metal filled in the contact holes forms good ohmic contact with the first emitter area and the second emitter area, thereby forming a blank that completes the front side process.
[0017] The sixth step is to thin the back side of the blank that has completed the front side process so that the blank reaches the set thickness. The single crystal silicon substrate needs to be completely removed and the heavily doped epitaxial layer needs to be thinned.
[0018] The seventh step is to process the collector structure on the back of the blank.
[0019] In the third step, an oxide layer is grown on the entire front side of the blank having the gate groove by dry oxygen method.
[0020] Step 7: The specific process of processing the collector structure on the back of the blank is as follows:
[0021] First, the second conductivity type is injected into the back of the blank, and laser annealing is performed to form a collector electrode of the second conductivity type heavily doped on the back; then, metal is made on the back to form a back electrode.
[0022] The above solution has the following advantages:
[0023] Since there is a transition zone between the back side of the semiconductor substrate and the collector structure of the longitudinal variable doping IGBT structure of the present invention, the transition zone includes an electric field gradual change layer and a field stop layer sequentially covering the back side of the semiconductor substrate, the collector structure covers the back side of the field stop layer, the electric field gradual change layer is a variable doping layer of the first conductivity type, and the field stop layer is a heavily doped layer of the first conductivity type. This IGBT structure utilizes the variable doping layer to make the electric field drop slowly in the drift region, and finally reaches the field stop layer with a lower electric field, thereby avoiding device failure caused by subsequent electric field elevation. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Figure 1 It is a schematic diagram of the longitudinal variable doping IGBT structure of the present invention;
[0025] Figure 2It is a schematic diagram of the longitudinal variable doping IGBT structure of the present invention after the first step in the preparation process is completed;
[0026] Figure 3 It is a schematic diagram of the longitudinal variable doping IGBT structure of the present invention after the second step of the preparation process is completed;
[0027] Figure 4 It is a schematic diagram of the longitudinal variable doping IGBT structure of the present invention after the third step in the preparation process is completed;
[0028] Figure 5 It is a schematic diagram of the longitudinal variable doping IGBT structure of the present invention after the fourth step in the preparation process is completed;
[0029] Figure 6 It is a schematic diagram of the longitudinal variable doping IGBT structure of the present invention after the fifth step in the preparation process is completed;
[0030] Figure 7 It is a schematic diagram of the longitudinal variable doping IGBT structure of the present invention after the sixth step in the preparation process is completed; DETAILED DESCRIPTION
[0031] In the above “first conductivity type” and “second conductivity type”, for N-type IGBT devices, the first conductivity type refers to N-type, and the second conductivity type refers to P-type; for P-type IGBT devices, the first conductivity type and the second conductivity type refer to the types that are exactly opposite to those of N-type semiconductor devices. Figure 1-7 The present invention is described in further detail.
[0032] like Figure 1 As shown, the longitudinal variable doping IGBT structure of the present invention includes a semiconductor substrate of the first conductivity type, i.e., an N-type voltage-resistant layer 103. The front side of the semiconductor substrate has a cell region. The cell region contains at least two gate trenches 106 arranged side by side, and a gate oxide layer is grown on the sidewalls and bottom walls of the gate trenches 106. The gate trenches 106 with the gate oxide layer are filled with gate polysilicon, and the gate polysilicon is insulated and isolated from the metal layer 112 deposited on the front side of the semiconductor substrate by an interlayer oxide layer 109 arranged at the notch of the gate trenches 106. There is an emitter structure between the two connected gate trenches.
[0033] like Figure 1As shown, the emitter structure includes a first emitter region of a first conductivity type and a second emitter region of a second conductivity type from top to bottom, the first emitter region is an N-type region 108, and the second emitter region is a P-type region 107. Both the N-type region 108 and the P-type region 107 are in contact with the corresponding sidewalls of the gate trench 106, and the depth of the P-type region 107 is less than the depth of the gate trench 106. A contact hole 110 is provided on the upper portion of the P-type region 107, which penetrates the N-type region 108, and the contact hole is filled with metal, which is connected to the metal layer 113, and the filling metal is in ohmic contact with the N-type region 108 and the P-type region 107.
[0034] like Figure 1 As shown, there is a transition zone between the back side of the semiconductor substrate and the collector structure. The transition zone includes an electric field gradual change layer 102 and a field stop layer 101 sequentially covering the back side of the semiconductor substrate, and the collector structure covers the back side of the field stop layer 101. The electric field gradual change layer 102 is an N-type variable doping layer, and the field stop layer 101 is an N-type heavily doped layer.
[0035] like Figure 1 As shown, the collector structure includes a collector of the second conductivity type formed by heavy doping on the back side of the field stop layer, namely a heavily doped P-type collector 111. A metal layer is deposited on the back side of the P-type collector 111 to form a back electrode 112.
[0036] The method for preparing the vertical variable doping IGBT structure of the present invention is characterized by comprising the following steps:
[0037] In the first step, an N-type heavily doped epitaxial layer is firstly epitaxially grown on the front side of the single crystal silicon substrate 100 as the field stop layer 101 of the device; then, an N-type variable doping epitaxial layer is grown on the front side of the heavily doped epitaxial layer as the electric field gradual change layer 102 of the device; then, an N-type low doped epitaxial layer is grown on the front side of the variable doping epitaxial layer as the voltage resistance layer 103 of the device, and the low doped epitaxial layer is the semiconductor substrate, thereby obtaining a blank after epitaxial growth, such as Figure 2 shown.
[0038] In the second step, an oxide layer is grown on the outer layer of the blank after epitaxial growth, and the redundant area is selectively etched by photolithography to form a gate trench 106 etching window, and the gate trench of the device is etched to obtain a blank with a gate trench, such as Figure 3 shown.
[0039] In the third step, an oxide layer is first grown on the front surface of the blank with the gate trench, so that the sidewalls and bottom walls of the gate trench form a gate oxide layer; then, polysilicon is deposited on the whole, and only the polysilicon in the gate trench is retained by Etch Back to form a blank with a complete gate trench structure, such as Figure 4In order to ensure the quality of the oxide layer and improve the reliability of the device, a layer of oxide layer is grown on the front side of the blank with the gate trench by dry oxygen method.
[0040] In the fourth step, a thin oxide layer is grown as a barrier layer for P-type injection on the blank containing a complete gate trench structure. Then, P-type injection is performed on the front side and a thermal process is performed to push the junction to form a second emitter region, namely, P-type region 107. After that, the oxide layer thickened by the thermal process on the front side is thinned to form a new thin oxide layer as a barrier layer for N-type injection. Through photolithography, the N-type injection region is selected. After the injection is completed, the photoresist is removed and a thermal process is performed to push the junction to form a first emitter region, namely, N-type region 108. After that, an oxide layer is deposited on the surface to form an interlayer oxide layer 109. Figure 5 shown.
[0041] In the fifth step, the contact hole 110 is selectively etched by photolithography and filled with metal to ensure that the metal filled in the contact hole 110 forms a good ohmic contact with the P-type region 107 and the N-type region 108, so as to form a blank that completes the front process, such as Figure 6 shown.
[0042] The sixth step is to thin the back of the blank after the front process is completed, so that the blank reaches a set thickness. The single crystal silicon substrate 100 needs to be completely removed, and the heavily doped epitaxial layer is thinned. Figure 4 As shown,.
[0043] Step 7: The specific process of processing the collector structure on the back of the blank is as follows:
[0044] First, P-type implantation is performed on the back of the blank, and laser annealing is performed to form a heavily doped P-type collector 111 on the back. After that, metal is made on the back to form a back electrode 112, such as Figure 1 shown.
[0045] Compared with the conventional FS-IGBT structure, the present invention mainly improves the device drift region and field stop region, adds a transition region, reduces the electric field strength reaching the back FS layer, and achieves a smooth transition of the electric field. The introduction of the variable doping region reduces the injection of holes on the back side and reduces the short-circuit saturation current of the device; at the same time, the lower minority carrier lifetime in the variable doping region enables the holes injected into the back side to recombine faster after being turned off, reducing the tail current of the device and reducing the overall turn-off loss of the device. Therefore, the variable doping IGBT of the present invention brings an IGBT with higher short-circuit robustness and reduces the switching loss of the IGBT.
Claims
1. A vertically variable doped IGBT structure, comprising a semiconductor substrate of a first conductivity type; the front surface of the semiconductor substrate has a cell region; characterized in that: There is a transition zone between the back side of the semiconductor substrate and the collector structure; the transition zone includes an electric field gradual change layer and a field stop layer sequentially covering the back side of the semiconductor substrate, and the collector structure covers the back side of the field stop layer; the electric field gradual change layer is a variable doping layer of the first conductivity type, and the field stop layer is a heavily doped layer of the first conductivity type.
2. The vertically variable doped IGBT structure according to claim 1, characterized in that: The cell region contains at least two gate trenches arranged side by side, with gate oxide layers grown on the side walls and bottom walls of the gate trenches, the gate trenches with the gate oxide layers are filled with gate polysilicon, and the gate polysilicon is insulated and isolated from the metal layer deposited on the front side of the semiconductor substrate by an interlayer oxide layer arranged at the notch of the gate trench; there is an emitter structure between the two connected gate trenches.
3. The vertically variable doped IGBT structure according to claim 2, characterized in that: The emitter structure contains a first emitter region of a first conductivity type and a second emitter region of a second conductivity type from top to bottom, the first emitter region and the second emitter region are both in contact with the corresponding gate trench side walls, and the depth of the second emitter region is less than the depth of the gate trench; a contact hole penetrating the first emitter region is provided at the upper part of the second emitter region, the contact hole is filled with metal, the filling metal is connected to the metal layer, and the filling metal is in ohmic contact with the first emitter region and the second emitter region.
4. The vertically variable doped IGBT structure according to claim 1, characterized in that: The collector structure comprises a collector electrode of the second conductivity type formed by implantation on the back side of the field stop layer, and a metal layer is deposited on the back side of the collector electrode to form a back electrode.
5. The vertically variable doped IGBT structure according to claim 4, characterized in that: The collector of the second conductivity type is heavily doped.
6. The method for preparing a vertically variable doped IGBT structure according to claim 3, characterized in that: The steps include: The first step is to epitaxially grow a heavily doped epitaxial layer of the first conductivity type on the front side of the single crystal silicon substrate as a field stop layer of the device; then, grow a variable doping epitaxial layer of the first conductivity type on the front side of the heavily doped epitaxial layer as an electric field gradual change layer of the device; then, grow a low doped epitaxial layer of the first conductivity type on the front side of the variable doping epitaxial layer as a voltage-resistant layer of the device, the low doped epitaxial layer being the semiconductor substrate, and thereby obtain a blank after epitaxial growth is completed; The second step is to grow an oxide layer on the outer layer of the blank after epitaxial growth, selectively etch away the redundant area by photolithography to form a gate trench etching window, and then etch to form the gate trench of the device to obtain a blank with a gate trench; In the third step, an oxide layer is first grown on the front surface of the blank with the gate trench, so that the sidewalls and bottom walls of the gate trench form a gate oxide layer; then, polysilicon is deposited on the whole, and only the polysilicon in the gate trench is retained by etch back, so as to form a blank with a complete gate trench structure; The fourth step is to grow a thin oxide layer as a barrier layer for the second conductivity type implantation on the blank with the complete gate trench structure, and then implant the second conductivity type on the front side and perform a thermal process to push the junction to form a second emitter region; Afterwards, the oxide layer thickened by the thermal process on the front side is thinned to form a new thin oxide layer as a barrier layer for the first conductive type injection. Through photolithography, the first conductive type injection area is selected. After the injection is completed, the photoresist is removed and the junction is pushed by thermal process to form the first emitter area. Afterwards, an oxide layer is deposited on the surface to form an interlayer oxide layer. Step 5: selectively etch contact holes through photolithography and fill them with metal to ensure that the metal filled in the contact holes forms good ohmic contact with the first emitter region and the second emitter region, thereby forming a blank that completes the front side process; The sixth step is to thin the back of the blank after the front process is completed so that the blank reaches the set thickness. The single crystal silicon substrate needs to be completely removed and the heavily doped epitaxial layer needs to be thinned. The seventh step is to process the collector structure on the back of the blank.
7. The method for preparing a vertically variable doped IGBT structure according to claim 6, characterized in that: In the third step, an oxide layer is grown on the entire front side of the blank having the gate trench by dry oxygen method.
8. The method for preparing a vertically variable doped IGBT structure according to claim 6, characterized in that: Step 7: The specific process of processing the collector structure on the back of the blank is as follows: First, the second conductivity type is injected into the back of the blank, and laser annealing is performed to form a collector electrode of the second conductivity type heavily doped on the back; then, metal is made on the back to form a back electrode.
Citation Information
Patent Citations
Bipolar punch-through semiconductor device and method for manufacturing such a semiconductor device
CN103518252A
IGBT with novel buffer layer structure and manufacturing method thereof
CN104103682A
Superjunction reverse-resistance IGBT with variable doped field stop layer
CN110391290A
Substrate, semiconductor device and preparation method thereof
CN112582469A
RC-IGBT structure with JBS and preparation method
CN117038719A