Intermediate joint structure of three-phase coaxial superconducting cable
By designing a junction box structure containing U-shaped connectors and multi-layer expansion joints, the length mismatch problem caused by thermal expansion and contraction of the cable core in three identical shaft superconducting cables is solved, which simplifies the structure and reduces losses, and achieves the The length direction of the three-phase conductor layer is decoupled and the low-temperature insulated enclosure.
Patent Information
- Application Number
- CN202411086955.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-08
- Publication Date
- 2024-11-15
AI Technical Summary
When the intermediate joint structure of the three identical shaft superconducting cable is peeled off layer by layer in a compact space, the cable radius increases, the electrical, magnetic and thermal relationships are complex, and the AC loss of the overlap structure increases, and the cable core is thermally expanded and cold. The shrinkage causes the problem that the length does not match the outer tube body.
A junction box including the first and second metal housing components is designed, and the junction box is connected through a sealing interface flange, and the three-phase conductor layers are connected one by one by one using a U-shaped connector and a cable connector, and the three-phase conductor layers are expanded by multiple layers. Thermal expansion and contraction problem is solved by the joints and low constant temperature containers, and the superconducting state is maintained through liquid nitrogen flow.
The length direction decoupling of three identical axes superconducting cables is achieved, which reduces AC losses, simplifies the structure, is easy to be assembled on-site and controls costs, and solves the problem of mismatch between the cable core length and the outer tube body.
Smart Images

Figure CN118970516A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of superconducting electrical engineering, and in particular to a three-phase coaxial superconducting cable intermediate joint structure. Background Art
[0002] In the prior art, since the three-phase coaxial superconducting cable has low conductor loss and strong coupling between its three phases, the joint structure of the three-phase coaxial superconducting cable must not only meet the general electrical transition, low temperature transition, vacuum transition, etc., but also take into account the problem of sequential peeling and decoupling of the three phases of the three-phase coaxial cable in the length direction.
[0003] The existing three-phase coaxial superconducting cable intermediate joint structure is peeled off layer by layer in a compact space. When connecting each functional layer, the cable radius is often locally increased, and the relationship between electricity, magnetism and heat is complicated. In addition, the intermediate joint structure with a lap joint structure has a large volume of the lap joint and a large transition metal contact area of the junction box, which will lead to an increase in the AC loss generated by the lap joint. Summary of the invention
[0004] The technical problem to be solved by the present invention is to provide an intermediate joint structure for a three-phase coaxial superconducting cable, which can solve the problem of mismatch between the cable core length and the outer tube body of the three-phase coaxial superconducting cable caused by thermal expansion and contraction of the cable core; the structure is simple, easy to assemble on site and control costs.
[0005] In order to solve the above technical problems, the present invention provides a three-phase coaxial superconducting cable intermediate joint structure, comprising: a first metal shell component capable of accommodating a first superconducting cable and a second metal shell component capable of accommodating a second superconducting cable, a junction box for providing a low-temperature insulation accommodation space, the first metal shell component and the second metal shell component are respectively connected to the junction box through a sealing interface flange, and the stripped section of the cable core of the first superconducting cable and the stripped section of the cable core of the second superconducting cable are respectively accommodated in the junction box; a U-shaped connector for connecting the corrugated tube of the cable core stripped section of the first superconducting cable and the corrugated tube of the cable core stripped section of the second superconducting cable, the U-shaped connector is fastened in the junction box; and a cable connector fastened between the conductor layer of the cable core stripped section of the first superconducting cable and the conductor layer of the cable core stripped section of the second superconducting cable, the cable connector is installed in the junction box, wherein: the three phases of the two superconducting cables are connected one by one through the cable connector, so as to decouple the three phases of the two superconducting cables in the length direction.
[0006] The first metal shell component comprises: a U-shaped metal shell and a plurality of expansion joints mounted on the U-shaped metal shell, wherein: the thermal expansion and contraction of the U-shaped metal shell caused by temperature changes are compensated by the plurality of expansion joints.
[0007] The first metal shell assembly further includes: a low-temperature Dewar tube end interface flange installed at the end of the U-shaped metal shell and a displacement sensor for detecting the contraction amount of the first superconducting cable, a sensor bracket is installed on the U-shaped metal shell, and the displacement sensor is fastened to the sensor bracket; The bending radius of the U-shaped metal shell is within the maximum bending radius of the first superconducting cable.
[0008] The cable core stripping section of the first superconducting cable and the cable core stripping section of the second superconducting cable respectively include: a corrugated tube, a plurality of conductor layers and insulating layers alternately wound outside the corrugated tube, a superconducting shielding layer wound outside the plurality of conductor layers and insulating layers, a low-temperature container coated outside the superconducting shielding layer, and a sheath arranged outside the low-temperature container.
[0009] Among them, the low constant temperature container is a high vacuum multi-layer insulation structure to reduce convective heat transfer and heat conduction; the low constant temperature container is mainly composed of a multi-layer tube structure, a multi-layer reflective layer, support bars and adsorbents.
[0010] The multi-layer tube structures are arranged to be concentric, vacuum is drawn between the multi-layer tube structures, and aluminum foil or aluminum-plated film is respectively wound around the multi-layer tube structures.
[0011] Among them, the junction box includes: a box body and double through holes opened on the box body, a sealing interface flange is installed at the position of the double through holes, and chamfered corners are arranged around the box body; the box body is a double-layer insulation structure, the middle layer of which is a vacuum layer, the box body is made of stainless steel material, and a film with a high reflection coefficient is covered on the wall of the middle layer.
[0012] The U-shaped connector comprises: a U-shaped connector body and a hard shell installed outside the U-shaped connector body, wherein: the opposite ends of the U-shaped connector body are respectively connected to the corrugated tube of the cable core stripping section of the first superconducting cable and the corrugated tube of the cable core stripping section of the second superconducting cable by welding, so that liquid nitrogen can flow between the two corrugated tubes.
[0013] The invention also includes: a joint fixing part for fastening the hard shell and the junction box; the hard shell and the joint fixing part are respectively made of oxygen-free copper material.
[0014] Among them, the cable connector is two pieces that can be buckled together to form a complete tube; any one of the cable connectors includes: a semicircular metal ring, bolt fastening holes are opened on both sides of the metal ring, and a flux inlet hole is opened on the top of the metal ring; the cable connector is made of oxygen-free copper material.
[0015] The three-phase coaxial superconducting cable intermediate joint structure of the present invention has the following beneficial effects: the three-phase coaxial superconducting cable intermediate joint structure comprises: a first metal shell component capable of accommodating a first superconducting cable and a second metal shell component capable of accommodating a second superconducting cable, a junction box for providing a low-temperature insulation accommodation space, the first metal shell component and the second metal shell component are respectively connected to the junction box through a sealing interface flange, the stripped section of the cable core of the first superconducting cable and the stripped section of the cable core of the second superconducting cable are respectively accommodated in the junction box; a corrugated tube and a A U-shaped connector of the corrugated tube of the cable core stripping section of the second superconducting cable, the U-shaped connector is fastened in the junction box; and a cable connector fastened between the conductor layer of the cable core stripping section of the first superconducting cable and the conductor layer of the cable core stripping section of the second superconducting cable, the cable connector is installed in the junction box, wherein: the three phases of the two superconducting cables are connected one by one through the cable connector, so as to decouple the three phases of the two superconducting cables in the length direction, which can solve the problem of mismatch between the cable core length and the outer tube body of the three-phase coaxial superconducting cable caused by thermal expansion and contraction of the cable core; the structure is simple, easy to assemble on site and control costs. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0017] Figure 1 This is a schematic diagram of the partial cross-sectional structure of the intermediate joint structure of the coaxial superconducting cable in accordance with the third embodiment of the present invention.
[0018] Figure 2 It is a schematic structural diagram of a cable core stripping section of a first superconducting cable and a cable core stripping section of a second superconducting cable according to an embodiment of the present invention.
[0019] Figure 3 Schematic diagram of the external structure of the junction box according to an embodiment of the present invention.
[0020] Figure 4 The figure is a schematic diagram of the overall structure of a cable connector according to an embodiment of the present invention. DETAILED DESCRIPTION
[0021] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0022] like Figure 1-Figure 4 The figure shows the first embodiment of the intermediate joint structure of three-phase coaxial superconducting cables according to the present invention.
[0023] The three-phase coaxial superconducting cable intermediate joint structure in this embodiment includes: a first metal shell component 1 capable of accommodating a first superconducting cable 8 and a second metal shell component 2 capable of accommodating a second superconducting cable 9, and a junction box 3 for providing a low-temperature insulation accommodation space.
[0024] The first metal shell assembly 1 and the second metal shell assembly 2 are respectively connected to the junction box 3 through the sealing interface flange T, and the stripped section of the cable core of the first superconducting cable 8 and the stripped section of the cable core of the second superconducting cable 9 are respectively accommodated in the junction box 3; a U-shaped connector 4 is used to connect the corrugated tube of the cable core stripped section of the first superconducting cable and the corrugated tube of the cable core stripped section of the second superconducting cable, and the U-shaped connector 4 is fastened in the junction box 3; and a cable connector 5 is fastened between the conductor layer of the cable core stripped section of the first superconducting cable 8 and the conductor layer of the cable core stripped section of the second superconducting cable 9, and the cable connector 5 is installed in the junction box 3.
[0025] The three phases of the two superconducting cables 8 and 9 are connected one by one through the cable connector 5, so as to decouple the three phases of the two superconducting cables 8 and 9 in the length direction.
[0026] In a specific implementation, the stripped sections of the two superconducting cables 8 and 9 have the same structure. The stripped section of the first superconducting cable 8 is taken as an example to illustrate the stripped section structure of the two superconducting cables 8 and 9.
[0027] The stripped sections of the two superconducting cables 8 include: a corrugated tube 81, a plurality of conductor layers 82a, 82b and 82c and a plurality of insulating layers 83c, 83b and 83a alternately wound around the outside of the corrugated tube, a superconducting shielding layer 84 wound around the outside of the plurality of conductor layers 82a, 82b and 82c and the plurality of insulating layers 83c, 83b and 83a, a low-temperature container 85 wrapped around the outside of the superconducting shielding layer 84, and a sheath 86 arranged on the outside of the low-temperature container 85.
[0028] During implementation, the bellows 81 is a circulation channel for the coolant liquid nitrogen and can also serve as an internal support core. The multiple conductor layers 82a, 82b and 82c are current-carrying layers that carry and transmit current and are the core components of the superconducting cable. The multiple conductor layers 82a, 82b and 82c and the multiple insulating layers 83c, 83b and 83a are fixed on the bellows 81 in a winding manner one by one. For example: the conductor layer 82a is wound on the bellows 81 and then the insulating layer 83c is wound, and so on.
[0029] Preferably, the plurality of conductor layers 82a, 82b and 82c are usually wound on the support at a certain helix angle and pitch, and are sequentially the A phase, B phase and C phase of the superconducting cable 8. The insulating layer materials selected for the plurality of insulating layers 83c, 83b and 83a should be able to maintain certain mechanical properties and good insulation properties at low temperatures (generally about 77K at liquid nitrogen temperature). For example: cable paper, polyimide tape (PI), polypropylene laminated paper (PPLP) and polyaramid fiber paper (Nomex), etc.
[0030] The superconducting shielding layer 84 is wound around the outside of the assembly of multiple conductor layers 82a, 82b and 82c and multiple insulating layers 83c, 83b and 83a. Its function is to shield the magnetic field, mainly to prevent the leakage of the induced magnetic field generated when the conductor layer is energized. It usually uses the same superconducting tape as the superconducting layer, but the winding direction is opposite. The cryostat is long and has a large ratio of length to diameter. The diameter is generally 50-150mm, and the length can reach tens of meters to hundreds of meters.
[0031] Furthermore, the low constant temperature container 85 is coated on the outside of the superconducting shielding layer 84. The low constant temperature container 85 is a high vacuum multi-layer insulation structure to reduce convective heat transfer and heat conduction. The low constant temperature container 85 is mainly composed of a multi-layer tube structure, a multi-layer reflective layer, support bars and adsorbents.
[0032] Preferably, the multi-layer tube structures of the low constant temperature container 85 are arranged to be concentric, the multi-layer tube structures are evacuated, and aluminum foil or aluminum-plated film is respectively wrapped around the multi-layer tube structures. In this embodiment, the low constant temperature container 85 is a multi-layer tube body structure, and the multi-layer tube bodies are evacuated to 10-2Pa or lower to reduce convective heat transfer and conductive heat. Aluminum foil or aluminum-plated film is respectively wrapped around the multi-layer tube structure, and spacers are installed between the multi-layer structures. The purpose of such an arrangement is to help the inner and outer tubes maintain a relatively uniform spacing and reduce conductive heat leakage. The spacer generally adopts a polytetrafluoroethylene tube with low thermal conductivity. A gas adsorbent, such as activated carbon, is installed between the multi-layer insulation material and the inner layer of the corrugated tube to adsorb residual gas and improve the vacuum degree.
[0033] The sheath 86 is arranged outside the low temperature container 85, and its function is to provide physical, chemical and environmental protection. The commonly used sheath materials are PVC and PE.
[0034] In practice, the stripped section of the cable core of the second superconducting cable 9 has the same structure as the stripped section of the cable core of the first superconducting cable 8 , and both are accommodated in the junction box 3 through corresponding metal shell components.
[0035] Furthermore, the first metal shell assembly 1 is used to accommodate part of the body of the first superconducting cable 8 except the stripped section. The first metal shell assembly 1 includes: a U-shaped metal shell 11 and a plurality of expansion joints 12 installed on the U-shaped metal shell 11, wherein: the thermal expansion and contraction of the U-shaped metal shell 11 caused by temperature changes is compensated by the plurality of expansion joints 12.
[0036] Preferably, the first metal shell assembly 1 also includes: a low-temperature Dewar tube end interface flange 13 installed at the end of the U-shaped metal shell 11 and a displacement sensor 15 for detecting the contraction amount of the first superconducting cable 8. A sensor bracket 14 is installed on the U-shaped metal shell 11, and the displacement sensor 15 is fastened to the sensor bracket 14.
[0037] In specific implementation, the first superconducting cable 8 passes through the U-shaped metal shell 11. In this embodiment, the bending radius of the U-shaped metal shell 11 is within the maximum bending radius of the first superconducting cable 8. A low-temperature Dewar tube end interface flange 13 is provided at one end of the U-shaped metal shell 11 for connecting the low-temperature Dewar tube.
[0038] The function of the low-temperature Dewar tube end interface flange 13 is to have good vacuum sealing at low temperatures, and the flange connection is preferably a knife-edge sealing structure.
[0039] The expansion joints 12 are arranged at equal intervals outside the U-shaped metal shell 11. The function of the expansion joints 12 is to compensate for the thermal expansion and contraction of the pipeline caused by temperature changes. If contraction occurs, the U-shaped part moves in the contraction direction, and the expansion joints 12 remain stationary.
[0040] The function of the displacement sensor 15 is to detect the shrinkage of the cable. For example, when the stainless steel material used in the U-shaped metal shell 11 shrinks from 300K to 77K, the shrinkage rate is about 0.3%. For a 1m long stainless steel tube, it shrinks by about 3mm. When the temperature drops, the outer tube remains at room temperature, and the inner tube gradually drops to 77K. The shrinkage of the inner tube will cause stress on the material and welds, which may easily cause leakage. The measurement of the displacement sensor 15 helps to detect the stability of the connection at the joint, prevent it from loosening and falling off, avoid the mismatch between the cable core length and the low-temperature Dewar tube length caused by thermal expansion and contraction of the cable core, and help ensure that the system can operate safely and reliably under various environmental conditions.
[0041] Furthermore, the second metal shell component 2 is mainly composed of a U-shaped metal shell and a low-temperature Dewar tube end interface flange T at its end, and its structure is similar to that of the first metal shell component 1 .
[0042] Furthermore, the junction box 3 is used to provide a low-temperature insulation accommodation space. The junction box 3 includes: a grounded box body 31 and a double through hole 32 opened on the box body 31. A sealing interface flange T is installed at the position of the double through hole 32. The box body 31 is a double-layer insulation structure, and the middle layer is a vacuum layer, so that the superconducting cable body and the junction box 3 form a connected and closed low-temperature environment.
[0043] The box body 31 is made of stainless steel material, such as 304, 304L or 316. The purpose of such setting is: since the three phases of the cable have been peeled and decoupled in sequence in the length direction, the symmetry is broken, the magnetic field distribution is uneven, and eddy currents may be generated. The box body made of stainless steel material can make the eddy currents smaller and the performance at low temperatures is better.
[0044] Preferably, a film with a high reflectivity is pasted on the wall of the middle interlayer of the box body 31. The purpose of such a setting is to achieve a good thermal insulation effect. The so-called super insulation layer refers to a composite body composed of a film with a high reflectivity (such as polished aluminum foil, aluminum-plated plastic film, etc.) and a low thermal conductivity wire mesh (such as glass fiber mesh, polyethylene mesh, etc.). After this composite body is wound, heat radiation and heat conduction can be effectively reduced. By evacuating the inner and outer layer cavities, heat convection is greatly reduced, and heat conduction is further reduced.
[0045] Preferably, the box body 31 is provided with rounded corners around its periphery to prevent the film from short-circuiting.
[0046] Furthermore, the U-shaped connector 4 includes: a U-shaped connector body 41 and a hard shell 42 installed outside the U-shaped connector body 41, wherein: the opposite ends of the U-shaped connector body 41 are respectively connected to the corrugated tube 81 of the cable core stripping section of the first superconducting cable 8 and the corrugated tube of the cable core stripping section of the second superconducting cable 9 by welding, so that liquid nitrogen can flow between the two corrugated tubes.
[0047] During implementation, the U-shaped connector body 41 is welded to connect the two superconducting cable cryogenic circuits, so that liquid nitrogen can flow smoothly and the strip can be in a superconducting state. Soldering is preferred, because the bellows will not melt during soldering, and there is no need to reserve the parent material as solder during splicing. At the same time, it can also avoid deformation after soldering, ensuring the splicing accuracy at the joint. The hard shell 42 fixes the U-shaped connector body 41.
[0048] Preferably, it also includes: a joint fixing part 6 for fastening the hard shell 42 and the connector body 41; the hard shell 42 and the joint fixing part 6 are respectively made of oxygen-free copper material.
[0049] In this embodiment, the cable connector 5 is two pieces that can be buckled together to form a complete tube; any one of the cable connectors includes: a semicircular metal ring 51, bolt fastening holes 52 are opened on both sides of the metal ring 51, and a flux inlet hole 53 is opened on the top of the metal ring 51.
[0050] During implementation, the cable connector 5 is respectively installed on the outer peripheral wall of the conductor layer of the cable core stripping section of the two superconducting cables, and is buckled together to form a complete tubular shape to fix the two cables. The current carrying capacity of the cable connector 5 should be appropriate. If the current carrying capacity is too large, it is easy to cause excessive heat. If the current carrying capacity is too small, the volume of the connector is too large. Preferably, the two cables can be connected by welding or crimping.
[0051] Preferably, the cable connector 5 is made of oxygen-free copper with a high RRR value, so as to meet the flow requirements and ensure that the heat load inside the intermediate joint is not too large, resulting in a decrease in local thermal stability.
[0052] When the cable connector 5 is specifically assembled, welding or crimping can be used. During welding, the metal sleeve of the bolt fastening hole is pressed tightly on the conductor layer 82a, 82b or 82c with a bolt, and the metal ring is evenly heated to weld the metal ring and the superconducting conductor layer. A flux with a melting temperature of 78% is used, and the composition mass ratio is Sn9.3%, Pb34.5%, Bi50%, and Cd6.2%. The flux is injected from the flux inlet hole 53 so that the flux is evenly distributed between the metal ring and the superconducting tape. It should be noted that the heating temperature should be strictly controlled during welding. On the one hand, overheating is avoided to weaken the performance of the electrical insulation layer, and on the other hand, local overheating is avoided to damage the superconducting tape. The method of controlling the temperature is to pad a heat-insulating film between the conductor layer and the insulating layer and between each layer of superconducting tape. A thermometer is laid on the superconducting tape to measure and control the temperature of the metal ring and the superconducting tape during welding so as not to exceed the allowable temperature. The maximum allowable temperature of different insulating materials is different. For polypropylene laminated paper, the temperature cannot exceed 130°C, which is much lower than the maximum allowable temperature of superconducting tape (300°C).
[0053] During crimping, a soft metal, such as indium, is placed in the middle. Indium is a silvery-white soft metal with strong plasticity and ductility. It can be pressed into sheets and can flow in all directions under external pressure to fill the gaps on the sealing surface, which can also play a sealing role. The thermal conductivity and physical properties of indium metal make its heat dissipation performance much better than other metal materials. The thermal conductivity of indium can reach 86W / cm·℃. During crimping, the indium sheet in the middle makes the connection between the two connectors denser, reduces the interface resistance, has good flow capacity, and less heat dissipation.
[0054] The present invention provides a three-phase coaxial superconducting cable intermediate joint structure, which has the following beneficial effects: the three-phase coaxial superconducting cable intermediate joint structure comprises: a first metal shell component capable of accommodating a first superconducting cable and a second metal shell component capable of accommodating a second superconducting cable, a junction box for providing a low-temperature insulation accommodation space, the first metal shell component and the second metal shell component are respectively connected to the junction box through a sealing interface flange, the stripped section of the cable core of the first superconducting cable and the stripped section of the cable core of the second superconducting cable are respectively accommodated in the junction box; a corrugated tube and a A U-shaped connector of the corrugated tube of the cable core stripping section of the second superconducting cable, the U-shaped connector is fastened in the junction box; and a cable connector fastened between the conductor layer of the cable core stripping section of the first superconducting cable and the conductor layer of the cable core stripping section of the second superconducting cable, the cable connector is installed in the junction box, wherein: the three phases of the two superconducting cables are connected one by one through the cable connector, so as to decouple the three phases of the two superconducting cables in the length direction, which can solve the problem of mismatch between the cable core length and the outer tube body of the three-phase coaxial superconducting cable caused by thermal expansion and contraction of the cable core; the structure is simple, easy to assemble on site and control costs.
Claims
1. A three-phase coaxial superconducting cable intermediate joint structure, characterized in that: include: a first metal housing assembly capable of accommodating a first superconducting cable and a second metal housing assembly capable of accommodating a second superconducting cable, A junction box for providing a low-temperature insulation accommodation space, wherein the first metal shell assembly and the second metal shell assembly are respectively connected to the junction box through sealing interface flanges, and the stripped section of the cable core of the first superconducting cable and the stripped section of the cable core of the second superconducting cable are respectively accommodated in the junction box; A U-shaped connector for connecting the corrugated tube of the cable core stripping section of the first superconducting cable and the corrugated tube of the cable core stripping section of the second superconducting cable, wherein the U-shaped connector is fastened in the junction box; as well as A cable connector fastened between the conductor layer of the cable core stripping section of the first superconducting cable and the conductor layer of the cable core stripping section of the second superconducting cable, wherein the cable connector is installed in the junction box, wherein: the three phases of the two superconducting cables are connected one by one through the cable connector to decouple the three phases of the two superconducting cables in the length direction.
2. The three-phase coaxial superconducting cable intermediate joint structure according to claim 1, characterized in that: The first metal shell component comprises: a U-shaped metal shell and a plurality of expansion joints mounted on the U-shaped metal shell, wherein: the thermal expansion and contraction of the U-shaped metal shell caused by temperature changes are compensated by the plurality of expansion joints.
3. The intermediate joint structure of three-phase coaxial superconducting cables according to claim 2, characterized in that: The first metal shell assembly further comprises: a low-temperature Dewar tube end interface flange installed at the end of the U-shaped metal shell and a displacement sensor for detecting the contraction amount of the first superconducting cable, a sensor bracket is installed on the U-shaped metal shell, and the displacement sensor is fastened to the sensor bracket; A bending radius of the U-shaped metal shell is within a maximum bending radius of the first superconducting cable.
4. The three-phase coaxial superconducting cable intermediate joint structure according to claim 1, characterized in that: The cable core stripping section of the first superconducting cable and the cable core stripping section of the second superconducting cable respectively include: a corrugated tube, a plurality of conductor layers and insulating layers alternately wound outside the corrugated tube, a superconducting shielding layer wound outside the plurality of conductor layers and insulating layers, a low-temperature container coated outside the superconducting shielding layer, and a sheath arranged outside the low-temperature container.
5. The three-phase coaxial superconducting cable intermediate joint structure according to claim 4, characterized in that: The low constant temperature container is a high vacuum multi-layer insulation structure to reduce convection heat transfer and heat conduction; The low constant temperature container is mainly composed of a multi-layer tube structure, a multi-layer reflective layer, a support bar and an adsorbent.
6. The three-phase coaxial superconducting cable intermediate joint structure according to claim 5, characterized in that: The multi-layer tube structures are arranged to be concentric, vacuum is drawn between the multi-layer tube structures, and aluminum foil or aluminum-plated film is respectively wound around the multi-layer tube structures.
7. The three-phase coaxial superconducting cable intermediate joint structure according to claim 1, characterized in that: The junction box comprises: a box body and double through holes provided on the box body, the sealing interface flange is installed at the position of the double through holes, and the box body is provided with rounded corners around; The box body is a double-layer insulation structure, wherein the middle layer is a vacuum layer. The box body is made of stainless steel material, and a film with a high reflection coefficient is pasted on the wall of the middle layer.
8. The three-phase coaxial superconducting cable intermediate joint structure according to claim 1, characterized in that: The U-shaped connector comprises: a U-shaped connector body and a hard shell installed outside the U-shaped connector body, wherein: the opposite ends of the U-shaped connector body are respectively connected to the corrugated tube of the cable core stripping section of the first superconducting cable and the corrugated tube of the cable core stripping section of the second superconducting cable by welding, so that liquid nitrogen can flow between the two corrugated tubes.
9. The intermediate joint structure of three-phase coaxial superconducting cables according to claim 8, characterized in that: Also includes: A joint fixing piece fastens the hard shell and the junction box; the hard shell and the joint fixing piece are respectively made of oxygen-free copper material.
10. The three-phase coaxial superconducting cable intermediate joint structure according to claim 1, characterized in that: The cable connector is two pieces that can be buckled together to form a complete tube; Any cable connector includes: a semicircular metal ring, bolt fastening holes are provided on both sides of the metal ring, and a flux inflow hole is provided on the top of the metal ring; The cable connectors are made of oxygen-free copper.