Display module and display device comprising same
By setting the absorption layer of the matrix resin and porous absorbing material between the display panel and the polarization assembly, the problem of the polarizer failure of the flexible display device under high temperature and high humidity conditions is solved, the display effect and touch performance are improved, and the product is improved. Quality and yield.
Patent Information
- Application Number
- CN202411038167.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-30
- Publication Date
- 2024-11-15
AI Technical Summary
The existing flexible display devices are prone to failure under high temperature and high humidity conditions, resulting in abnormal display effects and degradation of touch performance, especially in foldable flexible display devices, which affects the yield and quality of the product.
An absorption layer is arranged between the display panel and the polarizing assembly. The absorption layer is composed of a matrix resin and a porous absorbing material. It has excellent gas adsorption function and can absorb gases escaped from the polarizing assembly and the display panel under high temperature and high humidity conditions, blocking the barrier Water vapor reduces the risk of failure of polarizers.
It effectively solves the poor display and poor touch control problems caused by polarizer failure, improves the display effect and touch performance of the display module and display device, improves the quality and yield of the product, and ensures higher reliability.
Smart Images

Figure CN118973343A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the field of display technology, and particularly relates to a display module and a display device comprising the same. Background Art
[0002] In recent years, in order to meet the diverse display needs, new display devices with different functions have emerged to provide convenience for people's lives and work. Intelligence, portability and flexibility are the main development directions of display devices. Flexible display devices break the traditional two-dimensional display concept and can be folded and bent as needed to reduce the size, increase the screen-to-body ratio and improve the user's visual experience. In recent years, flexible display devices have gradually become mainstream products in the display field.
[0003] Display devices usually include a panel and a polarizer located on the light-emitting side of the panel. Existing polarizers are prone to failure problems, especially under high temperature and high humidity conditions. Polarizer failure and fading not only lead to abnormal display effects, but also deteriorate the touch performance of the product, resulting in reduced touch sensitivity or even touch failure. Such failure problems are particularly serious in flexible display devices, seriously affecting the display effect and product yield of the device. Therefore, how to avoid the poor display and touch problems caused by polarizer failure and provide higher quality display devices is the research focus of this field. Summary of the invention
[0004] In order to solve the problems of poor display and poor touch caused by the failure of polarizers and provide a higher quality display device, one of the objects of the present invention is to provide a display module, which includes a display panel, a polarizing component and an absorption layer arranged between the display panel and the polarizing component; the absorption layer includes a combination of a base resin and a porous absorption material.
[0005] In the display module provided by the present invention, an absorption layer is arranged between the display panel and the polarizing component. The absorption layer contains a matrix resin and a porous absorption material. The porous absorption material has an excellent gas adsorption function and can fully absorb various gases escaping from the polarizing component and the display panel under conditions of high temperature and high humidity, thereby preventing the gas from corroding the internal structure of the display panel and the polarizing component, and blocking the invading water vapor, reducing or avoiding the risk of failure of the polarizer, thereby solving the problems of poor display and poor touch caused by the failure of the polarizer, so that the display module and the display device containing it have better display and touch effects, and improve the quality and yield of the product.
[0006] A second object of the present invention is to provide a display device, comprising the display module as described in one of the objects.
[0007] Compared with the prior art, the present invention has the following beneficial effects:
[0008] In the display module provided by the present invention, an absorption layer containing a porous absorption material is arranged between the display panel and the polarizing component, so that various gases escaping from the display module under harsh conditions such as high temperature and high humidity can be fully absorbed, thereby preventing the gas from corroding the internal structure of the display panel and the polarizing component, and blocking the invading water vapor, thereby reducing or avoiding the risk of failure of the polarizer, and effectively solving the problems of poor display and poor touch caused by the failure of the polarizer, so that the display module and the display device containing the same have better display and touch effects, higher reliability, and improved product quality and yield. BRIEF DESCRIPTION OF THE DRAWINGS
[0009] Figure 1 A schematic diagram of the structure of a display device in the research process of the present invention;
[0010] Figure 2 A schematic diagram of a partial structure of a display module provided in one embodiment of the present invention;
[0011] Figure 3 A schematic diagram of a partial structure of a display module provided in another embodiment of the present invention;
[0012] Figure 4 A schematic diagram of the structure of a display module provided in another embodiment of the present invention;
[0013] Figure 5 It is a schematic top view of the structure of a display module provided in another embodiment of the present invention. DETAILED DESCRIPTION
[0014] The technical solution of the present invention is further described below by specific implementation methods. It should be understood by those skilled in the art that the embodiments are only to help understand the present invention and should not be regarded as specific limitations of the present invention.
[0015] In the present invention, the directions or positional relationships indicated by terms such as "upper", "lower", "inside", "outside", "vertical", and "horizontal" are based on the directions or positional relationships shown in the accompanying drawings and are only for the convenience of describing the present invention and simplifying the description. They do not indicate or imply that the devices or elements referred to must have a specific direction, be constructed and operated in a specific direction, and should not be understood as limiting the present invention.
[0016] In the present invention, unless otherwise clearly specified and limited, the terms "connected", "connected", "installed", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above-mentioned terms in the present invention can be understood according to specific circumstances.
[0017] After research, the present invention has found that a display device usually includes a display panel and a polarizer located on the light-emitting side of the display panel. Under conditions of high temperature and high humidity, the polarizer is very likely to fail and fade, which not only causes abnormal display effects, but also deteriorates the touch performance of the product, resulting in reduced touch sensitivity or even touch failure. Such failure problems are particularly obvious in foldable flexible display devices, seriously affecting the touch display effect and product yield of the display device.
[0018] like Figure 1 As shown, Figure 1 The structure diagram of a display device in the process of the present invention is shown in FIG. 1 , wherein the display device includes a display panel 10 and a polarizing component 30, wherein the display panel 10 includes a touch layer 101, an encapsulation layer 102 and a light-emitting layer 103 arranged in sequence, and the touch layer 101 is located on a side close to the polarizing component 30; the polarizing component 30 includes a protective layer 301, a linear polarizing layer 302, a wave plate layer 303 and a glue layer 304 arranged in sequence, and the glue layer 304 is located on a side close to the display panel 10. The current mainstream material of the linear polarizing layer 302 is iodine-based PVA, which is a material containing polyiodine compounds (including I3 - and I5 - ) of PVA (polyvinyl alcohol) material to achieve polarization. The present invention found that in a high temperature and high humidity environment, polyiodine compounds are easily affected by water vapor, making I3 - and I5 - The content ratio changes, resulting in the hue change of the polarizing component, affecting the display effect; at the same time, the polyiodine compound reacts with water to form I2 or I - It is easy to diffuse to the surroundings, especially to the touch layer 101 and react with the metal and other materials therein, causing corrosion of the touch layer and failure of related touch functions. In addition, the encapsulation layer 102 releases NH3 and the like at high temperatures. The escape of NH3 accelerates the decomposition and content change of the polyiodine compounds in the linear bias layer 302, exacerbating the degradation of I2, I - The generation of the touch layer 101 is accompanied by corrosion, which further aggravates the deterioration of the display effect and the touch function, thereby causing poor display of the display device and failure of the touch function, and reducing the product yield and quality.
[0019] In order to solve the above technical problems, an embodiment of the present invention provides a display module and a display device including the same. By setting an absorption layer between the display panel and the polarizing component, the absorption layer contains a matrix resin and a porous absorption material, which can block the invading water vapor and avoid the adverse effects of water vapor on the polarizing component (especially the linear polarization layer), and fully absorb various gases escaping from the polarizing component (linear polarization layer) and the display panel (encapsulation layer) under high temperature and high humidity conditions, so as to prevent the gas from corroding and damaging the internal structure of the display panel and the polarizing component, reduce or avoid the risk of failure of the polarizer, and especially effectively reduce the corrosion of the metal layer that begins to occur at the edge of the display module under high temperature and high humidity conditions, overcome the defects of poor display and poor touch caused by the failure of the polarizer, so that the display module and the display device have better display and touch effects, improve product quality and yield, thereby solving the above technical problems.
[0020] In order to make the above-mentioned purpose, features and effects of the present invention more obvious, the present invention is further described in detail below in conjunction with the accompanying drawings and specific embodiments. It should be noted that the drawings of the present invention are not necessarily drawn according to the actual scale.
[0021] like Figure 2 As shown, Figure 2 This is a schematic diagram of the partial structure of a display module provided in one embodiment of the present invention, wherein the display module includes a display panel 10, an absorption layer 20 and a polarizing component 30, wherein the absorption layer 20 is disposed between the display panel 10 and the polarizing component 30; the absorption layer 20 includes a combination of a matrix resin and a porous absorption material.
[0022] In the display module of the present invention, the absorption layer 20 between the display panel 10 and the polarizing component 30 contains a porous absorption material, which gives it an excellent gas adsorption function. On the one hand, the absorption layer 20 can effectively block the invasion of water vapor, reduce or avoid the adverse effects of water vapor on the polarizing component 30 and the display panel 10; on the other hand, the absorption layer 20 can fully absorb the various gases escaping from the polarizing component 30 and the display panel 10 under conditions of high temperature and high humidity, and prevent the gas from corroding and damaging the internal structure of the display module, thereby reducing or avoiding the risk of failure of the polarizing component, solving the problems of poor display and poor touch caused by the failure of the polarizing component, so that the display module has better display and touch effects, and improves product quality and yield.
[0023] In some optional embodiments of the present invention, the display panel includes a light-emitting layer, a touch layer, and an encapsulation layer disposed between the light-emitting layer and the touch layer; the touch layer is located on a side close to the polarizing component.
[0024] In some optional embodiments of the present invention, the polarizing assembly includes a glue layer, a wave plate layer, a linear polarization layer and a protective layer arranged in sequence; the glue layer is located on a side close to the display panel.
[0025] like Figure 3 As shown, Figure 3 A schematic diagram of the partial structure of a display module provided for another embodiment of the present invention includes a display panel 10, an absorption layer 20 and a polarizing component 30; the display panel 10 includes a touch layer 101, an encapsulation layer 102 and a light-emitting layer 103 arranged in sequence, and the touch layer 101 is located on a side close to the polarizing component 30; the polarizing component 30 includes a protective layer 301, a linear polarization layer 302, a wave plate layer 303 and a glue layer 304 arranged in sequence, and the glue layer 304 is located on a side close to the display panel 10.
[0026] In some optional embodiments of the present invention, the touch layer 101 includes a metal touch layer.
[0027] It should be noted that the present invention does not specifically limit the structure and material of the metal touch layer, and any metal touch layer known in the art that can be used for display modules is applicable to the present invention. Metal materials have excellent electrical conductivity, but their light transmittance is relatively low. As an optional implementation, the metal touch layer includes a metal grid unit, and further optionally, the metal grid unit is formed by crossing metal wires, so as to have better transmittance, avoid the metal touch layer from affecting the light-emitting effect, and have the characteristics of low impedance and flexibility.
[0028] Optionally, the material of the metal touch layer may be any one of Ti, Al, Cu, Mo, and Ag, or a combination of at least two thereof, and the combination thereof includes but is not limited to: Ti / Al / Ti, Mo / Al / Mo.
[0029] In some optional embodiments of the present invention, the encapsulation layer 102 includes silicon nitride and silicon oxide.
[0030] In some optional embodiments of the present invention, the linear polarization layer 302 is an iodine-based polarizer.
[0031] Since the linear polarization layer 302 is an iodine-based polarizer, the material is iodine-based PVA, which contains polyiodine compounds (including I3 - and I5 - ) and PVA (polyvinyl alcohol), in a high temperature and high humidity environment, polyiodine compounds react with water to form I2 or I - Easy to spread around, I2 or I - In the presence of water, it will react with the metal (such as Al) in the metal touch layer, causing corrosion and failure of related touch functions; the encapsulation layer 102 will release NH3 at high temperatures, accelerating the decomposition of polyiodine compounds and the degradation of I2, I- The display module of the present invention is provided with an absorption layer, which can effectively block the intrusion of water vapor, absorb I2 generated by the linear polarization layer 302 and NH3 generated by the encapsulation layer 102 under high temperature and high humidity conditions, thereby reducing or avoiding the failure risk of the polarization component, preventing the gas from corroding the metal touch layer, and especially effectively reducing the corrosion of the metal touch layer that begins at the edge of high temperature and high humidity, avoiding touch failure, and making the display module have better display and touch effects.
[0032] It should be noted that the present invention does not specifically limit the light-emitting layer 103, and any light-emitting layer known in the art that can be used for display modules is applicable to the present invention. The light-emitting layer 103 can include multiple pixels according to display requirements to display image information. The multiple pixels can be of the same color, or can include two colors, three or more colors.
[0033] The present invention does not specifically limit the protective layer 301, wave plate layer 303 and adhesive layer 304 in the polarizing assembly 30. The protective layer, wave plate layer and adhesive layer that can be used for the polarizing assembly (polarizer) known in the art are all applicable to the present invention. Exemplarily, the protective layer includes TAC (triacetyl cellulose), which has high light transmittance, good water resistance and mechanical strength, and can provide protection for the linear polarization layer 302. The wave plate layer includes quartz or other transparent materials, which can play a role in controlling the polarization state of the light beam. The adhesive layer includes optical adhesive (OCA).
[0034] In some optional embodiments of the present invention, the porous absorption material includes any one of molecular sieves, activated carbon, organic conjugated materials containing acidic groups, and metal organic framework materials, or a combination of at least two of them.
[0035] In the present invention, the molecular sieve and activated carbon contain rich porous structures, which can physically adsorb a variety of gas molecules; the organic conjugated material containing acidic groups can achieve specific absorption of NH3; the metal organic framework material can achieve specific absorption of I2. The porous absorption material includes any one or a combination of at least two of molecular sieves, activated carbon, organic conjugated materials containing acidic groups, and metal organic framework materials, which can fully absorb the I2 gas generated from the linear polarization layer 302 and the NH3 gas generated from the encapsulation layer 102 under high temperature and high humidity conditions from the aspects of physical adsorption and / or specific absorption, prevent the gas from corroding and damaging the internal structure of the display module, reduce or avoid the risk of failure of the polarizing component, solve the problems of poor display and poor touch, and make the display module have better display effect and touch effect.
[0036] In some optional embodiments of the present invention, the acidic group in the organic conjugated material containing an acidic group includes at least one of a carboxylic acid group, a phosphoric acid group, and a sulfonic acid group.
[0037] And / or, the organic conjugated structure in the organic conjugated material containing an acidic group includes a C6-C60 aromatic structure, such as a monocyclic or condensed aromatic structure of C6, C9, C10, C12, C14, C16, C18, C20, C22, C24, C26, C28, C30, C32, C34, C36, C38, C40, C42, C44, C46, C48, C50, C52, C54, C56 or C58, illustratively including but not limited to: a benzene structure, a biphenyl structure, a naphthalene structure, an anthracene structure, a phenanthrene structure, a triphenylene structure, a pyrene structure, At least one of the structures.
[0038] In the present invention, the connection mode and connection site of the acidic group and the organic conjugated structure in the organic conjugated material containing the acidic group are not limited. At the same time, materials containing both the acidic group and the organic conjugated structure are suitable for the present invention and can play a role in specifically absorbing NH3.
[0039] For example, the organic conjugated material containing an acidic group can refer to the material type disclosed in the prior art, such as “Ammonia capture in porous organic polymers densely functionalized with Bronsted acid groups”, JFV Humbeck et al., Journal of the American Chemical Society, 2014, 136, 2432-2440.
[0040] In some optional embodiments of the present invention, the metal organic framework material is a metal organic framework material containing electron-rich groups.
[0041] Optionally, the metal organic framework material comprises a zeolite imidazolate framework material (ZIF), wherein the metal ions comprise transition metal ions, such as Co 2+ and / or Zn 2+ The organic ligand includes any one of imidazole and imidazole derivatives (such as 2-methylimidazole Hmim and benzimidazole bIm) or a combination of at least two thereof. Exemplarily, the metal organic framework material includes ZIF-8 (an octahedral metal organic framework composed of zinc and 2-methylimidazole).
[0042] In some optional embodiments of the present invention, the pore size of the activated carbon is 0.1-50nm, for example, it can be 0.5nm, 1nm, 2nm, 5nm, 8nm, 10nm, 12nm, 15nm, 18nm, 20nm, 22nm, 25nm, 28nm, 30nm, 32nm, 35nm, 38nm, 40nm, 42nm, 45nm or 48nm, as well as specific point values between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values included in the range.
[0043] In some optional embodiments of the present invention, the pore size of the molecular sieve is 0.4-10nm, for example, it can be 0.5nm, 0.8nm, 1nm, 1.5nm, 2nm, 2.5nm, 3nm, 3.5nm, 4nm, 4.5nm, 5nm, 5.5nm, 6nm, 6.5nm, 7nm, 7.5nm, 8nm, 8.5nm, 9nm or 9.5nm, as well as specific point values between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values included in the range.
[0044] And / or, the pore size of the organic conjugated material containing an acidic group is 0.1-50 nm, for example, it can be 0.5 nm, 1 nm, 2 nm, 5 nm, 8 nm, 10 nm, 12 nm, 15 nm, 18 nm, 20 nm, 22 nm, 25 nm, 28 nm, 30 nm, 32 nm, 35 nm, 38 nm, 40 nm, 42 nm, 45 nm or 48 nm, as well as specific point values between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values included in the range.
[0045] And / or, the pore size of the metal organic framework material is 0.1-50nm, for example, it can be 0.5nm, 1nm, 2nm, 5nm, 8nm, 10nm, 12nm, 15nm, 18nm, 20nm, 22nm, 25nm, 28nm, 30nm, 32nm, 35nm, 38nm, 40nm, 42nm, 45nm or 48nm, as well as specific point values between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values included in the range.
[0046] In the present invention, the pore structure of the porous absorption material can be directional and / or random holes, and can be independent holes and / or continuous holes according to its shape. The present invention does not specifically limit the arrangement direction and shape of the holes. The porous absorption material contains a rich pore structure. By optimizing the pore structure in the material, it can form a more effective and sufficient adsorption of gases such as I2 and NH3, block the invasion of water vapor, and prevent the gas from corroding and damaging the internal structure of the display module.
[0047] As used herein, the term "pore size" refers to the size of the pores in a porous absorbent material and can be understood as the equivalent diameter of the pores.
[0048] In some optional embodiments of the present invention, the porous absorbent material may be a micrometer-sized granular material, which is uniformly dispersed in the matrix resin to form the absorbent layer.
[0049] In some optional embodiments of the present invention, the particle size of the porous absorbent material is 0.01-40 μm, for example, it can be 0.1 μm, 0.2 μm, 0.5 μm, 0.8 μm, 1 μm, 2 μm, 3 μm, 5 μm, 8 μm, 10 μm, 12 μm, 15 μm, 18 μm, 20 μm, 22 μm, 25 μm, 28 μm, 30 μm, 32 μm, 35 μm or 38 μm, as well as specific point values between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values included in the range, and the optional range is 0.1-20 μm.
[0050] In some optional embodiments of the present invention, the porous absorption material comprises a combination of an organic conjugated material containing an acidic group, a metal organic framework material and optionally a molecular sieve.
[0051] In the present invention, the organic conjugated material containing an acidic group has a specific absorption effect on NH3 generated by the encapsulation layer, the metal organic framework material specifically absorbs I2 generated by the linear polarization layer, and the molecular sieve has a good physical adsorption effect on a variety of gases. Through the compounding of the organic conjugated material containing an acidic group, the metal organic framework material and the optional molecular sieve, the absorption layer plays a role in both specific absorption and physical adsorption, fully absorbs the gas escaping under high temperature and high humidity conditions, and effectively blocks water vapor, comprehensively preventing the gas from corroding and infringing the internal structure of the display module, and more thoroughly solves the problems of poor display and poor touch caused by failure, so that the display module has better display effect and touch effect.
[0052] In some optional embodiments of the present invention, the mass ratio of the organic conjugated material containing acidic groups to the metal organic framework material in the porous absorption material is (1-2):1, for example, it can be 1.1:1, 1.2:1, 1.3:1, 1.4:1, 1.5:1, 1.6:1, 1.7:1, 1.8:1 or 1.9:1, etc.
[0053] And / or, the mass percentage of molecular sieve in the porous absorption material is ≤50%, for example, it can be 0, 1%, 2%, 5%, 8%, 10%, 12%, 15%, 18%, 20%, 22%, 25%, 28%, 30%, 32%, 35%, 38%, 40%, 42%, 45% or 48%, as well as specific point values between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values included in the range, and a further optional value is 2-40%.
[0054] The present invention optimizes the types and proportions of the porous absorption materials in the absorption layer, so that the mass ratio of the organic conjugated material containing the acidic group to the metal organic framework material is (1-2):1, and the mass content of the molecular sieve in the porous absorption material is 2-40%. The three types of materials work together to more fully specifically absorb and physically adsorb gases such as NH3 and I2, and enable the absorption layer to block the invasion of water vapor, thereby preventing the gas from corroding and damaging the internal structure of the display module, and comprehensively improving the display touch effect and reliability of the display module.
[0055] In some optional embodiments of the present invention, the base resin includes polyacrylate.
[0056] In some optional embodiments of the present invention, the mass ratio of the matrix resin to the porous absorbent material in the absorption layer is 1:(0.2-1), for example, it can be 1:0.3, 1:0.4, 1:0.5, 1:0.6, 1:0.7, 1:0.8 or 1:0.9, etc.
[0057] In the present invention, the matrix resin in the absorption layer can disperse the porous absorption material and provide cohesion and adhesion. By further optimizing the mass ratio of the matrix resin to the porous absorption material to 1: (0.2-1), the absorption layer can more stably and reliably absorb gas and block water vapor intrusion, thereby improving the display effect and touch effect of the display module. If the amount of the matrix resin is too low, the adhesion between the absorption layer and the display panel and the polarizing component will be reduced, affecting the long-term stability of the absorption layer; if the amount of the matrix resin is too high, it will affect the absorption effect of the absorption layer on gas.
[0058] In some optional embodiments of the present invention, the display panel includes a display area and a non-display area surrounding the display area; and the projection of the absorption layer on the display panel is located in the non-display area.
[0059] like Figure 4 and Figure 5 As shown, Figure 4 A schematic diagram of the structure of a display module provided in another embodiment of the present invention includes a display panel 10, an absorption layer 20 and a polarizing component 30; the display panel 10 includes a touch layer 101, an encapsulation layer 102 and a light-emitting layer 103 arranged in sequence, and the touch layer 101 is located on a side close to the polarizing component 30; the polarizing component 30 includes a protective layer 301, a linear polarization layer 302, a wave plate layer 303 and a glue layer 304 arranged in sequence, and the glue layer 304 is located on a side close to the display panel 10. The display panel 10 includes a display area A1 and a non-display area A2 surrounding the display area A1, Figure 5 for Figure 4 The top view of the display module shown in the figure shows that the projection of the absorption layer 20 on the display panel 10 is located in the non-display area A2, so that under the premise that the absorption layer does not affect the display effect of the display module, it can fully absorb the I2, NH3 and other gases escaping from the polarizing component (linear polarization layer 302) and the display panel (encapsulation layer 102) under high temperature and high humidity conditions, prevent the gas from corroding and damaging the internal structure of the display panel and the polarizing component, and effectively reduce the corrosion of the metal touch layer that begins to occur at the edge of the display module under high temperature and high humidity conditions.
[0060] In some optional embodiments of the present invention, the width of the absorption layer 20 is 1.5-5mm, for example, it can be 1.8mm, 2mm, 2.2mm, 2.5mm, 2.8mm, 3mm, 3.2mm, 3.5mm, 3.8mm, 4mm, 4.2mm, 4.5mm or 4.8mm, as well as specific point values between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values included in the range.
[0061] The present invention further designs the width of the absorption layer 20 to be 1.5-5 mm, so that on the one hand, it can fully absorb the I2, NH3 and other gases escaping from the polarizing component (linear polarization layer 302) and the display panel (packaging layer 102) under high temperature and high humidity conditions, and block water vapor, effectively preventing the gas from corroding and damaging the internal structure of the display panel and the polarizing component, avoiding the risk of poor display and touch failure; on the other hand, the width of the absorption layer 20 is relatively narrow, which will not have an adverse effect on the display area and its display effect.
[0062] In some optional embodiments of the present invention, the thickness of the absorption layer 20 is L1, the thickness of the adhesive layer 304 is L2, L1 / L2≤0.3, for example, L1 / L2 can be 0.05, 0.06, 0.08, 0.1, 0.12, 0.15, 0.18, 0.2, 0.22, 0.25 or 0.28, as well as specific point values between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values included in the said range.
[0063] The present invention further designs the thickness ratio of the absorption layer 20 to the glue layer 304 in the polarizing assembly to be L1 / L2≤0.3, so that the thickness of the absorption layer 20 can fully meet the requirements of absorbing the I2 and NH3 gases escaping from the polarizing assembly (linear polarization layer 302) and the display panel (encapsulation layer 102) under high temperature and high humidity conditions, and effectively block water vapor to prevent the gas from corroding and damaging the internal structure of the display module, especially effectively reducing the corrosion of the metal touch layer that begins at the edge of the display module under high temperature and high humidity conditions, avoiding the risk of poor display and touch failure. At the same time, the absorption layer 20 has little effect on the overall thickness of the display module, so that the display module remains thin and portable.
[0064] In some optional embodiments of the present invention, the thickness of the polarizing component 30 is 40-150 μm, for example, it can be 50 μm, 60 μm, 70 μm, 80 μm, 90 μm, 100 μm, 110 μm, 120 μm, 130 μm or 140 μm, as well as specific point values between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values included in the said range.
[0065] In some optional embodiments of the present invention, the display module is a foldable display module.
[0066] Compared with non-foldable display modules, foldable display modules with flexible features are more likely to experience polarizer failure and fading, display abnormality, reduced touch sensitivity, and even touch failure under high temperature and high humidity conditions. The present invention can effectively block water vapor through the design of the absorption layer, fully absorb the I2 and NH3 gases escaping from the polarizing assembly (linear polarization layer 302) and the display panel (encapsulation layer 102) under high temperature and high humidity conditions, and prevent the gas from corroding and damaging the internal structure of the foldable display module, especially effectively reducing the corrosion of the metal touch layer starting from the edge of the foldable display module under high temperature and high humidity conditions, thereby significantly improving the yield, reliability, and quality of the foldable display module.
[0067] In some optional embodiments of the present invention, the thickness of the polarizing component in the folding display module is 40-80μm, for example, it can be 42μm, 45μm, 48μm, 50μm, 52μm, 55μm, 58μm, 60μm, 62μm, 65μm, 68μm, 70μm, 72μm, 75μm or 78μm, as well as specific point values between the above point values. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values included in the said range.
[0068] In some optional embodiments, the present invention conducts reliability evaluation on the display module and the folding display module provided in the aforementioned embodiments under high temperature and high humidity conditions. Specifically, after a preset time of double 85 (85°C, humidity 85% RH) or 6090 test, a scanning electron microscope (SEM) and an X-ray energy spectrometer (EDX) are used to test the edge structure of the display module and the folding display module. Due to the design of the absorption layer, the display module and the folding display module of the present invention have excellent reliability in a high temperature and high humidity environment, and there is no problem of corrosion of the edge of the metal touch layer, failure of the polarizing component, or poor display and touch.
[0069] In some optional embodiments of the present invention, the method for preparing the display module includes:
[0070] providing an absorbent adhesive comprising a combination of a prepolymer and a porous absorbent material;
[0071] The absorption adhesive is coated between the display panel and the polarizing component, and is cured to form an absorption layer to obtain the display module.
[0072] Optionally, the prepolymer includes an acrylate prepolymer, which is cured to obtain a polyacrylate as the matrix resin of the absorption layer. The present invention does not specifically limit the specific type of the acrylate prepolymer, and any acrylate prepolymer containing unsaturated double bond functional groups known in the art can be applied to the present invention.
[0073] Optionally, the absorbent adhesive further comprises any one of an initiator, a cross-linking agent, a diluent, and an auxiliary agent, or a combination of at least two of them.
[0074] Optionally, the initiator includes a photoinitiator, which enables the absorbing adhesive to be cured under ultraviolet light irradiation conditions to obtain the absorbing layer.
[0075] Optionally, the photoinitiator includes any one of alkyl phenone compounds, benzophenone compounds, benzil compounds, benzoin compounds, and acylphosphine oxide compounds, or a combination of at least two thereof.
[0076] Optionally, the crosslinking agent includes an acrylate compound with a functionality ≥ 2 (eg, a functionality of 2, 3, 4, 5, 6, etc.), which is cured with an acrylate prepolymer in the presence of an initiator to obtain a polyacrylate as a matrix resin of the absorption layer.
[0077] Optionally, the auxiliary agent includes any one or a combination of at least two of a coupling agent (such as a silane coupling agent, a titanate coupling agent, etc.), a dispersant, a leveling agent, a defoaming agent, an antioxidant, a viscosity regulator, and a stabilizer.
[0078] An embodiment of the present invention further provides a display device, which includes any display module provided by the embodiment of the present invention.
[0079] Since the display device adopts the above display module, the display device also has the technical effect of the display module described in the above embodiment. It should be noted that the display device provided in the embodiment of the present invention may also include other circuits and devices for supporting the normal operation of the display device. The display device exemplarily includes but is not limited to: any one of a mobile phone, a tablet computer, an electronic photo frame, and an electronic paper.
[0080] The applicant declares that the present invention illustrates the display module of the present invention and the display device including the same through the above-mentioned embodiments, but the present invention is not limited to the above-mentioned process steps, that is, it does not mean that the present invention must rely on the above-mentioned process steps to be implemented. Those skilled in the art should understand that any improvement of the present invention, equivalent replacement of the raw materials selected by the present invention, addition of auxiliary components, selection of specific methods, etc., all fall within the protection scope and disclosure scope of the present invention.
Claims
1. A display module, characterized in that: The display module comprises a display panel, a polarizing component and an absorption layer arranged between the display panel and the polarizing component; the absorption layer comprises a combination of a matrix resin and a porous absorption material.
2. The display module according to claim 1, characterized in that: The display panel comprises a light-emitting layer, a touch layer and a packaging layer arranged between the light-emitting layer and the touch layer; the touch layer is located on a side close to the polarizing component.
3. The display module according to claim 2, characterized in that: The encapsulation layer includes silicon nitride and silicon oxide.
4. The display module according to claim 2, characterized in that: The touch layer includes a metal touch layer.
5. The display module according to claim 1, characterized in that: The polarizing assembly comprises a glue layer, a wave plate layer, a linear polarization layer and a protective layer which are arranged in sequence; the glue layer is located on a side close to the display panel.
6. The display module according to claim 5, characterized in that: The linear polarization layer is an iodine-based polarizer.
7. The display module according to claim 1, characterized in that: The porous absorption material includes any one of molecular sieves, activated carbon, organic conjugated materials containing acidic groups, and metal organic framework materials, or a combination of at least two of them.
8. The display module according to claim 7, characterized in that: The acidic group in the organic conjugated material containing an acidic group includes at least one of a carboxylic acid group, a phosphoric acid group, and a sulfonic acid group; And / or, the organic conjugated structure in the organic conjugated material containing an acidic group includes a benzene structure, a biphenyl structure, a naphthalene structure, an anthracene structure, a phenanthrene structure, a triphenylene structure, a pyrene structure, At least one of the structures.
9. The display module according to claim 7, characterized in that: The metal organic framework material is a metal organic framework material containing electron-rich groups.
10. The display module according to claim 7, characterized in that: The pore size of the molecular sieve is 0.4-10 nm; and / or the pore size of the organic conjugated material containing an acidic group is 0.1-50 nm; and / or the pore size of the metal organic framework material is 0.1-50 nm.
11. The display module according to claim 7, characterized in that: The porous absorption material comprises a combination of an organic conjugated material containing an acidic group, a metal organic framework material and optionally a molecular sieve.
12. The display module according to claim 11, characterized in that: The mass ratio of the organic conjugated material containing an acidic group to the metal organic framework material in the porous absorption material is (1-2):1; And / or, the mass percentage of molecular sieve in the porous absorption material is ≤50%.
13. The display module according to claim 1, characterized in that: The base resin includes polyacrylate.
14. The display module according to claim 1, characterized in that: The mass ratio of the matrix resin to the porous absorbent material in the absorbent layer is 1:(0.2-1).
15. The display module according to claim 1, characterized in that: The display panel comprises a display area and a non-display area surrounding the display area; a projection of the absorption layer on the display panel is located in the non-display area.
16. The display module according to claim 15, characterized in that: The width of the absorption layer is 1.5-5 mm.
17. The display module according to claim 5, characterized in that: The thickness of the absorption layer is L1, the thickness of the adhesive layer is L2, and L1 / L2≤0.
3.
18. The display module according to claim 1, characterized in that: The thickness of the polarizing component is 40-150 μm.
19. The display module according to claim 1, characterized in that: The display module is a foldable display module.
20. The display module according to claim 19, characterized in that: The thickness of the polarizing component in the folding display module is 40-80 μm.
21. A display device, characterized in that: The display device comprises the display module as described in any one of claims 1-20.