Systems and methods for using polyacrylamide gels to resist corrosion of wellhead components in square wells

By using uncrosslinked polyacrylamide gel to cover wellhead components and extend to the base and sidewalls of the square well, a barrier is formed, solving the corrosion problem of wellhead components in square wells, achieving effective protection, reducing maintenance costs and time, and improving production efficiency.

CN118974203APending Publication Date: 2024-11-15SAUDI ARABIAN OIL CO
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380030985.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-03-31
Filing Date
2023-03-31
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

Wellhead components in square wells are susceptible to corrosion from water and dissolved oxygen, leading to corrosion problems. Existing technologies are unable to effectively prevent or slow down this corrosion, especially the corrosion of the casing head base and the surface casing.

Method used

Uncrosslinked polyacrylamide gel is used to cover the outer surface of the wellhead component and extend to the base and sidewalls of the square well to form a barrier to prevent water and other liquids from contacting the wellhead component. A sand layer is then applied over the polyacrylamide gel to further seal the pores.

Benefits of technology

It effectively prevents or slows down the corrosion of wellhead components, reduces the need for maintenance and replacement of wellhead components, lowers costs and time, improves production efficiency, and reduces safety and environmental risks.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0005062646190000071
    Figure BDA0005062646190000071
  • Figure HDA0005062646200000011
    Figure HDA0005062646200000011
  • Figure HDA0005062646200000021
    Figure HDA0005062646200000021
Patent Text Reader

Abstract

Systems and methods are disclosed that use a polyacrylamide gel to resist corrosion of one or more wellhead components in a square well. Examples of such wellhead components include a surface casing and a casing head chassis. The square well is part of a well, such as an oil, gas or water well.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] Priority declaration

[0002] This application claims priority to U.S. patent application No. 17 / 710,021, filed on March 31, 2022, the entire contents of which are incorporated herein by reference. Technical Field

[0003] The present disclosure generally relates to systems and methods for resisting corrosion of wellhead components in square wells using polyacrylamide gels. Typically, the polyacrylamide in the gel is not cross-linked. Background Art

[0004] Typically, an oil production well has an above-ground wellhead component and an underground wellhead component. Some of the underground wellhead components are present in the well. Examples of such wellhead components include surface casing and casing head chassis. Typically, the wellhead components in the well are covered with sand. In some cases, the above-ground wellhead components (such as injection pipeline flanges) may leak and cause the sand in the well to become wet. In some cases, rainwater causes the sand in the well to become wet. Other water sources may also make the sand in the well wet. The water in the sand in the well may cause corrosion of one or more of the wellhead components present in the well (such as casing head chassis and / or surface casing). In addition to the water itself, corrosion may also be caused by oxygen dissolved in the water. Summary of the invention

[0005] The present disclosure generally relates to systems and methods for resisting corrosion of wellhead components in square wells using polyacrylamide gel. For example, the well of the system can be an oil well, a gas well or a water well. Typically, the polyacrylamide in the gel is not cross-linked. In general, the present disclosure provides a polyacrylamide gel that occupies a volume extending from the surface of the wellhead component to the base and sidewalls of the square well, rather than simply covering the surface of the wellhead component with a relatively thin coating. As an example, in some embodiments, the polyacrylamide gel covers a portion of the surface of the wellhead surface casing and extends to the base and sidewalls of the square well, so that the polyacrylamide gel occupies the spatial volume between the square well and the covered surface of the surface casing. As another example, in certain embodiments, the polyacrylamide gel covers at least a portion of the surface of the casing head chassis (e.g., completely covers) and extends to the base and sidewalls of the square well, so that the polyacrylamide gel occupies the spatial volume between the square well and the covered surface of the casing head chassis. As another example, in some embodiments, the polyacrylamide gel covers a portion of the surface of the wellhead surface casing and at least a portion of the surface of the casing head chassis (e.g., completely covers) and extends to the base and sidewalls of the square well, so that the polyacrylamide gel occupies the spatial volume between the square well and the covered surface of the wellhead surface casing and the covered surface of the casing head chassis. Typically, sand is arranged on top of the polyacrylamide gel and completely covers the upper surface of the gel. Therefore, typically, the polyacrylamide gel is not directly exposed to the surface.

[0006] For a considerable period of time, little if any water in the sand covered with polyacrylamide gel is able to penetrate through the polyacrylamide gel to reach one or more gel-covered wellhead components. Therefore, the polyacrylamide gel helps to resist or even completely prevent corrosion of the gel-covered wellhead components. Without wishing to be bound by theory, it is believed that the polyacrylamide gel in contact with the sand can seal the pores in the sand to prevent water from dispersing into the sand mesh. For example, when water is placed on top of such sand, the water will not enter the mesh. Instead, the water is retained on the top of the sand mesh and eventually evaporates. In this way, the gel can behave as a barrier to water and optionally other liquids.

[0007] These systems and related methods can be relatively cheap and easy to produce and implement. In addition, these systems and methods can alleviate safety issues and environmental impacts associated with corrosion of wellhead components. In addition, these systems and methods can reduce or eliminate the need to repair and / or replace corroded wellhead components, which may be expensive and difficult to repair and / or replace corroded wellhead components. In addition, the system and method according to the present disclosure can reduce the time and cost associated with monitoring and inspecting the corrosion of wellhead components. As an example, the casing head chassis is a wellhead component located in a square well. Usually, the casing head chassis cannot be replaced at will. As a result, the loss of use time of the well and / or the cost associated with repairing or replacing the casing head chassis may be considerable. As another example, a portion of the wellhead surface casing in a square well may be severely corroded by moisture. Repairing such corroded surface casing may involve deep excavation of the wellhead, and replacing such corroded surface casing may involve workover. Therefore, using polyacrylamide gel to reduce or eliminate the corrosion of the casing head chassis and / or the wellhead surface casing can greatly save and improve productivity.

[0008] In a first aspect, the present disclosure provides a system comprising a square well, a wellhead, and a polyacrylamide gel. The square well has a base and a sidewall extending from the base. The wellhead has an above-ground region extending above the square well and an underground region in the square well. The underground region of the wellhead includes a wellhead component having an outer surface. The polyacrylamide gel occupies a volume extending from the base and sidewall of the square well to the outer surface of the wellhead component. The polyacrylamide gel covers the outer surface of the wellhead component.

[0009] In some embodiments, the polyacrylamide in the gel is not cross-linked.

[0010] In some embodiments, the polyacrylamide in the gel has a number average molecular weight of 1,000 to 10,000,000 g / mol.

[0011] In some embodiments, the polyacrylamide in the gel has a weight average molecular weight of 1,000 to 10,000,000 g / mol.

[0012] In some embodiments, the polyacrylamide gel substantially prevents water from passing through the polyacrylamide gel to the outer surface of the wellhead member.

[0013] In some embodiments, the system further comprises a solid covering the upper surface of the polyacrylamide gel.

[0014] In some embodiments, the system further comprises sand covering the upper surface of the polyacrylamide gel. The polyacrylamide gel can seal the pores in the sand.

[0015] In some embodiments, the wellhead component includes a casing head chassis.

[0016] In some embodiments, the wellhead component includes surface casing.

[0017] In some embodiments, the polymer gel covers an outer surface of the additional wellhead component.

[0018] In some embodiments, the polymer gel covers the exterior surfaces of various components of the wellhead, such as the surface casing and the casing head chassis.

[0019] In some embodiments, the system includes a well selected from the group consisting of an oil well, a gas well, and a water well.

[0020] In some embodiments, the volume occupied by the gel is at least one cubic foot.

[0021] In some embodiments, the base of the square well has an opening, and the wellhead includes a plurality of casings extending through and below the base of the square well.

[0022] In some embodiments, the plurality of sleeves includes a surface sleeve that receives the other sleeves.

[0023] In a second aspect, the present disclosure provides a well, which is an oil well, a gas well or a water well. The well includes a square well, a wellhead and a polyacrylamide gel. The square well has a base and a sidewall extending from the base. The wellhead has an above-ground area extending above the square well and an underground area in the square well. The underground area of ​​the wellhead includes a wellhead component having an outer surface. The polyacrylamide gel occupies a volume extending from the base and sidewall of the square well to the outer surface of the wellhead component. The polyacrylamide gel covers the outer surface of the wellhead component.

[0024] In a third aspect, the present disclosure provides a method for reducing corrosion of an outer surface of a wellhead component in a square well. The method includes placing a polyacrylamide gel in the square well so that the polymer gel covers the outer surface of the wellhead component and extends to the base and sidewalls of the square well.

[0025] In some embodiments, disposing the polyacrylamide gel in the square well includes disposing polyacrylamide in the square well, and adding water to the polyacrylamide to form the polyacrylamide gel.

[0026] In some embodiments, the method further comprises covering the polyacrylamide gel with sand. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] Figure 1 is a schematic diagram of the system.

[0028] Figure 2 is a schematic diagram of the system.

[0029] Figure 3 is a schematic diagram of the system.

[0030] Figure 4 is a schematic diagram of the system.

[0031] Figure 5 are photographs of sand and polyacrylamide powder in various test tubes.

[0032] Figure 6 is a photograph of water formation on a polyacrylamide gel which in turn is supported by sand.

[0033] Figure 7 is a photograph of wet sand supported by a polyacrylamide gel which in turn is supported by the sand. DETAILED DESCRIPTION

[0034] Figure 1 Schematically depicted is a system 1000 which may be, for example, part of a well such as an oil well, a gas well, or a water well.

[0035] System 1000 includes a square well 1010 having a bottom 1020 and sidewalls 1030. An uppermost surface 1012 of square well 1010 substantially corresponds to a ground surface 1040, such that square well 1010 is generally located underground.

[0036] System 1000 also includes a wellhead 1050 having an above-ground wellhead region 1060 extending above surface 1040 and a subsurface wellhead region 1070 extending below surface 1040 through wellbore 1010 and through an opening 1025 in bottom 1020 of wellbore 1010. Typically, wellhead regions 1060 and 1070 have a variety of different components. As an example, Figure 1 As shown, the above-ground wellhead area 1060 may include a water injection pipeline flange 1062 and a crown adapter 1064, and the underground wellhead area 1070 may include a casing head chassis 1072 and a tubing head 1074. The wellhead 1050 includes a surface casing 1076, the outer surface of which is exposed in the square well 1010. The surface casing 1076 accommodates a plurality of nested casings, which are exposed below the bottom 1020 of the square well 1010 (see Figures 2 to 4 ).

[0037] Figure 2The system 2000 is schematically depicted, and includes a wellhead 2050 having an above-ground region 2060 and a subsurface region 2070, respectively. The above-ground region 2060 includes a water injection valve 2062, a crown adapter 2064, an additional valve 2066, and a tubing head 2068. The subsurface region 2070 includes a casing head chassis 2072 and a tubing head 2074, which are arranged above the bottom 2020 of the square well. The subsurface region 2070 also includes a plurality of nested casings, which are housed within surface casings (generally depicted at 2076) and extend below the bottom 2020 of the square well.

[0038] Figure 3 The system 3000 is schematically depicted, and includes a wellhead 3050 having an above-ground region 3060 and a subsurface region 3070. The above-ground region 3060 includes a water flow conduit 3061 in fluid communication with an injection valve 3062. In addition, the above-ground region includes a crown adapter 3064 and additional valves 3066 and 3067. The subsurface region 3070 includes a casing head chassis 3072 and a tubing head 3074, which are arranged above the bottom 3020 of the square well. The subsurface region 3070 further includes surface casing and a plurality of nested casings (generally depicted as 3076), which extend through the bottom 3020 of the square well and below the bottom. In some embodiments, the injection line flange between the water flow conduit 3061 and the injection valve 3062 may leak, for example, due to air exposure and continuous water flow. This may cause leaking water to overflow onto the sand covering the wellbore, which may cause corrosion of the surface casing 3076, casing head chassis 3072 and / or tubing head 3074.

[0039] Figure 4 The underground area of ​​the wellhead 4050 is schematically depicted. Above the bottom 4020 of the square well, the wellhead 4050 includes a casing head chassis 4072, a circular ring plate 4073, and a surface casing 4076. The surface casing 4076 extends through the opening 4025 in the bottom 4020 of the square well and enters the conductor 4075. The surface casing 4076 accommodates a plurality of nested casings 4077, 4078, and 4079. In some embodiments, the bottom 4020 of the square well is made of cement. The integrity of cement is sometimes low, and cracks may occur in the cement, which may allow water to penetrate, thereby causing corrosion, for example, at the interface of the surface casing 4076 and the bottom 4020 of the square well. Polyacrylamide gel can reduce, for example, prevent such corrosion.

[0040] Reference again Figure 1, the system 1000 also includes a polyacrylamide gel 1080 that completely covers a portion of the outer surface of the surface casing 1076 and the casing head chassis 1072 and extends to the bottom 1020 and the sidewalls 1030 of the square well 1010. Therefore, the polyacrylamide gel 1080 occupies the spatial volume between the square well 1010 and the gel-covered outer surfaces of the surface casing 1076 and the casing head chassis 1072. The sand layer 1090 is arranged on top of the polyacrylamide gel 1080. With this arrangement, the polyacrylamide gel 1080 acts as a barrier that prevents water present in the sand 1090 from reaching the gel-covered outer surfaces of the surface casing 1076 and the casing head chassis 1072 for a considerable period of time, thereby maintaining a substantially dry condition around the gel-covered outer surfaces of the surface casing 1076 and the casing head chassis 1072. As a result, the polyacrylamide gel helps resist and even completely prevent corrosion of the gel-covered exterior surfaces of the skin sleeve 1076 and the sleeve head chassis 1072 during these time periods.

[0041] Typically, polyacrylamide gel 1080 contains polyacrylamide and water. Typically, polyacrylamide gel is formed by exposing polyacrylamide to water to swell the polyacrylamide to form a gel, after which the gel 1080 can be arranged in the square well 1010 using any suitable method. In some embodiments, polyacrylamide is arranged in the square well 1010 in a dry solid form (such as a powder). Water is then added to form the gel, after which sand 1090 is arranged on top of the gel 1080. In certain embodiments, water and polyacrylamide are first mixed (with stirring if appropriate), and then placed in the square well 1010 to form the gel 1080, after which the sand 1090 is arranged on top of the gel 1080.

[0042] In some embodiments, gel 1080 contains at least 1 kg (eg, at least 10 kg, at least 100 kg) of polyacrylamide and at most 1000 kg (eg, at most 500 kg, at most 300 kg) of polyacrylamide.

[0043] In certain embodiments, gel 1080 contains at least 0.1 bbl (eg, at least 0.25 bbl, at least 0.5 bbl) of water and at most 5 bbl (eg, at most 2 bbl, at most 1 bbl) of water.

[0044] In some embodiments, gel 1080 contains at least 5 (e.g., 5.88, at least 10, at least 15, at least 20, at least 25, at least 30, at least 35, at least 40, at least 45, at least 50, at least 55, at least 55.71) weight percent (wt.%) polyacrylamide and at most 56 (e.g., 55.7, at most 55, at most 50, at most 45, at most 40, at most 35, at most 30, at most 25, at most 20, at most 15, at most 10) wt.% polyacrylamide.

[0045] In some embodiments, gel 1080 contains at least 44 (e.g., 44.29, at least 45, at least 50, at least 55, at least 60, at least 65, at least 70, at least 75, at least 80, at least 85, at least 90, at least 94, at least 94.12) wt % water and at most 95 (e.g., at most 94.12, at most 94, at most 90, at most 85, at most 80, at most 75, at most 70, at most 65, at most 60, at most 55, at most 50, at most 45) wt % water.

[0046] Optionally, gel 1080 may contain one or more additional ingredients, such as a corrosion inhibitor (e.g., O-3670R) and / or an oxygen scavenger (e.g., sodium sulfite (Na2SO3), OXYGON TM Or FE-20). In some embodiments, gel 1080 contains at least 0.04 wt.% (e.g., at least 0.07 wt.%, at least 0.1 wt.%) of an oxygen scavenger and at most 1 wt.% (e.g., at most 0.9 wt.%, at most 0.8 wt.%) of an oxygen scavenger. In certain embodiments, gel 1080 contains at least 5 wt.% (e.g., at least 8 wt.%, at least 10 wt.%) of a corrosion inhibitor and at most 15 wt.% (e.g., at most 12 wt.%) of a corrosion inhibitor.

[0047] Generally, polyacrylamide contains repeating units having the following chemical structure.

[0048]

[0049] In certain embodiments, polyacrylamide can be a copolymer containing the above repeating unit and one or more different repeating units. Examples of such repeating units (except acrylamide) include, but are not limited to, N, N'-methylenebisacrylamide, N, N'-bisacryloylcystamine, N, N'diallyltartaric acid diamide, N, N'-(1,2-dihydroxyethylene)bisacrylamide, ethylene glycol diacrylate, and piperazine diacrylate.

[0050] In some embodiments, the polyacrylamide is substantially uncrosslinked. For example, the polyacrylamide has less than 10-8 (For example, less than 10 -9 , less than 10 -10 )mol / cm 3 In certain embodiments, the polyacrylamide is a linear polyacrylamide, that is, the polyacrylamide is completely uncrosslinked.

[0051] In certain embodiments, the polyacrylamide can have a weight of at least 1,000 (e.g., at least 10,000, at least 40,000, at least 50,000, at least 100,000, at least 150,000, at least 200,000, at least 300,000, at least 400,000, at least 500,000, at least 520,000, at least 600,000, at least 700,000, at least 800,000, at least 900,000, at least 1,000,000, at least 2,000,000, at least 3,000,000, at least 4,000,000, at least 5,000,000, at least 6,000,000, at least 7,000,000, at least 8,000,000, at least 9,000,000) g / m ol and up to 10,000,000 (e.g., up to 9,000,000, up to 8,000,000, up to 7,000,000, up to 6,000,000, up to 5,000,000, up to 4,000,000, up to 3,000,000, up to 2,000,000, up to 1,000,000, up to 900,000, up to The number average molecular weight of the polymer may be up to 800,000, up to 700,000, up to 600,000, up to 520,000, up to 500,000, up to 400,000, up to 300,000, up to 200,000, up to 150,000, up to 100,000, up to 50,000, up to 40,000, up to 10,000) g / mol.

[0052] In certain embodiments, the polyacrylamide can have a weight of at least 1,000 (e.g., at least 10,000, at least 40,000, at least 50,000, at least 100,000, at least 150,000, at least 200,000, at least 300,000, at least 400,000, at least 500,000, at least 520,000, at least 600,000, at least 700,000, at least 800,000, at least 900,000, at least 1,000,000, at least 2,000,000, at least 3,000,000, at least 4,000,000, at least 5,000,000, at least 6,000,000, at least 7,000,000, at least 8,000,000, at least 9,000,000) g / m ol and up to 10,000,000 (e.g., up to 9,000,000, up to 8,000,000, up to 7,000,000, up to 6,000,000, up to 5,000,000, up to 4,000,000, up to 3,000,000, up to 2,000,000, up to 1,000,000, up to 900,000, up to The weight average molecular weight of the polymer may be up to 800,000, up to 700,000, up to 600,000, up to 520,000, up to 500,000, up to 400,000, up to 300,000, up to 200,000, up to 150,000, up to 100,000, up to 50,000, up to 40,000, up to 10,000) g / mol.

[0053] In some embodiments, the volume occupied by the gel is at least 1 ft 3 (For example, at least 5ft 3 , at least 10ft 3 ) and up to 30ft 3 (For example, up to 25ft 3 , up to 20ft 3 ).

[0054] Examples

[0055] A layer of dry sand was placed in a test tube to simulate a square well. 1.25 g of polyacrylamide powder ( Linear polyacrylamide, Merck (MERCK)) was disposed on the sand to form a polyacrylamide layer. Figure 5 Shown are sand and polyacrylamide in separate test tubes before polyacrylamide powder is placed on top of the sand. 7.5 mL of water is added to the polyacrylamide, which causes swelling of the mixture, and then 5 mL of additional water is added, confirming by visual inspection that the polyacrylamide gel is impermeable to water. Figure 6A test tube with a sand layer covered with a polyacrylamide gel is shown, which is covered by a water layer formed by an additional 5 mL of water. After 3 hours, the sand is placed on top of the polyacrylamide gel. Then, 5 mL of water is added and it is confirmed by visual observation that the polyacrylamide gel is impermeable to water. Figure 7 An underlying layer of sand is shown covered by a polyacrylamide gel which in turn is covered by a layer of wet sand.

[0056] Other embodiments

[0057] Although certain embodiments have been disclosed, the disclosure is not limited to such embodiments.

[0058] As an example, although embodiments have been disclosed in which a sand layer is disposed on top of a polyacrylamide gel layer, in some embodiments, there is no sand layer above the polyacrylamide gel. As an example, in certain embodiments, the polyacrylamide gel may be covered with a different material, such as, but not limited to, silica, alumina, or small gravel rocks. As another example, in some embodiments, the polyacrylamide gel extends to the upper surface of the well, i.e., the ground surface.

Claims

1. A system comprising: A square well, the square well comprising a base and side walls extending from the base; a wellhead, the wellhead comprising an above-ground region extending above the square well and an underground region in the square well, the underground region of the wellhead comprising a wellhead component having an outer surface; as well as A polyacrylamide gel occupies a volume extending from the base and sidewalls of the square well to the outer surface of the wellhead member, wherein the polyacrylamide gel covers the outer surface of the wellhead member.

2. The system of claim 1, wherein: The polyacrylamide in the gel is not cross-linked.

3. The system of claim 1, wherein: The polyacrylamide in the gel has a number average molecular weight of 1,000 to 10,000,000 g / mol.

4. The system of claim 1, wherein: The polyacrylamide in the gel has a weight average molecular weight of 1,000 to 10,000,000 g / mol.

5. The system of claim 1, wherein: The polyacrylamide gel substantially prevents water from passing through the polyacrylamide gel to the outer surface of the wellhead member.

6. The system of claim 1, further comprising a solid covering the upper surface of the polyacrylamide gel.

7. The system of claim 1, further comprising sand covering the upper surface of the polyacrylamide gel.

8. The system of claim 7, wherein: The polyacrylamide gel seals the pores in the sand.

9. The system of claim 1, wherein: The wellhead assembly includes a casing head chassis.

10. The system of claim 1, wherein: The wellhead component includes a surface casing.

11. The system of claim 10, wherein: The polymer gel covers the outer surface of the additional wellhead component.

12. The system of claim 11, wherein: The additional wellhead components include a casing head chassis.

13. The system of claim 1, wherein: The system includes a well selected from the group consisting of an oil well, a gas well, and a water well.

14. The system of claim 1, wherein: The volume occupied by the gel is at least 1 ft 3 .

15. The system of claim 1, wherein: The base of the square well has an opening, and the wellhead includes a plurality of casings extending through the base of the square well and below the base of the square well.

16. The system of claim 15, wherein: The plurality of casings include a surface casing that receives the other casings.

17. A well comprising: A square well, the square well comprising a base and side walls extending from the base; a wellhead, the wellhead comprising an above-ground region extending above the wellhead and a subterranean region within the wellhead, the subterranean region of the wellhead comprising a member having an outer surface; as well as A polyacrylamide gel occupies a volume extending from the outer surface of the member to the base and sidewalls of the square well, wherein the well comprises a member selected from the group consisting of an oil well, a gas well, and a water well.

18. A method for reducing corrosion of an outer surface of a wellhead component in a square well, the method comprising: A polyacrylamide gel is arranged in the square well so that the polymer gel covers the outer surface of the wellhead member and extends to the base and sidewalls of the square well.

19. The method of claim 18, wherein: Arranging the polyacrylamide gel in the square well comprises: Arrange polyacrylamide in the square well: and Water is added to the polyacrylamide to form the polyacrylamide gel.

20. The method of claim 18, further comprising covering the polyacrylamide gel with sand.