Lens unit, display body, and display method
By using a combination of reflective polarization member, semi-reflective mirror and multi-layered member in the lens part of the VR goggles, combined with the optimized configuration of the adhesive layer, the problems of large weight and poor visual recognition of the existing VR goggles are solved, and the problem of high weight and poor visual recognition is realized. Lightweight and visual effects are improved.
Patent Information
- Application Number
- CN202380027586.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-12-28
- Filing Date
- 2023-03-08
- Publication Date
- 2024-11-15
AI Technical Summary
The lens part of the existing VR goggles is relatively large, which affects the visual recognition and makes it difficult to achieve lightweight and improve visual recognition.
Using a combination of reflective polarization members, semi-reflective mirrors and multi-layered members, the optimized configuration of the adhesive layer can achieve precise control of the optical path and optical characteristics optimization, including the configuration of reflective polarization members, absorption polarization members and protective members. Controls ISC values and surface roughness to reduce the full emission and reflection of light.
The lightweight and visual recognition of VR goggles are achieved, and the clarity and visual effect of the image are improved by suppressing the full emission and unevenness of light.
Smart Images

Figure CN118974640A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a lens portion, a display body and a display method. Background Art
[0002] Image display devices represented by liquid crystal display devices and electroluminescent (EL) display devices (e.g., organic EL display devices) are rapidly becoming popular. In image display devices, optical components such as polarization components and phase difference components are generally used to realize image display and improve image display performance (e.g., refer to Patent Document 1).
[0003] In recent years, new uses for image display devices have been developed. For example, goggles with displays (VR goggles) for realizing Virtual Reality (VR) have begun to be commercialized. Since the use of VR goggles in various scenarios has been studied, it is expected that they will be lightweight and have improved visual recognition. Lightweighting can be achieved, for example, by thinning the lenses used for VR goggles. On the other hand, it is also expected to develop optical components suitable for display systems using thin lenses.
[0004] Prior art literature
[0005] Patent Literature
[0006] Patent Document 1: Japanese Patent Application Publication No. 2021-103286 Summary of the invention
[0007] Problems to be solved by the invention
[0008] In view of the above circumstances, a main object of the present invention is to provide a lens unit that can achieve weight reduction and improved visibility of VR goggles.
[0009] Solutions to the problem
[0010] 1. A lens unit according to an embodiment of the present invention is used in a display system for displaying an image to a user,
[0011] The lens unit includes:
[0012] a reflective polarizing member that reflects light emitted from a display surface of a display element that displays an image and that passes through the polarizing member and a first λ / 4 member; a first lens portion that is disposed on an optical path between the display element and the reflective polarizing member; a half mirror that is disposed between the display element and the first lens portion and transmits light emitted from the display element and reflects light reflected by the reflective polarizing member toward the reflective polarizing member; a second lens portion that is disposed in front of the reflective polarizing member; and a second λ / 4 member that is disposed on an optical path between the half mirror and the reflective polarizing member.
[0013] The ISC values of the first laminated portion including the second λ / 4 member and at least one adhesive layer and the second laminated portion including the reflective polarizing member and at least one adhesive layer are 100 or less.
[0014] 2. In the lens section described in 1 above, the second stacked section may include an absorptive polarization element disposed between the reflective polarization element and the second lens section.
[0015] 3. In the lens unit described in 1 or 2 above, the second stacked portion may include a third λ / 4 element disposed between the reflective polarization element and the second lens unit.
[0016] 4. In the lens portion according to any one of 1 to 3 above, the first stacked portion may be disposed separately from the second stacked portion.
[0017] 5. In the lens section according to any one of 1 to 4 above, the second stacked section may include a second protective member disposed behind the reflective polarization element.
[0018] 6. In the lens unit according to any one of 1 to 5 above, the first stacked portion may include a first protective member disposed in front of the second λ / 4 member.
[0019] 7. In the lens portion according to any one of 1 to 6 above, the total number of the adhesive layer contained in the first laminated portion and the adhesive layer contained in the second laminated portion may be three or more layers.
[0020] 8. In the lens portion according to any one of 1 to 7 above, the pressure-sensitive adhesive layer included in the first laminated portion and the pressure-sensitive adhesive layer included in the second laminated portion may each have a thickness of 20 μm or less.
[0021] 9. In the lens portion according to any one of 1 to 8 above, the adhesive layer included in the first laminated portion and the adhesive layer included in the second laminated portion may each have a surface roughness Ra of 20 nm or less.
[0022] 10. In the lens section according to any one of 1 to 9 above, the pressure-sensitive adhesive layer included in the first laminated portion and the pressure-sensitive adhesive layer included in the second laminated portion may each be a single layer body.
[0023] 11. In the lens unit according to any one of 1 to 10 above, the first lens unit and the half mirror may be integrated.
[0024] 12. A display according to an embodiment of the present invention includes the lens unit according to any one of 1 to 11 above.
[0025] 13. The display method according to the embodiment of the present invention has the following features:
[0026] a step of allowing the light of the display image emitted through the polarization element and the first λ / 4 element to pass through the half mirror and the first lens portion;
[0027] A step of allowing the light that has passed through the half mirror and the first lens portion to pass through a second λ / 4 member;
[0028] A step of causing the light that has passed through the second λ / 4 member to be reflected toward the half mirror by the reflective polarization member;
[0029] a step of allowing the light reflected by the reflective polarization member and the half mirror to pass through the reflective polarization member via the second λ / 4 member; and
[0030] a step of allowing the light transmitted through the reflective polarizing member to pass through a second lens unit,
[0031] The ISC values of the first laminated portion including the second λ / 4 member and at least one adhesive layer and the second laminated portion including the reflective polarizing member and at least one adhesive layer are 100 or less.
[0032] Effects of the Invention
[0033] According to the lens unit of the embodiment of the present invention, it is possible to achieve a reduction in weight and improvement in visibility of VR goggles. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] Figure 1 This is a schematic diagram showing a schematic configuration of a display system according to one embodiment of the present invention.
[0035] Figure 2 It is shown Figure 1 A schematic cross-sectional view showing an example of details of a lens unit of the display system shown.
[0036] Figure 3 This is a schematic perspective view showing an example of a multilayer structure included in a reflective polarizing film.
[0037] Figure 4 This is a diagram for explaining the method of measuring the ISC value.
[0038] Explanation of symbols
[0039] 2 Display system
[0040] 4 Lens section
[0041] 12 Display components
[0042] 14 Reflective polarizing element
[0043] 16. First lens unit
[0044] 18 Half Mirror
[0045] 20 first phase difference member
[0046] 22. Second phase difference member
[0047] 24 Second lens unit
[0048] 28 Absorption type polarization element
[0049] 30 third phase difference member
[0050] 31 First protection member
[0051] 32. Second protective member
[0052] 41 Adhesive layer
[0053] 42 Adhesive layer
[0054] 43 Adhesive layer
[0055] 44 Adhesive layer
[0056] 45 Adhesive layer
[0057] 46 Adhesive layer
[0058] 100 First lamination section
[0059] 200 Second lamination section DETAILED DESCRIPTION
[0060] Hereinafter, the embodiments of the present invention will be described with reference to the accompanying drawings, but the present invention is not limited to these embodiments. In addition, in order to explain more clearly, the accompanying drawings sometimes schematically show the width, thickness, shape, etc. of each part compared with the embodiments, but this is only an example and does not limit the interpretation of the present invention.
[0061] (Definition of Terms and Symbols)
[0062] The definitions of terms and symbols in this specification are as follows.
[0063] (1) Refractive index (nx, ny, nz)
[0064] "nx" is the refractive index in the direction where the refractive index in the plane reaches the maximum (ie, the slow axis direction), "ny" is the refractive index in the direction orthogonal to the slow axis in the plane (ie, the fast axis direction), and "nz" is the refractive index in the thickness direction.
[0065] (2) In-plane phase difference (Re)
[0066] "Re(λ)" is the in-plane phase difference measured at 23°C with light of wavelength λnm. For example, "Re(550)" is the in-plane phase difference measured at 23°C with light of wavelength 550nm. When the thickness of the layer (film) is d(nm), Re(λ) can be calculated by the formula: Re(λ) = (nx-ny)×d.
[0067] (3) Retardation in the thickness direction (Rth)
[0068] "Rth(λ)" is the phase difference in the thickness direction measured at 23°C with light of wavelength λnm. For example, "Rth(550)" is the phase difference in the thickness direction measured at 23°C with light of wavelength 550nm. When the thickness of the layer (film) is d(nm), Rth(λ) can be calculated by the formula: Rth(λ) = (nx-nz)×d.
[0069] (4) Nz coefficient
[0070] The Nz coefficient can be calculated by Nz=Rth / Re.
[0071] (5) Angle
[0072] In this specification, when an angle is mentioned, the angle includes both clockwise and counterclockwise angles relative to a reference direction. Therefore, for example, "45°" means ±45°.
[0073] Figure 1 Schematic diagram showing a simplified structure of a display system according to an embodiment of the present invention. Figure 1, the configuration and shape of each component of the display system 2 are schematically shown. The display system 2 includes a display element 12, a reflective polarization member 14, a first lens unit 16, a half mirror 18, a first phase difference member 20, a second phase difference member 22, and a second lens unit 24. The reflective polarization member 14 is arranged on the display surface 12a side of the display element 12, that is, in front, and can reflect the light emitted from the display element 12. The first lens unit 16 is arranged on the optical path between the display element 12 and the reflective polarization member 14, and the half mirror 18 is arranged between the display element 12 and the first lens unit 16. The first phase difference member 20 is arranged on the optical path between the display element 12 and the half mirror 18, and the second phase difference member 22 is arranged on the optical path between the half mirror 18 and the reflective polarization member 14.
[0074] Components arranged in front of the half mirror (in the illustrated example, the half mirror 18 , the first lens unit 16 , the second phase difference element 22 , the reflective polarization element 14 , and the second lens unit 24 ) are sometimes collectively referred to as a lens unit (lens unit 4 ).
[0075] The display element 12 is, for example, a liquid crystal display or an organic EL display, and has a display surface 12a for displaying images. Light emitted from the display surface 12a passes through a polarizing member (typically a polarizing film) that may be included in the display element 12 and then emitted as first linearly polarized light.
[0076] The first phase difference member 20 includes a first λ / 4 member capable of converting the first linear polarization light incident on the first phase difference member 20 into a first circular polarization light. When the first phase difference member does not include a member other than the first λ / 4 member, the first phase difference member may be equivalent to the first λ / 4 member. The first phase difference member 20 may be integrally provided on the display element 12.
[0077] The half mirror 18 transmits the light emitted from the display element 12 and reflects the light reflected by the reflective polarization member 14 toward the reflective polarization member 14. The half mirror 18 is integrally provided with the first lens portion 16.
[0078] The second phase difference member 22 includes a second λ / 4 member that allows the light reflected by the reflective polarization member 14 and the half mirror 18 to pass through the reflective polarization member 14. When the second phase difference member does not include a member other than the second λ / 4 member, the second phase difference member may be equivalent to the second λ / 4 member. The second phase difference member 22 may be integrally provided on the first lens portion 16.
[0079] The first circularly polarized light emitted from the first λ / 4 member included in the first phase difference member 20 passes through the half mirror 18 and the first lens unit 16, and is converted into the second linearly polarized light by the second λ / 4 member included in the second phase difference member 22. The second linearly polarized light emitted from the second λ / 4 member does not pass through the reflective polarization member 14, but is reflected toward the half mirror 18. At this time, the polarization direction of the second linearly polarized light incident on the reflective polarization member 14 is the same direction as the reflection axis of the reflective polarization member 14. Therefore, the second linearly polarized light incident on the reflective polarization member 14 is reflected by the reflective polarization member 14.
[0080] The second linear polarized light reflected by the reflective polarization member 14 is converted into the second circular polarized light by the second λ / 4 member included in the second phase difference member 22, and the second circular polarized light emitted from the second λ / 4 member passes through the first lens unit 16 and is reflected by the half mirror 18. The second circular polarized light reflected by the half mirror 18 passes through the first lens unit 16 and is converted into the third linear polarized light by the second λ / 4 member included in the second phase difference member 22. The third linear polarized light is transmitted through the reflective polarization member 14. At this time, the polarization direction of the third linear polarized light incident on the reflective polarization member 14 is the same direction as the transmission axis of the reflective polarization member 14. Therefore, the third linear polarized light incident on the reflective polarization member 14 is transmitted through the reflective polarization member 14.
[0081] The light transmitted through the reflective polarization element 14 passes through the second lens portion 24 and enters the eye 26 of the user.
[0082] For example, the absorption axis of the polarization component included in the display element 12 and the reflection axis of the reflective polarization component 14 can be arranged approximately parallel to each other, or can be arranged approximately orthogonal to each other. The angle formed by the absorption axis of the polarization component included in the display element 12 and the slow axis of the 1st λ / 4 component included in the first phase difference component 20 is, for example, 40° to 50°, 42° to 48°, or approximately 45°. The angle formed by the absorption axis of the polarization component included in the display element 12 and the slow axis of the 2nd λ / 4 component included in the second phase difference component 22 is, for example, 40° to 50°, 42° to 48°, or approximately 45°.
[0083] The in-plane phase difference Re(550) of the first λ / 4 component is, for example, 100 nm to 190 nm, 110 nm to 180 nm, 130 nm to 160 nm, or 135 nm to 155 nm. The first λ / 4 component preferably exhibits an inverse dispersion wavelength characteristic in which the phase difference value increases in accordance with the wavelength of the measurement light. The Re(450) / Re(550) of the first λ / 4 component is, for example, not less than 0.75 and less than 1, or not less than 0.8 and not more than 0.95.
[0084] The in-plane phase difference Re(550) of the second λ / 4 component is, for example, 100 nm to 190 nm, 110 nm to 180 nm, 130 nm to 160 nm, or 135 nm to 155 nm. The second λ / 4 component preferably exhibits an inverse dispersion wavelength characteristic in which the phase difference value increases with the wavelength of the measurement light. The Re(450) / Re(550) of the second λ / 4 component is, for example, not less than 0.75 and less than 1, or not less than 0.8 and not more than 0.95.
[0085] In the lens portion 4, a space can be formed between the first lens portion 16 and the second lens portion 24. In this case, the component arranged between the first lens portion 16 and the second lens portion 24 is preferably provided integrally in any one of the first lens portion 16 and the second lens portion 24. For example, the component arranged between the first lens portion 16 and the second lens portion 24 is preferably integrated with any one of the first lens portion 16 and the second lens portion 24 via an adhesive layer. According to such a method, for example, the handling properties of each component can be excellent. The adhesive layer can be formed by an adhesive or an adhesive. Specifically, the adhesive layer can be an adhesive layer or an adhesive layer. The thickness of the adhesive layer is, for example, 0.05μm to 30μm.
[0086] Figure 2 It is shown Figure 1 Schematic cross-sectional view of an example of the details of the lens unit of the display system shown. Specifically, Figure 2 The first lens portion, the second lens portion, and a member disposed therebetween are shown. The lens portion 4 includes: a first lens portion 16, a first laminated portion 100 disposed adjacent to the first lens portion 16, a second lens portion 24, and a second laminated portion 200 disposed adjacent to the second lens portion 24. Figure 2 In the example shown, the first stacked portion 100 and the second stacked portion 200 are arranged separately. Although not shown, a half mirror may be provided integrally with the first lens portion 16 .
[0087] In the lens portion 4, the ISC value of the first laminated portion 100 and the second laminated portion 200 is less than 100, preferably less than 90, more preferably less than 80, and further preferably less than 70. By satisfying such an ISC value, a display system with excellent visual recognition can be achieved. Specifically, by satisfying such an ISC value, the generation of full-reflection light can be suppressed in the lens portion, thereby suppressing the image from becoming unclear. The ISC value can be an indicator of smoothness or unevenness. The lower limit of the ISC value of the first laminated portion 100 and the second laminated portion 200 is substantially about 5.
[0088] The first laminated part 100 includes a second phase difference member 22, and an adhesive layer 41 disposed between the first lens portion 16 and the second phase difference member 22, and is integrally provided on the first lens portion 16 through the adhesive layer 41. The first laminated part 100 further includes a first protective member 31 disposed in front of the second phase difference member 22. The first protective member 31 is laminated on the second phase difference member 22 via the adhesive layer 42. The first protective member 31 may be located on the outermost surface of the first laminated part 100.
[0089] exist Figure 2 In the example shown, the second phase difference member 22 includes, in addition to the second λ / 4 member 22a, a member (so-called positive C plate) 22b whose refractive index characteristic can show the relationship of nz>nx=ny. The second phase difference member 22 has a stacked structure of the second λ / 4 member 22a and the positive C plate 22b. Figure 2 As shown, in the second phase difference member 22, the second λ / 4 member 22a is preferably located in front of the positive C plate 22b. The second λ / 4 member 22a and the positive C plate 22b can be laminated via an adhesive layer (not shown), for example.
[0090] The refractive index characteristics of the second λ / 4 component preferably show a relationship of nx>ny≥nz. Here, "ny=nz" includes not only the case where ny and nz are completely equal, but also the case where they are substantially equal. Therefore, within the range that does not impair the effect of the present invention, ny<nz may sometimes be satisfied. The Nz coefficient of the second λ / 4 component is preferably 0.9 to 3, more preferably 0.9 to 2.5, further preferably 0.9 to 1.5, and particularly preferably 0.9 to 1.3.
[0091] The second λ / 4 member is formed of any appropriate material that can satisfy the above-mentioned characteristics. The second λ / 4 member may be, for example, a stretched film of a resin film or an alignment fixing layer of a liquid crystal compound.
[0092] As the resin contained in the above-mentioned resin film, there can be mentioned: polycarbonate resin, polyester carbonate resin, polyester resin, polyvinyl acetal resin, polyarylate resin, cyclic olefin resin, cellulose resin, polyvinyl alcohol resin, polyamide resin, polyimide resin, polyether resin, polystyrene resin, acrylic resin, etc. These resins can be used alone or in combination. As a method of combination, for example, blending and copolymerization can be mentioned. In the case where the second λ / 4 component shows a reverse dispersion wavelength characteristic, a resin film containing a polycarbonate resin or a polyester carbonate resin (hereinafter, sometimes referred to as a polycarbonate resin) can be suitably used.
[0093] As the above-mentioned polycarbonate resin, any appropriate polycarbonate resin can be used. For example, the polycarbonate resin contains structural units derived from fluorene dihydroxy compounds, structural units derived from isosorbide dihydroxy compounds, and structural units derived from at least one dihydroxy compound selected from alicyclic diols, alicyclic dimethanols, di, tri or polyethylene glycols and alkylene glycols or spirodiols. Preferably, the polycarbonate resin contains structural units derived from fluorene dihydroxy compounds, structural units derived from isosorbide dihydroxy compounds, structural units derived from alicyclic dimethanols and / or structural units derived from di, tri or polyethylene glycols; more preferably, it contains structural units derived from fluorene dihydroxy compounds, structural units derived from isosorbide dihydroxy compounds, and structural units derived from di, tri or polyethylene glycols. The polycarbonate resin may also contain structural units derived from other dihydroxy compounds as needed. It should be noted that details of the polycarbonate resin that can be suitably used for the second λ / 4 component and the method for forming the second λ / 4 component are recorded in, for example, Japanese Patent Gazette No. 2014-10291, Japanese Patent Gazette No. 2014-26266, Japanese Patent Gazette No. 2015-212816, Japanese Patent Gazette No. 2015-212817, and Japanese Patent Gazette No. 2015-212818, and the records in these gazettes are cited as references in this specification.
[0094] The thickness of the second λ / 4 member formed of a stretched film of a resin film is, for example, 10 μm to 100 μm, preferably 10 μm to 70 μm, and more preferably 20 μm to 60 μm.
[0095] The orientation fixing layer of the above-mentioned liquid crystal compound is a layer in which the liquid crystal compound is oriented along a given direction within the layer and its orientation state is fixed. It should be noted that the "orientation fixing layer" is a concept that includes an orientation solidification layer obtained by solidifying a liquid crystal monomer as described later. In the 2ndλ / 4 component, representatively, the rod-shaped liquid crystal compound is oriented in a state arranged along the slow axis direction of the 2ndλ / 4 component (parallel orientation (homogeneous alignment)). As rod-shaped liquid crystal compounds, for example, liquid crystal polymers and liquid crystal monomers can be cited. The liquid crystal compound is preferably capable of polymerization. If the liquid crystal compound is capable of polymerization, the orientation state of the liquid crystal compound can be fixed by polymerizing after orienting the liquid crystal compound.
[0096] The orientation fixing layer (liquid crystal orientation fixing layer) of the above-mentioned liquid crystal compound can be formed by the following method: an orientation treatment is applied to the surface of a given substrate, a coating liquid containing a liquid crystal compound is applied to the surface, and the liquid crystal compound is oriented along the direction corresponding to the above-mentioned orientation treatment to fix the orientation state. As an orientation treatment, any appropriate orientation treatment can be adopted. Specifically, mechanical orientation treatment, physical orientation treatment, and chemical orientation treatment can be cited. As specific examples of mechanical orientation treatment, friction treatment and stretching treatment can be cited. As specific examples of physical orientation treatment, magnetic field orientation treatment and electric field orientation treatment can be cited. As specific examples of chemical orientation treatment, inclined evaporation method and optical orientation treatment can be cited. The processing conditions of various orientation treatments can adopt any appropriate conditions according to the purpose.
[0097] The liquid crystal compound can be aligned by treating it at a temperature corresponding to the type of the liquid crystal compound at which it exhibits a liquid crystal phase. By such a temperature treatment, the liquid crystal compound is in a liquid crystal state and is aligned in the alignment treatment direction of the substrate surface.
[0098] In one embodiment, the alignment state is fixed by cooling the aligned liquid crystal compound as described above. When the liquid crystal compound is polymerizable or crosslinkable, the alignment state can be fixed by subjecting the aligned liquid crystal compound to polymerization or crosslinking treatment as described above.
[0099] As the above-mentioned liquid crystal compound, any appropriate liquid crystal polymer and / or liquid crystal monomer can be used. Liquid crystal polymer and liquid crystal monomer can be used alone or in combination. Specific examples of liquid crystal compounds and methods for making liquid crystal orientation fixing layers are described in, for example, Japanese Patent Publication No. 2006-163343, Japanese Patent Publication No. 2006-178389, and International Publication No. 2018 / 123551. The records of these publications are cited as references in this specification.
[0100] The thickness of the second λ / 4 member composed of the liquid crystal alignment solid layer is, for example, 1 μm to 10 μm, preferably 1 μm to 8 μm, more preferably 1 μm to 6 μm, and further preferably 1 μm to 4 μm.
[0101] The thickness direction phase difference Rth(550) of the positive C plate is preferably -50nm to -300nm, more preferably -70nm to -250nm, further preferably -90nm to -200nm, and particularly preferably -100nm to -180nm. Here, "nx=ny" includes not only the case where nx and ny are strictly equal, but also the case where nx and ny are substantially equal. The in-plane phase difference Re(550) of the positive C plate is, for example, less than 10nm.
[0102] The positive C plate can be formed of any appropriate material, but the positive C plate is preferably composed of a film containing a liquid crystal material fixed in a homeotropic orientation. The liquid crystal material (liquid crystal compound) capable of homeotropic orientation can be a liquid crystal monomer or a liquid crystal polymer. As a specific example of such a liquid crystal compound and a method for forming a positive C plate, there can be cited the liquid crystal compound and the method for forming the phase difference layer described in
[0020] to
[0028] of Japanese Patent Gazette No. 2002-333642. In this case, the thickness of the positive C plate is preferably 0.5 μm to 5 μm.
[0103] Typically, the first protective member includes a substrate. The thickness of the substrate is preferably 5 μm to 80 μm, more preferably 10 μm to 50 μm, and further preferably 15 μm to 40 μm. The substrate can be composed of any appropriate film. As the material of the main component of the film constituting the substrate, for example, cellulose resins such as triacetyl cellulose (TAC), polyesters, polyvinyl alcohols, polycarbonates, polyamides, polyimides, polyether sulfones, polysulfones, polystyrenes, cycloolefins such as polynorbornene, polyolefins, (meth) acrylic acid, acetates, etc. can be cited. Here, (meth) acrylic acid refers to acrylic acid and / or methacrylic acid. In one embodiment, the substrate is preferably formed by a (meth) acrylic resin. By adopting a (meth) acrylic resin, film formation of a substrate with excellent smoothness can be achieved by extrusion molding. And a protective member with excellent smoothness can be obtained.
[0104] The first protective member preferably has a substrate and a surface treatment layer formed on the substrate. The first protective member having a surface treatment layer can be configured so that the surface treatment layer is located on the front side. Specifically, the surface treatment layer can be located on the outermost surface of the first laminated portion. The surface treatment layer can have any appropriate function. For example, from the perspective of improving visual recognition, the surface treatment layer preferably has an anti-reflection function. The thickness of the surface treatment layer is preferably 0.5μm to 10μm, more preferably 1μm to 7μm, and further preferably 2μm to 5μm.
[0105] The second stacking section 200 includes a reflective polarizing member 14 and an adhesive layer disposed between the reflective polarizing member 14 and the second lens portion 24. From the viewpoint of improving visual recognition, the second stacking section 200 further includes, for example, an absorptive polarizing member 28 disposed between the reflective polarizing member 14 and the second lens portion 24. The absorptive polarizing member 28 is stacked in front of the reflective polarizing member 14 via an adhesive layer 44. The reflection axis of the reflective polarizing member 14 and the absorption axis of the absorptive polarizing member 28 can be arranged substantially parallel to each other, and the transmission axis of the reflective polarizing member 14 and the transmission axis of the absorptive polarizing member 28 can be arranged substantially parallel to each other. By stacking via an adhesive layer, the reflective polarizing member 14 and the absorptive polarizing member 28 can be fixed, thereby preventing the displacement of the axis configuration of the reflection axis and the absorption axis (transmission axis and transmission axis). In addition, it is possible to suppress the adverse effects caused by the air layer that may be formed between the reflective polarizing member 14 and the absorptive polarizing member 28.
[0106] The second laminated part 200 further includes a second protective member 32 disposed behind the reflective polarizing member 14. The second protective member 32 is laminated on the reflective polarizing member 14 via an adhesive layer 43. The second protective member 32 can be located on the outermost surface of the second laminated part 200. The second protective member, like the first protective member, can include a substrate. In addition, the second protective member preferably has a substrate and a surface treatment layer formed on the substrate. In this case, the surface treatment layer can be located on the outermost surface of the second laminated part. Regarding the details of the substrate and the surface treatment layer, the same description as the first protective member can be applied.
[0107] like Figure 2As shown, the second stacked section 200 may further include a third phase difference member 30 disposed between the absorption type polarization member 28 and the second lens section 24. The third phase difference member 30 is stacked on the absorption type polarization member 28 via an adhesive layer 45. In addition, the third phase difference member 30 is stacked on the second lens section 24 via an adhesive layer 46, and the second stacked section 200 is integrally provided on the second lens section 24. The third phase difference member 30 includes, for example, a 3rd λ / 4 member. The angle formed by the absorption axis of the absorption type polarization member 28 and the slow axis of the 3rd λ / 4 member included in the third phase difference member 30 is, for example, 40° to 50°, may be 42° to 48°, or may be approximately 45°. By providing such a member, it is possible to prevent, for example, reflection of external light from the second lens section 16 side. In the case where the third phase difference member does not include a member other than the 3rd λ / 4 member, the third phase difference member may be equivalent to the 3rd λ / 4 member.
[0108] The above-mentioned reflective polarizing component can transmit polarized light (representatively linear polarized light) parallel to its transmission axis while maintaining its polarization state, and reflect light of other polarization states. As a reflective polarizing component, it is typically composed of a film with a multilayer structure (sometimes referred to as a reflective polarizing film). In this case, the thickness of the reflective polarizing component is, for example, 10 μm to 150 μm, preferably 20 μm to 100 μm, and more preferably 30 μm to 60 μm.
[0109] Figure 3 14 is a schematic stereoscopic diagram showing an example of a multilayer structure included in a reflective polarizing film. The multilayer structure 14a alternately comprises a layer A having birefringence and a layer B having substantially no birefringence. The total number of layers constituting the multilayer structure may be 50 to 1000. For example, the refractive index nx of the A layer in the x-axis direction is greater than the refractive index ny in the y-axis direction, the refractive index nx of the B layer in the x-axis direction is substantially the same as the refractive index ny in the y-axis direction, and the refractive index difference between the A layer and the B layer is large in the x-axis direction and substantially zero in the y-axis direction. As a result, the x-axis direction can be made a reflection axis and the y-axis direction can be made a transmission axis. The refractive index difference between the A layer and the B layer in the x-axis direction is preferably 0.2 to 0.3.
[0110] The above-mentioned A layer is typically formed of a material that exhibits birefringence by stretching. Examples of such materials include naphthalene dicarboxylic acid polyesters (e.g., polyethylene naphthalate), polycarbonates, and acrylic resins (e.g., polymethyl methacrylate). The above-mentioned B layer is typically formed of a material that does not substantially exhibit birefringence even when stretched. Examples of such materials include copolyesters of naphthalene dicarboxylic acid and terephthalic acid. The above-mentioned multilayer structure can be formed by combining coextrusion with stretching. For example, after the material constituting the A layer and the material constituting the B layer are extruded, they are multilayered (e.g., using a multiplier). Then, the obtained multilayer laminate is stretched. The x-axis direction of the illustrated example can correspond to the stretching direction.
[0111] Examples of commercially available reflective polarizing films include "DBEF" and "APF" manufactured by 3M Co., Ltd. and "APCF" manufactured by Nitto Denko Corporation.
[0112] The orthogonal transmittance (Tc) of the reflective polarizing component (reflective polarizing film) can be, for example, 0.01% to 3%. The single transmittance (Ts) of the reflective polarizing component (reflective polarizing film) can be, for example, 43% to 49%, preferably 45% to 47%. The polarization degree (P) of the reflective polarizing component (reflective polarizing film) can be, for example, 92% to 99.99%.
[0113] The above-mentioned orthogonal transmittance, single transmittance and polarization degree can be measured, for example, using an ultraviolet visible spectrophotometer. The polarization degree P can be measured using an ultraviolet visible spectrophotometer for single transmittance Ts, parallel transmittance Tp and orthogonal transmittance Tc, and can be obtained by the following formula based on the obtained Tp and Tc. It should be noted that Ts, Tp and Tc are Y values obtained by measuring with a 2-degree field of view (C light source) of JIS Z8701 and correcting for visibility.
[0114] Polarization degree P (%) = {(Tp-Tc) / (Tp+Tc)} 1 / 2 ×100
[0115] The absorption-type polarizing member may typically include a resin film containing a dichroic substance (sometimes referred to as an absorption-type polarizing film). The thickness of the absorption-type polarizing film is, for example, 1 μm to 20 μm, 2 μm to 15 μm, 12 μm to 10 μm, 8 μm to 8 μm, or 5 μm to 5 μm.
[0116] The absorption-type polarizing film may be produced by a single-layer resin film or by using a laminate of two or more layers.
[0117] In the case of a single-layer resin film, for example, a hydrophilic polymer film such as a polyvinyl alcohol (PVA) film, a partially formalized PVA film, or a partially saponified ethylene-vinyl acetate copolymer film can be subjected to dyeing treatment using a dichroic substance such as iodine or a dichroic dye, stretching treatment, etc., thereby obtaining an absorption-type polarizing film. Among them, an absorption-type polarizing film obtained by dyeing a PVA film with iodine and uniaxially stretching the film is preferred.
[0118] The dyeing using iodine can be performed by, for example, immersing the PVA film in an iodine aqueous solution. The stretching ratio of the uniaxial stretching is preferably 3 to 7 times. The stretching can be performed after the dyeing treatment or while dyeing. In addition, the dyeing can also be performed after the stretching. The PVA film can be subjected to swelling treatment, cross-linking treatment, cleaning treatment, drying treatment, etc. as needed.
[0119] As a laminate made using the above-mentioned two or more layers, there can be cited a laminate of a resin substrate and a PVA-type resin layer (PVA-type resin film) laminated on the resin substrate, or a laminate of a resin substrate and a PVA-type resin layer formed by coating on the resin substrate. The absorption-type polarizing film obtained by using a laminate of a resin substrate and a PVA-type resin layer formed by coating on the resin substrate can be made by the following method: for example, a PVA-type resin solution is applied to a resin substrate, dried to form a PVA-type resin layer on the resin substrate, and a laminate of a resin substrate and a PVA-type resin layer is obtained; the laminate is stretched and dyed to make the PVA-type resin layer into an absorption-type polarizing film. In this embodiment, it is preferred to form a polyvinyl alcohol-type resin layer containing a halide and a polyvinyl alcohol-type resin on one side of the resin substrate. Stretching typically includes immersing the laminate in a boric acid aqueous solution for stretching. In addition, stretching can further include stretching the laminate in a gas atmosphere at a high temperature (for example, above 95°C) before stretching in a boric acid aqueous solution as needed. In addition, in the present embodiment, it is preferred that the laminate is subjected to a drying shrinkage treatment in which the laminate shrinks by more than 2% in the width direction by heating while being conveyed in the length direction. Representatively, the manufacturing method of the present embodiment includes sequentially performing an auxiliary stretching treatment in a gas atmosphere, a dyeing treatment, a stretching treatment in an aqueous solution, and a drying shrinkage treatment on the laminate. By introducing auxiliary stretching, the crystallinity of the PVA can be improved even when the PVA is coated on the thermoplastic resin, and high optical properties can be achieved. In addition, by simultaneously improving the orientation of the PVA in advance, it is possible to prevent problems such as the reduction of the orientation and dissolution of the PVA when immersed in water in the subsequent dyeing process and the stretching process, and high optical properties can be achieved. In addition, when the PVA-type resin layer is immersed in a liquid, the orientation disorder of the polyvinyl alcohol molecules and the reduction of the orientation can be suppressed compared to the case where the PVA-type resin layer does not contain a halide. Thus, the optical properties of the absorption-type polarizing film obtained by the treatment process of immersing the laminate in a liquid such as a dyeing treatment and a stretching treatment in an aqueous solution can be improved. Further, the laminate is shrunk in the width direction by drying and shrinking treatment, thereby improving the optical properties. The obtained laminate of resin substrate / absorption type polarizing film can be used directly (that is, the resin substrate can be used as a protective layer of absorption type polarizing film), or the resin substrate can be peeled off from the laminate of resin substrate / absorption type polarizing film, and any appropriate protective layer corresponding to the purpose can be stacked on the peeling surface or on the side opposite to the peeling surface. The details of the manufacturing method of such an absorption type polarizing film are recorded in, for example, Japanese Patent Publication No. 2012-73580 and Japanese Patent No. 6470455. The records of these publications as a whole are cited in this specification as a reference.
[0120] The orthogonal transmittance (Tc) of the absorption type polarization component (absorption type polarizing film) is preferably 0.5% or less, more preferably 0.1% or less, and further preferably 0.05% or less. The single transmittance (Ts) of the absorption type polarization component (absorption type polarizing film) is, for example, 41.0% to 45.0%, and preferably 42.0% or more. The polarization degree (P) of the absorption type polarization component (absorption type polarizing film) is, for example, 99.0% to 99.997%, and preferably 99.9% or more.
[0121] The in-plane phase difference Re(550) of the above-mentioned third λ / 4 component is, for example, 100nm to 190nm, 110nm to 180nm, 130nm to 160nm, or 135nm to 155nm. The third λ / 4 component preferably shows an inverse dispersion wavelength characteristic in which the phase difference value increases corresponding to the wavelength of the measured light. The Re(450) / Re(550) of the third λ / 4 component is, for example, greater than 0.75 and less than 1, or greater than 0.8 and less than 0.95. The refractive index characteristics of the third λ / 4 component preferably show the relationship of nx>ny≥nz. The Nz coefficient of the third λ / 4 component is preferably 0.9 to 3, more preferably 0.9 to 2.5, further preferably 0.9 to 1.5, and particularly preferably 0.9 to 1.3.
[0122] The 3rd λ / 4 member is formed of any appropriate material that can satisfy the above-mentioned characteristics. The 3rd λ / 4 member can be, for example, a stretched film of a resin film or an orientation-fixed layer of a liquid crystal compound. The same description as that of the above-mentioned 2nd λ / 4 member can be applied to the 3rd λ / 4 member composed of a stretched film of a resin film or an orientation-fixed layer of a liquid crystal compound. The 2nd λ / 4 member and the 3rd λ / 4 member can be members of the same composition (for example, forming material, thickness, optical characteristics, etc.) or members of different compositions.
[0123] exist Figure 2 In the example shown, each member disposed between the first lens portion 16 and the second lens portion 24 is integrally provided on the first lens portion 16 or the second lens portion 24, and six adhesive layers 41 to 46 are used. Figure 2In the example shown, the total of the adhesive layers included in the first laminated part 100 and the adhesive layers included in the second laminated part 200 is 6 layers. For example, the number of adhesive layers varies depending on the number of components arranged between the first lens portion 16 and the second lens portion 24. The total of the adhesive layers included in the first laminated part and the adhesive layers included in the above-mentioned second laminated part is, for example, more than 3 layers, more than 4 layers, more than 5 layers, or more than 6 layers. The more the number of adhesive layers arranged between the first lens portion 16 and the second lens portion 24 increases, the more likely the smoothness of the laminated part will decrease. However, by making the lens portion as a whole have the above-mentioned ISC value, excellent visual recognition can be achieved.
[0124] The thickness of the laminated adhesive layer used for each of the above-mentioned components can be set to any appropriate thickness. The thickness of each laminated adhesive layer used for each of the above-mentioned components is preferably less than 20 μm, less than 15 μm, less than 10 μm, or less than 7 μm. According to such a thickness, the degree of concavity and convexity on the surface of the adhesive layer can be suppressed, and the ISC value of the entire lens portion can be well achieved. On the other hand, the thickness of the adhesive layer is, for example, more than 3 μm.
[0125] The surface roughness Ra of each adhesive layer used for laminating the above-mentioned components is preferably 20 nm or less, and more preferably 15 nm or less. With such a surface roughness Ra, a good ISC value of the entire lens unit can be achieved.
[0126] The adhesive layer can be composed of any appropriate adhesive. As specific examples, acrylic adhesives, rubber adhesives, silicone adhesives, polyester adhesives, urethane adhesives, epoxy adhesives, and polyether adhesives can be cited. By adjusting the type, quantity, combination and ratio of the monomers of the base resin forming the adhesive, as well as the amount of the cross-linking agent, the reaction temperature, the reaction time, etc., it is possible to prepare an adhesive with the desired characteristics corresponding to the purpose. The base resin of the adhesive can be used alone or in combination of two or more. As the base resin, an acrylic resin can be preferably used. Specifically, the adhesive layer is preferably formed by an acrylic adhesive.
[0127] For example, the adhesive layer can be formed by applying an adhesive composition comprising a base resin, an additive such as a crosslinking agent, and a solvent and drying the adhesive composition. The adhesive composition can be directly applied to the adherend or applied to a substrate such as a separately prepared base film. Typically, drying is performed by heating.
[0128] For example, the surface roughness Ra can be satisfied by adjusting the film thickness of the adhesive composition coating film. If the film thickness is too thick, liquid flow may occur in the coating film due to temperature difference due to heating, resulting in a adhesive layer with a large degree of surface unevenness.
[0129] In addition, for example, by controlling the drying conditions of the coating film of the adhesive composition, the above-mentioned surface roughness Ra can be satisfied. Specifically, the above-mentioned surface roughness Ra can be satisfied by adjusting the air volume and wind speed of the wind blown to the coating film during drying. If the air volume and wind speed of the wind blown to the coating film are too large, undulations will occur in the coating film, and an adhesive layer with a large degree of surface unevenness will be obtained. In one embodiment, the coating film is preferably dried in a temperature environment of 65°C to 110°C with the wind speed adjusted to a range of 2m / min to 15m / min, and more preferably adjusted to 2m / min to 8m / min for drying. For example, it is preferred to adjust to such a temperature and wind speed near the entrance of the drying oven after coating. Specifically, such a temperature and wind speed can be adjusted from the entrance of the oven to the central part of the oven.
[0130] The adhesive layers for laminating the above-mentioned components are preferably composed of a single layer. For example, each adhesive layer preferably does not have a multilayer structure formed by applying the adhesive composition more than twice. By making the adhesive layer composed of a single layer, it is possible to meet, for example, the above-mentioned surface roughness Ra.
[0131] Example
[0132] The present invention will be described in detail below with reference to examples, but the present invention is not limited to these examples. It should be noted that the thickness, surface roughness Ra and phase difference value are values measured by the following measurement methods.
[0133] <Thickness>
[0134] The thickness of 10 μm or less was measured using a scanning electron microscope (manufactured by JEOL Ltd., product name “JSM-7100F”). The thickness exceeding 10 μm was measured using a digital micrometer (manufactured by Anritsu Co., Ltd., product name “KC-351C”).
[0135] <Surface roughness Ra>
[0136] The arithmetic mean surface roughness Ra (μm) was measured in accordance with JIS B 0601 (1994 edition).
[0137] The adhesive layer of the measurement object was pasted on a glass plate (manufactured by MATSUNAMI, MICRO SLIDE GLASS, product number S, thickness 1.3mm, 45mm×50mm) to prepare a measurement sample. The pasting of the adhesive layer was performed by transferring the adhesive layer formed on the substrate film from the substrate film to the glass plate. The obtained measurement sample was measured using a scanning white light interferometer (manufactured by Zygo, product name "Newview7300"). Specifically, the measurement sample was placed on a measurement table with an anti-vibration table, and interference fringes were generated using a single white LED illumination. An interference objective lens (2.5 times) with a reference plane was scanned along the Z direction (thickness direction), thereby selectively obtaining the smoothness (surface smoothness) of the outermost surface of the adhesive layer within a field of view of 2mm□. Based on this measurement, the arithmetic mean surface roughness Ra was calculated.
[0138] <Phase difference value>
[0139] The phase difference value at each wavelength at 23° C. was measured using a Mueller matrix polarimeter (manufactured by Axometrics, product name “Axoscan”).
[0140] [Example 1]
[0141] (Formation of Adhesive Layer)
[0142] A monomer mixture containing 92 parts by weight of butyl acrylate, 2.9 parts by weight of acrylic acid, 0.1 parts by weight of 2-hydroxyethyl acrylate, and 5 parts by weight of N-acryloylmorpholine was added to a four-necked flask equipped with a stirring blade, a thermometer, a nitrogen inlet tube, and a condenser. Furthermore, 0.1 parts by weight of 2,2'-azobisisobutyronitrile as a polymerization initiator was added together with 200 parts by weight of ethyl acetate to 100 parts by weight of the monomer mixture, and nitrogen was introduced while slowly stirring to replace the flask with nitrogen. The liquid temperature in the flask was maintained at about 55°C for 8 hours for polymerization reaction, and a solution of an acrylic polymer with a weight average molecular weight (Mw) of 1.78 million was prepared.
[0143] The acrylic polymer solution was applied to the substrate film, and the coating film on the substrate film was dried in an oven to form an adhesive layer with a thickness of 5 μm and a surface roughness Ra of 12 nm. It should be noted that the wind speed in the oven was adjusted from the oven entrance to the center of the oven within a range of 15 m / min or less to perform drying. It should be noted that the wind speed was measured by an anemometer installed in the oven.
[0144] (Fabrication of λ / 4 member)
[0145] The polymerization was carried out using a batch polymerization apparatus consisting of two vertical reactors equipped with stirring blades and a reflux condenser controlled at 100° C. 29.60 parts by mass (0.046 mol) of bis[9-(2-phenoxycarbonylethyl)fluoren-9-yl]methane, 29.21 parts by mass (0.200 mol) of isosorbide (ISB), 42.28 parts by mass (0.139 mol) of spiroglycol (SPG), 63.77 parts by mass (0.298 mol) of diphenyl carbonate (DPC), and 1.19×10-6 parts by mass of calcium acetate monohydrate as a catalyst were added. -2 Mass parts (6.78×10 -5 mol). After the reactor was replaced with nitrogen under reduced pressure, it was heated by a heat medium and stirring was started when the internal temperature reached 100°C. The internal temperature reached 220°C 40 minutes after the start of the temperature rise, and the pressure was reduced while controlling to maintain the temperature, so that it reached 13.3kPa after 90 minutes after reaching 220°C. The phenol vapor produced as a by-product during the polymerization reaction was introduced into a 100°C reflux condenser, so that a certain amount of monomer components contained in the phenol vapor was returned to the reactor, and the uncondensed phenol vapor was introduced into a 45°C condenser for recovery. After nitrogen was introduced into the first reactor to temporarily restore it to atmospheric pressure, the reaction liquid after oligomerization in the first reactor was transferred to the second reactor. Next, the temperature rise and pressure reduction in the second reactor were started, so that it reached an internal temperature of 240°C and a pressure of 0.2kPa after 50 minutes. Then, the polymerization was carried out until the given stirring power was reached. When the predetermined power was reached, nitrogen gas was introduced into the reactor to restore the pressure, and the produced polyester carbonate resin was extruded into water, and the strands were cut to obtain pellets.
[0146] The obtained polyester carbonate resin (pellets) was vacuum dried at 80°C for 5 hours, and then a long strip of resin film with a thickness of 135 μm was produced using a film-making device equipped with a single screw extruder (manufactured by Toshiba Machine Co., Ltd., cylinder setting temperature: 250°C), a T-die (width 200 mm, setting temperature: 250°C), a chill roll (setting temperature: 120-130°C) and a winder. The obtained long strip of resin film was stretched in the width direction at a stretching temperature of 143°C and a stretching ratio of 2.8 times to obtain a stretched film with a thickness of 47 μm. The Re(550) of the obtained stretched film was 143 nm, Re(450) / Re(550) was 0.86, and the Nz coefficient was 1.2.
[0147] (Formation of positive C plate)
[0148] A liquid crystal coating liquid was prepared by dissolving 20 parts by weight of a side chain liquid crystal polymer represented by the following chemical formula (1) (the numbers 65 and 35 in the formula represent the molar % of the monomer unit, and for convenience, the block polymer is represented: the weight average molecular weight is 5000), 80 parts by weight of a polymerizable liquid crystal showing a nematic liquid crystal phase (manufactured by BASF: trade name Paliocolor LC242), and 5 parts by weight of a photopolymerization initiator (manufactured by Chiba Specialty Chemicals: trade name IRGACURE 907) in 200 parts by weight of cyclopentanone. Then, the coating liquid was applied to a PET substrate subjected to a vertical alignment treatment using a wire bar coater, and then heated and dried at 80°C for 4 minutes to align the liquid crystal. The liquid crystal layer was irradiated with ultraviolet rays to cure the liquid crystal layer, thereby forming a positive C plate with a thickness of 4 μm and an Rth (550) of -100 nm on the substrate.
[0149] [Chemical formula 1]
[0150]
[0151] (Production of protective components)
[0152] The following hard coat forming material was applied to an acrylic film (thickness 40 μm) having a lactone ring structure, heated at 90° C. for 1 minute, and irradiated with a high pressure mercury lamp to a cumulative light intensity of 300 mJ / cm 2 The coating layer was cured by ultraviolet rays to produce an acrylic film (thickness 44 μm) having a hard coat layer with a thickness of 4 μm.
[0153] Next, the antireflection layer forming coating liquid A described below was applied onto the hard coating layer using a wire bar, and the applied coating liquid was heated at 80°C for 1 minute to dry to form a coating film. The dried coating film was irradiated with a high pressure mercury lamp at a cumulative light intensity of 300 mJ / cm 2 The coating was cured by ultraviolet light to form an anti-reflection layer A with a thickness of 140 nm.
[0154] Next, the following antireflection layer forming coating liquid B was applied onto the antireflection layer A using a wire bar, and the applied coating liquid was heated at 80° C. for 1 minute to dry to form a coating film. The dried coating film was irradiated with a high pressure mercury lamp at a cumulative light intensity of 300 mJ / cm 2 The coating was cured by ultraviolet light to form an anti-reflection layer B with a thickness of 105 nm.
[0155] In this manner, a protective member (thickness 44 μm) was obtained.
[0156] (Hard coat forming material)
[0157] A urethane acrylate oligomer (“NK Oligo UA-53H” manufactured by Shin-Nakamura Chemical Co., Ltd.), 50 parts of a polyfunctional acrylate having pentaerythritol triacrylate as a main component (“Viscoat#300” manufactured by Osaka Organic Chemical Co., Ltd.), 30 parts of 4-hydroxybutyl acrylate (manufactured by Osaka Organic Chemical Co., Ltd.), 20 parts of leveling agent (“GRANDIC PC4100” manufactured by DIC Corporation), 1 part of a photopolymerization initiator (“IRGACURE907” manufactured by Ciba Japan Co., Ltd.) were mixed and diluted with methyl isobutyl ketone so as to have a solid content concentration of 50%, thereby preparing a hard coat layer forming material.
[0158] (Anti-reflection layer forming coating liquid A)
[0159] 100 parts by weight of a multifunctional acrylate (manufactured by Arakawa Chemical Industries, Ltd., trade name "OPSTAR KZ6728", solid content 20% by weight), 3 parts by weight of a leveling agent (manufactured by DIC Corporation, "GRANDIC PC4100"), and 3 parts by weight of a photopolymerization initiator (manufactured by BASF Corporation, trade name "OMNIRAD907", solid content 100% by weight) were mixed. The mixture was stirred using butyl acetate as a diluent so that the solid content became 12% by weight, thereby preparing a coating liquid A for forming an antireflection layer.
[0160] (Anti-reflection layer forming coating liquid B)
[0161] 100 parts by weight of a multifunctional acrylate containing pentaerythritol triacrylate as the main component (manufactured by Osaka Organic Chemical Industry Co., Ltd., trade name "Viscoat #300", solid content 100% by weight), 150 parts by weight of hollow nano-silica particles (manufactured by JGC Catalysts & Chemicals Co., Ltd., trade name "THRULYA 5320", solid content 20% by weight, weight average particle size 75 nm), 50 parts by weight of solid nano-silica particles (manufactured by Nissan Chemical Industries, Ltd., trade name "MEK-2140Z-AC", solid content 30% by weight, weight average particle size 10 nm), 12 parts by weight of an additive containing a fluorine element (manufactured by Shin-Etsu Chemical Co., Ltd., trade name "KY-1203", solid content 20% by weight), and 3 parts by weight of a photopolymerization initiator (manufactured by BASF, trade name "OMNIRAD 907", solid content 100% by weight) were mixed. A mixed solvent of TBA (tert-butyl alcohol), MIBK (methyl isobutyl ketone) and PMA (propylene glycol monomethyl ether acetate) in a weight ratio of 60:25:15 was added to the mixture as a diluent so that the overall solid content reached 4 weight %, and the mixture was stirred to prepare a coating liquid B for forming an anti-reflection layer.
[0162] (First Lamination Section)
[0163] The positive C plate was bonded to the λ / 4 member (stretched film) via an ultraviolet curable adhesive (thickness after curing: 1 μm) to obtain a phase difference member.
[0164] The obtained phase difference member was bonded to a glass plate (Micro Slide Glass, product number S, thickness 1.3 mm, 180 mm x 250 mm, manufactured by MATSUNAMI) via the 5 μm thick adhesive layer so that the positive C plate of the phase difference member was located on the glass plate side.
[0165] Next, the protective member was bonded to the phase difference member via the 5 μm thick adhesive layer to obtain a first laminated portion on the glass plate. Here, the protective member was bonded so that the acrylic film of the protective member was located on the phase difference member side.
[0166] (Production of Absorption-Type Polarizing Film)
[0167] As the thermoplastic resin substrate, a long amorphous polyethylene terephthalate copolymer film (thickness: 100 μm) having a water absorption rate of 0.75% and a Tg of about 75° C. was used. One surface of the resin substrate was subjected to a corona treatment.
[0168] To 100 parts by weight of a PVA-based resin prepared by mixing polyvinyl alcohol (degree of polymerization 4200, degree of saponification 99.2 mol%) and acetoacetyl-modified PVA (manufactured by Mitsubishi Chemical Corporation, trade name "GOHSENX Z410") in a ratio of 9:1, 13 parts by weight of potassium iodide were added, and the resulting mixture was dissolved in water to prepare a PVA aqueous solution (coating solution).
[0169] The PVA aqueous solution was applied to the corona-treated surface of the resin substrate and dried at 60° C., thereby forming a PVA-based resin layer with a thickness of 13 μm, thereby producing a laminate.
[0170] The obtained laminate was subjected to free-end uniaxial stretching to 2.4 times in the longitudinal direction (longitudinal direction) between rolls having different peripheral speeds in an oven at 130° C. (auxiliary stretching treatment in an atmosphere).
[0171] Next, the laminate was immersed in an insolubilization bath (boric acid aqueous solution prepared by mixing 4 parts by weight of boric acid with 100 parts by weight of water) at a liquid temperature of 40° C. for 30 seconds (insolubilization treatment).
[0172] Next, the film was immersed in a dyeing bath (an iodine aqueous solution obtained by mixing iodine and potassium iodide in a weight ratio of 1:7 relative to 100 parts by weight of water) at a liquid temperature of 30°C for 60 seconds (dyeing treatment) while adjusting the concentration so that the single body transmittance (Ts) of the final polarizing film would reach 42.0% or more.
[0173] Next, the sample was immersed in a crosslinking bath (boric acid aqueous solution containing 3 parts by mass of potassium iodide and 5 parts by mass of boric acid per 100 parts by mass of water) at a liquid temperature of 40° C. for 30 seconds (crosslinking treatment).
[0174] Then, the laminate was immersed in an aqueous boric acid solution (boric acid concentration 4 wt%, potassium iodide concentration 5 wt%) at a liquid temperature of 70°C, and simultaneously uniaxially stretched (stretching treatment in aqueous solution) in the longitudinal direction (length direction) between rollers with different circumferential speeds so that the total stretching ratio reached 5.5 times.
[0175] Then, the laminated body was immersed in a cleaning bath (an aqueous solution containing 4 parts by weight of potassium iodide per 100 parts by weight of water) at a liquid temperature of 20° C. (cleaning treatment).
[0176] Then, the laminate was dried in an oven maintained at 90° C. and brought into contact with a SUS heating roll maintained at a surface temperature of about 75° C. for about 2 seconds (drying shrinkage treatment). The shrinkage rate in the width direction of the laminate due to the drying shrinkage treatment was 5.2%.
[0177] In this manner, a polarizing film (absorption-type polarizing film) having a thickness of 5 μm was formed on the resin substrate.
[0178] (Second laminated portion)
[0179] The absorption-type polarizing film was bonded to a glass plate (manufactured by MATSUNAMI CORPORATION, MICRO SLIDE GLASS, product number S, thickness 1.3 mm, 180 mm×250 mm) via the 5 μm-thick adhesive layer.
[0180] Next, a reflective polarizing film (“APCF” manufactured by Nitto Denko Corporation) was bonded to the absorptive polarizing film via the 5 μm thick adhesive layer so that the reflection axis of the reflective polarizing film and the absorption axis of the absorptive polarizing film were parallel to each other.
[0181] Next, the protective member was laminated onto the reflective polarizing film to obtain a second laminated portion on the glass plate. Here, the protective member was laminated so that the acrylic film of the protective member was located on the reflective polarizing film side.
[0182] [Example 2]
[0183] A first laminated portion and a second laminated portion were obtained in the same manner as in Example 1 except that the adhesive layer described below was used.
[0184] (Formation of Adhesive Layer)
[0185] A monomer mixture containing 94.9 parts by weight of butyl acrylate, 5 parts by weight of acrylic acid and 0.1 parts by weight of 2-hydroxyethyl acrylate was added to a four-necked flask equipped with a stirring blade, a thermometer, a nitrogen inlet tube and a condenser. Furthermore, 0.3 parts by weight of dibenzoyl peroxide as a polymerization initiator was added together with ethyl acetate to 100 parts by weight of the monomer mixture, and nitrogen was introduced while slowly stirring to replace the flask with nitrogen. The liquid temperature in the flask was maintained at 60° C. and a polymerization reaction was performed for 7 hours. Next, ethyl acetate was added to the obtained reaction solution to adjust the solid content concentration to 30% by weight, thereby preparing a solution of an acrylic polymer having a weight average molecular weight (Mw) of 2.2 million.
[0186] An acrylic adhesive was prepared by adding 0.6 parts by weight of a trimethylolpropane / toluene diisocyanate adduct (trade name: Coronate L, manufactured by Tosoh Corporation) and 0.075 parts by weight of a silane coupling agent (trade name: KBM403, manufactured by Shin-Etsu Chemical Co., Ltd.) to 100 parts by weight of the solid content of the obtained acrylic polymer solution.
[0187] The obtained acrylic adhesive was applied to a substrate film, and the coated film on the obtained substrate film was dried in an oven to form an adhesive layer having a thickness of 15 μm and a surface roughness Ra of 16 nm. It should be noted that the drying was performed by adjusting the wind speed in the oven from the oven entrance to the center of the oven within a range of 15 m / min or less.
[0188] [Comparative Example 1]
[0189] During the formation of the adhesive layer, the first laminated part and the second laminated part were obtained in the same manner as in Example 2 except that the wind speed in the oven was adjusted within a range of 15 m / min or less to obtain an adhesive layer having a thickness of 15 μm and a surface roughness Ra of 22 nm.
[0190] [Comparative Example 2]
[0191] In the formation of the adhesive layer, the coating thickness of the acrylic adhesive was changed, and the wind speed in the oven was adjusted within a range below 15 m / min, thereby obtaining an adhesive layer with a thickness of 23 μm and a surface roughness Ra of 29 nm. Except for this, the first and second laminated parts were obtained in the same manner as in Example 2.
[0192] For Examples and Comparative Examples, ISC values were measured using EyeScale-4W manufactured by I System Co., Ltd. Specifically, based on the operating method of the measuring device, the in-plane variations of the first laminated portion and the second laminated portion were calculated as ISC values in the ISC measurement mode of the 3CCD image sensor.
[0193] Figure 4 This is a diagram used to explain the method of measuring the ISC value. It is a simplified diagram of the configuration of the light source, measurement sample, screen, and CCD camera as viewed from above. Figure 4 As shown, the light source L, the first stacked unit 100, the second stacked unit 200, and the screen S were arranged in this order, and the transmission image projected onto the screen S was measured by the CCD camera C.
[0194] The first laminated part 100 and the second laminated part 200, which are the measurement samples, are arranged with a gap of 0.001 to 3 mm in a manner that the protective members face each other (the first laminated part 100 is arranged so that the adjacent glass plate G is located on the light source L side, and the second laminated part 200 is arranged so that the adjacent glass plate G is located on the screen S side). The arrangement is such that the distance from the light source L to the measurement sample in the X-axis direction is 10 to 60 cm. The arrangement is such that the distance from the light source L to the screen S in the X-axis direction is 70 to 130 cm. The arrangement is such that the distance from the CCD camera C to the measurement sample in the Y-axis direction is 3 to 30 cm. The arrangement is such that the distance from the CCD camera C to the screen S in the X-axis direction is 70 to 130 cm.
[0195] It should be noted that in order to make the figure easier to observe, Figure 4 The measurement results are shown in Table 1.
[0196] For the Examples and Comparative Examples, the appearance (light transmitted through the lens) was evaluated using an optical lens (manufactured by Thorabs, trade name “LA1145”) and a point light source (manufactured by Hamamatsu Photonics Co., Ltd., model “L8425-01”).
[0197] Specifically, the first laminated portion and the second laminated portion cut into a 45 mm φ circle were laminated on the flat side of the optical lens while gently pressing with a hand roller in order to not introduce foreign matter, bubbles, or deformed stripes onto the surface. Next, in order to remove the influence of tiny bubbles, degassing was performed using a pressurized degassing device (autoclave). The degassing conditions were set to 50°C, 0.5 MPa, and 30 minutes. After degassing, the sample was naturally cooled at room temperature for more than 30 minutes to obtain a measurement sample.
[0198] A point light source, an optical lens (measurement sample), and a screen were set up in sequence, and the light from the point light source after passing through the optical lens was projected onto the screen to evaluate its aesthetics. The lens was held by a holding fixture at a position where the light from the point light source was incident from the convex side of the optical lens. The distance from the point light source to the screen was set to 1050 mm, and the distance from the optical lens to the screen was set to 130 mm.
[0199] The light projected on the screen through the optical lens was observed with the naked eye, and the appearance was evaluated according to the following evaluation criteria. The measurement results are shown in Table 1.
[0200] (Evaluation Criteria)
[0201] Good: No wrinkles / ripples observed
[0202] · Bad: Wrinkles / ripples were observed
[0203] [Table 1]
[0204]
[0205] The present invention is not limited to the above-described embodiments, and various modifications are possible. For example, the above-described embodiments may be replaced with substantially the same configuration, a configuration that exhibits the same effects, or a configuration that achieves the same purpose.
[0206] Industrial Applicability
[0207] The lens unit according to the embodiment of the present invention can be used for a display body such as VR goggles, for example.
Claims
1. A lens unit used in a display system for displaying an image to a user, The lens portion comprises: A reflective polarizing member that reflects light emitted forward from a display surface of a display element that displays an image and that passes through the polarizing member and the first λ / 4 member; A first lens portion disposed on an optical path between the display element and the reflective polarization component; a half mirror disposed between the display element and the first lens portion, transmitting light emitted from the display element and reflecting light reflected from the reflective polarization member toward the reflective polarization member; a second lens portion disposed in front of the reflective polarization component; as well as a second λ / 4 member disposed on an optical path between the half mirror and the reflective polarization member, The ISC values of the first laminated portion including the second λ / 4 member and at least one adhesive layer and the second laminated portion including the reflective polarizing member and at least one adhesive layer are 100 or less.
2. The lens unit according to claim 1, wherein: The second stacked portion includes an absorptive polarization element disposed between the reflective polarization element and the second lens portion.
3. The lens unit according to claim 1, wherein: The second stacked portion includes a 3λ / 4 element disposed between the reflective polarization element and the second lens portion.
4. The lens unit according to claim 1, wherein: The first stacked portion and the second stacked portion are arranged separately.
5. The lens unit according to claim 1, wherein: The second stacked section includes a second protective member disposed behind the reflective polarization element.
6. The lens unit according to claim 1, wherein: The first stacked portion includes a first protective member disposed in front of the second λ / 4 member.
7. The lens portion according to claim 1, wherein: The total number of the adhesive layers included in the first laminated portion and the adhesive layers included in the second laminated portion is three or more.
8. The lens portion according to claim 1, wherein The thickness of each of the adhesive layer included in the first laminated portion and the adhesive layer included in the second laminated portion is 20 μm or less.
9. The lens portion according to claim 1, wherein: The adhesive layer included in the first laminated portion and the adhesive layer included in the second laminated portion each have a surface roughness Ra of 20 nm or less.
10. The lens portion according to claim 1, wherein The adhesive layer included in the first laminated portion and the adhesive layer included in the second laminated portion are each a single layer body.
11. The lens portion according to claim 1, wherein The first lens portion is integral with the half mirror. 12 . A display body comprising the lens portion according to claim 1 .
13. A display method, comprising: a step of allowing the light of the display image emitted through the polarization element and the first λ / 4 element to pass through the half mirror and the first lens portion; a step of allowing the light that has passed through the half mirror and the first lens portion to pass through a second λ / 4 member; A step of causing the light after passing through the second λ / 4 member to be reflected toward the half mirror by a reflective polarization member; A step of allowing the light reflected by the reflective polarization member and the half mirror to pass through the reflective polarization member via the second λ / 4 member; as well as a step of allowing the light transmitted through the reflective polarizing member to pass through a second lens unit, The ISC values of the first laminated portion including the second λ / 4 member and at least one adhesive layer and the second laminated portion including the reflective polarizing member and at least one adhesive layer are 100 or less.
Citation Information
Patent Citations
Homeotropic alignment liquid-crystalline composition, method for producing homeotropic alignment liquid crystal film and homeotropic alignment liquid crystal film
JP2002333642A
Elliptical polarization plate and picture display device using it
JP2006163343A
Method of producing elliptically polarizing plate and image display using the elliptically polarizing plate
JP2006178389A
Circularly polarizing plate and display device
JP2014010291A
Polarizing plate and organic el panel
JP2014026266A