Memory fabric with wrinkle recovery capability and preparation method thereof
By combining polyester fiber, elastic fiber and shape memory alloy fiber in memory fabrics and air jet spinning technology, the problem of degradation of wrinkle recovery ability of traditional fabrics is solved, and efficient wrinkle recovery and wrinkle resistance of fabrics during multiple uses is achieved. Performance improvement.
Patent Information
- Application Number
- CN202411049343.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-01
- Publication Date
- 2024-11-19
AI Technical Summary
After multiple washing and wearing traditional memory fabrics, the wrinkle recovery performance has significantly decreased, making it difficult to meet the requirements of efficient recovery.
Polyester fiber, elastic fiber and shape memory alloy fiber are mixed in preset proportions, spun into yarns through air jet spinning technology, and fabrics are prepared in combination with advanced weaving technology, and shape memory alloy fibers are activated by air jet spinning technology and heat treatment to enhance Fabric pleat recovery ability.
It significantly improves the wrinkle recovery ability of the fabric, ensures good flatness and comfort in daily use, reduces wrinkle generation, and enhances the wrinkle resistance and structural stability of the fabric.
Smart Images

Figure CN118979328A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of textile fabric preparation, in particular to a memory fabric with wrinkle recovery capability and a preparation method thereof. Background Art
[0002] With the continuous advancement of textile technology, the types and properties of fabrics are becoming increasingly diverse. Among them, memory fabrics have attracted widespread attention due to their unique shape memory function. However, the wrinkle recovery ability of traditional memory fabrics still needs to be improved, especially after multiple washings and wearing, the wrinkle recovery performance of the fabric will be significantly reduced. Therefore, how to improve the wrinkle recovery ability of memory fabrics is a technical problem that needs to be solved urgently. Summary of the invention
[0003] In order to improve the wrinkle recovery ability of fabric, the present application provides a memory fabric with wrinkle recovery ability and a preparation method thereof.
[0004] The above-mentioned invention objective of the present application is achieved through the following technical solutions: A memory fabric with wrinkle recovery capability and a preparation method thereof, the memory fabric with wrinkle recovery capability and the preparation method thereof comprising: The polyester fiber, the elastic fiber, and the shape memory alloy fiber are mixed in a preset ratio to obtain a mixed fiber; The mixed fiber is spun into yarn by jet spinning technology, and the yarn is woven into memory fabric with wrinkle recovery capability.
[0005] By adopting the above technical solutions, polyester fiber has good strength and wear resistance, ensuring the durability of the fabric. Polyester fiber itself has a certain wrinkle resistance and can maintain the flatness of the fabric. Elastic fiber provides good elasticity, making the fabric have better stretchability and comfort. Elastic fiber can quickly return to its original shape after being stressed, enhancing the wrinkle recovery ability of the fabric. Shape memory alloy fiber can return to its original shape after heating, which gives the fabric excellent wrinkle recovery ability. Jet spinning technology can effectively mix different types of fibers together to form uniform yarns, ensuring that each yarn has the same physical properties. Jet spinning technology uses high-speed airflow to stretch and twist the fibers, making the fiber arrangement more compact and orderly, and improving the strength and elasticity of the yarn. In the process of weaving yarn into fabric, a reasonable weaving process is used to ensure the stability and consistency of the fabric structure, avoiding the influence of uneven yarn on the performance of the fabric. The combination of synthetic fibers and advanced weaving technology enables the fabric to maintain good flatness and reduce wrinkles in daily use. The introduction of shape memory alloy fibers enables the fabric to quickly return to its original shape after being deformed by force, significantly improving the fabric's wrinkle recovery ability.
[0006] In a preferred example, the present application can be further configured as follows: the polyester fiber, the elastic fiber, and the shape memory alloy fiber are mixed in a preset ratio to obtain a mixed fiber, specifically comprising: The polyester fiber is used in an amount of 75%-85%, the elastic fiber is selected from polyurethane elastic fiber or polyester elastic fiber, and the amount is 8%-12%, and the shape memory alloy fiber is selected from nickel-titanium alloy fiber, and the amount is 5%-7%.
[0007] By adopting the above technical solutions, a high proportion of polyester fibers ensures that the fabric has good strength and wear resistance, allowing it to withstand daily wear and stretching. Polyester fibers themselves have a certain wrinkle resistance, providing basic wrinkle resistance for the fabric. Elastic fibers can give the fabric better elasticity, allowing it to quickly return to its original shape after being stressed, increasing the comfort of the fabric. An appropriate amount of elastic fibers can provide the necessary flexibility and ductility in the fiber structure and enhance the fabric's ability to recover. Nitinol fibers can return to their original shape after heating, a feature that greatly improves the fabric's ability to recover from wrinkles. Shape memory alloy fibers can automatically return to flatness when the fabric is heated, ensuring that the fabric maintains a good appearance under various temperature environments. By mixing different types of fibers in proportion, the advantages of each fiber can be comprehensively utilized to improve the overall performance of the fabric.
[0008] In a preferred example, the present application can be further configured as follows: the mixed fiber is spun into yarn by jet spinning technology, and the yarn is woven into a memory fabric with wrinkle recovery ability, specifically including: According to the air-jet spinning technology, the mixed fibers are opened to obtain opened fibers; Combing the opened fibers to obtain a continuous fiber web; stretching the continuous fiber web to obtain stretched fiber strips; The fiber bundles in the stretched fiber strips are twisted by high-speed airflow to obtain the yarn, and the yarn is woven into the memory fabric with wrinkle recovery ability.
[0009] By adopting the above technical scheme, the opening process will fully separate the mixed fibers, ensuring that each fiber is evenly distributed in the subsequent process, which is conducive to the uniform performance of the final fabric. The fibers after opening are looser, which is conducive to the uniform mixing and arrangement of the fibers, and prevents the fibers from agglomerating and affecting the flatness of the fabric. The combing process straightens the fibers, improves the parallelism of the fibers, and forms a uniform fiber network, providing a good foundation for subsequent drafting and twisting. Combing can remove impurities and short fibers in the fibers, further improving the quality of yarn and fabric. The drafting process stretches the fiber network into fiber strips, enhances the strength and uniformity of the yarn, and ensures that the yarn is not easy to break during the weaving process. Drafting makes the fibers more closely arranged, improves the bonding force between the fibers, and increases the stability and durability of the yarn and fabric. The twisting process makes the fibers tightly entangled together to form a stable yarn structure, and improves the yarn's tensile and bending resistance. Through twisting, the yarn obtains better elasticity and recovery, which helps the fabric to quickly return to its original state after being stressed and reduce wrinkles. High-quality yarns ensure uniform fabric structure and improve the overall quality and appearance of the fabric through reasonable weaving processes. The reasonable distribution of shape memory alloy fibers during the weaving process enables the fabric to return to its original shape when heated, significantly improving the wrinkle recovery ability.
[0010] In a preferred example, the present application can be further configured as follows: the fiber bundles in the stretched fiber strips are twisted by using high-speed airflow to obtain the yarn, and the yarn is woven into the memory fabric with wrinkle recovery ability, specifically including: Performing quality inspection on the yarn to obtain inspected yarn; According to the design requirements, the loom parameters are adjusted to divide the inspected yarns into warp yarns and weft yarns, wherein the warp yarns are used for weaving longitudinal yarns and the weft yarns are used for weaving transverse yarns; The warp yarn is lifted by an opening device to form a shed, the weft yarn is inserted into the shed by a weft insertion device, and the weft yarn is pressed against the edge of the woven fabric by a beating-up device until the fabric reaches a desired length.
[0011] By adopting the above technical solutions, through strict quality inspection, defective yarns can be eliminated to ensure that the yarns used for weaving have consistent strength, elasticity and other key properties. By adjusting the loom parameters, the tension of the warp and weft yarns is moderate, and the yarns are prevented from breaking or relaxing during the weaving process, thereby improving the uniformity and stability of the fabric. Reasonable allocation of warp and weft yarns ensures that the yarns are evenly distributed in the fabric, improving the structural stability and wrinkle resistance of the fabric. The precise operation of the opening device and the weft insertion device ensures that the weft yarn is accurately inserted into the shed, making the fabric structure tight and uniform, which helps to improve the wrinkle resistance of the fabric. The uniform pressing of the beating device makes the weft yarn and the warp yarn closely combined, enhances the elasticity and recovery of the fabric, helps the fabric to quickly return to its original state after being stressed, and reduces wrinkles. The fine weaving process ensures the flatness and smoothness of the fabric surface, and improves the appearance quality and comfort of the fabric.
[0012] In a preferred example, the present application can be further configured as follows: the memory fabric with wrinkle recovery ability and the preparation method thereof further include: The memory fabric with wrinkle recovery capability is heat-treated to activate the shape memory alloy fibers, thereby giving the fabric wrinkle recovery capability.
[0013] By adopting the above technical solution, shape memory alloy fibers are activated by heat treatment, and these fibers can return to a preset shape after being heated. When wrinkles appear on the fabric, the fabric can be restored to flatness by heating, thereby greatly improving the wrinkle recovery ability of the fabric. Heat treatment not only activates the shape memory alloy fibers, but also makes the fiber structure of the entire fabric more stable, reduces slippage and deformation between fibers, and helps the fabric maintain its original shape and function. Heat treatment helps the elastic properties of shape memory alloy fibers to be exerted, so that the fabric can quickly return to its original shape after being stretched or compressed, and improves the elasticity and comfort of the fabric.
[0014] In a preferred example, the present application can be further configured as follows: the memory fabric with wrinkle recovery ability and the preparation method thereof further include: By coating nanoparticles on the memory fabric with wrinkle recovery ability, the wrinkle resistance and recovery of the fabric can be enhanced.
[0015] By adopting the above technical solution, the nanoparticles are small in size and can penetrate deep into the gaps between fibers to form a uniform coating, effectively filling the gaps between fibers, reducing friction and slippage between fibers, and thus enhancing the wrinkle resistance of the fabric. After coating with nanoparticles, the surface of the fabric becomes smoother, reducing the friction between fibers, making it easier for the fabric to return to a flat state after being compressed. Nanoparticles can change the surface properties of the fabric, such as increasing the smoothness and hydrophobicity of the surface and reducing the generation and accumulation of wrinkles.
[0016] In a preferred example, the present application can be further configured as follows: coating nanoparticles on the memory fabric with wrinkle recovery ability to enhance the wrinkle resistance and recovery of the fabric, and further comprising: Titanium dioxide nanoparticles are prepared by a sol-gel method to prepare a nanoparticle dispersion with a concentration of 1%, and the titanium dioxide nanoparticles are sprayed on the wrinkle recovery memory fabric to obtain the wrinkle recovery memory fabric after spraying; The sprayed memory fabric with wrinkle recovery ability is dried at 80° C. for 1 hour to obtain a dried memory fabric with wrinkle recovery ability, and the dried memory fabric with wrinkle recovery ability is cured at 120° C. for 30 minutes to form a firm bond between the titanium dioxide nanoparticles and the memory fabric with wrinkle recovery ability.
[0017] By adopting the above technical solution, the titanium dioxide nanoparticles prepared by the sol-gel method can evenly cover the surface of the fabric, penetrate into the gaps between fibers, form a dense coating, and improve the wrinkle resistance and structural stability of the fabric. The titanium dioxide nanoparticle coating makes the surface of the fabric smoother, reduces fiber friction, assists the recovery function of the shape memory alloy fiber, and improves the wrinkle recovery ability of the fabric.
[0018] In summary, the present application includes at least one of the following beneficial technical effects: 1. Polyester fiber has good strength and wear resistance, which ensures the durability of the fabric. Polyester fiber itself has a certain wrinkle resistance and can maintain the flatness of the fabric. Elastic fiber provides good elasticity, which makes the fabric have better stretchability and comfort. Elastic fiber can quickly return to its original shape after being stressed, enhancing the wrinkle recovery ability of the fabric. Shape memory alloy fiber can return to its original shape after heating, which gives the fabric excellent wrinkle recovery ability. Jet spinning technology can effectively mix different types of fibers together to form uniform yarns, ensuring that each yarn has the same physical properties. Jet spinning technology uses high-speed airflow to stretch and twist the fibers, making the fiber arrangement more compact and orderly, and improving the strength and elasticity of the yarn. In the process of weaving yarn into fabric, a reasonable weaving process is used to ensure the stability and consistency of the fabric structure, avoiding the influence of uneven yarn on the performance of the fabric. The combination of synthetic fibers and advanced weaving technology enables the fabric to maintain good flatness and reduce wrinkles in daily use. The introduction of shape memory alloy fibers enables the fabric to quickly return to its original shape after being deformed by force, significantly improving the wrinkle recovery ability of the fabric; 2. Activate shape memory alloy fibers through heat treatment. These fibers can return to the preset shape after being heated. When wrinkles appear on the fabric, heating can restore the fabric to flatness, thereby greatly improving the wrinkle recovery ability of the fabric. Heat treatment not only activates shape memory alloy fibers, but also makes the fiber structure of the entire fabric more stable, reduces slippage and deformation between fibers, and helps the fabric maintain its original shape and function. Heat treatment helps the elastic properties of shape memory alloy fibers to be exerted, so that the fabric can quickly return to its original shape after being stretched or compressed, improving the elasticity and comfort of the fabric; 3. Nanoparticles are small in size and can penetrate into the gaps between fibers to form a uniform coating, effectively filling the gaps between fibers, reducing friction and slippage between fibers, and thus enhancing the wrinkle resistance of fabrics. After coating with nanoparticles, the surface of the fabric becomes smoother, reducing the friction between fibers, making it easier for the fabric to return to a flat state after being compressed. Nanoparticles can change the surface properties of fabrics, such as increasing surface smoothness and hydrophobicity, and reducing the generation and accumulation of wrinkles. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 This is a flow chart of a memory fabric with wrinkle recovery capability and a preparation method thereof in one embodiment of the present application; Figure 2 It is a flowchart for implementing step S10 in a memory fabric with wrinkle recovery capability and a preparation method thereof in one embodiment of the present application; Figure 3 It is a flowchart for implementing step S20 in a memory fabric with wrinkle recovery capability and a preparation method thereof in an embodiment of the present application; Figure 4 It is a flowchart for implementing step S24 in a memory fabric with wrinkle recovery capability and a preparation method thereof in an embodiment of the present application; Figure 5 This is a flowchart of the memory fabric with wrinkle recovery ability and the preparation method thereof after step S20 in one embodiment of the present application; Figure 6 It is a flowchart for implementing step S30 in a memory fabric with wrinkle recovery capability and a preparation method thereof in an embodiment of the present application; Figure 7 This is a flowchart of the memory fabric with wrinkle recovery ability and the method for preparing the same after step S20 in one embodiment of the present application; Figure 8 This is a flowchart for implementing step S40 in a memory fabric with wrinkle recovery capability and a preparation method thereof in one embodiment of the present application. DETAILED DESCRIPTION
[0020] The present application is further described in detail below in conjunction with the accompanying drawings.
[0021] In one embodiment, if Figure 1 As shown, the present application discloses a memory fabric with wrinkle recovery ability and a preparation method thereof, which specifically comprises the following steps: S10: The polyester fiber, the elastic fiber, and the shape memory alloy fiber are mixed according to a preset ratio to obtain a mixed fiber.
[0022] Specifically, the polyester fiber, elastic fiber and shape memory alloy fiber are quality inspected to ensure that they meet the specification requirements. The weighting and proportioning are carried out according to the preset ratio. According to the characteristics of the fiber and the mixing requirements, the appropriate mixing equipment is selected. Commonly used equipment includes an opener, a cotton mixer or a blender. The opener is used to open, loosen and preliminarily mix the fibers. The cotton mixer is used to further mix the fibers so that they are evenly distributed. The blender is used to finally evenly mix the fibers to ensure consistent proportions. The weighed fibers are placed in the opener for opening treatment. The opener opens the fibers and loosens them into a single fiber state. The polyester fiber is placed in the opener for opening treatment. The elastic fiber is placed in the opener for opening treatment. The shape memory alloy fiber is placed in the opener for opening treatment. The opened polyester fiber, elastic fiber and shape memory alloy fiber are placed in the blender according to the preset ratio for preliminary mixing. The blender preliminarily mixes different fibers evenly through airflow and mechanical action. The preliminarily mixed fibers are placed in the blender for further mixing. The mixer uses rollers, stirring and airflow to further mix the fibers evenly to ensure consistent proportions.
[0023] S20: The blended fibers are spun into yarns through air-jet spinning technology, and the yarns are woven into memory fabrics with wrinkle recovery capabilities.
[0024] In this embodiment, the jet spinning technology refers to applying a drafting force to the fibers through a high-speed airflow, so that the individual fibers in the fiber bundle are fully stretched and separated, thereby forming a uniform, fine and high-strength yarn.
[0025] Specifically, polyester fibers, elastic fibers and shape memory alloy fibers mixed in a preset ratio are opened to ensure that the fibers are uniformly loose. The opened mixed fibers are uniformly fed into the drafting system of the air jet spinning machine through a feeding device (such as a feeding roller). The fibers are gradually stretched and thinned in the drafting system by step-by-step drafting. The fiber bundle enters the nozzle area. The nozzle applies additional drafting force to the fiber bundle through high-speed airflow to further stretch and separate the fibers. The kinetic energy of the high-speed airflow separates the individual fibers in the fiber bundle and moves rapidly in the direction of the airflow. In the nozzle area, the high-speed airflow not only drafts the fibers, but also bundles and rotates the separated fibers to form uniform yarns. The yarns made by air jet spinning technology are prepared according to the requirements of the fabric design. The yarns should be uniform, knot-free, and have sufficient strength and elasticity. The prepared yarns are installed on the loom, and the various parameters of the loom (such as the tension of the warp and weft yarns, weaving density, etc.) are adjusted to ensure the smooth weaving process. The yarns are arranged into warp yarns according to the designed pattern and density. The warp yarn is the longitudinal yarn of the fabric and needs to maintain proper tension. During the weaving process, the weft yarn (transverse yarn) is inserted between the warp yarns and guided between the warp yarns by the shuttle or air jet device of the loom to form the fabric. The interweaving of the warp and weft yarns forms a fabric with a specific pattern and structure.
[0026] In one embodiment, if Figure 2 As shown, in step S10, polyester fiber, elastic fiber, and shape memory alloy fiber are mixed in a preset ratio to obtain mixed fiber, which specifically includes: S11: The dosage of polyester fiber is 75%-85%, the elastic fiber selects polyurethane elastic fiber or polyester elastic fiber, the dosage is 8%-12%, and the shape memory alloy fiber selects nickel-titanium alloy fiber, the dosage is 5%-7%.
[0027] Specifically, a high-precision electronic balance is used for weighing to ensure that the proportion of each fiber is accurate. Weigh the polyester fiber at a ratio of 75%-85%. For example, assuming the total weight is 100kg, weigh 75kg to 85kg of polyester fiber. Weigh the elastic fiber (polyurethane elastic fiber or polyester elastic fiber) at a ratio of 8%-12%. For example, weigh 8kg to 12kg of elastic fiber. Weigh the nickel-titanium alloy fiber at a ratio of 5%-7%. For example, weigh 5kg to 7kg of nickel-titanium alloy fiber. The weighed polyester fiber, elastic fiber and shape memory alloy fiber are opened separately to make them loose. The opened fibers are put into the mixer in proportion for full mixing to ensure that the fibers are evenly distributed.
[0028] In one embodiment, if Figure 3As shown, in step S20, the mixed fiber is spun into yarn by jet spinning technology, and the yarn is woven into a memory fabric with wrinkle recovery ability, which specifically includes: S21: Opening the mixed fibers according to the jet spinning technology to obtain opened fibers.
[0029] Specifically, the polyester fiber, elastic fiber (polyurethane elastic fiber or polyester elastic fiber) and shape memory alloy fiber mixed in proportion are preliminarily loosened to make them easy to feed into the opener. The pretreated mixed fiber is uniformly fed into the feeding device of the opener. The fiber is fed into the entrance of the opener using a conveyor belt or a feeding roller. The fiber is mechanically opened by multiple rollers and nail plates of the opener. The rollers and nail plates rotate to gradually loosen the fiber bundles into a single fiber state. The airflow device in the opener further separates and loosens the fibers through high-speed airflow. The high-speed airflow exerts additional traction on the fibers, making the fibers looser and more evenly distributed. The opened fibers are transported to the collection area through a conveying system or an airflow conveying device. A collector or a collection box is used to collect the opened fibers. At the same time, it is ensured that the fibers remain loose during the collection process to avoid re-agglomeration.
[0030] S22: combing the opened fibers to obtain a continuous fiber web.
[0031] Specifically, the fibers are preliminarily combed by the first set of rollers and pins in the carding machine. The rollers and pins rotate to separate the fiber bundles and preliminarily arrange them in parallel. The fibers enter the combing part of the carding machine, and are further combed by multiple sets of pins and combing rollers to make the fibers more parallel and uniform. The combed fibers pass through the output part of the carding machine to form a continuous fiber web. The rotation speed and spacing of the rollers and pins in the carding machine are precisely controlled to ensure the uniformity and continuity of the fiber web. The combed continuous fiber web is transported to the collection area through a conveying device or an air conveying device. The fiber web is wound or folded and collected using a collection roller or a collection frame. At the same time, it is ensured that the fiber web maintains continuity and uniformity during the collection process to avoid breakage and overlap.
[0032] S23: stretching the continuous fiber web to obtain stretched fiber strips.
[0033] Specifically, the fiber web is initially drafted by the first set of rollers of the drafting machine. The rotation speed of the rollers gradually increases, so that the fiber web is subjected to traction and begins to stretch. The fiber web enters the multi-stage drafting section of the drafting machine and is drafted step by step by multiple sets of drafting rollers. The speed of each roller is faster than the previous one, so that the fibers are gradually stretched, the density of the fibers is reduced and made more uniform. Finally, the fiber web passes through the fine drafting section of the drafting machine, which further stretches and refines the fibers, making the fibers more uniform and parallel. The drafted fiber strips are collected by the output device, and the fiber strips can be wound or folded and collected using the collecting rollers or the collecting frame. At the same time, ensure that the fiber strips maintain continuity and uniformity during the collection process to avoid breakage and overlap.
[0034] S24: Utilize high-speed airflow to twist the fiber bundles in the drawn fiber strips to obtain yarns, and weave the yarns into memory fabrics with wrinkle recovery capability.
[0035] Specifically, the fiber strips enter the twisting zone through the drafting rollers, where the fiber strips are drafted into single fibers and form fiber bundles. The fiber bundles enter the nozzle area of the air jet spinning machine and are twisted by the high-speed rotating airflow. The rotation speed and pressure of the airflow can be adjusted to ensure that the yarn is twisted evenly and tightly. The twisted fiber bundles form yarns at the nozzle outlet, which are pulled out through the drafting system and finally wound on the cheese yarn. The formed yarns are evenly wound on the cheese yarns through the yarn guide device. Ensure that the yarns maintain uniform tension and twist during the winding process. The prepared yarns are prepared as warp yarns and weft yarns respectively, the warp yarns are arranged through the warp beam, and the weft yarns are arranged through the shuttle or weft insertion device. Interweaving of warp and weft yarns: The warp yarns and weft yarns are interwoven into fabrics on the loom according to the design requirements. The warp yarns and weft yarns are interwoven through the shed of the loom and the shuttle insertion device to form the required fabric structure. The loom gradually forms a continuous fabric through the interweaving action of the warp yarns and weft yarns. Control loom tension, speed and weft insertion angle to ensure fabric uniformity and quality.
[0036] In one embodiment, if Figure 4 As shown, in step S24, the fiber bundles in the stretched fiber strips are twisted by using high-speed airflow to obtain yarns, and the yarns are woven into memory fabrics with wrinkle recovery ability, which specifically includes: S241: Performing quality inspection on the yarn to obtain inspected yarn.
[0037] Specifically, samples are randomly selected from mass-produced yarns and subjected to strength test, twist test, uniformity test and appearance inspection in sequence. Each test should be repeated several times, and the average value and standard deviation are recorded. The test results are obtained. The test results are compared with the standard requirements to evaluate the eligibility of the yarn.
[0038] S242: According to the design requirements, the loom parameters are adjusted to divide the inspected yarns into warp yarns and weft yarns, wherein the warp yarns are used for longitudinal yarns for weaving and the weft yarns are used for transverse yarns for weaving.
[0039] Specifically, the density, tension and other parameters of the warp and weft yarns are determined according to the design requirements of the fabric. This includes the fabric structure (such as plain, twill, satin, etc.), as well as the specific distribution and arrangement of the warp and weft yarns. The inspected yarns are divided into warp and weft yarns. The yarns for the warp yarns are distributed on the warp beams according to the design density. The yarns are evenly arranged on the warp beams according to the design requirements to ensure that the yarn tension is uniform and there is no knotting or entanglement. The warp tension device is adjusted to ensure that the warp tension is consistent to ensure the stability of the weaving process. The yarns for the weft yarns are wound on the weft yarn bobbins and the weft yarn insertion device for the shuttle is prepared. The yarns are evenly wound on the weft yarn bobbins to ensure that the weft yarns are appropriately tight and avoid being too tight or too loose. The tension of the weft yarn during the weaving process is ensured to be uniform by adjusting the tension of the weft yarn insertion device. According to the design requirements, the warp tension control device is adjusted. Ensure that the warp tension is uniform and meets the design requirements. The tension of the warp yarn is controlled by adjusting the tension control device on the loom, such as the tension rod, tension disk, etc. Adjust the parameters of the weft insertion device to ensure that the insertion speed and angle of the weft meet the design requirements. Adjust the speed, angle and tension control of the weft insertion device according to the fabric structure and design requirements. Adjust the height and position of the heald frame according to the design requirements to ensure that the warp and weft are accurately interwoven during the weaving process. Adjust the height of the heald frame so that the warp forms a suitable opening during the weaving process to facilitate the insertion of the weft. Adjust the position of the heald frame to ensure that the warp yarns remain parallel during the weaving process. Adjust the parameters of the beating-up device to ensure that the beating-up force and beating-up angle meet the design requirements. By adjusting the beating-up force of the beating-up device, ensure that the weft yarn is fully beaten into the warp yarn during the weaving process to form a tight fabric structure. Adjust the beating-up angle so that the weft yarn is evenly arranged during the weaving process to avoid uneven beating-up. Pass the warp yarn through the heald and dropper according to the design requirements to ensure that the warp yarn is arranged according to the design during the weaving process. Pass the warp yarn through the heald and dropper in the design order to ensure that the warp yarn is accurately arranged and not staggered. Check the yarn arrangement during the drawing-in process to ensure that the warp yarn tension is uniform and not damaged. The weft yarns are inserted and beat-up as required by the design, gradually forming the fabric. The weft yarns are inserted into the warp openings one by one through a shuttle or other weft insertion device as required by the design. The weft yarns are beaten into the warp yarns by the beat-up device, ensuring a tight and uniform fabric structure.
[0040] S243: The warp yarn is lifted by the opening device to form a shed, the weft yarn is inserted into the shed by the weft insertion device, and the weft yarn is pressed against the edge of the woven fabric by the beating device until the fabric reaches the required length.
[0041] Specifically, the warp yarns are passed through the heald frame and the healds. The up and down movement of the heald frame controls the lifting and lowering of the warp yarns to form the shed. The heald frame is fixed to the loom, ensuring that the height and position of the heald frame are correct. Each warp yarn is passed through the healds in turn, and the warp yarns are arranged neatly and without staggering. The parameters of the shedding device of the loom are set to ensure that the heald frame can be raised and lowered accurately according to the designed structure to form the shed. The weft yarn is inserted into the shed by a weft insertion device (such as a shuttle, air jet, rapier or water jet device). The weft yarn is wound on the weft yarn bobbin to ensure that the weft yarn is appropriately loose. The weft insertion device is installed and its position and parameters are adjusted to ensure that it can accurately insert the weft yarn into the shed. The weft insertion device is started and the weft yarn is inserted into each shed in turn. According to different weft insertion methods, the speed, angle and force of the weft insertion device can be adjusted. The weft yarn inserted into the shed is tightened by a weft beating device (such as a beating sword or a beating shuttle) so that it presses against the edge of the woven fabric. According to the design requirements of the fabric, set the beating force and beating angle of the beating device to ensure that the beating device can beat the weft yarn into the warp yarn evenly and tightly. Start the beating device, and after the weft yarn is inserted into the shed, the beating device presses the weft yarn to ensure that the weft yarn is tightly integrated into the woven fabric. Monitor and record the length of the fabric through the length control device on the loom until it reaches the required length. According to production requirements, set the length control parameters on the loom to ensure that the fabric can automatically stop when it reaches the required length. During the weaving process, monitor the length of the fabric in real time and record the length data of the fabric through mechanical or electronic devices. When the fabric reaches the preset length, the loom automatically stops and stops the weft insertion and beating operations.
[0042] In one embodiment, if Figure 5 As shown, after step S20, the memory fabric with wrinkle recovery ability and the preparation method thereof further include: S30: Heat treatment is performed on the memory fabric with wrinkle recovery ability to activate the shape memory alloy fiber and give the fabric wrinkle recovery ability.
[0043] Specifically, lay the memory fabric to be heat-treated flat on the workbench of the heat treatment equipment to ensure that the fabric is not folded or wrinkled. Lay the fabric flat to ensure that there are no impurities and dirt on the surface of the fabric to prevent the heat treatment effect from being affected. Depending on the equipment, a fixed clamp or a heavy object can be used to lightly press the edge of the fabric to prevent the fabric from shifting during the heat treatment. Start the heat treatment equipment and let the equipment reach the set temperature before starting the heat treatment of the fabric. Start the heat treatment equipment and let it reach the set temperature to ensure that the temperature of the equipment is stable. Place the fabric in the heat treatment equipment and perform heat treatment according to the set time and temperature.
[0044] In one embodiment, if Figure 6As shown, in step S30, the memory fabric with wrinkle recovery ability is heat-treated to activate the shape memory alloy fiber and give the fabric wrinkle recovery ability, which specifically includes: S31: The heat treatment temperature is controlled at 80-120°C for 10-30 minutes to ensure activation of the shape memory alloy fiber.
[0045] Specifically, select and calibrate appropriate heat treatment equipment, including ovens or heat presses, to ensure that they have precise temperature and time control functions. Preheat the equipment to the set temperature range, and lay the fabric to be treated flat in the equipment to ensure that there are no folds and wrinkles. Start the equipment, monitor the temperature in real time to ensure that it is stable at 80-120℃, and use the timing device to ensure that the heat treatment time is within 10-30 minutes. After the treatment is completed, turn off the equipment and let the fabric cool naturally to room temperature in the equipment to avoid rapid cooling and damage to the fabric performance.
[0046] In one embodiment, if Figure 7 As shown, after step S20, the memory fabric with wrinkle recovery ability and the preparation method thereof further include: S40: Nanoparticles are coated on memory fabrics with wrinkle recovery capabilities to enhance the fabric's wrinkle resistance and recovery.
[0047] Specifically, a nanoparticle solution is prepared, the surface of the fabric is cleaned to ensure that there are no impurities, the nanoparticle solution is evenly coated on the fabric by spraying, dipping or rolling, and then heat-curing or ultraviolet curing is performed to make the nanoparticles firmly adhere to the surface of the memory fabric with wrinkle recovery ability.
[0048] In one embodiment, if Figure 8 As shown, in step S40, nanoparticles are coated on the memory fabric with wrinkle recovery ability to enhance the wrinkle resistance and recovery of the fabric, and the method further includes: S41: Titanium dioxide nanoparticles are prepared by a sol-gel method to prepare a nanoparticle dispersion with a concentration of 1%, and the titanium dioxide nanoparticles are sprayed on a memory fabric with wrinkle recovery ability to obtain a memory fabric with wrinkle recovery ability after spraying.
[0049] Specifically, tetrabutyl titanate is prepared as a titanium source. Ethanol is prepared as a solvent. Deionized water and sodium hydroxide solution are prepared as a hydrolyzing agent and a solution for adjusting pH. A certain amount of tetrabutyl titanate is dissolved in ethanol to form a uniform solution. Deionized water is added dropwise to the tetrabutyl titanate solution, the addition speed is controlled to prevent an overly rapid reaction, and continuous stirring is maintained. The pH value of the solution is adjusted to about neutral (pH 7) to promote the hydrolysis and gelation reaction of the TiO2 precursor. The mixed solution is left to stand at room temperature and wait for it to form a gel. The gel is aged at room temperature for 24 hours to enhance the stability of the gel. The gel is dried to remove the solvent and moisture, and dried in an oven at 60°C for 24 hours. After drying, the product is calcined at 400-500°C for 2 hours to obtain pure titanium dioxide nanoparticles. The calcined titanium dioxide nanoparticles are dispersed in deionized water or ethanol to a concentration of 1%. The 1% titanium dioxide nanoparticle dispersion is loaded into a spraying device. Evenly spray the surface of the memory fabric with wrinkle recovery ability.
[0050] S42: Dry the sprayed wrinkle recovery memory fabric at 80° C. for 1 hour to obtain a dried wrinkle recovery memory fabric, and cure the dried wrinkle recovery memory fabric at 120° C. for 30 minutes to form a firm bond between the titanium dioxide nanoparticles and the wrinkle recovery memory fabric.
[0051] Specifically, the sprayed memory fabric is placed in an oven preheated to 80°C. Ensure that the temperature in the oven is uniform and stable. Dry the fabric at 80°C for 1 hour to remove moisture and solvent residues, and at the same time promote the initial bonding of titanium dioxide nanoparticles to the fabric. Adjust the oven temperature to 120°C and preheat. Place the dried memory fabric in an oven preheated to 120°C. Curing at 120°C for 30 minutes allows the titanium dioxide nanoparticles to bond more firmly to the memory fabric. During the curing process, monitor the temperature and time to ensure that the set conditions are not exceeded during the curing process to avoid overheating and damage to the fabric performance. After curing is completed, remove the fabric from the oven and cool it naturally to room temperature.
[0052] It should be understood that the size of the serial numbers of the steps in the above embodiments does not mean the order of execution. The execution order of each process should be determined by its function and internal logic, and should not constitute any limitation on the implementation process of the embodiments of the present application.
[0053] Those skilled in the art can clearly understand that for the convenience and simplicity of description, only the division of the above-mentioned functional units and modules is used as an example. In actual applications, the above-mentioned functions can be distributed and completed by different functional units and modules as needed, that is, the internal structure of the device can be divided into different functional units or modules to complete all or part of the functions described above.
[0054] The above embodiments are only used to illustrate the technical solutions of the present application, rather than to limit them. Although the present application has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. These modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present application, and should all be included in the protection scope of the present application.
Claims
1. A memory fabric with wrinkle recovery ability and a preparation method thereof, characterized in that: The memory fabric with wrinkle recovery ability and the preparation method thereof include: The polyester fiber, the elastic fiber, and the shape memory alloy fiber are mixed in a preset ratio to obtain a mixed fiber; The mixed fiber is spun into yarn by jet spinning technology, and the yarn is woven into memory fabric with wrinkle recovery capability.
2. The memory fabric with wrinkle recovery ability and the preparation method thereof according to claim 1, characterized in that: The polyester fiber, the elastic fiber, and the shape memory alloy fiber are mixed in a preset ratio to obtain the mixed fiber, which specifically includes: The polyester fiber is used in an amount of 75%-85%, the elastic fiber is selected from polyurethane elastic fiber or polyester elastic fiber, and the amount is 8%-12%, and the shape memory alloy fiber is selected from nickel-titanium alloy fiber, and the amount is 5%-7%.
3. The memory fabric with wrinkle recovery ability and the preparation method thereof according to claim 1, characterized in that: The method of spinning the mixed fiber into yarn by jet spinning technology and weaving the yarn into memory fabric with wrinkle recovery ability specifically includes: According to the air-jet spinning technology, the mixed fibers are opened to obtain opened fibers; Combing the opened fibers to obtain a continuous fiber web; stretching the continuous fiber web to obtain stretched fiber strips; The fiber bundles in the stretched fiber strips are twisted by high-speed airflow to obtain the yarn, and the yarn is woven into the memory fabric with wrinkle recovery ability.
4. The memory fabric with wrinkle recovery ability and the preparation method thereof according to claim 3, characterized in that: The method of using a high-speed airflow to twist the fiber bundles in the stretched fiber strips to obtain the yarn, and weaving the yarn into the memory fabric with wrinkle recovery ability, specifically includes: Performing quality inspection on the yarn to obtain inspected yarn; According to the design requirements, the loom parameters are adjusted to divide the inspected yarns into warp yarns and weft yarns, wherein the warp yarns are used for weaving longitudinal yarns and the weft yarns are used for weaving transverse yarns; The warp yarn is lifted by an opening device to form a shed, the weft yarn is inserted into the shed by a weft insertion device, and the weft yarn is pressed against the edge of the woven fabric by a beating-up device until the fabric reaches a desired length.
5. The memory fabric with wrinkle recovery ability and the preparation method thereof according to claim 1, characterized in that: The memory fabric with wrinkle recovery ability and the preparation method thereof also include: The memory fabric with wrinkle recovery capability is heat-treated to activate the shape memory alloy fibers, thereby giving the fabric wrinkle recovery capability.
6. The memory fabric with wrinkle recovery ability and the preparation method thereof according to claim 5, characterized in that: The method of heat treating the memory fabric with wrinkle recovery ability to activate the shape memory alloy fibers and give the fabric wrinkle recovery ability specifically includes: The heat treatment temperature is controlled at 80-120° C. and the duration is 10-30 minutes to ensure activation of the shape memory alloy fiber.
7. The memory fabric with wrinkle recovery ability and the preparation method thereof according to claim 1, characterized in that: The memory fabric with wrinkle recovery ability and the preparation method thereof also include: By coating nanoparticles on the memory fabric with wrinkle recovery ability, the wrinkle resistance and recovery of the fabric can be enhanced.
8. The memory fabric with wrinkle recovery ability and the preparation method thereof according to claim 1, characterized in that: The method of coating nanoparticles on the memory fabric with wrinkle recovery ability to enhance the wrinkle resistance and recovery of the fabric also includes: Titanium dioxide nanoparticles are prepared by a sol-gel method to prepare a nanoparticle dispersion with a concentration of 1%, and the titanium dioxide nanoparticles are sprayed on the wrinkle recovery memory fabric to obtain the wrinkle recovery memory fabric after spraying; The sprayed memory fabric with wrinkle recovery ability is dried at 80° C. for 1 hour to obtain a dried memory fabric with wrinkle recovery ability, and the dried memory fabric with wrinkle recovery ability is cured at 120° C. for 30 minutes to form a firm bond between the titanium dioxide nanoparticles and the memory fabric with wrinkle recovery ability.
Citation Information
Patent Citations
Shape memory polyurethane yarn and fabric
CN101033286A
A textile with shape memory function and treatment process thereof
CN101883889A
Production method of shape memory cotton fabric
CN104532441A
Novel shrink-proof non-ironing cotton fabric and processing method thereof
CN109914005A
Novel crease-resistant fabric
CN110948969A